Vehicle-mounted power module sintering method and mold

By designing multiple supporting bosses on the die under sintering of the vehicle power module, the module avoids interference and extrusion during sintering, the problem of interference and extrusion of tooling and AMB substrates during sintering is solved, and the sintering effect is improved. Consistency and temperature adaptability.

CN118919436APending Publication Date: 2024-11-08基本半导体(无锡)有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410873076.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-06-28
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

During the sintering process of the on-board power module, the tooling and AMB substrate are prone to interference and extrusion, resulting in inconsistent sintering effects and difficult to be compatible with different temperature requirements and materials.

Method used

Design a sintering method of vehicle-mounted power module. By exposing the step surfaces of multiple tool support bosses on the sintered mold, the lower surface of the power module to be sintered is connected to the AMB support bosses, and the indentation head of the mold on the sintered mold is sintered with Before the mold contacts, the tooling support boss falls through pneumatic support, so that the module falls off and falls on the AMB support boss, thereby avoiding interference and squeezing.

Benefits of technology

It realizes no interference and no extrusion during the sintering process of tooling and AMB substrate, improves the consistency of the sintering effect of the on-board power module, and is compatible with the sintering needs of smaller chip spacing and larger temperature intervals.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118919436A_ABST
    Figure CN118919436A_ABST
Patent Text Reader

Abstract

The invention provides a vehicle-mounted power module sintering method and a mold. The invention provides a vehicle-mounted power module sintering method. The vehicle-mounted power module sintering method comprises the steps that a tool where a to-be-sintered power module is placed is placed on step faces of a plurality of tool supporting bosses; before a pressing head of the upper sintering mold is in contact with the power module to be sintered, and when the distance between the lower end face of a bent part of the upper sintering mold and the upper surface of the lower sintering mold is smaller than a second preset distance, the tool is separated from the power module to be sintered, and the power module to be sintered falls on the AMB supporting boss; and sintering the power module to be sintered after the lower end face of the bent part of the upper sintering die is in contact with the upper surface of the lower sintering die and a pressure head arranged on the upper sintering die is in contact with the upper surface of the power module to be sintered. According to the method, interference and mutual extrusion between the tool and the AMB substrate in the sintering process of the vehicle-mounted power module can be avoided, and meanwhile the consistency of the sintering effect of the vehicle-mounted power module can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of vehicle-mounted power modules, and in particular to a sintering method and a mold for a vehicle-mounted power module. Background Art

[0002] In order to achieve the interconnection between the chip and substrate of the vehicle power module, the chip and the substrate can be soldered or silver sintered. The advantages of using sintering between the chip and the substrate compared to traditional soldering include that the sintered silver layer has a higher melting point than tin solder and has stronger thermal and electrical conductivity.

[0003] As the chip density of automotive power modules increases, the gap between chips gradually decreases, which makes the layout design of the sintering independent pressure head and the design of the pressure head size more and more difficult. When the margin of the pressure head relative to the chip size is not enough to make up for the design tolerance, processing tolerance, positioning tolerance and thermal expansion coefficient differences of various materials such as products, tooling, and molds, the sintering of the independent pressure head will not be achieved. Since the thermal expansion of various materials varies significantly under high temperature differences, fixed sintering molds are difficult to accommodate sintering of different temperature requirements and different materials. The thermal expansion of the tooling and AMB substrate will cause the tooling and AMB substrate to interfere and squeeze each other during the sintering process, which will cause cracks in the ceramic of the AMB substrate and deformation of the tooling. It will also cause the AMB substrate to be displaced relative to its initial position. The displacement direction and degree of the AMB substrate at different positions of the tooling are inconsistent, which will lead to poor consistency in the sintering effect of the automotive power module. Summary of the invention

[0004] The purpose of the present invention is to provide a sintering method and mold for an on-board power module to solve the technical problems in the prior art that the tooling and the AMB substrate are prone to interference and mutual extrusion during the sintering process, and the consistency of the sintering effect of the on-board power module is poor.

