Semiconductor device and manufacturing method thereof
By forming a narrow upper and wide upper edge wall layer on the sensitive material layer of the MEMS device, the problem of interface layer corrosion is solved, and the stability and structural integrity of the semiconductor device are improved.
Patent Information
- Application Number
- CN202310538233.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-12
- Publication Date
- 2024-11-12
AI Technical Summary
When removing the sacrificial layer by existing MEMS devices, etching reaction gas or liquid will corrode the interface layer, causing cracks between the functional layer and the side wall layer, resulting in serious process problems, affecting the effectiveness of the device.
By forming a narrow upper and wide upper edge wall layer on the sensitive material layer, the actual length of the interface layer is increased, and the difficulty of the interface layer being corroded is reduced, thereby enhancing the overall structure of the semiconductor device.
Effectively slows down the corrosion rate of the interface layer, improves the stability and structural integrity of semiconductor devices, and avoids device failure.
Smart Images

Figure CN118929562A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor device and a method for manufacturing the same. Background Art
[0002] MEMS (Micro-Electro-Mechanical System) refers to a micro system that integrates mechanical components, drive components, optical systems, and electronic control systems into a whole. MEMS devices have advantages such as small size and low power consumption, and have a wide range of application scenarios in smart phones, tablets, game consoles, automobiles, drones, and other fields. Similar to integrated circuits, MEMS devices are also developing in the direction of high performance, miniaturization, low cost, and integration.
[0003] The cavity structure of existing MEMS devices is formed by removing the sacrificial layer between the MEMS functional layer and the sidewall layer through the release hole using a wet or dry etching process. However, there is usually an interface layer between the MEMS functional layer and the sidewall layer. When removing the sacrificial layer, the etching reaction gas or liquid will corrode the interface layer, causing cracks in the MEMS functional layer and the sidewall layer, resulting in serious process problems and causing device failure. Summary of the invention
[0004] A series of simplified concepts are introduced in the Summary of the Invention, which will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0005] In view of the existing problems, an embodiment of the present invention provides a method for manufacturing a semiconductor device, the method comprising:
[0006] providing a semiconductor substrate;
[0007] forming a sensitive material layer on the semiconductor substrate;
[0008] forming a first sacrificial layer and a first sidewall layer surrounding the first sacrificial layer on the sensitive material layer, wherein the first sidewall layer has a first width;
[0009] forming a second sacrificial layer and a second sidewall layer surrounding the second sacrificial layer above the first sacrificial layer and the first sidewall layer, wherein the second sidewall layer is connected to the first sidewall layer and has a second width that is smaller than the first width;
[0010] forming a release hole in the second sidewall layer connected to the second sacrificial layer;
[0011] The first sacrificial layer and the second sacrificial layer are removed through the release hole to form a cavity structure in the first sidewall layer and the second sidewall layer.
[0012] In some embodiments, forming a first sacrificial layer and a first sidewall layer surrounding the first sacrificial layer on the sensitive material layer includes:
[0013] forming a first sacrificial layer on the sensitive material layer, wherein a first groove penetrating the first sacrificial layer is formed in the first sacrificial layer, the first groove is used to define a boundary of the cavity structure, and the first groove has the first width;
[0014] forming a first sidewall layer filling the first trench and covering the first sacrificial layer;
[0015] The first sidewall layer above the first sacrificial layer is removed to obtain a first sidewall layer surrounding the first sacrificial layer.
[0016] In some embodiments, forming a second sacrificial layer on the first sacrificial layer and around the first sidewall layer and a second sidewall layer surrounding the second sacrificial layer includes:
[0017] forming a second sacrificial layer covering the first sacrificial layer and the first sidewall layer, wherein a second trench connected to the first sidewall layer is formed in the second sacrificial layer, and the second trench has the second width;
[0018] A second sidewall layer is formed to fill the second trench and cover the second sacrificial layer.
[0019] In some embodiments, before forming the first sidewall layer, the method further includes:
[0020] The sensitive material layer exposed at the bottom of the first groove is etched to form a recessed portion on the surface of the sensitive material layer.
[0021] In some embodiments, the bottom of the recessed portion is arc-shaped, and the etching of the sensitive material layer exposed at the bottom of the first groove to form a recessed portion on the surface of the sensitive material layer includes:
[0022] The sensitive material layer exposed at the bottom of the first groove is etched using an isotropic etching process to form the recessed portion with an arc-shaped bottom.
