Method for regenerating lead by side-blowing immersion smelting of composite iron balls
By preparing composite iron balls and immersing the molten pool in the oxygen-rich side blower for combustion and reduction reaction, the problems of low combustion efficiency of anthracite and dust from iron oxide powder foam are solved, the efficiency and economicality of smelting and regenerating lead are improved, and the Optimization of bed capacity and energy consumption per unit area.
Patent Information
- Application Number
- CN202410994621.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2044-07-24
AI Technical Summary
During the smelting and regeneration of lead, the existing oxygen-rich side blower has problems such as low combustion heat transfer efficiency of anthracite, large dust from iron oxide powder foam, and difficulty in melting red iron ore, resulting in high bed capacity and energy consumption per unit area, and soot ash production The rate and sulfur dioxide concentration are difficult to stabilize.
Compound iron balls are prepared by mixing 30% dry-based coke foam with 70% dry-based iron ore powder, and the combustion and reduction reaction is carried out by immersing the molten pool in an oxygen-rich side blower, combined with strengthening The oxygen-rich air in the material area is injected to improve the melting and reduction efficiency, and the combustion and reduction process is optimized by adjusting the air nozzle distribution and feeding ratio.
Improve the bed capacity per unit area of smelting and recycled lead and the utilization rate of lead paste, reduce the unit consumption of anthracite and iron ore powder, reduce the unit price cost of coal, reduce the dust and moisture loss of iron oxide powder foam, and steadily improve Soot production rate and sulfur dioxide concentration index.
Smart Images

Figure CN118910420A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of smelting furnaces, and in particular to a method for composite iron ball side-blowing immersion smelting recycled lead. Background Art
[0002] Oxygen-enriched side-blown furnaces are widely used to smelt lead paste and other lead-containing materials produced by the decomposition of waste lead-acid batteries to produce recycled lead. Generally, 3-5w% of iron oxide powder or red iron ore blocks, 1.5-2w% of limestone blocks, and 10-13% of anthracite blocks are added to the oxygen-enriched side-blown furnace to produce recycled lead. Its disadvantages: Anthracite has a low specific gravity of 0.8-1.0t / m 3 , and the density of the molten slag layer is 3.5-4.0t / m 3 , floating on the molten slag for combustion and reduction, the external flame heat transfer effect is poor, and the lead-containing material and anthracite form a solid-solid or gas-solid contact reduction efficiency, which is low.
[0003] 2) Disadvantages in the use of iron oxide powder or rutile block auxiliary materials: iron oxide powder content: Fe60-65w%, SiO23-5w% and moisture 8-12%, large dust is generated during powder unloading and feeding, high moisture loss is large and it is not conducive to slag preparation; rutile block content: Fe50-60w%, SiO25-8w%, moisture 3-5%, high silica is not conducive to the flow of molten slag, and the block is dense and difficult to melt.
[0004] 3) There are usually 10 tuyere for the oxygen-enriched side-blowing furnace, which are staggered on the left and right. There are many materials in the feeding area but the tuyere are evenly distributed. The amount of oxygen-enriched air sprayed is insufficient and the efficiency is low, which is not conducive to material melting and reduction, and affects the bed capacity per unit area.
