Manufacturing method of semiconductor device and semiconductor device
Through the two wafer bonding connection and Taiko process thinning, the curvature and chipping problems of semiconductor devices during the thinning process are solved, thinner thickness and lower power consumption are achieved, and electrical and mechanical properties are improved.
Patent Information
- Application Number
- CN202410972502.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-19
- Publication Date
- 2024-11-08
AI Technical Summary
In the process of thinning semiconductor devices, the wafer surface stress accumulation leads to fragmentation problems, and the prior art is difficult to achieve thinner thickness. At the same time, the support effect of supporting wafers decreases during the thinner process, which poses a risk of curvature and chipping.
The two wafer bonding and connection are used to form a stacked structure, and the support wafer is thinned through Taiko process and wet etching process to form a ring structure, which enhances mechanical strength and reduces defects and improves yield.
Thinner thickness reduction is achieved, power consumption and input impedance are reduced, electrical and heat dissipation are improved, warping and chip risks are reduced, and mechanical strength and yield of semiconductor devices are improved.
Smart Images

Figure CN118919489A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor manufacturing, and in particular relates to a method for manufacturing a semiconductor device and a semiconductor device. Background Art
[0002] With the development of semiconductor technology, the demand for reducing the size of power semiconductor devices is increasing. For example, with the popularity of mobile devices (smartphones, tablets, etc.), users have higher and higher requirements for thin and portable devices. Miniaturized semiconductor devices can further reduce the size of devices and achieve higher energy efficiency and lower power consumption. It can be seen that further reducing the size of power semiconductor devices plays an important role in the development of current electronic products.
[0003] As an important means to reduce the volume of power semiconductor devices, thinning power semiconductors has always been the most direct and effective way to achieve the requirements of thin, compact and multifunctional semiconductor devices, and to achieve low power consumption and low input impedance for power components. Thinning can not only effectively reduce the volume of subsequent packaging materials, but also reduce the on-resistance and thus reduce the thermal energy accumulation effect, thus increasing the service life of the chip.
[0004] However, the thinning thickness is limited by the problem of stress accumulation on the wafer surface during the thinning process, which causes fragmentation. Currently, the thinning process for power devices can achieve a thinning process of about 100μm. In addition, there is currently a process that uses bonding to another wafer to further thin it, but even if there is a supporting effect of the supporting wafer, when the overall thinning needs to be thinned to a thinner thickness, the supporting effect of the supporting wafer will be greatly reduced, and there will still be a large risk of warping and fragmentation. Summary of the invention
[0005] In view of the deficiencies existing in the related art, the present invention provides a method for manufacturing a semiconductor device and a semiconductor device, which can further reduce the thickness of the wafer, reduce the generation of defects, and improve the yield rate.
[0006] A first aspect of the present application provides a method for manufacturing a semiconductor device, comprising at least the following steps:
[0007] Providing a device wafer;
[0008] performing a front side process on the front side of the device wafer to form a device functional area;
[0009] forming a hard mask layer covering the front side of the device wafer;
[0010] Providing a support wafer, the support wafer having a bonding surface that matches the shape of the front side of the device wafer;
[0011] Bonding the hard mask layer on the device wafer to the bonding surface of the support wafer, so that the device wafer and the support wafer are stacked up and down to form a wafer assembly, and the two side surfaces of the wafer assembly in the thickness direction are respectively the first surface and the second surface, wherein the first surface is the back side of the device wafer, and the second surface is the surface of the support wafer on the other side away from the bonding surface;
[0012] Performing a grinding process on the first surface of the wafer assembly until the device wafer reaches a target thickness;
[0013] A Taiko process is performed on the second surface of the wafer assembly, and the area of the support wafer except the edge is thinned by the Taiko process, and a ring structure is formed at the edge after thinning.
[0014] In some embodiments of the first aspect, a width of the annular structure is less than 4 mm, a height of the annular structure is 20 μm to 800 μm, and a surface roughness of the thinned region of the support wafer is less than 10 nm.
[0015] In some embodiments of the first aspect, after performing a grinding process on the first surface of the wafer combination and before performing a Taiko process on the second surface, it also includes: attaching a blue film on one side of the first surface of the wafer combination; after performing the Taiko process on the second surface of the wafer combination, it also includes: removing the blue film on the first surface.
