Semiconductor device and manufacturing method thereof

By setting a recess at the connection between the sensitive material layer of the MEMS device and the side wall layer, the actual length of the interface layer is increased, the problem of corrosion of the interface layer is solved, and the overall structural stability and production efficiency of the semiconductor device are improved.

CN118929561APending Publication Date: 2024-11-12RUNXIN SENSING TECHNOLOGY (NANCHANG) CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310535678.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

When removing the sacrificial layer of existing MEMS devices, the interface layer between the sensitive material layer and the side wall layer is easily corroded, resulting in device failure, and the removal process is high and the production capacity is limited.

Method used

The recesses are provided at the connection between the sensitive material layer and the side wall layer. By forming arc-shaped or concave-shaped recesses at the bottom of the groove, the actual length of the interface layer is increased, the difficulty of the interface layer being corroded, and through the side wall The high etching ratio of the layer to the sacrificial layer is removed to form a cavity structure.

Benefits of technology

On the premise of ensuring that the cavity structure volume and the projection length of the interface layer remain unchanged, the actual length of the interface layer is increased, the corrosion difficulty of the interface layer is reduced, and the overall structural stability and production efficiency of the semiconductor device are enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118929561A_ABST
    Figure CN118929561A_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor device and a manufacturing method thereof. The method comprises the following steps: providing a semiconductor substrate; forming a sensitive material layer on the semiconductor substrate; a sacrificial layer is formed on the sensitive material layer, a groove penetrating through the sacrificial layer is formed in the sacrificial layer, and the groove is used for defining the boundary of a cavity structure; etching the sensitive material layer exposed at the bottom of the groove so as to form a concave part on the surface of the sensitive material layer; forming a side wall layer which fills the groove and covers the surface of the sacrificial layer; forming a release hole connected with the sacrificial layer in the side wall layer; and removing the sacrificial layer surrounded by the side wall layer through the release hole so as to form a cavity structure in the side wall layer. The corrosion speed of the interface layer between the sensitive material layer and the side wall layer can be reduced, and cracking between the sensitive material layer and the side wall layer is avoided.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art

[0002] MEMS (Micro-Electro-Mechanical System) refers to a micro system that integrates mechanical components, drive components, optical systems, and electronic control systems into a whole. MEMS devices have advantages such as small size and low power consumption, and have a wide range of application scenarios in smart phones, tablets, game consoles, automobiles, drones, and other fields. Similar to integrated circuits, MEMS devices are also developing in the direction of high performance, miniaturization, low cost, and integration.

[0003] The cavity structure of existing MEMS devices is formed by removing the sacrificial layer between the sensitive material layer and the sidewall layer through the release hole using a wet or dry etching process. However, there is usually an interface layer between the sensitive material layer and the sidewall layer. When removing the sacrificial layer, the etching reaction gas or liquid will corrode the interface layer, causing cracks in the sensitive material layer and the sidewall layer, resulting in serious process problems and causing device failure. Summary of the invention

[0004] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.

[0005] In view of the existing problems, an embodiment of the present invention provides a method for manufacturing a semiconductor device, the method comprising:

[0006] providing a semiconductor substrate;

[0007] forming a sensitive material layer on the semiconductor substrate;

[0008] forming a sacrificial layer on the sensitive material layer, wherein a groove penetrating the sacrificial layer is formed in the sacrificial layer, and the groove is used to define a boundary of a cavity structure;

[0009] Etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer;

[0010] forming a sidewall layer filling the groove and covering the surface of the sacrificial layer;

[0011] forming a release hole in the sidewall layer connected to the sacrificial layer;

[0012] The sacrificial layer surrounded by the sidewall layer is removed through the release hole to form a cavity structure in the sidewall layer.

[0013] In some embodiments, the bottom of the recessed portion is arc-shaped.

[0014] In some embodiments, when the bottom of the recessed portion is arc-shaped, etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer includes:

[0015] The sensitive material layer exposed at the bottom of the groove is etched using an isotropic etching process to form the concave portion with an arc-shaped bottom.

