Continuous casting device for extra-thick slabs

By designing a super-thick slab continuous casting device, the concave and straight working surface structure of narrow-face copper plates, combined with the guide support mechanism, the problems of double drum defects and corner cracks are solved, and the material yield and production efficiency of thick plates are improved .

CN118950964APending Publication Date: 2024-11-15NORTHEASTERN UNIV CHINA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411055196.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the rolling process of extra-thick slabs, double drum shape defects cause the depth of the drum joint in the middle of the narrow surface of the steel plate to reach 30-80mm, resulting in a decrease in material yield and production efficiency. It is necessary to cut edges at the deepest position of the drum joint, bringing economics to the enterprise loss.

Method used

Design a very thick slab continuous casting device, including a pair of wide-side copper plates and a pair of narrow-side copper plates. The first working face of the narrow-side copper plate is a concave structure and the second working face is a straight structure, and the guide support mechanism is used. Support the forming of the casting blank, forming a narrow surface convex and right angles at the corners to avoid double-bulb defects and corner cracks during the rolling process.

Benefits of technology

After rolling, the double-drum drum joint depth of the casting billet becomes shallow, the amount of edge cutting of the steel plate is reduced, the material yield of thick plates is improved, and the occurrence of corner cracks in the casting billet is avoided, and the production efficiency and product quality are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118950964A_ABST
    Figure CN118950964A_ABST
Patent Text Reader

Abstract

The invention provides an extra-thick slab continuous casting device which comprises a crystallizer and a guide supporting mechanism, the crystallizer comprises a pair of wide-face copper plates and a pair of narrow-face copper plates, and the pair of wide-face copper plates and the pair of narrow-face copper plates form an internal space for molten steel to be solidified into a casting blank; the side, close to the casting blank, of the narrow-face copper plate is provided with a first working face and two second working faces, and the two second working faces are connected with the first working face; the cross section of the first working face is a concave arc line, the midpoint of the concave arc line coincides with the transverse center line of the first working face, the two second working faces are symmetrically arranged with the transverse center line of the first working face as the symmetric center, and the two second working faces are further perpendicular to the wide-face copper plate; wherein the guiding and supporting mechanism is arranged at a lower opening of the narrow-face copper plate, comprises 3-6 guiding and supporting rollers with the characteristics that the two ends are cylindrical and the middle part is reduced, and is used for producing the extra-thick casting blank with the narrow-face middle part being a convex cambered surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the technical field of metal casting, and in particular relates to a continuous casting device for extra-thick slabs. Background Art

[0002] Double-drum deformation is a defect parallel to the rolling direction that occurs at the edge during the rolling process of extra-thick slabs. This type of defect is located on the narrow side of the steel plate, and the narrow side of the steel plate is double-drum shaped. After rolling, the depth of the drum seam in the middle of the narrow side of the steel plate caused by the double-drum defect ranges from 30 to 80 mm. In the actual production process, it is necessary to trim the edge at the deepest position of the drum seam, which leads to a decrease in the yield rate and production efficiency of the thick plate, causing huge economic losses to the enterprise. Therefore, eliminating the double-drum defect is an important aspect of improving the yield rate of thick plates. Summary of the invention

[0003] Therefore, the technical problem to be solved by the present application is to provide a super thick slab continuous casting device, which can realize the production of slabs with an arc-shaped convex middle narrow surface and defect-free corners by setting the first working surface to be concave and the second working surface to be straight.

[0004] In order to solve the above problems, the present application provides an ultra-thick slab continuous casting device, comprising a crystallizer, the crystallizer comprising a pair of wide copper plates and a pair of narrow copper plates, the pair of wide copper plates each extending in one direction and being installed to face each other in a direction intersecting the extending direction, the pair of narrow copper plates respectively extending to intersect with the wide copper plates, and the pair of narrow copper plates being installed to face each other, thereby sealing a portion between the pair of wide copper plates to form an internal space for molten steel to solidify into a cast billet;

[0005] The narrow copper plate has a first working surface and a second working surface on one side close to the ingot, wherein two second working surfaces are provided, one second working surface is provided on one side of the first working surface, and the other second working surface is provided on the other side of the first working surface, and the first working surface is connected to the two second working surfaces respectively;

[0006] The cross-section of the first working surface is a concave arc, the midpoint of the concave arc coincides with the transverse center line of the first working surface, the two second working surfaces are symmetrically arranged with the transverse center line of the first working surface as the center of symmetry, and the two second working surfaces are also perpendicular to the wide copper plate.

[0007] Optionally, the ultra-thick slab continuous casting device further comprises a guide support mechanism, and the guide support mechanism is arranged at the lower opening of the narrow copper plate;

[0008] The guide support mechanism comprises a guide support roller, the guide support roller comprises a first section, the first section comprises two diameter reduction sections, the diameters of the two diameter reduction sections are gradually reduced in the direction facing each other, so that the roller surface of the guide support roller contacting the casting billet is in a concave arc line which is the same as the cross section of the first working surface, so as to support the casting billet of the narrow convex part formed by the first working surface;

[0009] The guide support roller also includes a second section, two of which are arranged on both sides of the first section along the axial direction of the first section, the first section is connected to the two second sections respectively, and the two second sections are cylindrical, so that the two second sections are suitable for supporting the narrow straight part of the cast billet formed under the action of the two second working surfaces.

