Production method of high-molecular-weight copolymer BOPP (biaxially-oriented polypropylene) pre-coating film
By using the design of a base layer composed of high molecular weight PP, homopolymer PP and talc powder and liftable turntable fixture, the problem of low puncture intensity detection efficiency of BOPP pre-coated film is solved, and rapid and accurate detection of the puncture intensity of the film is achieved, including The puncture intensity of the film block movement when the needle is stationary.
Patent Information
- Application Number
- CN202310518846.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-12
AI Technical Summary
The puncture intensity detection efficiency of the existing BOPP pre-coated film is low, and it is impossible to detect the puncture intensity when the needle is stationary and the film block is moved.
The base layer consisting of high molecular weight PP, homopolymer PP and talc powder is used to prepare films through an extruder, a longitudinal puller and a transverse tensile mechanism, and a liftable turntable and multiple fixtures are installed on the puncture strength test machine to achieve the films. Continuous rapid detection.
The efficiency and accuracy of film puncture intensity detection are improved, and the puncture intensity parameters of the film can be obtained in a short time, including the puncture intensity when the needle is stationary and the film block is moved.
Smart Images

Figure CN118927682A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of BOPP films, in particular to a method for producing a high molecular weight copolymer BOPP pre-coating film. Background Art
[0002] Pre-coated film is a flexible packaging material used for printed products. It is first coated with glue on the film by the pre-coated film processing factory according to the specifications and format, and then rewound for the user to choose, and then laminated with the printed matter. The puncture resistance of the film is one of the important indicators for testing packaging materials. The BOPP pre-coated film will also be tested for puncture force after it is produced. During the test, the film is placed on the fixture of the test machine through a film puncture strength tester, and then the needle on the linear slide moves downward to puncture the film. The puncture force is obtained by the change in force and displacement during work. The same batch of film needs to be cut into multiple small film block samples for testing. The samples are usually 5 to 10, but there is only one fixture on the film puncture strength tester, so the film can only be taken and placed piece by piece during the test, and the work efficiency is not high. Moreover, the film is still during the test, and the needle is moving. It is impossible to detect the puncture strength when the needle is still and the film block is moving. Summary of the invention
[0003] In view of the above-mentioned defects of the prior art, an object of the present invention is to provide a method for producing a high molecular weight copolymer BOPP pre-coating film.
[0004] To solve the above problems, the technical solution of the present invention is: a method for producing a high molecular weight copolymer BOPP pre-coating film, the BOPP pre-coating film comprising a base layer, a primer layer and a hot melt adhesive layer arranged in sequence from bottom to top, the base layer being composed of high molecular weight PP, homopolymer PP and talcum powder; The production method comprises the following steps: (1) The base material is fed into an extruder for mixing and plasticizing, and the molten melt is fed into a die head. The melt passes through a flat die head opening to form a molten sheet. The sheet is then attached to a chilled roller by an air knife to form an unshaped sheet. The sheet is then shaped into a cast sheet after being cooled in a water bath. The cast sheet is then passed through a longitudinal stretching machine and a transverse stretching machine to draw the sheet into a film to obtain the base layer. (2) Corona treatment of the surface of the base layer; (3) Apply the primer layer on the surface of the base layer and dry it after application; (4) Compounding a layer of hot melt adhesive on the surface of the primer layer, and then cooling and shaping; (5) The puncture strength tester is used to test the puncture force of the film. The puncture strength tester is provided with a turntable that can be raised and lowered, and a plurality of clamps are evenly distributed on the turntable.
[0005] Furthermore, the components of the base layer are as follows by mass ratio: 20% high molecular weight PP, 70% homopolymer PP, and 10% talc.
[0006] Furthermore, in step (5), the puncture strength testing machine includes a main machine, a frame is provided on the top of the main machine, a linear module is provided in the up-down direction at the front end of the frame, a slide is provided at the front end of the linear module, a load sensor is installed at the front end of the slide, a needle is provided at the lower end of the load sensor, a lifting device is provided at the top of the main machine and is located in front of the frame, a motor is provided at the top of the lifting device, an output shaft at the upper end of the motor is connected to a turntable, a plurality of clamps are evenly distributed on the outer edge of the turntable, and the needle is located above the clamp.
[0007] Furthermore, the lifting device includes two lifting cylinders fixed on the top of the main machine and arranged in the up-down direction and a lifting plate fixed on the top of the two lifting cylinders, and the motor is fixed on the top of the lifting plate.