[0016] In some embodiments, the bottom of the recessed portion is concave-convex.

[0017] In some embodiments, when the bottom of the recessed portion is concave-convex, etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer includes:

[0018] forming photoresist layers of different thicknesses at the bottom of the groove;

[0019] The sensitive material layer exposed at the bottom of the groove is etched based on the photoresist layers with different thicknesses to form the concave portion with a concave-convex bottom.

[0020] In some embodiments, the sensitive material layer includes a sensitive material layer;

[0021] Before forming the sensitive material layer on the semiconductor substrate, the method further comprises: forming a first electrode on the semiconductor substrate;

[0022] Before forming the sensitive material layer on the semiconductor substrate and after forming the sacrificial layer on the sensitive material layer, the method further includes: forming a second electrode on the sensitive material layer.

[0023] A second aspect of an embodiment of the present invention provides a method for manufacturing a semiconductor device, the method comprising:

[0024] providing a semiconductor substrate;

[0025] forming a sensitive material layer on the semiconductor substrate;

[0026] Etching the sensitive material layer to form a recessed portion on the surface of the sensitive material layer, wherein the recessed portion is used to define a boundary of the cavity structure;

[0027] forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the sensitive material layer, wherein the sidewall layer is connected to the sensitive material layer through the recessed portion;

[0028] forming a release hole in the sidewall layer connected to the sacrificial layer;

[0029] The sacrificial layer surrounded by the sidewall layer is removed through the release hole to form a cavity structure in the sidewall layer.

[0030] A third aspect of an embodiment of the present invention provides a semiconductor device, the semiconductor device comprising:

[0031] Semiconductor substrate;

[0032] A sensitive material layer formed on the semiconductor substrate, the sensitive material layer comprising a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface;

[0033] A recessed portion formed on the second surface of the sensitive material layer, wherein the recessed portion is used to define a boundary of a cavity structure;

[0034] A cavity structure and a sidewall layer surrounding the cavity structure are formed on the second surface of the sensitive material layer, wherein the sidewall layer is connected to the sensitive material layer through the recessed portion.

[0035] In some embodiments, the bottom of the recessed portion is arc-shaped or concave-convex.

[0036] In some embodiments, the sensitive material layer includes a sensitive material layer; the semiconductor device further includes: a first electrode formed on a first surface of the sensitive material layer, and a second electrode formed on a second surface of the sensitive material layer.

[0037] According to the semiconductor device manufacturing method and semiconductor device provided by the embodiment of the present invention, by setting a recessed portion at the connection between the sensitive material layer and the sidewall layer, the actual length of the interface layer is increased while ensuring that the volume of the cavity structure remains unchanged and the projected length of the interface layer remains unchanged, thereby increasing the difficulty of corrosion of the interface layer, thereby enhancing the overall structure of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] The following drawings of the present invention are used to understand the present invention as part of the present invention. The embodiments of the present invention are shown in the drawings and the description thereof is used to explain the principle of the present invention.

[0039] In the attached figure:

[0040] Figures 1A to 1C A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing each step according to an existing method for manufacturing a semiconductor device is shown;

[0041] Figure 2A schematic flow chart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention;

[0042] Figures 3A to 3G A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing various steps in a method for manufacturing a semiconductor device according to an embodiment of the present invention is shown;

[0043] Figure 4 A schematic flow chart showing a method for manufacturing a semiconductor device according to another specific embodiment of the present invention. DETAILED DESCRIPTION

[0044] In the following description, a large number of specific details are provided to provide a more thorough understanding of the present invention. However, it is apparent to those skilled in the art that the present invention can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present invention, some technical features well known in the art are not described.

[0045] It should be understood that the present invention can be implemented in different forms and should not be construed as being limited to the embodiments presented herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present invention to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.

[0046] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below can be represented as a second element, component, region, layer or part.

[0047] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.