[0010] Optionally, the guide support rollers are provided in two rows, and the guide support rollers in the two rows are arranged symmetrically.

[0011] Optionally, the narrow copper plate has a width that gradually decreases in a downward direction.

[0012] Optionally, the narrow copper plate includes a thickness reduction zone, which is arranged near the lower opening of the narrow copper plate, has a height of 50 mm to 200 mm, and has a thickness that gradually decreases in a downward direction.

[0013] Optionally, the narrow copper plate has a cooling surface on a side facing away from the ingot;

[0014] A first cooling water tank is provided on the cooling surface at a position relative to the first working surface;

[0015] A second cooling water trough is provided on the cooling surface at a position relative to the second working surface;

[0016] A plurality of the first cooling water troughs are provided, and two second cooling water troughs are provided. The plurality of the first cooling water troughs are located between two of the second cooling water troughs and are arranged at equal intervals.

[0017] Optionally, the first cooling water trough is a straight water trough, and the first cooling water trough is perpendicular to the cooling surface;

[0018] The second cooling water trough is an inclined water trough, and the second cooling water trough is inclined in a direction away from the first cooling water trough.

[0019] Optionally, the bottoms of several of the first cooling water troughs are located on the same arc surface, and the cross-section of the arc surface is parallel to the cross-section of the first working surface.

[0020] Optionally, the distance between the transverse center line of the bottom of the first cooling water trough and the first working surface complies with the formula:

[0021] D=h 1 +h 2

[0022] In the formula, h 1 h is the maximum thickness of the narrow copper plate, ranging from 10 mm to 20 mm; 2 It is the safe distance between the bottom of the first cooling water trough and the first working surface at the maximum use thickness, and its value is 8mm to 15mm.

[0023] Optionally, the spacing distance between the bottom of the second cooling water trough and the second working surface is smaller than the spacing distance between the bottom of the first cooling water trough and the first working surface by 1 mm to 3 mm.

[0024] Beneficial Effects

[0025] The extra-thick slab continuous casting device provided in the embodiment of the present invention can realize the production of slabs with narrow surfaces having convex structures by setting the first working surface of the narrow copper plate contacting the slab as an inner concave structure, thereby causing the depth of the double-drum seam of the slab after rolling to become shallower, reducing the trimming amount of the steel plate, and thereby improving the yield rate of the thick plate; at the same time, by setting the second working surfaces on both sides of the first working surface as a straight structure, the corners of the slabs produced by the extra-thick slab continuous casting device are right-angle structures, which can avoid cracks at the corners of the slabs when producing micro-alloyed steels containing NB, AI, and V. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is a schematic structural diagram of a crystallizer of an optional embodiment of the present application;

[0027] Figure 2 This is a schematic structural diagram of a narrow copper plate of an optional embodiment of the present application;

[0028] Figure 3 A transverse cross-sectional view of a narrow copper plate of an optional embodiment of the present application;

[0029] Figure 4 A schematic structural diagram of a crystallizer according to another optional embodiment of the present application;

[0030] Figure 5 This is a schematic structural diagram of a narrow copper plate of another optional embodiment of the present application;

[0031] Figure 6 A transverse cross-sectional view of a narrow copper plate according to another optional embodiment of the present application;

[0032] Figure 7This is a schematic structural diagram of a guide support roller according to an optional embodiment of the present application.

[0033] The reference numerals are:

[0034] 100, wide copper plate; 200, narrow copper plate; 300, casting billet;

[0035] 1. First working surface; 2. Second working surface; 3. Guide support roller; 31. First section; 32. Second section; 4. Cooling surface; 5. First cooling water trough; 6. Second cooling water trough. DETAILED DESCRIPTION

[0036] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0037] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0038] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0039] The preferred embodiments of the present invention are described below in conjunction with the accompanying drawings. It should be understood that the preferred embodiments described herein are only used to illustrate and explain the present invention, and are not used to limit the present invention.

[0040] See also Figures 1 to 7As shown, according to an embodiment of the present application, a super thick slab continuous casting device is provided, comprising a crystallizer, the crystallizer comprising a pair of wide copper plates 100 and a pair of narrow copper plates 200, the pair of wide copper plates 100 each extending in one direction and being installed to face each other in a direction intersecting the extending direction, the pair of narrow copper plates 200 respectively extending to intersect with the wide copper plates 100, and the pair of narrow copper plates 200 being installed to face each other, thereby sealing a portion between the pair of wide copper plates 100 to form an internal space for solidifying molten steel into a cast billet 300; the narrow copper plates 200 are close to the cast billet One side of 300 has a first working surface 1 and a second working surface 2, two second working surfaces 2 are arranged, one second working surface 2 is arranged on one side of the first working surface 1, and the other second working surface 2 is arranged on the other side of the first working surface 1, and the first working surface 1 is connected to the two second working surfaces 2 respectively; the cross-section of the first working surface 1 is a concave arc, the midpoint of the concave arc coincides with the transverse center line of the first working surface 1, the two second working surfaces 2 are symmetrically arranged with the transverse center line of the first working surface 1 as the symmetry center, and the two second working surfaces 2 are also perpendicular to the wide copper plate 100.

