Antistatic treatment manufacturing process for transfer film
By immersing and vibrating the transfer film, and using the heating and uniform pressing technology of the press box, the problems of electrostatic interference and coating uniformity of the transfer film are solved, and the long-term and uniform distribution of the antistatic agent is achieved. , ensuring efficient use of transfer membranes.
Patent Information
- Application Number
- CN202411119823.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing transfer films are often affected by electrostatic interference during use, and the commonly used antistatic agent spraying method is limited by humidity, which is prone to deactivation and fall off, affecting the uniformity of the evaporated coating.
Using an antistatic treatment manufacturing process, using a device including an immersion box and a press-fit box, the antistatic agent is immersed on the middle layer film through the immersion box, and the diffusion and bonding of the antistatic agent is promoted by using a vibration mechanism and a heating device to form a The network structure improves antistatic properties, and ensures uniform distribution and long-term use of antistatic agents through heating and uniform compression box.
It extends the effective service life of the antistatic agent, improves the antistatic performance, saves the investment of the antistatic agent, ensures the uniform coating effect of the transfer film, and avoids static interference.
Smart Images

Figure CN118952653A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of transfer film production, in particular to an antistatic treatment manufacturing process for a transfer film. Background Art
[0002] Transfer film is a kind of chemical elastic film that is an intermediate carrier and exists on a transfer paper base or a plastic base. It carries the printed or printed pattern and is used to transfer it to the printed object. Since the transfer film is a poor conductor, a large amount of charge often accumulates on the surface of the transfer film, which will generate static electricity when the transfer film is used or processed later, causing interference with its use.
[0003] Common methods of removing static electricity are to spray antistatic agents on the surface of the transfer film. The antistatic agent conducts the charge to the moisture in the air, thereby avoiding the generation of static electricity. However, the antistatic effect of the antistatic agent sprayed on the surface of the transfer film is limited by the humidity in the environment, and the antistatic agent on the surface is prone to inactivation and shedding, resulting in a decrease in antistatic performance. At the same time, the transfer film is often evaporated with metal coating according to demand during use. The antistatic agent sprayed on the surface will reduce the uniformity of the evaporated coating to a certain extent. Summary of the invention
[0004] 1. Technical issues to be solved
[0005] In view of the deficiencies in the prior art, the present invention provides a transfer film antistatic treatment manufacturing process to solve the problems raised in the above background technology.
[0006] (II) Technical solution
[0007] To achieve the above purpose, the present invention is implemented through the following technical solutions: a transfer film antistatic treatment manufacturing process, using an antistatic treatment device for treatment and lamination, the antistatic treatment device includes a device body, an impregnation box and a lamination box are installed in the device body at intervals, the impregnation box impregnates the middle film with an antistatic agent, and the lamination box laminates the upper, middle and lower films, the device body includes an installation box, and the inner wall of the installation box is installed with three groups of unwinding rollers, two groups of guide rollers, one group of driving rollers and a winding roller, and the antistatic treatment process includes the following steps:
[0008] S1. Install the upper film, the middle film and the lower film on the corresponding unwinding rollers respectively, add antistatic agent into the impregnation box, and add glue into the pressing box to complete the preparation of raw materials and equipment;
[0009] The impregnation box comprises a first box body, the inner wall of the first box body is rotatably connected to a limiting roller shaft, and a vibration mechanism is installed at the bottom of the limiting roller shaft;
[0010] S2, the middle film is passed through the first box body, and passes through the lower end of the limiting roller shaft and then passes through the opposite side. The upper film and the lower film are guided by the guide roller together with the middle film that passes through the pressure box, and finally passes through the bottom of the driving roller and is wound up to the outer wall of the winding roller, thus completing the preparation and installation of the three films;
[0011] The pressing box comprises a pressing box body, a pressing assembly and a rubber roller are installed on the inner wall of the pressing box, and the pressing assembly comprises an upper pressing assembly and a lower pressing assembly which are arranged at intervals;
[0012] S3. Set the heating temperature of the temperature controller to 55-60°C, drive the upper pressing assembly downward to adjust the gap between the upper pressing assembly and the lower pressing assembly according to the finished product requirements, control the motor speed, and complete the equipment parameter adjustment;
[0013] S4, the motor works, so that the upper film, the middle film and the lower film move toward the guide roller, the middle film drives the limiting roller shaft to rotate in the first box, and the limiting roller shaft periodically drives the vibration mechanism to vibrate when rotating, the upper end of the vibration mechanism contacts the middle film to knock, and the lower end of the vibration mechanism stirs the antistatic agent at the same time;
[0014] S5, the upper, middle and lower films guided by the guide rollers enter the pressing box in the order of upper, middle and lower from top to bottom, and are pressed by heating and the upper pressing assembly and the lower pressing assembly with gradually decreasing spacing, and the motor drives the driving roller to rotate to promote the pressing process;
[0015] S6. The bottom of the pressed transfer film passes through the upper end surface of the rubber roller, and the rubber roller rotates to apply glue to the lower end of the lower layer of the transfer film. After gluing, the transfer film is rolled up to the winding roller, and the antistatic treatment and manufacturing of the transfer film are completed.