[0048] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present invention. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0049] like Figure 1A-Figure 1C As shown, in the current manufacturing method of semiconductor devices, in order to obtain a cavity structure, it is first necessary to form a sacrificial layer 103 surrounded by a sidewall layer 102 on the sensitive material layer 101, wherein the sidewall layer 102 and the sacrificial layer 103 have a higher etching selectivity ratio; then, a wet or dry process is used to remove the sacrificial layer 103 through a release hole 104 formed in the sidewall layer 102, thereby forming a cavity structure 106 surrounded by the sidewall layer 102.

[0050] However, there is usually an interface layer 105 between the sensitive material layer 101 and the sidewall layer 102. The interface layer is generally formed by oxidation of the surface of the sensitive material layer 101 when the sidewall layer 102 is formed, and is relatively difficult to remove. When removing the sacrificial layer 103, the etching reaction gas or liquid will react with the interface layer 105, causing the interface layer 105 to be etched away, thereby causing the sensitive material layer 101 and the sidewall layer 102 connected by the interface layer 105 to crack, resulting in serious process problems and causing device failure.

[0051] The main reason why the interface layer 105 is corroded from the side during the process of releasing the sacrificial layer 103 is that the interface layer 105 and the sacrificial layer 103 are made of the same or similar materials, and the etchant used to remove the sacrificial layer 103 will also react with the interface layer 105. If an etchant that is not prone to damaging the interface layer 105 is used to remove the sacrificial layer 103, it will take a long time to release the sacrificial layer 103, resulting in high costs and limited mass production capacity.

[0052] In response to the above problems, Figure 2 As shown, the embodiment of the present invention provides a method 200 for manufacturing a semiconductor device, comprising the following steps:

[0053] Step S210: providing a semiconductor substrate;

[0054] Step S220: forming a sensitive material layer on the semiconductor substrate;

[0055] Step S230: forming a sacrificial layer on the sensitive material layer, wherein a groove penetrating the sacrificial layer is formed in the sacrificial layer, and the groove is used to define a boundary of a cavity structure;

[0056] Step S240: etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer;

[0057] Step S250: forming a sidewall layer filling the groove and covering the surface of the sacrificial layer;

[0058] Step S260: forming a release hole in the sidewall layer connected to the sacrificial layer;

[0059] Step S270: removing the sacrificial layer surrounded by the sidewall layer through the release hole to form a cavity structure in the sidewall layer.

[0060] The manufacturing method 200 of the semiconductor device in the embodiment of the present invention increases the actual length of the interface layer and makes it more difficult to corrode the interface layer, thereby enhancing the overall structure of the semiconductor device by setting a recessed portion at the connection position between the sensitive material layer and the sidewall layer, while ensuring that the volume of the cavity structure and the projection length of the interface layer remain unchanged.

[0061] In order to fully understand the present invention, detailed structures and steps will be presented in the following description to illustrate the technical solutions proposed by the present invention. The preferred embodiments of the present invention are described in detail below, but in addition to these detailed descriptions, the present invention may also have other implementations.

[0062] Combine the following Figure 3A to Figure 3G The implementation process of a method for manufacturing a semiconductor device according to an embodiment of the present invention is described exemplarily. Figure 3A to Figure 3GThe cross-sectional view of a semiconductor device obtained by sequentially performing various steps in a method for manufacturing a semiconductor device according to an embodiment of the present invention is shown.

[0063] First, step S210 is performed to provide a semiconductor substrate (not shown). The semiconductor substrate can be any suitable semiconductor substrate, such as a bulk silicon substrate, and can also be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or can also be double-sided polished silicon wafers (Double Side Polished Wafers, DSP), or can also be ceramic substrates such as alumina, quartz or glass substrates, etc.

[0064] Exemplarily, a first electrode (not shown) may also be formed on the semiconductor substrate. In one example, the method for forming the first electrode includes: depositing a first electrode material layer to cover the semiconductor substrate, then forming a patterned mask layer on the first electrode material layer, the mask layer defining a pattern of the first electrode, then etching the first electrode material layer using the patterned mask layer as a mask to form the first electrode, and finally removing the patterned mask layer.

