Reinforcing system for silicon-based negative electrode material of lithium ion battery
Through the composite of SiOx with carbon nanotubes and graphene and ultraviolet irradiation curing technology, the volume change problem of lithium-ion battery silicon-based anode material during lithium deintercalation is solved, and the stability and performance of lithium batteries are improved.
Patent Information
- Application Number
- CN202411087609.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-08
AI Technical Summary
The volume changes in the silicon-based anode material of lithium-ion batteries during the lithium deintercalation process lead to rapid decay of cycling performance, affecting the capacitance, and the prior art is difficult to effectively overcome this problem.
SiOx is used to combine with new carbon material carbon nanotubes and graphene, and the composite active material coating mechanism is applied to the copper foil, and the composite active material is polymerized and cured by ultraviolet light to improve the stability of the silicon-based negative electrode. and performance.
By reducing the sharp reduction in capacity, the stability and performance of silicon-based negative electrode lithium batteries are improved and the production efficiency of silicon-based negative electrodes is improved.
Smart Images

Figure CN118919635A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of battery production equipment, and in particular to a reinforcing system for silicon-based negative electrode materials of lithium-ion batteries. Background Art
[0002] As a representative of emerging energy storage devices, lithium-ion batteries have become the focus of research in various countries due to their high energy density, long cycle life, high output voltage, green environmental protection, and no memory effect. At present, the main negative electrode of lithium-ion batteries is graphite negative electrode, and its capacity has been close to the theoretical specific capacity (372mAh·g -1 ), so the development of negative electrode materials with higher specific capacity is urgent. Silicon-based negative electrode is a well-known high-capacity negative electrode material, which can maximize the lithium ion embedding to generate Li 22 Si 5 It can reach 4200mAh / g, and the lithium insertion potential is only 0.4V. Due to its ultra-high specific capacity (theoretical value 4200mAh / g) and low lithium insertion potential (300%), silicon causes the active material to pulverize, the electrical contact in the electrode to fail, and the new solid electrolyte layer SEI to be repeatedly generated, which ultimately leads to a rapid decline in cycle performance. Silicon materials have a large volume after the lithium extraction / insertion process. With such repeated cycles, the internal structure of the material is quickly destroyed, resulting in a sharp drop in capacity. The reasons that affect the capacitance may be poor conductivity, the actual capacitance is difficult to reach the theoretical capacitance, and the insufficient cycle performance caused by the interface. How to overcome the huge volume change of the silicon negative electrode during the lithium extraction and insertion process is a problem that all researchers are eager to solve.
[0003] Research has found that carbon materials are often used in composites with SiOx because of their good stability, small volume change and excellent conductivity. Using carbon materials as composite materials can first improve the conductivity of SiOx, and secondly act as an inert buffer layer to reduce its volume effect. In addition, the most commonly used method, such as carbon coating, can effectively reduce the contact area between SiOx and the electrolyte, thereby improving the coulombic efficiency.
[0004] Based on the deficiencies in the prior art, the present invention discloses a strengthening system for silicon-based negative electrode materials for lithium-ion batteries, wherein a composite active material is prepared by compounding SiOx with new carbon materials such as carbon nanotubes and graphene, and a composite active material coating mechanism for coating copper foil is provided, thereby reducing the sharp drop in capacity, improving the stability of silicon-based negative electrode lithium batteries, enhancing their performance, and achieving the strengthening of negative electrode copper foil. Summary of the invention
[0005] In view of the shortcomings of the prior art, the present invention provides a strengthening system for silicon-based negative electrode materials of lithium-ion batteries, so as to solve the technical problems raised in the background technology.
[0006] The specific technical solutions are as follows: A reinforcing system for silicon-based negative electrode materials of lithium-ion batteries comprises a base, support plates are respectively arranged vertically upward at the left and right ends of the upper end surface of the base, a composite active material coating mechanism for applying composite active materials to both side surfaces of a copper foil is also arranged above the base, a lateral displacement mechanism is arranged at the upper end of the composite active material coating mechanism, the left and right ends of the lateral displacement mechanism are respectively connected to the upper ends of two support plates through a longitudinal displacement mechanism, and the lower ends of the two support plates are respectively provided with flippable clamping mechanisms for clamping the left and right end portions of the copper foil.
