Method for manufacturing 2T0C DRAM (dynamic random access memory) with 3D (three-dimensional) stacked external ring gate structure based on ALD (atomic layer deposition) technology

By employing a 3D stacked external ring gate structure with ALD technology in DRAM, the problems of insufficient gate control capability and low integration of write transistors are solved, achieving higher gate control capability, lower leakage current and higher integration, and providing flexible electrode layout and device interconnection.

CN118921985APending Publication Date: 2024-11-08FUDAN UNIVERSITY +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410948628.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The existing 2T0CDRAM write transistors have weak gate control capability, are prone to leakage, have low integration density, are not flexible enough, and the built-in gate is difficult to lead out as an electrode.

Method used

A 3D stacked external ring gate structure based on ALD technology is adopted. By building read and write transistors on the same plane, using an external gate structure and process, an electrode is led out from the middle of the vertical channel, and combined with amorphous metal oxide semiconductor thin film material, the transistor geometry is optimized.

Benefits of technology

It improves the gate control capability of write transistors, reduces leakage current, enhances charge retention capability, reduces device area, enables more flexible electrode layout and device interconnection, and improves the integration and performance of DRAM.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118921985A_ABST
    Figure CN118921985A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a 2T0C DRAM (dynamic random access memory) with a 3D (three-dimensional) stacked external ring gate structure based on an ALD (atomic layer deposition) technology, and relates to the field of computer manufacturing. A channel material is grown based on an ALD technology, a 2T0C DRAM with a gate-all-around thin film transistor structure is manufactured, three-dimensional stacking of read-write transistors is built in the 2T0C DRAM based on external gate design by optimizing the geometric position and basic structure of the read-write transistors, the integration level and the performance of the DRAM in all aspects are effectively improved, and a solution is provided for achieving DRAM multi-layer stacking. According to the invention, the switching performance of the write transistor is improved, the electric leakage is low, the storage window is high, and the retention time is long; the device area is reduced, and the requirement for small-size overlay precision is lowered; more flexible electrode layout and read-write operation can be realized, and interconnection and integration of the 2T0C DRAM and other devices are facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of computer manufacturing, and in particular to a method for manufacturing a 3D stacked external ring gate structure 2T0CDRAM based on ALD technology. Background Art

[0002] DRAM is an important type of memory in modern information storage systems, which serves as a data cache. In the existing advanced integrated circuit process, DRAM with a single transistor-single capacitor (1T1C) as the main structure has been developing closely with Moore's Law, continuously increasing in size and performance, and has approached the minimum size limit that can be produced by the corresponding process. In order to improve DRAM integration and performance in small-size processes, capacitor-free (2T0C) DRAM made of thin-film transistors based on various new materials has been continuously developed, providing a feasible solution for improving DRAM performance.

[0003] Therefore, technicians in this field are committed to developing a manufacturing method for a 3D stacked external ring gate structure 2T0CDRAM based on ALD technology. Summary of the invention

[0004] In view of the above-mentioned defects of the prior art, the technical problem to be solved by the present invention is that the gate control capability of the 2T0CDRAM write transistor is not strong, the write transistor is prone to leakage, and the integration is low.

[0005] To achieve the above objectives, the present invention provides a method for manufacturing a 3D stacked external ring-gate structure 2T0CDRAM based on ALD technology, which adopts a ring-gate structure and process.

[0006] Furthermore, a three-dimensional stack of read-write transistors is constructed.

[0007] Furthermore, the read and write transistors are placed on the same plane.

[0008] Furthermore, an external gate structure and process are adopted.

[0009] Furthermore, an electrode is led out from the middle of the vertical channel according to the wiring layer.

[0010] Further, it includes: depositing a metal thin film material on a medium-heavy doped Si substrate having an oxide thin film;

[0011] Defining the write transistor gate region by photolithography;

[0012] Etch the metal and oxide layers outside the transistor gate area.

[0013] Furthermore, the oxide film includes silicon dioxide and high-k material.

[0014] Furthermore, the metal thin film material deposition technology includes magnetron sputtering technology and electron beam evaporation technology.

[0015] Furthermore, the photolithography includes ultraviolet photolithography and electron beam photolithography.