[0065] In another example, a lift-off process may be used to form the first electrode, that is, a patterned mask layer is first formed on the surface of the semiconductor substrate, and then a first electrode material layer covering the patterned mask layer is formed. Finally, the patterned mask layer is lifted off and the first electrode material layer above it is removed to obtain the first electrode.

[0066] The material of the first electrode can be a conductive material or a semiconductor material, wherein the conductive material can be a metal material with conductive properties, and the metal material can be aluminum (Al), copper (Cu), gold (Au), platinum (Pt) and other metals or alloys of metals and copper, etc. The semiconductor material can be Si, Ge, SiGe, SiC, SiGeC and the like.

[0067] Then, if Figure 3AAs shown, step S220 is performed to form a sensitive material layer 301 on the semiconductor substrate. Among them, the semiconductor device of the embodiment of the present invention is a MEMS device, and the sensitive material layer 301 is used to realize the micro-electromechanical function of the MEMS device. Sensitive materials refer to materials that can sense slight changes in physical quantities, chemical quantities or biological quantities, and can show obvious characteristic changes according to the changes, specifically including thermosensitive materials, force-sensitive materials, photosensitive materials, voltage-sensitive materials, etc. In some embodiments, the sensitive material layer can be a piezoelectric layer. The piezoelectric layer will generate voltage when subjected to external pressure. On the contrary, if there is voltage on both sides of it, the piezoelectric layer will be slightly deformed. Based on the above characteristics of the piezoelectric layer, the mutual conversion between sound waves and electrical signals can be realized.

[0068] Exemplarily, a deposition method such as chemical vapor deposition, physical vapor deposition or atomic layer deposition can be used to deposit a piezoelectric material, and a metal element can be doped into the piezoelectric material to form a piezoelectric layer, and the doped metal element includes one or more of scandium, zirconium, calcium, titanium, magnesium, etc. Exemplarily, the material of the piezoelectric layer can specifically include aluminum nitride, lead zirconate titanate, zinc oxide, etc., and the embodiment of the present invention is not limited to this.

[0069] Continue to refer to Figure 3A After forming the sensitive material layer 301, a second electrode 302 may be formed on the sensitive material layer 301. When the sensitive material layer 301 is a piezoelectric layer, the first electrode, the piezoelectric layer, and the second electrode constitute a composite film, and the composite film may also include other film layers in addition to the above-mentioned film layers, which may be reasonably arranged according to the actual device, and is not specifically limited here.

[0070] In one example, the method for forming the second electrode 302 includes: depositing a second electrode material layer to cover the semiconductor substrate, the second electrode material layer may be a metal material layer or a semiconductor material layer. Then, forming a patterned mask layer on the second electrode material layer, the mask layer defining a pattern of the second electrode, and then etching the second electrode material layer using the patterned mask layer as a mask to form the second electrode 302, and finally, removing the patterned mask layer.

[0071] In another example, a lift-off process may be used to form the second electrode 302, that is, a patterned mask layer is first formed on the surface of the semiconductor substrate, and then a second electrode material layer covering the patterned mask layer is formed, and finally the patterned mask layer is lifted off and the second electrode material layer above it is removed to obtain a second electrode.

[0072] Next, step S230 is performed to form a sacrificial layer 303 on the sensitive material layer 301. A groove penetrating the sacrificial layer 303 is formed in the sacrificial layer 303, and the groove is used to define the boundary of the cavity structure. The sensitive material layer 301 includes a first surface in contact with the semiconductor substrate and a second surface arranged opposite to the first surface; the bottom of the groove in the sacrificial layer 303 exposes the first surface of the sensitive material layer 301.