[0005] 4) Oxygen-enriched side-blown furnace smelting lead paste to produce recycled lead is optimal: bed capacity per unit area 80t / (m 2 .d), anthracite consumption is 245Kg / t, iron oxide consumption is 50Kg / t or red iron ore consumption is 53Kg / t, energy consumption and auxiliary material cost is 340 yuan / ton, ash production rate is 18w%, sulfur dioxide concentration in flue gas during oxidation period is 2.5-4.5v% and difficult to stabilize. For many years, there has been no new method to break through the above indicators. Summary of the invention
[0006] The object of the present invention is to provide a method for smelting recycled lead by side-blowing immersion of composite iron balls, which adopts coke foam and iron ore powder to form composite iron balls by mixing and pressing balls, replacing the auxiliary materials of iron oxide scale or rutile. The composite iron balls have a large specific gravity, are immersed in the molten pool of lead-containing materials in the oxygen-enriched side-blown furnace to smelt recycled lead, contact with the molten slag for combustion and reduction reaction, enhance the reaction efficiency through solid-liquid mass transfer and heat transfer, and improve the utilization rate of coal. Strengthen the oxygen-enriched air in the feeding area, accelerate the melting of iron oxide, and enhance the reduction of lead oxide. More importantly, the unit price cost of coke foam is low relative to anthracite, which improves the overall utilization efficiency of coal and iron, and can also reduce the unit price cost of coal. It not only solves the low heat transfer efficiency and poor reduction effect of lead-containing materials and anthracite combustion, but also solves the problems of dust and loss of iron oxide scale and difficulty in melting rutile ore. More importantly, the key indicators of the production of recycled lead by smelting lead paste in the oxygen-enriched side-blown furnace have reached a historical high.
[0007] To achieve the above object, the present invention provides the following technical solutions: A method for composite iron ball side-blowing immersion smelting of recycled lead, comprising: (1) Preparation of composite iron balls: 30% dry basis coke foam and 70% dry basis iron ore are evenly mixed and subjected to the processes of ball pressing, drying and screening to form composite iron balls; (2) Feeding lead-containing materials, composite iron balls, limestone blocks, and anthracite in a certain proportion, transporting them to a mixer for mixing, and then transporting them to the feeding port at the top of the side-blown furnace and adding them into the molten pool of the oxygen-enriched side-blown furnace; (3) Water-cooled air nozzles are provided on both sides of the molten pool to spray oxygen-enriched air into the molten pool. Due to their high specific gravity, the composite iron balls are immersed in the molten pool under the impact of wind pressure. Lead paste and other lead-containing materials, limestone blocks, and anthracite are mixed and piled on the surface of the molten pool due to their low specific gravity. The materials are smelted in the molten pool in two stages: oxidation smelting and reduction smelting. Smelting in the oxidation period is 6.5-7 hours: the coke foam and anthracite in the composite iron balls generate a lot of heat under the combustion support of oxygen-rich air, continuously melting the mixed materials, and most of the PbSO4 in the lead-containing materials is decomposed into PbO at a temperature above 850°C; the coke foam in the composite iron balls immersed in the molten pool preferentially and rapidly reacts with PbO for reduction, and a large amount of liquid lead gathers and settles to the bottom of the molten pool, and then flows out through the siphon channel for refining process to produce refined lead; During the reduction period, the smelting is performed for 1-1.5 hours, and only anthracite is added without other materials, so that the PbSO4 in the molten pool is further decomposed. The PbO in the molten pool is intensively reduced by the anthracite to form liquid lead and separate from the upper slag. After slag sampling, if the upper slag contains less than 1.2% Pb, the slag outlet is opened to discharge the slag; the molten slag is impacted by a large amount of flowing water to form small granular water-quenched slag; (4) Slag type and reducing atmosphere control Insert an iron rod into the furnace to take out the slag probe, and use an X-ray fluorescence instrument to detect the contents of Pb, FeO, SiO2, and CaO in the slag probe. The smelting control requirements during the oxidation period are Pb: 18-23%, FeO: 20-22%, SiO2: 19-21%, and CaO: 8-11%. If they are not within this range, the feeding speed of anthracite, composite iron balls, and limestone blocks should be increased or decreased to adjust. (5) The smelting reaction produces flue gas containing sulfur dioxide and smoke. After dust reduction and cooling, it enters the electrostatic precipitator for further dust reduction, and finally enters the full ion desulfurization and acid production system to produce refined acid.
[0008] Preferably, in step (1), the 30% coke foam material formula is: fixed carbon ≥81%, volatile matter ≤6%, ash ≤13%, water ≤6.5%, and particle size 0-3mm; the 70% iron ore powder material formula is: Fe ≥60%, SiO2 ≤6%, water ≤12%, and particle size 0-2mm.
