Construction method for reinforcing historical building wall through high-ductility compound
Through the high-ductile composite reinforcement method, the problems of structural damage and complex construction in the repair of historical buildings are solved, lightweight reinforcement is achieved, process simplification, cost and foundation load are reduced, and structural safety is improved.
Patent Information
- Application Number
- CN202411325286.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-23
- Publication Date
- 2024-11-12
AI Technical Summary
The existing technology is prone to damage the original structure when repairing the walls of historical buildings, the construction process is cumbersome, and the walls after repair are heavy, which has a large load on the foundation, which increases the construction cost and construction period.
The reinforcement method of high ductility composites is adopted, including wall peeling, filling holes, setting anti-shear bonds, base layer treatment, removing lime mortar from gaps, setting ash cake, wetting the wall surface, filling the high ductility composites in the gaps of bricks multiple times, Press the high-ductile composite to form a tight bond and reduce foundation load.
It has achieved reinforcement without destroying the core structure of the brick wall of historical buildings, with simple construction processes and light weight, avoiding foundation reinforcement, reducing costs, and improving structural safety.
Smart Images

Figure CN118933399A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of wall repair, and in particular relates to a construction method for reinforcing the walls of historical buildings with a high-ductility composite material. Background Art
[0002] Buildings from different periods not only reflect the architectural level of each period, but are also a microcosm of the history of the corresponding period and an important part of culture. Most of the existing historical buildings in my country are brick-wood structures, with single-story and multi-story houses made of brick exterior walls and wooden doors, windows, roofs, beams, columns, and floor slabs. The passage of time and the erosion of wind and rain have caused varying degrees of damage to historical buildings. The original parts of the buildings are the social and historical significance of historical buildings, and must be strictly preserved during protection and repair.
[0003] The building wall is an important part of the building, which is related to the safety of the structure. The collapse of the wall will directly cause the loss of historical value. Generally, reinforced concrete plywood walls are used to reinforce the walls. To reinforce the brick walls of historical buildings with reinforced concrete plywood walls, it is necessary to plant steel bars in the walls, which requires drilling holes in the walls, destroying the original structure of the brick walls. At the same time, the thickness of the plywood wall is generally more than 60mm, and its own weight is heavy, which also increases the load on the foundation. At the same time, the construction process is cumbersome, requiring planting steel bars, tying steel bars, supporting formwork, setting up scaffolding and other processes. In addition, because the space of historical buildings is generally narrow, construction is difficult, which increases the construction cost and the construction period is long.
[0004] Therefore, a construction method for reinforcing the walls of historical buildings with high ductility composite materials is developed to solve the problem of not destroying the core structure of the brick walls of historical buildings. The manual troweling technology is used, the construction process is simple, and it is tightly combined with the brick wall to form an integrated whole, which ensures the construction quality and light weight. It reduces the foundation load and avoids reinforcement of the foundation, which is a technical problem that needs to be solved urgently. Summary of the invention
[0005] The purpose of the present invention is to provide a construction method for reinforcing the walls of historical buildings with a high-ductility composite material, so as to solve the problems existing in the prior art that the original walls will be damaged during the repair of the walls of historical buildings, the construction process is cumbersome, the weight of the repaired walls is heavy, and a large load is generated on the foundation.
[0006] In order to achieve the above-mentioned purpose, the present invention adopts the following technical solutions: The present invention proposes a construction method for reinforcing the walls of historical buildings with a high-ductility composite material, comprising: S1: Chiseling off the wall of the historic building; S2: filling the hole in the wall after the wall skin is removed; S3: providing a shear key on the wall surface; S4: Base treatment: grinding the lime mortar on the wall surface to the surface of the bricks in the wall; S5: removing the lime mortar in the gaps between adjacent bricks; S6: Make ash cake: A plurality of the ash cakes are dispersedly arranged on the wall surface, and the surfaces of the plurality of the ash cakes form a reference surface; S7: Wetting the wall surface: S8: grouting: using a high ductility composite material to fill the gaps between adjacent bricks at least twice, compacting and roughening; S9: applying a high-ductility composite material on the wall surface.
[0007] In some embodiments of the present application, the S3: setting a shear key comprises the following steps: S31: Mark the position of the shear key: Marking the setting positions of a plurality of the shear keys on the wall, wherein the plurality of the shear keys are distributed in a plum blossom shape, and the distance between the shear keys close to the edge of the wall and the edge of the wall is 25 cm to 30 cm; S32: Chiseling out shear key grooves: According to the positions of the plurality of shear keys marked in S31, the shear key grooves are chiseled out.