[0041] The ultra-thick slab continuous casting device provided in the embodiment of the present application can realize the production of the narrow-surface cast 300 with a convex structure by setting the first working surface 1 of the narrow copper plate 200 contacting the cast 300 as a concave structure, thereby enabling the depth of the double-drum middle drum seam of the cast 300 after rolling to become shallower, reducing the trimming amount of the steel plate, and thereby improving the yield rate of the thick plate; at the same time, by setting the second working surfaces 2 on both sides of the first working surface as a straight structure, the corners of the cast 300 produced by the ultra-thick slab continuous casting device are right-angle structures, which can avoid cracks at the corners of the cast 300 when producing micro-alloyed steel containing NB, AI, and V.

[0042] Among them, the ultra-thick slab continuous casting device includes: a ladle, which stores molten steel refined in the steelmaking process; a tundish, which receives the molten steel through an injection nozzle connected to the ladle and temporarily stores the molten steel; a crystallizer, which receives the molten steel stored in the tundish and makes the molten steel initially solidify into a predetermined shape; an immersed water nozzle, which supplies the molten steel in the tundish to the crystallizer; and a spray area, which is arranged below the crystallizer, and is used to provide water spray cooling to the ingot 300 pulled out of the crystallizer, to help the ingot 300 to solidify quickly, so as to facilitate a series of molding processes.

[0043] Among them, in the embodiment of the present application, the crystallizer is used to produce an extra-thick billet 300 with a narrow surface having a convex structure and no corner defects. It should be noted that the extra-thick billet 300 can be a billet 300 with a thickness of 300mm to 600mm. When the narrow surface of the extra-thick billet 300 has a convex structure, the depth of the double-drum middle drum seam of the extra-thick billet 300 after rolling is relatively shallow.

[0044] The crystallizer includes a pair of wide copper plates 100, each of which extends in one direction and is spaced apart from each other in a direction intersecting or perpendicular to the extending direction; and a pair of narrow copper plates 200 arranged between the pair of wide copper plates 100, each of which extends in a direction intersecting or perpendicular to the wide copper plates 100, and the pair of narrow copper plates 200 are also spaced apart from each other in a direction intersecting or perpendicular to the extending direction.

[0045] Specifically, in the embodiment of the present application, the extension direction of the pair of wide copper plates 100 is perpendicular to the extension direction of the pair of narrow copper plates 200. For example, the extension direction of the pair of wide copper plates 100 is defined as the X-axis direction, and the extension direction of the pair of narrow copper plates 200 is the Y-axis direction. At this time, the pair of wide copper plates 100 are spaced apart in the Y-axis direction, and the pair of narrow copper plates 200 are spaced apart in the X-axis direction. The pair of wide copper plates 100 and the pair of narrow copper plates 200 form an internal space for solidifying molten steel into a casting billet 300.

[0046] A pair of wide copper plates 100 and a pair of narrow copper plates 200 are combined to form an inner cavity of a crystallizer to solidify molten steel into a casting slab 300 .

[0047] The narrow copper plate 200 includes a working surface, which may be a wall surface of the narrow copper plate 200 facing the inner space of the crystallizer, and the working surface is used to contact the solidified shell.

[0048] The working surface includes a first working surface 1 and a second working surface 2, and the first working surface 1 and the second working surface 2 extend along the height direction of the narrow copper plate 200. It can be understood that the height direction of the narrow copper plate 200 can be the length direction of the ingot 300.

[0049] There are two second working surfaces 2, which are arranged on both sides of the first working surface 1 along the width direction of the narrow copper plate 200 and are respectively connected to the first working surface 1. It can be understood that the width direction of the narrow copper plate 200 can be the thickness direction of the ingot 300.

[0050] Specifically, the first working surface 1 is located in the middle of the narrow copper plate 200, and the second working surface 2 is located at the edge of the narrow copper plate 200. The first working surface 1 is smoothly connected with the two second working surfaces 2, which can reduce the probability of double drum shape defects in the billet 300 during rolling.

[0051] The first working surface 1 is recessed in a direction away from the ingot 300 to form an inner concave structure, so that the portion of the ingot 300 that contacts the first working surface 1 after solidification presents an outer convex structure.

[0052] The depression of the first working surface 1 can be 5 mm to 50 mm. For example, the depression of the first working surface 1 is 5 mm, and the height of the narrow surface middle part protrusion of the solidified casting 300 is 5 mm; the depression of the first working surface 1 is 25 mm, and the height of the narrow surface middle part protrusion of the solidified casting 300 is 25 mm; the depression of the first working surface 1 is 50 mm, and the height of the narrow surface middle part protrusion of the solidified casting 300 is 50 mm.

[0053] Specifically, the cross section of the first working surface 1 is a concave arc, which can reduce the wear of the narrow copper plate 200 when the solidified billet shell moves downward during the continuous casting process, thereby extending the service life of the narrow copper plate 200.

[0054] The second working surface 2 is a plane, so that the portion of the solidified ingot 300 that contacts the second working surface 2 is a straight structure.

