Construction method and application of double transition metal nitride heterojunction modified graphite phase carbon nitride-based photoelectrochemical aptamer sensor
By modifying the surface of g-C3N4 with a dual transition metal nitride heterojunction, the problem of insufficient sensor sensitivity was solved, enabling efficient detection of pesticide residues in the aquatic environment and improving the photoelectric performance and detection sensitivity of the sensor.
Patent Information
- Application Number
- CN202410900118.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-05
- Publication Date
- 2024-11-12
AI Technical Summary
Existing photoelectrochemical aptamer sensors suffer from insufficient sensitivity when detecting organic pesticide residues in aquatic environments, mainly due to the limited light absorption range and high recombination rate of graphitic carbon nitride (g-C3N4) materials.
By modifying the surface of g-C3N4 with dual transition metal nitride heterojunctions (such as Ni3N/Ni3FeN, Ni4N/VN or Ni3N/Co3N), the strong electron absorption capability and lattice expansion effect of the heterojunction can be used to promote the directional migration and separation of charge carriers. Furthermore, the heterojunction can be used as an efficient transport path for photogenerated charges, thereby improving the optoelectronic properties of the material.
It significantly improves the sensitivity and selectivity of the sensor, enabling efficient detection of pesticide residues in aquatic environments, and has efficient light absorption and rapid charge transport capabilities.
Smart Images

Figure CN118937445A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of photoelectrochemistry and analytical detection technology, and specifically relates to a method for constructing a double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptamer sensor and its use in the detection of organic pesticide residues in aquatic environments. Background Art
[0002] Organic pesticides are a class of harmful chemicals used to control harmful agricultural and forestry crops and their products. In order to ensure the yield and quality of crops in the global market demand, organic pesticides have become a necessity for agricultural development. For a long time, due to the unreasonable overall structure distribution of organic pesticide products, irregular use methods and insufficient supervision, the phenomenon of excessive pesticide residues in crops and aquatic environments has continued to intensify. In addition, due to the characteristics of organic pesticides such as difficult biodegradation and bioaccumulation, trace amounts of organic pesticide residues will accumulate in soil, air and water to reach toxic concentrations, posing a serious threat to food, water quality and human health. Therefore, sensitive and rapid detection of organic pesticide residues in aquatic environments is of great significance for protecting the environment and life safety. So far, the methods commonly used to detect organic pesticide residues include gas chromatography, enzyme-linked immunosorbent assay, capillary chromatography, liquid chromatography and capillary electrophoresis. Although these technologies can achieve accurate detection, sample pretreatment is complicated and costly. Therefore, it is crucial to develop simple, economical and reliable organic pesticide residue detection technologies.
[0003] The principle of photoelectrochemical aptamer sensor is that under light, the aptamer recognizes the target and causes the change of the photocurrent signal at the sensor detection interface. There is a certain linear relationship between the change value and the concentration of the target, so that the specific concentration of the target in the actual water environment can be determined by the change of the photoelectric signal. The performance of the photoelectric active material is the key to determining the sensitivity of the sensor. Graphite phase carbon nitride (g-C3N4) has attracted much attention due to its non-toxicity, high photothermal stability, adjustable chemical structure and excellent photoelectrochemical performance. However, the limited light absorption and high recombination rate of photogenerated carriers of g-C3N4 limit its application. Therefore, broadening the light absorption range of g-C3N4 and accelerating the separation and transfer of carriers are the key to improving the photoelectrochemical performance of g-C3N4. As a class of metal interstitial compounds, transition metal nitrides have attracted great attention in the application of photoelectric conversion due to their unique physical and chemical properties and characteristics similar to precious metals, such as strong conductivity, narrow band gap and strong visible light response, which are conducive to the efficient transfer and separation of photogenerated carriers. In transition metal nitrides, the introduction of nitrogen atoms causes the lattice expansion of the metal structure, and the density of states near the Fermi level increases compared to the parent metal. Therefore, when g-C3N4 is compounded with transition metal nitrides, a strong charge space region will be generated at the interface, increasing the charge concentration, thereby accelerating the electron transfer of the g-C3N4 material. There is a strong electronic interaction between transition metals. When two transition metal nitrides are constructed into a heterojunction, the formation of its internal electric field causes a high-density charge to be generated at the heterojunction interface, which can prompt the g-C3N4 material to generate more carriers. In addition, the introduction of this heterostructure to the surface of g-C3N4 can serve as an efficient transmission path for photogenerated charges, promoting the effective separation of photogenerated carriers on g-C3N4, thereby further improving the photoelectric properties of the material and ultimately improving the sensitivity of the sensor.
[0004] Therefore, the development of a double transition metal nitride heterojunction modified graphene phase carbon nitride-based photoelectrochemical aptamer sensor not only provides an efficient photoelectric signal amplification strategy for the construction of g-C3N4-based photoelectrochemical aptamer sensors, but also effectively improves the sensitivity of organic pesticide residue detection in the aquatic environment, which is of great significance for protecting human life safety. Summary of the invention
[0005] The present invention aims to solve the problems existing in the prior art and proposes a method for preparing a double transition metal nitride heterojunction modified graphite phase carbon nitride based photoelectrochemical aptamer sensor, which is applied to detect pesticide residues in water environments.
[0006] The present invention achieves the above technical objectives through the following technical means.
[0007] A double transition metal nitride heterojunction modified graphite phase carbon nitride based photoelectrochemical aptamer sensor, a type of double transition metal nitride heterojunction (Ni3N / Ni3FeN, Ni4N / VN or Ni3N / Co3N) is modified on the surface of g-C3N4. On the one hand, the transition metal nitride has a strong electron absorption ability, which can induce the transfer of electrons in the g-C3N4 conduction band to the transition metal nitride, resulting in directional migration and rapid separation of carriers. On the other hand, the introduction of nitrogen atoms in the transition metal nitride causes the lattice expansion of the metal structure. Compared with the parent metal, the state density near the Fermi level increases. When compounded with g-C3N4, a strong charge space region will be generated at the interface, increasing the charge concentration and resulting in a large number of carriers. More importantly, the formation of the double transition metal nitride heterojunction leads to the existence of an internal electric field, which makes the heterojunction interface produce high-density charges, which can effectively improve the photoelectric performance of the photoelectric active material. At the same time, the heterojunction can serve as an efficient transmission path for photogenerated charges, promoting the effective separation of photogenerated carriers on g-C3N4, thereby further improving the photoelectric properties of the material and ultimately improving the sensitivity of the sensor.