[0016] In some embodiments of the first aspect, after performing the Taiko process on the second surface of the wafer assembly, the method further includes: performing a wet etching process on the second surface of the wafer assembly to continue thinning the wafer assembly to a target thickness.
[0017] In some embodiments of the first aspect, in the wet etching process, the corrosive liquid is selected from one or a combination of more than two of hydrogen fluoride, nitric acid, and acetic acid, the etching time is 3 to 5 minutes, and the etching temperature is 25 to 35°C.
[0018] In some embodiments of the first aspect, after the second surface of the wafer assembly is subjected to a wet etching process, the thickness of the thinned region of the support wafer is 0 to 100 μm.
[0019] In some embodiments of the first aspect, the device functional area formed on the front side of the device wafer includes a metal-oxide-semiconductor field-effect transistor; after thinning the second surface of the wafer combination, the step of performing an IGBT back side process on the second surface of the wafer combination is also included.
[0020] In some embodiments of the first aspect, after the grinding process is performed on the first surface of the wafer assembly, the thickness of the device wafer is thinned to 5 μm to 100 μm.
[0021] In some embodiments of the first aspect, the hard mask layer on the device wafer is connected to the bonding surface of the support wafer by fusion bonding, and before bonding, the surface of the hard mask layer and / or the bonding surface is plasma activated.
[0022] A second aspect of the present application provides a semiconductor device, which is manufactured using the method for manufacturing a semiconductor device as described in any one of the first aspects.
[0023] Compared with the prior art, the advantages and positive effects of the present invention are:
[0024] (1) A method for manufacturing a semiconductor device provided in at least one embodiment of the present application utilizes two wafers to be bonded together to form a wafer assembly having a stacked structure, which can provide good support to each other during the subsequent thinning process, thereby preventing the device wafer from warping, fragmentation, and other problems;
[0025] (2) The method for manufacturing a semiconductor device provided in at least one embodiment of the present application uses the Taiko process to thin the support wafer, which can enhance the mechanical strength of the wafer assembly while having a thinner thinning thickness, reduce the probability of damage during subsequent processing and operation, and improve the yield rate;
[0026] (3) The semiconductor device provided in at least one embodiment of the present application has an overall thin thickness, which reduces power consumption and input impedance, improves the electrical performance of the semiconductor device, and also has good heat dissipation performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of this application. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:
[0028] Figure 1 A flow chart of an exemplary embodiment of a method for manufacturing a semiconductor device provided by the present invention;
[0029] Figure 2a A cross-sectional view of a wafer assembly after performing step S301 according to an illustrative embodiment of a method for manufacturing a semiconductor device provided by the present invention;
[0030] Figure 2b A cross-sectional view of a wafer assembly after performing step S302 according to an illustrative embodiment of a method for manufacturing a semiconductor device provided by the present invention;
[0031] Figure 2c A cross-sectional view of a wafer assembly with a blue film attached thereto according to an exemplary embodiment of a method for manufacturing a semiconductor device provided by the present invention;
[0032] Figure 2d A cross-sectional view of a wafer assembly after step S303 is performed according to an exemplary embodiment of a method for manufacturing a semiconductor device provided by the present invention;
[0033] Figure 2e It is a cross-sectional view of a wafer assembly after executing step S304 according to an illustrative embodiment of a method for manufacturing a semiconductor device provided by the present invention.
[0034] In the figure:
[0035] 1. Device wafer; 2. Support wafer; 21. Ring structure; 3. Hard mask layer; 4. Blue film. DETAILED DESCRIPTION
[0036] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0037] Obviously, the drawings described below are only some examples or embodiments of the present application. For ordinary technicians in this field, the present application can also be applied to other similar scenarios based on these drawings without creative work. In addition, it can also be understood that although the efforts made in this development process may be complicated and lengthy, for ordinary technicians in this field related to the content disclosed in this application, some changes in design, manufacturing or production based on the technical content disclosed in this application are just conventional technical means, and should not be understood as insufficient content disclosed in this application.
[0038] Reference to "embodiments" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those of ordinary skill in the art that the embodiments described in this application may be combined with other embodiments without conflict.
