Semiconductor structure preparation method and preparation system

In the integrated circuit contact hole interconnection process, the reaction source gas is reacted with the reducing gas to form a metal nitride layer, and the plasma treatment is used to remove impurities, the problem of low density of the barrier layer is solved and the lower resistance is achieved. and better device performance.

CN118943077APending Publication Date: 2024-11-12WUHAN CHUXING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310530466.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-10
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

In the integrated circuit contact hole interconnection process, the barrier layer of the metal nitride layer is low in density, resulting in high resistance and affecting device performance.

Method used

By reacting the reaction source gas with the reducing gas at a specific temperature, a metal nitride layer is formed, and impurities are removed by plasma treatment to form a high-density conductive layer.

Benefits of technology

The impurity content of the deposited metal nitride layer is reduced, the density is improved, the resistance is reduced, and the device performance is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118943077A_ABST
    Figure CN118943077A_ABST
Patent Text Reader

Abstract

The invention provides a preparation method and a preparation system of a semiconductor structure. The method comprises the following steps: providing a substrate; forming a dielectric layer on one side of the substrate; and etching the dielectric layer to form a channel penetrating through the dielectric layer to expose the surface of the substrate so as to facilitate the formation of a subsequent conductive interconnection structure. A reaction source gas and a reducing gas are mixed in advance and then are introduced into a reaction chamber, the reaction source gas and the reducing gas react at a first temperature, and a metal nitride layer is formed on the inner wall of a channel and the surface of an exposed substrate. And after the reaction source gas reacts with the reducing gas, volatile substances can be formed, so that the impurity content during deposition of the metal nitride layer is reduced, the compactness of the deposited metal nitride layer can be improved, the resistance can be reduced, and the performance of a device can be improved. And finally, forming a metal filling layer on one side, far away from the substrate, of the metal nitride layer, wherein the metal nitride layer and the metal filling layer form a conductive layer of an interconnection structure. Therefore, a semiconductor interconnection structure with good conductivity is formed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure preparation method and preparation system. Background Art

[0002] With the continuous development of integrated circuits, in the integrated circuit contact hole interconnection process, a metal nitride layer is usually used as a barrier layer for the contact hole filling metal to avoid diffusion of the contact hole filling metal.

[0003] Taking the metal nitride layer as a titanium nitride layer as an example, the conventional preparation of the titanium nitride barrier layer requires multiple cycles of deposition and plasma treatment. This treatment method has a poor effect on thinning the sidewalls of the contact holes, and the sidewall resistance is high, which affects the device performance.

[0004] Therefore, how to reduce impurities in the deposited barrier layer, improve the density of the deposited barrier layer, reduce resistance, and improve device performance in the integrated circuit contact hole interconnection process is a technical problem that needs to be solved in this field. Summary of the invention

[0005] In view of this, this summary of the invention is provided to introduce the concepts in a brief form, which will be described in detail in the detailed description section below. This summary of the invention is not intended to identify the key features or essential features of the technical solution claimed for protection, nor is it intended to be used to limit the scope of the technical solution claimed for protection.

[0006] The purpose of the present application is to provide a semiconductor structure preparation method and preparation system, which can reduce impurities in the deposited barrier layer, improve the density of the deposited barrier layer, reduce resistance, and improve device performance in the integrated circuit contact hole interconnection process.

[0007] To achieve the above purpose, this application has the following technical solutions:

[0008] In a first aspect, an embodiment of the present application provides a method for preparing a semiconductor structure, comprising:

[0009] providing a substrate;

[0010] forming a dielectric layer on one side of the substrate;

[0011] Etching the dielectric layer to form a channel penetrating the dielectric layer to expose the surface of the substrate;

[0012] Pre-mixing a reaction source gas with a reducing gas, and then introducing the mixture into a reaction chamber, wherein the reaction source gas reacts with the reducing gas at a first temperature to form a metal nitride layer on the inner wall of the channel and the exposed surface of the substrate;

[0013] A metal filling layer is formed on a side of the metal nitride layer away from the substrate, and the metal nitride layer and the metal filling layer form a conductive layer of an interconnect structure.