[0016] As a further preference, the thickness of the upper membrane is -mm, the thickness of the middle membrane is -mm, the thickness of the lower membrane is -mm, the middle membrane is a porous structure, and the upper and lower membranes are both thin film structures.
[0017] As a further preference, the limiting roller shaft comprises a rotating shaft, an outer wall of the rotating shaft is fixedly connected with an anti-skid roller, and an outer wall of the anti-skid roller is provided with a plurality of groups of anti-skid grooves at intervals.
[0018] As a further preference, the vibration mechanism includes a vibration rod and a support sleeve, the vibration rod is slidably connected in the support sleeve and the lower end of the vibration rod is fixedly connected to a first elastic component, the first elastic component is fixedly connected to the bottom of the inner cavity of the support sleeve at one end facing away from the vibration rod, two groups of vibration wings are symmetrically fixedly connected to the outer wall of the vibration rod, and several groups of vibration components are installed at intervals on the upper end surface of the vibration wing.
[0019] As a further preference, the vibration component includes a mounting sleeve, a striking rod is slidably connected inside the mounting sleeve, a connecting rod is fixedly connected to the lower end of the striking rod, the lower end of the connecting rod passes through the bottom of the mounting sleeve and is rotatably connected to a rotating wheel, a second elastic component is provided on the outer wall of the connecting rod, and the second elastic component is located in the area adjacent to the lower end of the striking rod and the bottom of the inner cavity of the mounting sleeve.
[0020] As a further preference, the pressing box includes a second box, which has an inlet on the side close to the impregnation box and an outlet on the side away from the impregnation box, a first heating wire is installed at the bottom of the inner cavity of the second box, and the bottom of the inner cavity of the second box is filled with glue.
[0021] As a further preference, the upper pressing assembly includes an upper placing box, an electric push rod is installed on the top of the upper placing box, the electric push rod passes through the second box body and is fixedly connected to the upper placing box, a second heating wire is installed on the inner wall of the upper placing box, and several groups of upper rollers are installed on the bottom of the second heating wire.
[0022] As a further preference, an upper heat spreader is fixedly connected to the lower end of the inner wall of the upper placement box, the lower end of the upper heat spreader is an inclined surface, and a plurality of groups of upper mounting grooves are spaced apart on the lower end surface of the upper heat spreader, and the outer wall of the upper roller shaft is rotatably connected in the upper mounting groove.
[0023] As a further preference, the lower pressing assembly includes a lower heat spreader, and a plurality of groups of lower mounting grooves are provided at intervals on the upper surface of the lower heat spreader, and a lower roller is rotatably connected in the lower mounting groove.
[0024] As a further preference, the upper end surfaces of several groups of lower roller shafts and the upper end surface of the rubber roller are located at the same horizontal height.
[0025] Beneficial Effects
[0026] The present invention provides a transfer film antistatic treatment manufacturing process, which has the following beneficial effects:
[0027] 1. The device sets up the structure of upper, middle and lower membranes, and attaches antistatic agent to the porous middle membrane. The antistatic agent forms a network structure by diffusion and movement, and some polar groups migrate to the upper surface to improve the binding force between the antistatic agent and the membrane layer. While playing an antistatic role, it extends the effective service life of the antistatic agent. At the same time, the thickness of the upper membrane is smaller than that of the lower membrane. The antistatic agent is preferentially concentrated in the upper area of the transfer membrane, which can save the investment proportion of the antistatic agent under the premise of the same antistatic ability.