[0005] The technical solution of the present invention is as follows, providing a method for sintering a vehicle-mounted power module, comprising:

[0006] The stepped surfaces of the plurality of tooling support bosses are exposed on the upper surface of the sintering lower mold;

[0007] Placing the tooling with the power module to be sintered placed on the step surface of the plurality of tooling support bosses, so that the lower surface of the power module to be sintered is opposite to the AMB support boss on the sintering lower mold and is separated by a first preset distance;

[0008] Before the pressure head of the sintering upper mold contacts the power module to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, the tooling support boss falls along the first through hole of the sintering lower mold, so that the tooling is separated from the power module to be sintered, and the power module to be sintered falls on the AMB support boss;

[0009] When the lower end surface of the bent portion of the sintering upper mold contacts the upper surface of the sintering lower mold, and the pressing head arranged on the sintering upper mold contacts the upper surface of the power module to be sintered, the power module to be sintered is sintered.

[0010] Furthermore, before placing the tooling on which the power module to be sintered is placed on the stepped surfaces of the plurality of tooling support bosses, the method further comprises:

[0011] The power module to be sintered is placed on the bottom wall of the placement hole unit of the tooling, and the placement hole unit also includes a second through hole formed on the bottom wall, a side wall circumferentially arranged around the bottom wall, a first step on the side wall close to the bottom wall, and a second step away from the bottom wall.

[0012] Further, the tooling support boss is made to fall along the first through hole of the sintering lower mold to separate the tooling from the power module to be sintered, comprising:

[0013] Make the tooling support boss fall along the first through hole of the sintering lower mold, separate the tooling from the power module to be sintered, make the step surface of the tooling support boss fall into the first through hole of the sintering lower mold, and make the tooling fall on the sintering lower mold.

[0014] Furthermore, when the tooling falls on the sintering lower mold, it also includes allowing the AMB supporting boss to pass through the second through hole of the tooling.

[0015] Further, the step surfaces of the plurality of tooling support bosses are exposed on the upper surface of the sintering lower mold, including:

[0016] Through pneumatic support, the step surfaces of a plurality of tooling support bosses corresponding to a plurality of first through holes in the sintering lower mold are exposed on the upper surface of the sintering lower mold.

[0017] Furthermore, before the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, it also includes: moving the sintering lower mold upward so that the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold gradually decreases.

[0018] Another technical solution of the present invention is as follows: a sintering die for a vehicle-mounted power module is also provided, comprising a sintering lower die, a tooling, a tooling support boss, an AMB support boss, a sintering upper die, a plurality of tooling support bosses, and a pressing head arranged on the sintering upper die;

[0019] The step surfaces of the multiple tooling support bosses are exposed on the upper surface of the sintering lower mold, the tooling with the power module to be sintered is placed on the step surfaces of the multiple tooling support bosses, and the lower surface of the power module to be sintered is opposite to the AMB support boss on the sintering lower mold and is separated by a first preset distance;

[0020] Before the pressure head of the sintering upper mold contacts the power module to be sintered, and the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, the tooling support boss falls along the first through hole of the sintering lower mold, the tooling is separated from the power module to be sintered, and the power module to be sintered falls on the AMB support boss.

[0021] Furthermore, the power module to be sintered is placed on the bottom wall of the placement hole unit of the tooling, and the placement hole unit also includes a second through hole formed on the bottom wall, a side wall circumferentially arranged around the bottom wall, a first step on the side wall close to the bottom wall, and a second step away from the bottom wall.

[0022] Furthermore, the tooling support boss falls along the first through hole of the sintering lower mold, and the tooling is separated from the power module to be sintered, comprising:

[0023] The tooling support boss falls along the first through hole of the sintering lower mold, the tooling is separated from the power module to be sintered, the step surface of the tooling support boss falls into the first through hole of the sintering lower mold, and the tooling falls on the sintering lower mold.