[0008] A method for preparing a double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptamer sensor is carried out according to the following steps:
[0009] (1) Preparation of g-C3N4 materials:
[0010] A certain amount of carbon and nitrogen source was weighed into a covered crucible and g-C3N4 was obtained by a one-step calcination method;
[0011] (2) Preparation of double transition metal nitride heterojunction modified g-C3N4 materials:
[0012] First, transition metal salt 1, transition metal salt 2, urea and ammonium salt are dissolved in deionized water in proportion and fully dissolved to obtain solution A;
[0013] Next, weigh the g-C3N4 powder obtained in step (1), dissolve it in deionized water, and fully disperse it to obtain solution B;
[0014] Under continuous stirring, solution B was uniformly added dropwise to solution A, and the mixture was transferred into a polytetrafluoroethylene-lined reactor for constant temperature hydrothermal reaction. After the reaction was completed, the reactor was taken out and naturally cooled to room temperature. The sample was centrifuged, washed with water and alcohol for several times, and dried in vacuum to obtain a double transition metal LDH / g-C3N4 precursor.
[0015] Then, a certain amount of double transition metal LDH / g-C3N4 precursor was weighed and calcined in a tubular furnace with ammonia gas to obtain a double transition metal heterojunction / g-C3N4 material.
[0016] (3) Preparation of double transition metal nitride heterojunction modified g-C3N4-ITO electrode:
[0017] A certain amount of double transition metal nitride heterojunction / g-C3N4 composite material is dispersed in deionized water and evenly dispersed by ultrasonication to obtain a stable suspension; the suspension is then dropwise coated on the surface of ITO conductive glass, naturally dried, rinsed with deionized water and dried at room temperature to obtain a double transition metal nitride heterojunction / g-C3N4-ITO electrode (DTMNH / g-C3N4-ITO).
[0018] (4) Preparation of DTMNH / g-C3N4 / aptamer-ITO electrode:
[0019] Take the carbendazim aptamer, oxydemeton-methyl aptamer or bromophos aptamer and apply it on the surface of the DTMNH / g-C3N4-ITO photoelectrode prepared in step (3). After incubation at room temperature for a certain period of time, rinse the unanchored aptamer on the electrode surface with deionized water and dry it at room temperature to obtain a DTMNH / g-C3N4 / aptamer-ITO photoelectrode sensor.
[0020] In step (1), the carbon and nitrogen source is one or more mixtures of thiourea, cyanamide, dicyandiamide, melamine or urea; the calcination temperature is 450-650° C., and the insulation time is 2-8 hours.
[0021] In step (2),
[0022] The transition metal salt 1 is nickel chloride hydrate or nickel nitrate hydrate;
[0023] One of the transition metal salts selected from ferric chloride hydrate, ferric nitrate hydrate, sodium metavanadate, cobalt nitrate hydrate or cobalt chloride;
[0024] The ammonium salt is ammonium fluoride or hexamethylenetetramine;
[0025] The ratio of the transition metal salt 1, transition metal salt 2, ammonium salt, urea and g-C3N4 is 0.01-1mmol: 0.01-1mmol: 0.01-1mmol: 6mmol: 0.01-5mmol;
[0026] The constant temperature hydrothermal reaction temperature is 100-200°C, and the constant temperature reaction time is 8-24h;
[0027] The flow rate of ammonia is 10-100 mL / min; the calcination temperature is 300-450° C., the calcination rate is 1-20° C. / min, and the insulation time is 2-8 h.
[0028] In step (3), the concentration of the suspension is 0.2-4 mg / mL, and the drop coating amount is 10-100 μL.
[0029] In step (4),
[0030] The carbendazim aptamer sequence is: 5′-CGACACAGCGGAGGCCACCCGCCCACCAGCCCCTGCAGCTCCTGTACCTGT GTGTGTG-3′;
[0031] The omethoate aptamer sequence is: 5′-AGCTTGCTGCAGCGATTCTTGATCGCCACAGAGCT-3′;
[0032] The sequence of the profenofos aptamer is:
[0033] 5′-AAGCTTGCTTTAGCCTGCAGCGATTCTTGATCGGAAAAGGCTGAGAG CTACGC-3′.
[0034] The concentrations of the carbendazim aptamer, omethoate aptamer or profenofos aptamer are all 0.1-5 μmol / L, and the drop-coating amounts are all 10-50 μL.
[0035] Another object of the present invention is to provide a double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptamer sensor for detecting pesticide residues in aquatic environments. By means of the conjugated interaction between g-C3N4 and the aptamer corresponding to the pesticide, the aptamer corresponding to the pesticide is introduced as a specific recognition element to improve the selectivity of the sensor, and finally achieve high selectivity and high sensitivity detection of pesticide residues. The specific steps are as follows:
[0036] (5) Determination of standard curve:
[0037] The prepared DTMNH / g-C3N4 / aptamer-ITO electrode was used as the working electrode, Ag / AgCl as the reference electrode, Pt as the counter electrode, and phosphate buffer solution as the electrolyte. The photocurrent of the working electrode was tested under a certain bias voltage in the presence of known concentrations of carbendazim, oxydemeton-methyl, or profenofos, and a series of concentration-photocurrent correspondences were obtained, and then the standard curve of the sensor for different concentrations of pesticides was obtained.
