3D ferroelectric memory structure and manufacturing method thereof
Patent Information
- Application Number
- CN202411285786.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-08
AI Technical Summary
但是现有的三维铁电存储单元中,如图2所示,在刻蚀深孔时,由于钨与S iON/S iOx的刻蚀速率不同,因此刻蚀到电容器导电柱时刻蚀停止,但导电柱周围的介质层继续向下刻蚀,会在电容器导电柱周边形成凹陷,导致电容单元无法着陆(l and on),即电容单元会下陷到钨与接触孔之间的凹槽内的现象(Foot ing i ssue),进而可能使得电容电极接触不良,影响铁电存储器性能
[0041] The invention provides a 3D ferroelectric memory structure and its manufacturing method, which uses dielectric layers with different etching rates, so that during the process of etching deep holes, the bottom speed is slower to significantly reduce the bottom of the deep holes. width, so that it is completely located on the capacitor conductive pillar, forming a specifically formed deep hole to ensure full contact between the capacitor electrode and the capacitor conductive pillar, thus effectively solving the foot inssue in the existing structure.
Smart Images

Figure CN118921988A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of ferroelectric memory, and in particular to a 3D ferroelectric memory structure and a manufacturing method thereof. Background Art
[0002] Ferroelectric memory is a non-volatile memory with a special process. When an electric field is applied to the ferroelectric transistor, the central atom stops at the first low energy state along the electric field, and when the electric field is reversed and applied to the same ferroelectric transistor, the central atom moves in the crystal along the direction of the electric field and stops at the second low energy state. A large number of central atoms move and couple in the crystal unit cell to form ferroelectric domains, which form polarized charges under the action of the electric field. The polarized charge formed by the reversal of the ferroelectric domain under the electric field is higher, and the polarized charge formed by the non-reversal of the ferroelectric domain under the electric field is lower. This binary stable state of ferroelectric materials allows ferroelectrics to be used as memory.
[0003] When the electric field is removed, the central atom remains in a low energy state and the state of the memory is preserved and will not disappear. Therefore, the ferroelectric domain can be reversed under the electric field to form a high polarization charge, or no inversion to form a low polarization charge to determine whether the storage unit is in the "1" or "0" state. The reversal of the ferroelectric domain does not require a high electric field, and only a normal operating voltage can change the state of the storage unit to "1" or "0". There is no need for a charge pump to generate high voltage data erasure, so there is no erase delay phenomenon. This feature enables ferroelectric memory to continue to save data after power failure, with fast write speed and unlimited write life, and it is not easy to be damaged. In addition, compared with existing non-volatile memory technology, ferroelectric memory has a higher write speed and a longer read and write life.
[0004] In order to improve the integration of ferroelectric memory cells, some products have begun to use three-dimensional ferroelectric memory structures. Figure 1 As shown in FIG. 1 , a deep hole capacitor is used in a three-dimensional ferroelectric memory structure, which can effectively reduce the overall volume of the memory cell while ensuring the capacitor area. However, in the existing three-dimensional ferroelectric memory cell, Figure 2 As shown in the figure, when etching deep holes, due to the interaction between tungsten and SiON / SiO x The etching rates are different, so the etching stops when the capacitor conductive column is etched, but the dielectric layer around the conductive column continues to etch downward, which will form a depression around the capacitor conductive column, resulting in the capacitor unit failing to land (l and on), that is, the capacitor unit will sink into the groove between the tungsten and the contact hole (Footing issue), which may cause poor contact between the capacitor electrodes and affect the performance of the ferroelectric memory. Summary of the invention
[0005] In view of some or all of the problems in the prior art, the present invention provides a method for manufacturing a 3D ferroelectric memory structure in a first aspect, comprising:
[0006] Providing a semiconductor substrate, the semiconductor substrate comprising a ferroelectric memory cell region, the ferroelectric memory cell region having a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region;
[0007] forming a first interconnect structure, the first interconnect structure comprising a capacitor conductive pillar, a bit line conductive pillar, and a first dielectric layer between the conductive pillars;
[0008] On the surface of the first dielectric layer, an etching stop layer, a second dielectric layer, a third dielectric layer and a hard mask layer are sequentially formed, wherein the etching rate of the second dielectric layer is lower than that of the third dielectric layer;
[0009] The hard mask layer is patterned by photolithography and etching processes, and the patterned hard mask layer is used as a mask for etching to form deep holes in the second dielectric layer and the third dielectric layer, and then the hard mask layer is removed, wherein the portion of the deep hole located in the third dielectric layer is cylindrical, and the portion located in the second dielectric layer is inverted cone, and the bottom area of the deep hole is not larger than the top area of the capacitor conductive column;
[0010] forming a first electrode layer, a high-K ferroelectric oxide layer and a second electrode layer in the deep hole in sequence to form a deep hole capacitor; and
[0011] Form metal interconnects, plate lines, and bit lines.
