Graphene-based thermal insulation coating and production method thereof
By adding modified zeolite powder and hollow glass beads to the epoxy resin matrix and using specific additives, the problem of unstable performance of thermal insulation coatings in the prior art is solved, and a more stable thermal insulation effect and a longer service life are achieved.
Patent Information
- Application Number
- CN202411065138.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-05
- Publication Date
- 2024-11-12
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The semiconductor and metal powder doped in existing insulation coatings have unstable insulation performance and short service life due to uncontrollable factors.
Using graphene-based insulation coating, modified zeolite powder and hollow glass beads are added to the epoxy resin matrix, and aqueous silicone emulsion defoaming agent, leveling agent, film forming agent and adhesion promoter are used to modify Elastic treatment and uniform stirring improve the insulation effect and viscosity of the paint.
It achieves a more stable and long-lasting insulation performance of the paint, enhances the overall insulation effect and viscosity of the paint, improves the solidification and molding ability after coating, and avoids the paint falling off.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of coatings, and in particular relates to a graphene-based thermal insulation coating and a production method thereof. Background Art
[0002] Paint, a chemical product, is not unfamiliar to consumers. Paint is widely used and can be used for insulation, rust prevention, mildew prevention, heat resistance and other functions. It is used in many places, such as construction sites, cars, furniture and other places.
[0003] The Chinese invention patent with application number 201710808268.1 discloses a thermal insulation coating, which is doped with semiconductors and metal powders to achieve thermal insulation performance. However, semiconductors and metal powders are added to the coating, and there are too many uncontrollable factors when the coating is used, and it cannot stably exert its predetermined thermal insulation performance.
[0004] Therefore, it is necessary to develop a thermal insulation coating with stable thermal insulation performance and long service life. Summary of the invention
[0005] The purpose of the present invention is to overcome the deficiencies of the prior art and provide an antibacterial ceramic material and a manufacturing method thereof.
[0006] The present invention adopts the following technical solution: The graphene-based thermal insulation coating includes the following components in parts by mass: 80-100 parts of epoxy resin, 10-12 parts of defoaming agent, 9-10 parts of leveling agent, 15-20 parts of graphene, 8-11 parts of film-forming agent, 9-11 parts of curing agent, 18-23 parts of zeolite powder, and 25-31 parts of 40-50 μm hollow glass beads.
[0007] Furthermore, the defoaming agent is defoaming agent JY-810.
[0008] Furthermore, the leveling agent is AKN-UV1151.
[0009] Furthermore, the film-forming agent is alcohol ester dodecahydrate.
[0010] Furthermore, the curing agent is epoxy powder coating curing agent EPH180.
[0011] Furthermore, the composition further comprises 10 to 13 parts by weight of AKN-6000 adhesion promoter.
[0012] The production method of the graphene-based thermal insulation coating comprises the following steps: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass fractions, the zeolite powder and hollow glass beads are added to 60-70 parts of water, and then 25-30 parts of hexadecyltrimethylammonium bromide are added, and stirred at 70-80° C. for 20-30 minutes without filtering to obtain a modified zeolite powder containing a liquid; Step 2: Mixing According to the mass fraction, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 10 to 20 minutes. Then, the graphene, leveling agent, film-forming agent, curing agent, defoaming agent and AKN-6000 adhesion promoter are added in sequence, and the stirring time is 5 to 7 minutes between the addition of each raw material. Finally, stirring is performed for 20 to 30 minutes to obtain a graphene-based thermal insulation coating.
[0013] Compared with the prior art, the present invention has the following beneficial effects: The thermal insulation coating of the present invention uses epoxy resin as a matrix, uses hexadecyltrimethylammonium bromide as a surfactant, and modifies zeolite powder so that it is fully mixed with hollow glass beads having thermal insulation performance, and is dispersed more evenly during the stirring process with other graphene-based raw materials, thereby further improving the overall thermal insulation effect of the coating; At the same time, in order to improve the overall performance of the coating, water-based silicone emulsion defoamer JY-810, leveling agent AKN-UV1151, film-forming agent alcohol ester twelve and AKN-6000 adhesion promoter are added to improve the effective solidification and molding of the coating after it is applied to the product surface, and it has extremely strong adhesion to the product surface and is not easy to fall off. DETAILED DESCRIPTION
[0014] The raw materials used in the present invention are all commercially available products.