[0023] In some embodiments, the bottom of the recessed portion is concave-convex, and etching the sensitive material layer exposed at the bottom of the first groove to form a recessed portion on the surface of the sensitive material layer includes:
[0024] forming a photoresist layer with different thicknesses at the bottom of the first trench;
[0025] The sensitive material layer exposed at the bottom of the first trench is etched based on the photoresist layers with different thicknesses to form the concave portion with a concave-convex bottom.
[0026] In some embodiments, the first sacrificial layer and the first sidewall layer have a first thickness, the second sacrificial layer and the second sidewall layer have a second thickness, and the first thickness is less than the second thickness.
[0027] In some embodiments, the sensitive material layer includes a piezoelectric layer;
[0028] Before forming the sensitive material layer on the semiconductor substrate, the method further includes: forming a first electrode on the semiconductor substrate;
[0029] Before forming a sensitive material layer on the semiconductor substrate and after forming a sacrificial layer on the sensitive material layer, the method further includes: forming a second electrode on the sensitive material layer.
[0030] Another aspect of an embodiment of the present invention provides a semiconductor device, the semiconductor device comprising:
[0031] Semiconductor substrate;
[0032] A sensitive material layer formed on the semiconductor substrate, the sensitive material layer comprising a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface;
[0033] A first sidewall layer is formed on the second surface of the sensitive material layer, the first sidewall layer has a first width, and an interface layer is formed between the first sidewall layer and the sensitive material layer;
[0034] A second sidewall layer is formed above the first sidewall layer, the second sidewall layer is connected to the first sidewall layer, the second sidewall layer has a second width, and the second width is smaller than the first width;
[0035] A cavity structure is formed in the first sidewall layer and the second sidewall layer.
[0036] In some embodiments, the semiconductor device further includes: a recessed portion formed on the second surface of the sensitive material layer, and the first sidewall layer is connected to the sensitive material layer through the recessed portion.
[0037] According to the semiconductor device manufacturing method and semiconductor device provided by the embodiment of the present invention, the actual length of the interface layer is increased by forming a sidewall layer that is narrow at the top and wide at the bottom, which increases the difficulty of the interface layer being corroded, thereby enhancing the overall structure of the semiconductor device. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] The following drawings of the present invention are used to understand the present invention as part of the present invention. The embodiments of the present invention are shown in the drawings and the description thereof is used to explain the principle of the present invention.
[0039] In the attached figure:
[0040] Figures 1A to 1C A cross-sectional schematic diagram of a semiconductor device obtained by sequentially implementing each step according to an existing method for manufacturing a semiconductor device is shown;
[0041] Figure 2 A schematic flow chart showing a method for manufacturing a semiconductor device according to a specific embodiment of the present invention;
[0042] FIG. 3A to FIG. 3I The cross-sectional view of a semiconductor device obtained by sequentially performing various steps in a method for manufacturing a semiconductor device according to an embodiment of the present invention is shown. DETAILED DESCRIPTION
[0043] In the following description, a large number of specific details are provided to provide a more thorough understanding of the present invention. However, it is apparent to those skilled in the art that the present invention can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present invention, some technical features well known in the art are not described.
[0044] It should be understood that the present invention can be implemented in different forms and should not be construed as being limited to the embodiments presented herein. On the contrary, providing these embodiments will make the disclosure thorough and complete and fully convey the scope of the present invention to those skilled in the art. In the accompanying drawings, the sizes and relative sizes of layers and regions may be exaggerated for clarity. The same reference numerals throughout represent the same elements.
[0045] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer or part discussed below can be represented as a second element, component, region, layer or part.
[0046] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.
[0047] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present invention. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.
[0048] like Figure 1A-Figure 1CAs shown, in the current manufacturing method of MEMS devices, in order to obtain a cavity structure, it is first necessary to form a sacrificial layer 103 surrounded by a sidewall layer 102 on the sensitive material layer 101, wherein the sidewall layer 102 and the sacrificial layer 103 have a higher etching selectivity ratio; then, a wet or dry process is used to remove the sacrificial layer 103 through a release hole 104 formed in the sidewall layer 102, thereby forming a cavity structure 106 surrounded by the sidewall layer 102.