[0024] Furthermore, the vehicle-mounted power module sintering mold also includes that when the tooling falls on the sintering lower mold, the AMB supporting boss passes through the second through hole of the tooling.

[0025] The beneficial effects of the present invention are as follows: the stepped surfaces of a plurality of tooling support bosses are exposed on the upper surface of the sintering lower mold; the tooling on which the power module to be sintered is placed is placed on the stepped surfaces of the plurality of tooling support bosses, so that the lower surface of the power module to be sintered is opposite to the AMB support boss on the sintering lower mold and is at a first preset distance; before the pressure head of the sintering upper mold contacts the power module to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, the tooling support boss is dropped along the first through hole of the sintering lower mold, so that the tooling is in contact with the power module to be sintered. The power module is separated and the power module to be sintered is made to fall on the AMB supporting boss; when the lower end surface of the bent portion of the sintering upper mold contacts the upper surface of the sintering lower mold, and the pressure head arranged on the sintering upper mold contacts the upper surface of the power module to be sintered, the power module to be sintered is sintered; through the above technical scheme, the tooling is separated from the power module to be sintered, and the power module to be sintered can be made to fall on the AMB supporting boss, and the tooling and the AMB substrate will not interfere with or squeeze each other during the sintering process of the vehicle-mounted power module, and at the same time, the consistency of the sintering effect of the vehicle-mounted power module can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 A schematic diagram of a process flow of a vehicle-mounted power module sintering method provided by an embodiment of the present invention;

[0027] Figure 2 A schematic diagram of the structure of a power module to be sintered provided in an embodiment of the present invention;

[0028] Figure 3 A schematic diagram of the structure of a sintering upper mold and a sintering lower mold provided in an embodiment of the present invention;

[0029] Figure 4 A schematic structural diagram of a sintering mold for a vehicle-mounted power module provided in an embodiment of the present invention;

[0030] Figure 5 A top view of a tool provided in an embodiment of the present invention;

[0031] Figure 6 The embodiment of the present invention provides Figure 5 A schematic diagram of the cross-sectional structure cut along the transverse AA cutting line;

[0032] Figure 7 A schematic diagram of a structure in which a power module to be sintered provided in an embodiment of the present invention is placed on a placement hole unit of a tool;

[0033] Figure 8 This is a schematic diagram after step S103 is completed in an embodiment of the present invention.

[0034] Figure numerals: 10-power module to be sintered; 11-copper foil layer; 12-second nanosilver material layer; 13-chip; 14-first nanosilver material layer; 15-copper circuit layer; 16-ceramic layer; 17-copper heat dissipation layer; 18-AMB substrate; 21-sintering upper mold; 211-bending portion; 212-plate-like body; 22-pressing head; 23-AMB supporting boss; 24-tooling supporting boss; 25-sintering lower mold; 26-tooling; 261-placement hole unit; 2611-second through hole; 2612-bottom wall; 2613-side wall; 2614-first step; 2615-second step. DETAILED DESCRIPTION

[0035] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0036] Reference to "embodiments" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present invention. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.

[0037] Figure 1 FIG. 1 is a schematic flow chart of a sintering method for a vehicle-mounted power module according to an embodiment of the present invention. It should be noted that the sintering method for a vehicle-mounted power module according to the present invention is not limited to the sintering method for a vehicle-mounted power module according to an embodiment of the present invention if substantially the same results are achieved. Figure 1 The process sequence shown is limited. Figure 1 As shown, the vehicle-mounted power module sintering method comprises the following steps:

[0038] S101, making the stepped surfaces of the plurality of tooling support bosses 24 exposed on the upper surface of the sintering lower mold 25;

[0039] In some embodiments, the step surfaces of the plurality of tooling support bosses 24 are exposed on the upper surface of the sintering lower mold 25, including:

[0040] Through pneumatic support, the stepped surfaces of the plurality of tooling support bosses 24 corresponding to the plurality of first through holes in the sintering lower mold 25 are exposed on the upper surface of the sintering lower mold 25 .