[0016] Furthermore, the write transistor gate region includes a rectangle or a circle.

[0017] Most amorphous metal oxide semiconductors have high uniformity coverage and high mobility. They use active outermost electrons such as In and Zn to provide carriers to achieve conductivity, and can adjust the conductivity by adjusting the type and proportion of metal elements. Atomic layer deposition (ALD) technology uses self-adsorption saturated chemical reactions at low temperatures to grow metal oxide films that can cover high aspect ratio, small-sized microstructures, and achieve gate control functions for small-sized devices through its semiconductor properties.

[0018] Ring-gate transistors can use a matching channel structure to reduce size and improve transistor performance. They can give full play to the advantages of ALD technology and improve transistor integration. Through the optimization of transistor geometry, multi-layer device-level interconnection and three-dimensional stacking can be achieved. It is a feasible device structure that breaks through the integration limit of DRAM. The channel size limit of similar structures can reach the order of 10nm. The leads of vertical channel thin-film transistors with external ring-gate structures can be freely arranged by layer, without being restricted by device structure, and can provide more flexible wiring and read-write operations.

[0019] Amorphous metal oxide semiconductor films grown using ALD technology generally have high uniformity and high coverage, and can also ensure sufficient mobility. Channel materials are grown using ALD technology to produce 2T0C DRAM with a gate-all-around thin-film transistor structure. By optimizing the geometric position and basic structure of the read-write transistors and building a three-dimensional stack of read-write transistors in the 2T0C DRAM based on an external gate design, the integration level and various aspects of DRAM performance can be effectively improved, providing a solution for realizing DRAM multi-layer stacking.

[0020] The existing 2T0C DRAM write transistor has weak gate control capability, and the write transistor is prone to leakage, which limits the retention time and read / write window. The present invention adopts a ring gate structure and process to manufacture 2T0C DRAM, greatly strengthening gate control and improving DRAM performance. Under the same device size, the ring gate achieves a longer effective channel length, so that the write transistor has better gate control capability and lower leakage, and improves the charge retention capability.

[0021] The existing 2T0C DRAM has low integration and occupies a large area. The present invention designs a device-level three-dimensional stacking structure, places the read and write transistors on the same plane, reduces the occupied plane area, improves integration, and reduces the requirements for overlay accuracy. The device film scale of a few nanometers to more than ten nanometers is much lower than the device size scale of hundreds of nanometers to micrometers. The 3D stacking has little effect on the thickness, but can greatly save chip area.

[0022] The existing 2T0C DRAM is not flexible enough, and it is difficult to lead out the electrode from the built-in gate. The present invention adopts an external gate structure and process to manufacture 2T0C DRAM, and can flexibly lead out the electrode from the middle of the vertical channel according to the wiring layer. The external gate can directly lead out the electrode according to the wiring layer, which can realize device interconnection more flexibly.

[0023] Compared with the prior art, the present invention has the following obvious substantial features and significant advantages:

[0024] 1. The ring gate of the present invention has stronger gate control capability, improves the switch performance of the write transistor, and enables the 2T0C DRAM to have lower leakage, higher storage window and higher retention time.

[0025] 2. The present invention realizes 3D stacking of read-write transistors on the same plane, which can reduce the device area by at least one third and lower the requirements for small-size overlay accuracy.

[0026] 3. The external gate of the present invention can realize more flexible electrode layout and read-write operation, which is beneficial to the interconnection integration of 2T0C DRAM and other devices.

[0027] The concept, specific structure and technical effects of the present invention will be further described below in conjunction with the accompanying drawings to fully understand the purpose, characteristics and effects of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a schematic diagram of a preferred embodiment 1 of the present invention;

[0029] Figure 2 It is a schematic diagram of a preferred embodiment 2 of the present invention;

[0030] Figure 3 It is a schematic diagram of a preferred embodiment 3 of the present invention;

[0031] Figure 4 It is a schematic diagram of a preferred embodiment 4 of the present invention;

[0032] Figure 5 It is a schematic diagram of a preferred embodiment 5 of the present invention;

[0033] Figure 6 It is a schematic diagram of a preferred embodiment 6 of the present invention;

[0034] Figure 7 is a schematic diagram of a preferred embodiment 7 of the present invention;

[0035] Figure 8 It is a schematic diagram of a preferred embodiment 8 of the present invention. DETAILED DESCRIPTION

[0036] The following describes several preferred embodiments of the present invention with reference to the drawings in the specification, so that the technical content is clearer and easier to understand. The present invention can be embodied in many different forms of embodiments, and the protection scope of the present invention is not limited to the embodiments mentioned in the text.