[0014] In a possible implementation manner, after forming the metal nitride layer and before forming the metal filling layer, the method further includes:

[0015] The formed metal nitride layer is treated by using a first plasma to remove impurities in the metal nitride layer.

[0016] In a possible implementation manner, the first plasma includes at least nitrogen plasma and hydrogen plasma.

[0017] In a possible implementation, the premixing of the reaction source gas with the reducing gas includes: mixing the reducing gas with a diluent gas to obtain a first mixed gas, and before entering the reaction chamber, fully mixing the first mixed gas with the reaction source gas to obtain a second mixed gas.

[0018] In a possible implementation, after obtaining the second mixed gas and before introducing the second mixed gas into the reaction chamber, the process further includes:

[0019] The second mixed gas is preheated at a second temperature to pass the preheated second mixed gas into the reaction chamber. In a possible implementation, the first temperature range is [380° C., 450° C.], and the second temperature range is [80° C., 100° C.].

[0020] In a possible implementation, the forming of the reaction source gas includes: using a carrier gas at a third temperature to carry a liquid reaction source, and converting the liquid reaction source into the gaseous reaction source gas.

[0021] In a second aspect, an embodiment of the present application provides a preparation system using the semiconductor structure preparation method as described above, the preparation system comprising:

[0022] a reaction chamber, in which the substrate is placed;

[0023] A first pipeline, connected to the reaction chamber, for delivering the reaction source gas to the reaction chamber;

[0024] a second pipeline, connected to the first pipeline, and used to transport reducing gas to the first pipeline;

[0025] A temperature control device is used to adjust the temperature of the reaction chamber and the first pipeline.

[0026] In a possible implementation, the preparation system further includes:

[0027] A storage device, used for storing a reaction source, and the storage device is connected to the first pipeline;

[0028] The third pipeline is connected to the storage device and is used to introduce a carrier gas into the storage device to transport the liquid reaction source to the first pipeline.

[0029] In a possible implementation, the preparation system further includes:

[0030] a gasification valve, a mixing valve and a fourth pipeline, wherein the gasification valve is located on the first pipeline and the mixing valve is located on the second pipeline;

[0031] The fourth pipeline is used to transport the dilution gas to the mixing valve; the mixing valve is used to mix the dilution gas and the reducing gas to obtain a first mixed gas;

[0032] The second pipeline introduces the first mixed gas into the first pipeline, and mixes the first mixed gas with the reaction source carried by the carrier gas to obtain a second mixed gas.

[0033] Compared with the prior art, the embodiments of the present application have the following beneficial effects:

[0034] The embodiment of the present application provides a method and system for preparing a semiconductor structure, which includes: providing a substrate; forming a dielectric layer on one side of the substrate; etching the dielectric layer to form a channel penetrating the dielectric layer to expose the surface of the substrate for subsequent formation of a conductive interconnection structure. After the reaction source gas is mixed with the reducing gas in advance, it is introduced into the reaction chamber. At a first temperature, the reaction source gas reacts with the reducing gas to form a metal nitride layer on the inner wall of the channel and the surface of the exposed substrate. Since the reaction source gas reacts with the reducing gas to form a volatile substance, the impurity content during the deposition of the metal nitride layer is reduced, the compactness of the deposited metal nitride layer can be improved, the resistance can be reduced, and the device performance can be improved. Finally, a metal filling layer is formed on the side of the metal nitride layer away from the substrate, and the metal nitride layer and the metal filling layer form a conductive layer of the interconnection structure. In order to form a semiconductor interconnection structure with good conductive properties. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0036] The above and other features, advantages and aspects of the embodiments of the present disclosure will become more apparent with reference to the following detailed description in conjunction with the accompanying drawings. Throughout the accompanying drawings, the same or similar reference numerals represent the same or similar elements. It should be understood that the drawings are schematic and the originals and elements are not necessarily drawn to scale.