[0008] In some embodiments of the present application, in the process of S32: chiseling out the shear key grooves, loose bricks are removed and filled with high-ductility composite materials.
[0009] In some embodiments of the present application, S5: picking the gaps: in the process of removing the lime mortar in the gaps between adjacent bricks, the lime mortar in the gaps between the bricks is removed to a depth of 20 mm to 25 mm; the remaining lime mortar is polished to the surface of the bricks, the wall surface is cleaned and rinsed, and the dust on the surface of the bricks is cleaned.
[0010] In some embodiments of the present application, during the step S7: wetting the wall surface, the wall body with the wall skin removed is moistened by watering, and before the step S9: applying the high-ductility composite material, the wall surface is moistened by slowly and evenly pouring the water from top to bottom, and the water immersion thickness of the wall body is not less than 2 cm.
[0011] In some embodiments of the present application, in the process of making ash cakes in S6, the following steps are included: the ash cakes are rectangular structures with a side length of 3 cm to 5 cm made by using cement mortar, the distance between adjacent ash cakes is not more than 60 cm, and the distance between the ash cakes adjacent to the edge of the wall and the edge of the wall is not more than 30 cm.
[0012] In some embodiments of the present application, after the grouting is completed in S8, the gaps between the bricks are filled with a high-ductility composite that is recessed into the surface of the brick by 2 mm to 3 mm.
[0013] In some embodiments of the present application, in S9: in the process of applying the high-ductility composite material on the wall surface, before applying the high-ductility composite material, the wall surface is repeatedly watered to moisten it, and the application is performed after the wall surface is slightly dry; the application is performed continuously at the corner of the wall, and the rubbing position is not less than 500 mm from the corner of the wall; According to the designed thickness of the pressed high-ductility composite, the pressed high-ductility composite is applied once or multiple times, and the latter pressing high-ductility composite should be carried out when the former pressing high-ductility composite is in the initial hardening state.
[0014] In some embodiments of the present application, within 12 hours after the completion of S9: pressing and applying the high-ductility composite material, S10: curing is performed by spraying with an electric sprayer, the curing time is not less than 7 days, and the curing is performed not less than 4 times a day.
[0015] In some embodiments of the present application, the ratio of the high ductility composite material is to add 780g~820g chemical fiber, 1Kg to 1.2Kg cellulose, 0.75Kg to 0.78Kg wetting agent, 0.3Kg to 0.33Kg defoaming agent, and 19Kg to 23Kg water into 100Kg micro-nano cement; the order of adding the high ductility composite material is to first add 75% to 80% water, stir the cellulose into the mixture and mix evenly, then add the micro-nano cement and stir, and add the chemical fiber in a dispersed manner during the stirring process, and then add the defoaming agent and the wetting agent; finally, add the remaining water and stir.
[0016] Compared with the prior art, the advantages and positive effects of the present invention are: The wall skin of the historical building is removed and the exposed wall holes are filled; then a shear key is opened on the front; then the base is treated, that is, the lime mortar on the front is polished to the surface of the bricks of the wall, and then the lime mortar in the gaps between adjacent bricks is removed to a set depth; multiple ash cakes are dispersed on the wall, and the surfaces of multiple ash cakes are coplanar to form a reference surface; then, under the condition of wetting the front, a high-ductility compound is used to fill the gaps between adjacent bricks at least twice, compact and roughen; using the reference surface formed by multiple ash cakes as a reference, the high-ductility compound is pressed on the wall. Thus, a close connection between adjacent bricks is achieved. The above method is used to reinforce the walls of historical buildings by using high-ductility composite materials, aiming to solve the problem of not destroying the core structure of the brick wall masonry of the historical building. The manual troweling technology is used, the construction process is simple, the construction progress is fast, and it meets the requirements of green environmental protection. At the same time, it avoids common quality problems such as cracks and hollows. It is tightly combined with the brick wall to form an integrated whole, which ensures the construction quality, is light in weight, reduces the foundation load, avoids reinforcement of the foundation, reduces construction costs, and improves structural safety.
[0017] After reading the specific embodiments of the present invention in conjunction with the accompanying drawings, other features and advantages of the present invention will become more clear. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0019] Figure 1 It is a flow chart of a construction method for reinforcing the walls of historical buildings with a high-ductility composite material proposed by the present invention. DETAILED DESCRIPTION
[0020] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0021] In the description of the present application, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.
