Manufacturing method of aluminum alloy composite well lid
Through the production method of aluminum alloy composite manhole cover, the integrated molding of the lining frame and aluminum alloy and the fusion through holes are used to solve the problem of insufficient corrosion resistance of existing metal manhole covers, high wear resistance and corrosion resistance are achieved, and the Lifespan and cost-effective, suitable for high-end decoration and economical use.
Patent Information
- Application Number
- CN202411327307.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-23
- Publication Date
- 2024-11-15
AI Technical Summary
The existing metal manhole covers are not durable in corrosion protection and are prone to rust and corrosion, resulting in advance replacement and repair, which increases the economic burden of municipal roads and community properties. The unit price of high-end decorative manhole covers is relatively high and the market acceptance is limited.
Using the production method of aluminum alloy composite manhole cover, the inner lining skeleton and aluminum alloy are formed integrally, polishing and fusion through holes are carried out, combined with high-pressure injection or gravity cast aluminum alloy solution, to increase wear resistance and corrosion resistance, and through rivets Sealed for increased strength and tear resistance.
It realizes wear resistance and corrosion resistance of aluminum alloy composite manhole covers, extends service life, maintains a high-end appearance, reduces costs, and improves the durability and market acceptance of the product.
Smart Images

Figure CN118951624A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of manhole cover manufacturing, and in particular to a manufacturing method of an aluminum alloy composite manhole cover. Background Art
[0002] Most of the existing manhole cover products on the market are made of cast iron, resin composite materials, and cement composites. The unit price is not high and they are used in the field of functional products. In the field of high-end decorative manhole covers, there are cast iron colored artistic manhole covers and single-material stainless steel manhole covers. The surface of the cast iron artistic colored manhole covers ages and fades over time. The manhole covers made of pure stainless steel have high toughness but slightly insufficient strength. They are not suitable for large-scale application and promotion. In addition, the unit prices of both are high and the market acceptance is limited.
[0003] Among them, rainwater grates and manhole covers made of traditional cast iron and steel products are the main products used for drainage ditches and drainage wells in municipal roads and residential areas. Although the appearance is painted for corrosion protection, due to the rust and corrosion characteristics of metal materials, they are generally insufficient in terms of corrosion protection and durability. Most cast iron and steel rainwater grates and manhole covers with a design life (theoretical life) of 25 to 30 years are replaced and repaired in advance due to the quality degradation caused by corrosion and insufficient durability, which is a great economic consumption for municipal road maintenance departments and community property management. How to extend the durability of metal products at a low cost and present high-end decorativeness is a major research direction in the industry. Although zinc plating, nickel plating, chrome plating, aluminum plating and other appearance anti-corrosion can delay corrosion to a certain extent, they can only achieve a thinner coating due to electroplating technology. Because the coating is easy to fall off due to the friction of vehicles and pedestrians on the road, the maintenance time is not long, and the appearance performance cannot be maintained for a long time. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a method for manufacturing an aluminum alloy composite manhole cover.
[0005] The technical solution adopted by the present invention to solve the technical problem is: construct a method for manufacturing an aluminum alloy composite manhole cover, wherein the aluminum alloy composite manhole cover is compositely formed by an inner lining frame and an aluminum alloy, and comprises the following steps:
[0006] S1. The workpiece after stamping is used as the inner lining skeleton of the aluminum alloy composite manhole cover, and a corresponding polishing treatment is performed according to the material of the inner lining skeleton;
[0007] S2. According to the size of the aluminum alloy composite manhole cover, at least one positioning hole is processed on the inner lining frame;
[0008] S3. According to the application requirements of the aluminum alloy composite manhole cover, processing interlaced through holes on the inner lining frame;
[0009] S4. Place the processed inner lining skeleton into a composite cavity, and add an aluminum alloy solution into the composite cavity. At a preset temperature, the aluminum alloy solution solidifies, so that the inner lining skeleton and the aluminum alloy are formed into one body.