[0038] (6) Take a certain amount of carbendazim, oxydemeton-methyl or propyl bromide droplets and apply them on the surface of the DTMNH / g-C3N4 / aptamer-ITO electrode, dry them naturally at room temperature, rinse them with deionized water, and then dry them at room temperature. The photocurrent value is tested in the above electrolyte; and the photocurrent value is substituted into the standard curve for conversion to obtain the concentration of the pesticide in the test solution.
[0039] In step (5), the amount of carbendazim, omethoate or profenofos added is 10 to 100 μL, and the concentration is 1 fM to 1000 nM;
[0040] In step (6), the amount of the test solution of carbendazim, omethoate or profenofos is 10 to 100 μL.
[0041] In step (5) and step (6), the phosphate buffer solution is prepared by mixing 0.1 mol / L sodium dihydrogen phosphate and disodium hydrogen phosphate to adjust the pH value to 7.0, and the concentration thereof is 0.1 to 2 M.
[0042] The beneficial effects of the present invention are:
[0043] (1) In view of the high-speed electron transmission characteristics of transition metal nitride heterostructures, the introduction of double transition metals can further improve the conductivity and visible light absorption capacity of g-C3N4, so that the prepared double transition metal nitride heterojunction modified carbon nitride-based photoelectrode has efficient light absorption capacity and fast charge transfer / separation ability, thereby realizing the amplification of photoelectric signals.
[0044] (2) The present invention utilizes the advantages of the double transition metal nitride heterostructure. The formation of the heterojunction leads to the existence of an internal electric field, which causes the heterojunction interface to generate high-density charges, which can effectively improve the photoelectric performance of the photoelectrically active material. At the same time, the heterojunction can serve as an efficient transmission path for photogenerated charges, promoting the effective separation of photogenerated carriers on g-C3N4, thereby further improving the photoelectric performance of the material and ultimately improving the sensitivity of the sensor. Based on this, the sensitivity of the sensing system to the detection of pesticide residues in the water environment was evaluated, which promoted the application of g-C3N4 materials and transition metal nitrides in the fields of photoelectric sensing and environmental monitoring.
[0045] (3) Considering that double transition metal nitride heterojunction modified carbon nitride is used as a photoelectric active material and the aptamer is used as a specific recognition substance, efficient detection of pesticide residues in aquatic environments can be achieved, which has obvious practicality. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] Figure 1 It is the X-ray diffraction (XRD) pattern of Ni3N / Ni3FeN / g-C3N4 composite material, where a is g-C3N4 and b is Ni3N / Ni3FeN / g-C3N4.
[0047] Figure 2 These are the transmission electron microscopy (TEM) and high magnification transmission electron microscopy (HRTEM) images of the Ni3N / Ni3FeN / g-C3N4 composite material, where a is the TEM image and b is the HRTEM image.
[0048] Figure 3 Solid ultraviolet diffuse reflectance (DRS) diagram of Ni3N / Ni3FeN / g-C3N4 composite material, where a is g-C3N4 and b is Ni3N / Ni3FeN / g-C3N4.
[0049] Figure 4 This is the X-ray photoelectron spectroscopy (XPS) diagram of Ni3N / Ni3FeN / g-C3N4 composite material, where a-d are high-resolution spectra of C1s, N 1s, Ni 2p and Fe 2p respectively. In the figure, a is g-C3N4 and b is Ni3N / Ni3FeN / g-C3N4.
[0050] Figure 5 These are the electrochemical impedance spectroscopy (EIS) diagrams of Ni3N / Ni3FeN / g-C3N4 composite materials, where a is g-C3N4-ITO, b is Ni3N / Ni3FeN / g-C3N4-ITO, c is Ni3N / Ni3FeN / g-C3N4-aptamer-ITO, and d is Ni3N / Ni3FeN / g-C3N4-aptamer-PFF-ITO.
[0051] Figure 6 These are the photocurrent diagrams of Ni3N / Ni3FeN / g-C3N4 composite materials, where a is g-C3N4-ITO, b is Ni3N / Ni3FeN / g-C3N4-ITO, c is Ni3N / Ni3FeN / g-C3N4-aptamer-ITO, and d is Ni3N / Ni3FeN / g-C3N4-aptamer-PFF-ITO.
[0052] Figure 7 This is the photoelectric signal response diagram of Ni3N / Ni3FeN / g-C3N4-aptamer-ITO detecting bromophos, where a is the photocurrent diagram obtained by detecting different concentrations of PFF, and b is the linear relationship diagram of bromophos concentration-photocurrent.
[0053] Figure 8 Selectivity (a), stability (b) and repeatability (c) of Ni3N / Ni3FeN / g-C3N4-aptamer-ITO in detecting bromofosinate. DETAILED DESCRIPTION
[0054] The present invention is further described below in conjunction with specific implementation examples so that those skilled in the art can better understand the present invention, but the protection scope of the present invention is not limited to the following embodiments.
[0055] Embodiment 1:
[0056] (1) The preparation method of g-C3N4 is as follows:
[0057] Weigh 2.5 g of melamine and put it into a 10 mL crucible. Then, place the crucible in a muffle furnace and heat it to 550 °C at a fixed heating rate of 5 °C / min, maintain it for 4 h, and obtain g-C3N4 after cooling.
[0058] (2) The preparation method of Ni3N / Ni3FeN heterojunction modified g-C3N4 (Ni3N / Ni3FeN / g-C3N4) is as follows:
[0059] First, 0.24 mmol nickel chloride hexahydrate and 0.04 mmol ferric chloride hexahydrate were dissolved in 12 mL deionized water and stirred for 0.5 h, and then 6 mmol urea and 1.5 mmol ammonium fluoride were added and stirred for 10 min to obtain solution A;
[0060] Secondly, 80 mg of g-C3N4 powder was weighed into a beaker and 8 mL of deionized water was added to fully disperse it to obtain solution B;
[0061] Under continuous stirring, solution B was uniformly added to solution A, and the mixture was transferred to a 25 mL polytetrafluoroethylene-lined reactor and heated in an oven at 120 ° C for 12 h. After cooling to room temperature, the obtained mixture was centrifuged, washed with distilled water and ethanol 3 times each, and dried in a vacuum oven at 60 ° C for 12 h to obtain NiFe LDH / g-C3N4. Weigh 50 mg NiFe LDH / g-C3N4, place it in an ark and put it into a tube furnace, pass ammonia at a flow rate of 100 mL / min, and heat to 380 ° C at a heating rate of 5 ° C / min for 3 h to obtain Ni3N / Ni3FeN / g-C3N4.