[0022] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.
[0023] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, a direct connection, or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0024] In the present invention, unless otherwise clearly stipulated and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.
[0025] The disclosure below provides many different embodiments or examples to implement different structures of the present invention. In order to simplify the disclosure of the present invention, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present invention. In addition, the present invention can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplification and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed.
[0026] Buildings from different periods not only reflect the architectural level of each period, but are also a microcosm of the history of the corresponding period and an important part of culture. Most of the existing historical buildings in my country are brick-wood structures, with single-story and multi-story houses made of brick exterior walls and wooden doors, windows, roofs, beams, columns, and floor slabs. The passage of time and the erosion of wind and rain have caused varying degrees of damage to historical buildings. The original parts of the buildings are the social and historical significance of historical buildings, and must be strictly preserved during protection and repair.
[0027] The building wall is an important part of the building, which is related to the safety of the structure. The collapse of the wall will directly cause the loss of historical value. Generally, reinforced concrete plywood walls are used to reinforce the walls. To reinforce the brick walls of historical buildings with reinforced concrete plywood walls, it is necessary to plant steel bars in the walls, which requires drilling holes in the walls, destroying the original structure of the brick walls. At the same time, the thickness of the plywood wall is generally more than 60mm, and its own weight is heavy, which also increases the load on the foundation. At the same time, the construction process is cumbersome, requiring planting steel bars, tying steel bars, supporting formwork, setting up scaffolding and other processes. In addition, because the space of historical buildings is generally narrow, construction is difficult, which increases the construction cost and the construction period is long.
[0028] In some embodiments of the present application, a construction method for reinforcing the walls of historical buildings with high-ductility composites is provided, which aims to repair the walls of historical buildings without destroying the core structure of the brick walls of the historical buildings, and to repair the walls of the historical buildings while ensuring that the historical buildings retain their original main wall structure.
[0029] A construction method for reinforcing the walls of historical buildings with high ductility composite materials, such as Figure 1 As shown, the following steps are included: S1: Chiseling off the wall of the historic building; S2: Filling of holes in the wall after the wall skin is removed; S3: Set up shear keys on the wall; S4: Base treatment: Grind the lime mortar on the wall to the surface of the bricks inside the wall; S5: Remove the lime mortar in the gaps between adjacent bricks; S6: Make ash cake: A plurality of ash cakes are dispersedly arranged on the wall surface, and the surfaces of the plurality of ash cakes form a reference surface; S7: Wet wall; S8: Pointing: Use high ductility compound to fill the gaps between adjacent bricks at least twice, compact and roughen; S9: Press high ductility compound onto the wall.
[0030] In some embodiments of the present application, before S1: removing the original wall skin, it is necessary to perform S01: collecting information on historical buildings and S02: marking the locations of walls that need to be repaired.
[0031] In S01: The process of collecting information on historical buildings, a 3D scanner and on-site survey were used to digitally collect the building's size data and damage conditions to obtain an information model of the building.
[0032] According to the collected information model, S02 is performed: marking the location of the wall that needs to be repaired.
[0033] In some embodiments of the present application, in S1: the process of chiseling off the wall skin of the historical building, the wall skin is manually chiseled off and cleaned to reduce the disturbance to the original wall, the harm to the wall, and avoid damaging the bricks.
[0034] After the original wall of a historical building is removed, there may be loose bricks left. In this case, whole bricks or half bricks need to be used to partially replace the loose bricks.
[0035] After the original wall skin is removed, S2 is performed: filling the hole in the wall after the wall skin is removed; The holes left by the removal of the cable duct are filled with a high-ductility compound.
[0036] In some embodiments of the present application, in S3: setting the anti-shear key, the specific steps of setting the anti-shear key are as follows: S31: Shear key position mark Mark multiple shear key locations on the wall. The multiple shear keys are distributed in a plum blossom shape. The shear keys close to the edge of the wall are 25 cm to 30 cm away from the edge of the wall. S32: Chiseling out the shear key groove According to the positions of the multiple shear keys marked in S31, chisel out the shear key grooves. To avoid disturbing the wall during the chiseling process, use an electric chisel with a power of less than 1500W to chisel from top to bottom. If there are loose bricks during the chiseling process, they can be removed together and filled with high-ductility concrete. The height, width and depth of the shear key groove are all 28mm to 35mm. If the wall is reinforced on both sides, the positions of the shear key grooves on both sides should be staggered.