[0010] In some embodiments, in step S1, the material of the liner skeleton is carbon steel or cast iron;
[0011] If the material of the lining frame is carbon steel, the surface of the lining frame is mechanically polished by a sanding machine to make the surface bright and free of oxide scale;
[0012] If the material of the lining skeleton is cast iron, the surface of the lining skeleton is finely sandblasted and polished by a front and back polishing machine so that there is no molding sand on the surface.
[0013] In some embodiments, in step S3, the application requirements include: anti-slip particles are provided on the aluminum alloy composite manhole cover; reinforcing ribs are provided on the aluminum alloy composite manhole cover; the force direction of the aluminum alloy composite manhole cover; the size of the aluminum alloy composite manhole cover; and the load-bearing grade of the aluminum alloy composite manhole cover.
[0014] In some embodiments, in step S3, if the aluminum alloy composite manhole cover is provided with anti-skid particles, a fusion hole is provided within a preset radius range of the position of the lining frame corresponding to the anti-skid particles.
[0015] In some embodiments, in step S3, if the aluminum alloy composite manhole cover is provided with reinforcing ribs, a fusion hole having a diameter not less than a preset diameter is provided in the reinforcing ribs of the lining frame.
[0016] In some embodiments, in step S3, a finite element model is constructed according to the size of the aluminum alloy composite manhole cover, and fusion holes are set on the lining frame according to the force direction and load-bearing level of the aluminum alloy composite manhole cover.
[0017] In some embodiments, in step S4, the preset temperature is not less than 200°C.
[0018] In some embodiments, in step S4, the aluminum alloy solution is injected under high pressure or gravity cast using a die casting machine.
[0019] In some embodiments, the method for manufacturing the aluminum alloy composite manhole cover further includes step S5:
[0020] The aluminum alloy composite manhole cover formed in step S4 is polished, and the positioning holes are coated with sealant and then hot-riveted and sealed with aluminum alloy rivets.
[0021] The implementation of the present invention has the following beneficial effects: the aluminum alloy composite manhole cover is formed by an inner lining skeleton and an aluminum alloy in one piece, and the aluminum alloy composite manhole cover has the wear resistance and corrosion resistance of the aluminum alloy layer and the appearance, is easy to maintain and has a high-end appearance, and the density of the aluminum alloy material is relatively light, which can bring long-term use value and appearance retention effect. At the same time, the inner lining skeleton is provided with a fusion through hole, which can greatly improve the composite strength between the aluminum alloy and the inner lining skeleton. When the surface of the aluminum alloy composite manhole cover is subjected to a certain impact yield, the surface alloy layer and the middle metal layer can be synchronously yielded, thereby increasing the transverse tear resistance. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to more clearly illustrate the technical solution of the present invention, the present invention will be further described below in conjunction with the accompanying drawings and embodiments. It should be understood that the following drawings only show certain embodiments of the present invention and should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work. In the drawings:
[0023] Figure 1 is a schematic flow chart of a method for manufacturing an aluminum alloy composite manhole cover in some embodiments of the present invention;
[0024] Figure 2 is a schematic diagram of the composite structure of an aluminum alloy composite manhole cover in some embodiments of the present invention;
[0025] Figure 3 It is a structural schematic diagram of an embodiment of an aluminum alloy composite manhole cover. DETAILED DESCRIPTION
[0026] In order to have a clearer understanding of the technical features, purposes and effects of the present invention, the specific embodiments of the present invention are now described in detail with reference to the accompanying drawings. In the following description, it should be understood that the directions or positional relationships indicated by "front", "back", "up", "down", "left", "right", "longitudinal", "horizontal", "vertical", "horizontal", "top", "bottom", "inside", "outside", "head", "tail", etc. are based on the directions or positional relationships shown in the accompanying drawings, are constructed and operated in a specific direction, and are only for the convenience of describing the present technical solution, rather than indicating that the device or element referred to must have a specific direction, and therefore cannot be understood as a limitation to the present invention.
