Method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid

By adjusting the pH of the calcium chloride waste liquid and the alkalinity of the fluorine-containing waste liquid, the calcium chloride waste liquid is added to form a highly concentrated calcium fluoride suspension, which solves the purity and filtration problems of calcium fluoride and achieves high efficiency. The low-cost calcium fluoride resource recycling reduces the risk of environmental pollution.

CN118929728APending Publication Date: 2024-11-12ANHUI QINGZHI TECH DEV CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411075645.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-07
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

During the treatment of fluorine-containing waste liquid, existing calcium salt treatment agents cause calcium fluoride sludge to contain too much non-reactive calcium salt, which reduces the purity of calcium fluoride, and the calcium fluoride crystals are fine and difficult to filter, resulting in Resource waste and environmental pollution risks.

Method used

By adding neutralizing reagents to the acidic calcium chloride waste liquid to adjust the pH to neutrality, measuring and increasing the calcium chloride concentration, treating the fluorine-containing waste liquid with alkaline oxides, and calculating and adding calcium chloride waste liquid to form a high The calcium fluoride suspension was concentrated, and impurities were removed after concentration and filtration to obtain high-purity calcium fluoride powder.

Benefits of technology

It has achieved efficient acquisition of high-purity calcium fluoride, reduced the cost of enterprises to process calcium chloride waste liquid, avoided resource waste and environmental pollution, and simplified the process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118929728A_ABST
    Figure CN118929728A_ABST
Patent Text Reader

Abstract

The invention provides a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid. The method comprises the following steps: step (A), adding a certain amount of neutralizing reagent into the calcium chloride waste liquid in an acidic state to adjust the pH value of the calcium chloride waste liquid to be neutral; (B) measuring the concentration of calcium ions in the calcium chloride waste liquid with neutral PH in the step (A), and converting to obtain the concentration of calcium chloride in the calcium chloride waste liquid; (C) when the concentration of calcium chloride in the calcium chloride waste liquid obtained in the step (B) is lower than 15%, the concentration of calcium chloride is increased to 15-30%, and the high-concentration calcium chloride waste liquid is obtained.The structure is reasonable, the low-cost and water-soluble calcium chloride-containing waste liquid is used as the raw material, concentration and filter pressing processes are combined, a calcium fluoride product with high purity can be efficiently obtained, and the calcium chloride waste liquid can be recycled. The method is low in cost and simple in process, reduces the calcium chloride waste liquid treatment cost of enterprises, and realizes recycling of calcium fluoride resources.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the preparation of calcium fluoride from fluorine-containing waste liquid, and in particular, to a method for preparing calcium fluoride from fluorine-containing waste liquid by treating calcium chloride-containing waste liquid. Background Art

[0002] In the treatment process of fluoride-containing waste liquid, commonly used calcium salt treatment agents include water-insoluble calcium hydroxide and calcium carbonate. Due to the insolubility of these calcium salts, when they react with fluoride ions to generate calcium fluoride, a layer of calcium fluoride will be formed on the surface of the calcium ions, which hinders the full reaction of calcium hydroxide or calcium carbonate with all fluoride ions. In order to ensure that fluoride ions can meet the emission standards, the treatment company has to add excessive calcium salts. However, this excessive addition leads to excessive non-reactive calcium salts in the calcium fluoride sludge, reducing the purity of calcium fluoride. At the same time, since the product calcium fluoride has fine crystals and the liquid-to-solid ratio is still very small after sedimentation, it is difficult to filter and needs to be treated with flocculants, which also increases the content of impurities in calcium fluoride, making it unable to meet the quality requirements as an industrial raw material. These impure calcium fluorides can only be treated as solid waste, either landfilled or used as part of building materials. This not only leads to the waste of precious fluorine resources, but also occupies a large amount of land resources and has potential environmental pollution risks. Therefore, a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride waste liquid is urgently needed to solve the above problems. Summary of the invention

[0003] In view of the shortcomings of the prior art, the purpose of this application is to provide a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid, so as to solve the problems raised in the above background technology.