[0009] Preferably, in step (1), the quality standard of the composite iron ball is: spherical particle size 10-50mm, ≤10mm sieve undersize ≤8%, Fe: 42-45%, fixed carbon: 21-24%, SiO2≤5%, water≤4%, specific gravity 4.5-5.2t / m 3 .
[0010] Preferably, in step (2), the feed ratio is 100w% of lead-containing material, 4-4.2w% of composite iron balls, 1.6-1.8w% of limestone blocks, and 10.5-11% of anthracite blocks.
[0011] Preferably, in step (2), the feed rate of lead-containing waste is 46-60 t / h, the feed rate of limestone blocks is 1.6-1.8w% of the feed rate of lead-containing waste, the feed rate of composite iron balls is 4.0-4.2w% of the feed rate of lead-containing waste, and the feed rate of anthracite is 11.5-12w% of the feed rate of lead-containing waste minus 28-30% of the feed rate of composite iron balls.
[0012] Preferably, in step (3), during the oxidation period, the total amount of oxygen added is the carbon content of the anthracite plus the carbon content of the composite iron ball 90-102Nm 3 / kg, the number of air nozzles is 10-12, and the oxygen concentration is 75-78%; during the reduction period: the amount of anthracite is 5t / h, the number of air nozzles is 8-10, and the total amount of oxygen added is 4000Nm 3 , oxygen concentration 50-55%.
[0013] Preferably, tuyere A1, tuyere A2, tuyere A3, tuyere A4, tuyere A5, tuyere A6, tuyere A7, tuyere A8, tuyere A9, tuyere A10 and tuyere B1, tuyere B2, tuyere B3, tuyere B4, tuyere B5, tuyere B6, tuyere B7, tuyere B8, tuyere B9, tuyere B10 are respectively arranged on both sides of the molten pool, wherein: tuyere A4 and tuyere B5 have a caliber of 32 mm, and the others have a caliber of 30 mm; during the oxidation period, they are normally opened In production, tuyere A1, A3, A4, A5, A7, A9, B2, B4, B5, B6, B8 and B10 control the pressure at 0.09-0.11MPa and the air volume of a single oxygen-enriched air at 600-650Nm3 / h. During smelting in the oxidation period, there are 3 tuyere on each side of the feeding area and the diameter of one tuyere is enlarged to enhance the injection of oxygen-enriched air, strengthen the combustion in this area and accelerate the melting and reduction of materials.
[0014] Compared with the prior art, the present invention has the following beneficial effects: 1. Composite iron balls replace iron oxide scale or red iron ore to avoid insufficient physical properties.
[0015] The composite iron balls are spherical, have high strength, are not easy to form fragments, generate little dust during loading and unloading, and are easy to unload on unloading machines equipped with ventilation hoods, avoiding iron oxide powder dust and spillage pollution and loss caused by loaders.
[0016] 2. The composite iron balls are intensively immersed in the molten pool for smelting in the feeding area, and the melting and reduction effects are enhanced.
[0017] First, the coke foam and anthracite in the composite iron balls generate a large amount of heat under the assistance of oxygen-rich air, and burn and reduce in contact with the molten slag. The reaction efficiency is enhanced through solid-liquid mass transfer and heat transfer, the utilization rate of coal is improved, and the smelting of materials is accelerated.
[0018] Second, due to its high specific gravity, the composite iron balls are immersed in the molten pool under the impact of wind pressure. The coke foam in the composite iron balls reacts with PbO quickly and preferentially, thereby enhancing the reduction effect.
[0019] Thirdly, there are three tuyere nozzles on the left and right sides of the feeding area, and the diameter of one tuyere nozzle is enlarged to enhance the injection of oxygen-rich air, strengthen the combustion in the feeding area, and accelerate the melting and reduction of materials.
[0020] 3. Use low-priced coke foam to replace anthracite to reduce costs.
[0021] The unit price of coke foam is 900 yuan / ton, and the unit price of anthracite is 1,200 yuan / ton, and the general price difference is 300 yuan / ton; the unit price of composite iron balls and oxidized iron scale are both 900 yuan / ton, and the relative price difference can reduce costs by 14 yuan / ton.