[0007] Preferably, the composite active material is composed of a certain proportion of silicon monoxide powder, a new carbon material, anhydrous ethanol and PVDF.
[0008] Preferably, the novel carbon material includes one or a combination of carbon nanotube conductive paste and graphene.
[0009] Preferably, a support plate mechanism for supporting the copper foil is further provided in the middle of the upper end surface of the base, and the support plate mechanism comprises a horizontally arranged support plate, and the lower end surface of the support plate is connected to the base via a plurality of third electric cylinders.
[0010] Preferably, the composite active substance coating mechanism includes a coating cavity, which is in the shape of a rectangular parallelepiped, a coating head is provided at the lower port of the coating cavity, a piston plate is adapted inside the coating cavity, the upper end surface of the coating cavity is connected to a movable plate via a connecting rod, a feeding material assembly for longitudinally displacing the piston plate is provided between the movable plate and the coating cavity, and a sealing assembly is provided at the lower port of the coating head.
[0011] Preferably, a feeding pipe for conveying the composite active substance is further provided on the side of the coating head, and a solenoid valve is provided at one end of the feeding pipe close to the coating head.
[0012] Preferably, ultraviolet lighting components are also provided at the left and right ends of the coating cavity, and the ultraviolet lighting components include ultraviolet lamp posts, and the length direction of the ultraviolet lamp posts is arranged along the length direction of the coating cavity. Cover bodies for shielding light on the left and right sides and above the ultraviolet lamp posts are also provided at the left and right ends of the coating cavity.
[0013] Preferably, the feeding material assembly includes a first vertically arranged screw rod, the upper and lower ends of the first screw rod are respectively connected to the lower end surface of the movable plate and the upper end surface of the coating cavity through bearings, the first screw rod is adapted to be equipped with a first ball nut block, the first ball nut block is horizontally provided with a first connecting plate, a plurality of first guide rods are vertically arranged downward on the lower end surface of the first connecting plate, the lower ends of the plurality of first guide rods are respectively connected to the upper end surface of the piston plate, the upper end surface of the coating cavity is provided with a plurality of first guide cylinders adapted to the first guide rods, and the upper end surface of the movable plate is provided with a first motor for driving the first screw rod.
[0014] Preferably, the sealing assembly includes a horizontally arranged sealing plate, the length direction of the sealing plate is arranged along the length direction of the applicator head, and the front and rear sides of the applicator head are respectively horizontally provided with first electric cylinders, and the movable ends of the two first electric cylinders are respectively connected to the front and rear ends of the sealing plate through second connecting rods.
[0015] Preferably, the lateral displacement mechanism includes a second movable plate horizontally arranged in the left and right directions, the upper and lower end surfaces of the second movable plate are provided with first rectangular openings along its length direction, a second screw rod is provided on the inner side of the first rectangular opening along its length direction, a second ball nut block is adapted to the second screw rod, the second ball nut block is connected to the rear end portion of the movable plate, a second guide rod is further provided on the inner side of the first rectangular opening along its length direction, a second guide cylinder adapted to the second guide rod is provided at the front end portion of the movable plate, and a second motor for driving the second screw rod is provided at the right end of the second movable plate.
[0016] Preferably, left and right side surfaces of the upper end of the support plate are provided with second rectangular openings along the height direction thereof, and left and right end portions of the second movable plate are respectively located in the two second rectangular openings.
[0017] Preferably, the longitudinal displacement mechanism includes a third screw rod arranged vertically, the upper and lower ends of the third screw rod are respectively connected to the upper and lower inner sides of the second rectangular opening through bearings, the third screw rod is equipped with a third ball nut block, the third ball nut block is connected to the end of the second movable plate, and the upper end of the support plate is also provided with a third motor for driving the third screw rod.