[0039] It is worth to be understood that, although the drawings may show a specific order of method steps, the order of the steps may be different from the order depicted. In addition, two or more steps may be performed simultaneously or partially simultaneously.
[0040] The first aspect of the present application provides a method for manufacturing a semiconductor device. In an exemplary embodiment, Figure 1 As shown, the method for manufacturing the semiconductor device comprises at least the following steps:
[0041] S101: providing a device wafer;
[0042] S102: performing a front process on the front side of the device wafer to form a device functional area;
[0043] S103: forming a hard mask layer covering the front side of the device wafer;
[0044] S201: providing a support wafer, wherein the support wafer has a bonding surface that matches the shape of the front side of the device wafer;
[0045] S301: bonding a hard mask layer on a device wafer to a bonding surface of a support wafer, so that the device wafer and the support wafer are stacked up and down to form a wafer assembly, wherein two side surfaces of the wafer assembly in a thickness direction are respectively a first surface and a second surface, wherein the first surface is the back side of the device wafer, and the second surface is the surface of the support wafer on the other side away from the bonding surface;
[0046] S302: performing a grinding process on the first surface of the wafer assembly until the device wafer reaches a target thickness;
[0047] S303: Performing a Taiko process on the second surface of the wafer assembly, thinning the area of the support wafer except the edge through the Taiko process, and forming a ring structure at the edge after thinning.
[0048] In the manufacturing method of the semiconductor device provided in the above-mentioned embodiment, two wafers are used as the device wafer and the support wafer respectively, and the two wafers are bonded and connected to form a wafer combination with a stacked structure before thinning the wafers. In the subsequent thinning process, the device wafer and the support wafer are thinned from both sides respectively; in the process of thinning the device wafer, the support wafer can provide good support to avoid warping, fragmentation and other problems of the device wafer, so that the device wafer can be thinned to a thinner thickness, which is beneficial to reduce the power consumption and input impedance of the power device and improve the electrical performance of the power device.
[0049] In addition, in the manufacturing process of the above-mentioned semiconductor device, the support wafer and the device wafer can be connected by a permanent bonding method, that is, the support wafer is a part of the semiconductor device without peeling. In this case, considering reducing the volume of the semiconductor device as a whole, it is necessary to thin the support wafer. However, when the support wafer is thinned, the device wafer connected to it has been thinned to a thinner thickness, so its support effect on the support wafer is limited. In the subsequent manufacturing process, it is still easy to cause warping, fragmentation or even fragmentation, causing the product to be scrapped as a whole. In order to reduce the risk of the above-mentioned problems, in this application, the Taiko process is used to thin the support wafer. On the one hand, the Taiko process can be used to thin the support wafer to a thinner thickness (for example, less than 50 μm) without defects, which is conducive to further reducing the volume of the device. On the other hand, the special ring structure formed by the Taiko process limits the edge of the wafer combination from warping, and enhances the mechanical strength of the wafer combination, reducing the probability of damage during subsequent processing and operation.
[0050] It is understandable that in the above method, only the steps related to the improvement of the present application are shown rather than all the steps. Therefore, the steps are not seamlessly connected, and other necessary steps may be interspersed between two steps as needed.
[0051] Hereinafter, each step of the method for manufacturing a semiconductor device provided in an embodiment of the present application will be described in detail in conjunction with a cross-sectional view of the semiconductor device during the manufacturing process.
[0052] First, in step S101, a device wafer 1 is provided. The device wafer 1 is also referred to as a semiconductor substrate in some cases. The device wafer 1 can specifically be made of silicon block, doped or undoped semiconductor substrate, or silicon-on-insulator (SOI) and any other semiconductor material that can be used to make a chip substrate. In the present application, there is no restriction on the specifications and thickness of the device wafer 1, which can be selected by the designer according to actual needs. For example, in one embodiment, the thickness of the device wafer 1 is 50 to 800 μm. The two side surfaces of the device wafer 1 in the thickness direction are generally referred to as the front and back sides, and relevant processes are performed on the front and / or back sides of the device wafer 1 to form the desired semiconductor device.