[0037] Figure 1 A schematic diagram of performing barrier layer deposition in an interconnect channel provided by an embodiment of the present application is shown;

[0038] Figure 2 A flow chart showing a method for preparing a semiconductor structure provided in an embodiment of the present application is shown;

[0039] Figure 3 A schematic diagram of a semiconductor structure provided by an embodiment of the present application is shown;

[0040] Figure 4 A schematic diagram of another semiconductor structure provided by an embodiment of the present application is shown;

[0041] Figure 5 A schematic diagram of another semiconductor structure provided by an embodiment of the present application is shown;

[0042] Figure 6 A schematic diagram of another semiconductor structure provided by an embodiment of the present application is shown;

[0043] Figure 7 A schematic diagram of another semiconductor structure provided by an embodiment of the present application is shown;

[0044] Figure 8 A schematic diagram of a semiconductor system provided by an embodiment of the present application is shown;

[0045] Fig. 9 A schematic diagram of another semiconductor system provided by an embodiment of the present application is shown. DETAILED DESCRIPTION

[0046] In order to make the above-mentioned objects, features and advantages of the present application more obvious and easy to understand, the specific implementation methods of the present application are described in detail below with reference to the accompanying drawings.

[0047] In the following description, many specific details are set forth to facilitate a full understanding of the present application, but the present application may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present application. Therefore, the present application is not limited to the specific embodiments disclosed below.

[0048] As described in the related art, in order to solve the problem that in the integrated circuit contact hole interconnection process, there are more impurities in the barrier layer formed by thermal decomposition, resulting in lower density of the barrier layer, larger resistance, and further leading to poor device performance, the present application proposes a semiconductor structure preparation method and system, by reacting the reaction source gas with the reducing gas to form a metal nitride layer as a barrier layer, volatile substances can be formed in the reaction, thereby reducing the impurity content when depositing the metal nitride layer, which can improve the density of the deposited metal nitride layer, reduce resistance, and improve device performance.

[0049] See also Figure 1 As shown, it is a schematic diagram of barrier layer deposition in an interconnection channel, a dielectric layer 2 is formed on a substrate 1, a metal 3 is deposited as an adhesion layer and a metal nitride layer 4 is deposited as a barrier layer in the interconnection channel 31 of the dielectric layer 2 in sequence.

[0050] Taking the material of the metal nitride layer 4 as titanium nitride as an example, the material used for the deposition of the titanium nitride layer is TDMAT [Tetrakis dimethylamino titanium, tetrakis (dimethylamino) titanium], and the molecular formula is Ti[N(CH3)2]4. When the temperature is greater than 350°C, TDMAT is thermally decomposed into TiN. At this time, the deposited titanium nitride barrier layer contains a large amount of impurity carbon, the film is loose, and the resistivity is very high (50000μΩ·cm). For example, see Figure 1 As shown, the metal nitride layer 4 contains impurities, including TiN(C) and (CH3)2·NH2 in addition to TiN. The deposition of titanium nitride by MOCVD (Metal-organic Chemical Vapor Deposition) dominated by TDMAT generally has two steps. The titanium nitride generated by the thermal reaction alone has an amorphous structure and contains a large amount of carbon and hydrogen elements.

[0051] Therefore, N2 and / or H2 plasma treatment is required to remove impurities and transform amorphous into amorphous through plasma treatment, thereby reducing resistance (300μΩ·cm) and improving the density of the deposited titanium nitride barrier layer. In order to ensure the barrier effect, the barrier layer must have a corresponding thickness. Since the plasma penetration depth is lower than Therefore, during the preparation of the TiN film, it is necessary to cycle through the two steps of deposition and plasma treatment multiple times to reduce the overall impurity content of the TiN layer. This treatment method has a poor effect on thinning the side walls of the contact holes, and the side wall resistance is high, which affects the device performance.

