Preparation method of microporous copper foil
In the preparation of microporous copper foil by electrochemical etching, the problems of complex equipment and low efficiency of traditional methods are solved, and the process is simplified and the preparation of microporous copper foil is achieved, which is suitable for a variety of microporous metal materials.
Patent Information
- Application Number
- CN202410992766.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-23
- Publication Date
- 2024-11-12
AI Technical Summary
The existing microporous copper foil preparation method adopts traditional mechanical processing and chemical etching. The equipment is complex, the operation is complex, the preparation efficiency is low, and multiple steps and a large number of chemical agents are required.
By electrochemical etching, by applying a polymer solution to the surface of copper foil, applying current to allow positive ions in the electrolyte to pass through the polymer gap to form holes, and controlling the polymer species, molecular weight, electrolyte composition and current density to A uniform and controllable micropore structure is obtained.
The preparation process is simplified and the production efficiency is improved. The obtained microporous copper foil has a uniform and controllable pore size and an accurate pore structure, while maintaining the performance of the original copper foil, which is suitable for the preparation of other microporous metal materials.
Smart Images

Figure CN118932471A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of microporous copper foil, in particular to a preparation method of microporous copper foil. Background Art
[0002] Microporous copper foil is a secondary process based on the original copper foil, and holes are made by mechanical processing or other processing methods. This material has important applications in manufacturing. The through-hole diameter of microporous copper foil is small, and the depth-to-diameter ratio is controlled within a certain range. This structure gives it unique performance advantages in specific applications. With copper foil as the substrate, it ensures its good conductivity and ductility. In the field of lithium batteries, microporous copper foil can significantly improve the rate performance of lithium batteries, reduce internal resistance, and improve electrolyte infiltration efficiency through laser drilling and other methods, thereby improving the overall performance of lithium batteries. For foils of the same specifications, increased porosity can significantly reduce weight, which helps to improve the portability and endurance of electronic products. The microporous structure makes the migration path of lithium ions more complicated, but at the same time it also increases the contact area between the negative electrode material and the foil, thereby reducing the migration radius of lithium ions and improving the conductivity efficiency. The production process of microporous copper foil mainly includes two steps: copper foil preparation and microporous processing. Copper foil is usually prepared by electrolysis or calendering, while microporous processing may use a variety of methods such as laser drilling and chemical corrosion. Laser drilling is widely used due to its advantages such as high production efficiency and good processing accuracy. With the continuous development and popularization of high-end electronic products, the demand for high-performance materials such as microporous copper foil is also growing. In the future, with the continuous advancement of production technology and the reduction of costs, microporous copper foil is expected to be applied and promoted in more fields such as electromagnetic shielding. In summary, as a material with unique structure and excellent performance, microporous copper foil has important applications in the manufacture of batteries, supercapacitors, and electromagnetic shielding. With the continuous development of related technologies and the continuous expansion of the market, the market prospects of microporous copper foil are very broad.
[0003] The prior art method for preparing microporous copper foil adopts traditional mechanical processing and chemical etching methods, which have numerous and complex equipment, require multi-step processing and the use of a large amount of chemical agents, are complicated and troublesome to operate, and have low preparation efficiency. To address this problem, a method for preparing microporous copper foil is provided. Summary of the invention
[0004] The purpose of the present invention is to provide a method for preparing a microporous copper foil to solve the problems raised in the above background technology. To achieve the above purpose, the present invention provides the following technical solution: A method for preparing a microporous copper foil, comprising the following steps:
[0005] Step 1: Applying polymer solution I on the surface of copper foil II, and after the solvent evaporates, forming polymer-covered copper foil III;
[0006] Step 2, immersing the copper foil III prepared in step 1 as an anode into an electrolyte IV, and another inert conductive electrode V as a cathode to form an electrolytic cell with a power source and the electrolyte VI;
[0007] Step three, using the device shown in step two, apply current to the copper foil electrode III and the V electrode, and maintain for a certain period of time. After the reaction is completed, take out the copper foil electrode III, clean the surface, and dry it to obtain a microporous copper foil product VIII.
[0008] Preferably, the polymer in the polymer solution I is a water-soluble or oil-soluble polymer, which is one or more of sodium carboxymethyl cellulose, polyvinyl pyrrolidone, cellulose acetate, cellulose ether, starch, polyvinyl alcohol, polyacrylate, polyethylene glycol, gelatin, carboxymethyl chitosan, polyacrylamide, polyacrylic acid, xanthan gum, poly(3,4-ethylenedioxythiophene) poly(styrene sulfonate), polymerized vinyl sulfonic acid, polyacrylamide, polyaniline, polyimide, and polymethyl methacrylate.
