Environment-friendly colored super-hydrophobic coating
By using components such as pigments, alumina aerogel, and methyl silicone resin, combined with a simple dip-coating or spray-coating process, the environmental protection and cost issues of superhydrophobic coatings have been solved, enabling the environmentally friendly production and widespread application of colored superhydrophobic coatings.
Patent Information
- Application Number
- CN202411301079.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-11-15
AI Technical Summary
Existing superhydrophobic coating materials suffer from problems such as expensive raw materials, complex preparation processes, and poor environmental friendliness, especially the use of fluorine compounds, which is harmful to human health and the environment.
Using pigments, alumina aerogel, methyl silicone resin and ethanol as the main components, a colored superhydrophobic coating is formed on the substrate surface through dip coating or spray coating process, avoiding the use of harmful fluorine compounds.
It has enabled the environmentally friendly production of colored superhydrophobic coatings, reduced costs, simplified processes, expanded the application range, and met the dual requirements of modern design for aesthetics and functionality.
Smart Images

Figure CN118956261A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of coatings, and in particular to an environmentally friendly colorful super-hydrophobic coating. Background Art
[0002] Superhydrophobicity refers to the performance state that the water contact angle on the surface of the material is greater than 150° and the water rolling angle is less than 5°. Superhydrophobicity can make water form almost spherical drops on the surface of the material, thereby giving the surface of the material self-cleaning, anti-pollution and anti-icing properties. In recent years, with the increasing research and application of superhydrophobic coatings in many fields such as the automotive industry, construction, and aerospace, the market has also put forward higher technical requirements for it. Among them, it is urgent to overcome the limitations of monotonous colors such as black, white or gray of traditional superhydrophobic materials, give the coating a variety of color characteristics, expand its application in the fields of decoration and aesthetics, and research and develop environmentally friendly colored superhydrophobic coating technology.
[0003] Colored super-hydrophobic coating refers to an advanced functional coating that combines super-hydrophobicity and colored appearance formed on the surface of the material through specific technical means. It not only provides surface super-hydrophobicity, but also can be customized with different coating colors according to needs, thereby increasing the visual appeal of the coating, expanding the application range and aesthetics of the coating, and meeting the dual requirements of modern design for beauty and functionality. These advantages make colored super-hydrophobic coatings have important application value in designing novel, personalized, and multifunctional super-hydrophobic products.
[0004] At present, most super-hydrophobic coatings have restrictive problems such as expensive raw materials, complex preparation processes, and high toxicity of chemical reagents. In particular, fluorine compounds have been widely used in traditional super-hydrophobic coatings. However, expensive fluorine compounds can cause relatively serious toxic effects on the human body and the environment, so they are poor in environmental friendliness. Summary of the invention
[0005] In view of the problems existing in the prior art, the present invention discloses an environmentally friendly colored super-hydrophobic coating, the main components and weight parts of which are:
[0006] As a preferred embodiment of the present invention, the pigment is selected from red, yellow, blue or green inorganic silicate or organic pigment with an average particle size of 1-3 microns.
[0007] As a preferred embodiment of the present invention, the average particle size of the alumina aerogel is 100-300 microns.
[0008] As a preferred embodiment of the present invention, the colorant, alumina aerogel, methyl silicone resin and ethanol are uniformly mixed according to weight to obtain a colored super-hydrophobic coating.
[0009] As a preferred embodiment of the present invention, the colored super hydrophobic coating is applied to the substrate surface by dipping or spraying to form a colored super hydrophobic coating, so that the substrate surface water contact angle is 150-160° and the water rolling angle is 3-5°. The material of the substrate is ceramic, metal, plastic, glass or cloth.
[0010] Beneficial effects of the present invention: the present invention uses colorant, alumina aerogel, methyl silicone resin and ethanol as raw materials, fundamentally solves the problems such as color design and environmental protection of super hydrophobic coating, and combines simple dip coating or spraying process, and through natural drying, colored super hydrophobic coating can be obtained. The present invention has many advantages such as simple process, easy large-scale production, low cost, green environmental protection, in addition, because of avoiding the use of harmful fluorine compounds, significantly reducing the damage to the environment, and its applicability is wide, rich in color, and application prospects are very broad, meeting the major demand of modern society for colored super hydrophobic coating products, for promoting the performance upgrade of super hydrophobic materials and promoting its wide application is of great significance. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 A product coated with a colored super-hydrophobic coating according to the present invention;
[0012] Figure 2 It is the water contact angle and rolling angle of the substrate surface of the colored super-hydrophobic coating of the present invention. DETAILED DESCRIPTION
[0013] Example 1
[0014] The present invention discloses an environmentally friendly colored super-hydrophobic coating, the main components and weight parts of which are:
[0015] The colorant is selected from red, yellow, blue or green inorganic silicate or organic colorant with an average particle size of 1 micron; the average particle size of the alumina aerogel is 100 microns.