[0053] The front side process is performed on the front side of the device wafer 1 through step S102, so as to form a device functional area on the front side of the device wafer 1. The formed device functional area may include one or more of active devices (e.g., transistors, diodes, etc.) and passive devices (e.g., resistors, capacitors, inductors, etc.), which are selected and designed specifically according to the function of the semiconductor device. For example, in some embodiments, a metal-oxide-semiconductor field effect transistor (MOSFET) is formed on the front side of the device wafer 1.
[0054] Then, step 103 is performed to form a hard mask layer 3 covering the front side of the device wafer 1. In some embodiments, the hard mask layer 3 includes a silicon dioxide layer and a silicon nitride layer sequentially formed on the front side of the device wafer 1, but it is understood that other materials may also be used. In addition, the hard mask layer 3 may be formed by deposition or furnace thermal oxidation.
[0055] A supporting wafer 2 is provided through step S201, and the supporting wafer 2 has a bonding surface that matches the front shape of the device wafer 1. The present application does not limit the type and thickness of the supporting wafer 2. For example, in some embodiments, the thickness of the supporting wafer 2 is 50μm to 800μm, depending on the final thickness of the semiconductor device to be obtained and the designer's choice. The supporting wafer 2 has a bonding surface that matches the front shape of the device wafer 1, which means that the bonding surface of the supporting wafer 2 is consistent or substantially consistent with the shape of the front of the device wafer 1 and the area is equal or similar, so that the bonding surface of the supporting wafer 2 and the device wafer 1 can be butted against each other, which is beneficial to improve the stability of the bonding connection.
[0056] Then, if Figure 2a As shown, in step S301, the hard mask layer 3 on the device wafer 1 is bonded to the bonding surface of the support wafer 2. After bonding, the device wafer 1 and the support wafer 2 are stacked up and down to form a wafer assembly, and the wafer assembly is used as a whole in the subsequent manufacturing process. For the convenience of description, the two side surfaces of the wafer assembly in the thickness direction are defined as the first surface and the second surface, wherein the first surface is the back side of the device wafer 1, and the second surface is the surface of the support wafer 2 on the other side away from the bonding surface.
[0057] In some embodiments, bonding can be performed by fusion bonding, where the hard mask layer 3 and the bonding surface of the support wafer 2 are directly contacted and combined together by interatomic forces to form a stable connection. Necessary surface cleaning and flattening processes may be performed before bonding to improve the effect of bonding. In addition, in some cases, surface activation may be performed to grow an oxide layer on the surface to increase surface energy and hydrophilicity and improve bonding strength. Optionally, the bonding temperature can be 800 to 1100°C.
[0058] In a specific embodiment, before bonding, the surface of the hard mask layer 3 and / or the bonding surface of the support wafer 2 is plasma activated, for example, the frequency can be first low frequency 25W and then high frequency 60W; after plasma activation, the activated surface is cleaned with deionized water (DI Water), and then bonding is performed. During the bonding process, a bonding mark is used for alignment as needed.
[0059] The device wafer 1 and the support wafer 2 are bonded together to form a wafer assembly through step S301. In the subsequent manufacturing process, the wafer assembly will be used as a whole to perform subsequent processes.
[0060] In the subsequent step S302, a grinding process is performed on the first surface of the wafer assembly until the device wafer 1 reaches the designed thickness. The cross-sectional view of the wafer assembly after grinding is as shown in FIG. Figure 2b As shown. During the grinding process, the support wafer 2 can provide effective support for it. Even if the device wafer 1 is thinned to a very thin thickness, there will be no defects such as warping and fragmentation, which reduces the volume of the device and improves the yield rate. In some embodiments, the thickness of the device wafer 1 after grinding is thinned to 5μm to 100μm, and in particular, it can be thinned to 5μm to 50μm, depending on the design.