[0052] Based on the above technical problems, the embodiment of the present application provides a method and system for preparing a semiconductor structure, which includes: providing a substrate; forming a dielectric layer on one side of the substrate; etching the dielectric layer to form a channel penetrating the dielectric layer to expose the surface of the substrate for the subsequent formation of a conductive interconnection structure. After the reaction source gas is mixed with the reducing gas in advance, it is introduced into the reaction chamber. At a first temperature, the reaction source gas reacts with the reducing gas to form a metal nitride layer on the inner wall of the channel and the surface of the exposed substrate. Since the reaction source gas reacts with the reducing gas to form a volatile substance, the impurity content during the deposition of the metal nitride layer is reduced, the compactness of the deposited metal nitride layer can be improved, the resistance can be reduced, and the device performance can be improved. Finally, a metal filling layer is formed on the side of the metal nitride layer away from the substrate, and the metal nitride layer and the metal filling layer form a conductive layer of the interconnection structure. In order to form a semiconductor interconnection structure with good conductive properties.

[0053] In order to better understand the technical solution and technical effects of the present application, specific embodiments will be described in detail below with reference to the accompanying drawings.

[0054] Exemplary Methods

[0055] See also Figure 2 As shown, Figure 2 A flowchart of a method for preparing a semiconductor structure provided in an embodiment of the present application includes:

[0056] S101: providing a substrate;

[0057] S102: forming a dielectric layer on one side of the substrate;

[0058] S103: etching the dielectric layer to form a channel penetrating the dielectric layer to expose the surface of the substrate.

[0059] In the examples of this application, see Figure 3 As shown, it is a schematic diagram of a semiconductor structure provided in an embodiment of the present application, and the substrate 1 can be a semiconductor substrate, for example, it can be a Si substrate, a Ge substrate, a SiGe substrate, SOI (Silicon On Insulator) or GOI (Germanium On Insulator), etc. In other embodiments, the semiconductor substrate can also be a substrate including other element semiconductors or compound semiconductors, such as GaAs, InP or SiC, etc., and can also be a stacked structure, such as Si / SiGe, etc., and can also be other epitaxial structures, such as SGOI (Silicon Germanium On Insulator), etc. In this embodiment, the substrate 1 is a bulk silicon substrate.

[0060] The dielectric layer 2 may be made of an insulating material. For example, the material of the dielectric layer 2 may include at least one of a silicon oxide layer, a silicon nitride layer and a silicon oxynitride layer. Optionally, in this embodiment, the dielectric layer 2 is a silicon oxide layer.

[0061] In order to form a subsequent interconnection structure, the embodiment of the present application can etch the dielectric layer 2 to form a channel 31 that penetrates the dielectric layer. The channel 31 penetrates the dielectric layer 2 along the thickness direction to expose the upper surface of the substrate 1.

[0062] Optionally, the channel 31 may include a through hole or a groove, which is not specifically limited in the embodiment of the present application and may be specifically set by those skilled in the art according to the shape of the actual interconnection structure.

[0063] S104: Pre-mixing a reaction source gas with a reducing gas and introducing the mixture into a reaction chamber, wherein the reaction source gas reacts with the reducing gas at a first temperature to form a metal nitride layer on the inner wall of the channel and the exposed surface of the substrate;

[0064] S105: forming a metal filling layer on a side of the metal nitride layer away from the substrate, the metal nitride layer and the metal filling layer forming a conductive layer of an interconnect structure.

[0065] See also Figure 4 , which is a schematic diagram of another semiconductor structure provided in an embodiment of the present application.

[0066] That is, in the embodiment of the present application, the reaction source gas and the reducing gas can react at the first temperature to form the metal nitride layer 4 on the inner wall of the channel 31 and the surface of the exposed substrate 1. In the embodiment of the present application, the reaction source gas and the reducing gas are mixed in advance and then introduced into the reaction chamber, so that the reaction source gas and the reducing gas can be mixed more fully, so as to fully react later and better reduce impurities in the formed metal nitride layer 4.

[0067] Since the reaction source gas reacts with the reducing gas, volatile substances can be generated, thereby reducing the impurity content when depositing the metal nitride layer 4, thereby improving the density of the deposited metal nitride layer 4, reducing resistance, and improving device performance.