[0009] Preferably, the copper foil II is electrolytic copper foil or rolled copper foil.
[0010] Preferably, the electrode V is one of platinum, carbon, titanium, stainless steel, copper, platinum, gold, silver and nickel.
[0011] Preferably, the electrolyte VI is one or more of sodium chloride, potassium perchlorate, potassium sulfate, copper chloride, copper sulfate, sodium carbonate, ammonium nitrate, ammonium bicarbonate, and ferric chloride.
[0012] Preferably, the concentration of the electrolyte is 0.01 mol / L-5 mol / L.
[0013] Preferably, the electrolysis current in step three is 0.01A / dm2-100A / dm2.
[0014] Preferably, the electrolysis temperature in step three is 20-85°C.
[0015] Preferably, the electrolysis time in step three is 1s-60min.
[0016] Preferably, the microporous copper foil product VIII has a micropore size of 0-150 μm, including blind holes and through holes.
[0017] Compared with the prior art, the present invention has the following beneficial effects:
[0018] By applying an external current or voltage to the copper foil electrode III, the positive ions in the electrolyte are forced to pass through the tiny gaps of the polymer to reach the copper surface, and form a path with the electrons in the external circuit for electrochemical etching reaction to form holes; the area with good polymer coverage maintains the original copper foil surface state. By controlling the type of polymer, molecular weight, coating thickness, electrolyte composition, temperature, current density and electrolysis time, microporous copper foils with different pore sizes and pore structures can be obtained. The method of the present invention is simple and convenient to operate, and has strong practicality. The obtained microporous copper foil material has a uniform and controllable pore size and a precise pore structure, and maintains the performance of the original copper foil material. The method uses electrochemical etching to prepare microporous copper foil, which is simple to operate, overcomes the use of complex equipment, multiple steps and a large amount of chemicals in traditional mechanical processing and chemical etching methods, and significantly improves production efficiency. The method is also applicable to the production and preparation of other microporous metal materials such as steel, nickel, iron-nickel alloy, tin, titanium, aluminum and their alloy foils. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 A flowchart of a method for preparing a microporous copper foil according to the present invention;
[0020] Figure 2 The present invention provides a method for preparing a microporous copper foil and a scanning electron microscope image. DETAILED DESCRIPTION
[0021] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technical personnel in this field without creative work are within the scope of protection of the present invention.
[0022] See also Figure 1 The present invention provides a technical solution: a method for preparing a microporous copper foil, comprising the following steps:
[0023] Step 1: Applying polymer solution I on the surface of copper foil II, and after the solvent evaporates, forming polymer-covered copper foil III;
[0024] Step 2: immerse the copper foil III prepared in step 1 as an anode into the electrolyte IV, and another inert conductive electrode V as a cathode to form an electrolytic cell with a power source and the electrolyte VI;
[0025] Step 3, using the device shown in step 2, applying current to the copper foil electrode III and the V electrode, maintaining for a certain period of time, after the reaction is completed, taking out the copper foil electrode III, cleaning the surface, and drying it to obtain a microporous copper foil product VIII;
[0026] By applying an external current or voltage to the copper foil electrode III, the positive ions in the electrolyte are forced to pass through the tiny gaps in the polymer to reach the copper surface, forming a path with the electrons in the external circuit for electrochemical etching reaction to form holes; the area with good polymer coverage maintains the original copper foil surface state, and by controlling the polymer type, molecular weight, coating thickness, as well as the electrolyte composition, temperature, current density and electrolysis time, microporous copper foils with different pore sizes and pore structures can be obtained. The method of the present invention is simple and convenient to operate and has strong practicality. The obtained microporous copper foil material has a uniform and controllable pore size and a precise pore structure, and maintains the performance of the original copper foil material. The method uses electrochemical etching to prepare microporous copper foil, which is simple to operate and overcomes the use of complex equipment, multiple steps and a large amount of chemicals in traditional mechanical processing and chemical etching methods, and significantly improves production efficiency. The method is also applicable to the production and preparation of other microporous metal materials such as steel, nickel, iron-nickel alloy, tin, titanium, aluminum and their alloy foils.