[0022] Various economic and technological achievements have reached new historical highs, with significant comprehensive benefits.
[0023] The economic and technical indicators of the process for smelting recycled lead in an oxygen-enriched side-blown furnace have been significantly improved. The bed capacity per unit area has increased from 80t / (m2.d) to 84.2t / (m2.d), the ash production rate has dropped from 18w% to 16w%, and the sulfur dioxide concentration in flue gas during the oxidation period has changed from 2.5-4.5v% to 3.5-4.2v% and is more stable.
[0024] Compared with the historical best level, the unit consumption of anthracite has dropped from 245kg / t to 228kg / t, the unit consumption of composite iron balls has increased from 50kg / t to 59kg / t, and the cost of energy consumption and auxiliary materials has dropped from 340 yuan / ton to 316 yuan / ton, reducing the cost by 14 yuan / ton. If it is promoted nationwide, based on 5 million tons of recycled lead, it can save 70 million yuan in costs annually. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a schematic diagram of the position of the air nozzle of the present invention.
[0026] Figure 2 It is a schematic diagram of the process of the present invention.
[0027] In the figure: A1-10 / B1-10 air nozzle, C1-C2 charging port, D siphon lead discharge port, E slag discharge port, 1-1 lead-containing material, 1-2 composite iron balls, 1-3 limestone blocks, 1-4 anthracite, 2-1 / 2-2 belts, 3 round shaft drum mixer, 4 discharge port, 5 side-blowing furnace, 6 waste heat boiler, 7 electrostatic precipitator, 8 full ion desulfurization and acid making system, 9 slag discharge port, 10 siphon lead discharge port. DETAILED DESCRIPTION
[0028] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation mode, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0029] like Figure 2 As shown, a method for composite iron ball side-blowing immersion smelting recycled lead comprises: 1. Preparation method and quality standard of composite iron balls 30% dry coke foam and 70% dry iron ore are mixed evenly and made into composite iron balls through the processes of ball pressing, drying and screening. Material standards of 70% iron ore powder: Fe ≥ 60%, SiO2 ≤ 6%, water ≤ 12%, particle size 0-2mm. Material standards of 30% coke foam: low calorific value ≥ 6100 kcal / Kg, fixed carbon ≥ 81%, volatile matter ≤ 6%, ash ≤ 13%, water ≤ 6.5%, particle size 0-3mm. Quality standards of composite iron balls: spherical particle size 10-50mm, ≤ 10mm sieve undersize ≤ 8%, Fe: 42-45%, fixed carbon: 21-24%, SiO2 ≤ 5%, water ≤ 4%, specific gravity 4.5-5.2t / m 3 .
[0030] 2. Composite iron ball side blowing immersion smelting recycled lead process Lead paste and other lead-containing materials 1-1, composite iron balls 1-2, limestone blocks 1-3, and anthracite 1-4 are fed through a quantitative belt silo according to the ratio of lead-containing materials 100w%, composite iron balls 4-4.2w%, limestone blocks 1.6-1.8w%, and anthracite blocks 10.5-11%, and then conveyed to a round shaft drum mixer 3 for mixing through a belt 2-1, and then conveyed to a top feeding port of a side-blown furnace 5 through a belt 2-2, and finally added to a molten pool of an oxygen-enriched side-blown furnace through a discharge port 4; Water-cooled air nozzles are arranged on both sides of the molten pool to spray oxygen-rich air into the molten pool. Due to their high specific gravity, the composite iron balls are immersed in the molten pool under the impact of wind pressure. Lead paste and other lead-containing materials, limestone blocks, and anthracite are mixed and piled on the surface of the molten pool due to their low specific gravity. The materials are divided into two stages in the molten pool: oxidation smelting and reduction smelting. The oxidation period is 6.5-7 hours: the coke foam and anthracite in the composite iron balls generate a lot of heat under the combustion of oxygen-rich air, which continuously melts the mixed materials. Most of the PbSO4 in the lead-containing materials decomposes into PbO at a temperature above 850°C. The coke foam in the composite iron balls immersed in the