[0061] Through step S302, the device wafer 1 can be thinned to a thinner thickness as much as possible, but in order to control the overall volume of the semiconductor device, the support wafer 2 needs to be further thinned. Therefore, by executing step S303, a thinning process is performed on the second surface of the wafer assembly to reduce the thickness of the support wafer 2, so that the wafer assembly as a whole has a smaller thickness. Considering the need for overall support and as thin as possible, the thinning process used in this step is the Taiko process, which uses the Taiko process to thin the area of the support wafer 2 except the edge, and after thinning, a ring structure 21 is formed at the edge, such as Figure 2d In some embodiments, the height of the ring structure 21 formed after the Taiko process is performed on the second surface of the wafer assembly can be 20μm to 800μm, depending on the initial thickness of the supporting wafer 2 and the final thinning thickness. The ring structure 21 with a height within this range can enhance the strength of the wafer assembly, reduce the probability of damage during subsequent processing and operation, and improve the yield rate. Figure 2d In the illustrated embodiment, the initial thickness of the support wafer 2 is 775 μm, and the height of the ring structure 21 formed after thinning by the Taiko process is 600 μm.
[0062] In addition, compared with the traditional Taiko process, the Taiko process is used in the wafer combination in this application. Considering the overall mechanical properties of the wafer combination and the requirements of subsequent process treatment, higher requirements are put forward for the control of temperature, stress distribution and other aspects of the thinning process. In view of these considerations, in some embodiments of the present application, the relevant process parameters of the Taiko process are adjusted. After the Taiko process is executed, the width of the annular structure 21 is less than 4mm, the height of the annular structure 21 is 20μm to 800μm, and the surface roughness of the thinning area of the supporting wafer 2 is less than 10nm. It can be understood that the width of the annular structure 21 is equal to the radius of the supporting wafer 2 minus the radius of the thinning area. In addition, the Taiko process can be performed at room temperature.
[0063] In some embodiments, before performing a thinning process on the second surface of the wafer assembly in step S303, the method further includes: Figure 2c As shown, a step of attaching a blue tape 4 on one side of the first surface of the wafer assembly; after step S303, the step of removing the blue tape 4 on the first surface is also included. Since the overall thickness of the wafer assembly has been reduced a lot in step S302 when the thinning process is performed on the second surface of the wafer assembly, before further thinning is performed through step S303, attaching a blue tape 4 on the back of the thinned surface can provide additional support and structural stability for the wafer assembly, further reducing various defects caused by thinning. In addition, after step S303 is executed, since the annular structure 21 has good support for the entire wafer assembly, the blue tape 4 can be easily removed without defects.
[0064] In some embodiments, the thinning process performed on the second surface of the wafer assembly further includes a wet etching process. Specifically, after the Taiko process is performed in step S303, step S304 is further included: performing a wet etching process on the second surface of the wafer assembly to further thin the wafer assembly to a target thickness, such as Figure 2e As shown. By combining the Taiko process with the wet etching process, not only can the strength of the wafer combination be improved, but also the wafer combination can be made thinner, so that the obtained semiconductor device has a smaller volume, the power consumption of the semiconductor device is reduced, and the heat dissipation performance of the semiconductor device is improved, creating unlimited possibilities for the development of power devices.
[0065] In order to better cooperate with the Taiko process to achieve the target thickness and ensure the performance and quality of the device, in some embodiments of the present application, the main process parameters of the wet etching process are controlled. For example, the etching solution is selected from one or a combination of two or more of hydrogen fluoride, nitric acid, and acetic acid, the etching time is 3 to 5 minutes, and the etching temperature is 25 to 35°C. After wet etching, the thickness of the thinned area of the support wafer 2 can be thinned to 0 to 100μm, in particular, it can be thinned to 0 to 50μm, which can be determined according to the design. Figure 2e In the illustrated embodiment, after the Taiko process and the wet etching process, the thickness of the thinned area of the support wafer 2 is thinned to nearly 0 μm.
[0066] In some embodiments, the semiconductor device is an IGBT device, and the metal-oxide-semiconductor field effect transistor (MOSFET) is formed on the front side of the device wafer 1 in step S102. After the wafer assembly is thinned, step S305 is also included: performing an IGBT backside process on the second surface after the wafer assembly is thinned. The IGBT backside process includes ion implantation, annealing, and metallization processes.
[0067] During the ion implantation process, N-type impurities (e.g., phosphorus, arsenic, sulfur, antimony or selenium, etc.) required for the field stop region (FS region) and P-type impurities (e.g., boron, indium, etc.) required for forming the collector region (P-type region) are implanted; low-temperature annealing is performed to allow the N-type impurities and the P-type impurities to be fully diffused; a metal layer is formed on the second surface of the wafer assembly through a metallization process, which can be achieved by deposition, etc., and the material of the metal layer can be aluminum, titanium, nickel, etc. For specific details of the IGBT backside process not disclosed in this application, reference can be made to the prior art.