[0041] In a specific embodiment, an air source is connected below the first through hole. In an initial state, the air source is in an open state, and the tooling support boss 24 is in a suspended state.

[0042] S102, placing the tooling 26 with the power module 10 to be sintered placed thereon on the stepped surfaces of the plurality of tooling support bosses 24, so that the lower surface of the power module 10 to be sintered is opposite to the AMB support boss 23 on the sintering lower mold 25, and the distance is a first preset distance;

[0043] In a specific embodiment, the structural diagram of the power module 10 to be sintered is as follows: Figure 2 As shown, Figure 2 From bottom to top, the copper heat dissipation layer 17, the ceramic layer 16, the copper circuit layer 15, the first nano-silver material layer 14, the chip 13, the second nano-silver material layer 12 and the copper foil layer 11 are included, wherein the copper heat dissipation layer 17, the ceramic layer 16 and the copper circuit layer 15 form an AMB (Active Metal Brazing) substrate, the first nano-silver material layer 14 and the second nano-silver material layer 12 can both be formed of nano-silver paste or nano-silver film, and the above-mentioned sintering of the power module to be sintered is to sinter the first nano-silver material layer 14 and the second nano-silver material layer 12.

[0044] In a specific embodiment, the sintering equipment of the vehicle-mounted power module may include a preheating zone, a sintering zone, and a cooling zone. The preheating zone includes a preheating platform on which a temperature can be set. The preheating temperature during preheating is 30 to 80° C. The sintering zone includes a sintering upper mold 21 and a sintering lower mold 25. The sintering upper mold 21 is provided with several independent pressing heads 22 arranged according to the product (vehicle-mounted power module) chip 13. The sintering lower mold 25 has an AMB supporting boss 23 supporting the AMB substrate 18 and a tooling supporting boss 24 supporting the tooling 26. The structural schematic diagram of the sintering upper mold 21 and the sintering lower mold 25 is as shown in FIG. Figure 3 As shown, the cooling zone includes a cooling platform connected to nitrogen. The size design of the press head 22 needs to consider the positioning tolerance of the tooling 26 under the sintering mold 25, the limit tolerance of the tooling 26 and the AMB substrate 18, the processing tolerance of the AMB substrate 18, and the chip position tolerance of the chip 13 on the AMB substrate 18. In the case of the above cumulative tolerance limit, it is also necessary to ensure that the press head 22 can completely cover the chip 13 area that needs to be sintered.

[0045] In some embodiments, before placing the tool 26 with the power module 10 to be sintered on the stepped surfaces of the plurality of tool support bosses 24, the method further includes:

[0046] The power module 10 to be sintered is placed on the bottom wall 2612 of the placement hole unit 261 of the tooling 26, and the placement hole unit 261 also includes a second through hole 2611 formed on the bottom wall 2612, a side wall 2613 circumferentially arranged around the bottom wall 2612, a first step 2614 on the side wall 2613 close to the bottom wall 2612, and a second step 2615 away from the bottom wall 2612.

[0047] In a specific embodiment, the power module 10 to be sintered is placed on the bottom wall 2612 of the placement hole unit 261 of the tooling 26 for preheating, and then the tooling 26 with the power module 10 to be sintered is placed on the stepped surface of the plurality of tooling support bosses 24. A schematic diagram of the structure of a vehicle-mounted power module sintering mold, as shown in FIG. Figure 4 As shown, Figure 4 The figure shows that a tool 26 on which the power module 10 to be sintered is placed is placed on the stepped surfaces of a plurality of tool support bosses 24. Figure 4 24 is a cross-sectional view, the height from the tooling support boss 24 to the upper surface of the sintering lower mold 25 is greater than the height from the AMB support boss 23 to the upper surface of the sintering lower mold 25, and there is a certain gap between the AMB substrate 18 and the AMB support boss 23, and the gap can be greater than 3mm to avoid heat transfer between the AMB substrate 18 and the AMB support boss 23, thereby increasing the temperature of the AMB substrate 18. The top view of the tooling 26 is as shown in FIG. Figure 5 As shown, the tooling 26 includes a plurality of placement hole units 261, Figure 5 The schematic diagram of the cross-sectional structure cut along the transverse AA cutting line is as follows: Figure 6 As shown, the placement hole unit 261 includes a bottom wall 2612, a second through hole 2611 formed on the bottom wall 2612, a side wall 2613 circumferentially arranged around the bottom wall 2612, a first step 2614 on the side wall 2613 close to the bottom wall 2612, and a second step 2615 away from the bottom wall 2612. In specific implementation, 4 to 10 placement hole units 261 may be arranged on the tooling 26, arranged in at least 2 rows and 2 columns; and a plurality of chips 13 are arranged on each AMB substrate 18, the number of which is at least 2.