[0012] Further, forming the first electrode layer includes:
[0013] depositing a first electrode layer; and
[0014] The first electrode layer on the top surface of the third dielectric layer is removed, and only the first electrode layer on the bottom and side surfaces of the deep hole is retained.
[0015] Furthermore, the material of the etch stop layer is SiN.
[0016] Furthermore, the manufacturing method further comprises:
[0017] After forming the high-K ferroelectric oxide layer and the second electrode layer, depositing tungsten metal on the surface of the second electrode layer; and
[0018] At least a portion of the tungsten metal, the high-K ferroelectric oxide layer and the second electrode layer on the top surface of the third dielectric layer are removed by chemical grinding, so that each deep hole capacitor is separated from each other.
[0019] Furthermore, the manufacturing method further comprises:
[0020] A bit line conductive plug is formed on the second dielectric layer and the third dielectric layer, and the bit line conductive plug is electrically connected to the bit line conductive column in the first interconnect structure.
[0021] Further, forming metal interconnects and plate lines and bit lines includes:
[0022] forming a fourth dielectric layer on the top surface of the third dielectric layer;
[0023] Drilling holes on the fourth dielectric layer and forming conductive structures, wherein the conductive structures are electrically connected to the second electrode layer and the bit line conductive plugs respectively;
[0024] forming a plate line above the conductive structure, the plate line being electrically connected to the second electrode layer; and
[0025] A bit line and an external pad are formed above the plate line, and the bit line is electrically connected to a bit line conductive plug.
[0026] Furthermore, the manufacturing method further comprises:
[0027] After forming the high-K ferroelectric oxide layer and the second electrode layer, at least a portion of the first electrode layer, the high-K ferroelectric oxide layer and the second electrode layer on the top surface are removed by photolithography, etching and other processes, so that each capacitor is separated from each other.
[0028] Further, forming metal interconnects and plate lines and bit lines includes:
[0029] forming a fourth dielectric layer on the top surface of the third dielectric layer;
[0030] Drilling holes on the fourth dielectric layer and forming conductive structures, wherein the conductive structures are electrically connected to the second electrode layer and the bit line conductive plug, respectively, wherein the conductive structure electrically connected to the second electrode layer extends from the second electrode layer at the bottom of the deep hole to the top of the fourth dielectric layer, or the conductive structure electrically connected to the second electrode layer extends from the second electrode layer around the top of the deep hole to the top of the fourth dielectric layer;
[0031] forming a plate line above the conductive structure, the plate line being electrically connected to the second electrode layer; and
[0032] A bit line and an external pad are formed above the board line, and the bit line is electrically connected to the bit line conductive plug.
[0033] Based on the manufacturing method as described above, the second aspect of the present invention provides a 3D ferroelectric memory structure, comprising:
[0034] A semiconductor substrate, wherein the semiconductor substrate comprises a ferroelectric memory cell region, wherein the ferroelectric memory cell region comprises a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region,
[0035] A first interconnect structure disposed above the semiconductor substrate, the first interconnect structure comprising a capacitor conductive pillar, a bit line conductive pillar, and a first dielectric layer between the conductive pillars;
[0036] a second dielectric layer, and a third dielectric layer stacked on the second dielectric layer, wherein the etching rate of the second dielectric layer is lower than that of the third dielectric layer;
[0037] A deep hole penetrating through the second dielectric layer and the third dielectric layer, wherein the deep hole exposes the capacitor conductive column, wherein the portion of the deep hole located in the third dielectric layer is cylindrical, and the portion located in the second dielectric layer is inverted conical, and the bottom area of the deep hole is not greater than the top area of the capacitor conductive column;
[0038] A first electrode layer, a high-K ferroelectric oxide layer, and a second electrode layer are sequentially deposited on the sidewall and bottom of the deep hole; and
[0039] Plate lines and bit lines.
