Manufacturing method of formula for preparing hollow brick by using waste polyurethane foam
By mixing fly ash with waste polyurethane foam recycling liquid and pouring it into the hollow brick, the problem of insufficient degradation and seismic resistance of polyurethane foam materials is solved, and higher seismic resistance and thermal insulation effect are achieved. It is suitable for building exterior walls. type of application.
Patent Information
- Application Number
- CN202310516926.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-09
- Publication Date
- 2024-11-12
AI Technical Summary
Polyurethane foam materials lack the recycling characteristics of primary and secondary degradation in terms of degradation, and hollow bricks for construction have shortcomings in seismic resistance and load-bearing capacity, making it difficult to effectively utilize their thermal insulation and sound insulation effects.
Mix fly ash with waste polyurethane foam recovery liquid, polyisocyanate PAPI, catalyst and foam stabilizer, pour it into the hollow brick, cure and foam mold at room temperature to improve its earthquake resistance and insulation effect.
It improves the earthquake resistance level and load-bearing capacity of hollow bricks, enhances the insulation, sound insulation and noise reduction effects, and reduces costs. It is suitable for insulation, sound insulation, shock absorption and moisture-proof applications of building exterior walls.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of building thermal insulation materials, and in particular relates to a method for preparing a formula for hollow bricks by utilizing waste polyurethane foam. Background Art
[0002] Polyurethane foam sealant is an optimized petroleum product with isocyanate and polyether as the main raw materials. It is a new type of synthetic material with thermal insulation and waterproofing functions. Its thermal conductivity is low, equivalent to half of that of extruded board, and is the lowest thermal conductivity of all thermal insulation materials. It is colorless and odorless, and has a variety of solid shapes. Polyurethane foam has a high utilization rate in industry and agriculture, but the degradation of polyurethane foam is a problem, and it does not have the characteristics of primary and secondary degradation and recycling.
[0003] Hollow bricks for construction have more holes, which reduce the total weight of the building and make the house have a certain effect of heat preservation, sound insulation and noise reduction, but the overall earthquake resistance and load-bearing capacity of the house are deteriorated. The present invention is to make secondary waste of polyurethane foam plastics, make foaming prepolymer and pour it into the inside of the hollow bricks, so as to improve the strength, heat preservation, sound insulation and noise reduction effects of the hollow bricks for construction.
[0004] In view of this, the present invention is proposed. Summary of the invention
[0005] In order to solve the above technical problems, the basic concept of the technical solution adopted by the present invention is:
[0006] A method for preparing a hollow brick formula using waste polyurethane foam comprises the following steps:
[0007] The first step: first feed the fly ash into the pulverizer according to the weight and grind it into uniform powder;
[0008] Step 2: Mix the crushed powder with the waste polyurethane foam recovery liquid, polyisocyanate PAPI, catalyst, and foam stabilizer, and stir the mixture evenly;
[0009] Step 3: pour the evenly stirred mixture into the interior of hollow bricks, solidify and foam at room temperature to obtain the polyurethane foam recovery liquid for pouring hollow bricks for construction.
[0010] As a preferred embodiment of the present invention, the first step is to crush the raw materials into 250-300 meshes.
[0011] As a preferred embodiment of the present invention, in the third step, the curing time at room temperature is 24-48 hours.
[0012] As a preferred embodiment of the present invention, the foam stabilizer is organic silicon or polyol or silicone or sulfonated fatty alcohol or sulfonated fatty acid.
[0013] Compared with the prior art, the present invention has the following beneficial effects:
[0014] The present invention pours waste polyurethane recycled foam inside the hollow brick, and the overall compressive strength is moderate. It can be crushed and absorbed preferentially when resisting earthquakes, thereby improving the earthquake resistance level and load-bearing capacity of the hollow bricks for construction, and further improving the thermal insulation, sound insulation and noise reduction effects. The polyurethane foam recycled liquid poured into the hollow bricks for construction prepared by the method has low cost, controllable density and strength of the hollow bricks, and good on-site construction performance, and is suitable for applications such as thermal insulation, sound insulation and noise reduction, shock absorption, and moisture resistance of building exterior walls. DETAILED DESCRIPTION
[0015] A method for preparing a hollow brick formula using waste polyurethane foam comprises the following steps:
[0016] Step 1: First, feed the fly ash into the pulverizer according to the weight, and crush it into a uniform powder, crushing it into 250-300 mesh;
[0017] Step 2: Mix the crushed powder with the waste polyurethane foam recovery liquid, polyisocyanate PAPI, catalyst, and foam stabilizer, and stir the mixture evenly;
[0018] Step 3: pour the evenly stirred mixture into the hollow bricks, solidify and foam at room temperature, the solidification time at room temperature is 24-48 hours, and the polyurethane foam recovery liquid is obtained for pouring hollow bricks for construction.
[0019] The foam stabilizer is organic silicon, polyol, silicone, sulfonated fatty alcohol or sulfonated fatty acid.
[0020] The present invention pours waste polyurethane recycled foam inside the hollow brick, and the overall compressive strength is moderate. It can be crushed and absorbed preferentially when resisting earthquakes, thereby improving the earthquake resistance level and load-bearing capacity of the hollow bricks for construction, and further improving the thermal insulation, sound insulation and noise reduction effects. The polyurethane foam recycled liquid poured into the hollow bricks for construction prepared by the method has low cost, controllable density and strength of the hollow bricks, and good on-site construction performance, and is suitable for applications such as thermal insulation, sound insulation and noise reduction, shock absorption, and moisture resistance of building exterior walls.
[0021] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of the present invention.
[0022] It is to be understood that the present invention is described by some embodiments, and it is known to those skilled in the art that various changes or equivalent substitutions may be made to these features and embodiments without departing from the spirit and scope of the present invention. In addition, under the teachings of the present invention, these features and embodiments may be modified to adapt to specific circumstances and materials without departing from the spirit and scope of the present invention. Therefore, the present invention is not limited by the specific embodiments disclosed herein, and all embodiments falling within the scope of the claims of this application are within the scope of protection of the present invention.
Claims
1. A method for preparing a hollow brick formula using waste polyurethane foam, characterized in that: The following steps are included: The first step: first feed the fly ash into the pulverizer according to the weight and grind it into uniform powder; Step 2: Mix the crushed powder with the waste polyurethane foam recovery liquid, polyisocyanate PAPI, catalyst, and foam stabilizer, and stir the mixture evenly; Step 3: pour the evenly stirred mixture into the interior of hollow bricks, solidify and foam at room temperature to obtain the polyurethane foam recovery liquid for pouring hollow bricks for construction.
2. The method for preparing a hollow brick formula using waste polyurethane foam according to claim 1, characterized in that: In the first step, the particles are crushed into 250-300 meshes.
3. The method for preparing a formula for preparing hollow bricks using waste polyurethane foam according to claim 1, characterized in that: In the third step, the curing time at room temperature is 24-48 hours.
4. The method for preparing a hollow brick formula using waste polyurethane foam according to any one of claims 1 to 3, characterized in that: The foam stabilizer is organic silicon, polyol, silicone, sulfonated fatty alcohol or sulfonated fatty acid.