[0027] In this embodiment, the polymer in the polymer solution I is a water-soluble or oil-soluble polymer. The water-soluble polymer, also known as a water-soluble resin or a water-soluble high molecular compound, is a high molecular material with special hydrophilicity. Its molecular structure contains a large number of hydrophilic groups (such as cationic groups, anionic groups, polar non-ionic groups), so it can dissolve or swell in water to form an aqueous solution or a dispersed system. The water-soluble polymer has multifunctionality and broad application prospects. It can control the viscosity and rheological properties of the solution, suspend solid particles, change the properties of the solid interface, and can be used as a conditioner, excipient, film-forming agent, etc. The preparation of the water-soluble polymer is mainly obtained by homopolymerization, copolymerization or grafting in a free radical manner. For example, polyacrylamide, polypropylene, etc. are synthesized by monomer homopolymerization; hydrophilic monomers are introduced by copolymerization to make the polymer water-soluble; or hydration groups are introduced by group reactions of the macromolecules themselves, etc., oil-soluble polymers Oil-soluble polymers refer to polymer materials that can dissolve or swell in the oil phase. They usually have a non-polar or weakly polar molecular structure and have good compatibility with oils. Oil-soluble polymers can form a stable dispersion system in the oil phase to improve the viscosity, stability and other physical properties of the oil. They can also be used as thickeners, emulsifiers, lubricants, etc. There are various methods for preparing oil-soluble polymers, including solution polymerization, emulsion polymerization, suspension polymerization, etc. The specific preparation method depends on the type and performance requirements of the required polymer, which is one or more of sodium carboxymethyl cellulose, polyvinyl pyrrolidone, cellulose acetate, cellulose ether, starch, polyvinyl alcohol, polyacrylate, polyethylene glycol, gelatin, carboxymethyl chitosan, polyacrylamide, polyacrylic acid, xanthan gum, poly(3,4-ethylenedioxythiophene) poly(styrene sulfonate), polymerized ethylene sulfonic acid, polyacrylamide, polyaniline, polyimide, and polymethyl methacrylate.
[0028] In this embodiment, copper foil II is electrolytic copper foil or rolled copper foil. Electrolytic copper foil is a product made by copper electrolysis using electrochemical principles. Its production process mainly includes solution foil production, surface treatment and product slitting. The production process of electrolytic copper foil seems simple, but it actually integrates electronics, mechanics and electrochemistry, and has particularly strict requirements on the production environment. The internal structure of electrolytic copper foil is a vertical needle-shaped crystal structure, and the production cost is relatively low. Rolled copper foil is a product made by repeatedly rolling and annealing a high-precision copper strip (thickness is usually less than 150 microns) using the principle of plastic processing. Its internal structure is a lamellar crystal structure, and its ductility, bending resistance and conductivity are better than those of electrolytic copper foil, and its copper purity is also higher than that of electrolytic copper foil. The production process of rolled copper foil is complicated, the process is long, and the equipment precision requirements are high. The following table is a performance comparison table of electrolytic copper foil and rolled copper foil:
[0029]
[0030]
[0032] In this embodiment, the electrode V is one of platinum, carbon, titanium, stainless steel, copper, platinum, gold, silver, nickel or their alloys. Platinum is an excellent conductor with stable thermoelectric properties. Among all metal elements, dense platinum group metals have the best oxidation resistance and corrosion resistance. Platinum is basically inert in common single acids and alkalis, and has a high degree of corrosion resistance. Platinum has good ductility, but the processing cost is high. Platinum is a rare and precious metal with high price. It is mainly used in high-end fields such as jewelry and catalysts. Carbon conductive fillers such as graphite have good conductivity, but the conductivity may vary depending on the material form and purity. Carbon materials have good chemical stability under normal conditions, but may be affected by certain strong oxidants or acid-base environments. The mechanical strength of carbon materials varies depending on the specific form (such as graphite, carbon fiber, etc.), but generally have good wear resistance and corrosion resistance. The price of carbon materials is relatively low and the source is wide. The conductivity of titanium is relatively general, not as good as silver, copper and other metals. Titanium is a very active metal, but it is easy to form a dense oxide film on its surface, so it has good corrosion resistance and oxidation resistance. Titanium has high mechanical strength and