Cast iron piston and machining method
By adopting an integrated structure and CNC lathe finishing method, the performance problem of cast iron piston welded sealed cooling oil cavity is solved, the stability and cooling effect of the piston is improved, and the service life of the piston is extended.
Patent Information
- Application Number
- CN202310508674.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-11-08
AI Technical Summary
The existing cast iron pistons adopt welding-type closed cooling oil chambers. The performance at the welding joints is poor, and debris such as welding slag are difficult to clean, which affects the cooling effect of the oil chamber and the life of the piston.
Cast iron piston adopts an integrated structure, the piston head and skirt are integrally formed, and an annular cooling oil passage is provided inside, and designed through oil inlet, oil outlet and process holes to ensure the integrity and cleanliness of the cooling oil passage. , use CNC lathe for finishing to improve surface quality.
It improves the overall performance stability and service life of the piston, ensures the effectiveness and internal cleaning of the cooling oil chamber, and enhances product reliability.
Smart Images

Figure CN118911863A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pistons and processing methods, in particular to a cast iron piston and a processing method. Background Art
[0002] The piston is a reciprocating part in the cylinder block of a car engine. Pistons can be divided into cast iron pistons, steel pistons, aluminum alloy pistons and combined pistons according to the materials used in their manufacture. Cast iron pistons have been widely used due to their low cost and good processing performance. However, the design of the cooling oil chamber of the cast iron piston is relatively complicated. For example, Chinese invention patent application No. 202110548352.0 discloses a high-performance friction-welded cast iron piston and a preparation method thereof, which adopts a welded closed cooling oil chamber method, that is, the head and skirt of the piston adopt a split design method, and cold zone oil channels are respectively provided at the corresponding positions of the head and skirt, and then friction welding is used to form a closed cooling oil channel cavity. However, using this method, not only is the performance of the welding joint unstable, but also welding slag and other debris are difficult to clean, affecting the cooling effect of the oil chamber and the life of the piston. Summary of the invention
[0003] In view of the problem that the existing cast iron piston adopts a welded closed cooling oil chamber, the performance of the welded joint is poor, and it is difficult to clean up debris such as welding slag, which affects the cooling effect of the oil chamber and the life of the piston, the present invention provides a cast iron piston with an integrated structure, which has more stable piston performance and is not affected by other impurities, thereby improving product reliability.
[0004] The technical solution is as follows: a cast iron piston, comprising a piston head and a piston skirt, characterized in that the piston head and the piston skirt are an integrally formed structure, an annular cooling oil channel is provided inside the piston head, an oil inlet hole and an oil outlet hole are provided in one diagonal direction of the cooling oil channel, and process holes are provided in the other diagonal direction of the cooling oil channel.
[0005] It is further characterized in that: the cast iron piston is made of QT900-5 ductile iron material, and has a tensile strength of ≥900MPa, a yield strength of ≥485MPa, and an elongation of ≥5%. The QT900-5 ductile iron material has a spheroidization level of 1-3, a graphite size of 5-8, a pearlite content of ≥85%, and a hardness of 280-360HB; The cast iron piston is made of QT700-5 ductile iron material and has a tensile strength of >700MPa, a yield strength of >420MPa, and a hardness of 225-305HB.
[0006] A method for processing the above cast iron piston, characterized in that: The method comprises the following steps: S1, placing the cast iron piston blank obtained by rough machining with its head facing downward and clamping and fixing it with a special fixture; S2, using a CNC lathe to roughly machine the outer circle of the skirt, the end face and the stopper of the cast iron piston blank, and to roughly machine the head end face and the combustion chamber of the cast iron piston blank; S3, firstly rough boring the pin hole of the cast iron piston blank; S4, using a CNC lathe to drill oil holes and oil outlet holes at corresponding positions of the cast iron piston blank, and then using a tapered reamer to process the process hole of the cast iron piston blank to a reasonable size and tap the thread, and installing a blind screw to thread the process hole; S5, using a finishing lathe for finishing, the speed of the finishing lathe is 180-250r / min and the feed is 0.1-0.3mm / r to process the head, the first ring groove, the second ring groove and the pressure relief groove of the cast iron piston blank, the speed of the finishing lathe is 180-250r / min and the feed is 0.3-0.5mm / r to finish the end face of the head of the cast iron piston blank and the combustion chamber, the speed of the finishing lathe is 2500-3500r / min and the feed is 500-700mm / min to finish the valve pit of the cast iron piston blank; S6, the speed of the finishing lathe is 200-300 r / min and the feed is 0.3-0.7 mm / r for finishing the skirt periphery of the cast iron piston blank, the speed of the lathe is 4000-5500 r / min and the feed is 0.15-0.5 mm / r for finishing the pin hole and the cutting groove of the cast iron piston blank, the speed of the finishing lathe is 150-250 r / min and the feed is 0.15-0.25 mm / r for finishing the stop end face of the cast iron piston blank; S7, using ECK6520BL CNC piston profiled outer circle vertical lathe to rough-process the skirt outer circle, the first ring groove, the second ring groove and the pressure relief groove of the cast iron piston blank, at this time, the speed of the ECK6520BL CNC piston profiled outer circle vertical lathe is 500-650r / min, the feed groove is 20-50mm / min, and the outer circle is 200-300mm; S8. Use ETK2708A CNC steel piston special-shaped pin hole boring machine to fine bore the pin hole of the cast iron piston blank to a standard size. At this time, the rotation speed of the ETK2708A CNC steel piston special-shaped pin hole boring machine is 1000-1500 r / min, and the feed groove is 100-300 mm / min.