[0055] Specifically, the second working surface 2 is perpendicular to the wide copper plate 100, so that the ultra-thick slab continuous casting device can prepare a casting slab 300 with a right-angle structure at the corner, avoiding cracks at the corner when the casting slab 300 contains NB, AI, V micro-alloyed steel. It can be understood that the corner of the casting slab 300 can be a casting slab 300 corresponding to the angle formed at the intersection of the wide copper plate 100 and the narrow copper plate 200.

[0056] The narrow copper plate 200 further includes a top surface and a bottom surface, wherein the top surface is flush with the upper opening of the crystallizer, and the bottom surface is flush with the lower opening of the crystallizer. It can be understood that the upper opening of the crystallizer can be the end where the molten steel enters the inner space of the crystallizer, and the lower opening of the crystallizer can be the end where the ingot 300 leaves the inner space of the crystallizer.

[0057] The narrow copper plate 200 further includes a side surface, which may be a wall surface in contact with the wide copper plate 100 , and two side surfaces are provided, and the two side surfaces are arranged opposite to each other.

[0058] In some possible embodiments provided in the present application, the narrow copper plate 200 has a width that gradually decreases in the downward direction, so that the side surface of the wide copper plate 100 in contact with the narrow copper plate 200 is gradually inclined in the downward direction relative to the center of the narrow copper plate 200 in the width direction, which can meet the dynamic shrinkage characteristics of the ingot 300 in the extension direction of the narrow copper plate 200 when the ingot 300 solidifies downward, and ensures that the ingot 300 and the wide copper plate 100 are highly fitted and solidified, so that the heat transfer between the two is uniform.

[0059] The narrow copper plate 200 has a width that gradually decreases in the downward direction, so that the spacing distance between a pair of wide copper plates 100 gradually decreases in the downward direction.

[0060] Specifically, when the pair of wide copper plates 100 face each other, the lower spacing distance of the pair of wide copper plates 100 is shorter than the upper spacing distance. It should be noted that the above-mentioned change in the spacing distance of the pair of wide copper plates 100 is ultimately represented by the thickness of the ingot 300 gradually decreasing in the downward direction, so as to meet the characteristics of the dynamic solidification of the ingot 300 and ensure that the ingot 300 is well attached to the wide copper plate 100 during the entire solidification process.

[0061] The width of the narrow copper plate 200 can be linearly reduced by 0mm to 4mm in the downward direction. For example, the width of the narrow copper plate 200 can be linearly reduced by 1mm, 2mm, 3mm, or 4mm in the downward direction. It can be understood that the value of the linear reduction of the width of the narrow copper plate 200 in the downward direction can also be other values ​​besides the above values, as long as the width of the narrow copper plate 200 is linearly reduced by 0mm to 4mm in the downward direction.

[0062] In some possible embodiments disclosed in the present application, the widths of the first working surface 1 and the second working surface 2 are gradually reduced in a downward direction at a constant ratio. By setting the widths of the first working surface 1 and the second working surface 2 to be gradually reduced in a downward direction at a constant ratio, the dynamic shrinkage change of the casting slab 300 can be better adapted, which helps to improve the quality of the casting slab 300.

[0063] The width of the first working surface 1 can be determined according to the width of the second working surface 2 .

[0064] Specifically, the width of the second working surface 2 can be linearly reduced by 0mm to 1mm in the downward direction. For example, the width of the second working surface 2 can be linearly reduced by 0.1mm, or 0.2mm, or 0.3mm, or 0.4mm, or 0.5mm, or 0.6mm, or 0.7mm, or 0.8mm, or 0.9mm, or 1.0mm in the downward direction. It can be understood that the value of the width of the second working surface 2 linearly reduced in the downward direction can also be other values ​​in addition to the above values, as long as the width of the second working surface 2 is linearly reduced by 0mm to 1mm in the downward direction.

[0065] When the width of the narrow copper plate 200 decreases by 4 mm in the downward direction and the width of the second working surface 2 decreases by 1 mm in the downward direction, the width of the first working surface 1 decreases by 2 mm in the downward direction.

[0066] In some possible embodiments provided in the present application, the narrow copper plate 200 includes a thickness reduction zone, which is arranged near the lower mouth of the narrow copper plate 200. The height of the thickness reduction zone is 50 mm to 200 mm. The thickness reduction zone has a thickness that gradually decreases in the downward direction, which can reduce the wear of the narrow copper plate 200 when the solidified billet shell moves downward during the continuous casting process, solves the problem of severe wear in the lower area of ​​the crystallizer in the actual continuous casting process, and further ensures the long service life of the crystallizer.

[0067] The thickness reduction area may be a portion of the narrow copper plate 200 corresponding to the lower region of the crystallizer.

[0068] Specifically, the height of the thickness reduction zone can be 50 mm to 200 mm. For example, when the height of the thickness reduction zone is 50 mm, the area between the position 50 mm away from the lower opening of the narrow copper plate 200 and the lower opening of the narrow copper plate 200 is the thickness reduction zone; when the height of the thickness reduction zone is 125 mm, the area between the position 125 mm away from the lower opening of the narrow copper plate 200 and the lower opening of the narrow copper plate 200 is the thickness reduction zone; when the height of the thickness reduction zone is 200 mm, the area between the position 200 mm away from the lower opening of the narrow copper plate 200 and the lower opening of the narrow copper plate 200 is the thickness reduction zone.