[0062] (3) Preparation of Ni3N / Ni3FeN / g-C3N4-conductive glass (ITO) photoelectrode:
[0063] First, the ITO conductive glass was pretreated. The ITO conductive glass was ultrasonically cleaned in deionized water and ethanol for half an hour, and then rinsed with deionized water several times. Then, the conductive glass was placed in a 0.1mol / L NaOH aqueous solution, boiled, and kept for 30 minutes, washed with deionized water and dried for use. A 1mg / mL Ni3N / Ni3FeN / g-C3N4 aqueous solution was prepared and placed in an ultrasonic machine for ultrasonic dispersion to obtain a stable suspension; then, 50μL of the suspension was dropped on the pretreated ITO conductive glass and dried under an infrared lamp for 30 minutes. The prepared modified electrode was recorded as Ni3N / Ni3FeN / g-C3N4-ITO.
[0064] A double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptasensor was used to detect propyl bromide (PFF) pesticide residues in aquatic environments.
[0065] (4) Construction of Ni3N / Ni3FeN / g-C3N4 / aptamer-ITO sensor:
[0066] Use a pipette to transfer 10 μL of the profenofos PFF aptamer (sequence: 5′-AAG CTT GCT TTA TAG CCTGCAGCG ATT CTT GAT CGG AAA AGG CTG AGA GCT ACG C-3′, concentration: 1.5 μmol / L) and drop-coat it on the surface of the Ni3N / Ni3FeN / g-C3N4-ITO electrode prepared in step (3), incubate at room temperature for 8 h, rinse with deionized water, and continue to dry at room temperature to obtain a photoelectrochemical aptamer sensor, recorded as Ni3N / Ni3FeN / g-C3N4-aptamer-ITO.
[0067] (5) Preparation of target detection substance PFF: PFFs of concentrations of 0.01 nM, 0.1 nM, 1 nM, 10 nM, 100 nM and 1000 nM were prepared for testing.
[0068] (6) Photoelectrochemical detection methods and conditions:
[0069] The electrochemical experiments were performed using a CHI660E electrochemical workstation (Shanghai Chenhua Instrument Co., Ltd.) using a traditional three-electrode system: the modified electrode was the working electrode, the platinum wire electrode was the counter electrode, and the saturated Ag / AgCl electrode was the reference electrode. The excitation light source was a 300W xenon lamp (PLS-SXE300, Beijing Bofeilai Technology Co., Ltd.). The electrochemical experiments were performed at room temperature in a phosphate buffer solution (0.1 mol / L, pH = 7.0) without applying any bias. The EIS experiment was performed in a solution containing 5 mmol / L Fe(CN)6 3- / 4- The experiment was carried out in a phosphate buffer solution (0.1 mol / L, pH=7.0) containing 0.1 mol / L KCl, with a frequency range of 0.01 Hz to 10 kHz, an initial potential of 0.24 V, and an AC amplitude of 5 mV.
[0070] Embodiment 2:
[0071] (1) The preparation method of g-C3N4 is as follows:
[0072] Weigh 4 g of urea and put it into a 10 mL crucible. Then, place the crucible in a muffle furnace and heat it to 550 °C at a fixed heating rate of 5 °C / min, maintain it for 4 h, and obtain g-C3N4 after cooling.
[0073] (2) The preparation method of Ni4N / VN heterojunction modified g-C3N4 (Ni4N / VN / g-C3N4) is as follows:
[0074] First, 0.3 mmol nickel nitrate hexahydrate and 0.1 mmol sodium metavanadate were dissolved in 12 mL deionized water and stirred for 0.5 h, and then 6 mmol urea and 0.5 mmol ammonium fluoride were added and stirred for 10 min to obtain solution A;
[0075] Secondly, weigh 30 mg of g-C3N4 g-C3N4 powder in a beaker, and add 8 mL of deionized water to fully disperse to obtain solution B; under continuous stirring, add solution B to solution A at a uniform rate, and transfer the mixture into a 25 mL polytetrafluoroethylene-lined reactor and heat it in an oven at 120 ° C for 12 h. After cooling to room temperature, the obtained mixture is centrifuged, washed with distilled water and ethanol 3 times each, and dried in a vacuum drying oven at 60 ° C for 12 h to obtain NiV LDH / g-C3N4. Weigh 50 mg NiFe LDH / g-C3N4 and place it in an ark and put it into a tube furnace, pass ammonia at a flow rate of 100 mL / min, and heat to 380 ° C at a heating rate of 5 ° C / min for 3 h to obtain Ni4N / VN / g-C3N4.
[0076] (3) Preparation of Ni4N / VN / g-C3N4-conductive glass (ITO) photoelectrode:
[0077] First, the ITO conductive glass was pretreated. The ITO conductive glass was ultrasonically cleaned in deionized water and ethanol for half an hour, and then rinsed with deionized water several times. Then, the conductive glass was placed in a 0.1mol / L NaOH aqueous solution, boiled, and kept for 30 minutes, washed with deionized water and dried for use. A 1mg / mL Ni4N / VN / g-C3N4 aqueous solution was prepared and placed in an ultrasonic machine for ultrasonic dispersion to obtain a stable suspension; then, 50μL of the suspension was dropped on the pretreated ITO conductive glass and dried under an infrared lamp for 30 minutes. The prepared modified electrode was recorded as Ni4N / VN / g-C3N4-ITO.