[0015] The water-based silicone emulsion defoamer JY-810 was purchased from Jiangsu Jianyu Additive Technology Co., Ltd.; Leveling agent AKN-UV1151 was purchased from Foshan Qianyou Chemical Co., Ltd.; Film-forming agent alcohol ester XII was purchased from Shanghai Kaiyin Chemical Co., Ltd.; Epoxy powder coating curing agent EPH180 was purchased from Nanjing Qinghai Trading Co., Ltd.; AKN-6000 adhesion promoter was purchased from Foshan Qianyou Chemical Co., Ltd.
[0016] Example 1 The graphene-based thermal insulation coating includes the following components in parts by mass: 80 parts of epoxy resin, 10 parts of defoaming agent, 9 parts of leveling agent, 15 parts of graphene, 8 parts of film-forming agent, 9 parts of curing agent, 18 parts of zeolite powder, 25 parts of 40 hollow glass beads, and 10 parts of AKN-6000 adhesion promoter.
[0017] Wherein, the defoamer is defoamer JY-810, the leveling agent is AKN-UV1151, the film-forming agent is alcohol ester twelve, and the curing agent is epoxy powder coating curing agent EPH180.
[0018] A method for producing a graphene-based thermal insulation coating comprises the following steps: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass fractions, the zeolite powder and hollow glass beads are added to 60 parts of water, and then 25 parts of hexadecyltrimethylammonium bromide are added, and stirred at 70° C. for 20 minutes without filtering to obtain a modified zeolite powder containing a liquid; Step 2: Mixing According to the mass fractions, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 10 minutes. Then, the graphene, leveling agent, film-forming agent, curing agent, defoaming agent and AKN-6000 adhesion promoter are added in sequence, and the stirring time is 5 minutes between each raw material addition. Finally, stirring is performed for 20 minutes to obtain a graphene-based thermal insulation coating.
[0019] Example 2 The graphene-based thermal insulation coating includes the following components in parts by mass: 100 parts of epoxy resin, 12 parts of defoaming agent, 10 parts of leveling agent, 20 parts of graphene, 11 parts of film-forming agent, 11 parts of curing agent, 23 parts of zeolite powder, 31 parts of 50μm hollow glass beads, and 13 parts of AKN-6000 adhesion promoter.
[0020] Wherein, the defoamer is defoamer JY-810, the leveling agent is AKN-UV1151, the film-forming agent is alcohol ester twelve, and the curing agent is epoxy powder coating curing agent EPH180.
[0021] A method for producing a graphene-based thermal insulation coating comprises the following steps: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass fractions, the zeolite powder and hollow glass beads are added to 70 parts of water, and then 30 parts of hexadecyltrimethylammonium bromide are added, and stirred at 80° C. for 30 minutes without filtering to obtain a modified zeolite powder containing a liquid; Step 2: Mixing According to the mass fractions, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 20 minutes. Then, the graphene, leveling agent, film-forming agent, curing agent, defoaming agent and AKN-6000 adhesion promoter are added in sequence, and the stirring time is 7 minutes between each raw material addition. Finally, stirring is performed for 30 minutes to obtain a graphene-based thermal insulation coating.
[0022] Example 3 The graphene-based thermal insulation coating includes the following components in parts by mass: 90 parts of epoxy resin, 11 parts of defoaming agent, 10 parts of leveling agent, 18 parts of graphene, 10 parts of film-forming agent, 10 parts of curing agent, 21 parts of zeolite powder, 28 parts of 45μm hollow glass beads, and 12 parts of AKN-6000 adhesion promoter.
[0023] Wherein, the defoamer is defoamer JY-810, the leveling agent is AKN-UV1151, the film-forming agent is alcohol ester twelve, and the curing agent is epoxy powder coating curing agent EPH180.
[0024] A method for producing a graphene-based thermal insulation coating comprises the following steps: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass parts, the zeolite powder and hollow glass beads are added to 65 parts of water, and then 28 parts of hexadecyltrimethylammonium bromide are added, and stirred at 75° C. for 25 minutes without filtering to obtain modified zeolite powder containing liquid; Step 2: Mixing According to the mass fractions, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 15 minutes. Then, the graphene, leveling agent, film-forming agent, curing agent, defoaming agent and AKN-6000 adhesion promoter are added in sequence, and the stirring time is 6 minutes between each raw material addition. Finally, stirring is performed for 25 minutes to obtain a graphene-based thermal insulation coating.