[0004] In order to achieve the above object, the present application provides a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid, comprising the following steps:

[0005] Step (A) adding a certain amount of neutralizing agent into the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral;

[0006] Step (B) measures the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A) and converts the concentration of calcium chloride in the calcium chloride waste liquid;

[0007] Step (C) when the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is lower than 15%, increasing the concentration of calcium chloride to 15-30% to obtain a high-concentration calcium chloride waste liquid;

[0008] When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated;

[0009] Step (D) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to be alkaline, and measuring the mass of the fluorine-containing waste liquid with an alkaline pH and the concentration of fluoride ions therein;

[0010] Step (E) According to the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid;

[0011] Step (F) according to the mass of the calcium chloride-containing waste liquid calculated in step (E), an excess of 2% to 10% of the calcium chloride-containing waste liquid with a neutral pH in step (C) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D), and stirred and aged at room temperature to obtain a calcium fluoride suspension A;

[0012] Step (G) using a concentrating device to increase the solid content of the calcium fluoride suspension A obtained in step (F) to 30-70% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon;

[0013] Step (H) mixing the crude calcium fluoride filter cake obtained in step (G) with a sodium hydroxide solution having a Ph value of 8-10, stirring for reaction, removing impurity silicon in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B;

[0014] In step (I), the calcium fluoride suspension B obtained in step (H) is filtered by a filter press to obtain a calcium fluoride filter cake, and then the calcium fluoride filter cake is repeatedly washed with water to remove impurity ions and then dried, and finally pulverized to obtain a calcium fluoride powder with high purity.

[0015] Preferably, the neutralizing agent in step (A) is calcium oxide or calcium hydroxide.

[0016] Preferably, the pH value of the acidic calcium chloride waste liquid in step (A) is measured by an online pH measuring instrument, and the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (B) is measured by an online calcium ion concentration meter.

[0017] Preferably, the formula for conversion in step (B) is:

[0018] If the measured calcium ion concentration in the waste liquid is ng / L, then the concentration of calcium chloride is 2.775ng / L.

[0019] Preferably, in step (C), the MVR technology is used to increase the calcium chloride concentration to 15-30% to obtain high-concentration calcium chloride waste liquid.

[0020] Preferably, the concentration of fluoride ions in the fluorine-containing waste liquid with an alkaline pH in step (D) is measured by an online measurement and control instrument, and the pH of the fluorine-containing waste liquid is adjusted to be greater than 8 in step (D).

[0021] Preferably, the formula for calculating the mass of the calcium chloride-containing waste liquid to be added to the fluorine-containing waste liquid in step (E) is as follows:

[0022]

[0023] in:

[0024] m1 is the amount of fluorine-containing waste liquid, kg;

[0025] c1 is the concentration of fluoride ions in the fluoride-containing waste liquid, kg / L;

[0026] m2 is the amount of waste liquid containing calcium chloride, kg;

[0027] c2 is the concentration of calcium chloride in the calcium chloride-containing waste liquid, kg / L.

[0028] Preferably, the stirring and aging in step (F) is specifically: stirring at a speed of 200-500 rpm for 2-3 hours and aging for 12-24 hours.

[0029] Preferably, the stirring reaction in step (H) is specifically: stirring at a rotation speed of 300-2000 rpm and reacting for 1-6 hours.

[0030] Preferably, the impurity silicon in the crude calcium fluoride filter cake in step (H) is silicon and silicon dioxide, and the reaction chemical equation is as follows:

[0031] SiO2+2NaOH→Na2SiO3+H2O

[0032] Si+2NaOH+H2O→Na2SiO3+2H2↑.

[0033] According to the present invention, a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid is disclosed. The present invention uses low-cost and water-soluble calcium chloride-containing waste liquid as raw material, and combines concentration and filter pressing processes to avoid the introduction of other impurities and improve production efficiency. The method has low cost and simple process, reduces the cost of enterprises for treating calcium chloride waste liquid, and realizes the recycling of calcium fluoride resources. BRIEF DESCRIPTION OF THE DRAWINGS

[0034] Other features, objects and advantages of the present application will become more apparent by reading the detailed description of non-limiting embodiments with reference to the following drawings:

[0035] Figure 1 The present invention is a flow chart of a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to one embodiment of the present application. DETAILED DESCRIPTION

[0036] In order to make the technical means, creative features, objectives and effects achieved by this application easy to understand, this application is further explained below in conjunction with specific implementation methods.