[0049] However, there is usually an interface layer 105 between the sensitive material layer 101 and the sidewall layer 102. The interface layer is generally formed by oxidation of the surface of the sensitive material layer 101 when the sidewall layer 102 is formed, and is relatively difficult to remove. When removing the sacrificial layer 103, the etching reaction gas or liquid will react with the interface layer 105, causing the interface layer 105 to be etched away, thereby causing the sensitive material layer 101 and the sidewall layer 102 connected by the interface layer 105 to crack, resulting in serious process problems and causing device failure.
[0050] The main reason why the interface layer 105 is corroded from the side during the process of releasing the sacrificial layer 103 is that the interface layer 105 and the sacrificial layer 103 are made of the same or similar materials, and the etchant used to remove the sacrificial layer 103 will also react with the interface layer 105. If an etchant that is not prone to damaging the interface layer 105 is used to remove the sacrificial layer 103, it will take a long time to release the sacrificial layer 103, resulting in high costs and limited mass production capacity.
[0051] In response to the above problems, Figure 2 As shown, the embodiment of the present invention provides a method 200 for manufacturing a semiconductor device, comprising the following steps:
[0052] Step S210: providing a semiconductor substrate;
[0053] Step S220: forming a sensitive material layer on the semiconductor substrate;
[0054] Step S230: forming a first sacrificial layer and a first sidewall layer surrounding the first sacrificial layer on the sensitive material layer, wherein the first sidewall layer has a first width;
[0055] Step S240: forming a second sacrificial layer and a second sidewall layer surrounding the second sacrificial layer above the first sacrificial layer and the first sidewall layer, wherein the second sidewall layer is connected to the first sidewall layer, and the second sidewall layer has a second width, and the second width is smaller than the first width;
[0056] Step S250: forming a release hole in the second sidewall layer connected to the second sacrificial layer;
[0057] Step S260: removing the first sacrificial layer and the second sacrificial layer through the release hole to form a cavity structure in the first sidewall layer and the second sidewall layer.
[0058] The semiconductor device manufacturing method 200 of the embodiment of the present invention increases the actual length of the interface layer by forming a sidewall layer that is narrow at the top and wide at the bottom while ensuring that the size of the cavity structure remains basically unchanged, thereby increasing the difficulty of corrosion of the interface layer and enhancing the overall structure of the semiconductor device.
[0059] In order to fully understand the present invention, detailed structures and steps will be presented in the following description to illustrate the technical solutions proposed by the present invention. The preferred embodiments of the present invention are described in detail below, but in addition to these detailed descriptions, the present invention may also have other implementations.
[0060] Combine the following Figure 3A to Figure 3I The implementation process of a method for manufacturing a semiconductor device according to an embodiment of the present invention is described exemplarily. Figure 3A to Figure 3I The cross-sectional view of a semiconductor device obtained by sequentially performing various steps in a method for manufacturing a semiconductor device according to an embodiment of the present invention is shown.
[0061] First, step S210 is performed to provide a semiconductor substrate (not shown). The semiconductor substrate can be any suitable semiconductor substrate, such as a bulk silicon substrate, and can also be at least one of the following materials: Si, Ge, SiGe, SiC, SiGeC, InAs, GaAs, InP or other III / V compound semiconductors, including multilayer structures composed of these semiconductors, or silicon on insulator (SOI), stacked silicon on insulator (SSOI), stacked silicon germanium on insulator (S-SiGeOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or can also be double-sided polished silicon wafers (Double Side Polished Wafers, DSP), or can also be ceramic substrates such as alumina, quartz or glass substrates, etc.
[0062] Exemplarily, a first electrode (not shown) may also be formed on the semiconductor substrate. In one example, the method for forming the first electrode includes: depositing a first electrode material layer to cover the semiconductor substrate, then forming a patterned mask layer on the first electrode material layer, the mask layer defining a pattern of the first electrode, then etching the first electrode material layer using the patterned mask layer as a mask to form the first electrode, and finally removing the patterned mask layer.
[0063] In another example, a lift-off process may be used to form the first electrode, that is, a patterned mask layer is first formed on the surface of the semiconductor substrate, and then a first electrode material layer covering the patterned mask layer is formed. Finally, the patterned mask layer is lifted off and the first electrode material layer above it is removed to obtain the first electrode.