[0028] 2. The device is provided with an impregnation box, and the middle layer film enters the first box body, is then wound around the lower end of the anti-skid roller, and passes through the first box body from the opposite side. The anti-static agent is placed at the bottom of the inner cavity of the first box body, and the pulled middle layer film pushes the anti-skid roller to roll. The anti-skid groove arranged on the surface of the anti-skid roller can increase the friction between the middle layer film and the anti-skid roller. Since the anti-skid roller is an elliptical roller, as the anti-skid roller rotates, the long end of the anti-skid roller pushes the vibration rod to compress the first elastic component and move downward. When the long end of the anti-skid roller is removed, the compressed first elastic component pushes the vibration rod to move upward. As the anti-skid roller rotates, the vibration rod drives the vibration wing to vibrate up and down periodically. When the vibration wing vibrates upward, the upper end of the impact rod knocks on the middle layer film, promotes the overflow of bubbles attached to the middle layer film, and improves the wettability of the middle layer film. The impact rod pushes the connecting rod downward to move, and the rotating wheel rotates due to the resistance of the anti-static agent, thereby stirring the anti-static agent to avoid stratification of the anti-static agent and affecting the uniformity of adhesion of the middle layer film.
[0029] 3. By setting up a pressing box, the three-layer film enters the adjacent area of the upper pressing assembly and the lower pressing assembly from the box entrance after being corrected by the guide roller. Since the lower end of the upper heat spreader is in an inclined state, the distance between several groups of upper rollers and the lower rollers gradually decreases, thereby pressing the three-layer film. The first heating wire heats the lower roller through the glue and the lower heat spreader to prevent the glue from solidifying while improving the stability of the heating temperature. The second heating wire also improves the uniformity of heating the upper roller at the upper end through the upper heat spreader, thereby improving the uniformity of pressing. At the same time, the driving roller transports the transfer film outward, and the transfer film pushes several groups of upper rollers and lower rollers to rotate, thereby ensuring the pressing force and avoiding deformation of the transfer film caused by uneven pressure distribution. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic structural diagram of a transfer film antistatic treatment manufacturing device of the present invention;
[0031] Figure 2 It is a schematic diagram of a half-section structure of the device of the present invention;
[0032] Figure 3 It is a schematic diagram of the main structure of the device of the present invention;
[0033] Figure 4 It is a schematic diagram of the structure of the impregnation box of the present invention;
[0034] Figure 5 It is a schematic diagram of the limiting roller structure of the present invention;
[0035] Figure 6 It is a schematic diagram of the cross-sectional structure of the vibration mechanism of the present invention;
[0036] Figure 7 It is a schematic diagram of the cross-sectional structure of the vibration component of the present invention;
[0037] Figure 8It is a schematic diagram of a half-section structure of a pressing box of the present invention;
[0038] Fig. 9 It is a schematic diagram of a half-section structure of a press-fit assembly of the present invention;
[0039] Fig.10 It is a schematic diagram of a half-section structure of a box body of the present invention;
[0040] Fig.11 It is a schematic diagram of the cross-sectional structure of the upper pressing assembly of the present invention;
[0041] Fig.12 It is a schematic diagram of the structure of the lower pressing assembly of the present invention.
[0042] In the figure: 1 device body, 11 installation box, 12 unwinding roller, 13 guide roller, 14 temperature controller, 15 glue adding port, 16 driving roller, 17 winding roller, 2 impregnation box, 21 first box body, 22 limiting roller shaft, 221 anti-skid groove, 222 anti-skid roller, 223 rotating shaft, 23 vibration mechanism, 231 vibration rod, 232 first elastic component, 233 support sleeve, 234 vibration wing, 235 vibration component, 2351 impact rod, 2352 installation sleeve, 2353 second elastic component, 2 354 connecting rod, 2355 rotating wheel, 3 pressing box, 31 pressing box body, 311 second box body, 312 box inlet, 313 first heating wire, 314 box outlet, 32 pressing assembly, 321 upper pressing assembly, 3211 upper placement box, 3212 electric push rod, 3213 upper heat spreader, 3214 upper mounting groove, 3215 upper roller, 3216 second heating wire, 322 lower pressing assembly, 3221 lower heat spreader, 3222 lower mounting groove, 3223 lower roller, 33 rubber roller. DETAILED DESCRIPTION
[0043] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be understood as limiting the present invention.