[0037] like Figure 1 As shown, the present application provides a technical solution: a method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid, comprising the following steps:

[0038] Step (A) adding a certain amount of neutralizing agent into the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral;

[0039] Step (B) measures the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A) and converts the concentration of calcium chloride in the calcium chloride waste liquid;

[0040] Step (C) when the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is lower than 15%, increasing the concentration of calcium chloride to 15-30% to obtain a high-concentration calcium chloride waste liquid;

[0041] When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated;

[0042] Step (D) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to be alkaline, and measuring the mass of the fluorine-containing waste liquid with an alkaline pH and the concentration of fluoride ions therein;

[0043] Step (E) According to the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid;

[0044] Step (F) is calculated based on the mass of the calcium chloride-containing waste liquid calculated in step (E), and an excess of 2% to 10% of the calcium chloride-containing waste liquid with a neutral pH in step (C) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D), and stirred and aged at room temperature to obtain a calcium fluoride suspension A, which is designed to allow all fluoride ions in the fluorine-containing waste liquid to react;

[0045] Step (G) using a concentration device to increase the solid content of the calcium fluoride suspension A obtained in step (F) to 30-70% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon. The impurity silicon here is because the fluorine-containing waste liquid mainly comes from photovoltaic enterprises, and there will be a certain amount of impurity silicon during the treatment process. Due to the increase in the solid content of the calcium fluoride suspension A, this design avoids the phenomenon that when the filter press equipment is directly used for solid-liquid separation when the solid content is low, the surface load of the filter cloth is insufficient, which affects the filtering effect;

[0046] Step (H) mixing the crude calcium fluoride filter cake obtained in step (G) with a sodium hydroxide solution having a Ph value of 8-10, stirring for reaction, removing impurity silicon in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B;

[0047] In step (I), the calcium fluoride suspension B obtained in step (H) is filtered by a filter press to obtain a calcium fluoride filter cake, and then the calcium fluoride filter cake is repeatedly washed with water to remove impurity ions and then dried, and finally pulverized to obtain a calcium fluoride powder with high purity.

[0048] Preferably, the neutralizing agent in step (A) is calcium oxide or calcium hydroxide, which not only adjusts the pH value but also increases the concentration of calcium chloride in the waste liquid.

[0049] Preferably, the pH value of the acidic calcium chloride waste liquid in step (A) is measured by an online pH measuring instrument, and the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (B) is measured by an online calcium ion concentration meter.

[0050] Preferably, the formula for conversion in step (B) is:

[0051] If the measured calcium ion concentration in the waste liquid is ng / L, then the concentration of calcium chloride is 2.775ng / L.

[0052] Preferably, the MVR technology is used to increase the calcium chloride concentration to 15-30% to obtain high-concentration calcium chloride waste liquid in step (C), and the specific steps are as follows:

[0053] The calcium chloride waste liquid with a low calcium chloride concentration obtained in step (B) is pressurized by a feed pump and then enters an MVR evaporation system. After a large-flow forced circulation, it is continuously circulated and heated in a separator and a heater, and concentrated by an MVR evaporator. The material is evaporated and concentrated, and the concentration of the calcium chloride material is continuously increased. When the concentration reaches 15-30%, it is discharged to a liquid storage tank to obtain a high-concentration calcium chloride waste liquid. The MVR technology is a prior art.

[0054] Preferably, the concentration of fluoride ions in the fluorine-containing waste liquid with an alkaline pH in step (D) is measured by an online measurement and control instrument, and the pH of the fluorine-containing waste liquid is adjusted to be greater than 8 in step (D).

[0055] Preferably, the formula for calculating the mass of the calcium chloride-containing waste liquid to be added to the fluorine-containing waste liquid in step (E) is as follows:

[0056]

[0057] in:

[0058] m1 is the amount of fluorine-containing waste liquid, kg;

[0059] c1 is the concentration of fluoride ions in the fluoride-containing waste liquid, kg / L;

[0060] m2 is the amount of waste liquid containing calcium chloride, kg;

[0061] c2 is the concentration of calcium chloride in the calcium chloride-containing waste liquid, kg / L, where 111 is the relative atomic mass of calcium chloride and 38 is the relative atomic mass of two fluoride ions, because one calcium in CaF2 corresponds to two fluoride ions, and the relative atomic mass of fluorine is 19.

[0062] Preferably, the stirring and aging in step (F) is specifically: stirring at a speed of 200-500 rpm for 2-3 hours and aging for 12-24 hours.

[0063] Preferably, the stirring reaction in step (H) is specifically: stirring at a rotation speed of 300-2000 rpm and reacting for 1-6 hours.