[0068] Optionally, the reaction source gas may be a metal organic nitride. Taking the reaction source gas as tetrakis(dimethylamino)titanium and the reducing gas as hydrogen as an example, the reaction principle of tetrakis(dimethylamino)titanium and hydrogen is:

[0069]

[0070] Among them, R in HNR2 refers to a hydrocarbon group (a group containing only carbon and hydrogen atoms).

[0071] In another possible implementation, the reaction source gas may also be tetrakis diethylamino titanium (TDEAT).

[0072] That is, in the embodiment of the present application, the reaction source gas and the reducing gas can be thermally decomposed into the metal nitride layer 4 at a high temperature, that is, the first temperature provided in the embodiment of the present application is greater than or equal to 380°C and less than or equal to 450°C.

[0073] Taking the metal nitride layer 4 as TiN as an example, the impurities at this time only include TiN (C), and the other reaction products can be volatilized. The impurities are removed in advance during the thermal decomposition reaction, thereby reducing the impurity content in the metal nitride layer 4, and a thinner, higher purity and better density metal nitride layer 4 can be obtained, effectively reducing the thickness of the metal nitride layer 4 on the side wall of the channel 31, which can reduce resistance and improve the process window.

[0074] Finally, see Figure 5 , which is a schematic diagram of another semiconductor structure provided by an embodiment of the present application. A metal filling layer 5 is formed on the side of the metal nitride layer 4 away from the substrate 1. The metal nitride layer 4 and the metal filling layer 5 form a conductive layer of the interconnect structure, so as to form a semiconductor interconnect structure with good conductive properties. Optionally, the metal filling layer 5 may include a metal material such as tungsten.

[0075] It should be noted that the embodiment of the present application does not specifically limit the deposition process of the metal filling layer 5. For example, it may include deposition processes such as chemical vapor deposition (CVD), physical vapor deposition (PVD) or atomic layer deposition (ALD), and the specific setting can be made by technical personnel in this field according to actual conditions.

[0076] In a possible implementation, after forming the metal nitride layer 4 and before forming the metal filling layer 5, the method provided in the embodiment of the present application may further include:

[0077] The formed metal nitride layer 4 is treated with the first plasma to remove impurities in the metal nitride layer 4 .

[0078] Specifically, in the embodiment of the present application, the first plasma can be used to react with the carbon impurities and / or hydrogen impurities in the metal nitride layer 4 to remove the carbon impurities and / or hydrogen impurities.

[0079] That is, in the embodiment of the present application, since the metal nitride layer 4 obtained by thermal decomposition of the reaction source gas and the reducing gas still contains a small amount of carbon impurities and / or hydrogen impurities, in order to further improve the purity and density of the metal nitride layer 4, the metal nitride layer 4 can be plasma treated to remove the remaining impurities.

[0080] The first plasma provided in the embodiment of the present application may include at least nitrogen plasma and hydrogen plasma. For example, when hydrogen impurities are present, nitrogen plasma may be used to generate volatile ammonia for volatilization; when carbon impurities are present, hydrogen plasma may be used to generate volatile methane for volatilization. This further reduces the resistance and thickness of the metal nitride layer 4.

[0081] At the same time, since the thickness of the metal nitride layer 4 is thinned by thermal decomposition of the reaction source gas and the reducing gas in advance in the embodiment of the present application, the number of plasma treatments of the metal nitride layer 4 can be reduced, thereby improving the efficiency of preparing the semiconductor structure and saving energy consumption.

[0082] In a possible implementation, the pre-mixing of the reaction source gas and the reducing gas provided in the embodiment of the present application may specifically include: mixing the reducing gas with the diluent gas to obtain a first mixed gas, and before entering the reaction chamber, fully mixing the first mixed gas with the reaction source gas to obtain a second mixed gas. That is, in the embodiment of the present application, taking hydrogen as the reducing gas as an example, since there is also oxygen in the reaction chamber, hydrogen and oxygen will explode when encountering an open flame, and after the inactive diluent gas is filled, the gas inside the reaction chamber will be diluted to obtain the first mixed gas, so that the concentration of hydrogen is reduced to outside the explosion limit, thereby avoiding explosion and improving the safety of the semiconductor structure preparation process.