[0037] During S4: base treatment, grind the remaining lime mortar to the surface of the bricks, first use an angle grinder or wire brush to clean the remaining sand, ash, brick slag and debris on the wall, and then use a high-pressure water gun to rinse the wall to ensure that the base is clean, not loose, and the connection is reliable.
[0038] In S5: the process of picking out the joints, the lime mortar in the gaps between adjacent bricks is picked out, and the lime mortar in the gaps is picked out to a depth of 20 mm to 25 mm.
[0039] Because the gap is deep enough, it can ensure that the wall is reinforced after S7: grouting, and at the same time, it can ensure that the bricks and high-ductility concrete are closely combined and do not delaminate. After the joints are grouted, use a wire brush to clean the residual ash and blow off the surface ash powder.
[0040] In S6: during the process of making ash cakes, a plurality of ash cakes are dispersedly arranged on the wall surface, and the plane where the surfaces of the plurality of ash cakes are located forms a reference surface for forming a verticality reference surface and a flatness reference surface on the surface where the surfaces are located.
[0041] The ash cake is a rectangular structure with a side length of 3cm to 5cm made of cement mortar. The distance between adjacent ash cakes is not more than 60cm, and the distance between the ash cakes adjacent to the edge of the wall is not more than 30cm from the edge of the wall.
[0042] In some embodiments of the present application, in the process of S7: wetting the wall surface, the wall with the wall skin removed is moistened by watering, and before S9: applying the high-ductility composite material, the wall surface is moistened by slowly and evenly pouring it from top to bottom, and the thickness of the wall soaked in water is not less than 2 cm.
[0043] After the wet wall surface is completed, S8 grouting is performed: the high ductility composite is used to fill the gaps between adjacent bricks at least twice, and compacted and roughened; after the grouting is completed, the gaps between the formed bricks are filled with the high ductility composite recessed into the surface of the brick.
[0044] During the grouting process, the one-time grouting forming method cannot be used.
[0045] In some embodiments of the present application, after S8 grouting, S9: pressing and applying the high-ductility composite is performed. During S9: pressing and applying the high-ductility composite on the wall, before pressing and applying the high-ductility composite, the wall is repeatedly watered to moisten it, and pressing and applying is performed after the wall is slightly dry; the wall is continuously pressed and applied at the corners, and the rubbing position is left not less than 500 mm away from the corners.
[0046] According to the designed thickness of the pressed high-ductility composite, the pressed high-ductility composite is applied once or multiple times. The latter layer of pressed high-ductility composite should be constructed when the previous layer of pressed high-ductility composite is in the initial hardening state. After the construction of the high-ductility composite is completed, it is strictly forbidden to use cement mortar surface leveling.
[0047] Within 12 hours after S9: applying the high-ductility composite material, S10: curing is carried out by spraying with an electric sprayer. The curing time is not less than 7 days and the curing is carried out not less than 4 times a day.
[0048] In some embodiments of the present application, the ratio of the high ductility composite is to add 780g~820g chemical fiber, 1Kg to 1.2Kg cellulose, 0.75Kg to 0.78Kg wetting agent, 0.3Kg to 0.33Kg defoaming agent, and 19Kg to 23Kg water into 100Kg micro-nano cement.
[0049] The order of adding high ductility composite materials is to add 75% to 80% water first, stir the cellulose in and mix evenly, then add micro-nano cement and stir, add chemical fiber evenly dispersed during the stirring process, then add defoamer and wetting agent; finally add the remaining water and stir.
[0050] In summer, the high-ductility compound can be discharged within 40 minutes, and in winter, the high-ductility compound can be discharged within 60 minutes.
[0051] In the mix ratio, various components are added to improve the performance of concrete and enhance its ductility, crack resistance, durability and other characteristics.
[0052] Here are some advantages of this mix: Improve ductility: Micro-nano cement particles are small and can fill the gaps between ordinary cement particles, increase the density of concrete, and thus improve its ductility.
[0053] The addition of chemical fibers and cellulose can increase the toughness of concrete, allowing it to withstand greater deformation without breaking when subjected to stress.
[0054] Improve crack resistance: The addition of chemical fiber and cellulose fiber can inhibit the generation of early shrinkage cracks and improve the crack resistance of concrete. The fine particles of micro-nano cement can fill the micropores inside the concrete and reduce the generation of cracks.