[0073] For example, first Figure 3A As shown, a sacrificial layer 303 is deposited on the sensitive material layer 301, and the deposition process used includes chemical vapor deposition, physical vapor deposition, etc. Then, the sacrificial layer 303 is etched to form a groove exposing the first surface of the sensitive material layer 301. Specifically, a patterned photoresist layer is formed on the sacrificial layer 303, and a window defining the position of the groove is provided in the photoresist layer. Afterwards, the sacrificial layer 303 is dry-etched using the photoresist layer as a mask to form a groove penetrating the sacrificial layer 303. The etching of the sacrificial layer 303 stops at the surface of the sensitive material layer 301. After the etching of the sacrificial layer 303 is completed, the photoresist layer can be removed by a process such as photoresist ashing.

[0074] Next, execute step S240, such as Figure 3C As shown, the sensitive material layer 301 exposed at the bottom of the groove is etched to form a recessed portion on the surface of the sensitive material layer 301. The recessed portion extends downward in a direction perpendicular to the surface of the sensitive material layer 301. Before the recessed portion is formed, the actual length of the sensitive material layer 301 exposed at the bottom of the groove is consistent with the width of the groove; after the recessed portion is formed, the projected length of the sensitive material layer 301 exposed at the bottom of the groove is still consistent with the width of the groove, but the actual length of the sensitive material layer 301 is greater than the projected length, thereby increasing the actual length of the interface layer subsequently formed on the surface of the sensitive material layer 301.

[0075] In one embodiment, Figure 3C As shown, the bottom of the recessed portion is in an arc shape. When the bottom of the recessed portion is in an arc shape, an isotropic etching process can be used to etch the sensitive material layer 301 exposed at the bottom of the groove to form a recessed portion with an arc bottom. Compared with a flat bottom, the actual length of the arc-shaped bottom is greater, thereby increasing the actual length of the interface layer formed subsequently.

[0076] In another embodiment, the bottom of the recessed portion is concave-convex. The concave-convex shape includes a convex portion and a concave portion, and the convex portion and the concave portion can be rectangular, triangular, trapezoidal, etc. Figure 3F and Figure 3G As shown, Figure 3F The concave part of the triangle is shown, Figure 3G A rectangular concave-convex concave portion is shown. The concave-convex bottom further increases the actual length of the bottom of the concave portion.

[0077] When the bottom of the recessed portion is concave-convex, the sensitive material layer exposed at the bottom of the groove is etched to form a recessed portion on the surface of the sensitive material layer, including: forming photoresist layers of different thicknesses at the bottom of the groove; etching the sensitive material layer 301 exposed at the bottom of the groove based on the photoresist layers of different thicknesses to form a recessed portion with a concave-convex bottom.

[0078] Among them, photoresist layers of different thicknesses can be formed by grayscale lithography, that is, when using a photoresist plate to expose the photoresist, the photoresist plate used is a grayscale photoresist plate, and the transmittance of each position of the grayscale photoresist plate is different; after the exposure and development based on the grayscale photoresist plate are completed, the photoresist pattern formed also has corresponding different thicknesses.

[0079] Specifically, the main components of the photoresist layer are resin and photosensitizer. The resin has adhesive properties. For positive photoresist, the resin is relatively insoluble before exposure. After exposure, a chemical reaction occurs, and the resin changes from insoluble to soluble. The photosensitizer acts as a dissolution inhibitor before exposure to reduce the dissolution rate of the resin, and acts as a dissolution enhancer after exposure to improve the solubility of the photoresist in the developer. After the photoresist layer is formed, the photoresist layer is exposed using a grayscale photomask, and the developer is used for development. For positive photoresist, the properties of the photoresist layer that has undergone exposure treatment change and is easily soluble in the developer, while the photoresist layer that has not undergone exposure treatment will not dissolve in the developer. Since the transmittance of each position of the grayscale photomask is different, the photoresist layer corresponding to the part with high transmittance after exposure is easier to remove, and the photoresist layer corresponding to the part with low transmittance is relatively difficult to remove. Therefore, after immersion in the developer, photoresist layers of different thicknesses are formed.