molten pool reacts with PbO first and quickly, and a large amount of liquid lead gathers and settles to the bottom of the molten pool, and then flows out through the siphon to produce refined lead in the refining process; During the reduction period, the smelting is performed for 1-1.5 hours, that is, only anthracite is added without other materials, so that the PbSO4 in the molten pool is further decomposed, and the PbO in the molten pool is intensively reduced by the anthracite to form liquid lead and separate from the upper slag. After slag sampling, if the upper slag contains less than 1.2% Pb, the slag outlet is opened to discharge the slag. The molten slag is impacted by a large amount of flowing water to form small granular water-quenched slag; The smelting reaction produces flue gas containing sulfur dioxide and smoke dust, which passes through the vertical waste heat boiler 6 for dust reduction and temperature reduction, then enters the electrostatic precipitator 7 for further dust reduction, and finally enters the full ion desulfurization and acid production system 8 to produce refined acid; 3. Quantitative batching and oxygen-enriched air usage The feeding rate of lead-containing waste such as lead paste is 46-60t / h, the feeding rate of limestone blocks is 1.6-1.8w% of the feeding rate of lead-containing waste, the feeding rate of composite iron balls is 4.0-4.2w% of the feeding rate of lead-containing waste, and the feeding rate of anthracite is 11.5-12w% of the feeding rate of lead-containing waste minus 28-30% of the feeding rate of composite iron balls. Oxidation period: the total amount of oxygen added is the carbon content of anthracite plus the carbon content of composite iron balls 90-102Nm3 / kg, the number of air nozzles is 10-12, and the oxygen concentration is 75-78%; reduction period: only 5t / h of anthracite is added, no other materials are added, the number of air nozzles is 8-10 oxygen, the total amount of oxygen added is about 4000Nm3, and the oxygen concentration is 50-55%.
[0031] 4. Nozzle distribution method like Figure 1 As shown, A1-10 and B1-10 are tuyere, whose main function is to spray oxygen-enriched air into the molten slag layer in the furnace to assist the combustion of coal. Among them, the diameters of A4 and B5 are 32mm, and the diameters of the others are 30mm. During the oxidation period, tuyere A1, A3, A4, A5, A7, A9 and B2, B4, B5, B6, B8, B10 are normally opened for production, and the pressure is controlled at 0.09-0.11MPa, and the air volume of a single oxygen-enriched air is 600-650Nm3 / h. During the oxidation period smelting, there are 3 tuyere on the left and right sides of the charging area, and the diameter of one tuyere is enlarged to enhance the injection of oxygen-enriched air, strengthen the combustion in this area, and accelerate the melting and reduction of materials. Especially under the action of the solid-liquid reaction of the composite iron ball immersed in the molten slag, the reaction efficiency in this area is higher.
[0032] 5. Slag type and reducing atmosphere control After the composite ductile iron contains coke foam and is immersed in the molten pool, its reducibility is enhanced, and excessive reduction also promotes the formation of PbS side reaction, which leads to an increase in the slag content of the output secondary lead. Therefore, it is very important to control the oxygen-enriched side-blowing slag type and reducing atmosphere. This technical method is to insert an iron rod into the furnace to take out the slag probe, and use an X-ray fluorescence instrument to detect the content of Pb, FeO, SiO2, and CaO in the slag probe. The oxidation period smelting control requires Pb: 18-23%, FeO: 20-22%, SiO2: 19-21%, and CaO: 8-11%. If it is not within this range, the feeding speed of anthracite, composite iron balls, and limestone blocks should be increased or decreased to adjust.
[0033] Experimental data: On May 28, 2024, a batch of composite iron balls was outsourced for processing. The results of the factory inspection were as follows: ≤10mm undersize: 7.63%, Fe: 44.2%, fixed carbon: 21.7%, SiO2: 3.2%, water: 2.4%, specific gravity 4.8t / m 3 .