[0064] The material of the first electrode can be a conductive material or a semiconductor material, wherein the conductive material can be a metal material with conductive properties, and the metal material can be aluminum (Al), copper (Cu), gold (Au), platinum (Pt) and other metals or alloys of metals and copper, etc. The semiconductor material can be Si, Ge, SiGe, SiC, SiGeC and the like.
[0065] Then, if Figure 3A As shown, step S220 is performed to form a sensitive material layer 301 on the semiconductor substrate. The semiconductor device of the embodiment of the present invention is a MEMS device, and the sensitive material layer 301 is used to realize the micro-electromechanical function of the MEMS device. The sensitive material refers to a material that can sense slight changes in physical quantities, chemical quantities or biological quantities, and can show obvious characteristic changes according to the changes, specifically including thermosensitive materials, force-sensitive materials, photosensitive materials, voltage-sensitive materials, etc. In some embodiments, the sensitive material layer can be a piezoelectric layer, which will generate voltage when subjected to external pressure. On the contrary, if there is voltage on both sides of the piezoelectric layer, the piezoelectric layer will be slightly deformed. Based on the above characteristics of the piezoelectric layer, the mutual conversion between sound waves and electrical signals can be realized.
[0066] Exemplarily, a deposition method such as chemical vapor deposition, physical vapor deposition or atomic layer deposition can be used to deposit a piezoelectric material, and a metal element can be doped into the piezoelectric material to form a piezoelectric layer, and the doped metal element includes one or more of scandium, zirconium, calcium, titanium, magnesium, etc. Exemplarily, the material of the piezoelectric layer can specifically include aluminum nitride, lead zirconate titanate, zinc oxide, etc., and the embodiment of the present invention is not limited to this.
[0067] Continue to refer to Figure 3A After forming the sensitive material layer 301, a second electrode 302 may be formed on the sensitive material layer 301. When the sensitive material layer 301 is a piezoelectric layer, the first electrode, the piezoelectric layer, and the second electrode constitute a composite film, and the composite film may also include other film layers in addition to the above-mentioned film layers, which may be reasonably arranged according to the actual device, and is not specifically limited here.
[0068] In one example, the method for forming the second electrode 302 includes: depositing a second electrode material layer to cover the semiconductor substrate, the second electrode material layer may be a metal material layer or a semiconductor material layer. Then, forming a patterned mask layer on the second electrode material layer, the mask layer defining a pattern of the second electrode, and then etching the second electrode material layer using the patterned mask layer as a mask to form the second electrode 302, and finally, removing the patterned mask layer.
[0069] In another example, a lift-off process may be used to form the second electrode 302, that is, a patterned mask layer is first formed on the surface of the semiconductor substrate, and then a second electrode material layer covering the patterned mask layer is formed, and finally the patterned mask layer is lifted off and the second electrode material layer above it is removed to obtain a second electrode.
[0070] Next, step S230 is performed to form a first sacrificial layer 303A and a first sidewall layer 304A surrounding the first sacrificial layer 303A on the sensitive material layer 301. The first sidewall layer 304A has a first width. The first sidewall layer 304A surrounds the first sacrificial layer 303A, that is, the first sidewall layer 304A does not need to cover the first sacrificial layer 303A.
[0071] For example, first Figure 3A As shown, a first sacrificial layer 303A is formed on the sensitive material layer 301, and a first groove penetrating the first sacrificial layer 303A is formed in the first sacrificial layer 303A, and the first groove is used to define the boundary of the bottom of the cavity structure. The sensitive material layer 301 includes a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface; the bottom of the first groove in the first sacrificial layer 303 exposes the first surface of the sensitive material layer 301.
[0072] For example, first Figure 3A As shown, a first sacrificial layer 303A is deposited on the sensitive material layer 301, and the deposition process used includes chemical vapor deposition, physical vapor deposition, etc. Figure 3B As shown, the first sacrificial layer 303A is etched to form a groove exposing the first surface of the sensitive material layer 301. Specifically, a patterned photoresist layer is formed on the first sacrificial layer 303A, and a window defining the position of the first groove is provided in the photoresist layer. Afterwards, the first sacrificial layer 303A is dry-etched using the photoresist layer as a mask to form a groove penetrating the first sacrificial layer 303A. The etching of the first sacrificial layer 303A stops at the surface of the sensitive material layer 301. After the etching of the first sacrificial layer 303A is completed, the photoresist layer can be removed by a process such as photoresist ashing.
