Focused ion beam automatic cutting method for blind hole bottom

By using automated vertical slice and deposition identification and identification technology during blind hole bottom detection and cutting, the problem of human operation dependence in the existing technology is solved, efficient automatic cutting and multi-sample detection are achieved, and equipment utilization is improved and cutting efficiency.

CN118951265APending Publication Date: 2024-11-15SHANGHAI MEADVILLE SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411321704.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

There is a human dependence on artificial operations during the existing blind hole bottom detection and cutting process, resulting in inefficiency and waste of human resources. The existing FIB-SEM dual-beam system is not suitable for multi-sample automated inspection.

Method used

By first obtaining multiple vertical slices and polishing them to make them highly consistent, deposition identification marks and cutting parameters are set in the FIB-SEM dual-beam system to realize automatic positioning and cutting, and automatic roughing and finishing of different samples are realized.

Benefits of technology

It improves the equipment utilization rate of FIB-SEM dual-beam system, saves labor costs, realizes efficient continuous automatic cutting, and can cut out the bottom section of the blind hole of the sample with smooth surface and clear details to meet production needs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118951265A_ABST
    Figure CN118951265A_ABST
Patent Text Reader

Abstract

The invention provides an automatic focused ion beam cutting method for the bottom of a blind hole, which comprises the following steps of: firstly obtaining a plurality of vertical slices, polishing to enable the heights of the plurality of vertical slices to be consistent, depositing identification marks in to-be-cut areas of the vertical slices, setting rough machining parameters and finish machining parameters in an FIB-SEM (Focused Ion Beam-Scanning Electron Microscope) double-beam system, and cutting the bottom of the blind hole. And finally, the system performs positioning according to the identification mark and performs automatic cutting according to the rough machining parameters and the finish machining parameters. The steps of automatic rough machining, finish machining and the like of blind hole bottoms of different samples can be achieved, the cutting positions of different samples are accurately positioned, continuous and automatic cutting is achieved, the cutting efficiency is high, the equipment utilization rate of an FIB-SEM double-beam system is increased, and meanwhile the labor cost is saved; in addition, the sample blind hole bottom section with smooth surface and clear crystal lattices, defects and other details can be cut, the effect is consistent with that of manual cutting, and the production requirement can be met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of manufacturing semiconductor integrated circuit packaging substrates, and in particular to a focused ion beam automatic cutting method for blind hole bottoms. Background Art

[0002] As the core of modern electronic devices, the manufacturing technology of printed circuit boards (PCB) and integrated circuit boards (IC) is becoming more and more advanced. Blind hole manufacturing technology is a mainstream PCB and IC board manufacturing technology. It adopts a multi-layer structure and punches blind holes on one side of the board to achieve connectivity between different layers of circuits, thereby improving the performance and reliability of PCB and IC boards.

[0003] However, in the actual manufacturing process, some blind hole defects may occur, such as diameter deviation, eccentricity, length mismatch, internal voids, cracks or fractures, etc. In order to avoid these blind hole defects, the processing parameters and quality inspections need to be strictly controlled during the PCB manufacturing process, especially the use of high-precision equipment, such as the use of a focused ion beam microscope system (FIB-SEM) to perform quality inspection on the bottom of the blind hole to reduce the occurrence of blind hole defects.

[0004] At present, the detection of blind hole defects requires the preparation of slices first, and then positioning, rough processing, and fine processing on the FIB-SEM dual-beam system. The above steps are all manually operated and controlled. Each sample requires real-time follow-up of the entire process by the operator. When the number of test samples is large, 24-hour uninterrupted operation is required, resulting in a waste of human resources. In addition, the existing FIB-SEM dual-beam system can realize the automatic preparation of transmission electron microscope (TEM) samples, but it is only for the TEM sample preparation of a single sample, and is not applicable to the bottom test of blind holes of different samples of PCB and IC substrates. Summary of the invention