[0027] It should also be noted that, unless otherwise clearly specified and limited, the terms such as "installed", "connected", "connected", "fixed", "set" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. When an element is referred to as being "on" or "under" another element, the element can be "directly" or "indirectly" located on the other element, or there may be one or more intermediate elements. The terms "first", "second", "third", etc. are only for the convenience of describing the present technical solution, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first", "second", "third", etc. can explicitly or implicitly include one or more of the features. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.
[0028] See also Figure 1 , is a method for manufacturing an aluminum alloy composite manhole cover in some embodiments of the present invention, such as Figure 2 As shown, the aluminum alloy composite manhole cover is compositely formed by an inner lining frame 1 and an aluminum alloy 2. The manufacturing method of the aluminum alloy composite manhole cover includes the following steps:
[0029] S1, using the workpiece after stamping as the inner lining skeleton 1 of the aluminum alloy composite manhole cover, and performing corresponding polishing treatment according to the material of the inner lining skeleton 1;
[0030] S2. According to the size of the aluminum alloy composite manhole cover, at least one positioning hole 11 is processed on the lining frame 1;
[0031] S3. According to the application requirements of the aluminum alloy composite manhole cover, a fusion hole 12 is processed on the inner lining frame 1;
[0032] S4, placing the processed liner skeleton 1 into the composite cavity 13, and adding the aluminum alloy 2 solution into the composite cavity 13, and solidifying the aluminum alloy 2 solution at a preset temperature, so that the liner skeleton 1 and the aluminum alloy 2 are formed into one body.
[0033] It can be understood that the aluminum alloy composite manhole cover is formed by an inner lining frame 1 and an aluminum alloy 2 in one piece. The aluminum alloy composite manhole cover has the wear resistance and corrosion resistance of the aluminum alloy 2 layer and the appearance, is easy to maintain and has a high-end appearance. The density of the aluminum alloy 2 material is relatively light, which can bring long-term use value and appearance retention effect. At the same time, the inner lining frame 1 is provided with a fusion hole 12, which can greatly improve the composite strength between the aluminum alloy 2 and the inner lining frame 1. When the surface of the aluminum alloy composite manhole cover is subjected to a certain impact and yields, the surface alloy layer and the intermediate metal layer can yield synchronously, increasing the lateral tear resistance.
[0034] Among them, the material of the lining skeleton 1 is carbon steel or cast iron. If the material of the lining skeleton 1 is carbon steel, the surface of the lining skeleton 1 is mechanically polished by a sanding machine to make the surface bright and free of oxide scale. If the material of the lining skeleton 1 is cast iron, the surface of the lining skeleton 1 is finely sandblasted and the front and back sides are polished by a sanding machine to make the surface free of molding sand. Polishing treatment may not affect the metal bonding effect, and the lining skeleton 1 can be cut to a suitable size by a punching machine or laser, and then the carbon steel lining skeleton or the cast iron lining skeleton is used as the load-bearing lining skeleton of the aluminum alloy composite manhole cover to ensure the strength of the aluminum alloy composite manhole cover, which reduces the cost compared to the manhole cover made of pure aluminum alloy in the past.
[0035] In step S2, the inner lining skeleton 1 can be processed with more than one number of positioning holes 11 according to the size of the aluminum alloy composite manhole cover. The number of the positioning holes 11 can be 1 to 2, or 4 to 6.
[0036] In step S3, the application requirements include: anti-slip particles are provided on the aluminum alloy composite manhole cover; reinforcing ribs are provided on the aluminum alloy composite manhole cover; the force direction of the aluminum alloy composite manhole cover; the size of the aluminum alloy composite manhole cover; and the load-bearing grade of the aluminum alloy composite manhole cover.
[0037] Among them, if the aluminum alloy composite manhole cover is provided with anti-skid particles, a fusion hole 12 is set within a preset radius range of the position corresponding to the inner lining skeleton 1 and the anti-skid particles. It can be understood that if the aluminum alloy composite manhole cover is provided with anti-skid particles in actual needs, the anti-skid particles need to be provided with more than one fusion hole 12 within a preset radius range at the position corresponding to the inner lining skeleton 1, and the preset radius is preferably 5 cm. The purpose of setting the fusion hole is to make the inner lining skeleton 1 and the aluminum alloy 2 solution interactively fuse in the composite cavity 13 to achieve the effect of increasing strength. When the surface of the finished product is subjected to a certain impact yield, the surface aluminum alloy 2 layer and the metal layer of the inner lining skeleton 1 can yield synchronously, thereby increasing the lateral tear resistance.