[0073] In some embodiments, after forming the first groove, the sensitive material layer 301 exposed at the bottom of the first groove is etched to form a recessed portion on the surface of the sensitive material layer 301. The recessed portion extends downward in a direction perpendicular to the surface of the sensitive material layer 301. Before forming the recessed portion, the actual length of the sensitive material layer 301 exposed at the bottom of the first groove is consistent with the width of the first groove; after forming the recessed portion, the projected length of the sensitive material layer 301 exposed at the bottom of the first groove is still consistent with the width of the first groove, but its actual length is greater than the projected length, thereby increasing the actual length of the interface layer subsequently formed on the surface of the sensitive material layer 301.
[0074] In one embodiment, Figure 3H As shown, the bottom of the recessed portion is in an arc shape. When the bottom of the recessed portion is in an arc shape, the sensitive material layer 301 exposed at the bottom of the first groove can be etched by an isotropic etching process to form a recessed portion with an arc-shaped bottom. Compared with a planar bottom, the actual length of the arc-shaped bottom is greater, thereby increasing the actual length of the interface layer formed subsequently.
[0075] In another embodiment, the bottom of the recessed portion is concave-convex. The concave-convex shape includes a convex portion and a concave portion, and the convex portion and the concave portion can be rectangular, triangular, trapezoidal, etc. Fig. 3I As shown, a rectangular concave-convex concave portion is shown. The concave-convex bottom further increases the actual length of the bottom of the concave portion.
[0076] When the bottom of the recessed portion is concave-convex, the sensitive material layer exposed at the bottom of the first groove is etched to form a recessed portion on the surface of the sensitive material layer, including: forming photoresist layers of different thicknesses at the bottom of the first groove; etching the sensitive material layer 301 exposed at the bottom of the first groove based on the photoresist layers of different thicknesses to form a recessed portion with a concave-convex bottom.
[0077] Among them, photoresist layers of different thicknesses can be formed by grayscale lithography, that is, when using a photoresist plate to expose the photoresist, the photoresist plate used is a grayscale photoresist plate, and the transmittance of each position of the grayscale photoresist plate is different; after the exposure and development based on the grayscale photoresist plate are completed, the photoresist pattern formed also has corresponding different thicknesses.
[0078] Specifically, the main components of the photoresist layer are resin and photosensitizer. The resin has adhesive properties. For positive photoresist, the resin is relatively insoluble before exposure. After exposure, a chemical reaction occurs, and the resin changes from insoluble to soluble. The photosensitizer acts as a dissolution inhibitor before exposure to reduce the dissolution rate of the resin, and acts as a dissolution enhancer after exposure to improve the solubility of the photoresist in the developer. After the photoresist layer is formed, the photoresist layer is exposed using a grayscale photomask, and the developer is used for development. For positive photoresist, the properties of the photoresist layer that has undergone exposure treatment change and is easily soluble in the developer, while the photoresist layer that has not undergone exposure treatment will not dissolve in the developer. Since the transmittance of each position of the grayscale photomask is different, the photoresist layer corresponding to the part with high transmittance after exposure is easier to remove, and the photoresist layer corresponding to the part with low transmittance is relatively difficult to remove. Therefore, after immersion in the developer, photoresist layers of different thicknesses are formed.
[0079] Next, when the sensitive material layer 301 at the bottom of the first groove is etched using photoresist layers of different thicknesses as masks, the etching amount of the sensitive material layer 301 under the photoresist layer with a larger thickness is smaller, and the etching amount of the sensitive material layer 301 under the photoresist layer with a smaller thickness is larger, thereby forming a recessed portion with a concave-convex bottom in the sensitive material layer 301.
[0080] It should be noted that the bottom of the recessed portion of the embodiment of the present invention is not limited to an arc shape or a concave-convex shape, and a recessed portion of other shapes can be formed as needed. Compared with a flat bottom, a recessed portion of any shape can increase the actual length of the bottom of the first groove.