is a representative of lightweight and high-strength materials. The price of titanium is relatively high, but it is widely used in aerospace, medical and other fields due to its excellent performance. Although the conductivity of stainless steel is not as good as pure metals such as silver and copper, it is still a good conductive material among metal alloys. Stainless steel contains chromium, nickel and other elements, forming a strong chromium oxide film on the surface of the alloy, which has excellent corrosion resistance and oxidation resistance. Stainless steel has high mechanical strength and rigidity, is easy to process and form, and has a relatively moderate price, which is widely used in various fields. Copper is an excellent conductor, and its conductivity is second only to silver. Copper has good chemical stability under normal conditions, but it is easy to be oxidized, so the conductivity stability may be affected. Copper has good ductility and machinability. The price of copper is relatively low, and it is one of the widely used conductive materials. Gold is an excellent conductor, but its conductivity is usually not its main application point. Gold has extremely high chemical stability and hardly reacts chemically with any substance. Gold has good ductility and plasticity. Gold is one of the rare and precious metals, and its price is high. It is mainly used in high-end fields such as jewelry and investment. Silver is one of the metals with the best conductivity and is widely used in the electronic and electrical industry. Silver has good chemical stability under normal conditions, but it may be corroded by long-term exposure to humid or sulfur-containing environments. It has good ductility and machinability. The price of silver is relatively high, but it is widely used because of its excellent conductivity. Nickel has good conductivity, with an electrical conductivity of 12.9S / m. Nickel has excellent corrosion resistance, oxidation resistance and electromagnetic interference resistance. Nickel does not oxidize in the air and still does not oxidize when heated to 700-800℃. Nickel has good mechanical strength and ductility. Nickel is moderately priced and is widely used in stainless steel manufacturing, electroplating and other fields.In summary, different electrode materials have their own characteristics in terms of conductivity, chemical stability, mechanical strength and cost. When selecting electrode materials, it is necessary to make comprehensive considerations based on specific application scenarios and needs.
[0033] In this embodiment, the electrolyte VI is one or more of sodium chloride, potassium perchlorate, potassium sulfate, copper chloride, copper sulfate, sodium carbonate, ammonium nitrate, ammonium bicarbonate, and ferric chloride.
[0034] In this embodiment, the concentration of the electrolyte is 0.01mol / L-5mol / L. By adding an appropriate amount of solvent (such as distilled water) or solute (such as chemical reagent) to the electrolyte, the volume or solute content of the electrolyte can be changed, thereby adjusting its concentration. For scenarios where the viscosity of the electrolyte needs to be increased, an appropriate amount of thickener (such as silica gel, carboxymethyl cellulose, etc.) can be added, but it is necessary to control the amount and order of addition to avoid affecting the stability of the electrolyte and the processing effect. In some cases, the pH value of the electrolyte can also indirectly affect the viscosity and reaction efficiency of the electrolyte. For example, in the electrolytic processing of stainless steel, the pH value of the electrolyte can be adjusted by appropriately adding alkaline substances (such as sodium hydroxide), thereby achieving the effect of adjusting the concentration.
[0035] In the present embodiment, the electrolysis current in step 3 is 0.01A / dm2-100 A / dm2, and the electrolysis current density (usually in A / dm 2 The electrolytic current density (in units) is an important parameter in the electrolysis process. It reflects the current intensity passing through a unit area. The size of the electrolytic current density directly affects the speed, efficiency, and quality and output of the electrolytic reaction. The larger the electrolytic current density, the more charge passes through the electrolyte per unit time, thereby accelerating the speed of the electrolytic reaction. The current density has a certain influence on the crystal morphology, purity, and particle size of the product. In some cases, too high a current density may lead to a decrease in product quality, such as the generation of dendrites, powderization, and other adverse phenomena. Although increasing the current density can speed up the reaction, it will also increase energy consumption, because the electrolysis process requires electrical energy to drive the migration of ions in the electrolyte and the redox reaction on the electrode. Too high a current density may cause the electrode to overheat, corrode or passivate, thereby affecting the stability and life of the electrolysis process.