[0064] Preferably, the impurities in the crude calcium fluoride filter cake in step (H) are silicon and silicon dioxide, and the reaction chemical equation is as follows:

[0065] SiO2+2NaOH→Na2SiO3+H2O

[0066] Si+2NaOH+H2O→Na2SiO3+2H2↑.

[0067] The following is a specific embodiment of the method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to the present invention.

[0068] Example 1: Step (A1) The pH of the acidic calcium chloride waste liquid is measured by an online pH measuring instrument, and then a certain amount of calcium oxide is added to the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral;

[0069] Step (B1) measures the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A1) by an online calcium ion concentration meter and converts the concentration of calcium chloride in the calcium chloride waste liquid to obtain the concentration of calcium chloride in the calcium chloride waste liquid. The conversion formula is: if the calcium ion concentration in the waste liquid is measured to be ng / L, the concentration of calcium chloride is 2.775ng / L;

[0070] Step (C1) When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B1) is lower than 15%, the MVR technology is used to increase the concentration of calcium chloride to 15% to obtain a high-concentration calcium chloride waste liquid as follows: the calcium chloride waste liquid with a low calcium chloride concentration obtained in step (B1) is pressurized by a feed pump and enters an MVR evaporation system, is continuously heated in a separator and a heater through a large-flow forced circulation, is concentrated through an MVR evaporator, and the material is evaporated and concentrated, and the concentration of the calcium chloride material is continuously increased. When the concentration reaches 15%, it is discharged to a liquid storage tank to obtain a high-concentration calcium chloride waste liquid, thereby increasing the concentration of calcium chloride to 15%;

[0071] When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B1) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated;

[0072] Step (D1) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to alkaline, adjusting the pH to 9, and measuring the mass of the fluorine-containing waste liquid with an alkaline pH and the concentration of fluoride ions therein, wherein the concentration of fluoride ions in the fluorine-containing waste liquid is measured using an online measurement and control instrument;

[0073] Step (E1) is based on the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C1) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D1) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid;

[0074] Step (F1) is calculated based on the mass of the calcium chloride-containing waste liquid calculated in step (E1), and 2% of the calcium chloride-containing waste liquid with a neutral pH in step (C1) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D1), and stirred at a speed of 200 rpm for 2 hours and aged for 20 hours at room temperature to obtain a calcium fluoride suspension A;

[0075] Step (G1) using a concentrating device to increase the solid content of the calcium fluoride suspension A obtained in step (F1) to 30% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon;

[0076] Step (H1) mixing the crude calcium fluoride filter cake obtained in step (G1) with a sodium hydroxide solution having a Ph value of 10, stirring at a speed of 300 rpm, reacting for 5 hours, removing silicon and silicon dioxide in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B;

[0077] Step (I1) uses a filter press to filter the calcium fluoride suspension B obtained in step (H1) to obtain a calcium fluoride filter cake, and then repeatedly washes the calcium fluoride filter cake with water to remove Na + 、SiO3 2- After removing impurity ions, it is dried and finally pulverized to obtain calcium fluoride powder with high purity.

[0078] Embodiment 2: Step (A2) measures the pH of the acidic calcium chloride waste liquid by an online pH measuring instrument, and then adds a certain amount of calcium hydroxide to the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral;

[0079] Step (B2) measures the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A2) by an online calcium ion concentration meter and converts the concentration of calcium chloride in the calcium chloride waste liquid to obtain the concentration of calcium chloride. The conversion formula is: if the calcium ion concentration in the waste liquid is measured to be ng / L, the concentration of calcium chloride is 2.775ng / L;

[0080] Step (C2) When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B2) is lower than 15%, the MVR technology is used to increase the concentration of calcium chloride to 20% to obtain a high-concentration calcium chloride waste liquid as follows: the calcium chloride waste liquid with a low calcium chloride concentration obtained in step (B2) is pressurized by a feed pump and enters an MVR evaporation system, is continuously heated in a separator and a heater through a large-flow forced circulation, is concentrated through an MVR evaporator, and the material is evaporated and concentrated, and the concentration of the calcium chloride material is continuously increased. When the concentration reaches 20%, it is discharged to a liquid storage tank to obtain a high-concentration calcium chloride waste liquid, thereby increasing the concentration of calcium chloride to 20%;

[0081] When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B2) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated;

[0082] Step (D2) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to alkaline, adjusting the pH to 10, and measuring the mass of the fluorine-containing waste liquid with alkaline pH and the concentration of fluoride ions therein, wherein the concentration of fluoride ions in the fluorine-containing waste liquid is measured using an online measurement and control instrument;