[0040] Furthermore, the 3D ferroelectric memory structure further includes a bit line conductive plug, and the bit line conductive plug includes a metal conductive column electrically connected to the bit line conductive column.
[0041] The present invention provides a 3D ferroelectric memory structure and a manufacturing method thereof, which adopts dielectric layers with different etching rates, so that in the process of etching deep holes, the bottom rate is slower, so as to significantly reduce the bottom width of the deep holes, so that the bottom width of the deep holes is completely located on the capacitor conductive column, forming a specifically formed deep hole, ensuring that the capacitor electrode is in full contact with the capacitor conductive column, thereby effectively solving the footing problem in the existing structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] To further illustrate the above and other advantages and features of various embodiments of the present invention, a more specific description of various embodiments of the present invention will be presented with reference to the accompanying drawings. It will be understood that these drawings only depict typical embodiments of the present invention and are therefore not to be considered as limiting the scope thereof. In the accompanying drawings, for clarity, identical or corresponding parts will be represented by identical or similar reference numerals.
[0043] Figure 1 A schematic diagram showing a 3D ferroelectric memory structure in the prior art;
[0044] Figure 2 A schematic diagram showing the foot-printing of a 3D ferroelectric memory structure in the prior art;
[0045] Figure 3 A schematic flow chart showing a method for manufacturing a 3D ferroelectric memory structure according to an embodiment of the present invention; and
[0046] Figure 4 A schematic structural diagram of a 3D ferroelectric memory structure according to an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0047] In the following description, the present invention is described with reference to various embodiments. However, those skilled in the art will recognize that various embodiments may be implemented without one or more specific details or with other replacement and / or additional methods, materials or components. In other cases, well-known structures, materials or operations are not shown or described in detail to avoid obscuring aspects of various embodiments of the present invention. Similarly, for the purpose of explanation, specific quantities, materials and configurations are set forth to provide a comprehensive understanding of embodiments of the present invention. However, the present invention may be implemented without specific details. In addition, it should be understood that the various embodiments shown in the drawings are illustrative representations and are not necessarily drawn to scale.
[0048] In this specification, reference to "one embodiment" or "the embodiment" means that a particular feature, structure, or characteristic described in conjunction with the embodiment is included in at least one embodiment of the present invention. The phrase "in one embodiment" appearing in various places in this specification does not necessarily all refer to the same embodiment.
[0049] In general, terms can be understood, at least in part, based on the context in which they are used. For example, the term "one or more" as used herein can be used to describe any feature, structure, or characteristic in the singular, or to describe a combination of features, structures, or characteristics in the plural, based at least in part on the context. Similarly, terms such as "a," "an," or "the" can also be understood, at least in part, based on the context, to express singular usage or to express plural usage.
[0050] It can be easily understood that the meaning of “on,” “over,” and “above” in the present invention should be interpreted in the broadest manner, so that “on” refers not only to being directly on something, but also includes being on something with intermediate features or intermediate layers between the two, and “on,” or “above” refers not only to being on or over something, but also includes being on or over something (i.e., directly on something) without intermediate features or intermediate layers between the two.
[0051] In addition, spatially relative terms, such as "below", "beneath", "lower", "above", "upper", etc., may be used herein for convenience to describe the relationship of one element or feature relative to another element or feature as illustrated in the drawings. Spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings. The device may be otherwise oriented (rotated 90° or at other orientations) and the spatially relative descriptors used herein interpreted likewise accordingly.
[0052] The term "substrate" as used herein refers to the material to which subsequent material layers are added. The substrate itself may be patterned. The material added to the substrate may be patterned, or may remain unpatterned. In addition, the substrate may include a variety of semiconductor materials, such as silicon, germanium, gallium arsenide, indium phosphide, etc. Alternatively, the substrate may also be made of electrically non-conductive materials, such as glass, plastic, or sapphire wafers.