[0078] A double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptasensor was used to detect the residues of oxydemeton-methyl pesticide in aquatic environments.
[0079] (4) Construction of Ni4N / VN / g-C3N4 / aptamer-ITO sensor:
[0080] Use a pipette to transfer 10 μL of oxydemeton-methyl aptamer (sequence: 5′-AGCTTGCTGCAGCGATTCTTGATCGCCACAGAGCT-3′, concentration: 2 μmol / L) and apply it on the surface of the Ni4N / VN / g-C3N4-ITO electrode prepared in step (3), incubate at room temperature for 8 h, rinse with deionized water, and continue to dry at room temperature to obtain a photoelectrochemical aptamer sensor, recorded as Ni4N / VN / g-C3N4-aptamer-ITO.
[0081] (5) Preparation of target test substance omethoate: 0.01 nM, 0.1 nM, 1 nM, 10 nM, 100 nM and 1000 nM omethoate were prepared for testing.
[0082] (6) Photoelectrochemical detection methods and conditions: The electrochemical experiments used a CHI660E electrochemical workstation (Shanghai Chenhua Instrument Co., Ltd.) and a traditional three-electrode system: the modified electrode was the working electrode, the platinum wire electrode was the counter electrode, and the saturated Ag / AgCl electrode was the reference electrode. The excitation light source was a 300W xenon lamp (PLS-SXE300, Beijing Bofeilai Technology Co., Ltd.). The electrochemical experiments were all carried out at room temperature in a phosphate buffer solution (0.1 mol / L, pH = 7.0) without applying any bias. The EIS experiment was carried out in a solution containing 5 mmol / L Fe(CN)6 3- / 4- The experiment was carried out in a phosphate buffer solution (0.1 mol / L, pH=7.0) containing 0.1 mol / L KCl, with a frequency range of 0.01 Hz to 10 kHz, an initial potential of 0.24 V, and an AC amplitude of 5 mV.
[0083] Embodiment 3:
[0084] (1) The preparation method of g-C3N4 is as follows:
[0085] Weigh 4 g of melamine and put it into a 10 mL crucible. Then, place the crucible in a muffle furnace and heat it to 600 °C at a fixed heating rate of 2 °C / min, maintain it for 8 h, and obtain g-C3N4 after cooling.
[0086] (2) The preparation method of Ni3N / Co3N heterojunction modified g-C3N4 (Ni3N / Co3N / g-C3N4) is as follows:
[0087] First, 0.3 mmol nickel nitrate hexahydrate and 0.3 mmol cobalt nitrate hexahydrate were dissolved in 12 mL deionized water and stirred for 0.5 h, and then 6 mmol urea and 1.5 mmol hexamethylenetetramine were added and stirred for 10 min to obtain solution A;
[0088] Secondly, weigh 70mg of g-C3N4 powder in a beaker, and add 8mL of deionized water to fully disperse it to obtain solution B; under continuous stirring, add solution B to solution A at a uniform rate, and transfer the mixture into a 25mL polytetrafluoroethylene-lined reactor and heat it in an oven at 120°C for 12h. After cooling to room temperature, the obtained mixture is centrifuged, washed with distilled water and ethanol 3 times each, and dried in a vacuum drying oven at 60°C for 12h to obtain NiCo LDH / g-C3N4. Weigh 50mg NiCo LDH / g-C3N4 and place it in an ark and put it into a tube furnace. Pass ammonia at a flow rate of 80mL / min, and heat it to 380°C at a heating rate of 5°C / min for 3h to obtain Ni3N / Co3N / g-C3N4.
[0089] (3) Preparation of Ni3N / Co3N / g-C3N4-conductive glass (ITO) photoelectrode:
[0090] First, the ITO conductive glass was pretreated. The ITO conductive glass was ultrasonically cleaned in deionized water and ethanol for half an hour, and then rinsed with deionized water several times. Then, the conductive glass was placed in a 0.1mol / L NaOH aqueous solution, boiled, and kept for 30 minutes, washed with deionized water and dried for use. A 1.5mg / mL Ni3N / Co3N / g-C3N4 aqueous solution was prepared and placed in an ultrasonic machine for ultrasonic dispersion to obtain a stable suspension; then, 50μL of the suspension was dropped on the pretreated ITO conductive glass and dried under an infrared lamp for 30 minutes. The prepared modified electrode was recorded as Ni3N / Co3N / g-C3N4-ITO.
[0091] A double transition metal nitride heterojunction modified g-C3N4-based photoelectrochemical aptasensor was used to detect carbendazim pesticide residues in aquatic environments.
[0092] (4) Construction of Ni3N / Co3N / aptamer-ITO sensor:
[0093] Use a pipette to transfer 10 μL of carbendazim aptamer (sequence: 5′-CGACACAGCGGAGGCCACCCGCCCACCAGCCCCTGCAGCTCCTGTACCTGTGT GTGTG-3′, concentration: 2 μmol / L) and apply it on the surface of the Ni3N / Co3N / g-C3N4-ITO electrode prepared in step (3), incubate at room temperature for 8 h, rinse with deionized water, and continue to dry at room temperature to obtain a photoelectrochemical aptamer sensor, recorded as Ni3N / Co3N / g-C3N4-aptamer-ITO.
[0094] (5) Preparation of the target detection substance carbendazim: Carbendazim at concentrations of 0.01 nM, 0.1 nM, 1 nM, 10 nM, 100 nM and 1000 nM were prepared for testing.