[0068] In addition, it should be noted that in order to achieve external electrical connection, a conductive connection structure connected to the device functional area is also formed in the wafer assembly, such as metallized TSV, etc. This part can refer to the existing technology and is not described separately as a focus in this application.
[0069] The second aspect of the present application provides a semiconductor device, which is manufactured according to the method for manufacturing a semiconductor device as described in any embodiment of the first aspect above. The semiconductor device as a whole can have a relatively thin thickness, and at the same time has low power consumption and good heat dissipation performance. For example, in some embodiments, a thickness of less than 50 μm can be achieved.
[0070] Finally, it should be noted that: the various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0071] The above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, ordinary technicians in the field should understand that the specific implementation methods of the present invention can still be modified or some technical features can be replaced by equivalents without departing from the spirit of the technical solution of the present invention, which should be included in the scope of the technical solution for protection of the present invention.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: At least the following steps are included: Providing a device wafer; Performing a front process on the front side of the device wafer to form a device functional area; forming a hard mask layer covering the front side of the device wafer; Providing a support wafer, wherein the support wafer has a bonding surface that matches the shape of the front side of the device wafer; Bonding the hard mask layer on the device wafer to the bonding surface of the support wafer, so that the device wafer and the support wafer are stacked up and down to form a wafer assembly, and the two side surfaces of the wafer assembly in the thickness direction are respectively a first surface and a second surface, wherein the first surface is the back side of the device wafer, and the second surface is the surface of the support wafer on the other side away from the bonding surface; Performing a grinding process on the first surface of the wafer assembly until the device wafer reaches a target thickness; A Taiko process is performed on the second surface of the wafer assembly, and the area of the support wafer except the edge is thinned by the Taiko process, so that a ring structure is formed at the edge after thinning.
2. The method for manufacturing a semiconductor device according to claim 1, wherein: The width of the annular structure is less than 4 mm, the height of the annular structure is 20 μm to 800 μm, and the surface roughness of the thinned area of the support wafer is less than 10 nm.
3. The method for manufacturing a semiconductor device according to claim 1, wherein: After performing a grinding process on the first surface of the wafer combination and before performing a Taiko process on the second surface, it also includes: attaching a blue film on one side of the first surface of the wafer combination; after performing the Taiko process on the second surface of the wafer combination, it also includes: removing the blue film on the first surface.
4. The method for manufacturing a semiconductor device according to claim 1, wherein: After performing the Taiko process on the second surface of the wafer assembly, the method further includes: performing a wet etching process on the second surface of the wafer assembly to continue thinning the wafer assembly to a target thickness.
5. The method for manufacturing a semiconductor device according to claim 4, wherein: In the wet etching process, the etching solution is selected from hydrogen fluoride, nitric acid, acetic acid or a combination of two or more thereof, the etching time is 3 to 5 minutes, and the etching temperature is 25 to 35°C.
6. The method for manufacturing a semiconductor device according to claim 4, wherein: After the second surface of the wafer assembly is subjected to a wet etching process, the thickness of the thinned region of the support wafer is 0 to 100 μm.
7. The method for manufacturing a semiconductor device according to any one of claims 1 to 6, characterized in that: The device functional area formed on the front side of the device wafer includes a metal-oxide-semiconductor field effect transistor; after thinning the second surface of the wafer combination, the step of performing an IGBT back side process on the second surface of the wafer combination is also included.
8. The method for manufacturing a semiconductor device according to claim 1, wherein: After the first surface of the wafer assembly is subjected to a grinding process, the thickness of the device wafer is reduced to 5 μm to 100 μm.
9. The method for manufacturing a semiconductor device according to claim 1, wherein: The hard mask layer on the device wafer is connected to the bonding surface of the support wafer by fusion bonding. Before bonding, the surface of the hard mask layer and / or the bonding surface is plasma activated.
10. A semiconductor device, characterized in that: The semiconductor device is manufactured according to the method for manufacturing a semiconductor device according to any one of claims 1 to 9.