[0053] The term "layer" as used herein refers to a material portion including a certain area with thickness. A layer may extend over the entirety of a structure below or above, or may have an extension less than that of a structure below or above. In addition, a layer may be a region of a homogeneous or heterogeneous continuous structure, the thickness of which is less than the thickness of the continuous structure. For example, a layer may be located between any pair of horizontal planes, or at the top or bottom surface of the continuous structure. A layer may extend horizontally, vertically, and / or along a tapered surface. A substrate may be a layer, may include one or more layers therein, and / or may have one or more layers thereon, and / or one or more layers below it. A layer may include multiple layers. For example, an interconnect layer may include one or more conductors and contact layers (wherein contacts, interconnects and / or vias are formed) and one or more dielectric layers.
[0054] In the manufacturing process of the existing 3D ferroelectric memory, when etching deep holes, due to the interaction between tungsten and SiON, SiO x The etching rates of the tungsten metal through hole are different, so when the etching stops on the surface of the tungsten metal through hole, the two sides continue to etch, forming a depression. Then, when the capacitor electrode material is deposited, it may sink into the groove between the tungsten metal and the deep hole, resulting in insufficient contact and serious footing. To solve this problem, the present application uses dielectric layers with different etching rates to gradually slow down the deep hole etching rate in the later stage, thereby reducing the bottom CD of the deep hole, and finally completely landing on the surface of the tungsten through hole.
[0055] The technical solution of the present invention is further described below in conjunction with the accompanying drawings of the embodiments.
[0056] Figure 3FIG. 1 is a flow chart showing a method for manufacturing a 3D ferroelectric memory structure according to an embodiment of the present invention. Figure 3 As shown, a method for manufacturing a 3D ferroelectric memory structure comprises:
[0057] First, in step 301, a semiconductor substrate is provided. The substrate may have completed the manufacturing process of the functional area. For example, the substrate includes a circuit area and a ferroelectric memory cell area. The circuit area and the ferroelectric memory cell area have formed a source area, a drain area, a gate area, an isolation area between devices, and electrodes and interconnecting metal lines above each functional area. The circuit area can be used to control the ferroelectric memory cell area;
[0058] Next, in step 302, a first interconnection structure is formed. A first interconnection structure is formed on the semiconductor substrate. In one embodiment of the present invention, the formation of the first interconnection structure may include: forming a first dielectric layer on the surface of the substrate, and then forming a through hole in the first dielectric layer by through hole lithography and etching to expose the external electrodes of each functional area on the semiconductor substrate, and then sequentially depositing an adhesion layer, i.e., a tungsten metal layer to fill the through hole, and finally performing a chemical mechanical polishing process to remove excess first dielectric layer, adhesion layer and tungsten metal layer to form a plurality of tungsten conductive pillars extending from the electrode on the surface of the semiconductor substrate to the top surface of the first dielectric layer. In one embodiment of the present invention, titanium nitride may be formed as an adhesion layer between the tungsten conductive pillar and the electrode on the surface of the semiconductor substrate and between the tungsten conductive pillar and the first dielectric layer. The plurality of tungsten conductive pillars may include circuit conductive pillars, capacitor conductive pillars, and bit line conductive pillars. The circuit conductive column is connected to the surface electrode of the circuit area, the capacitor conductive column is used to electrically connect the doped area (source or drain) of the transistor in the ferroelectric memory cell area with the capacitor, and the bit line conductive column is used to electrically connect another doped area (drain or source) of the transistor in the ferroelectric memory cell area with the bit line.
[0059] In one embodiment of the present invention, the first dielectric layer can be inorganic materials such as silicon oxide, silicon oxynitride, borosilicate glass, phosphorus silicate glass (PSG), borophosphosilicate glass (BPSG), fluorinated glass silicate glass (FSG), low-K dielectric, etc.; it can also be organic materials such as polyimide, photosensitive epoxy resin, solder mask ink, green paint, dry film, photosensitive build-up layer material, BCB (bisbenzocyclobutene resin) or PBO (phenylbenzobisoxazole resin). The first dielectric layer can be made by chemical vapor deposition, rolling, spin coating, spraying, printing, non-spin coating, hot pressing, vacuum lamination, immersion, pressure bonding, etc. The first dielectric layer can be a single material layer, or a composite material layer formed by stacking multiple layers of materials.