[0080] Next, when the sensitive material layer 301 at the bottom of the groove is etched using photoresist layers of different thicknesses as masks, the etching amount of the sensitive material layer 301 under the photoresist layer with a larger thickness is smaller, and the etching amount of the sensitive material layer 301 under the photoresist layer with a smaller thickness is larger, thereby forming a recessed portion with a concave-convex bottom in the sensitive material layer 301.

[0081] It should be noted that the bottom of the recessed portion of the embodiment of the present invention is not limited to an arc shape or a concave-convex shape, and a recessed portion of other shapes can be formed as needed. Compared with a flat bottom, a recessed portion of any shape can increase the actual length of the groove bottom.

[0082] Next, execute step S250, such as Figure 3DAs shown, a sidewall layer 304 is formed to fill the groove in the sacrificial layer and cover the surface of the sacrificial layer. That is, the sidewall layer 304 includes a portion formed in the groove and a portion covering the surface of the sacrificial layer 303. The sidewall layer 304 can be deposited by a deposition method such as chemical vapor deposition, physical vapor deposition or atomic layer deposition. There is a high etching selectivity between the sidewall layer 304 and the sacrificial layer 303, so that the sidewall layer 304 is not affected during the process of removing the sacrificial layer 303. For example, if the material of the sacrificial layer 303 is SiO2, polysilicon can be used as the material of the sidewall layer 304.

[0083] In the process of forming the sidewall layer 304, the first surface of the sensitive material layer 301 exposed at the bottom of the groove in the sacrificial layer 303 is oxidized, thereby forming an interface layer 305 between the sensitive material layer 301 and the sidewall layer 304. Since the embodiment of the present invention forms a recessed portion at the bottom of the groove before forming the sidewall layer 304, the actual length of the bottom of the groove is increased, and thus the actual length of the interface layer is increased, thereby increasing the difficulty of the interface layer 305 being corroded from the side, reducing the degree of the side corrosion of the interface layer 305, and increasing the connection stability between the sensitive material layer 301 and the sidewall layer 304.

[0084] Next, continue to refer to Figure 3D , executing step S260, forming a release hole 306 in the sidewall layer 304 connected to the sacrificial layer 303, and referring to Figure 3E , the sacrificial layer 303 surrounded by the sidewall layer 304 is removed through the release hole 306 to form a cavity structure in the sidewall layer 304. The release hole 306 is formed above the sacrificial layer 303, thereby exposing the top of the sacrificial layer 303. The etchant can contact the sacrificial layer 303 through the release hole 306, thereby etching away the sacrificial layer surrounded by the sidewall layer 304, forming a cavity structure surrounded by the sidewall layer 304. The sidewall and top of the cavity structure are the sidewall layer 304, and the bottom is the sensitive material layer 301.

[0085] Since the embodiment of the present invention forms a recessed portion between the sensitive material layer 301 and the sidewall layer 304, the interface layer grows along the recessed portion. In the process of etching gas or liquid corroding the interface layer from the inside to the outside, due to the influence of gravity, diffusion and other factors, the corrosion speed slows down, thereby alleviating the impact of the interface layer on the side corrosion. In addition, when the projection length of the interface layer remains unchanged, the actual length of the interface layer increases, which will also reduce the proportion of the projection length of the corroded interface layer in the overall projection length, thereby reducing the impact of the side corrosion on the overall structure.

[0086] At this point, the process steps implemented in the method for manufacturing a semiconductor device according to an embodiment of the present invention have been completed. It can be understood that the method for manufacturing a semiconductor device according to the embodiment of the present invention not only includes the above steps, but may also include other necessary steps before, during or after the above steps, which are all included in the scope of the manufacturing method according to the embodiment of the present invention.

[0087] According to the manufacturing method of the semiconductor device provided by the present invention, a recessed portion is formed at the connection between the sensitive material layer and the sidewall layer, which increases the actual length of the interface layer while ensuring that the volume of the cavity structure remains unchanged and the projected length of the interface layer remains unchanged, thereby increasing the difficulty of corrosion of the interface layer, thereby enhancing the overall structure of the semiconductor device.