[0007] After adopting the above structure, since the head and skirt of the cast iron piston are an integrally formed structure, there is no weak interface, which makes the overall performance more stable and improves the service life. At the same time, there are no impurities in the cooling oil cavity, thus ensuring the cooling effect. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figure 1 It is a schematic diagram of the overall structure of the present invention; Figure 2 It is a schematic diagram of the overall structure of the present invention in another direction; Figure 3 It is a bottom view of the overall structure of the present invention; Figure 4 It is a top view of the overall structure of the present invention; Figure 5 For the present invention Figure 4 Structural cross-section view along BB direction. DETAILED DESCRIPTION
[0009] like Figures 1 to 5 As shown, a cast iron piston comprises a piston head 1 and a piston skirt 2. The piston head 1 and the piston skirt 2 are an integrally formed structure. An annular cooling oil channel 3 is provided inside the piston head 1. An oil inlet hole 4 and an oil outlet hole 5 are provided in one diagonal direction of the cooling oil channel 3. Process holes 6 are provided in another diagonal direction of the cooling oil channel 3. The process holes 6 are threaded holes and are closed after being threadedly connected by corresponding screws. Two process holes are used on the inner cooling oil channel 3 to facilitate the casting of the cooling oil channel.
[0010] Specifically, the center of the piston head 1 is a combustion chamber 12 , and a valve pit 11 is provided on the end surface of the piston head 1 . The valve pit 11 includes four arc-shaped notch structures with a larger inner opening and a smaller outer opening.
[0011] Specifically, a first annular groove 13 , a second annular groove 14 and a pressure relief groove 15 are provided on the outer wall of the piston head 1 .
[0012] Furthermore, the cast iron piston of the present invention is made of QT900-5 ductile iron material, and has a tensile strength ≥900MPa, a yield strength ≥485MPa, and an elongation ≥5%. The higher tensile strength and yield strength ensure that the product can withstand greater pressure during work. At the same time, the spheroidization level of the QT900-5 ductile iron material is 1-3, the graphite size is 5-8, the pearlite content is ≥85%, and the hardness is 280-360HB. The higher hardness provides good wear resistance. The above requirements ensure that the mechanical properties of the cast iron piston are close to or even reach the mechanical properties of the steel piston.
[0013] Furthermore, the cast iron piston may be made of QT700-5 ductile iron material with a tensile strength of >700 MPa, a yield strength of >420 MPa, and a hardness of 225-305 HB.
[0014] Furthermore, the cast iron piston adopts an integral structure, that is, its piston head and piston skirt are integrated, and the internal cooling oil channel is directly cast, which is different from the split welded cast iron piston on the market (the split piston is a split head and skirt, and the two parts are processed separately and then welded). It not only reduces the machining and welding processes and improves production efficiency, but also has no weak interfaces, making the overall performance more stable and increasing the service life. At the same time, there are no impurities inside the cooling oil chamber, thereby ensuring the cooling effect.
[0015] The present invention provides a processing method based on the above cast iron piston. The method comprises the following steps: S1, placing the head of the cast iron piston blank obtained by rough machining downward and clamping it with a special fixture, wherein the head end face of the cast iron piston blank is positioned by a flat top, and the clamping body of the special fixture is inserted into the skirt of the cast iron piston blank to be tensioned, and then the flat top at the end face is released to start rough machining; S2, in order to ensure that the final cast iron piston formed by the cast iron piston blank meets the processing size and shape and position tolerances to reach the standard value, the standard value is 0.03 for coaxiality, 0.02 for parallelism, and 0.15 for position, rough machining is performed first, and then fine machining is performed, using a CNC lathe for rough machining, first rough machining the skirt outer circle 23, the end face 24 and the stop 22 of the cast iron piston blank, and then rough machining the head end face 16 and the combustion chamber 12 of the cast iron piston blank; S3, firstly rough boring the pin hole 21 of the cast iron piston blank; S4, using a CNC lathe to drill the oil hole 4 and the oil outlet hole 5 at the corresponding positions of the cast iron piston blank, and then using a taper reamer to process the process hole of the cast iron piston blank to a reasonable size and tap the thread, and install a blind screw to thread the process hole; S5, using a finishing lathe for finishing, the speed of the finishing lathe is 180-250r / min and the feed is 0.1-0.3mm / r to process the head, the first ring groove, the second ring groove and the pressure relief groove of the cast iron piston blank, the speed of the finishing lathe is 180-250r / min and the feed is 0.3-0.5mm / r to finish the end face of the head of the cast iron piston blank and the combustion chamber, the speed of the finishing lathe is 2500-3500r / min and the feed is 500-700mm / min to finish the valve pit of the cast iron piston blank; S6, the speed of the finishing lathe is 200-300 r / min and the feed is 0.3-0.7 mm / r for finishing the skirt periphery of the cast iron piston blank, the speed of the lathe is 4000-5500 r / min and the feed is 0.15-0.5 mm / r for finishing the pin hole and the cutting groove of the cast iron piston blank, the speed of the finishing lathe is 150-250 r / min and the feed is 0. 15~0.25mm / r finish machining the stop end face of the cast iron piston blank; S7, using ECK6520BL CNC piston profiled outer circle vertical lathe to rough-machine the skirt outer circle 23, the first ring groove 13, the second ring groove 14 and the pressure relief groove 15 of the cast iron piston blank, at this time, the speed of the ECK6520BL CNC piston profiled outer circle vertical lathe is 500~650r / min, the feed groove is 20~50mm / min, and the outer circle is 200~300mm; S8. Use ETK2708A CNC steel piston special-shaped pin hole boring machine to fine bore the pin hole of the cast iron piston blank to the standard size. At this time, the speed of the ETK2708A CNC steel piston special-shaped pin hole boring machine is 1000-1500r / min, and the feed groove is 100-300mm / min to complete the processing.