[0083] At the same time, before entering the reaction chamber, the first mixed gas can be fully mixed with the reaction source gas to obtain a second mixed gas, so that the reaction source gas and the reducing gas are mixed more fully, so as to fully react later and better reduce impurities in the formed metal nitride layer 4.

[0084] In a possible implementation, after obtaining the second mixed gas and before introducing the second mixed gas into the reaction chamber, the embodiment of the present application may further include:

[0085] The second mixed gas is preheated at the second temperature to pass the preheated second mixed gas into the reaction chamber.

[0086] Specifically, the second mixed gas can be preheated before entering the reaction chamber in the embodiment of the present application, so that the second mixed gas can be fully reacted after preheating. At the same time, preheating can promote the decomposition of the reaction source gas in the second mixed gas to a certain extent, decompose some volatile gases, and further reduce impurities in the metal nitride layer 4 formed subsequently.

[0087] Optionally, the first temperature range of the embodiment of the present application may be [380°C, 450°C], and the second temperature range may be [80°C, 100°C]. Thus, after preheating, the reaction is carried out, and the temperature gradually rises from the medium-temperature second temperature to the high-temperature first temperature, which can avoid the temperature fluctuation, thereby achieving a more complete and thorough reaction.

[0088] In a possible implementation, the formation of the reaction source gas in the embodiment of the present application may specifically include: using a carrier gas at a third temperature to carry a liquid reaction source, and converting the liquid reaction source into a gaseous reaction source gas.

[0089] That is, in the embodiment of the present application, since the gaseous reaction source gas is more likely to fully react with the reducing gas and can more fully remove impurities, the third temperature carrier gas can be used to carry the liquid reaction source into the gasification valve and converted into a gaseous reaction source gas. Optionally, the third temperature range can be [65°C, 110°C], so that the liquid reaction source can be preheated so that it can be vaporized more smoothly in the gasification valve.

[0090] It should be noted that the embodiment of the present application does not specifically limit the type of carrier gas, for example, it may include inert gases such as He, and the specific setting can be made by those skilled in the art according to actual conditions.

[0091] In one possible implementation, see Figure 6 As shown, it is a schematic diagram of another semiconductor structure provided by an embodiment of the present application. In the embodiment of the present application, a deposited metal 3 may be further included between the metal nitride layer 4 and the substrate 1 as an adhesive layer to achieve better contact between the metal nitride layer 4 and the substrate 1, reduce contact resistance, and avoid the fall-off defects caused by poor adhesion between the film layers affecting the device performance. Optionally, the type of metal 3 may be consistent with the type of metal in the metal nitride layer 4.

[0092] In the examples of this application, see Figure 7As shown, it is a schematic diagram of another semiconductor structure provided by the embodiment of the present application. The embodiment of the present application can form a stacked structure of a metal layer, a metal nitride layer 4 and a metal layer as a barrier layer of the semiconductor structure provided by the embodiment of the present application. In addition, the chemical mechanical polishing (CMP) process can be used to planarize the formed structure, and the redundant film layer structure located above the dielectric layer 2 can be polished away; the film layer structure located above the dielectric layer 2 includes: metal 3, metal nitride layer 4 and filling metal layer 5; after CMP removes these film layer structures, as shown in FIG. Figure 7 As shown, the remaining metal 3, the metal nitride layer 4 and the metal filling layer 5 located in the channel 31 together form an interconnection structure.

[0093] An embodiment of the present application provides a method for preparing a semiconductor structure. Since a reaction source gas can form a volatile substance after reacting with a reducing gas, the impurity content during the deposition of a metal nitride layer is reduced, the density of the deposited metal nitride layer can be improved, the resistance can be reduced, and the device performance can be improved.