[0083] Step (E2) is based on the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C2) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D2) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid;

[0084] Step (F2) is calculated based on the mass of the calcium chloride-containing waste liquid calculated in step (E2), and 5% of the calcium chloride-containing waste liquid with a neutral pH in step (C2) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D2), and stirred at a speed of 300 rpm for 2.5 hours and aged for 16 hours at room temperature to obtain a calcium fluoride suspension A;

[0085] Step (G2) using a concentrating device to increase the solid content of the calcium fluoride suspension A obtained in step (F2) to 50% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon;

[0086] Step (H2) mixing the crude calcium fluoride filter cake obtained in step (G2) with a sodium hydroxide solution having a Ph value of 10, stirring at a speed of 1000 rpm, reacting for 3 hours, removing silicon and silicon dioxide in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B;

[0087] Step (I2) uses a filter press to filter the calcium fluoride suspension B obtained in step (H2) to obtain a calcium fluoride filter cake, and then repeatedly washes the calcium fluoride filter cake with water to remove Na + 、SiO3 2- After removing impurity ions, it is dried and finally pulverized to obtain calcium fluoride powder with high purity.

[0088] Embodiment 3: Step (A3) The pH of the acidic calcium chloride waste liquid is measured by an online pH measuring instrument, and then a certain amount of calcium oxide is added to the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral;

[0089] Step (B3) measuring the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A3) by an online calcium ion concentration meter and converting the concentration of calcium chloride in the calcium chloride waste liquid, the conversion formula is: if the calcium ion concentration in the waste liquid is measured to be ng / L, then the concentration of calcium chloride is 2.775ng / L, which is obtained based on the relative atomic mass of calcium being 40 and the relative atomic mass of calcium chloride being 111;

[0090] Step (C3) When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B3) is lower than 15%, the MVR technology is used to increase the concentration of calcium chloride to 30% to obtain a high-concentration calcium chloride waste liquid as follows: the calcium chloride waste liquid with a low calcium chloride concentration obtained in step (B3) is pressurized by a feed pump and enters an MVR evaporation system, is continuously heated in a separator and a heater through a large-flow forced circulation, is concentrated through an MVR evaporator, and the material is evaporated and concentrated, and the concentration of the calcium chloride material is continuously increased. When the concentration reaches 30%, it is discharged to a liquid storage tank to obtain a high-concentration calcium chloride waste liquid, thereby increasing the concentration of calcium chloride to 30%;

[0091] When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B3) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated;

[0092] Step (D3) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to alkaline, adjusting the pH to 11, and measuring the mass of the fluorine-containing waste liquid with an alkaline pH and the concentration of fluoride ions therein, wherein the concentration of fluoride ions in the fluorine-containing waste liquid is measured using an online measurement and control instrument;

[0093] Step (E3) is based on the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C3) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D3) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid;

[0094] Step (F3) is calculated according to the mass of the calcium chloride-containing waste liquid calculated in step (E3), and 8% of the calcium chloride-containing waste liquid with a neutral pH in step (C3) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D3), and stirred at a speed of 500 rpm for 2 hours and aged for 12 hours at room temperature to obtain a calcium fluoride suspension A;

[0095] Step (G3) using a concentrating device to increase the solid content of the calcium fluoride suspension A obtained in step (F3) to 70% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon;

[0096] Step (H3) mixing the crude calcium fluoride filter cake obtained in step (G3) with a sodium hydroxide solution having a Ph value of 10, stirring at a speed of 800 rpm, reacting for 2 hours, removing silicon and silicon dioxide in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B;

[0097] Step (I3) uses a filter press to filter the calcium fluoride suspension B obtained in step (H3) to obtain a calcium fluoride filter cake, and then repeatedly washes the calcium fluoride filter cake with water to remove Na + 、SiO3 2- After removing impurity ions, it is dried and finally pulverized to obtain calcium fluoride powder with high purity.

[0098] The method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid in the present application uses low-cost and water-soluble calcium chloride-containing waste liquid as raw material, and combines concentration and filter pressing processes to avoid the introduction of other impurities and improve production efficiency, thereby being able to efficiently obtain a calcium fluoride product with high purity, with low cost and simple process, reducing the cost of enterprises in treating calcium chloride waste liquid and realizing the recycling of calcium fluoride resources.