[0016] Among them, S5 can choose to use VL-4 lathe or ERG0 315Y vertical lathe for finishing lathe.
[0017] Among them, the S5 can choose to use the VL-4 lathe or the TANDEM315 vertical lathe for finishing lathes.
[0018] Among them, S7 involves ECK6520BL CNC piston special-shaped external cylindrical vertical lathe, and you can also choose to use ERG0 260 OT vertical lathe.
[0019] Among them, S8 involves the ETK2708A CNC steel piston special-shaped pin hole boring machine, and you can also choose to use the ERG0 260 PH vertical boring machine.
[0020] The above are only preferred specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by anyone familiar with the technology within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A cast iron piston comprising a piston head and a piston skirt, Features: The piston head and the piston skirt are an integrally formed structure, an annular cooling oil channel is provided inside the piston head, an oil inlet hole and an oil outlet hole are provided in one diagonal direction of the cooling oil channel, and process holes are provided in the other diagonal direction of the cooling oil channel.
2. A cast iron piston according to claim 1, Features: The cast iron piston is made of QT900-5 ductile iron material, and has a tensile strength of ≥900MPa, a yield strength of ≥485MPa, and an elongation of ≥5%. The QT900-5 ductile iron material has a spheroidizing level of 1-3, a graphite size of 5-8, a pearlite content of ≥85%, and a hardness of 280-360HB.
3. A cast iron piston according to claim 1, Features: The cast iron piston is made of QT700-5 ductile iron material and has a tensile strength of >700MPa, a yield strength of >420MPa, and a hardness of 225-305HB.
4. A method for processing a cast iron piston according to any one of claims 1 to 3, Features: The following steps are involved: S1. Place the cast iron piston blank obtained by rough machining with its head facing downward and fix it with a special fixture; S2, using a CNC lathe to roughly machine the outer circle of the skirt, the end face and the stopper of the cast iron piston blank, and to roughly machine the head end face and the combustion chamber of the cast iron piston blank; S3, firstly rough boring the pin hole of the cast iron piston blank; S4, using a CNC lathe to drill oil holes and oil outlet holes at corresponding positions of the cast iron piston blank, and then using a tapered reamer to process the process hole of the cast iron piston blank to a reasonable size and tap the thread, and installing a blind screw to thread the process hole; S5, using a finishing lathe for finishing, the speed of the finishing lathe is 180-250r / min and the feed is 0.1-0.3mm / r to process the head, the first ring groove, the second ring groove and the pressure relief groove of the cast iron piston blank, the speed of the finishing lathe is 180-250r / min and the feed is 0.3-0.5mm / r to finish the end face of the head of the cast iron piston blank and the combustion chamber, the speed of the finishing lathe is 2500-3500r / min and the feed is 500-700mm / min to finish the valve pit of the cast iron piston blank; S6, the speed of the finishing lathe is 200-300 r / min and the feed is 0.3-0.7 mm / r for finishing the skirt periphery of the cast iron piston blank, the speed of the lathe is 4000-5500 r / min and the feed is 0.15-0.5 mm / r for finishing the pin hole and the cutting groove of the cast iron piston blank, the speed of the finishing lathe is 150-250 r / min and the feed is 0.15-0.25 mm / r for finishing the stop end face of the cast iron piston blank; S7, using ECK6520BL CNC piston profiled outer circle vertical lathe to rough-process the skirt outer circle, the first ring groove, the second ring groove and the pressure relief groove of the cast iron piston blank, at this time, the speed of the ECK6520BL CNC piston profiled outer circle vertical lathe is 500-650r / min, the feed groove is 20-50mm / min, and the outer circle is 200-300mm / min; S8. Use ETK2708A CNC steel piston special-shaped pin hole boring machine to fine bore the pin hole of the cast iron piston blank to a standard size. At this time, the rotation speed of the ETK2708A CNC steel piston special-shaped pin hole boring machine is 1000-1500 r / min, and the feed groove is 100-300 mm / min.