[0081] Then, if Figure 3C As shown, a first sidewall layer 304A is formed to fill the first groove in the first sacrificial layer and cover the surface of the first sacrificial layer. That is, the first sidewall layer 304A includes a portion formed in the first groove and a portion covering the surface of the first sacrificial layer 303A. The first sidewall layer 304A can be deposited by a deposition method such as chemical vapor deposition, physical vapor deposition or atomic layer deposition. There is a high etching selectivity between the first sidewall layer 304A and the first sacrificial layer 303A, so that the first sidewall layer 304A is not affected during the process of removing the first sacrificial layer 303A. For example, if the material of the first sacrificial layer 303A is SiO2, polysilicon can be used as the material of the first sidewall layer 304A.
[0082] In the process of forming the first sidewall layer 304A, the first surface of the sensitive material layer 301 exposed at the bottom of the groove in the first sacrificial layer 303A is oxidized, thereby forming an interface layer 305 between the sensitive material layer 301 and the first sidewall layer 304A. Since the width of the first groove is increased in the embodiment of the present invention, the length of the interface layer 305 is also increased, thereby increasing the difficulty of the interface layer 305 being corroded from the side, reducing the degree of the interface layer 305 being corroded from the side, and increasing the connection stability between the sensitive material layer 301 and the first sidewall layer 304A. When a recessed portion is formed at the bottom of the first groove, the interface layer 305 grows along the bottom of the recessed portion, which can further increase the actual length of the interface layer 305 and reduce the corrosion rate of the interface layer.
[0083] Then, if Figure 3D As shown, the first sidewall layer 304A above the first sacrificial layer 303A is removed to obtain the first sidewall layer 304A surrounding the first sacrificial layer 303A. Specifically, the first sidewall layer 304A above the first sacrificial layer 303A can be polished away using a chemical mechanical polishing process to make the first sacrificial layer 303A and the top of the first sidewall layer 304A flush.
[0084] With respect to step S230, in some embodiments, a first sidewall layer covering the sensitive material layer 301 may be formed first, a groove may be formed by etching in the first sidewall layer, and then a first sacrificial layer filling the groove may be formed. In this example, before forming the first sidewall layer, the region of the sensitive material layer 301 corresponding to the first sidewall layer may be etched to form a recessed portion.
[0085] Next, step S240 is performed to form a second sacrificial layer 303B and a second sidewall layer 304B surrounding the second sacrificial layer 303B above the first sacrificial layer 303A and the first sidewall layer 304A, wherein the second sidewall layer 304B is connected to the first sidewall layer 304A, and the second sidewall layer 304B has a second width, which is smaller than the first width. The projection of the second sidewall layer 304B is within the projection range of the first sidewall layer 304A, and the first sidewall layer 304A and the second sidewall layer 304B together form a sidewall layer that is narrow at the top and wide at the bottom, which increases the actual length of the interface layer 305 without changing the top size of the cavity structure, thereby effectively slowing down the etching speed of the interface layer 305 without affecting the overall structure of the device.
[0086] In some embodiments, first Figure 3E As shown, a second sacrificial layer 303B is formed to cover the first sacrificial layer 303A and the first sidewall layer 304A, and a second trench connected to the first sidewall layer 304A is formed in the second sacrificial layer 303B, and the second trench has a second width. Figure 3FAs shown, a second sidewall layer 304B is formed to fill the second groove and cover the second sacrificial layer 303B. Alternatively, a portion of the second sidewall layer 304B may be formed first, and a groove for forming the second sacrificial layer 303B may be formed in the second sidewall layer 304B; the second sacrificial layer may be filled in the groove, and the second sacrificial layer outside the groove may be removed by a grinding process; and finally, another portion of the second sidewall layer covering the second sacrificial layer may be formed. The specific method for forming the second sacrificial layer 303B and the second sidewall layer 304B may refer to the first sacrificial layer 303A and the first sidewall layer 304A, and will not be described in detail here.
[0087] In some embodiments, the first sacrificial layer 303A and the first sidewall layer 304A have a first thickness, the second sacrificial layer 303B and the second sidewall layer 304B have a second thickness, and the first thickness is less than the second thickness. In other words, the first sidewall layer 304A with a wider bottom has a smaller thickness, while the first sidewall layer 304B with a narrower top has a larger thickness, thereby achieving the effect of increasing the length of the interface layer 305 while reducing the impact on the volume of the cavity structure.