[0016] Colorant, alumina aerogel, methyl silicone resin and ethanol are uniformly mixed by weight to obtain colored super hydrophobic coating. During use, colored super hydrophobic coating is applied to the substrate surface of materials such as ceramics, metals, plastics, glass or cloth by dip coating or spraying process, and colored super hydrophobic coating is formed on the surface, so that the substrate surface water contact angle is 160 °, and the water rolling angle is 3 °, so as to have a hydrophobic effect.
[0017] Example 2
[0018] The present invention discloses an environmentally friendly colored super-hydrophobic coating, the main components and weight parts of which are:
[0019] The colorant is selected from red, yellow, blue or green inorganic silicate or organic colorant with an average particle size of 3 microns; the average particle size of the alumina aerogel is 300 microns.
[0020] Colorant, alumina aerogel, methyl silicone resin and ethanol are uniformly mixed by weight to obtain a colored super-hydrophobic coating. During use, the colored super-hydrophobic coating is applied to the substrate surface of materials such as ceramics, metals, plastics, glass or cloth using a dip coating or spraying process, and a colored super-hydrophobic coating is formed on the surface, so that the substrate surface water contact angle is 150 °, and the water rolling angle is 5 °, so as to have a hydrophobic effect.
[0021] Example 3
[0022] The present invention discloses an environmentally friendly colored super-hydrophobic coating, the main components and weight parts of which are:
[0023] The colorant is selected from red, yellow, blue or green inorganic silicate or organic colorant with an average particle size of 2 microns; the average particle size of the alumina aerogel is 200 microns.
[0024] Colorant, alumina aerogel, methyl silicone resin and ethanol are uniformly mixed by weight to obtain a colored super-hydrophobic coating. During use, the colored super-hydrophobic coating is applied to the substrate surface of materials such as ceramics, metals, plastics, glass or cloth by dip coating or spraying process, and a colored super-hydrophobic coating is formed on the surface, so that the substrate surface water contact angle is 155 °, and the water rolling angle is 4 °, so as to have a hydrophobic effect.
[0025] Components not described in detail herein are prior art.
[0026] Although the specific embodiments of the present invention are described in detail above, the present invention is not limited to the above embodiments. Various changes can be made within the knowledge of ordinary technicians in this field without departing from the purpose of the present invention, and modifications or deformations without creative labor are still within the protection scope of the present invention.
Claims
1. An environmentally friendly colored super-hydrophobic coating, characterized in that: Its main components and weight parts are: 20-40 parts of colorant, 10-20 parts of alumina aerogel, 3-10 parts of methyl silicone resin and 150-600 parts of ethanol.
2. An environmentally friendly colored super-hydrophobic coating according to claim 1, characterized in that: The pigment is selected from red, yellow, blue or green inorganic silicate or organic pigment with an average particle size of 1-3 microns.
3. An environmentally friendly colored super-hydrophobic coating according to claim 1, characterized in that: The average particle size of the alumina aerogel is 100-300 microns.
4. An environmentally friendly colored super-hydrophobic coating according to claim 1, characterized in that: The colorant, alumina aerogel, methyl silicone resin and ethanol are uniformly mixed according to weight to obtain a colorful super-hydrophobic coating.
5. An environmentally friendly colored super-hydrophobic coating according to claim 4, characterized in that: The colored super-hydrophobic coating is coated on the surface of the substrate by a dipping or spraying process to form a colored super-hydrophobic coating.
6. An environmentally friendly colored super-hydrophobic coating according to claim 5, characterized in that: The material of the substrate is one of ceramic, metal, plastic, glass and cloth.
Citation Information
Patent Citations
Inorganic high-temperature-resistant nanopore aerogel heat-insulating coating and preparation method thereof
CN117186679A
Preparation method of corrosion-resistant anti-icing wear-resistant super-hydrophobic coating and product prepared by preparation method
CN118460102A
Cited By
Solvent-free grinding preparation method of fluoride-free super-hydrophobic colored coating of milk and plants
CN120399577A
Chemical coupling-free milk-based super-hydrophobic plant pigment coating and alkaline preparation method thereof