[0018] Preferably, the longitudinal displacement mechanism also includes a third guide rod arranged vertically, the upper and lower ends of the third guide rod are respectively connected to the upper and lower inner sides of the second rectangular opening, and the end of the second movable plate is provided with a third guide cylinder adapted to the third guide rod.
[0019] Preferably, the flipable clamping mechanism includes a flip plate located at the end of the copper foil, the flip plate is vertically arranged, a fixed clamping plate is horizontally arranged at the lower end of one side of the flip plate close to the copper foil, a second connecting plate is horizontally arranged at the upper end of one side of the flip plate close to the copper foil, a dynamic clamping plate is arranged between the second connecting plate and the fixed clamping plate, the dynamic clamping plate is connected to the second connecting plate through a second electric cylinder, and the side of the flip plate away from the copper foil is connected to the support plate through a rotating electric cylinder.
[0020] Preferably, a fourth guide rod is vertically arranged on the upper end surface of the dynamic clamping plate, and a fourth guide cylinder matched with the fourth guide rod is arranged on the second connecting plate.
[0021] Compared with the prior art, the present invention has the following beneficial effects: (1) The present invention provides a reinforcing system for silicon-based negative electrode materials of lithium-ion batteries. By setting a composite active material coating mechanism, the composite active material can be conveniently coated on the upper and lower end surfaces of the negative electrode copper foil to achieve the reinforcement of the negative electrode copper foil. The composite active material is coated on the negative electrode copper foil by SiO x The combination with new carbon materials such as carbon nanotubes and graphene can reduce the sharp drop in capacity and improve the stability of silicon-based negative electrode lithium batteries.
[0022] (2) The present invention provides a strengthening system for silicon-based negative electrode materials for lithium-ion batteries. By adding a photoinitiator to a composite active material and arranging an ultraviolet light irradiation component on a coating head, the ultraviolet light column can irradiate the coating with ultraviolet light. The photoinitiator in the composite active material can undergo polymerization and curing after being irradiated for tens of seconds, thereby improving the curing efficiency of the composite active material on the copper foil and improving the production efficiency of the silicon-based negative electrode. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a structural schematic diagram of the present invention.
[0024] Figure 2 It is a schematic diagram of the structure of the composite active substance coating mechanism of the present invention.
[0025] Figure 3 It is a schematic structural diagram of the composite active substance coating mechanism of the present invention from another angle.
[0026] Figure 4 The present invention Figure 1 Schematic diagram of the cross-section at AA.
[0027] Figure 5 The present invention Figure 1 Schematic diagram of the cross-section at BB.
[0028] Figure 6 The present invention Figure 1A partial enlarged schematic diagram of point C.