[0048] In a specific embodiment, a schematic diagram of a structure in which a power module 10 to be sintered is placed on a placement hole unit 261 of a tool 26 is shown in FIG. Figure 7 As shown, Figure 7 In the embodiment, eight placement hole units 261 may be provided on the tooling 26 , and eight chips 13 may be provided on each AMB substrate 18 .

[0049] S103, before the pressure head 22 of the sintering upper mold 21 contacts the power module 10 to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than a second preset distance, the tooling support boss 24 is made to fall along the first through hole of the sintering lower mold 25, so that the tooling 26 is separated from the power module 10 to be sintered, and the power module 10 to be sintered falls on the AMB support boss 23;

[0050] In some embodiments, before the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than a second preset distance, it also includes: moving the sintering lower mold 25 upward so that the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 gradually decreases.

[0051] In a specific embodiment, Figure 3 As shown in FIG. 4 , the sintering upper mold 21 may be a cover-like structure. The sintering upper mold 21 includes a plate-like body 212 and a bending portion 211 bent downward from the plate-like body 212 . The plate-like body 212 and the bending portion 211 form a sintering upper mold 21 with a cover-like structure. Move the sintering lower mold 25 upward so that the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 gradually becomes smaller for mold closing. During the mold closing process of the sintering lower mold 25 and the sintering upper mold 21, a position sensing sensor can be used to identify the progress of the mold closing. Before the pressure head 22 of the sintering upper mold 21 contacts the power module 10 to be sintered, and the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than a second preset distance, the supporting force of the gas source below the first through hole can be reduced or the source can be completely closed, so that the tooling support boss 24 falls along the first through hole of the sintering lower mold 25, and the tooling 26 is separated from the power module 10 to be sintered.

[0052] In a specific embodiment, the schematic diagram after step S103 is completed is as follows: Figure 8 As shown, the above-mentioned second preset distance can be determined according to actual conditions, for example, it can be 5mm to 10mm. It should be noted that the distance between the lower end surface of the bending portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 needs to be greater than the distance between the pressure head 22 of the sintering upper mold 21 and the upper surface of the power module 10 to be sintered. The tooling support boss 24 is made to fall along the first through hole of the sintering lower mold 25, so that the tooling 26 is separated from the power module 10 to be sintered, and the power module 10 to be sintered falls on the AMB support boss 23, so that the subsequent sintering can avoid interference and mutual extrusion between the tooling 26 and the power module 10 to be sintered during the sintering process.

[0053] In some embodiments, the tooling support boss 24 is made to fall along the first through hole of the sintering lower mold 25 to separate the tooling 26 from the power module 10 to be sintered, including:

[0054] Make the tooling support boss 24 fall along the first through hole of the sintering lower mold 25, separate the tooling 26 from the power module 10 to be sintered, make the step surface of the tooling support boss 24 fall into the first through hole of the sintering lower mold 25, and make the tooling 26 fall on the sintering lower mold 25.