[0038] The aluminum alloy composite manhole cover is provided with reinforcing ribs, and the reinforcing ribs of the inner lining frame 1 are provided with intersecting holes 12 of a preset diameter not less than that. The preset diameter is preferably 1 mm, so that the reinforcing ribs and the surface can be subjected to synchronous stress when the final product is subjected to pressure yielding during use, thereby achieving a long-term composite effect.
[0039] Further, in step S3, a finite element model is constructed according to the size of the aluminum alloy composite manhole cover, and the fusion holes 12 are set on the lining frame 1 according to the force direction and load-bearing level of the aluminum alloy composite manhole cover. If the size of the aluminum alloy composite manhole cover is larger and the product load-bearing level is higher, the number of fusion holes 12 is increased accordingly. In a specific embodiment, Figure 3 As shown, the aluminum alloy composite manhole cover is generally a rectangular parallelepiped structure, which is mainly subjected to longitudinal force, and a fusion hole 12 can be added to the non-main force-bearing part of the surface of the lining frame 1 where the longitudinal force is applied. When the composite processing of the aluminum alloy composite manhole cover is completed, the fusion hole 12 will be completely filled with aluminum alloy solution.
[0040] In step S4, the preset temperature is not less than 200°C. The temperature in the composite cavity 13 is kept not less than 200°C, so that the composite process between the liner skeleton 1 and the aluminum alloy 2 solution is activated, so that the aluminum alloy 2 solution and the surface of the liner skeleton 1 are better combined. In addition, in step S4, the aluminum alloy 2 solution is injected with high pressure by a die-casting machine or gravity cast by a gravity casting machine. The composite cavity 13 is provided with more than one fixed / limiting column device, and the fixed / limiting column cooperates with the positioning hole 11. When the liner skeleton 1 is placed in the composite cavity 13, it is used to fix the liner skeleton 1 so that the liner skeleton 1 does not loosen inside to avoid affecting the bonding size.
[0041] The method for manufacturing the aluminum alloy composite manhole cover also includes step S5: polishing the aluminum alloy composite manhole cover formed in step S4, applying sealant to the positioning hole 11, and then performing heat riveting sealing with an aluminum alloy 2 rivet. Specifically, after the finished blank is cleaned and polished, the positioning hole 11 is filled with a highly weather-resistant sealant, and then heat riveting sealing is performed with a prefabricated aluminum alloy rivet.
[0042] The specific process of the manufacturing method of the aluminum alloy composite manhole cover is as follows: a carbon steel frame or a cast iron frame of suitable size is cut out by a punching machine or a laser as an inner lining frame 1, and the inner lining frame 1 may be provided with drainage holes, lifting holes, positioning holes 11 and blending holes 12, and the inner lining frame 1 may be placed in the composite cavity 13 of the mold of a die casting machine or a gravity casting machine, so that the positioning column of the mold and the positioning hole 11 of the inner lining frame 1 are combined, and after the mold is closed, the inner lining frame 1 is located in the middle position of the composite cavity 13, and after the inner lining frame 1 is fixed, a space of a certain size is provided for the aluminum alloy 2 solution to be coated, and the aluminum alloy 2 solution may be injected into the composite cavity 13 by high pressure, and filled into the blending holes 12 around the inner lining frame 1 and itself through the runner, so as to form an aluminum alloy 2 solution coating the inner lining frame 1. The aluminum alloy 2 solution may semi-coat or fully coat the inner lining frame 1.
[0043] It can be understood that the above embodiments only express the preferred implementation modes of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the patent scope of the present invention. It should be pointed out that, for ordinary technicians in this field, without departing from the concept of the present invention, the above technical features can be freely combined, and several deformations and improvements can be made, which all belong to the protection scope of the present invention. Therefore, all equivalent changes and modifications made to the scope of the claims of the present invention should belong to the scope covered by the claims of the present invention.
