Solid-free well killing fluid and preparation method thereof

By combining water, organic salt, inorganic salt and solubilizer in the solid-phase pressing fluid formula, the problems of unstable performance and high corrosion in the existing technology under high temperature and high pressure are solved, and the density is achieved Adjustable, low corrosion and environmentally friendly high temperature stability, suitable for deep well operations.

CN118931510APending Publication Date: 2024-11-12SICHUAN XINCHUANGNENG PETROLEUM ENG TECH CO LTD +2
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202410996198.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

The existing well pressing fluids have unstable performance under high temperature and high pressure conditions, and the commonly used halogen salt weighing agents lead to high corrosion, making it difficult to meet the operation requirements of deep wells or ultra-deep wells.

Method used

The solid-phase well pressing fluid formula is adopted, including a composite system of water, organic salt, inorganic salt and solubilizer. The density can be adjusted between 1.21 and 1.65g/cm3. The solubilizer is added to make the solubilizer micelle, thereby increasing the density. and stability, avoiding the use of solid phase admixture agent.

Benefits of technology

It achieves stable performance, low corrosion, adjustable density, low cost, environmentally friendly at 180℃, meets the requirements of deep well operation, and avoids pollution and corrosion damage to the formation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004960281780000041
    Figure BDA0004960281780000041
  • Figure BDA0004960281780000052
    Figure BDA0004960281780000052
  • Figure BDA0004960281780000061
    Figure BDA0004960281780000061
Patent Text Reader

Abstract

The invention belongs to the technical field of oil well industrial liquid, and discloses solid-free well killing fluid and a preparation method thereof. According to the solid-free well killing fluid, the raw materials are simple and easy to obtain, water serves as the base fluid, inorganic salt and organic salt are compounded, a small amount of solubilizer is added, the density of the solid-free well killing fluid can reach 1.65 g / cm < 3 >, the corrosion rate is as low as 0.043 mm / a, the solid-free well killing fluid can resist high temperature, and the performance of the solid-free well killing fluid can still be kept stable at 180 DEG C. And meanwhile, the inorganic salt does not contain bromide, and the system does not contain a solid-phase weighting agent, so that serious pollution and damage to the stratum are avoided. The well killing fluid has higher density, lower cost and corrosivity and more excellent high-temperature stability on the large premise of current environmental protection, and can meet the current deep well or ultra-deep well operation requirements.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of oil well industrial fluids, and in particular relates to a solid-free well killing fluid and a preparation method thereof, and specifically relates to a high-temperature resistant, low-corrosion solid-free high-density well killing fluid formula and a preparation method thereof. Background Art

[0002] Well killing is mainly to prevent the pressure of the liquid in the wellbore, such as the well killing fluid, from being lower than the pressure of the fluid in the formation during the well repair process, causing the fluid to flow into the wellbore, resulting in dangerous accidents such as well kicks or blowouts. During the well killing process, the relationship between the properties of the well killing fluid itself, the pressure of the well killing fluid column, and the bottom pore pressure becomes the main factor affecting the well killing effect.

[0003] At present, most well-killing fluids are water-based, mainly inorganic salt and organic salt systems. The density of domestic well-killing fluids is mostly only 1.50g / cm 3 Halogen salts (NaCl, CaCl2, MgCl2, NaBr, etc.) are commonly used as weighting agents, but halogen salts will significantly increase the corrosion of oil pipes and equipment, making it difficult to meet the requirements of well killing operations. Although the density of high-density cesium formate system well killing fluid can reach 1.80g / cm 3 The above methods are extremely expensive and difficult to promote. Therefore, weighted mud is often added during construction, but the addition of weighted mud will seriously damage the reservoir, and is not conducive to the corrosion control of the pipe string after completion, which prolongs the operation time. In addition, for deep wells or ultra-deep wells, there will be problems of high temperature and high pressure. The physical and chemical effects between the components of the clamping well-killing fluid under high temperature and high pressure affect the performance of the well-killing fluid, resulting in the inability to carry out the drilling project normally.

[0004] Therefore, it is an urgent need to develop a high-temperature resistant, low-corrosion, solid-free high-density drilling fluid, which is a technical problem that needs to be solved by technical personnel in this field. Summary of the invention

[0005] In view of this, the present invention provides a solid-free well killing fluid and a preparation method thereof.