[0055] In the embodiment of the present invention, the tooling support boss 24 is made to fall along the first through hole of the sintering lower mold 25, so that the tooling 26 is separated from the power module 10 to be sintered, and the step surface of the tooling support boss 24 falls into the first through hole of the sintering lower mold 25, so that the tooling 26 falls on the sintering lower mold 25 for subsequent sintering, which can avoid interference and mutual extrusion between the tooling 26 and the power module 10 to be sintered during the sintering process.

[0056] In some embodiments, when the tooling 26 falls on the sintering lower mold 25 , it further includes allowing the AMB supporting boss 23 to pass through the second through hole 2611 of the tooling 26 .

[0057] In a specific embodiment, Figure 6 As shown, when the tooling 26 falls on the sintering lower mold 25, the AMB supporting boss 23 penetrates the second through hole 2611 of the tooling 26, which can avoid interference and mutual extrusion between the tooling 26 and the power module 10 to be sintered during the sintering process.

[0058] S104, when the lower end surface of the bent portion of the sintering upper mold 21 contacts the upper surface of the sintering lower mold 25, and the pressing head 22 arranged on the sintering upper mold 21 contacts the upper surface of the power module 10 to be sintered, the power module 10 to be sintered is sintered.

[0059] In a specific embodiment, after the pressure head 22 of the sintering upper mold 21 contacts the upper surface of the power module 10 to be sintered, the pressure needs to be increased to a preset required value and maintained for a period of time to complete the sintering. In a specific embodiment, the sintering temperature is 200°C to 300°C, the sintering time is 150s to 650s, and the sintering pressure is 10 to 40Mpa.

[0060] The vehicle-mounted power module sintering method provided by the embodiment of the present invention makes the step surfaces of multiple tooling support bosses 24 exposed on the upper surface of the sintering lower mold 25; the tooling 26 on which the power module 10 to be sintered is placed is placed on the step surfaces of the multiple tooling support bosses 24, so that the lower surface of the power module 10 to be sintered is opposite to the AMB support boss 23 on the sintering lower mold 25, and is separated by a first preset distance; before the pressure head 22 of the sintering upper mold 21 contacts the power module 10 to be sintered, and the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than the second preset distance, the tooling support boss 24 is dropped along the first through hole of the sintering lower mold 25, so that the tooling 26 is separated from the power module 10 to be sintered, and the power module 10 to be sintered falls on the AMB support boss 23; when the lower end surface of the bent portion of the sintering upper mold 21 is in contact with the upper surface of the sintering lower mold 25, the pressure head 22 of the sintering upper mold 21 is in contact with the power module 10 to be sintered, and the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than the second preset distance, the tooling support boss 24 is dropped along the first through hole of the sintering lower mold 25, the tooling 26 is separated from the power module 10 to be sintered, and the power module 10 to be sintered falls on the AMB support boss 23; when the lower end surface of the bent portion of the sintering upper mold 21 is in contact with the The power module 10 to be sintered is sintered after the pressure head 22 arranged on the sintering upper mold 21 contacts the upper surface of the power module 10 to be sintered; the tooling 26 and the AMB substrate 18 will not interfere with or squeeze each other during the sintering process of the vehicle-mounted power module, and the ceramic cracks of the AMB substrate 18 and the deformation of the tooling 26 can be avoided. The expansion of the tooling 26 will not affect the AMB substrate 18. The expansion of the AMB substrate 18 after heating expands around from their respective center points, so that the expansion of each AMB and the coverage area of ​​the pressure head 22 are consistent, thereby improving the consistency of the sintering effect of the vehicle-mounted power module, and avoiding scratches and scratches caused by displacement of the AMB substrate 18, thereby avoiding the appearance of the vehicle-mounted power module and subsequent process steps, wherein the consistency of the sintering effect of the vehicle-mounted power module is improved, that is, the consistency of the sintering effect of the first nano-silver material layer 14 and the second nano-silver material layer 12 of the vehicle-mounted power module is improved. The vehicle-mounted power module sintering method provided by the embodiment of the present invention does not need to consider the thermal expansion of the tooling 26, so that during the packaging manufacturing process, it can be compatible with products with smaller chip 13 spacing and sintering requirements in a larger temperature range.