Claims
1. A method for manufacturing an aluminum alloy composite manhole cover, wherein the aluminum alloy composite manhole cover is compositely formed by an inner lining frame (1) and an aluminum alloy (2), characterized in that: Includes steps: S1, using the workpiece after stamping and shaping as the inner lining frame (1) of the aluminum alloy composite manhole cover, and performing corresponding polishing treatment according to the material of the inner lining frame (1); S2. According to the size of the aluminum alloy composite manhole cover, processing at least one positioning hole (11) on the inner lining frame (1); S3. According to the application requirements of the aluminum alloy composite manhole cover, a fusion hole (12) is processed on the inner lining frame (1); S4. Place the processed inner lining skeleton (1) into the composite cavity (13), and add the aluminum alloy (2) solution into the composite cavity (13). At a preset temperature, the aluminum alloy (2) solution solidifies, so that the inner lining skeleton (1) and the aluminum alloy (2) are formed into one body.
2. The method for manufacturing the aluminum alloy composite manhole cover according to claim 1, characterized in that: In step S1, the material of the liner frame (1) is carbon steel or cast iron; If the material of the lining frame (1) is carbon steel, the surface of the lining frame (1) is mechanically polished by a sanding machine to make the surface bright and free of oxide scale; If the material of the lining frame (1) is cast iron, the surface of the lining frame (1) is finely sandblasted and polished with a front and back polishing machine so that there is no molding sand on the surface.
3. The method for manufacturing the aluminum alloy composite manhole cover according to claim 1, characterized in that: In step S3, the application requirements include: anti-slip particles are provided on the aluminum alloy composite manhole cover; reinforcing ribs are provided on the aluminum alloy composite manhole cover; the force direction of the aluminum alloy composite manhole cover; the size of the aluminum alloy composite manhole cover; and the load-bearing grade of the aluminum alloy composite manhole cover.
4. The method for manufacturing the aluminum alloy composite manhole cover according to claim 3, characterized in that: In step S3, if the aluminum alloy composite manhole cover is provided with anti-skid particles, a fusion hole (12) is provided within a preset radius range of the position of the lining frame (1) corresponding to the anti-skid particles.
5. The method for manufacturing the aluminum alloy composite manhole cover according to claim 3, characterized in that: In step S3, if the aluminum alloy composite manhole cover is provided with reinforcing ribs, a fusion hole (12) having a diameter not less than a preset diameter is provided on the reinforcing ribs of the lining frame (1).
6. The method for manufacturing the aluminum alloy composite manhole cover according to claim 3, characterized in that: In step S3, a finite element model is constructed according to the size of the aluminum alloy composite manhole cover, and a fusion hole (12) is set on the lining frame (1) according to the force direction and load-bearing level of the aluminum alloy composite manhole cover.
7. The method for manufacturing an aluminum alloy composite manhole cover according to claim 1, characterized in that: In step S4, the preset temperature is not less than 200°C.
8. The method for manufacturing an aluminum alloy composite manhole cover according to claim 1, characterized in that: In step S4, the aluminum alloy (2) solution is injected under high pressure or gravity casted using a die casting machine.
9. The method for manufacturing an aluminum alloy composite manhole cover according to claim 1, characterized in that: The method for manufacturing the aluminum alloy composite manhole cover further comprises step S5: The aluminum alloy composite manhole cover formed in step S4 is polished, and the positioning hole (11) is coated with sealant and then heat-riveted and sealed with aluminum alloy rivets.
Citation Information
Patent Citations
Abrasion-proof composite roller, board and manufacturing method thereof
CN101239382A
Composite manhole cover and manufacturing method thereof
CN101899844A
Technology for producing robot joint part product by composite casting and melting of ferro-molybdenum
CN104959576A
Nodular cast iron well lid and preparation method thereof
CN114703902A
Metal composite cover plate and manufacturing method thereof
CN118241741A