[0088] Next, continue to refer to Figure 3F , performing step S250, forming a release hole 306 connected to the second sacrificial layer 303B in the second sidewall layer 304B, and referring to Figure 3G , the first sacrificial layer 303A and the second sacrificial layer 303B surrounded by the first sidewall layer 304A and the second sidewall layer 304B are removed through the release hole 306 to form a cavity structure in the first sidewall layer 304A and the second sidewall layer 304B. The release hole 306 is formed above the second sacrificial layer 303B, thereby exposing the top of the second sacrificial layer 303B. The etchant can first remove the second sacrificial layer 303B through the release hole 306, and then remove the first sacrificial layer 303A below, thereby forming a cavity structure surrounded by the first sidewall layer 304A and the second sidewall layer 304B. The lower sidewall of the cavity structure is the first sidewall layer 304A, the upper sidewall and the top are the second sidewall layer 304B, and the bottom is the sensitive material layer 301.
[0089] At this point, the process steps implemented in the method for manufacturing a semiconductor device according to an embodiment of the present invention have been completed. It can be understood that the method for manufacturing a semiconductor device according to the embodiment of the present invention not only includes the above steps, but may also include other necessary steps before, during or after the above steps, which are all included in the scope of the manufacturing method according to the embodiment of the present invention.
[0090] According to the method for manufacturing a semiconductor device provided by the present invention, the actual length of the interface layer is increased by forming a sidewall layer that is narrow at the top and wide at the bottom, thereby increasing the difficulty of corroding the interface layer, thereby enhancing the overall structure of the semiconductor device.
[0091] like Figure 3G , Figure 3H and Fig. 3I As shown, an embodiment of the present invention further provides a semiconductor device, which can be manufactured by the manufacturing method of the semiconductor device as described above. Specifically, the semiconductor device of the embodiment of the present invention includes: a semiconductor substrate (not shown); a sensitive material layer 301 formed on the semiconductor substrate, the sensitive material layer 301 including a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface; a first sidewall layer 304A formed on the second surface of the sensitive material layer 301, the first sidewall layer 304A having a first width, and an interface layer 305 formed between the first sidewall layer 304A and the sensitive material layer; a second sidewall layer 304B formed above the first sidewall layer 304A, the second sidewall layer 304B connected to the first sidewall layer 304A, the second sidewall layer 304B having a second width, and the second width is less than the first width; a cavity structure formed in the first sidewall layer 304A and the second sidewall layer 304B.
[0092] In some embodiments, the semiconductor device further comprises a recessed portion formed on the second surface of the sensitive material layer 301, and the first sidewall layer 304A passes through the recessed portion sensitive material layer 301. The bottom of the recessed portion is arc-shaped or concave-convex. The arc-shaped or concave-convex recessed portion increases the actual length of the interface layer 305 between the first sidewall layer 304A and the sensitive material layer 301, reduces the corrosion of the interface layer in the process of removing the sacrificial layer to form the cavity structure, thereby increasing the overall stability of the semiconductor device.
[0093] In some embodiments, the sensitive material layer 301 may be a piezoelectric layer; the semiconductor device further includes a first electrode (not shown) formed on a first surface of the sensitive material layer, and a second electrode 302 formed on a second surface of the sensitive material layer. The first electrode, the piezoelectric layer, and the second electrode constitute a composite film, which may also include other film layers in addition to the above-mentioned film layers, and may be reasonably arranged according to the actual device, and is not specifically limited here.
[0094] The semiconductor device of the embodiment of the present invention forms a sidewall layer that is narrow at the top and wide at the bottom, which can increase the actual length of the interface layer between the sidewall layer and the sensitive material layer, reduce the corrosion of the interface layer during the process of removing the sacrificial layer to form a cavity structure, and thus increase the overall stability of the semiconductor device.
[0095] The present invention has been described by the above embodiments, but it should be understood that the above embodiments are only for the purpose of example and description, and are not intended to limit the present invention to the scope of the described embodiments. In addition, it can be understood by those skilled in the art that the present invention is not limited to the above embodiments, and more variations and modifications can be made according to the teachings of the present invention, and these variations and modifications all fall within the scope of the protection claimed by the present invention. The protection scope of the present invention is defined by the attached claims and their equivalents.