[0005] In view of the shortcomings of the prior art described above, the present invention provides a focused ion beam automatic cutting method for the bottom of a blind hole, firstly obtaining a plurality of vertical slices, making the heights of the plurality of vertical slices consistent by polishing, then depositing identification marks on the to-be-cut area of ​​the vertical slices, setting roughing parameters and finishing parameters in the FIB-SEM dual-beam system, and finally positioning the system according to the identification marks, and automatically cutting according to the roughing parameters and finishing parameters. The present invention can realize the steps of automatic roughing and finishing of the bottom of blind holes of different samples, accurately locate the cutting positions of different samples, realize continuous automatic cutting, have high cutting efficiency, improve the equipment utilization rate of the FIB-SEM dual-beam system, and save labor costs at the same time; in addition, the present invention can cut a cross section of the bottom of the blind hole of a sample with a smooth surface and clear details such as lattices and defects, which is consistent with the effect of manual cutting and can meet production needs.

[0006] To achieve the above-mentioned object and other related objects, the present invention provides a focused ion beam automatic cutting method for the bottom of a blind hole, comprising the following steps:

[0007] Providing a packaging substrate, sampling a blind hole area on the packaging substrate to obtain a plurality of vertical slices, grinding and polishing the vertical slices to make the heights of the plurality of vertical slices consistent;

[0008] Place the plurality of vertical slices into a sample chamber of a FIB-SEM dual-beam system, turn on the electron beam and the ion beam, and adjust the system so that the electron beam and the ion beam are co-focused at the same position;

[0009] Depositing identification marks and protective layers on the area to be cut;

[0010] The parameters of the first cutting and the second cutting are set in the FIB-SEM dual beam system, the system is positioned according to the identification mark, and the first cutting and the second cutting are automatically performed according to the cutting parameters.

[0011] Optionally, before grinding and polishing the vertical slices, the method further includes: performing glue filling treatment on the vertical slices.

[0012] Optionally, after grinding and polishing the vertical slice, the method further includes: placing the vertical slice under a microscope and marking the area to be cut.

[0013] Optionally, after marking the area to be cut, the method further includes: performing conductive treatment on the vertical slices by spraying gold or carbon.

[0014] Optionally, after the conductive treatment, the method further includes: using conductive copper glue to stick the vertical slice to a base, and coating conductive silver glue on the surface of the vertical slice.

[0015] Optionally, after placing the plurality of vertical slices into a sample chamber of a FIB-SEM dual beam system, the sample chamber is evacuated to a vacuum degree less than or equal to 5×10 -3 Pa.

[0016] Optionally, adjusting the system so that the electron beam and the ion beam are co-focused at the same position includes:

[0017] Position the area to be cut, adjust the sample stage working distance to the concentric height of the electron beam and the ion beam, and adjust the image to be clear;

[0018] Rotate the sample stage to a fixed angle and adjust the Z-axis height of the sample stage and the ion beam offset until the confocal point of the ion beam and electron beam is found.

[0019] Optionally, depositing the identification mark on the area to be cut includes: first forming a deposition layer, and then forming the identification mark on the deposition layer by ion beam bombardment.

[0020] Optionally, the protective layer is one of a tungsten layer, a platinum layer, and a carbon layer.

[0021] Optionally, after the first cutting and the second cutting are completed, the system parameters are adjusted to make the image clear, and the cross-section of the slice after cutting is scanned and photographed.

[0022] The focused ion beam automatic cutting method for the bottom of a blind hole provided by the present invention has at least the following beneficial effects:

[0023] 1) Automatic cutting operation improves test efficiency and equipment utilization of FIB-SEM dual-beam system, while saving labor costs. It can realize automatic cutting, especially for some unconventional and large-sized blind hole bottom FIB cutting samples;

[0024] 2) It can realize the steps of automatic rough processing and fine processing of the bottom of blind holes of different samples, accurately locate the test positions of different samples, and automatically locate to the cutting position of the next sample after the sample cutting is completed, so as to realize continuous automatic cutting and have high cutting efficiency;

[0025] 3) It can cut out the bottom cross section of the sample blind hole with smooth surface, clear details such as lattice and defects, which is consistent with the effect of manual cutting and can meet production needs. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 Shown is a flow chart of a focused ion beam automatic cutting method for the bottom of a blind hole provided by an embodiment.