[0069] The thickness of the reduced thickness zone gradually decreases in the downward direction, which can make way for the descending solidified shell, thereby reducing the wear of the narrow copper plate 200 when the solidified shell descends during the continuous casting process.

[0070] Specifically, the thickness of the thickness-reducing zone can be linearly reduced by 0mm to 1mm in the downward direction. For example, the thickness of the thickness-reducing zone is linearly reduced by 0.1mm, or 0.2mm, or 0.3mm, or 0.4mm, or 0.5mm, or 0.6mm, or 0.7mm, or 0.8mm, or 0.9mm, or 1.0mm in the downward direction. It can be understood that the value of the thickness of the thickness-reducing zone linearly reduced in the downward direction can also be other values ​​in addition to the above values, as long as the thickness of the thickness-reducing zone is linearly reduced by 0mm to 1mm in the downward direction.

[0071] In some possible implementations provided in this application, see Figure 7As shown, the ultra-thick slab continuous casting device also includes a guiding support mechanism, which is arranged at the lower mouth of the narrow copper plate 200; the guiding support mechanism includes a guiding support roller 3, which includes a first section 31, and the first section 31 includes two reduced diameter sections, and the diameters of the two reduced diameter sections gradually decrease in the direction facing each other, so that the roller surface of the guiding support roller 3 contacting the billet 300 presents a concave arc with the same cross-section as the first working surface 1, so as to support the billet 300 of the narrow face convex part formed under the action of the first working surface 1; the guiding support roller 3 also includes a second section 32, and two second sections 32 are provided, and the two second sections 32 are arranged on both sides of the first section 31 along the axial direction of the first section 31, and the first section 31 is respectively connected to the two second sections 32, and the two second sections 32 are cylindrical, so that the two second sections 32 are suitable for supporting the billet 300 of the narrow face straight part formed under the action of the two second working surfaces 2. By arranging a guiding support mechanism at the lower mouth of the crystallizer, support can be provided for the ingot 300 pulled out of the crystallizer, maintaining the narrow surface of the ingot 300 with an outward convex structure, and preventing the incompletely solidified ingot 300 from deforming; at the same time, it is beneficial to reduce defects such as bulging of the ingot 300 and improve the surface quality and internal quality of the ingot 300.

[0072] A spraying area is provided below the narrow copper plate 200 , a frame is provided in the spraying area, and a guide support mechanism is installed on the frame.

[0073] Specifically, the guide support mechanism includes a guide support roller 3, and the guide support roller 3 can be a foot roller, and the foot roller is rotatably arranged on the frame.

[0074] The guide support roller 3 includes a first section 31 and a second section 32 which are coaxially arranged, two second sections 32 are arranged, the first section 31 is arranged between the two second sections 32, and the two ends of the first section 31 are respectively connected to the two second sections 32. In addition, it can be understood that the guide support roller 3 can also be made of an integral molding.

[0075] Specifically, the first section 31 is roughly hourglass-shaped, and the first section 31 includes two reduced diameter sections, and the diameter of each of the two reduced diameter sections gradually decreases in the direction facing each other, so that the first section 31 can adapt to the bulge in the middle of the narrow surface of the ingot 300; the second section 32 is roughly cylindrical, and the second section 32 is connected to the end of the reduced diameter section with a large end face area, and the diameter of the second section 32 is the same as the diameter of the end of the reduced diameter section with a large end face area, so that the second section 32 can adapt to the corner of the right-angle structure of the ingot 300.

[0076] The length of the first section 31 is the same as the width of the first working surface 1 .

[0077] In one embodiment, the length of the second section 32 is less than the width of the second working surface 2; in another embodiment, the length of the second section 32 is the same as the width of the second working surface 2. In this embodiment, the length of the second section 32 is less than the width of the second working surface 2.

[0078] Specifically, in this embodiment, the length of the second section 32 is 0 mm to 20 mm less than the width of the second working surface 2. It should be noted that the casting blank 300 has a lower angle temperature and a higher hardness, and does not require support, thereby reducing the production cost of the guide support mechanism.

[0079] Among them, in this embodiment, when the height of the narrow copper plate 200 is 800mm~1000mm, the width is 300mm~600mm, the thickness is 35mm~55mm, the width of the second working surface 2 can be 0mm~150mm, and the length of the second section 32 can be 0mm~130mm.

[0080] In some possible embodiments provided in the present application, at least two rows of guide support rollers 3 are provided, and at least two rows of guide support rollers 3 are symmetrically arranged.

[0081] In this embodiment, a row of guide support rollers 3 is disposed under each of a pair of narrow copper plates 200, so as to enhance the support effect of the guide support mechanism on the ingot 300 pulled out of the crystallizer.