[0060] It should be understood by those skilled in the art that the method for forming the first interconnect structure is not limited to the above specific examples. In addition, other processes may be performed before or after the first interconnect structure is formed, for example, forming one or more other conductive interconnect structures;
[0061] Next, in step 303, the second and third dielectric layers are formed. An etching stop layer, a second dielectric layer, a third dielectric layer, and a hard mask layer are sequentially formed on the surface of the first interconnect structure. In one embodiment of the present invention, the hard mask layer uses a carbon layer and a silicon oxynitride layer as a hard mask for deep hole etching. In one embodiment of the present invention, the etching rate of the second dielectric layer is lower than that of the third dielectric layer, so that in the subsequent deep hole etching process, the etching rate will gradually slow down, and the size of the deep hole will gradually decrease. In an embodiment of the present invention, the formation process and size of the second and third dielectric layers, the carbon layer and the silicon oxynitride layer can be selected according to specific requirements. For example, according to the top size of the tungsten conductive column and the total thickness of the second and third dielectric layers, the thickness of the second and third dielectric layers is determined respectively, and then according to the thickness of the second and third dielectric layers, the etching rate of the second and third dielectric layers is determined. According to different product requirements and / or processes, there will be certain differences in the etching rate ratio of the second and third dielectric layers. In one embodiment of the present invention, the etching rate ratio of the second and third dielectric layers is preferably in the range of 1:3 to 1:5, but is not limited to this range;
[0062] Next, in step 304, a deep hole is etched. A capacitor deep hole is formed in the second dielectric layer and the third dielectric layer by an etching process, and the carbon layer and the silicon oxynitride layer are removed. In one embodiment of the present invention, forming a capacitor deep hole by an etching process includes forming a window in the silicon oxynitride layer to expose the underlying carbon layer by a photolithography etching process, etching the carbon layer using the silicon oxynitride layer as a mask to form a window to expose the underlying third and second dielectric layers, etching the third and second dielectric layers using the carbon layer as a mask until the etching stop layer is reached, and finally removing the carbon layer 352 and the silicon oxynitride layer 353. As described above, since the etching rate of the second dielectric layer is lower than that of the third dielectric layer, the portion of the capacitor deep hole finally formed in the third dielectric layer is cylindrical or quasi-cylindrical, while the portion in the second dielectric layer is in an inverted cone shape as a whole due to the gradually slowing etching rate, and the bottom area of the deep hole can be made not larger than the top area of the capacitor conductive column by selecting a suitable second dielectric layer material;
[0063] Next, in step 305, a deep hole capacitor is formed. A first electrode layer, a high-K ferroelectric oxide layer and a second electrode layer are sequentially formed on the bottom and sidewall of the deep hole. The first electrode layer is an electrode layer of a capacitor, for example, it can be one or more of the following materials: titanium (Ti), titanium nitride (Tin), titanium silicon nitride (TiSiNx), titanium aluminum nitride (TiAlNx), titanium carbonitride (TiCNx), tantalum nitride (TaNx), tantalum silicon nitride (TaSiNx), tantalum aluminum nitride (TaAlNx), tungsten nitride (WNx), tungsten silicide (WSix), tungsten carbonitride (WCNx), ruthenium (Ru), ruthenium oxide (RuOx), iridium (Ir), doped polysilicon, transparent conductive oxide (TCO) or iridium oxide (IrOx) or a combination of these materials. The first electrode layer can be deposited by one or more processes such as atomic layer deposition ALD, chemical vapor deposition CVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD and similar deposition processes, and then the material layer on the top of the dielectric layer is removed, leaving only the material layer at the bottom and side of the deep hole. The high-K ferroelectric oxide layer is a dielectric layer of the capacitor, which can be, for