[0034] The trial production will be organized on May 29, 2024, and the details are as follows: During the oxidation period, lead paste and other lead-containing materials are dosed at a rate of 58t / h, composite iron balls 2.1t / h, limestone blocks 0.93t / h, and anthracite 5.93t / h through a quantitative feeder; nozzles A1, A3, A4, A5, A7, A9 and B2, B4, B5, B6, B8, B10 are used for production, and the pressure is controlled at 0.098MPa, and the oxygen flow rate is 5851Nm 3 / h, air volume 1224Nm 3 / h. After 2 hours of feeding, the following detection results were obtained: Pb: 19.2%, FeO: 20.1%, SiO2: 19.5%, CaO: 8.9%, S: 1.61%. After 6.5 hours of feeding, the reduction period began.
[0035] During the reduction period, anthracite was quantitatively fed at 5t / h, and nozzles A1, A3, A5, A7, A9 and B2, B4, B6, B8, B10 were opened for production, with a controlled pressure of 0.092MPa, an oxygen flow of 2051Nm3 / h, and an air volume of 2421Nm3 / h. The reduction time was 50 minutes, and the slag discharge time was 40 minutes. The discharged water-quenched slag was tested as follows: Pb: 0.87%, FeO: 28.3%, SiO2: 27.4%, CaO: 13.2%, S: 0.24%.
[0036] The materials put into the day included: 1096.2t of lead-containing materials, 34.93t of composite iron balls, 17.6t of limestone blocks and 134.9t of anthracite; the output included: 591.2t of recycled lead, 64.3t of water-quenched slag and 175.6t of fly ash.
[0037] Compared with the prior art, the present invention avoids the dust and loss of iron oxide or red iron ore, improves the melting and reduction efficiency of lead paste lead-containing materials in the process of smelting recycled lead in an oxygen-enriched side-blown furnace, significantly improves the bed capacity per unit area, and significantly reduces the cost of anthracite and composite iron balls. Indicators such as ash production rate and flue gas sulfur dioxide concentration are stable and improving and are significantly better than current industry indicators.
[0038] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A method for smelting recycled lead by side-blowing immersion of composite iron balls, Its characteristics are: include: (1) preparing composite iron balls by mixing 30% dry basis coke foam and 70% dry basis iron ore evenly and subjecting the mixture to ball pressing, drying and screening to prepare composite iron balls; (2) Feeding lead-containing materials, composite iron balls, limestone blocks, and anthracite in a certain proportion, transporting them to a mixer for mixing, and then transporting them to the feeding port at the top of the side-blown furnace and adding them into the molten pool of the oxygen-enriched side-blown furnace; (3) Water-cooled air nozzles are provided on both sides of the molten pool to spray oxygen-enriched air into the molten pool. Due to their high specific gravity, the composite iron balls are immersed in the molten pool under the impact of wind pressure. Lead paste and other lead-containing materials, limestone blocks, and anthracite are mixed and piled on the surface of the molten pool due to their low specific gravity. The materials are smelted in the molten pool in two stages: oxidation smelting and reduction smelting. Oxidation period smelting 6.5-7 hours: The coke foam and anthracite in the composite iron ball generate a lot of heat under the combustion of oxygen-rich air, continuously melting the mixed material, and PbSO in the lead-containing material 4 At temperatures above 850°C, most of it decomposes into PbO; the coke foam in the composite iron balls immersed in the molten pool preferentially and rapidly reacts with PbO for reduction, and a large amount of liquid lead gathers and settles to the bottom of the molten pool, and then flows out through the siphon channel for refining process to produce refined lead; During the reduction period, the smelting is carried out for 1-1.5 hours, and only anthracite is added without adding other materials, so that PbSO 4 Further decomposition, the PbO in the molten pool is intensively reduced by anthracite to form liquid lead and separate from the upper slag. After slag sampling, if the upper slag contains less than 1.2% Pb, the slag outlet is opened to discharge the slag; the molten slag is impacted by a large amount of flowing water to form small granular water-quenched slag; (4) Slag type and reducing atmosphere control Insert the iron rod into the furnace to take out the slag probe, and use the X-ray fluorescence instrument to detect the Pb, FeO and SiO in the slag probe. 2 , CaO content, oxidation period smelting control requirements Pb: 18-23%, FeO: 20-22%, SiO 2 : 19-21%, CaO: 8-11%; if it is not within this range, the feeding speed of anthracite, composite iron balls and limestone blocks should be increased or decreased to adjust.
2. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 1, Its characteristics are: In step (1), the 30% coke foam material formula is: fixed carbon ≥ 81%, volatile matter ≤ 6%, ash ≤ 13%, water ≤ 6.5%, and particle size 0-3 mm; the 70% iron ore powder material formula is: Fe ≥ 60%, SiO 2 ≤6%, water ≤12%, particle size 0-2mm.
3. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 1 or 2, Its characteristics are: In the step (1), the quality standard of the composite iron ball is: spherical particle size 10-50mm, ≤10mm sieve undersize ≤8%, Fe: 42-45%, fixed carbon: 21-24%, SiO 2 ≤5%, water ≤4%, specific gravity 4.5-5.2t / m 3 .
4. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 1, Its characteristics are: In the step (2), the quantitative feeding in a certain proportion is 100w% of lead-containing material, 4-4.2w% of composite iron balls, 1.6-1.8w% of limestone blocks, and 10.5-11w% of anthracite blocks.
5. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 4, Its characteristics are: In the step (2), the feed rate of lead-containing waste is 46-60 t / h, the feed rate of limestone blocks is 1.6-1.8w% of the feed rate of lead-containing waste, the feed rate of composite iron balls is 4.0-4.2w% of the feed rate of lead-containing waste, and the feed rate of anthracite is 11.5-12w% of the feed rate of lead-containing waste minus 28-30% of the feed rate of composite iron balls.
6. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 1, Its characteristics are: In the step (3), during the oxidation period, the total amount of oxygen added is equal to the carbon content of the anthracite plus the carbon content of the composite iron ball 90-102Nm 3 / kg, the number of tuyeres is 10-12, and the oxygen concentration is 75-78%; reduction period smelting: anthracite volume 5t / h, the number of tuyeres is 8-10, and the total amount of oxygen is 4000Nm 3 , oxygen concentration 50-55%.
7. A method for smelting recycled lead by side-blowing immersion of composite iron balls as claimed in claim 1 or 6, Its characteristics are: The two sides of the molten pool are respectively provided with tuyere A1, tuyere A2, tuyere A3, tuyere A4, tuyere A5, tuyere A6, tuyere A7, tuyere A8, tuyere A9, tuyere A10 and tuyere B1, tuyere B2, tuyere B3, tuyere B4, tuyere B5, tuyere B6, tuyere B7, tuyere B8, tuyere B9, tuyere B10, among which: tuyere A4 and tuyere B5 have a diameter of 32 mm, and the others have a diameter of 30 mm; during the oxidation period, the tuyere is normally opened. A1, tuyere A3, tuyere A4, tuyere A5, tuyere A7, tuyere A9 and tuyere B2, tuyere B4, tuyere B5, tuyere B6, tuyere B8, tuyere B10 are produced, the pressure is controlled at 0.09-0.11MPa, and the air volume of a single oxygen-enriched air is 600-650Nm3 / h; during the smelting in the oxidation period, there are 3 tuyere on the left and right sides of the feeding area and the diameter of one tuyere is enlarged to enhance the injection of oxygen-enriched air, strengthen the combustion in this area, and accelerate the melting and reduction of materials.
Citation Information
Patent Citations
Smelting reduction method for secondary lead
CN105648233A
Oxygen-enriched side-blown intensified smelting furnace capable of efficiently processing secondary materials containing lead
CN106766971A
Waste lead-acid battery lead plaster molten bath smelting treatment method
CN107083488A
Treatment method for secondary lead-containing material
CN109439924A
Smelting process for efficient and energy-saving regenerated lead
CN110551899A