[0082] Specifically, the single-row guide support roller 3 includes a plurality of guide support rollers 3 arranged vertically. As an embodiment, the plurality of guide support rollers 3 arranged vertically are in a straight line and are equally spaced; as another embodiment, the plurality of guide support rollers 3 arranged vertically are in a parabolic shape. It can be understood that when the plurality of guide support rollers 3 arranged vertically are in a parabolic shape, the support force received by the billet 300 pulled out of the crystallizer when passing through the guide support roller 3 is more uniform, local stress concentration is reduced, and the risk of cracks and deformation of the billet 300 is reduced; at the same time, it can also better adapt to the dynamic shrinkage changes of the billet 300 during the solidification process of the billet 300, reduce the constraints and obstacles on the billet 300, and help improve the quality of the billet 300.

[0083] In some possible embodiments provided in the present application, the narrow copper plate 200 has a cooling surface 4 on the side facing away from the ingot 300; a first cooling water trough 5 is provided on the cooling surface 4 at a position relative to the first working surface 1; a second cooling water trough 6 is provided on the cooling surface 4 at a position relative to the second working surface 2; a plurality of first cooling water troughs 5 are provided, and two second cooling water troughs 6 are provided, and the plurality of first cooling water troughs 5 are located between the two second cooling water troughs 6 and are arranged at equal intervals.

[0084] The cooling surface 4 may be a wall surface of the narrow copper plate 200 away from the ingot 300 , and the cooling surface 4 is arranged opposite to the working surface.

[0085] Specifically, as an implementation method, see Figure 3 As shown, the cooling surface 4 is a plane, and the cooling surface 4 is perpendicular to the wide copper plate 100; as another embodiment, see Figure 6 As shown, the cooling surface 4 has the same shape as the working surface, and the cooling surface 4 is parallel to the working surface.

[0086] Among them, fastening holes and cooling water troughs are provided on the cooling surface 4. The fastening holes are bolt holes used to fix the narrow copper plate 200 and the cooling water tank; the cooling water trough extends along the height direction of the narrow copper plate 200, and the cooling water trough is used to cool the narrow copper plate 200, and then cool the molten steel in the internal space of the crystallizer.

[0087] Specifically, in the width direction of the narrow copper plate 200, the fastening holes can be arranged in two to four rows, and the cooling water grooves can be arranged in multiple rows. It should be noted that when the fastening holes are arranged in two rows, the distance between the fastening holes and the adjacent cooling water grooves can be 3 to 6 mm; when the fastening holes are arranged in more than two rows, the distance between the fastening holes and the adjacent cooling water grooves can be 2 to 5 mm.

[0088] The widths of the plurality of cooling water grooves are the same, and the width of the cooling water grooves may be 4 to 7 mm.

[0089] The heights of the plurality of cooling water troughs are the same, and the distance between the cooling water trough and the top surface of the narrow copper plate 200 may be 20 to 25 mm, and the distance between the cooling water trough and the bottom surface of the narrow copper plate 200 may also be 20 to 25 mm.

[0090] The plurality of cooling water grooves include a first cooling water groove 5 and a second cooling water groove 6. The first cooling water groove 5 is provided on the cooling surface 4 at a position relative to the first working surface 1, and the second cooling water groove 6 is provided on the cooling surface 4 at a position relative to the two second working surfaces 2.

[0091] Specifically, in the embodiment of the present application, the fastening holes are arranged in two rows, ten first cooling water grooves 5 are arranged, and two second cooling water grooves 6 are arranged.

[0092] In the above embodiment, a plurality of thermocouple mounting holes are also provided on the cooling surface 4. By providing the thermocouple mounting holes on the cooling surface 4, a stable setting position is provided for the thermocouple, so that the temperature monitoring of the narrow copper plate 200 can be realized.

[0093] The thermocouple assembly hole may be a circular hole, and the diameter of the thermocouple assembly hole may be 5 to 6 mm.

[0094] Among them, several thermocouple assembly holes are arranged perpendicular to the cooling surface 4, and the spacing distances between several thermocouple assembly holes and the working surface of the narrow copper plate 200 are the same, and the spacing distances between several thermocouple assembly holes and the working surface of the narrow copper plate 200 can be 20 to 26 mm.

[0095] Specifically, a plurality of thermocouple assembly holes may be arranged in 2 to 4 rows in the height direction of the narrow copper plate 200, and a plurality of thermocouple assembly holes may be arranged in 1 to 2 columns in the width direction of the narrow copper plate 200. In the height direction of the narrow copper plate 200, the spacing distance between the first row of thermocouple assembly holes and the top surface of the narrow copper plate 200 may be 200 to 240 mm, and the spacing distance between two adjacent rows of thermocouple assembly holes may be 100 to 150 mm, and the spacing may be the same or different, and this application does not make further restrictions. For example, when a plurality of thermocouple assembly holes are arranged in a row in the width direction of the narrow copper plate 200, each of the thermocouple assembly holes coincides with the transverse center line of the narrow copper plate 200; when a plurality of thermocouple assembly holes are arranged in two rows in the width direction of the narrow copper plate 200, the two rows of thermocouple assembly holes are symmetrically arranged with the transverse center line of the narrow copper plate 200 as the center of symmetry. At this time, the spacing distance between the two rows of thermocouple assembly holes and the transverse center line of the narrow copper plate 200 can be 13% to 23% of the top surface width of the narrow copper plate 200.