[0061] The embodiment of the present invention provides a sintering mold for a vehicle-mounted power module, and its structural schematic diagram is as follows: Figure 4 As shown, the vehicle-mounted power module sintering mold includes a sintering lower mold 25, a tooling 26, a tooling support boss 24, an AMB support boss 23, a sintering upper mold 21, a plurality of tooling support bosses 24, and a pressing head 22 arranged on the sintering upper mold 21;

[0062] The stepped surfaces of the multiple tooling support bosses 24 are exposed on the upper surface of the sintering lower mold 25, and the tooling 26 on which the power module 10 to be sintered is placed is placed on the stepped surfaces of the multiple tooling support bosses 24, and the lower surface of the power module 10 to be sintered is opposite to the AMB support boss 23 on the sintering lower mold 25, and is separated by a first preset distance;

[0063] Before the pressure head 22 of the sintering upper mold 21 contacts the power module 10 to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold 21 and the upper surface of the sintering lower mold 25 is less than the second preset distance, the tooling support boss 24 falls along the first through hole of the sintering lower mold 25, the tooling 26 is separated from the power module 10 to be sintered, and the power module 10 to be sintered falls on the AMB support boss 23.

[0064] In some embodiments, the power module 10 to be sintered is placed on the bottom wall 2612 of the placement hole unit 261 of the tooling 26, and the placement hole unit 261 also includes a second through hole 2611 formed on the bottom wall 2612, a side wall 2613 circumferentially arranged around the bottom wall 2612, a first step 2614 on the side wall 2613 close to the bottom wall 2612, and a second step 2615 away from the bottom wall 2612.

[0065] In some embodiments, the tooling support boss 24 falls along the first through hole of the sintering lower mold 25, and the tooling 26 is separated from the power module 10 to be sintered, including:

[0066] The tooling support boss 24 falls along the first through hole of the sintering lower mold 25 , the tooling 26 is separated from the power module 10 to be sintered, the step surface of the tooling support boss 24 falls into the first through hole of the sintering lower mold 25 , and the tooling 26 falls on the sintering lower mold 25 .

[0067] In some embodiments, the vehicle-mounted power module sintering mold further includes: when the tooling 26 falls on the sintering lower mold 25, the AMB supporting boss 23 penetrates the second through hole 2611 of the tooling 26.

[0068] The vehicle-mounted power module sintering mold provided by the embodiment of the present invention, due to the separation of the tooling 26 and the AMB substrate 18 during the sintering of the vehicle-mounted power module, the design of the center position of the pressure head 22 does not need to consider the influence of the temperature increase expansion of the tooling 26 on the position of each AMB substrate 18, and the design of the size of the pressure head 22 does not need to include the deviation of the position change of the AMB substrate 18 caused by the expansion of the tooling 26, which in turn causes the position change of the chip 13, which greatly reduces the difficulty of the sintering mold design. In the design process of the tooling 26, there is no need to consider the more expensive material with a low thermal expansion coefficient, which makes the selection of the material of the tooling 26 more flexible and can also reduce a part of the cost. Since the tooling 26 is in a free state of thermal expansion and contraction, there is no AMB substrate 18, sintering lower mold 25 and sintering upper mold 21 to squeeze it, and the tooling 26 is less deformed and has a longer service life.

[0069] For other details of the above-mentioned vehicle-mounted power module sintering mold, reference may be made to the description of the vehicle-mounted power module sintering method provided in the above-mentioned invention embodiment, which will not be repeated here.