[0025] Comparison example The graphene-based thermal insulation coating comprises the following components in parts by mass: 90 parts of epoxy resin, 11 parts of defoaming agent, 10 parts of leveling agent, 10 parts of film-forming agent, 10 parts of curing agent, 21 parts of zeolite powder, and 28 parts of 45 μm hollow glass beads.
[0026] Wherein, the defoamer is defoamer JY-810, the leveling agent is AKN-UV1151, the film-forming agent is alcohol ester twelve, and the curing agent is epoxy powder coating curing agent EPH180.
[0027] A method for producing a graphene-based thermal insulation coating comprises the following steps: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass parts, the zeolite powder and hollow glass beads are added to 65 parts of water, and then 28 parts of hexadecyltrimethylammonium bromide are added, and stirred at 75° C. for 25 minutes without filtering to obtain modified zeolite powder containing liquid; Step 2: Mixing According to the mass fractions, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 15 minutes. Then, the leveling agent, film-forming agent, curing agent and defoaming agent are added in sequence, and the stirring time is 6 minutes between each raw material addition. Finally, stirring is performed for 25 minutes to obtain a graphene-based thermal insulation coating.
[0028] The thermal insulation coatings prepared in the above three embodiments and the control example were tested according to the TGZAS 009-2021 Thermal Insulation Coatings standard, where: The test results are shown in Table 1 below: Table 1: Test results As can be seen from Table 1, from the structures of the thermal insulation coatings prepared in Examples 1 to 3 and the control example, it can be seen that the thermal insulation coatings prepared in Examples 1 to 3 have better performance in all aspects than the control example.
[0029] The above is a preferred embodiment of the present invention, and it should be noted that for ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications are also considered as the protection scope of the present invention.
Claims
1. Graphene-based thermal insulation coatings, It is characterized in that The invention comprises the following components in parts by mass: 80-100 parts of epoxy resin, 10-12 parts of defoaming agent, 9-10 parts of leveling agent, 15-20 parts of graphene, 8-11 parts of film-forming agent, 9-11 parts of curing agent, 18-23 parts of zeolite powder and 25-31 parts of hollow glass beads.
2. The thermal insulation coating of Jiyu graphene according to claim 1, It is characterized in that The defoamer is defoamer JY-810.
3. The thermal insulation coating of Jiyu graphene according to claim 1, It is characterized in that The leveling agent is AKN-UV1151.
4. The thermal insulation coating of Jiyu graphene according to claim 1, It is characterized in that The film-forming agent is alcohol ester dodecahydrate.
5. The thermal insulation coating of Jiyu graphene according to claim 1, It is characterized in that The curing agent is epoxy powder coating curing agent EPH180.
6. The graphene-based thermal insulation coating according to claim 1, It is characterized in that The invention also includes 10 to 13 parts by weight of AKN-6000 adhesion promoter.
7. The method for producing the graphene-based thermal insulation coating according to claim 6, It is characterized in that The steps include: Step 1: Modified zeolite powder: S1. Mixing According to the mass fractions, zeolite powder and hollow glass beads are mixed evenly to obtain a mixture; S2. Modification According to the mass fractions, the zeolite powder and hollow glass beads are added to 60-70 parts of water, and then 25-30 parts of hexadecyltrimethylammonium bromide are added, and stirred at 70-80° C. for 20-30 minutes without filtering to obtain a modified zeolite powder containing a liquid; Step 2: Mixing According to the mass fraction, the modified zeolite powder containing liquid obtained in step 1 is added to the epoxy resin, and stirring is continued for 10 to 20 minutes. Then, the graphene, leveling agent, film-forming agent, curing agent, defoaming agent and AKN-6000 adhesion promoter are added in sequence, and the stirring time is 5 to 7 minutes between the addition of each raw material. Finally, stirring is performed for 20 to 30 minutes to obtain a graphene-based thermal insulation coating.
Citation Information
Patent Citations
Waterborne radiation type exterior wall coating
CN108570275A
High-temperature-resistant coating
CN108893036A
Glass bead, heavy anti-corrosion epoxy primer and preparation method of glass bead and heavy anti-corrosion epoxy primer
CN117603600A