[0027] Figure 2a~2f A scanning electron microscope image of a cross section formed by automated cutting provided for the Examples is shown.

[0028] Figure 3a~3f Shown is a scanning electron microscope image of a cross section formed by manual cutting in the prior art. DETAILED DESCRIPTION

[0029] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0030] It should be noted that the illustrations provided in this embodiment only illustrate the basic concept of the present invention in a schematic manner. Although the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation, the form, quantity, positional relationship and proportion of each component in actual implementation can be changed at will under the premise of realizing the technical solution of this party, and the component layout form may also be more complicated.

[0031] Example

[0032] This embodiment provides a focused ion beam automatic cutting method for the bottom of a blind hole, such as Figure 1 As shown, the following steps are included:

[0033] S1: providing a packaging substrate, sampling a blind hole area on the packaging substrate to obtain a plurality of vertical slices, and grinding and polishing the vertical slices to make the heights of the plurality of vertical slices consistent;

[0034] First, a package substrate is provided, and the blind hole area on the package substrate is cut and sampled by an automatic slicer to obtain a plurality of vertical slices, which are pre-grinded to 10 mm to 20 mm of the to-be-cut area by a grinder. As an example, the length of the vertical slice is less than 25 mm, the width is less than 15 mm, and the height is less than 5 mm; in this embodiment, the size of the vertical slice is 15 mm×10 mm×3 mm.

[0035] Next, the vertical slices are filled with glue, and the filling agent is cured. As an example, the filling agent used for the filling process includes epoxy resin or other suitable filling agents; the filling method includes scraping, compression molding or other suitable filling methods. As an example, there is no gap visible to the naked eye at the boundary between the vertical slices and the filling agent after filling with glue, so as to ensure the observation effect of the vertical slices under an optical microscope. As an example, during the filling process, the vertical slices can be fixed to protect other non-cutting surfaces and avoid the vertical slices being dragged and stretched and distorted during the subsequent grinding process.

[0036] Next, an automatic grinding and polishing machine is installed with a special fixture to grind and polish the vertical slices. As an example, the height of multiple vertical slices after grinding is made consistent, and the accuracy is less than or equal to 2μm, ensuring that the heights of all vertical slices are on the same level.

[0037] Next, the vertical slice is placed under a microscope to mark the area to be cut. For example, it can be marked with a marker pen, laser marking, etc., to facilitate the subsequent rapid finding of the position to be cut under the FIB-SEM dual-beam electron microscope.

[0038] Next, the vertical slices are treated for electrical conductivity by spraying gold or carbon, which can avoid oxidation of the surface of the packaging substrate and thus improve the accuracy of the analysis and test results.

[0039] Next, conductive copper glue is used to stick the vertical slice to the base to prevent the vertical slice from shaking and improve stability; and conductive silver glue is coated on the surface of the vertical slice to enhance conductivity and avoid charging.

[0040] S2: placing the plurality of vertical slices into a sample chamber of a FIB-SEM dual-beam system, turning on the electron beam and the ion beam, and adjusting the system so that the electron beam and the ion beam are cofocused at the same position;

[0041] First, multiple vertical slices were placed in the sample chamber of the FIB-SEM dual-beam system and the sample chamber was evacuated to a vacuum level less than or equal to 5×10 -3 Pa.

[0042] Next, select a reference position for the sample in the chamber and perform multiple 180° rotation calibrations to confirm the rotation accuracy of the equipment sample stage.

[0043] Next, locate the area to be cut, adjust the sample stage working distance to the concentric height of the electron beam and the ion beam, and adjust the image to be clear. Specifically, select the sample to be tested from the navigation photo, move the sample stage to adjust the sample to the concentric height of the electron beam and the electron beam, find the area to be cut, adjust the sample stage working distance to the concentric height of the ion beam and the electron beam, the concentric height value varies on different machines, it can be 5mm, 7mm, 10mm, etc., here take 7mm as an example, find a suitable positioning point at the area to be cut, adjust the electron beam voltage, current, observation mode, dwell time, focal length, phase dispersion, brightness, contrast and other parameters, adjust the image to be clear, "Link" the sample stage Z-axis working distance, if the "Link" Z-axis working distance is not the concentric height value of 7mm, the Z-axis distance needs to be adjusted to 7mm, and the image is adjusted to be clear again, re-"Link" the sample stage Z-axis working distance until Z is 7mm.