[0006] In order to achieve the above object, the present invention adopts the following technical solution:

[0007] The first technical purpose of the present invention is to provide a solid-free well-killing fluid, wherein the solid-free well-killing fluid comprises the following raw materials in parts by weight:

[0008] 100 parts of water, 0-600 parts of organic salt, 0-500 parts of inorganic salt and 0-20 parts of solubilizer.

[0009] It should be noted that, in the raw material composition of the solid-free well-killing fluid, one of the organic salt and the inorganic salt must be added, that is, the weight parts of both cannot be 0 at the same time, but the solubilizer does not need to be added.

[0010] Optionally, the solid-free well killing fluid comprises the following raw materials in parts by weight:

[0011] 100 parts of water, 200-600 parts of organic salt, 20-200 parts of inorganic salt and 4-16 parts of solubilizer.

[0012] Furthermore, the solid-free well killing fluid comprises the following raw materials in parts by weight:

[0013] 100 parts of water, 4 parts of Tween solubilizer, 540 parts of organic salt and 32 parts of inorganic salt.

[0014] Furthermore, the organic salt is one or a combination of sodium formate, potassium formate, sodium lignin sulfonate, calcium lignin sulfonate, sodium acetate, potassium acetate, and calcium acetate;

[0015] The inorganic salt is one or a combination of NaCl, CaCl2, MgCl2, Ca(NO3)2, and ZnCl2;

[0016] The solubilizing agent is one or a combination of Tween-20, Tween-40, Tween-60, Tween-80, sodium lignin sulfonate, and calcium lignin sulfonate.

[0017] It should be noted that the present invention adds a surfactant with a solubilizing effect, which can make the hydrophilic chain segment wrap the solute, or make the solute enter the solubilizing agent micelle, so as to achieve the purpose of solubilization.

[0018] Moreover, the density of the solid-free well-killing fluid of the present invention is 1.21-1.65 g / cm 3 Adjustable, the density of the well-killing fluid can be adjusted by the weight of the weighting agent and the solubilizing agent. The density of the well-killing fluid can be controlled and adjusted according to the needs of different oil and gas wells.

[0019] The raw materials of the solid-free well-killing fluid of the present invention are simple and easy to obtain. It uses water as the base fluid, adopts inorganic salt and organic salt to compound, and then adds a small amount of solubilizing agent. Its density can reach 1.65g / cm 3 , and the corrosion rate is as low as 0.043mm / a, it can withstand high temperatures, and its performance can remain stable at 180°C. At the same time, the inorganic salt of the present invention does not contain bromide, and the system does not contain a solid phase weighting agent, which will not cause serious pollution and damage to the formation. The well-killing fluid of the present invention has higher density, lower cost and corrosiveness, and better high-temperature stability under the current environmental protection premise, and can meet the current deep well or ultra-deep well operation requirements.

[0020] The second technical purpose of the present invention is to provide a method for preparing the solid-free well killing fluid as described above, the method specifically comprising the following steps:

[0021] According to the required density of the drilling fluid, a solubilizer is added to water, and the solubilizer and water are fully mixed after stirring at 25°C for 30 minutes to form a homogeneous emulsion, and then an organic salt is added to obtain a base fluid; an inorganic salt weighting agent is compounded in the obtained base fluid and fully dissolved to obtain the solid-free drilling fluid.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] (1) The solid-free well-killing fluid of the present invention adopts a compound system of a solubilizing agent, an organic salt and an inorganic salt, and has good high-temperature stability, low corrosiveness and little formation damage.

[0024] (2) The formula of the present invention is a compound of organic salt and inorganic salt, with a density of 1.21-1.65 g / cm 3 It is adjustable within a certain range, and its corrosion resistance is very low at high density, with the lowest corrosion rate reaching 0.043mm / a, which largely avoids the high corrosion of halogen salts.

[0025] (3) The solid-free well-killing fluid of the present invention can withstand high temperatures up to 180°C. After aging at 180°C, its density, viscosity, and precipitation-free properties do not change significantly.

[0026] (4) The present invention does not use expensive weighting agents such as cesium formate, nor does it use bromide weighting agents that cause significant environmental pollution. It is low-cost and has excellent environmental friendliness. DETAILED DESCRIPTION

[0027] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] The word "embodiment" used here as an "exemplary" does not necessarily mean that any embodiment described is superior to or better than other embodiments. Unless otherwise specified, the performance index tests in the embodiments of this application are performed using conventional test methods in the art. It should be understood that the terms described in this application are only used to describe specific implementation methods and are not used to limit the content disclosed in this application.