example, one or more of the following materials: the ferroelectric material includes oxygen and one or more ferroelectric metals, the ferroelectric metals include zirconium (Zr), hafnium (Hf), titanium (Ti), aluminum (Al), nickel (Ni) and / or iron (Fe), etc., and the ferroelectric material can be doped with Group II elements (such as calcium (Ca), strontium (Sr) or barium (Ba); Group III elements (such as scandium (Sc), yttrium (Y), aluminum (Al), gallium (Ga) and indium (I n)); and lanthanide elements (i.e., lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Eu), gadolinium (Gd), terbium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), ytterbium (Yb), lutetium (Lu)) or a combination of these materials. The high-K ferroelectric oxide layer can be deposited by one or more processes selected from atomic layer deposition ALD, chemical vapor deposition CVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD, and similar deposition processes.And the second electrode layer is another electrode layer of the capacitor, which can be, for example, one or more of the following materials: titanium (Ti), titanium nitride (TiN), titanium silicon nitride (TiSiNx), titanium aluminum nitride (TiAlNx), titanium carbonitride (TiCNx), tantalum nitride (TaNx), tantalum silicon nitride (TaSiNx), tantalum aluminum nitride (TaAlNx), tungsten nitride (WNx), tungsten silicide (WSix), tungsten carbonitride (WCNx), ruthenium (Ru), ruthenium oxide (RuOx), iridium (Ir), doped polysilicon, transparent conductive oxide (TCO) or iridium oxide (IrOx) or a combination of these materials. Similarly, the second electrode layer can be deposited by one or more processes of atomic layer deposition ALD, chemical vapor deposition CVD, physical vapor deposition PVD, electron beam Ebeam evaporation deposition, molecular beam epitaxy MBE deposition, pulsed laser deposition PLD and similar deposition processes;.
[0064] Next, in step 306, tungsten metal is filled. Tungsten metal is filled on the surface of the second electrode layer, and then at least part of the tungsten metal, the high-K ferroelectric oxide layer and the second electrode layer on the top surface of the third dielectric layer are removed by chemical grinding to separate the capacitors; and
[0065] Finally, in step 307, metal interconnection, plate line and bit line are formed. In one embodiment of the present invention, the formation of metal interconnection, plate line and bit line may include: first forming a fourth dielectric layer on the surface of the third dielectric layer; drilling holes on the fourth dielectric layer and forming multiple conductive pillars to connect to tungsten metal, circuit conductive pillars and bit line conductive plugs; then forming a fifth dielectric layer on the fourth dielectric layer, etching holes on the fifth dielectric layer, depositing metal copper in the holes to form metal lines as plate lines and metal interconnection; then forming a sixth dielectric layer on the fifth dielectric layer, and then slotting the sixth dielectric layer, and then depositing metal copper in the slots to form metal lines as bit lines. So far, the ferroelectric capacitor, plate line and bit line of the memory are formed, and then dielectric layers, metal interconnections and other metal layers are formed above the plate line and bit line to form external connections, which will not be described in detail here. In one embodiment of the present invention, the fourth, fifth and sixth dielectric layers can be the same material as the first dielectric layer, or different materials from the first dielectric layer. The bit line conductive plug can be formed simultaneously with the formation of the capacitor deep hole. Specifically, while forming the capacitor deep hole, a through hole is formed on the second dielectric layer and the third dielectric layer, and the through hole exposes the top surface of the bit line conductive column; then an adhesive layer and a tungsten metal layer are deposited in sequence to fill the through hole; finally, a chemical mechanical polishing process is performed to remove the excess third dielectric layer and tungsten metal layer, and a tungsten conductive column extending from the top surface of the bit line conductive column to the top surface of the third dielectric layer is formed as the bit line conductive plug. While forming the above bit line conductive plug, a tungsten conductive column electrically connected to the circuit conductive column can be formed above the circuit area, so that the circuit conductive column extends to the top surface of the dielectric layer bit line conductive plug.