[0044] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more features. In the description of the present invention, the meaning of "multiple" is two or more, unless otherwise clearly and specifically defined.
[0045] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or mutual communication; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0046] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0047] The disclosure below provides many different embodiments or examples to implement different structures of the present invention. In order to simplify the disclosure of the present invention, the parts and settings of specific examples are described below. Of course, they are only examples, and the purpose is not to limit the present invention. In addition, the present invention can repeat reference numbers and / or reference letters in different examples, and this repetition is for the purpose of simplicity and clarity, which itself does not indicate the relationship between the various embodiments and / or settings discussed. In addition, the present invention provides various specific examples of processes and materials, but those of ordinary skill in the art can appreciate the application of other processes and / or the use of other materials.
[0048] The embodiment of the present invention provides a transfer film antistatic treatment manufacturing process, comprising the following steps:
[0049] S1. Install the upper film, the middle film and the lower film on the corresponding unwinding rollers respectively, add antistatic agent into the impregnation box, and add glue into the pressing box to complete the preparation of raw materials and equipment;
[0050] The impregnation box comprises a first box body, the inner wall of the first box body is rotatably connected to a limiting roller shaft, and a vibration mechanism is installed at the bottom of the limiting roller shaft;
[0051] S2, the middle film is passed through the first box body, and passes through the lower end of the limiting roller shaft and then passes through the opposite side. The upper film and the lower film are guided by the guide roller together with the middle film that passes through the pressure box, and finally passes through the bottom of the driving roller and is wound up to the outer wall of the winding roller, thus completing the preparation and installation of the three films;
[0052] The pressing box comprises a pressing box body, a pressing assembly and a rubber roller are installed on the inner wall of the pressing box, and the pressing assembly comprises an upper pressing assembly and a lower pressing assembly which are arranged at intervals;
[0053] S3. Set the heating temperature of the temperature controller to 55-60°C, drive the upper pressing assembly downward to adjust the gap between the upper pressing assembly and the lower pressing assembly according to the finished product requirements, control the motor speed, and complete the equipment parameter adjustment;
[0054] S4, the motor works, so that the upper film, the middle film and the lower film move toward the guide roller, the middle film drives the limiting roller shaft to rotate in the first box, and the limiting roller shaft periodically drives the vibration mechanism to vibrate when rotating, the upper end of the vibration mechanism contacts the middle film to knock, and the lower end of the vibration mechanism stirs the antistatic agent at the same time;
[0055] S5, the upper, middle and lower films guided by the guide rollers enter the pressing box in the order of upper, middle and lower from top to bottom, and are pressed by heating and the upper pressing assembly and the lower pressing assembly with gradually decreasing spacing, and the motor drives the driving roller to rotate to promote the pressing process;
[0056] S6. The bottom of the pressed transfer film passes through the upper end surface of the rubber roller, and the rubber roller rotates to apply glue to the lower end of the lower layer of the transfer film. After gluing, the transfer film is rolled up to the winding roller, and the antistatic treatment and manufacturing of the transfer film are completed.
[0057] See also Figures 1 to 12 An embodiment of the present invention provides a transfer film antistatic treatment manufacturing device, including a device body 1, an impregnation box 2 and a pressing box 3.
[0058] See also Figure 1 - Figure 3 The device body 1 includes an installation box 11, and one end of the inner wall of the installation box 11 is rotatably connected to three groups of unwinding rollers 12, and the outer walls of the three groups of unwinding rollers 12 are respectively wound with an upper film, a middle film and a lower film, and a guide roller 13 is rotatably connected to the middle of the inner wall of the installation box 11, and the guide roller 13 guides the three groups of films. The other end of the inner wall of the installation box 11 is rotatably connected to a driving roller 16 and a winding roller 17, and an impregnation box 2 is fixedly connected to the bottom of the inner cavity of the installation box 11. The impregnation box 2 is located in the adjacent area of the guide roller 13 and the unwinding roller 12, and is used to infiltrate the middle film. A pressing box 3 is also installed at the bottom of the inner cavity of the installation box 11, and the pressing box 3 is located in the adjacent area of the guide roller 13 and the driving roller 16, and is used to heat and press the three-layer film, and to apply glue to the bottom of the pressed transfer film, and the glued transfer film is conducted through the driving roller 16 and finally rolled up to the outer wall of the winding roller 17.