[0029] Unless otherwise specified, the technical and scientific terms used in this document have the same meanings as commonly understood by ordinary technicians in the technical field to which this application belongs; other experimental methods and technical means not specifically specified in this application refer to experimental methods and technical means commonly used by ordinary technicians in this field.

[0030] In order to better illustrate the content of the present application, numerous specific details are provided in the specific examples below. It should be understood by those skilled in the art that the present application can also be implemented without certain specific details. In the embodiments, some methods, means, instruments, equipment, etc. well known to those skilled in the art are not described in detail in order to highlight the main purpose of the present application.

[0031] Under the premise of no conflict, the technical features disclosed in the embodiments of the present application can be combined arbitrarily, and the resulting technical solutions belong to the contents disclosed in the embodiments of the present application.

[0032] The invention discloses a solid-phase-free well-killing fluid and a preparation method thereof.

[0033] In order to better understand the present invention, the present invention is further specifically described below through the following examples, but it should not be understood as a limitation of the present invention. Some non-essential improvements and adjustments made by technicians in this field based on the above invention content are also considered to fall within the protection scope of the present invention.

[0034] The present invention adds a certain amount of solubilizer into water, stirs for 30 minutes at 25°C to fully mix the solubilizer and water to form a homogeneous emulsion, then adds an organic salt mixture (one or more of potassium formate, sodium formate, potassium acetate, and sodium acetate) and an inorganic salt mixture (one or more of NaCl, CaCl2, MgCl2, Ca(NO3)2, and ZnCl2) to fully dissolve and then test the density.

[0035] The density test method is as follows:

[0036] According to 4.3.3 density meter method in GB / T 4472-2011, the measurement temperature is 20℃. The specific steps are as follows:

[0037] 1) Determination at a constant temperature of (20±0.1)℃: Inject the sample to be tested into a clean, dry measuring cylinder without bubbles, and place the measuring cylinder in a constant temperature water bath at (20±0.1)℃. After the temperature is constant, slowly place a clean and dry densitometer into the sample, with its lower end at least 2 cm away from the bottom of the cylinder and not in contact with the cylinder wall. The upper end of the densitometer exposed outside the liquid surface should not be exposed to more than (2-3) scales of liquid. After the densitometer is stable in the liquid, read the scale at the lower edge of the meniscus of the densitometer (except for the densitometer marked with the upper edge of the meniscus), which is the density of the sample at 20℃.

[0038] 2) Determination at room temperature: When the temperature of the sample is consistent with room temperature, perform the above operation at room temperature.

[0039] 3) Test results

[0040] ① Determine the density ρ of the sample at room temperature t℃ t , grams per cubic centimeter (g / cm 3 ) is expressed as follows:

[0041] ρ t =ρ t +ρ t ×α(20-t)

[0042] Where:

[0043] ρ t ——The density meter reading of the sample at t℃, in grams per cubic centimeter (g / cm 3 );

[0044] α——Glass expansion coefficient of the density meter, generally 0.000025;

[0045] 20——Standard temperature of the density meter, in degrees Celsius (℃);

[0046] t——Temperature during measurement, in degrees Celsius (℃).

[0047] ②Measure the density ρ of the sample at room temperature t℃ t Density converted to 20℃ 20 , grams per cubic centimeter (g / cm 3 ) is expressed as follows:

[0048] ρ 20 =ρ t +k×(t-20)

[0049] Where:

[0050] k – Temperature correction coefficient of sample density (can be obtained by looking up a table or by actual measurement of different liquid chemical products).

[0051] Example 1

[0052] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0053] 100 parts of water, 0.5 parts of calcium lignin sulfonate, a certain amount of organic salt (potassium formate) (specific weight parts are shown in the table below). Add the lignin solubilizer to the water, stir thoroughly to dissolve, then add the organic salt and inorganic salt, stir thoroughly to dissolve, and then test its density. The test results are shown in the table below:

[0054] water Lignin solubilizer Potassium formate Inorganic salt <![CDATA[Density (g / cm 3 )]]> 100 copies 0.5 serving 78 servings 0 copies 1.28 100 copies 0.5 serving 114 copies 0 copies 1.36 100 copies 0.5 serving 225 copies 0 copies 1.50 100 copies 0.5 serving 322 copies 0 copies 1.56 100 copies 0.5 serving 400 copies 0 copies 1.60

[0055] Example 2

[0056] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0057] 100 parts of water, 4 parts of calcium lignin sulfonate, a certain amount of organic salt (potassium formate) (specific weight parts are shown in the table below). Add the lignin solubilizer to the water, stir thoroughly to dissolve, then add the organic salt and inorganic salt, stir thoroughly to dissolve, and then test its density. The test results are shown in the table below:

[0058]

[0059]

[0060] Example 3

[0061] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0062] 100 parts of water, 0.5 parts of Tween-40, a certain amount of organic salt (potassium formate) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the following table:

[0063] water Tween solubilizer Sodium formate Inorganic salt <![CDATA[Density (g / cm 3 )]]> 100 copies 0.5 serving 51 copies 0 copies 1.21 100 copies 0.5 serving 103 copies 0 copies 1.32 100 copies 0.5 serving 182 copies 0 copies 1.45 100 copies 0.5 serving 230 copies 0 copies 1.50 100 copies 0.5 serving 324 copies 0 copies 1.57

[0064] Example 4

[0065] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0066] 100 parts of water, 4 parts of Tween-60, a certain amount of organic salt (potassium formate) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the table below:

[0067] water Tween solubilizer Potassium formate Inorganic salt <![CDATA[Density (g / cm 3 )]]> 100 copies 4 servings 57 copies 0 copies 1.21 100 copies 4 servings 124 copies 0 copies 1.38 100 copies 4 servings 205 copies 0 copies 1.49 100 copies 4 servings 299 copies 0 copies 1.55 100 copies 4 servings 406 copies 0 copies 1.60

[0068] Example 5

[0069] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0070] 100 parts of water, 16 parts of Tween-20, a certain amount of organic salt (potassium formate) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the table below:

[0071]

[0072]

[0073] Example 6

[0074] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0075] 100 parts of water, 4 parts of Tween-80, a certain amount of organic salt (potassium formate) and inorganic salt (Ca(NO3)2) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the table below:

[0076] water Tween solubilizer Potassium formate Calcium Nitrate <![CDATA[Density (g / cm 3 )]]> 100 copies 4 servings 60 servings 20 servings 1.28 100 copies 4 servings 120 servings 20 servings 1.40 100 copies 4 servings 305 copies 20 servings 1.58 100 copies 4 servings 368 copies 20 servings 1.60 100 copies 4 servings 423 copies 20 servings 1.64

[0077] Example 7

[0078] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0079] 100 parts of water, 4 parts of Tween-20, a certain amount of organic salt (potassium formate) and inorganic salt (Ca(NO3)2) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the table below:

[0080] water Tween solubilizer Potassium formate Calcium Nitrate <![CDATA[Density (g / cm 3 )]]> 100 copies 4 servings 60 servings 32 servings 1.28 100 copies 4 servings 121 copies 32 servings 1.40 100 copies 4 servings 307 copies 32 servings 1.57 100 copies 4 servings 368 copies 32 servings 1.60 100 copies 4 servings 537 copies 32 servings 1.65

[0081] Example 8

[0082] A high-temperature-resistant, low-corrosion, solid-phase-free, high-density well-killing fluid comprises the following raw materials in parts by weight:

[0083] 100 parts of water, 4 parts of Tween-40, a certain amount of organic salt (potassium formate) and inorganic salt (Ca(NO3)2) (specific weight parts are shown in the table below). Add the Tween solubilizer to the water, stir thoroughly, add the organic salt and inorganic salt, stir and dissolve, and test its density. The test results are shown in the table below:

[0084]

[0085]

[0086] In order to further demonstrate the beneficial effects of the present invention and to better understand the present invention, the following comparative examples are used to further illustrate the technical features disclosed in the present invention, but they should not be construed as limiting the present invention. Other improvements made by those skilled in the art based on the above invention content without inventive work are also considered to fall within the scope of protection of the present invention.

[0087] Comparative Example 1

[0088] Without adding solubilizer, only organic salt and inorganic salt are added into water in different proportions to dissolve. The test results are shown in the following table.

[0089] water Solubilizer Sodium formate Calcium chloride <![CDATA[Density (g / cm 3 )]]> 100 copies 0 copies 25 servings 20 servings 1.15 100 copies 0 copies 36 servings 20 servings 1.20 100 copies 0 copies 58 servings 20 servings 1.25 100 copies 0 copies 78 servings 20 servings 1.30

[0090] Comparative Example 2

[0091] Without adding solubilizer, only organic salt and inorganic salt are added into water in different proportions to dissolve. The test results are shown in the following table.