[0066] As mentioned above, in order to form an independent ferroelectric capacitor structure, it is necessary to grind away part of the MIM film outside the deep hole structure, but this process is prone to metal ion residue, resulting in leakage of the upper and lower electrodes. If the upper electrode has a photolithography alignment deviation, it is easy to cause a direct short circuit between the upper and lower electrodes. To solve this problem, in one embodiment of the present invention, after forming the first electrode layer, the high-K ferroelectric oxide layer and the second electrode layer, tungsten metal is not filled, but the fourth dielectric layer is filled, and then at least part of the first electrode layer, the high-K ferroelectric oxide layer and the second electrode layer on the top surface are removed by photolithography, etching and other processes, so that each capacitor is separated from each other. Based on this, the subsequent formation of metal interconnection and plate line and bit line is also slightly different. Specifically, a hole is drilled in the fourth dielectric layer, and a plurality of conductive pillars are formed, which are respectively connected to the second electrode layer, the circuit conductive pillar, and the bit line conductive plug, wherein the conductive pillar connected to the second electrode layer is located at the center of the capacitor. The conductive pillar extends from the bottom of the capacitor deep hole to the top of the fourth dielectric layer. In another embodiment of the present invention, the conductive pillar connected to the second electrode layer of the capacitor can be set at the top edge of the capacitor deep hole. After forming the conductive pillar connected to the second electrode layer of the capacitor, a copper metal plate line connected to the conductive pillar, a dielectric layer and a copper metal bit line connected to the conductive pillar may be formed according to processes similar to the above embodiments.
[0067] Based on the manufacturing method described above, Figure 4 FIG. 2 is a schematic diagram showing a 3D ferroelectric memory structure according to an embodiment of the present invention. Figure 4 As shown, a 3D ferroelectric memory structure includes a semiconductor substrate 401, a first interconnect structure 402, an etch stop layer 403, a second dielectric layer 441, a second dielectric layer 442, a capacitor 405, a filled tungsten metal 406, a plate line, and a bit line.
[0068] The semiconductor substrate includes a ferroelectric memory cell area, which has a source area, a drain area, a gate area, an isolation area, and electrodes and interconnecting metal lines above each functional area. The first interconnection structure is arranged above the semiconductor substrate, including a capacitor conductive column 421, a bit line conductive column, and a first dielectric layer 422 between the conductive columns.
[0069] The etch stop layer is arranged on the surface of the first dielectric layer, and the second dielectric layer and the third dielectric layer are sequentially stacked on the surface of the etch stop layer, wherein the etching rate of the second dielectric layer is lower than that of the third dielectric layer.
[0070] The capacitor is formed at a deep hole that penetrates the second dielectric layer and the third dielectric layer, the deep hole exposes the capacitor conductive column, and the portion of the deep hole located in the third dielectric layer is cylindrical, and the portion located in the second dielectric layer is inverted cone, and the bottom area of the deep hole is not greater than the top area of the capacitor conductive column. The capacitor includes a first electrode layer, a high-K ferroelectric oxide layer, and a second electrode layer that are sequentially deposited on the sidewall and bottom of the deep hole.
[0071] The 3D ferroelectric memory structure further includes a bit line conductive plug, wherein the bit line conductive plug includes a metal conductive pillar electrically connected to the bit line conductive pillar.
[0072] Although various embodiments of the present invention are described above, it should be understood that they are presented as examples only and not as limitations. It is obvious to those skilled in the relevant art that various combinations, modifications and changes can be made thereto without departing from the spirit and scope of the present invention. Therefore, the breadth and scope of the present invention disclosed herein should not be limited by the exemplary embodiments disclosed above, but should only be defined according to the attached claims and their equivalents.
Claims
1. A method for manufacturing a 3D ferroelectric memory structure, characterized in that: Includes steps: Providing a semiconductor substrate, the semiconductor substrate comprising a ferroelectric memory cell region, the ferroelectric memory cell region having a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region; forming a first interconnect structure, the first interconnect structure comprising a capacitor conductive pillar, a bit line conductive pillar, and a first dielectric layer between the conductive pillars; On the surface of the first dielectric layer, an etching stop layer, a second dielectric layer, a third dielectric layer and a hard mask layer are sequentially formed, wherein the etching rate of the second dielectric layer is lower than that of the third dielectric layer; The hard mask layer is patterned by photolithography and etching processes, and the patterned hard mask layer is used as a mask for etching to form deep holes in the second dielectric layer and the third dielectric layer, and then the hard mask layer is removed, wherein the portion of the deep hole located in the third dielectric layer is cylindrical, and the portion located in the second dielectric layer is inverted cone, and the bottom area of the deep hole is not larger than the top area of the capacitor conductive column; forming a first electrode layer, a high-K ferroelectric oxide layer and a second electrode layer in the deep hole in sequence to form a deep hole capacitor; as well as Form metal interconnects, plate lines, and bit lines.