[0059] It should be noted that the guide roller 13 includes two sets of roller shafts arranged in parallel, and the two sets of roller shafts rotate in opposite directions to transport the three-layer film to the lamination box 3 for lamination.
[0060] It should also be noted that one end of the unwinding roller 12 passes through the mounting box 11 and is fixedly connected to a control block, which adjusts the rotational friction of the unwinding roller 12 and cooperates with the drive motor to control the film conveying speed and tension within an appropriate range.
[0061] It should be supplemented that one end of the driving roller 16 and the winding roller 17 passes through the outer wall of the installation box 11 and is fixedly connected to the output end of the driving motor to provide power for winding and pressing.
[0062] It should also be added that the outer wall of the installation box 11 is provided with a glue adding port 15 , and the glue adding port 15 is connected to the pressing box 3 .
[0063] For details, please refer to Figures 4 to 6In order to improve the wettability of the middle layer film, the impregnation box 2 includes a first box body 21, and two groups 24 are symmetrically opened on the front and rear end surfaces of the first box body 21. The inner wall of the first box body 21 is rotatably connected to a limiting roller shaft 22, and the limiting roller shaft 22 is arranged parallel to 24 to limit the depth of the middle layer film in the antistatic agent to ensure the residence time of the middle layer film in the antistatic agent. The limiting roller shaft 22 includes a rotating shaft 223, and an anti-skid roller 222 is fixedly connected to the outer wall of the rotating shaft 223. A plurality of groups of anti-skid grooves 221 are fixedly connected to the outer wall of the anti-skid roller 222 at intervals. The anti-skid grooves 221 can increase the friction between the middle layer film and the anti-skid roller 222, so that the anti-skid roller 222 can be pushed to rotate continuously during the transmission of the middle layer film. The vibration mechanism 23 includes a support sleeve 233, the lower end of the support sleeve 233 is fixedly connected to the bottom of the inner cavity of the first box body 21, the inner cavity of the support sleeve 233 is fixedly connected to a first elastic component 232, the first elastic component 232 is fixedly connected to a vibration rod 231 on the side away from the support sleeve 233, and two groups of vibration wings 234 are symmetrically fixedly connected on both sides of the vibration rod 231. The anti-slip roller 222 rotates to push the vibration rod 231 to drive the vibration wings 234 to compress the first elastic component 232 to vibrate periodically. When the vibration wings 234 vibrate, they hit the lower end of the middle film, causing the bubbles attached to the middle film to overflow, thereby improving the wettability of the middle film in the antistatic agent, thereby ensuring the uniformity of the antistatic agent content in the transfer film.
[0064] It should be noted that the inclination angle of the vibration wing 234 is the same as the installation inclination angle of the middle layer membrane, that is, the vibration wing 234 is arranged parallel to the middle layer membrane.
[0065] It should also be noted that an arc-shaped protrusion is provided on the top of the vibration rod 231 to improve the stability of the vibration rod 231 when the anti-slip roller 222 pushes the vibration rod 231.