[0094] Exemplary Systems

[0095] See also Figure 8 As shown, Figure 8 A schematic diagram of a manufacturing system for a semiconductor structure manufacturing method as described above provided in an embodiment of the present application includes:

[0096] A reaction chamber 9 in which a substrate 1 is placed; a first pipeline 11 connected to the reaction chamber 9 for conveying a reaction source gas to the reaction chamber 9; and a second pipeline 12 connected to the first pipeline 11 for conveying a reducing gas to the first pipeline 11.

[0097] The temperature control device (not shown in the figure) is used to adjust the temperature of the reaction chamber 9 and the first pipeline 11.

[0098] That is, in the embodiment of the present application, a first pipeline 11 and a second pipeline 12 can be added to achieve the mixing of the reaction source gas and the reducing gas and then transport them to the reaction chamber 9 for a thermal decomposition reaction. During the thermal decomposition reaction, impurities are removed in advance, thereby reducing the content of impurities in the metal nitride layer 4, and obtaining a thinner, purer and denser metal nitride layer 4, thereby reducing resistance and improving the performance of devices prepared using the system.

[0099] For details, see Figure 1 and Figure 4 As shown, taking the metal nitride layer 3 as a TiN layer as an example, Figure 1It is a schematic diagram of the structure after TDMAT thermal decomposition and plasma treatment in the existing process. The TiN layer generated by direct thermal decomposition of TDMAT contains more impurities, such as impurities including TiN(C) and (CH3)2·NH2. The formed TiN layer contains more impurities, the thickness a of the metal nitride layer 3 is thicker, and the resistance is higher, which affects the device performance.

[0100] See also Figure 4 , is a schematic diagram of the structure of the metal nitride layer 3 generated by a mixture of a reaction source gas and a reducing gas in an embodiment of the present application and after plasma treatment. The metal nitride layer 3 generated by a mixture of a reaction source gas and a reducing gas has fewer impurities, for example, only contains C impurities of TiN(C). The thickness b of the metal nitride layer 3 is thinner and the resistance is smaller, thereby improving the device performance.

[0101] In one possible implementation, see Figure 8 As shown, the system provided in the embodiment of the present application may also include:

[0102] The storage device 6 is used to store the reaction source, and the storage device 6 is connected to the first pipeline 11;

[0103] The third pipeline 13 is connected to the storage device 6 and is used to introduce carrier gas into the storage device 6 to transport the reaction source to the first pipeline 11. Optionally, the storage device 6 may include an ampoule bottle to facilitate storage of liquid reaction sources.

[0104] That is, in the embodiment of the present application, since the reaction source is generally liquid at room temperature, it can be stored in the storage device 6. When it is needed, the liquid reaction source is taken out of the storage device 6 by the carrier gas. The reaction source can also be in other forms, which can be adjusted according to the specific reaction source.

[0105] In one possible implementation, see Figure 8 As shown, the system provided in the embodiment of the present application may also include:

[0106] Gasification valve 8, mixing valve 7 and fourth pipeline 14, gasification valve 8 is located on first pipeline 11, mixing valve 7 is located on second pipeline 12; fourth pipeline 14 is used to transport dilution gas to mixing valve 7; mixing valve 7 is used to mix dilution gas 7 and reducing gas 7 to obtain first mixed gas;

[0107] The second pipeline 12 passes the first mixed gas into the first pipeline 11, and mixes it with the reaction source carried by the carrier gas to obtain a second mixed gas.

[0108] That is, in the embodiment of the present application, since the gaseous reaction source gas is easier to achieve a full reaction with the reducing gas and can remove impurities more fully, a gasification valve 8 can be set to convert the liquid reaction source into a gaseous reaction source gas so that the reaction can be more fully carried out.

[0109] At the same time, the mixing valve 7 and the fourth pipeline 14 are added to mix the dilution gas with the reduction gas, thereby reducing the explosion risk during the preparation of the semiconductor structure and improving the safety of the preparation.