[0029] Figure 7 It is a schematic structural diagram of the flippable clamping mechanism of the present invention when flipping. DETAILED DESCRIPTION
[0030] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0031] Example 1 like Figure 1-7As shown, a strengthening system for silicon-based negative electrode materials of lithium-ion batteries, the left and right ends of the upper end surface of the base 1 are respectively provided with support plates 2 vertically upward, and the upper end of the base 1 is also provided with a composite active material coating mechanism 3 for coating the two sides of the copper foil 4 with the composite active material, the composite active material coating mechanism 3 includes a coating cavity 31, the coating cavity is rectangular, the lower end of the coating cavity 31 is provided with a coating head 32, the interior of the coating cavity is adapted to be provided with a piston plate 33, the piston plate 33 is sealingly and slidably arranged with the inner wall of the coating cavity 31, the upper end surface of the coating cavity 31 is connected to a movable plate 35 through a connecting rod 34, and a feeding material assembly 36 for longitudinally displacing the piston plate 33 is arranged between the movable plate 35 and the coating cavity 31; the feeding material assembly 36 includes a first screw rod 361 which is vertically arranged, and the upper and lower ends of the first screw rod 361 are respectively connected to the lower end surface of the movable plate 35 and the upper end surface of the coating cavity 31 through bearings, and the first screw rod is adapted to be equipped with a first ball nut block 362, and the first ball nut block 362 is horizontally provided with a first connecting plate 363, and the lower end surface of the first connecting plate 363 is vertically downwardly provided with a plurality of first guide rods 364, and the lower ends of the plurality of first guide rods 364 are respectively connected to the upper end surface of the piston plate 33, and the upper end surface of the coating cavity 31 is provided with a plurality of first guide cylinders 365 adapted to the first guide rods, and the upper end surface of the movable plate 35 is provided with a first motor 366 for driving the first screw rod 361. A sealing assembly 37 is provided at the lower end of the smear head 32. The sealing assembly 37 includes a horizontally arranged sealing plate 371. The length direction of the sealing plate 371 is arranged along the length direction of the smear head 32. First electric cylinders 373 are horizontally arranged on the front and rear sides of the smear head 32. The movable ends of the two first electric cylinders 373 are connected to the front and rear ends of the sealing plate 371 through second connecting rods 372. A feeding pipe for conveying composite active substances is also provided on the side of the smear head 32, and a solenoid valve is provided at one end of the feeding pipe close to the smear head 32. The operation of the first motor can drive the first screw to rotate slowly, thereby causing the first ball nut slider to slowly move upward or downward. When the first ball nut slider moves upward, the solenoid valve opens and the sealing plate seals the lower port of the coating head. At this time, the interior of the coating cavity is in a closed state. The upward movement of the first connecting plate 363 and the first guide rod 364 drives the piston plate to move upward. The upward movement of the piston plate creates a negative pressure inside the coating cavity, which enables the composite active material prepared in the mixing box to enter the coating cavity and the coating head through the feed pipe. During the coating period, when the piston plate moves downward, the solenoid valve is closed and the sealing plate releases the seal on the lower port of the coating head. The composite active material is smeared on the upper end surface of the copper foil through the coating head through the downward movement of the piston plate, and the ultraviolet lamp column that moves with the coating head realizes ultraviolet light irradiation of the coating. The composite active material is cured after being irradiated for tens of seconds.
[0032] The upper end of the composite active substance coating mechanism 3 is provided with a lateral displacement mechanism 5; the lateral displacement mechanism 5 includes a second movable plate 51 horizontally arranged in the left and right directions, the upper and lower end surfaces of the second movable plate 51 are provided with first rectangular openings 52 along the length direction thereof, the inner side of the first rectangular opening is provided with a second screw rod 53 along the length direction thereof, the second screw rod is adapted with a second ball nut block 54, the second ball nut block 54 is connected to the rear end of the movable plate 35, the inner side of the first rectangular opening is also provided with a second guide rod 56 along the length direction thereof, the front end of the movable plate 35 is provided with a second guide cylinder 57 adapted with the second guide rod, and the right end of the second movable plate 51 is provided with a second motor 55 for driving the second screw rod. The operation of the second motor 55 can make the second screw rod rotate slowly, thereby making the second ball nut block 54 move slowly to the left or right, so as to realize the slow movement of the coating head to the left or right.
[0033] The left and right ends of the lateral displacement mechanism 5 are respectively connected to the upper ends of the two support plates 2 through the longitudinal displacement mechanism 6; the left and right side surfaces of the upper end of the support plate 2 are provided with a second rectangular opening 10 along its height direction, and the left and right end portions of the second movable plate 51 are respectively located in the two second rectangular openings 10; the longitudinal displacement mechanism 6 includes a third screw rod 61 arranged vertically, and the upper and lower ends of the third screw rod 61 are respectively connected to the upper and lower inner sides of the second rectangular opening 10 through bearings, and the third screw rod 61 is adapted with a third ball nut block 62, and the third ball nut block 62 is connected to the end of the second movable plate 51, and the upper end of the support plate 2 is also provided with a third motor 63 for driving the third screw rod; the longitudinal displacement mechanism 6 also includes a third guide rod 64 arranged vertically, and the upper and lower ends of the third guide rod 64 are respectively connected to the upper and lower inner sides of the second rectangular opening 10, and the end of the second movable plate 51 is provided with a third guide cylinder 65 adapted to the third guide rod. The synchronous operation of the two third motors can make the two third screw rods 61 rotate synchronously and slowly, so that the second movable plate 51 moves slowly upward or downward, and then drives the coating head to move slowly upward or downward, reducing the impact of the copper foil on the flipping due to the coating head position being too low when it needs to be flipped.