[0055] Enhanced durability: Micro-nano cement can increase the density of concrete, reduce the penetration of moisture and harmful substances, and thus improve the durability of concrete. Cellulose fiber can improve the impermeability of concrete and further enhance its durability.
[0056] Improve construction performance: Wetting agents can improve the workability of concrete, making it easier to mix and pour, and improving construction efficiency. Defoamers can reduce bubbles in concrete, improve the density and surface smoothness of concrete.
[0057] Improved structural safety: By increasing the ductility and crack resistance of concrete, the safety of structures during natural disasters such as earthquakes can be increased. Higher durability means that the structure can withstand environmental erosion over a long period of time, reducing the risk of structural failure.
[0058] Reduced costs and maintenance: By reducing cracks and improving durability, the need for structural maintenance can be reduced, reducing long-term maintenance costs. Improved construction performance can reduce construction time and labor costs.
[0059] Environmental performance: The use of micro-nano cement helps reduce the amount of ordinary cement used, thereby reducing carbon emissions. Reduced maintenance requirements also help reduce the impact on the environment.
[0060] In summary, this mix ratio can significantly improve the performance of concrete, enhance the safety and durability of the structure, while reducing construction costs and maintenance expenses. It is a high-performance concrete formula worthy of recommendation.
[0061] Micro-nano cement should be stored in a dry place that is not susceptible to moisture. If the outer packaging bag of micro-nano cement is intact, the storage time shall not exceed 90 days.
[0062] Build a storage area for special high-ductility composite materials that is moisture-proof, leak-proof and wind-proof.
[0063] When storing high-ductility composite materials, the ground pad should be 20 cm to 30 cm above the ground and at least 30 cm away from the wall. It is appropriate to stack 10 bags of bagged high-ductility composite materials, and the maximum should not exceed 15 bags. A passage with a width of not less than 70 cm should be left between each stack. If it is necessary to store them outdoors under special circumstances, they should be stacked in a place with high terrain, no water accumulation, and a ground pad higher than 30 cm, and covered tightly with rain cloth to prevent rain and dew from invading and causing the cement to get wet. In the work area and the floors of the building, the site must be cleaned after the work is completed, and those that cannot be transported away immediately should be neatly stacked. The garbage cleared on each floor shall not be piled on the floor for a long time and should be transported away in time.
[0064] A horizontal shaft forced mixer should be used to mix high ductility composites. If the mixer capacity is 300 to 400 liters, a 4kw motor is recommended. The mixer speed should be 45 to 70 rpm, and the distance between the mixing blade and the inner wall of the mixer barrel should not be greater than 5mm.
[0065] When the base wall is uneven, the high ductility compound is used to reinforce the wall to ensure the designed thickness. After the reinforcement is completed, ordinary mortar is used for leveling. It is not allowed to use mortar for leveling first and then use high ductility compound for reinforcement.
[0066] The above method is used to repair the walls of historical buildings, which can avoid implanting reinforcement in the walls, thereby avoiding damage to the walls caused by drilling holes in the walls, thereby ensuring that the core structure of the brick masonry of the historical buildings is not damaged.
[0067] The use of manual troweling technology simplifies the construction process, speeds up the construction progress, and meets the requirements of green environmental protection. At the same time, it avoids common quality problems such as cracks and hollows, and is tightly combined with the brick wall to form an integrated whole, ensuring the construction quality. It is light in weight, reduces the foundation load, and avoids the need for foundation reinforcement. It reduces construction costs and improves structural safety.
[0068] During the mixing and plastering process of the high-ductility composite material, no other materials shall be added and water shall not be added at will.
[0069] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for a person skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to replace some of the technical features therein by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions claimed to be protected by the present invention.
Claims
1. A construction method for reinforcing the walls of historical buildings with high ductility composite materials. It is characterized in that include: S1: Chiseling off the wall of the historic building; S2: filling the hole in the wall after the wall skin is removed; S3: providing a shear key on the wall surface; S4: Base treatment: removing the lime mortar on the wall surface to the surface of the bricks in the wall; S5: removing the lime mortar in the gaps between adjacent bricks; S6: Make ash cake: A plurality of the ash cakes are dispersedly arranged on the wall surface, and the surfaces of the plurality of the ash cakes form a reference surface; S7: Wetting the wall surface: S8: grouting: using a high ductility composite material to fill the gaps between adjacent bricks at least twice, compacting and roughening; S9: applying a high-ductility composite material on the wall surface.