[0095] (6) Photoelectrochemical detection methods and conditions: The electrochemical experiments used a CHI660E electrochemical workstation (Shanghai Chenhua Instrument Co., Ltd.) and a traditional three-electrode system: the modified electrode was the working electrode, the platinum wire electrode was the counter electrode, and the saturated Ag / AgCl electrode was the reference electrode. The excitation light source was a 300W xenon lamp (PLS-SXE300, Beijing Bofeilai Technology Co., Ltd.). The electrochemical experiments were all carried out at room temperature in a phosphate buffer solution (0.1 mol / L, pH = 7.0) without applying any bias. The EIS experiment was carried out in a solution containing 5 mmol / L Fe(CN)6 3- / 4- The experiment was carried out in a phosphate buffer solution (0.1 mol / L, pH=7.0) containing 0.1 mol / L KCl, with a frequency range of 0.01 Hz to 10 kHz, an initial potential of 0.24 V, and an AC amplitude of 5 mV.
[0096] The following is a detailed characterization of the material obtained in Example 1:
[0097] Figure 1 The X-ray diffraction (XRD) pattern of Ni3N / Ni3FeN / g-C3N4 composite material, where a is g-C3N4 and b is Ni3N / Ni3FeN / g-C3N4. The XRD pattern shows that g-C3N4 has a sharp peak at 27.7°, corresponding to the (002) plane generated by interlayer stacking reflection. Another weak peak is located at 13.1°, corresponding to the (100) plane in the plane of the continuous tri-s-triazine unit of g-C3N4. Ni3N, Ni3FeN and g-C3N4 species are found in the Ni3N / Ni3FeN / g-C3N4 composite material, corresponding to the Ni3N (PDF#10-0280) and Ni3FeN (PDF#50-1434) standard cards. The diffraction peaks at 39.2°, 41.5°, 44.6°, 58.5°, 70.9° and 78.1° correspond to the (110), (002), (111), (112), (300) and (113) crystal planes of Ni3N, respectively; the diffraction peaks at 41.5°, 48.3°, 70.8° and 85.6° belong to the (111), (200), (220) and (311) crystal planes of face-centered cubic Ni3FeN, respectively. In addition, the figure also shows that the diffraction peaks of Ni3N / Ni3FeN material are strong and the peak shape is sharp, indicating that the material has good crystallinity. XRD results confirm the successful synthesis of Ni3N / Ni3FeN / g-C3N4 composite material.
[0098] Figure 2 Figure 1 shows the transmission electron microscopy (TEM) and high magnification transmission electron microscopy (HRTEM) images of the Ni3N / Ni3FeN / g-C3N4 composite material, where a is the TEM image and b is the HRTEM image. Figure 2 As can be seen in a, the Ni3N / Ni3FeN heterostructure is uniformly loaded on the surface of g-C3N4. From HRTEM ( Figure 2 b), the composite material has obvious lattice fringes with lattice spacing of 0.20nm and 0.218nm, corresponding to the (111) crystal plane of Ni3N and the (111) crystal plane of Ni3FeN, respectively. In addition, the lattice cross distribution of Ni3N and Ni3FeN indicates that the Ni3N / Ni3FeN heterostructure is successfully formed.
[0099] Figure 3 This is the solid ultraviolet diffuse reflectance (DRS) diagram of the Ni3N / Ni3FeN / g-C3N4 composite material. Among them, a is g-C3N4, and b is Ni3N / Ni3FeN / g-C3N4. It can be clearly seen that the Ni3N / Ni3FeN / g-C3N4 composite material has a wide spectral response range, and the maximum absorption wavelength is broadened to ~559nm. This leads to an increase in the light absorption capacity of the material, indicating that the introduction of Ni3N / Ni3FeN significantly improves the utilization rate of visible light by the g-C3N4 material. At the same time, the presence of the Ni3N / Ni3FeN heterostructure is more conducive to the excitation of high-concentration carriers and enhances the photoelectric conversion efficiency.
[0100] Figure 4 Figure 1 is the X-ray photoelectron spectroscopy (XPS) diagram of Ni3N / Ni3FeN / g-C3N4 composite material, where a-d are high-resolution spectra of C1s, N 1s, Ni 2p and Fe 2p, respectively. Figure a is g-C3N4, and b is Ni3N / Ni3FeN / g-C3N4. The peaks of C 1s spectrum are located near 284.8 and 288 eV, which are attributed to CC / C=C and NC=N in g-C3N4. The three chemical states of N 1s near 398.50 eV, 399.5 eV and 400.7 eV correspond to C atoms (CN=C), (N-(C)3) and (CNH) species related to structural defects, respectively. Comparison of the Ni 2p and Fe 2p spectra of Ni3N / Ni3FeN and Ni3N / Ni3FeN / g-C3N4 composites shows that there are four peaks in the Ni 2p spectrum of the Ni3N / Ni3FeN / g-C3N4 composite, of which the peaks at 856.0 eV and 873.6 eV belong to Ni 2p, respectively. 3 / 2 and 2p 1 / 2, 862.2eV and 880.9eV are attributed to satellite peaks. In the Ni 2p spectrum of Ni3N / Ni3FeN, there are two additional peaks at 852.5eV and 869.7eV, indicating that the Ni3N / Ni3FeN heterostructure material may contain a small amount of nickel metal Ni. In the Fe 2p spectrum, the two peaks at 712.0 and 725.5eV belong to Fe 2p respectively. 3 / 2 and Fe 2p 1 / 2 The weak peaks at 706.7eV and 720.7eV represent the presence of a small amount of Fe metal, and there are two characteristic satellite peaks centered at 717.3eV and 733.4eV. In addition, from the comparison of Ni 2p and Fe 2p spectra of Ni3N / Ni3FeN and Ni3N / Ni3FeN / g-C3N4 composites, it can be seen that the metal binding energy has increased to varying degrees, indicating that after the heterostructure of g-C3N4 and Ni3N / Ni3FeN is composited, the strong electronic interaction between the two will cause the charge of g-C3N4 to move toward Ni3N / Ni3FeN, thereby reducing the surface charge density. The XPS results better verify the successful preparation of Ni3N / Ni3FeN / g-C3N4 composites.