[0044] Next, rotate the sample stage to a fixed angle, adjust the Z-axis height of the sample stage and the ion beam offset until the common focus of the ion beam and the electron beam is found. Specifically, rotate the sample stage to a fixed angle, for example, the fixed angle of rotation of the sample stage in this embodiment is 52°, adjust Stage Z under the electron beam to restore the focus to the positioning point; select a magnification that is no more than 1500x different from the electron beam magnification, select a pA-level beam current to refresh the image of the ion beam, and observe whether the image positioning points of the electron beam and the ion beam are consistent. Generally, the image recognition rate needs to be greater than 60%. If the image positioning points of the electron beam and the ion beam are inconsistent, the test position of the sample under the electron beam needs to be adjusted again until the image positioning points of the ion beam and the electron beam are consistent.

[0045] S3: depositing identification marks and a protective layer on the area to be cut;

[0046] First, a deposition layer is formed to protect the sample and avoid the "curtain effect" caused by cutting. As an example, under the ion beam, the deposition parameters are set to form a deposition layer in the area to be cut. The deposition layer can be one of a platinum layer, a tungsten layer, and a carbon layer. The thickness of the deposition layer is 1, and the size of the deposition layer is adjusted according to the sample size.

[0047] Next, an ion beam bombardment method is used to form an identification mark on the deposited layer, so as to etch and mark the cutting area of ​​the blind hole of different samples and improve the recognition rate of the image. As an example, the identification mark can be customized in shape, such as X, O, etc., to ensure that the system can capture and recognize it during automatic cutting. At this time, the image recognition rate must be greater than 80%. As an example, the ion beam bombardment depth is 0.6μm.

[0048] Next, a protective layer is deposited on the area to be cut. The Gas Injection System (GIS) can selectively remove a certain type of material or deposit material by combining physical sputtering with chemical gas reaction. The material deposition process is that the ion beam or electron beam decomposes the gas molecules adsorbed on the surface of the sample into volatile and non-volatile parts. The volatile part is extracted by the vacuum system, and the non-volatile part is deposited at the position irradiated by the ion beam or electron beam to form a thin film deposition. In this embodiment, the deposition voltage is 30kV, the deposition current is 3nA, the length of the protective layer is adjusted according to the different samples, the width of the protective layer is 2μm to 3μm, and the thickness of the protective layer is 1μm to 2μm; the protective layer is one of a tungsten layer, a platinum layer, and a carbon layer. By depositing one or more protective layers on the surface of the cutting area, it is possible to avoid damage to the sample surface caused by the ion beam during subsequent cutting.

[0049] S4: Setting the parameters of the first cutting and the second cutting in the FIB-SEM dual beam system, the system is positioned according to the identification mark, and automatically performs the first cutting and the second cutting according to the cutting parameters.

[0050] First, under the ion beam, set the cutting parameters, including roughing (first cutting) parameters and finishing (second cutting) parameters. As an example, since the plate thickness and material of the sample are different, the cutting depth is also different, so it is necessary to set different ion beam currents and cutting angles for different cutting depths. For specific parameter settings, refer to Table 1. As an example, during roughing, the sample needs to be rotated to 52° to ensure that the ion beam processes in the vertical direction of the sample; after completing the roughing, the cut section needs to be finely processed, and the sample stage is generally rotated to 50° to 54° to reduce the "curtain effect" so as to obtain a clear image of the fine processing of the section.

[0051] Table 1 Ion beam current and cutting angle parameter settings

[0052] Cutting Depth Rough machining current Fine machining current Fine processing angle 10um 15nA 3~5nA 53° 20um 30nA 5~7nA 53° 30um 30nA 5~7nA 53°~54° 40um 50nA 7~15nA 53°~54° >60um 65nA 15nA 50°~54°

[0053] In this embodiment, the rough machining voltage is 30kV and the current is 30nA~65nA; for the first fine machining, the voltage is 30kV and the current is 7nA~15nA when the sample stage rotates at an angle of 53°~54°; for the second fine machining, the sample stage rotation angle can be 50°~54°, the voltage is 30kV, and the current is 3nA~5nA.