[0037] In the drawings, components with the same structure are indicated by the same numerical reference numerals, and components with similar structures or functions are indicated by similar numerical reference numerals. The size and thickness of each component shown in the drawings are arbitrarily shown, and the present invention does not limit the size and thickness of each component. In order to make the illustration clearer, the thickness of the components is appropriately exaggerated in some places in the drawings.

[0038] Embodiment 1, as Figure 1 As shown, on a medium to heavy doped Si substrate 103 with 50-100nm silicon dioxide 102, a layer of 50-300nm thick metal film material 101 is deposited by magnetron sputtering (PVD) technology, the write transistor gate area is defined by photolithography, and the metal and oxide layer outside the write transistor gate area are etched. The write transistor gate area can be set to a rectangle with a length and width of 10nm-100μm respectively, or it can be set to a circle with a diameter of 10nm-100μm.

[0039] The oxide film on the medium and heavily doped Si substrate used can select other high-k materials, such as aluminum oxide, hafnium oxide, etc., to expand the range of choices; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., to expand the range of choices; the metal material used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, and can also be replaced with transparent conductive oxides such as ITO to expand the range of choices; the magnetron sputtering (PVD) technology here can be replaced with electron beam evaporation (EBE) technology to expand the range of choices.

[0040] Embodiment 2, as Figure 2 As shown, metal 201, heavily doped silicon substrate 203, a 10-200nm thick silicon dioxide gate dielectric film material 202 is deposited by atomic layer deposition (ALD) technology; the transistor active area is defined by photolithography, and the gate dielectric material in the active area is etched.

[0041] The silicon dioxide gate dielectric used here can be replaced with high-k dielectrics such as aluminum oxide or hafnium oxide to expand the range of options; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc.; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process to expand the range of options.

[0042] Embodiment 3, as Figure 3 As shown, metal 301, silicon dioxide or high-k dielectric 302, heavily doped silicon substrate 303, and a layer of amorphous metal oxide semiconductor thin film material 304 with a thickness of 10-200 nm are deposited by ALD technology.

[0043] The ALD technology is used to fill high aspect ratio grooves in cycles, and the filling of the grooves to a certain depth is the standard. The amorphous metal oxide semiconductor film can be IGZO, ITZO, IHO, ITGO, IGO and other metal oxide semiconductors that can be grown using ALD technology, expanding the range of choices.

[0044] Embodiment 4, as Figure 4 As shown, silicon dioxide or high-k dielectric 402, heavily doped silicon substrate 403, amorphous metal oxide semiconductor 404; a layer of 50-300nm thick metal film material 401 is deposited by magnetron sputtering (PVD) technology, the read transistor source region is defined by photolithography, and the metal in the read transistor source region is etched.

[0045] The photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., which expand the range of options; the metal material used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, or can be replaced with transparent conductive oxides such as ITO, expanding the range of options; the magnetron sputtering (PVD) technology here can be replaced with electron beam evaporation (EBE) technology, expanding the range of options; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process, expanding the range of options.

[0046] Embodiment 5, as Figure 5 As shown, metal 501, heavily doped silicon substrate 503, amorphous metal oxide semiconductor 504; a 10-200nm thick silicon dioxide electrical isolation layer thin film material 502 is deposited by ALD technology; interconnection windows are defined by photolithography, and the isolation layer material in the interconnection windows is etched.

[0047] The photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., which expand the range of options; the reactive ion etching (RIE) process used here can be replaced with an inductively coupled plasma etching (ICP) process, which expands the range of options; the silicon dioxide electrical isolation layer used here can be replaced with high-k materials such as aluminum oxide or hafnium oxide, which expands the range of options.