[0008] Further, detecting the puncture force of the film comprises the following steps: (51) Place the cut film blocks on the clamps and clamp them, with each clamp clamping one film block; (52) The slide table drives the needle to move downward, and the needle pierces the first film block. After the detection, the needle moves upward and resets, and then the turntable rotates one station to detect the second film block. All film blocks are detected in this way; Alternatively, (52) the needle remains stationary, and the lifting cylinder controls the lifting plate to move upward, driving the turntable and the clamp to move upward until the needle contacts and pierces the first film block. After the detection, the lifting cylinder controls the turntable to move downward and reset, and then the turntable rotates one station to detect the second film block. All film blocks are detected in this way.
[0009] The beneficial effects of the present invention are as follows: the base layer is composed of high molecular weight PP, homopolymer PP and talcum powder, excellent mechanical properties can be obtained by blending high molecular weight PP and homopolymer PP, and the added talcum powder has a significant improvement on the processing properties of the composite material; The puncture strength testing machine is equipped with a liftable turntable with multiple clamps evenly distributed on it, which can continuously and quickly test the puncture strength of the film, and is conducive to obtaining the puncture strength parameters of the film in a short time; because the turntable can be raised and lowered, the puncture strength can be tested when the needle is stationary and the film block is moving. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 It is a schematic structural diagram of the BOPP pre-coating film of the present invention; Figure 2 It is a structural schematic diagram of the puncture strength testing machine of the present invention.
[0011] 1—base layer, 2—primer layer, 3—hot melt adhesive layer, 4—turntable, 5—clamp, 6—main machine, 7—frame, 8—linear module, 81—slide, 9—load sensor, 10—needle, 11—motor, 12—lifting cylinder, 13—lifting plate. Implementation
[0012] In order to more intuitively and completely understand the technical solution of the present invention, a non-limiting feature description is now provided in conjunction with the accompanying drawings of the present invention as follows: like Figure 1 , Figure 2 As shown, a method for producing a high molecular weight copolymer BOPP pre-coating film, the BOPP pre-coating film comprises a base layer 1, a primer layer 2 and a hot melt adhesive layer 3 arranged in sequence from bottom to top, the base layer 1 is composed of high molecular weight PP, homopolymer PP and talcum powder; The production method comprises the following steps: (1) The raw materials of the base layer 1 are fed into an extruder for mixing and plasticizing, and the molten melt is fed into a die head. The melt passes through a flat die head opening to form a molten sheet, and then the sheet is attached to a chilled roller by an air knife to be quenched to form an unshaped sheet, and then the sheet is shaped into a cast sheet after being cooled in a water bath. The cast sheet is then passed through a longitudinal stretching machine and a transverse stretching machine respectively to draw the sheet into a film, thereby obtaining the base layer 1; (2) performing corona treatment on the surface of the base layer 1; (3) Applying the primer layer 2 on the surface of the base layer 1 and drying it after application; (4) Compounding a hot melt adhesive layer 3 on the surface of the primer layer 2, and then cooling and shaping; (5) The puncture strength tester is used to test the puncture force of the film. The puncture strength tester is provided with a liftable turntable 4 on which a plurality of clamps 5 are evenly distributed.
[0013] The components of the base layer 1 are as follows by mass ratio: 20% high molecular weight PP, 70% homopolymer PP, and 10% talc.
[0014] In step (5), if Figure 2As shown, the puncture strength tester includes a main machine 6, a frame 7 is provided on the top of the main machine 6, a linear module 8 is provided in the up-down direction at the front end of the frame 7, a slide 81 is provided at the front end of the linear module 8, a load sensor 9 is installed at the front end of the slide 81, and a needle 10 is provided at the lower end of the load sensor 9. A lifting device located in front of the frame 7 is provided on the top of the main machine 6, and a motor 11 is provided on the top of the lifting device. The output shaft at the upper end of the motor 11 is connected to the turntable 4, and a plurality of clamps 5 are evenly distributed on the outer edge of the turntable 4, and the needle 10 is located above the clamp 5. The lifting device includes two lifting cylinders 12 fixed on the top of the main machine 6 and arranged in the up-down direction, and a lifting plate 13 fixed on the top of the two lifting cylinders 12, and the motor 11 is fixed on the top of the lifting plate 13. The linear module 8 can drive the needle 10 to move up and down, the motor 11 can drive the turntable 4 to rotate, and the lifting cylinder 12 can drive the turntable 4 to move up and down.