[0101] Figure 5 The electrochemical impedance spectroscopy (EIS) diagram of the Ni3N / Ni3FeN / g-C3N4 composite material is shown in Figure 1. Among them, a is g-C3N4-ITO, b is Ni3N / Ni3FeN / g-C3N4-ITO, c is Ni3N / Ni3FeN / g-C3N4-aptamer-ITO, and d is Ni3N / Ni3FeN / g-C3N4-aptamer-PFF-ITO. The resistance of the material prepared by the present invention is detected by performing AC impedance test on the working electrode to further study the ability of the composite material to transfer electrons. The smaller the radius, the stronger its ability to transfer electrons. Figure 5 It can be seen that Ni3N / Ni3FeN / g-C3N4-ITO has the strongest charge transfer ability, because the heterostructure formed by Ni3N / Ni3FeN promotes the efficient transfer of photogenerated charges as an electron transfer bridge, which leads to better photoelectric performance of Ni3N / Ni3FeN / g-C3N4 composite materials. The PFF / Apt / Ni3N / Ni3FeN / g-C3N4 / ITO electrode shows an increased resistance value, which further illustrates the sensing mechanism that the combination of aptamer and PFF will hinder electron transfer.
[0102] Figure 6The photocurrent diagram of Ni3N / Ni3FeN / g-C3N4 composite materials, where a is g-C3N4-ITO, b is Ni3N / Ni3FeN / g-C3N4-ITO, c is Ni3N / Ni3FeN / g-C3N4-aptamer-ITO, and d is Ni3N / Ni3FeN / g-C3N4-aptamer-PFF-ITO. In order to explore the charge separation behavior of the samples and clarify the mechanism of enhanced photoelectric performance in Ni3N / Ni3FeN / g-C3N4 composite materials, the photoelectric performance of g-C3N4 and Ni3N / Ni3FeN / g-C3N4 composite materials was tested. As shown in the figure, the photoresponse current of g-C3N4 is lower, indicating that it has lower electron migration behavior. The photocurrent response of the Ni3N / Ni3FeN / g-C3N4 composite material is significantly improved, about 4 times that of g-C3N4, which improves the charge separation efficiency and verifies the mechanism by which Ni3N / Ni3FeN as a heterostructure enhances the photoelectric performance of g-C3N4. In addition, due to the synergistic effect between the two metals, the Ni3N / Ni3FeN / g-C3N4 composite material has a larger spatial area for electron regulation. Compared with the single transition metal nitride Ni3N / g-C3N4 composite material, the photocurrent response of the Ni3N / g-C3N4 composite material is only about 0.4 times that of the Ni3N / Ni3FeN / g-C3N4 composite material. This is mainly due to the unique surface configuration of the Ni3N / Ni3FeN heterostructure, which can produce a strong interaction with the g-C3N4 as a semiconductor, and can guide the electron transfer on the semiconductor. The electrons can be transferred to the surface of the Ni3N / Ni3FeN heterostructure through the semiconductor-heterogeneous interface, thereby efficiently transferring electrons and inhibiting the recombination of photogenerated electron-hole pairs, further demonstrating that the double transition metal nitride composite material has higher electron transfer efficiency and photoelectric activity. When the PFF aptamer is present, the photocurrent of the Apt / Ni3N / Ni3FeN / g-C3N4 / ITO electrode shows a downward trend. When PFF is specifically recognized by the aptamer modified on the electrode surface, the photocurrent of the Apt / Ni3N / Ni3FeN / g-C3N4 / ITO electrode continues to decrease. This is because the aptamer and PFF will form non-conductive macromolecules, produce steric hindrance, and inhibit the transfer of charge on the electrode surface. This result is consistent with the EIS graph results. These results show that the composite material is expected to be used to construct photoelectrochemical aptamer sensors and achieve efficient PFF detection.
[0103] Figure 7Figure 1 is the photoelectric signal response diagram of Ni3N / Ni3FeN / g-C3N4-aptamer-ITO detecting PFF, where a is the photocurrent diagram obtained by detecting different concentrations of PFF, and the PFF concentrations are 0.01nM, 0.1nM, 1nM, 10nM, 100nM and 1000nM respectively. b is the linear relationship diagram of the PFF concentration-photocurrent increment. Figure 7 It can be seen from a that with the increase of PFF concentration, the photocurrent signal of the sensor gradually decreases and shows a certain linear relationship. The linear range is 0.01nM~1000nM, and the linear equation is I(μA)=0.17712-0.02166log(C PFF / nM)(R 2 =0.995), the detection limit is 0.003nM, such as Figure 7 b.
[0104] Figure 8 Figure 1 shows the selectivity (a), stability (b) and repeatability (c) of Ni3N / Ni3FeN / g-C3N4-aptamer-ITO for detecting PFF. It can be seen that the sensor exhibits excellent selectivity, stability and reproducibility. Atrazine (ATZ), diazinon (DIA), cypermethrin (CYP), kewensan (KEW), imidacloprid (IMI) and omethoate (OME) were used as interfering species to investigate the selectivity of the sensor for detecting PFF target molecules. Figure a shows that in the presence of PFF aptamers, the photocurrent response of the sensor caused by interfering species is basically negligible. Thanks to the specific recognition between the PFF aptamer and PFF, the sensor shows obvious photocurrent changes for PFF, so the sensor has good anti-interference ability. After 600s of on-off light irradiation, the photocurrent of the sensor is in a stable trend, indicating that the sensor exhibits excellent stability (Figure b). At the same time, 5 identical Apt / Ni3N / Ni3FeN / g-C3N4 / ITO electrodes were prepared to test the reproducibility of the sensor. As can be seen from Figure c, the constructed sensor exhibits good reproducibility with a relative standard deviation (RSD) of 2.43%.