[0092] water Solubilizer Sodium formate Magnesium chloride <![CDATA[Density (g / cm 3 )]]> 100 copies 0 copies 60 servings 8 servings 1.30 100 copies 0 copies 90 servings 12 servings 1.30 100 copies 0 copies 85 copies 0 copies 1.40 100 copies 0 copies 130 copies 0 copies 1.45

[0093] Comparative Example 3

[0094] Take halide or potassium formate, sodium formate as weighting agent, add it into 100 parts of water and fully dissolve it. The test results of the saturated solution density are as follows:

[0095] <![CDATA[Ca(NO3)2]]> Potassium formate Sodium formate <![CDATA[Density (g / cm 3 )]]> 1.44 1.40 1.30

[0096] Corrosion rate determination: In the present invention, the corrosion rate test was performed on the sample with the highest density in the embodiment and the comparative example, and the test method was as follows:

[0097] Wipe the P110SS test piece with filter paper first, then put it into a container filled with acetone, remove the grease on the surface of the test piece with absorbent cotton, and then soak it in anhydrous ethanol for about 5 minutes for further degreasing and dehydration. Take out the test piece and place it on the filter paper, blow it dry with cold air, then wrap the test piece with filter paper, store it in a desiccator, and measure the size and mass after leaving it for 1 hour, with an accuracy of 0.1mg.

[0098] Fix the test piece on the hanging piece rack and then put it into the high temperature and high pressure aging tank. At least two parallel samples are made for each test group, and three test pieces are hung in each parallel test container. The test piece is not allowed to contact the container wall, and the distance between the test pieces should be more than 1cm.

[0099] According to the liquid volume of 20mL per square centimeter of the test piece surface area, a sufficient amount of annular protection liquid sample is injected into the high temperature and high pressure aging tank, and the upper end of the test piece should be more than 3cm away from the liquid surface. Nitrogen is injected into the aging tank using a pressurizing device until the pressure in the tank is not less than 1MPa, the aging tank is moved into the oven, heated to the test temperature, and the timing is started. The experimental time is 48h.

[0100] After the reaction reaches the preset time, cut off the power supply, wait for the aging tank to cool to room temperature and completely release the pressure, open the tank and take out the test piece, observe the corrosion condition and make detailed records. After observation, rinse the test piece with water immediately, then brush it with a soft brush; finally, wash each piece with acetone and anhydrous ethanol, wipe it dry with filter paper and continue to blow it dry with cold air, dry it in a dryer for 1 hour, and then weigh it with an accuracy of 0.1mg. Calculate the corrosion rate based on the mass difference before and after corrosion.

[0101] For corrosion rate calculation, the difference between parallel determination values ​​shall not exceed 6%, and the numerical rounding shall be carried out in accordance with GB / T 8170.

[0102]

[0103] Where:

[0104] r—uniform corrosion rate, mm / a;

[0105] m—mass of the test piece before the test, g;

[0106] mt—mass of the test piece after the test, g;

[0107] S—total area of ​​the test piece, cm 2 ;

[0108] t—test time, h;

[0109] ρ—density of the test piece material, g / cm 3 .

[0110] Thermal stability test: In the present invention, the thermal stability test was performed on the samples with the highest density in the embodiments and comparative examples. The test method is as follows:

[0111] 1) Appearance

[0112] The well-killing fluid is loaded into an aging tank and placed in a roller heating furnace at a constant temperature of 120°C for 24 hours. After cooling to room temperature, the sample is poured into a glass beaker for observation. The appearance should have no obvious change from that before heating.

[0113] 2) Density after 24h heat resistance

[0114] Take 350mL of well-killing fluid sample, measure its initial density at 20℃, put it into a roller heating furnace at 180℃ for 24h, cool it to 20℃ and measure the density again. The determination method is carried out according to 9.3.2. The density change rate is calculated as follows:

[0115]

[0116] Where:

[0117] D——density change rate, %;

[0118] ρ——initial density, g / cm3

[0119] ρ1——density after 24h heat resistance, g / cm 3 .

[0120] Core damage rate test: In the present invention, the core damage rate test is performed on the sample with the highest density in the embodiment and the comparative example, and the test method is as follows:

[0121] The original permeability of the core and the permeability of the core damaged by the killing fluid were measured at room temperature using a core intelligent flow gradient meter, and the core damage rate of the killing fluid was calculated.

[0122] According to 8.1~8.5 of SY / T6540-2002, the permeability before and after core damage was measured respectively, and the core damage rate was calculated according to the following formula.