[0088] Another aspect of the present invention provides a method for manufacturing a semiconductor device, such as Figure 4 As shown, the method 400 for manufacturing a semiconductor device includes the following steps:

[0089] In step S410, a semiconductor substrate is provided;

[0090] In step S420, a sensitive material layer is formed on the semiconductor substrate;

[0091] In step S430, the sensitive material layer is etched to form a recessed portion on the surface of the sensitive material layer, wherein the recessed portion is used to define a boundary of the cavity structure;

[0092] In step S440, a sacrificial layer and a sidewall layer surrounding the sacrificial layer are formed on the sensitive material layer, wherein the sidewall layer is connected to the sensitive material layer through the recessed portion;

[0093] In step S450, a release hole connected to the sacrificial layer is formed in the sidewall layer;

[0094] In step S460 , the sacrificial layer surrounded by the sidewall layer is removed through the release hole to form a cavity structure in the sidewall layer.

[0095] In the manufacturing method 400 of the semiconductor device of the present embodiment, the recessed portion may be formed before the sacrificial layer, and the sacrificial layer may be formed after the sidewall layer. Specifically, a recessed portion defining the boundary of the cavity structure may be formed in the sensitive material layer first, and then a first sidewall layer covering the sensitive material layer may be formed, an interface layer is formed between the first sidewall layer and the sensitive material layer, and the interface layer at the recessed portion is consistent with the shape of the bottom of the recessed portion; then, the first sidewall layer is etched to form a groove for forming the sacrificial layer, and the sacrificial layer is filled in the groove; after filling the sacrificial layer, the sacrificial layer on the top of the first sidewall layer may be removed by a chemical mechanical polishing process, and a second sidewall layer may be formed on the top of the first sidewall layer and the sacrificial layer, so that the first sidewall layer and the second sidewall layer surround the sacrificial layer. Finally, a release hole is formed in the second sidewall layer, and the sacrificial layer is removed through the release hole to form a cavity structure. More specific details of the manufacturing method 400 of the semiconductor device of the present embodiment can refer to the relevant description of the manufacturing method 200 of the semiconductor device, and will not be repeated here.

[0096] like Figure 3E , Figure 3F and Figure 3G As shown, an embodiment of the present invention further provides a semiconductor device, which can be manufactured by the manufacturing method of the semiconductor device as described above. Specifically, the semiconductor device of the embodiment of the present invention includes: a semiconductor substrate (not shown); a sensitive material layer 301 formed on the semiconductor substrate, the sensitive material layer 301 including a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface; a recessed portion formed on the second surface of the sensitive material layer 301, the recessed portion is used to define the boundary of the cavity structure; a cavity structure formed on the second surface of the sensitive material layer 301 and a sidewall layer 304 surrounding the cavity structure, wherein the sidewall layer 304 is connected to the sensitive material layer 301 through the recessed portion. An interface layer is also formed between the sidewall layer 304 and the sensitive material layer 301.

[0097] The bottom of the recessed portion is arc-shaped or concave-convex. The arc-shaped or concave-convex recessed portion increases the actual length of the interface layer between the sidewall layer 304 and the sensitive material layer 301, reduces the corrosion of the interface layer during the process of removing the sacrificial layer to form the cavity structure, thereby increasing the overall stability of the semiconductor device.

[0098] In some embodiments, the sensitive material layer 301 may be a sensitive material layer; the semiconductor device further includes a first electrode (not shown) formed on a first surface of the sensitive material layer, and a second electrode 302 formed on a second surface of the sensitive material layer. The first electrode, the sensitive material layer, and the second electrode constitute a composite film. The composite film may also include other film layers in addition to the above-mentioned film layers, which may be reasonably arranged according to the actual device, and is not specifically limited here.

[0099] The semiconductor device of the embodiment of the present invention has a recessed portion at the connection between the sidewall layer and the sensitive material layer, which can increase the actual length of the interface layer between the sidewall layer and the sensitive material layer, reduce the corrosion of the interface layer during the process of removing the sacrificial layer to form a cavity structure, and thus increase the overall stability of the semiconductor device.