Claims
1. A method for constructing a double transition metal nitride heterojunction modified graphite phase carbon nitride-based photoelectrochemical aptamer sensor, It is characterized in that The steps are as follows (1)gC 3 N 4 Preparation of materials: A certain amount of carbon and nitrogen source was weighed into a covered crucible and gC was obtained by one-step calcination. 3 N 4 ; (2) Double transition metal nitride heterojunction modified gC 3 N 4 Preparation of materials First, transition metal salt 1, transition metal salt 2, urea and ammonium salt are dissolved in deionized water in proportion and fully dissolved to obtain solution A; Next, weigh the gC obtained in step (1). 3 N 4 The powder was dissolved in deionized water and fully dispersed to obtain solution B; Under continuous stirring, solution B was uniformly added to solution A, and the mixture was transferred into a polytetrafluoroethylene-lined reactor for constant temperature hydrothermal reaction. After the reaction was completed, the reactor was taken out and naturally cooled to room temperature. The sample was centrifuged, washed with water and alcohol for several times, and dried in vacuum to obtain a double transition metal LDH / gC 3 N 4 Precursor; Then, a certain amount of double transition metal LDH / gC 3 N 4 The precursor was calcined in a tube furnace with ammonia to obtain a double transition metal heterojunction / gC 3 N 4 Material; (3) Double transition metal nitride heterojunction modified gC 3 N 4 -Preparation of ITO electrode: A certain amount of double transition metal nitride heterojunction / gC 3 N 4 The composite material is dispersed in deionized water and evenly dispersed by ultrasound to obtain a stable suspension. The suspension is then drop-coated on the surface of the ITO conductive glass, dried naturally, rinsed with deionized water and dried at room temperature to obtain a double transition metal nitride heterojunction / gC 3 N 4 -ITO electrode DTMNH / gC 3 N 4 -ITO; (4)DTMNH / gC 3 N 4 Preparation of aptamer-ITO electrode: Take the carbendazim aptamer, omethoate aptamer or profenofos aptamer and apply it dropwise on the DTMNH / gC prepared in step (3). 3 N 4 -ITO photoelectrode surface, after incubation at room temperature for a certain period of time, the unanchored aptamers on the electrode surface were rinsed with deionized water and dried at room temperature to obtain DTMNH / gC 3 N 4 / aptamer-ITO photoelectrode sensor.
2. The construction method according to claim 1, It is characterized in that In step (1), the carbon and nitrogen source is one or more mixtures of thiourea, cyanamide, dicyandiamide, melamine or urea; the calcination temperature is 450-650° C., and the insulation time is 2-8 hours.
3. The construction method according to claim 1, It is characterized in that In step (2), The transition metal salt 1 is nickel chloride hydrate or nickel nitrate hydrate; One of the transition metal salts selected from ferric chloride hydrate, ferric nitrate hydrate, sodium metavanadate, cobalt nitrate hydrate or cobalt chloride; The ammonium salt is ammonium fluoride or hexamethylenetetramine; The transition metal salt 1, transition metal salt 2, ammonium salt, urea, gC 3 N 4 The dosage ratio is 0.01~1mmol:0.01~1mmol:0.01~1mmol:6mmol:0.01~5mmol; The constant temperature hydrothermal reaction temperature is 100-200°C, and the constant temperature reaction time is 8-24h; The flow rate of ammonia is 10-100 mL / min; the calcination temperature is 300-450° C., the calcination rate is 1-20° C. / min, and the insulation time is 2-8 h.
4. The construction method according to claim 1, wherein in step (3), the concentration of the suspension is 0.2 to 4 mg / mL, and the drop coating amount is 10 to 100 μL.
5. The construction method according to claim 1, in step (4), The carbendazim aptamer sequence is: 5′-CGACACAGCGGAGGCCACCCGCCCACCAGCCCCTGCAGCTCCGTAC CTGTGTGTGTG-3′; The omethoate aptamer sequence is: 5′-AGCTTGCTGCAGCGATTCTTGATCGCCACA GAGCT-3′; The sequence of the profenofos aptamer is: 5′-AAGCTTGCTTTAGCCTGCAGCGATTCTTGATCGGAAAAGGCTGAGA GCTACGC-3′.
6. The construction method according to claim 1, wherein in step (4), the concentration of the carbendazim aptamer, omethoate aptamer or profenofos aptamer is 0.1-5 μmol / L, and the drop-coating amount is 10-50 μL.
7. Use of the double transition metal nitride heterojunction modified graphite phase carbon nitride-based photoelectrochemical aptamer sensor prepared by the construction method according to any one of claims 1 to 6 for detecting organic pesticide residues in aquatic environments.
8. The use according to claim 7, It is characterized in that Here are the steps: (5) Determination of standard curve: The prepared DTMNH / gC 3 N 4 / aptamer-ITO electrode was used as the working electrode, Ag / AgCl as the reference electrode, Pt as the counter electrode, and phosphate buffer solution as the electrolyte. The photocurrent of the working electrode in the presence of known concentrations of carbendazim, omethoate or profenofos was tested under a certain bias voltage, and a series of concentration-photocurrent correspondences were obtained, and then the standard curve of the sensor for different concentrations of pesticides was obtained; (6) Take a certain amount of carbendazim, omethoate or propyl bromide and apply it on DTMNH / gC 3 N 4 / aptamer-ITO electrode surface, naturally dried at room temperature, rinsed with deionized water, and then dried at room temperature, and the photocurrent value was tested in the above electrolyte; and the photocurrent value was substituted into the standard curve for conversion to obtain the concentration of the pesticide in the test solution.
9. The use according to claim 8, It is characterized in that In step (5), the amount of carbendazim, omethoate or profenofos added is 10 to 100 μL, and the concentration is 1 fM to 1000 nM; In step (6), the amount of the carbendazim, omethoate or profenofos test solution to be applied is 10 to 100 μL.
10. The use according to claim 8, It is characterized in that In step (5) and step (6), the phosphate buffer solution is prepared by mixing 0.1-1M sodium dihydrogen phosphate and disodium hydrogen phosphate to make the pH value 7.0, and the concentration thereof is 0.1-2M.
Citation Information
Cited By
Antibiotic resistance gene photoelectric detection sensor as well as preparation method and application thereof
CN119959324A