[0036] In this embodiment, the electrolysis temperature in step 3 is 20-85°C. The electrolysis temperature is the temperature of the electrolyte during the electrolysis production process. It has an important influence on the progress of the electrolysis reaction, the quality and output of the product, and the life of the electrolysis equipment. The specific range of the electrolysis temperature depends on the type of electrolyte, the characteristics of the electrolysis reaction, and the production requirements. Taking aluminum electrolysis as an example, the temperature of the electrolytic cell is generally about 945-965°C, and the electrolyte temperature is about 15-20°C higher than the primary crystallization temperature. This is because the electrolyte composition determines the primary crystallization temperature of the electrolyte, and the electrolysis temperature usually needs to exceed the primary crystallization temperature by a certain range to maintain normal electrolysis production. In addition to being related to the voltage drop between the electrodes, the electrolysis temperature mainly depends on the melting point of the electrolyte. The lower the melting point of the electrolyte, the lower the required electrolysis temperature. Therefore, in the electrolysis process, the electrolyte composition is usually adjusted to reduce its melting point, thereby reducing the electrolysis temperature and reducing energy consumption. Different electrolysis reactions have different temperature requirements. Some reactions require higher temperatures to proceed smoothly, while some reactions can proceed at lower temperatures. To achieve better results, the temperature of the electrolyte is adjusted by controlling the water cooling or air cooling device of the electrolytic cell. This method has low cost, but the temperature control accuracy is low and it is easily affected by the external environment. A temperature sensor is installed during the electrolysis process, and the temperature of the electrolyte is controlled by processing the signal output by the sensor. This method has higher accuracy and better stability. The method of continuously adjusting the temperature signal using proportional, integral, and differential operations is based on the temperature error and continuously adjusts the output result to achieve the purpose of controlling the temperature. The PID control method is simple to operate, has high accuracy and good stability, and is widely used in electrolytic processing, electrochemical corrosion and other fields. The electrolytic temperature has an important influence on the progress of the electrolytic reaction, the quality and output of the product, and the life of the electrolytic equipment. If the electrolytic temperature is too high or too low, the electrolytic reaction may not proceed or the product quality may decrease. At the same time, changes in the electrolytic temperature will also cause changes in other technical parameters, such as current efficiency, cell voltage, etc., thereby affecting the stability and economy of the entire electrolytic process.
[0037] In this embodiment, the electrolysis time in step three is 1s-60min.
[0038] In this embodiment, the micropore size of the microporous copper foil product VIII is 0-150 μm, including blind holes and through holes.
[0039] The above shows and describes the basic principles, main features and advantages of the present invention. Technical personnel in this industry should understand that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not used to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A method for preparing a microporous copper foil, characterized in that: The steps include: Step 1: Applying polymer solution I on the surface of copper foil II, and after the solvent evaporates, forming polymer-covered copper foil III; Step 2, immersing the copper foil III prepared in step 1 as an anode into an electrolyte IV, and another inert conductive electrode V as a cathode to form an electrolytic cell with a power source and the electrolyte VI; Step three, using the device shown in step two, apply current to the copper foil electrode III and the V electrode, and maintain for a certain period of time. After the reaction is completed, take out the copper foil electrode III, clean the surface, and dry it to obtain a microporous copper foil product VIII.
2. The method for preparing a microporous copper foil according to claim 1, characterized in that: The polymer in the polymer solution I is a water-soluble or oil-soluble polymer, and is one or more of sodium carboxymethyl cellulose, polyvinyl pyrrolidone, cellulose acetate, cellulose ether, starch, polyvinyl alcohol, polyacrylate, polyethylene glycol, gelatin, carboxymethyl chitosan, polyacrylamide, polyacrylic acid, xanthan gum, poly(3,4-ethylenedioxythiophene) poly(styrene sulfonate), polymerized vinyl sulfonic acid, polyacrylamide, polyaniline, polyimide, and polymethyl methacrylate.
3. The method for preparing a microporous copper foil according to claim 1, characterized in that: The copper foil II is electrolytic copper foil or rolled copper foil.
4. The method for preparing a microporous copper foil according to claim 1, characterized in that: The electrode V is one of platinum, carbon, titanium, stainless steel, copper, platinum, gold, silver, nickel or an alloy thereof.
5. The method for preparing a microporous copper foil according to claim 1, characterized in that: The electrolyte VI is one or more of sodium chloride, potassium perchlorate, potassium sulfate, copper chloride, copper sulfate, sodium carbonate, ammonium nitrate, ammonium bicarbonate, and ferric chloride.
6. The method for preparing a microporous copper foil according to claim 1, characterized in that: The concentration of the electrolyte is 0.01 mol / L-5 mol / L.
7. The method for preparing a microporous copper foil according to claim 1, characterized in that: The electrolysis current in the step 3 is 0.01A / dm2-100 A / dm2.
8. The method for preparing a microporous copper foil according to claim 1, characterized in that: The electrolysis temperature in step 3 is 20-85°C.
9. The method for preparing a microporous copper foil according to claim 1, characterized in that: The electrolysis time in step 3 is 1s-60min.
10. The method for preparing a microporous copper foil according to claim 1, characterized in that: The microporous copper foil product VIII has a micropore size of 0-150 μm, including blind holes and through holes.