[0100] The present invention has been described by the above embodiments, but it should be understood that the above embodiments are only for the purpose of example and description, and are not intended to limit the present invention to the scope of the described embodiments. In addition, it can be understood by those skilled in the art that the present invention is not limited to the above embodiments, and more variations and modifications can be made according to the teachings of the present invention, and these variations and modifications all fall within the scope of the protection claimed by the present invention. The protection scope of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for manufacturing a semiconductor device, It is characterized in that The method comprises: providing a semiconductor substrate; forming a sensitive material layer on the semiconductor substrate; forming a sacrificial layer on the sensitive material layer, wherein a groove penetrating the sacrificial layer is formed in the sacrificial layer, and the groove is used to define a boundary of a cavity structure; Etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer; forming a sidewall layer filling the groove and covering the surface of the sacrificial layer; forming a release hole in the sidewall layer connected to the sacrificial layer; The sacrificial layer surrounded by the sidewall layer is removed through the release hole to form a cavity structure in the sidewall layer.

2. The manufacturing method according to claim 1, It is characterized in that The bottom of the recessed portion is in an arc shape.

3. The manufacturing method according to claim 2, It is characterized in that When the bottom of the recessed portion is in an arc shape, etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer includes: The sensitive material layer exposed at the bottom of the groove is etched using an isotropic etching process to form the concave portion with an arc-shaped bottom.

4. The manufacturing method according to claim 1, It is characterized in that The bottom of the recessed portion is concave-convex.

5. The manufacturing method according to claim 4, It is characterized in that When the bottom of the recessed portion is concave-convex, etching the sensitive material layer exposed at the bottom of the groove to form a recessed portion on the surface of the sensitive material layer includes: forming photoresist layers of different thicknesses at the bottom of the groove; The sensitive material layer exposed at the bottom of the groove is etched based on the photoresist layers with different thicknesses to form the concave portion with a concave-convex bottom.

6. The manufacturing method according to any one of claims 1 to 5, It is characterized in that The sensitive material layer includes a piezoelectric layer; Before forming the sensitive material layer on the semiconductor substrate, the method further includes: forming a first electrode on the semiconductor substrate; Before forming a sensitive material layer on the semiconductor substrate and after forming a sacrificial layer on the sensitive material layer, the method further includes: forming a second electrode on the sensitive material layer.

7. A method for manufacturing a semiconductor device, It is characterized in that The method comprises: providing a semiconductor substrate; forming a sensitive material layer on the semiconductor substrate; Etching the sensitive material layer to form a recessed portion on the surface of the sensitive material layer, wherein the recessed portion is used to define a boundary of the cavity structure; forming a sacrificial layer and a sidewall layer surrounding the sacrificial layer on the sensitive material layer, wherein the sidewall layer is connected to the sensitive material layer through the recessed portion; forming a release hole in the sidewall layer connected to the sacrificial layer; The sacrificial layer surrounded by the sidewall layer is removed through the release hole to form a cavity structure in the sidewall layer.

8. A semiconductor device, It is characterized in that The semiconductor device comprises: Semiconductor substrate; A sensitive material layer formed on the semiconductor substrate, the sensitive material layer comprising a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface; A recessed portion formed on the second surface of the sensitive material layer, wherein the recessed portion is used to define a boundary of a cavity structure; A cavity structure and a sidewall layer surrounding the cavity structure are formed on the second surface of the sensitive material layer, wherein the sidewall layer is connected to the sensitive material layer through the recessed portion.

9. The semiconductor device according to claim 8, It is characterized in that The bottom of the recessed portion is arc-shaped or concave-convex.

10. The semiconductor device according to claim 8, It is characterized in that The sensitive material layer includes a sensitive material layer; the semiconductor device further includes: a first electrode formed on a first surface of the sensitive material layer, and a second electrode formed on a second surface of the sensitive material layer.