[0110] Optional, see Figure 8 As shown, the third pipeline 13 can be arranged above the liquid level, and the first pipeline 11 can be arranged below the liquid level, so that the carrier gas directly presses the liquid reaction source into the first pipeline 11. Alternatively, see Fig. 9 As shown, the third pipeline 13 can also be arranged below the liquid surface, and the first pipeline 11 can be arranged above the liquid surface, so that the carrier gas goes up from the bottom of the liquid and carries the liquid reaction source into the first pipeline.

[0111] Each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the system embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.

[0112] The above is only a preferred implementation of the present application. Although the present application has been disclosed as a preferred embodiment, it is not intended to limit the present application. Any technician familiar with the art can use the above disclosed methods and technical contents to make many possible changes and modifications to the technical solution of the present application without departing from the scope of the technical solution of the present application, or modify it into an equivalent embodiment of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments based on the technical essence of the present application without departing from the content of the technical solution of the present application still falls within the scope of protection of the technical solution of the present application.

Claims

1. A method for preparing a semiconductor structure, It is characterized in that include: providing a substrate; forming a dielectric layer on one side of the substrate; Etching the dielectric layer to form a channel penetrating the dielectric layer to expose the surface of the substrate; Pre-mixing a reaction source gas with a reducing gas, and then introducing the mixture into a reaction chamber, wherein the reaction source gas reacts with the reducing gas at a first temperature to form a metal nitride layer on the inner wall of the channel and the exposed surface of the substrate; A metal filling layer is formed on a side of the metal nitride layer away from the substrate, and the metal nitride layer and the metal filling layer form a conductive layer of an interconnect structure.

2. The method according to claim 1, It is characterized in that After forming the metal nitride layer and before forming the metal filling layer, the method further includes: The formed metal nitride layer is treated by using a first plasma to remove impurities in the metal nitride layer.

3. The method according to claim 2, It is characterized in that The first plasma includes at least nitrogen plasma and hydrogen plasma.

4. The method according to claim 1, It is characterized in that The premixing of the reaction source gas with the reducing gas includes: mixing the reducing gas with a diluent gas to obtain a first mixed gas, and before entering the reaction chamber, fully mixing the first mixed gas with the reaction source gas to obtain a second mixed gas.

5. The method according to claim 4, It is characterized in that After obtaining the second mixed gas and before introducing the second mixed gas into the reaction chamber, the method further includes: The second mixed gas is preheated at a second temperature to pass the preheated second mixed gas into the reaction chamber.

6. The method according to claim 5, It is characterized in that The first temperature range is [380° C., 450° C.], and the second temperature range is [80° C., 100° C.].

7. The method according to claim 1, It is characterized in that The forming of the reaction source gas includes: using a carrier gas at a third temperature to carry a liquid reaction source, and converting the liquid reaction source into the gaseous reaction source gas.

8. A preparation system using the semiconductor structure preparation method according to claims 1 to 7, It is characterized in that The preparation system comprises: a reaction chamber, in which the substrate is placed; A first pipeline, connected to the reaction chamber, for delivering the reaction source gas to the reaction chamber; a second pipeline, connected to the first pipeline, and used to transport reducing gas to the first pipeline; A temperature control device is used to adjust the temperature of the reaction chamber and the first pipeline.

9. The preparation system according to claim 8, It is characterized in that The preparation system also includes: A storage device, used for storing a reaction source, and the storage device is connected to the first pipeline; The third pipeline is connected to the storage device and is used to introduce a carrier gas into the storage device to transport the reaction source to the first pipeline.

10. The preparation system according to claim 9, It is characterized in that The preparation system further comprises: a gasification valve, a mixing valve and a fourth pipeline, wherein the gasification valve is located on the first pipeline, and the mixing valve is located on the second pipeline; The fourth pipeline is used to transport the dilution gas to the mixing valve; the mixing valve is used to mix the dilution gas and the reducing gas to obtain a first mixed gas; The second pipeline introduces the first mixed gas into the first pipeline, and mixes the first mixed gas with the reaction source carried by the carrier gas to obtain a second mixed gas.