[0054] Next, the system locates according to the identification mark, and then automatically performs the first and second cuts according to the above cutting parameters.

[0055] Finally, the operator adjusts the test parameters such as focus and astigmatism in the electron beam window of the FIB-SEM dual-beam system until the image is clear, and performs SEM scanning and photography on the automatically cut cross-section at the specified magnification of the test to further analyze the interconnection surface at the bottom of the blind hole.

[0056] The SEM image of the cross section cut in this embodiment at 8000x magnification is as follows: Figure 2a As shown, the SEM image at 15000x magnification is as follows Figure 2b As shown, the SEM image at 25000x magnification is as follows Figure 2c to Figure 2f shown, and Figure 2c is the image at the upper left of the cutout, Figure 2d The image is in the upper right corner of the cutout. Figure 2e is the image at the lower left of the cutout, Figure 2f The image at the lower right of the cut is shown in Figure 2. The SEM image of the cross section formed by traditional manual cutting at 8000x magnification is shown in Figure 2. Figure 3aAs shown, the SEM image at 15000x magnification is as follows Figure 3b As shown, the SEM image at 25000x magnification is as follows Figure 3c to Figure 3f shown, and Figure 3c is the image at the upper left of the cutout, Figure 3d The image is in the upper right corner of the cutout. Figure 3e is the image at the lower left of the cutout, Figure 3f It is an image of the lower right of the cut. By comparison, it can be seen that the method provided in this embodiment can cut a sample blind hole bottom cross section with a smooth surface and clear details such as lattices and defects, which is consistent with the effect of manual cutting and can meet production needs.

[0057] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A focused ion beam automatic cutting method for the bottom of a blind hole, characterized in that: The steps include: Providing a packaging substrate, sampling a blind hole area on the packaging substrate to obtain a plurality of vertical slices, grinding and polishing the vertical slices to make the heights of the plurality of vertical slices consistent; Place the plurality of vertical slices into a sample chamber of a FIB-SEM dual-beam system, turn on the electron beam and the ion beam, and adjust the system so that the electron beam and the ion beam are co-focused at the same position; Depositing identification marks and protective layers on the area to be cut; The parameters of the first cutting and the second cutting are set in the FIB-SEM dual beam system, the system is positioned according to the identification mark, and the first cutting and the second cutting are automatically performed according to the cutting parameters.

2. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: Before grinding and polishing the vertical slices, the method further includes: performing glue filling treatment on the vertical slices.

3. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: After grinding and polishing the vertical slice, the method further includes placing the vertical slice under a microscope and marking the area to be cut.

4. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 3, characterized in that: After marking the area to be cut, the method further includes: performing conductive treatment on the vertical slices by spraying gold or carbon.

5. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 4, characterized in that: After the conductive treatment, the method further includes: using conductive copper glue to stick the vertical slice to the base, and coating the surface of the vertical slice with conductive silver glue.

6. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: After placing the plurality of vertical slices into the sample chamber of the FIB-SEM dual beam system, the sample chamber is evacuated to a vacuum degree less than or equal to 5×10 -3 Pa.

7. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: Adjusting the system so that the electron beam and ion beam are co-focused at the same location involves: Position the area to be cut, adjust the sample stage working distance to the concentric height of the electron beam and the ion beam, and adjust the image to be clear; Rotate the sample stage to a fixed angle and adjust the Z-axis height of the sample stage and the ion beam offset until the confocal point of the ion beam and electron beam is found.

8. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: Depositing the identification mark on the area to be cut includes: first forming a deposition layer, and then forming the identification mark on the deposition layer by ion beam bombardment.

9. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: The protective layer is one of a tungsten layer, a platinum layer and a carbon layer.

10. The focused ion beam automatic cutting method for the bottom of a blind hole according to claim 1, characterized in that: After the first and second cutting are completed, the system parameters are adjusted to make the image clear, and the cross-section of the cut slices is scanned and photographed.