[0066] For details, please refer to Figure 6 and Figure 7In order to further improve the uniformity of the antistatic agent adhesion on the middle film, a plurality of groups of vibration components 235 are arranged at intervals on the upper end surface of the vibration wing 234. The vibration component 235 includes a mounting sleeve 2352, which is fixedly connected to the upper end surface of the vibration wing 234 and connects the upper and lower end surfaces of the vibration wing 234. The inner cavity 252 is slidably connected to a striking rod 2351, the top of the striking rod 2351 extends out of the upper end of the mounting sleeve 2352, the lower end of the striking rod 2351 is fixedly connected to a connecting rod 2354, the end of the connecting rod 2354 away from the striking rod 2351 passes through the mounting sleeve 2352 and is rotatably connected to a rotating wheel 2355, and the outer wall of the connecting rod 2354 is provided with a second elastic component 2353, and the second elastic component 2353 is arranged on the striking rod Between the lower end of 2351 and the bottom of the inner cavity of the installation sleeve 2352, the vibrating wing 234 drives the installation sleeve 2352 to move upward, and the installation sleeve 2352 drives the impact rod 2351 to knock on the middle membrane. During the knocking, the reaction force of the middle membrane on the impact rod 2351 causes the impact rod 2351 to compress the second elastic component 2353 to push the connecting rod 2354 to move downward. When the connecting rod 2354 moves, the rotating wheel 2355 rotates due to the resistance of the antistatic agent, thereby stirring the antistatic agent. When the installation sleeve 2352 moves downward following the vibrating wing 234, the deformed second elastic component 2353 pushes the impact rod 2351 to reset, and the impact rod 2351 drives the connecting rod 2354 to move upward, so that the rotating wheel 2355 rotates.
[0067] It should be noted that the rotating wheel 2355 is a double-layer stirring paddle, which can rotate and stir when the connecting rod 2354 moves up and down.
[0068] For details, please refer to Figures 8 to 10 In order to reduce the deformation of the film layer caused by uneven force on the film layer during lamination, the lamination box 3 includes a lamination box body 31, and the lamination box body 31 includes a second box body 311. The rear end surface of the second box body 311 is provided with an inlet 312, and the lower end of the inner cavity of the second box body 311 is provided with a first heating wire 313. The lower end of the inner cavity of the second box body 311 is filled with glue, and the first heating wire 313 heats to prevent the glue from solidifying. An outlet 314 is provided on the front end surface of the second box body 311, and a lamination component 32 is installed on the inner wall of the second box body 311. The lamination component 32 includes an upper lamination component 321 and a lower lamination component 322. The thickness of the transfer film after lamination can be adjusted by controlling the distance between the upper lamination component 321 and the lower lamination component 322. A rubber roller 33 is also installed on the inner wall of the lamination box body 31. The rubber roller 33 is located close to the outlet 314 to apply glue to the lower end surface of the transfer film after lamination.
[0069] See also Fig.11 and Fig.12In order to make the transfer film heated evenly, the upper pressing assembly 321 includes an upper placement box 3211, and an electric push rod 3212 is installed on the top of the upper placement box 3211. The electric push rod 3212 is installed on the top of the second box body 311. The extended end of the electric push rod 3212 passes through the top of the second box body 311 and is fixedly connected to the upper end surface of the upper placement box 3211, which is used to push the upper placement box 3211 to move up and down. The inner wall of the upper placement box 3211 is fixedly connected to an upper heat spreader 3213 The lower end of the upper heat spreader 3213 is an inclined surface, and the distance between the upper heat spreader 3213 and the lower pressing assembly 322 gradually decreases along the moving direction of the transfer film. A plurality of upper mounting grooves 3214 are provided at intervals on the lower end surface of the upper heat spreader 3213. An upper roller 3215 is rotatably connected in the upper mounting groove 3214. A second heating wire 3216 is installed in the inner cavity of the upper placement box 3211. The second heating wire 3216 is arranged at the top of the inner cavity of the upper heat spreader 3213 and the upper placement box 3211. The adjacent area is used to heat the upper roller 3215. The upper heat spreader 3213 improves the heat conduction between the upper rollers 3215 and improves the temperature uniformity between the groups of upper rollers 3215. The lower pressing assembly 322 includes a lower heat spreader 3221. The upper end surface of the lower heat spreader 3221 is provided with a plurality of lower mounting grooves 3222. The lower mounting groove 3222 is rotatably connected with the lower roller 3223. The first heating wire 313 heats the glue and the lower heat spreader 3221. Heating, the heat is evenly transferred to the lower roller 3223 through the lower heat sink 3221, so that the lower layer of the transfer film is heated evenly, and the driving roller 16 drives the transfer film to move between several groups of upper rollers 3215 and several groups of lower rollers 3223. As the distance between the upper rollers 3215 and the lower rollers 3223 gradually decreases, the three layers of film are gradually pressed together. When the film moves, it pushes the lower roller 3223 and the upper roller 3215 to roll, so as to avoid deformation of the transfer film caused by excessive pressing force.