[0096] In some possible implementations provided in this application, see Figure 3 and Figure 6 As shown, the first cooling water trough 5 is a straight water trough, and the first cooling water trough 5 is perpendicular to the cooling surface 4; the second cooling water trough 6 is an inclined water trough, and the second cooling water trough 6 is inclined in a direction away from the first cooling water trough 5. By setting the second cooling water trough 6 as an inclined water trough and making the second cooling water trough 6 inclined in a direction away from the first cooling water trough 5, it is possible to ensure uniform heat transfer of the narrow copper plate 200 in the width direction, so as to achieve uniform cooling of the ingot 300 in the internal space of the crystallizer.

[0097] The first cooling water trough 5 is a straight trough, and the first cooling water trough 5 is perpendicular to the cooling surface 4; the second cooling water trough 6 is an inclined trough, and the second cooling water trough 6 and the third cooling water trough are arranged at an angle to the cooling surface 4.

[0098] Specifically, the second cooling water trough 6 is inclined in a direction away from the first cooling water trough 5 , and the second cooling water trough 6 is used to cool the corner of the casting slab 300 corresponding to the second working surface 2 .

[0099] Among them, the angle between the second cooling water trough 6 and the cooling surface 4 is 70° to 85°. For example, the angle between the second cooling water trough 6 and the cooling surface 4 is 70°, or 71°, or 72°, or 73°, or 74°, or 75°, or 76°, or 77°, or 78°, or 79°, or 80°, or 81°, or 82°, or 83°, or 84°, or 85°. It can be understood that the angle between the second cooling water trough 6 and the cooling surface 4 can also be other values ​​in addition to the above values, as long as the angle between the second cooling water trough 6 and the cooling surface 4 is 70° to 85°. It should be noted that when the angle between the second cooling water trough and the cooling surface 4 is 70° to 85°, it can ensure that the temperature of the working surface of the narrow copper plate 200 is uniformly distributed laterally, ensure that the corners of the ingot 300 are straightened at high temperature in the second cooling zone, and prevent the occurrence of cracks in the corners of the ingot 300.

[0100] In some possible embodiments provided in the present application, the bottoms of several first cooling water troughs 5 are located on the same arc surface, and the cross section of the arc surface is parallel to the cross section of the first working surface 1. By setting the concave arc line of the cross section of the arc surface where the bottoms of several first cooling water troughs 5 are located to be parallel to the concave arc line of the cross section of the first working surface 1, it is possible to ensure uniform heat transfer in the middle of the working surface in the width direction of the narrow copper plate, so as to achieve uniform cooling of the ingot 300 in the inner cavity of the crystallizer.

[0101] Among them, at the same height, the concave arc of the cross section of the arc surface where the groove bottoms of the plurality of first cooling water grooves 5 are located can be obtained by translating the concave arc of the cross section of the first working surface 1 .

[0102] In some possible implementations provided in this application, see Figure 3 and Figure 6 As shown, the distance between the transverse center line of the bottom of the first cooling water tank 5 and the first working surface 1 conforms to the formula:

[0103] D=h 1 +h 2

[0104] In the formula, h 1 h is the maximum thickness of the narrow copper plate 200, ranging from 10mm to 20mm; 2 It is the safe distance between the bottom of the first cooling water trough 5 and the first working surface 1 at the maximum use thickness, and the value is 8mm to 15mm.

[0105] In some possible embodiments provided in the present application, the spacing distance between the transverse center line of the bottom of the second cooling water trough 6 and the second working surface 2 is smaller than the spacing distance between the transverse center line of the bottom of the first cooling water trough 5 and the first working surface 1, which is 1 mm to 3 mm. In the present application, by setting the spacing distance between the transverse center line of the bottom of the first cooling water trough 5 and the first working surface 1 to be greater than the spacing distance between the transverse center line of the bottom of the second cooling water trough 6 and the second working surface 2, which is 1 to 3 mm, so that the bottom of the first cooling water trough 5 is closer to the working surface than the bottom of the second cooling water trough 6, it can ensure that the temperature of each area of ​​the working surface of the narrow copper plate 200 is consistent, so as to achieve uniform cooling of the ingot 300 in the internal space of the crystallizer.

[0106] The ultra-thick slab continuous casting device provided in the embodiment of the present application can realize the production of the narrow-surface cast 300 with a convex structure by setting the first working surface 1 of the narrow copper plate 200 contacting the cast slab 300 as an inner concave structure, thereby enabling the depth of the double-drum drum seam of the cast slab 300 after rolling to become shallower, reducing the trimming amount of the steel plate, and thus improving the yield rate of the thick plate; at the same time, by setting the second working surfaces 2 on both sides of the first working surface as a straight structure, the corners of the cast slab 300 produced by the ultra-thick slab continuous casting device are made to be a right-angle structure, which can avoid cracks at the corners of the cast slab 300 when producing micro-alloyed steel containing NB, AI, and V.

[0107] It is easy for those skilled in the art to understand that, under the premise of no conflict, the above-mentioned advantageous methods can be freely combined and superimposed.