[0034] The lower ends of the two support plates 2 are also respectively provided with reversible clamping mechanisms 7 for clamping the left and right ends of the copper foil 4; the reversible clamping mechanism 7 includes a reversing plate 71 located at the end of the copper foil 4, the reversing plate is vertically arranged, a fixed clamping plate 72 is horizontally arranged at the lower end of one side of the reversing plate close to the copper foil 4, a second connecting plate 74 is horizontally arranged at the upper end of one side of the reversing plate close to the copper foil 4, a dynamic clamping plate 73 is arranged between the second connecting plate 74 and the fixed clamping plate 7272, the dynamic clamping plate 73 is connected to the second connecting plate 74 through a second electric cylinder 75, and the side of the reversing plate 71 away from the copper foil 4 is connected to the support plate 2 through a rotating electric cylinder 77. A fourth guide rod 76 is also vertically arranged upward on the upper end surface of the dynamic clamping plate 73, and a fourth guide cylinder adapted to the fourth guide rod 76 is arranged on the second connecting plate 74. By placing the left and right ends of the lower end surface of the copper foil respectively on two fixed clamping plates 72, and through the operation of two second electric cylinders 75, the two movable clamping plates 73 can be clamped on the left and right ends of the upper end surface of the copper foil, thereby clamping the copper foil. When it is necessary to coat the lower end surface of the copper foil, the two rotating electric cylinders 77 can be synchronously rotated 180 degrees, and the two flipping plates 71 can be rotated along the axis of the rotating electric cylinders 77 to flip the copper foil, and still be located on the same horizontal plane.
[0035] The composite active material is composed of a certain proportion of silicon monoxide powder, a new carbon material, anhydrous ethanol, and PVDF; the new carbon material includes one or a combination of carbon nanotube conductive paste and graphene. x The combination with new carbon materials such as carbon nanotubes and graphene can reduce the sharp drop in capacity and improve the stability of silicon-based negative electrode lithium batteries. In addition, through long-term stirring, the carbon material is successfully compounded into SiO, improving the performance of silicon electrode batteries.
[0036] A support plate mechanism 8 for supporting the copper foil sheet 4 is also provided in the middle of the upper end surface of the base 1, and the support plate mechanism 8 includes a horizontally arranged support plate 81, and the lower end surface of the support plate 81 is connected to the base 1 through a plurality of third electric cylinders 82. The support plate can support the lower end of the copper foil sheet so that each area of the copper foil sheet is on the same horizontal plane, thereby improving its stability and uniformity during coating.
[0037] Example 2 On the basis of Example 1, the composite active material is composited by silicon monoxide powder, new carbon material, anhydrous ethanol, PVDF, photosensitive prepolymer, photoinitiator, photosensitizer and active diluent in a certain proportion.
[0038] The novel carbon material comprises one or a combination of carbon nanotube conductive paste and graphene.
[0039] The photosensitive prepolymer is polyurethane; the photoinitiator is triaryl sulfonium salt; the photosensitizer is benzophenone; and the active diluent is methyl methacrylate. Polyurethane has the advantages of strong bonding, wear resistance, toughness, and good solvent resistance; triaryl sulfonium salt has the advantages of high photosensitivity, insensitivity to temperature, and excellent thermal stability.