[0070] It should be noted that the upper heat spreader 3213 and the lower heat spreader 3221 are both made of good thermal conductor materials, and the upper roller 3215 and the lower roller 3223 are metal rollers with good thermal conductivity.
[0071] In summary, the present invention provides a transfer film anti-static treatment manufacturing process, wherein the upper, middle and lower film layers are installed on the corresponding unwinding rollers 12, the middle film passes through the first box body 21 from 24, is wound from the lower end of the anti-skid roller 222, and then passes through the opposite side 24 for infiltration treatment, when the middle film moves, it pushes the anti-skid roller 222 to rotate continuously, when the anti-skid roller 222 rotates, it pushes the vibration rod 231 to drive the vibration wing 234 to vibrate up and down, when the impact rod 2351 at the upper end of the vibration wing 234 moves upward, it knocks on the middle film to promote the overflow of attached bubbles, so as to improve the infiltration degree of the middle film, and at the same time, the impact rod 2351 is acted on by the middle film The force compresses the second elastic component 2353 to push the connecting rod 2354 to move, and the connecting rod 2354 drives the rotating wheel 2355 to move. The rotating wheel 2355 rotates due to the resistance of the antistatic agent, thereby stirring the antistatic agent and improving the uniformity of the antistatic agent. The upper film, the middle film after infiltration and the lower film are guided by the guide roller 13, and pass through the box inlet 312 together. They are heated and pressed between several groups of upper roller shafts 3215 and several groups of lower roller shafts 3223. After the pressing, the lower layer of the transfer film contacts the glue roller 33 to complete the gluing. The transfer film after gluing is guided and driven by the driving roller 16 and finally rolled up on the outer wall of the winding roller 17.
[0072] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A transfer film antistatic treatment manufacturing process, using an antistatic treatment device for treatment and lamination, characterized in that: The antistatic treatment device comprises a device body (1), wherein an impregnation box (2) and a pressing box (3) are installed at intervals in the device body (1), wherein the impregnation box (2) impregnates the middle layer film with an antistatic agent, and the pressing box (3) presses the upper layer, the middle layer and the lower layer film, wherein the device body (1) comprises an installation box (11), wherein the inner wall of the installation box (11) is installed with three groups of unwinding rollers (12), two groups of guide rollers (13), a group of driving rollers (16) and a winding roller (17), and the antistatic treatment process comprises the following steps: S1. Install the upper film, the middle film and the lower film on the corresponding unwinding rollers respectively, add antistatic agent into the impregnation box, and add glue into the pressing box to complete the preparation of raw materials and equipment; The impregnation box comprises a first box body, the inner wall of the first box body is rotatably connected to a limiting roller shaft, and a vibration mechanism is installed at the bottom of the limiting roller shaft; S2, the middle film is passed through the first box body, and passes through the lower end of the limiting roller shaft and then passes through the opposite side. The upper film and the lower film are guided by the guide roller together with the middle film that passes through the pressure box, and finally passes through the bottom of the driving roller and is wound up to the outer wall of the winding roller, thus completing the preparation and installation of the three films; The pressing box comprises a pressing box body, a pressing assembly and a rubber roller are installed on the inner wall of the pressing box, and the pressing assembly comprises an upper pressing assembly and a lower pressing assembly which are arranged at intervals; S3. Set the heating temperature of the temperature controller to 55-60°C, drive the upper pressing assembly downward to adjust the gap between the upper pressing assembly and the lower pressing assembly according to the finished product requirements, set the motor speed, and complete the equipment parameter adjustment; S4, the motor works, so that the upper film, the middle film and the lower film move toward the guide roller, the middle film drives the limiting roller shaft to rotate in the first box, and the limiting roller shaft periodically drives the vibration mechanism to vibrate when rotating, the upper end of the vibration mechanism contacts the middle film to knock, and the lower end of the vibration mechanism stirs the antistatic agent at the same time; S5, the upper, middle and lower films guided by the guide rollers enter the pressing box in the order of upper, middle and lower from top to bottom, and are pressed by heating and the upper pressing assembly and the lower pressing assembly with gradually decreasing spacing, and the motor drives the driving roller to rotate to promote the pressing process; S6. The bottom of the pressed transfer film passes through the upper end surface of the rubber roller, and the rubber roller rotates to apply glue to the lower end of the lower layer of the transfer film. After gluing, the transfer film is rolled up to the winding roller, and the antistatic treatment and manufacturing of the transfer film are completed.