[0048] Embodiment 6, as Figure 6 As shown, silicon dioxide or high-k dielectric 602, heavily doped silicon substrate 603, amorphous metal oxide semiconductor 604; a layer of 50-300nm thick metal film material 601 is deposited by magnetron sputtering (PVD) technology, the double gate region of the read transistor is defined by photolithography, and the metal and oxide layers outside the double gate region of the read transistor are etched.

[0049] The photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., which expand the range of options; the metal material used here can be Al, Cr, Ti, Ni or W, and the above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, or can be replaced with transparent conductive oxides such as ITO, expanding the range of options; the magnetron sputtering (PVD) technology here can be replaced with electron beam evaporation (EBE) technology, expanding the range of options; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process, expanding the range of options.

[0050] Embodiment 7, as Figure 7 As shown, metal 701, heavily doped silicon substrate 703, amorphous metal oxide semiconductor 704; a 10-200nm thick silicon dioxide gate dielectric film material 702 is deposited by ALD technology; the read transistor active area is defined by photolithography, and the gate dielectric material in the active area is etched.

[0051] The silicon dioxide gate dielectric used here can be replaced with high-k dielectrics such as aluminum oxide or hafnium oxide to expand the range of options; the photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc.; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process to expand the range of options.

[0052] Embodiment 8, as Figure 8As shown, a silicon dioxide or high-k dielectric 802, a heavily doped silicon substrate 803, a layer of 10-200nm thick amorphous metal oxide semiconductor thin film material 804 is deposited by ALD technology, a layer of 50-300nm thick metal thin film material 801 is deposited by magnetron sputtering (PVD) technology, the drain area of ​​the read transistor is defined by photolithography, and the metal and amorphous metal oxide semiconductor materials outside the active area are etched.

[0053] The photolithography processes used here include ultraviolet lithography (UV, DUV, EUV) and electron beam lithography (EBL), etc., which expand the range of options; the ALD technology is used to fill the high aspect ratio grooves in cycles, and the filling of the grooves to a certain depth is the standard. The amorphous metal oxide semiconductor film can be IGZO, ITZO, IHO, ITGO, IGO and other metal oxide semiconductors that can be grown by ALD technology, which expands the range of options; the metal material used here can be Al, Cr, Ti, Ni or W. The above-mentioned metals can also be selectively co-sputtered to improve the chemical stability of the film, and can also be replaced with transparent conductive oxides such as ITO, which expands the range of options; the magnetron sputtering (PVD) technology here can be replaced with electron beam evaporation (EBE) technology, which expands the range of options; the etching process used here can be a reactive ion etching (RIE) process or an inductively coupled plasma etching (ICP) process, which expands the range of options.

[0054] The preferred specific embodiments of the present invention are described in detail above. It should be understood that ordinary technicians in the field can make many modifications and changes based on the concept of the present invention without creative work. Therefore, all technical solutions that can be obtained by technicians in the technical field based on the concept of the present invention through logical analysis, reasoning or limited experiments on the basis of the prior art should be within the scope of protection determined by the claims.

Claims

1. A method for manufacturing a 3D stacked gate-all-around 2T0C DRAM based on ALD technology, characterized in that: Adopting ring gate structure and process.

2. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology according to claim 1, characterized in that: Building a three-dimensional stack of read-write transistors.

3. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology as claimed in claim 1, characterized in that: Place the read and write transistors on the same plane.

4. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology according to claim 1, wherein: Adopt external gate structure and process.

5. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology as claimed in claim 1, characterized in that: Electrodes are drawn out from the middle of the vertical channel according to the wiring layer.

6. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology according to claim 1, characterized in that: include: Depositing a metal thin film material on a medium to heavy doped Si substrate having an oxide thin film; Defining the write transistor gate region by photolithography; Etch the metal and oxide layers outside the transistor gate area.

7. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology as claimed in claim 6, characterized in that: The oxide film includes silicon dioxide and high-k material.

8. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology as claimed in claim 6, characterized in that: The metal thin film material deposition technology includes magnetron sputtering technology and electron beam evaporation technology.

9. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology as claimed in claim 6, characterized in that: The photolithography includes ultraviolet photolithography and electron beam photolithography.

10. The method for manufacturing a 3D stacked gate-all-around 2TOC DRAM based on ALD technology according to claim 6, characterized in that: The write transistor gate region includes a rectangle and a circle.