[0040] Ultraviolet lighting components 9 are also provided at the left and right ends of the coating cavity 31. The ultraviolet lighting components 9 include ultraviolet lamp posts 91. The length direction of the ultraviolet lamp posts 91 is arranged along the length direction of the coating cavity 31. The left and right ends of the coating cavity 31 are also provided with cover bodies 92 for shielding the light on the left and right sides and above the ultraviolet lamp posts 91.
[0041] The ultraviolet lamp column can realize ultraviolet light irradiation on the coating film. The photoinitiator in the composite active material can undergo polymerization and curing after being irradiated for tens of seconds, thereby improving the curing efficiency of the composite active material on the copper foil and improving the production efficiency of the silicon-based negative electrode.
[0042] Example 3 Based on Example 2, a method for strengthening a silicon-based negative electrode material for a lithium-ion battery comprises the following steps: S1, in a stirring box, silicon monoxide powder, carbon nanotube conductive paste, and graphene are placed in anhydrous ethanol according to a certain ratio, stirred at room temperature for 12 hours, and dried for later use; S2, in a stirring box, stirring the dried powder of step S1, triarylsulfonium salt, benzophenone, methyl methacrylate and 5% polyurethane in a certain proportion until uniformly prepared a composite active material; S3, after the copper foil is clamped on the reversible clamping mechanism, the solenoid valve is opened, the sealing plate seals the lower port of the coating head, and the composite active substance in the mixing box enters the coating cavity and the coating head through the feeding pipe by moving the piston plate upward; S4, during the operation of the lateral displacement mechanism, the electromagnetic valve is closed, the sealing plate releases the seal on the lower port of the coating head, and the composite active material is smeared on the upper end surface of the copper foil through the coating head by the downward movement of the piston plate, and the ultraviolet lamp column moving with the coating head realizes ultraviolet irradiation of the coating film, and the composite active material is cured after being irradiated for tens of seconds; S5, then the lower end surface of the copper foil is turned upward by the operation of the reversible clamping mechanism. Before turning over, the coating head needs to be moved up and the supporting plate needs to be moved down. After turning over, the coating head and the supporting plate are reset; S6, through the reverse operation of the lateral displacement mechanism, the coating head moves from right to left to achieve coating and curing of the lower end surface of the copper foil; S7, cutting the coated copper foil sheet according to the required negative electrode sheet size.
[0043] The carbon nanotube conductive slurry is a carbon nanotube with a solvent of 4% NMP.
[0044] The technical features of the above-described embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above-described embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0045] The above-mentioned embodiments only express the implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the patent of the present invention. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be based on the attached claims.
Claims
1. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries, It is characterized in that The invention comprises a base (1), wherein support plates (2) are respectively arranged vertically upward at the left and right ends of the upper end surface of the base (1), and a composite active material coating mechanism (3) for coating the two side surfaces of a copper foil (4) with a composite active material is also arranged above the base (1), and a lateral displacement mechanism (5) is arranged at the upper end of the composite active material coating mechanism (3), and the left and right ends of the lateral displacement mechanism (5) are respectively connected to the upper ends of the two support plates (2) through longitudinal displacement mechanisms (6), and the lower ends of the two support plates (2) are also respectively provided with flip-type clamping mechanisms (7) for clamping the left and right end portions of the copper foil (4).
2. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that The composite active substance coating mechanism (3) comprises a coating cavity (31) which is in the shape of a rectangular parallelepiped. A coating head (32) is arranged at the lower end of the coating cavity (31). A piston plate (33) is adapted to be arranged inside the coating cavity. The upper end surface of the coating cavity (31) is connected to a movable plate (35) via a connecting rod (34). A feeding material assembly (36) for longitudinally displacing the piston plate (33) is arranged between the movable plate (35) and the coating cavity (31). A sealing assembly (37) is arranged at the lower end of the coating head (32).
3. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 2, It is characterized in that The feeding material assembly (36) includes a first screw rod (361) arranged vertically, and the upper and lower ends of the first screw rod (361) are respectively connected to the lower end surface of the movable plate (35) and the upper end surface of the coating cavity (31) through bearings; the first screw rod is adapted to be equipped with a first ball nut block (362); a first connecting plate (363) is horizontally arranged on the first ball nut block (362); a plurality of first guide rods (364) are vertically arranged downward on the lower end surface of the first connecting plate (363); the lower ends of the plurality of first guide rods (364) are respectively connected to the upper end surface of the piston plate (33); the upper end surface of the coating cavity (31) is provided with a plurality of first guide cylinders (365) adapted to the first guide rods; and the upper end surface of the movable plate (35) is provided with a first motor (366) for driving the first screw rod (361).
4. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that The sealing assembly (37) comprises a horizontally arranged sealing plate (371), the length direction of the sealing plate (371) being arranged along the length direction of the coating head (32), and first electric cylinders (373) being arranged horizontally on the front and rear side surfaces of the coating head (32), respectively, and the movable ends of the two first electric cylinders (373) are connected to the front and rear end portions of the sealing plate (371) respectively through second connecting rods (372).
5. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that The lateral displacement mechanism (5) comprises a second movable plate (51) arranged horizontally in the left-right direction, the upper and lower end surfaces of the second movable plate (51) are provided with first rectangular openings (52) along the length direction thereof, a second screw rod (53) is provided inside the first rectangular opening along the length direction thereof, a second ball nut block (54) is adapted to be mounted on the second screw rod, the second ball nut block (54) is connected to the rear end of the movable plate (35), a second guide rod (56) is further provided inside the first rectangular opening along the length direction thereof, a second guide cylinder (57) adapted to be matched with the second guide rod is provided at the front end of the movable plate (35), and a second motor (55) for driving the second screw rod is provided at the right end of the second movable plate (51).
6. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that The left and right side surfaces of the upper end of the support plate (2) are provided with second rectangular openings (10) along the height direction thereof, and the left and right end portions of the second movable plate (51) are respectively located in the two second rectangular openings (10).
7. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 6, It is characterized in that The longitudinal displacement mechanism (6) comprises a third screw rod (61) arranged vertically, the upper and lower ends of the third screw rod (61) are respectively connected to the upper and lower inner side surfaces of the second rectangular opening (10) through bearings, the third screw rod (61) is equipped with a third ball nut block (62), the third ball nut block (62) is connected to the end of the second movable plate (51), and the upper end of the support plate (2) is also provided with a third motor (63) for driving the third screw rod.
8. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 7, It is characterized in that The longitudinal displacement mechanism (6) further comprises a third guide rod (64) arranged vertically, the upper and lower ends of the third guide rod (64) being respectively connected to the upper and lower inner side surfaces of the second rectangular opening (10), and the end of the second movable plate (51) is provided with a third guide cylinder (65) adapted to the third guide rod.
9. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that The flip-type clamping mechanism (7) comprises a flip plate (71) located at the end of the copper foil (4), the flip plate being arranged vertically, a fixed clamping plate (72) being arranged horizontally at the lower end of a side surface of the flip plate close to the copper foil (4), a second connecting plate (74) being arranged horizontally at the upper end of a side surface of the flip plate close to the copper foil (4), a movable clamping plate (73) being arranged between the second connecting plate (74) and the fixed clamping plate (72) (72), the movable clamping plate (73) being connected to the second connecting plate (74) via a second electric cylinder (75), and a side surface of the flip plate (71) away from the copper foil (4) being connected to the support plate (2) via a rotating electric cylinder (77).
10. A strengthening system for silicon-based negative electrode materials for lithium-ion batteries according to claim 1, It is characterized in that A support plate mechanism (8) for supporting the copper foil (4) is also provided in the middle of the upper end surface of the base (1), the support plate mechanism (8) comprising a support plate (81) arranged horizontally, the lower end surface of the support plate (81) being connected to the base (1) via a plurality of third electric cylinders (82).