[0015] Testing the puncture force of a film includes the following steps: (51) Place the cut film blocks on the clamps 5 and clamp them, with each clamp 5 clamping one film block; (52) The slide 81 drives the needle 10 to move downward, and the needle 10 pierces the first film block. After the detection, the needle 10 moves upward to reset, and then the turntable 4 rotates one station to detect the second film block. In this way, all the film blocks are detected; or, step (52) is: the needle 10 remains stationary, the lifting cylinder 12 controls the lifting plate 13 to move upward, driving the turntable 4 and the clamp 5 to move upward until the needle 10 contacts and pierces the first film block. After the detection, the lifting cylinder 12 controls the turntable 4 to move downward to reset, and then the turntable 4 rotates one station to detect the second film block. In this way, all the film blocks are detected.
[0016] The base layer 1 of the present invention is composed of high molecular weight PP, homopolymer PP and talcum powder. Excellent mechanical properties can be obtained by blending high molecular weight PP and homopolymer PP, and the added talcum powder has a significant improvement on the processing properties of the composite material. The puncture strength tester is provided with a liftable turntable 4, on which a plurality of clamps 5 are evenly distributed, which can continuously and quickly detect the puncture strength of the film, and is conducive to obtaining the puncture strength parameters of the film in a short time; because the turntable 4 can be lifted and lowered, the puncture strength can be detected when the needle 10 is stationary and the film block is moving.
Claims
1. A method for producing a high molecular weight copolymer BOPP pre-coating film, the BOPP pre-coating film comprising a base layer, a primer layer and a hot melt adhesive layer arranged in sequence from bottom to top, characterized in that: The base layer is composed of high molecular weight PP, homopolymer PP and talcum powder; The production method comprises the following steps: (1) The base material is fed into an extruder for mixing and plasticizing, and the molten melt is fed into a die head. The melt passes through a flat die head opening to form a molten sheet. The sheet is then attached to a chilled roller by an air knife to form an unshaped sheet. The sheet is then shaped into a cast sheet after being cooled in a water bath. The cast sheet is then passed through a longitudinal stretching machine and a transverse stretching machine to draw the sheet into a film to obtain the base layer. (2) Corona treatment of the surface of the base layer; (3) Apply the primer layer on the surface of the base layer and dry it after application; (4) Compounding a layer of hot melt adhesive on the surface of the primer layer, and then cooling and shaping; (5) The puncture strength tester is used to test the puncture force of the film. The puncture strength tester is provided with a turntable that can be raised and lowered and a plurality of clamps are evenly distributed on the turntable.
2. The method for producing a high molecular weight copolymer BOPP pre-coating film according to claim 1, characterized in that: The components of the base layer are as follows by mass ratio: high molecular weight PP 20%, homopolymer PP 70%, and talc 10%.
3. The method for producing a high molecular weight copolymer BOPP pre-coating film according to claim 1, characterized in that: In step (5), the puncture strength testing machine includes a main machine, a frame is provided on the top of the main machine, a linear module is provided in the up-down direction at the front end of the frame, a slide is provided at the front end of the linear module, a load sensor is installed at the front end of the slide, a needle is provided at the lower end of the load sensor, a lifting device is provided at the top of the main machine and is located in front of the frame, a motor is provided at the top of the lifting device, an output shaft at the upper end of the motor is connected to a turntable, a plurality of clamps are evenly distributed on the outer edge of the turntable, and the needle is located above the clamp.
4. The method for producing a high molecular weight copolymer BOPP pre-coating film according to claim 3, characterized in that: The lifting device comprises two lifting cylinders fixed on the top of the main machine and arranged in the up-down direction and a lifting plate fixed on the top of the two lifting cylinders, and the motor is fixed on the top of the lifting plate.
5. The method for producing a high molecular weight copolymer BOPP pre-coating film according to claim 4, characterized in that: Testing the puncture force of a film includes the following steps: (51) Place the cut film blocks on the clamps and clamp them, with each clamp clamping one film block; (52) The slide table drives the needle to move downward, and the needle pierces the first film block. After the detection, the needle moves upward and resets, and then the turntable rotates one station to detect the second film block. All film blocks are detected in this way; Alternatively, (52) the needle remains stationary, and the lifting cylinder controls the lifting plate to move upward, driving the turntable and the clamp to move upward until the needle contacts and pierces the first film block. After the detection, the lifting cylinder controls the turntable to move downward and reset, and then the turntable rotates one station to detect the second film block. All film blocks are detected in this way.