[0108] The above are only preferred embodiments of the present application and are not intended to limit the present application. Any modifications, equivalent replacements and improvements made within the spirit and principles of the present application shall be included in the protection scope of the present application. The above are only preferred implementations of the present application. It should be pointed out that for ordinary technicians in this technical field, several improvements and variations can be made without departing from the technical principles of the present application, and these improvements and variations should also be regarded as the protection scope of the present application.

Claims

1. A super thick slab continuous casting device, It is characterized in that The crystallizer comprises a pair of wide copper plates (100) and a pair of narrow copper plates (200), wherein the pair of wide copper plates (100) extend in one direction and are installed to face each other in a direction intersecting the extending direction, and the pair of narrow copper plates (200) extend to intersect with the wide copper plates (100) and are installed to face each other, thereby sealing a portion between the pair of wide copper plates (100) to form an internal space for molten steel to solidify into a cast billet (300); The narrow copper plate (200) has a first working surface (1) and a second working surface (2) on one side close to the ingot (300), two second working surfaces (2) are provided, one second working surface (2) is provided on one side of the first working surface (1), and the other second working surface (2) is provided on the other side of the first working surface (1), and the first working surface (1) is connected to the two second working surfaces (2) respectively; The cross section of the first working surface (1) is a concave arc, the midpoint of the concave arc coincides with the transverse center line of the first working surface (1), the two second working surfaces (2) are symmetrically arranged with the transverse center line of the first working surface (1) as the symmetry center, and the two second working surfaces (2) are also perpendicular to the wide copper plate (100).

2. The ultra-thick slab continuous casting device according to claim 1, It is characterized in that The ultra-thick slab continuous casting device further comprises a guide support mechanism, wherein the guide support mechanism is arranged at the lower opening of the narrow copper plate (200); The guide support mechanism comprises a guide support roller (3), the guide support roller (3) comprises a first section (31), the first section (31) comprises two reduced diameter sections, the diameters of the two reduced diameter sections respectively gradually decrease in a direction facing each other, so that the roller surface of the guide support roller (3) contacting the casting (300) presents a concave arc line with the same cross section as the first working surface (1), so as to support the narrow convex part of the casting (300) formed under the action of the first working surface (1); The guide support roller (3) also includes a second section (32), two second sections (32) are provided, and the two second sections (32) are arranged on both sides of the first section (31) along the axial direction of the first section (31), the first section (31) is respectively connected to the two second sections (32), and the two second sections (32) are cylindrical, so that the two second sections (32) are suitable for supporting the narrow straight part of the cast billet (300) formed under the action of the two second working surfaces (2).

3. The ultra-thick slab continuous casting device according to claim 2, It is characterized in that The guide support rollers (3) are arranged in two rows, and the guide support rollers (3) in the two rows are symmetrically arranged.

4. The ultra-thick slab continuous casting device according to claim 1, It is characterized in that The narrow copper plate (200) has a width that gradually decreases in a downward direction.

5. The ultra-thick slab continuous casting device according to claim 1, It is characterized in that The narrow copper plate (200) comprises a thickness reduction zone, the thickness reduction zone is arranged close to the lower opening of the narrow copper plate (200), the height of the thickness reduction zone is 50 mm to 200 mm, and the thickness of the thickness reduction zone gradually decreases in a downward direction.

6. The ultra-thick slab continuous casting device according to claim 1, It is characterized in that The narrow copper plate (200) has a cooling surface (4) on a side facing away from the casting billet (300); A first cooling water trough (5) is provided on the cooling surface (4) at a position relative to the first working surface (1); A second cooling water trough (6) is provided on the cooling surface (4) at a position relative to the second working surface (2); A plurality of the first cooling water troughs (5) are provided, and two second cooling water troughs (6) are provided. The plurality of the first cooling water troughs (5) are located between the two second cooling water troughs (6) and are arranged at equal intervals.

7. The ultra-thick slab continuous casting device according to claim 6, It is characterized in that The first cooling water trough (5) is a straight water trough, and the first cooling water trough (5) is perpendicular to the cooling surface (4); The second cooling water trough (6) is an inclined water trough, and the second cooling water trough (6) is inclined in a direction away from the first cooling water trough (5).

8. The ultra-thick slab continuous casting device according to claim 6, It is characterized in that The bottoms of a plurality of the first cooling water grooves (5) are located on the same arc surface, and the cross section of the arc surface is parallel to the cross section of the first working surface (1).

9. The ultra-thick slab continuous casting device according to claim 6, It is characterized in that The distance between the transverse center line of the bottom of the first cooling water trough (5) and the first working surface (1) conforms to the formula: D=h 1 +h 2 In the formula, h 1 h is the maximum use thickness of the narrow copper plate (200), and is 10 mm to 20 mm; 2 The safe distance between the bottom of the first cooling water trough (5) and the first working surface (1) at the maximum use thickness is 8 mm to 15 mm.

10. The ultra-thick slab continuous casting device according to claim 9, It is characterized in that The spacing distance between the bottom of the second cooling water trough (6) and the second working surface (2) is smaller than the spacing distance between the bottom of the first cooling water trough (5) and the first working surface (1) by 1 mm to 3 mm.