Claims
1. A method for manufacturing a semiconductor device, characterized in that: The method comprises: providing a semiconductor substrate; forming a sensitive material layer on the semiconductor substrate; forming a first sacrificial layer and a first sidewall layer surrounding the first sacrificial layer on the sensitive material layer, wherein the first sidewall layer has a first width; forming a second sacrificial layer and a second sidewall layer surrounding the second sacrificial layer above the first sacrificial layer and the first sidewall layer, wherein the second sidewall layer is connected to the first sidewall layer and has a second width that is smaller than the first width; forming a release hole in the second sidewall layer connected to the second sacrificial layer; The first sacrificial layer and the second sacrificial layer are removed through the release hole to form a cavity structure in the first sidewall layer and the second sidewall layer.
2. The manufacturing method according to claim 1, characterized in that The step of forming a first sacrificial layer on the sensitive material layer and a first sidewall layer surrounding the first sacrificial layer comprises: forming a first sacrificial layer on the sensitive material layer, wherein a first groove penetrating the first sacrificial layer is formed in the first sacrificial layer, the first groove is used to define a boundary of the cavity structure, and the first groove has the first width; forming a first sidewall layer filling the first trench and covering the first sacrificial layer; The first sidewall layer above the first sacrificial layer is removed to obtain a first sidewall layer surrounding the first sacrificial layer.
3. The manufacturing method according to claim 1, characterized in that: The forming of a second sacrificial layer on the first sacrificial layer and around the first sidewall layer and a second sidewall layer surrounding the second sacrificial layer comprises: forming a second sacrificial layer covering the first sacrificial layer and the first sidewall layer, wherein a second trench connected to the first sidewall layer is formed in the second sacrificial layer, and the second trench has the second width; A second sidewall layer is formed to fill the second trench and cover the second sacrificial layer.
4. The manufacturing method according to claim 2, characterized in that: Before forming the first sidewall layer, the method further includes: The sensitive material layer exposed at the bottom of the first groove is etched to form a recessed portion on the surface of the sensitive material layer.
5. The manufacturing method according to claim 4, characterized in that: The bottom of the recessed portion is in an arc shape, and the etching of the sensitive material layer exposed at the bottom of the first groove to form a recessed portion on the surface of the sensitive material layer includes: The sensitive material layer exposed at the bottom of the first groove is etched using an isotropic etching process to form the recessed portion with an arc-shaped bottom.
6. The manufacturing method according to claim 4, characterized in that: The bottom of the recessed portion is concave-convex, and the etching of the sensitive material layer exposed at the bottom of the first groove to form a recessed portion on the surface of the sensitive material layer includes: forming a photoresist layer with different thicknesses at the bottom of the first trench; The sensitive material layer exposed at the bottom of the first trench is etched based on the photoresist layers with different thicknesses to form the concave portion with a concave-convex bottom.
7. The manufacturing method according to claim 1, characterized in that: The first sacrificial layer and the first sidewall layer have a first thickness, the second sacrificial layer and the second sidewall layer have a second thickness, and the first thickness is less than the second thickness.
8. The manufacturing method according to any one of claims 1 to 7, characterized in that: The sensitive material layer includes a piezoelectric layer; Before forming the sensitive material layer on the semiconductor substrate, the method further includes: forming a first electrode on the semiconductor substrate; Before forming a sensitive material layer on the semiconductor substrate and after forming a sacrificial layer on the sensitive material layer, the method further includes: forming a second electrode on the sensitive material layer.
9. A semiconductor device, characterized in that: The semiconductor device comprises: Semiconductor substrate; A sensitive material layer formed on the semiconductor substrate, the sensitive material layer comprising a first surface in contact with the semiconductor substrate, and a second surface arranged opposite to the first surface; A first sidewall layer is formed on the second surface of the sensitive material layer, the first sidewall layer has a first width, and an interface layer is formed between the first sidewall layer and the sensitive material layer; A second sidewall layer is formed above the first sidewall layer, the second sidewall layer is connected to the first sidewall layer, the second sidewall layer has a second width, and the second width is smaller than the first width; A cavity structure is formed in the first sidewall layer and the second sidewall layer.
10. The semiconductor device according to claim 9, wherein: Also includes: A recessed portion is formed on the second surface of the sensitive material layer, and the first sidewall layer is connected to the sensitive material layer through the recessed portion.