2. The antistatic treatment manufacturing process of transfer film according to claim 1, characterized in that: The thickness of the upper membrane is 2-3 mm, the thickness of the middle membrane is 1-2 mm, the thickness of the lower membrane is 3-5 mm, the middle membrane is a porous structure, and both the upper and lower membranes are thin film structures.
3. The antistatic treatment manufacturing process of transfer film according to claim 2, characterized in that: The limiting roller shaft (22) comprises a rotating shaft (223), the outer wall of the rotating shaft (223) is fixedly connected with an anti-skid roller (222), and the outer wall of the anti-skid roller (222) is provided with a plurality of groups of anti-skid grooves (221) at intervals.
4. The antistatic treatment manufacturing process of transfer film according to claim 3, characterized in that: The vibration mechanism (23) comprises a vibration rod (231) and a support sleeve (233); the vibration rod (231) is slidably connected in the support sleeve (233); a first elastic component (232) is fixedly connected to the lower end of the vibration rod (231); an end of the first elastic component (232) facing away from the vibration rod (231) is fixedly connected to the bottom of the inner cavity of the support sleeve (233); two groups of vibration wings (234) are symmetrically fixedly connected to the outer wall of the vibration rod (231); and a plurality of groups of vibration components (235) are installed at intervals on the upper end surface of the vibration wings (234).
5. The antistatic treatment manufacturing process of transfer film according to claim 4, characterized in that: The vibration component (235) includes a mounting sleeve (2352), the mounting sleeve (2352) is slidably connected to an impact rod (2351), the lower end of the impact rod (2351) is fixedly connected to a connecting rod (2354), the lower end of the connecting rod (2354) passes through the bottom of the mounting sleeve (2352) and is rotatably connected to a rotating wheel (2355), the outer wall of the connecting rod (2354) is provided with a second elastic component (2353), and the second elastic component (2353) is located in the area adjacent to the lower end of the impact rod (2351) and the bottom of the inner cavity of the mounting sleeve (2352).
6. The antistatic treatment manufacturing process of transfer film according to claim 1, characterized in that: The pressing box (31) comprises a second box (311), a box inlet (312) is provided on a side of the second box (311) close to the impregnation box (2), a box outlet (314) is provided on a side of the second box (311) away from the impregnation box (2), a first heating wire (313) is installed at the bottom of the inner cavity of the second box (311), and the bottom of the inner cavity of the second box (311) is filled with glue.
7. The antistatic treatment manufacturing process of transfer film according to claim 6, characterized in that: The upper pressing assembly (321) comprises an upper placement box (3211), an electric push rod (3212) is installed on the top of the upper placement box (3211), the electric push rod (3212) passes through the second box body (311) and is fixedly connected to the upper placement box (3211), a second heating wire (3216) is installed on the inner wall of the upper placement box (3211), and a plurality of groups of upper rollers (3215) are installed at the bottom of the second heating wire (3216).
8. The antistatic treatment manufacturing process of transfer film according to claim 7, characterized in that: An upper heat spreader (3213) is fixedly connected to the lower end of the inner wall of the upper placement box (3211); the lower end of the upper heat spreader (3213) is an inclined surface, and a plurality of groups of upper mounting grooves (3214) are spaced apart on the lower end surface of the upper heat spreader (3213); the outer wall of the upper roller shaft (3215) is rotatably connected to the upper mounting groove (3214).
9. The antistatic treatment manufacturing process of transfer film according to claim 8, characterized in that: The lower pressing assembly (322) comprises a lower heat spreader (3221), and a plurality of groups of lower mounting grooves (3222) are provided at intervals on the upper end surface of the lower heat spreader (3221), and a lower roller shaft (3223) is rotatably connected in the lower mounting groove (3222).
10. The antistatic treatment manufacturing process of transfer film according to claim 9, characterized in that: The upper end surfaces of the plurality of groups of lower roller shafts (3223) and the upper end surface of the rubber roller (33) are located at the same horizontal height.
Citation Information
Cited By
High-performance precipitation-free anti-static film and preparation system thereof