[0123]

[0124] Where:

[0125] D k ——Core penetration damage rate, %;

[0126] K1——core permeability after well killing fluid damage, 10 -3 μm 2 ;

[0127] K0——core permeability before killing fluid damage, 10 -3 μm 2 .

[0128] The specific test results are shown in the following table:

[0129] <![CDATA[Density (g / cm 3 )]]> Corrosion rate (mm / a) Density change rate % Core damage rate % Example 1 1.60 0.036 0.25 8.7 Example 2 1.60 0.047 0.31 7.6 Example 3 1.57 0.051 0.19 4.9 Example 4 1.60 0.039 0.18 6.5 Example 5 1.61 0.041 0.12 5.1 Example 6 1.64 0.042 0.18 5.8 Example 7 1.65 0.036 0.18 5.2 Example 8 1.57 0.043 0.12 4.6 Comparative Example 1 1.30 0.102 0.46 12.3 Comparative Example 2 1.45 0.072 0.34 9.6 Comparative Example 3 1.40 0.065 0.4 10.2

[0130] By comparing Example 1 with Example 2, it can be seen that increasing the amount of lignin solubilizer added has little effect on the increase in the density of the organic salt solution, and solubilization can be achieved by adding a small amount; the experimental results of Example 1 and Comparative Example 3 show that after adding the lignin solubilizer, the organic salt solubilization effect is very good, and the density can be increased from 1.40 g / cm 3 Increased to 1.60g / cm 3 Comparison of Example 3, Example 4, and Example 5 shows that increasing the amount of Tween-type solubilizer added can greatly increase the solubility and increase the density to 1.61 g / cm 3 Comparative Examples 3 to 7 show that the solution density can be increased to 1.64 g / cm by compounding inorganic and organic salts with Tween-type solubilizers. 3 Comparing Example 8 with Comparative Example 3, it is found that the solubilizing effect of Tween-type solubilizers on inorganic salts is also very obvious, reaching 1.65g / cm3 In addition, the experimental results of Comparative Examples 1 and 2 show that without using a solubilizing agent, the solubility of inorganic salts and organic salts in the system is much lower than that of Examples 1 to 8. This shows that the use of a solubilizing agent in the present invention can significantly improve the density of the solid-free well-killing fluid.

[0131] In addition, the performance test of the well killing fluid shows that the density can reach 1.65g / cm by compounding inorganic salts and organic salts and adding a small amount of solubilizer. 3 , and the density does not change much at 180°C, the corrosion rate is as low as 0.043mm / a, which is lower than the general requirement of 0.076mm / a, and will not cause serious pollution and damage to the formation. The core damage rate is 15% lower than the general requirement. The well-killing fluid of the present invention has higher density, lower cost and corrosiveness, and better high-temperature stability under the current environmental protection premise, and can meet the current deep well or ultra-deep well operation requirements.

[0132] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A solid-free well killing fluid, It is characterized in that The solid-free well killing fluid comprises the following raw materials in parts by weight: 100 parts of water, 0-600 parts of organic salt, 0-500 parts of inorganic salt and 0-20 parts of solubilizer.

2. The solid-free well killing fluid according to claim 1, It is characterized in that The solid-free well killing fluid comprises the following raw materials in parts by weight: 100 parts of water, 200-600 parts of organic salt, 20-200 parts of inorganic salt and 4-16 parts of solubilizer.

3. The solid-free well killing fluid according to claim 1 or 2, It is characterized in that The organic salt is one or a combination of sodium formate, potassium formate, sodium lignin sulfonate, calcium lignin sulfonate, sodium acetate, potassium acetate, and calcium acetate; The inorganic salt is NaCl, CaCl 2 MgCl 2 、Ca(NO 3 ) 2 、ZnCl 2 One or a combination of the following: The solubilizing agent is one or a combination of Tween-20, Tween-40, Tween-60, Tween-80, sodium lignin sulfonate, and calcium lignin sulfonate.

4. A method for preparing a solid-free well killing fluid as claimed in claim 1 or 2, It is characterized in that The method specifically comprises the following steps: A solubilizer is added to water, and the solubilizer and water are fully mixed after stirring at 25°C for 30 minutes to form a homogeneous emulsion, and then an organic salt is added to obtain a base liquid; an inorganic salt is compounded in the obtained base liquid and fully dissolved to obtain the solid-free well-killing fluid.

Citation Information

Cited By

  • Solid-free well killing fluid and preparation method thereof

    CN121652773A

  • A solid-free kill fluid and a preparation method thereof

    CN121652773B