2. The manufacturing method according to claim 1, characterized in that Forming the first electrode layer comprises the steps of: depositing a first electrode layer; and The first electrode layer on the top surface of the third dielectric layer is removed, and only the first electrode layer on the bottom and side surfaces of the deep hole is retained.
3. The manufacturing method according to claim 1, characterized in that: The material of the etching stop layer is SiN.
4. The manufacturing method according to claim 1, characterized in that: Also includes: A bit line conductive plug is formed on the second dielectric layer and the third dielectric layer, and the bit line conductive plug is electrically connected to the bit line conductive column in the first interconnect structure.
5. The manufacturing method according to claim 4, characterized in that: Also includes the steps: After forming the high-K ferroelectric oxide layer and the second electrode layer, depositing tungsten metal on the surface of the second electrode layer; as well as At least a portion of the tungsten metal, the high-K ferroelectric oxide layer and the second electrode layer on the top surface of the third dielectric layer are removed by chemical grinding, so that each deep hole capacitor is separated from each other.
6. The manufacturing method according to claim 5, characterized in that: Forming metal interconnects and plate and bit lines includes: forming a fourth dielectric layer on the top surface of the third dielectric layer; Drilling holes on the fourth dielectric layer and forming conductive structures, wherein the conductive structures are electrically connected to the tungsten metal and the bit line conductive plugs respectively; forming a plate line over the conductive structure, the plate line being electrically connected to the tungsten metal; and A bit line and an external pad are formed above the plate line, and the bit line is electrically connected to a bit line conductive plug.
7. The manufacturing method according to claim 4, characterized in that: Also includes: After forming the high-K ferroelectric oxide layer and the second electrode layer, at least a portion of the first electrode layer, the high-K ferroelectric oxide layer and the second electrode layer on the top surface are removed by photolithography, etching and other processes, so that each capacitor is separated from each other.
8. The manufacturing method according to claim 7, characterized in that: Forming metal interconnects and plate and bit lines includes: forming a fourth dielectric layer on the top surface of the third dielectric layer; Drilling holes on the fourth dielectric layer and forming conductive structures, wherein the conductive structures are electrically connected to the second electrode layer and the bit line conductive plug, respectively, wherein the conductive structure electrically connected to the second electrode layer extends from the second electrode layer at the bottom of the deep hole to the top of the fourth dielectric layer, or the conductive structure electrically connected to the second electrode layer extends from the second electrode layer around the top of the deep hole to the top of the fourth dielectric layer; forming a plate line above the conductive structure, the plate line being electrically connected to the second electrode layer; and A bit line and an external pad are formed above the board line, and the bit line is electrically connected to the bit line conductive plug.
9. A 3D ferroelectric memory structure, characterized in that: include: A semiconductor substrate, wherein the semiconductor substrate comprises a ferroelectric memory cell region, wherein the ferroelectric memory cell region comprises a source region, a drain region, a gate region, an isolation region, and electrodes and interconnecting metal lines above each functional region; A first interconnect structure disposed above the semiconductor substrate, the first interconnect structure comprising a capacitor conductive pillar, a bit line conductive pillar, and a first dielectric layer between the conductive pillars; a second dielectric layer, and a third dielectric layer stacked on the second dielectric layer, wherein the etching rate of the second dielectric layer is lower than that of the third dielectric layer; A deep hole penetrating through the second dielectric layer and the third dielectric layer, wherein the deep hole exposes the capacitor conductive column, wherein the portion of the deep hole located in the third dielectric layer is cylindrical, and the portion located in the second dielectric layer is inverted conical, and the bottom area of the deep hole is not greater than the top area of the capacitor conductive column; A first electrode layer, a high-K ferroelectric oxide layer, and a second electrode layer are sequentially deposited on the sidewall and bottom of the deep hole; as well as Plate lines and bit lines.
10. The 3D ferroelectric memory structure according to claim 9, characterized in that: Also included is a bit line conductive plug, wherein the bit line conductive plug includes a metal conductive pillar electrically connected to the bit line conductive pillar.