[0099] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A method for preparing calcium fluoride by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid, characterized in that: The following steps are involved: Step (A) adding a certain amount of neutralizing agent into the acidic calcium chloride waste liquid to adjust the pH of the calcium chloride waste liquid to neutral; Step (B) measures the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in step (A) and converts the concentration of calcium chloride in the calcium chloride waste liquid; Step (C) when the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is lower than 15%, increasing the concentration of calcium chloride to 15-30% to obtain a high-concentration calcium chloride waste liquid; When the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (B) is higher than 15%, it is a high-concentration calcium chloride waste liquid and does not need to be treated; Step (D) adding a certain amount of alkaline oxide or hydroxide to the fluorine-containing waste liquid to adjust the pH of the fluorine-containing waste liquid to be alkaline, and measuring the mass of the fluorine-containing waste liquid with an alkaline pH and the concentration of fluoride ions therein; Step (E) According to the chemical reaction equation Ca 2+ +2F - →CaF2↓, the concentration of calcium chloride in the calcium chloride waste liquid obtained in step (C) and the concentration and mass of fluoride ions in the fluorine-containing waste liquid measured in step (D) to calculate the mass of the calcium chloride waste liquid that needs to be added to the fluorine-containing waste liquid; Step (F) according to the mass of the calcium chloride-containing waste liquid calculated in step (E), an excess of 2% to 10% of the calcium chloride-containing waste liquid with a neutral pH in step (C) is gradually added to the fluorine-containing waste liquid with an alkaline pH in step (D), and stirred and aged at room temperature to obtain a calcium fluoride suspension A; Step (G) using a concentrating device to increase the solid content of the calcium fluoride suspension A obtained in step (F) to 30-70% to obtain a concentrated slurry with a high solid content, and then filtering the concentrated slurry through a filter press to obtain a crude calcium fluoride filter cake containing a certain amount of impurity silicon; Step (H) mixing the crude calcium fluoride filter cake obtained in step (G) with a sodium hydroxide solution having a Ph value of 8-10, stirring for reaction, removing impurity silicon in the crude calcium fluoride filter cake, and obtaining a calcium fluoride suspension B; In step (I), the calcium fluoride suspension B obtained in step (H) is filtered by a filter press to obtain a calcium fluoride filter cake, and then the calcium fluoride filter cake is repeatedly washed with water to remove impurity ions and then dried, and finally pulverized to obtain a calcium fluoride powder with high purity.

2. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The neutralizing agent in step (A) is calcium oxide or calcium hydroxide.

3. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The pH value of the acidic calcium chloride waste liquid in the step (A) is measured by an online pH measuring instrument, and the calcium ion concentration in the calcium chloride waste liquid with a neutral pH in the step (B) is measured by an online calcium ion concentration meter.

4. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The formula for conversion in step (B) is: If the measured calcium ion concentration in the waste liquid is ng / L, then the concentration of calcium chloride is 2.775ng / L.

5. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: In the step (C), the MVR technology is used to increase the concentration of calcium chloride to 15-30% to obtain high-concentration calcium chloride waste liquid.

6. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: In the step (D), the concentration of fluoride ions in the fluorine-containing waste liquid with an alkaline pH is measured by an online measurement and control instrument, and the pH of the fluorine-containing waste liquid is adjusted to be greater than 8 in the step (D).

7. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The formula for calculating the mass of the calcium chloride-containing waste liquid to be added to the fluorine-containing waste liquid in the step (E) is as follows: in: m1 is the amount of fluorine-containing waste liquid, kg; c1 is the concentration of fluoride ions in the fluoride-containing waste liquid, kg / L; m2 is the amount of waste liquid containing calcium chloride, kg; c2 is the concentration of calcium chloride in the calcium chloride-containing waste liquid, kg / L.

8. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The stirring and aging in step (F) specifically comprises: stirring at a speed of 200-500 rpm for 2-3 hours and aging for 12-24 hours.

9. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The stirring reaction in step (H) is specifically: stirring at a rotation speed of 300-2000 rpm and reacting for 1-6 hours.

10. The method for preparing calcium fluoride from fluorine-containing waste liquid by treating fluorine-containing waste liquid with calcium chloride-containing waste liquid according to claim 1, characterized in that: The impurity silicon in the crude calcium fluoride filter cake in step (H) is silicon and silicon dioxide, and the reaction chemical equation is as follows: SiO2+2NaOH→Na2SiO3+H2O Si+2NaOH+H2O→Na2SiO3+2H2↑.