[0070] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0071] The above embodiments only express the preferred implementation modes of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A sintering method for a vehicle-mounted power module, characterized in that: include: The stepped surfaces of the plurality of tooling support bosses are exposed on the upper surface of the sintering lower mold; Placing the tooling with the power module to be sintered placed on the step surface of the plurality of tooling support bosses, so that the lower surface of the power module to be sintered is opposite to the AMB support boss on the sintering lower mold and is separated by a first preset distance; Before the pressure head of the sintering upper mold contacts the power module to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, the tooling support boss falls along the first through hole of the sintering lower mold, so that the tooling is separated from the power module to be sintered, and the power module to be sintered falls on the AMB support boss; When the lower end surface of the bent portion of the sintering upper mold contacts the upper surface of the sintering lower mold, and the pressing head arranged on the sintering upper mold contacts the upper surface of the power module to be sintered, the power module to be sintered is sintered.

2. The vehicle-mounted power module sintering method according to claim 1, characterized in that: Before placing the tooling on which the power module to be sintered is placed on the step surfaces of the plurality of tooling support bosses, the method further comprises: The power module to be sintered is placed on the bottom wall of the placement hole unit of the tooling, and the placement hole unit also includes a second through hole formed on the bottom wall, a side wall circumferentially arranged around the bottom wall, a first step on the side wall close to the bottom wall, and a second step away from the bottom wall.

3. The vehicle-mounted power module sintering method according to claim 2, characterized in that: The tool support boss is made to fall along the first through hole of the sintering lower mold to separate the tool from the power module to be sintered, comprising: Make the tooling support boss fall along the first through hole of the sintering lower mold, separate the tooling from the power module to be sintered, make the step surface of the tooling support boss fall into the first through hole of the sintering lower mold, and make the tooling fall on the sintering lower mold.

4. The vehicle-mounted power module sintering method according to claim 3, characterized in that: When the tooling falls on the sintering lower mold, the method further includes allowing the AMB supporting boss to pass through the second through hole of the tooling.

5. The vehicle-mounted power module sintering method according to claim 1, characterized in that: The step surfaces of the plurality of tooling support bosses are exposed on the upper surface of the sintering lower mold, including: Through pneumatic support, the step surfaces of a plurality of tooling support bosses corresponding to a plurality of first through holes in the sintering lower mold are exposed on the upper surface of the sintering lower mold.

6. The vehicle-mounted power module sintering method according to claim 1, characterized in that: Before the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, it also includes: moving the sintering lower mold upward so that the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold gradually decreases.

7. A sintering mold for a vehicle-mounted power module, characterized in that: It includes a sintering lower mold, a tool, a tool support boss, an AMB support boss, a sintering upper mold, a plurality of tool support bosses, and a pressing head arranged on the sintering upper mold; The step surfaces of the multiple tooling support bosses are exposed on the upper surface of the sintering lower mold, the tooling with the power module to be sintered is placed on the step surfaces of the multiple tooling support bosses, and the lower surface of the power module to be sintered is opposite to the AMB support boss on the sintering lower mold and is separated by a first preset distance; Before the pressure head of the sintering upper mold contacts the power module to be sintered, and when the distance between the lower end surface of the bent portion of the sintering upper mold and the upper surface of the sintering lower mold is less than a second preset distance, the tooling support boss falls along the first through hole of the sintering lower mold, the tooling is separated from the power module to be sintered, and the power module to be sintered falls on the AMB support boss.

8. The vehicle-mounted power module sintering mold according to claim 7, characterized in that: The power module to be sintered is placed on the bottom wall of the placement hole unit of the tooling, and the placement hole unit also includes a second through hole formed on the bottom wall, a side wall circumferentially arranged around the bottom wall, a first step on the side wall close to the bottom wall, and a second step away from the bottom wall.

9. The vehicle-mounted power module sintering mold according to claim 8, characterized in that: The tooling support boss falls along the first through hole of the sintering lower mold, and the tooling is separated from the power module to be sintered, comprising: The tooling support boss falls along the first through hole of the sintering lower mold, the tooling is separated from the power module to be sintered, the step surface of the tooling support boss falls into the first through hole of the sintering lower mold, and the tooling falls on the sintering lower mold.