2. The method for reinforcing the walls of historic buildings with a high ductility composite material according to claim 1, It is characterized in that S3: Providing a shear key on the wall surface, which includes the following steps: S31: Mark the position of the shear key: Marking the setting positions of a plurality of the shear keys on the wall, wherein the plurality of the shear keys are distributed in a plum blossom shape, and the distance between the shear keys close to the edge of the wall and the edge of the wall is 25 cm to 30 cm; S32: Chiseling out shear key grooves: According to the positions of the plurality of shear keys marked in S31, the shear key grooves are chiseled out.
3. The construction method for reinforcing the wall of a historical building with a high ductility composite material according to claim 2, It is characterized in that In the process of S32: chiseling out the shear key grooves, the loose bricks are removed and filled with high-ductility composite materials.
4. The method for reinforcing the walls of historic buildings with high ductility composite materials according to claim 1, It is characterized in that S5: Picking out the gaps: in the process of removing the lime mortar in the gaps between the adjacent bricks, the lime mortar in the gaps between the bricks is removed to a depth of 20 mm to 25 mm; the remaining lime mortar is polished to the surface of the bricks, the wall surface is cleaned and rinsed, and the gray powder on the surface of the bricks is cleaned.
5. The construction method for reinforcing the wall of a historical building with a high ductility composite material according to claim 1, It is characterized in that In the process of S7: wetting the wall surface, the wall body with the wall skin removed is moistened by watering, and before the construction of S9: applying the high-ductility composite material, the wall surface is moistened by a top-down slow and even wetting method, and the water-soaked thickness of the wall body is not less than 2 cm.
6. The method for reinforcing the walls of historic buildings with high ductility composite materials according to claim 1, It is characterized in that In the process of making ash cakes in S6, the following steps are included: the ash cakes are rectangular structures with a side length of 3 cm to 5 cm made of cement mortar, the distance between adjacent ash cakes is not more than 60 cm, and the distance between the ash cakes adjacent to the edge of the wall and the edge of the wall is not more than 30 cm.
7. The method for reinforcing the walls of historic buildings with high ductility composite materials according to claim 1, It is characterized in that After S8: grouting is completed, the gaps between the bricks are filled with a high-ductility composite material that is recessed into the brick surface by 2 mm to 3 mm.
8. The construction method for reinforcing the wall of a historical building with a high ductility composite material according to claim 1, It is characterized in that In S9: in the process of applying the high-ductility composite material on the wall surface, before applying the high-ductility composite material, the wall surface is repeatedly watered to moisten it, and the application is performed after the wall surface is slightly dry; the application is performed continuously at the corner of the wall, and the rubbing position is not less than 500 mm from the corner of the wall; According to the designed thickness of the pressed high-ductility composite, the pressed high-ductility composite is applied once or multiple times, and the latter pressing high-ductility composite should be carried out when the former pressing high-ductility composite is in the initial hardening state.
9. The method for reinforcing the walls of historic buildings with high ductility composite materials according to claim 1, It is characterized in that Within 12 hours after the completion of S9: pressing and applying the high-ductility composite material, S10: curing is performed by spraying with an electric sprayer, the curing time is not less than 7 days, and the curing is performed not less than 4 times a day.
10. The construction method for reinforcing the wall of a historical building with a high ductility composite material according to claim 1, It is characterized in that The high ductility composite material is prepared by adding 780-820 g of chemical fiber, 1-1.2 kg of cellulose, 0.75-0.78 kg of wetting agent, 0.3-0.33 kg of defoaming agent, and 19-23 kg of water to 100 kg of micro-nano cement; The order of adding the high-ductility composite is to first add 75% to 80% water, stir the cellulose into it and mix it evenly, then add the micro-nano cement and mix it, add the chemical fiber evenly dispersed during the mixing process, then add the defoamer and the wetting agent; finally, add the remaining water and mix it.
Citation Information
Patent Citations
Reinforcing method for external wall of protective historical building
CN105464396A
High-ductility concrete caulking reinforced ancient building masonry wall and reinforcing construction process thereof
CN112096113A
Novel high-ductility refractory concrete
CN112661469A
Formwork-free reinforcement high-ductility concrete construction method for masonry reinforcement
CN114575620A
High-strength and high-ductility cement-based composite material and preparation method thereof, and application of nano-cellulose in composite material
CN115991589A
Cited By
Double-curve thin brick vault roof reinforcing method and reinforcing structure
CN120830399A