Polyacrylonitrile fiber and preparation method thereof
Through double-tube conveying pipelines and temperature control technology, the problem of uneven viscosity of polyacrylonitrile solution is solved, the stability of the spinning process and the performance of polyacrylonitrile fibers are improved, and high-quality carbon fiber production is achieved.
Patent Information
- Application Number
- CN202411284823.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-09-13
AI Technical Summary
During the preparation of existing polyacrylonitrile fibers, the uneven viscosity of the polyacrylonitrile solution leads to easily produce jelly or floc gel blocks during the transportation process, the filtration equipment is easily blocked, and the spinning process is poor, resulting in poor production stability. and performance indicators fluctuate greatly.
The double-tube-type conveying pipeline is adopted, and the inner tube and the second tube are used to store the insulation medium respectively. The polyacrylonitrile is controlled by setting two-stage conveying temperatures (after the booster pump and before the metering pump and after the metering pump to before the spinneret). The viscosity of the solution ensures temperature uniformity and viscosity uniformity during the transportation process, reduces temperature differences, and avoids clumping and clogging.
Through double-tube conveying pipelines and temperature regulation, the viscosity uniformity and fluidity of the polyacrylonitrile solution are ensured, the continuity and stability of the spinning process are improved, and polyacrylonitrile fibers with excellent performance and stable quality control are prepared.
Smart Images

Figure CN118957772A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of polyacrylonitrile-based carbon fiber production, and specifically relates to polyacrylonitrile fiber and a preparation method thereof. Background Art
[0002] Polyacrylonitrile fiber is the premise for producing high-performance carbon fiber. Polyacrylonitrile fiber is a polyacrylonitrile solution that is transported to a metering pump through a delivery pipeline under the action of a delivery pump, and then sprayed out from a spinneret into a coagulation bath after metering and filtration. It is coagulated into primary fibers under the action of double diffusion, and then goes through processes such as water washing, hot water drawing, oiling, drying and densification, and steam drawing, and finally rolled up to prepare polyacrylonitrile fiber. Among them, the viscosity of the polyacrylonitrile solution directly affects the filtration pressure, spinning pressure, spinnability, the formation of the stock solution flow, the tensile properties of the primary fibers, and the quality of the finished fiber (carbon fiber).
[0003] However, in the existing polyacrylonitrile fiber preparation process, the conveying pipeline used is a single sleeve, which leads to a large temperature difference between the core and the outer layer of the polyacrylonitrile solution during the conveying process, uneven viscosity of the polyacrylonitrile solution, and easy generation of jelly or floc gel blocks. The filtration accuracy of the filtration equipment is generally 1-10 μm, and the spinneret hole of the spinneret is generally 0.10-0.15 mm, both of which are relatively small. During the conveying process of the polyacrylonitrile solution, the filtration equipment is easily blocked when filtering before spinning, and the spinneret is easily blocked during the spinning process, and blocks and broken ends are generated, resulting in roller entanglement and broken wires, thereby resulting in poor production stability, high appearance hairiness rate, and large fluctuations in performance indicators of the prepared polyacrylonitrile fiber. Summary of the invention
[0004] Therefore, the present invention provides a polyacrylonitrile fiber and a preparation method thereof, which can solve the technical problem of uneven viscosity in the process of transporting polyacrylonitrile solution in the prior art.
[0005] In order to solve the above problems, on the one hand, the present invention provides a method for preparing polyacrylonitrile fiber, comprising the following steps:
[0006] The polyacrylonitrile solution is transferred to a spinning device through a conveying pipeline for spinning, and then spinning is performed to obtain polyacrylonitrile fibers;
[0007] Wherein, the conveying pipeline comprises an inner tube, a first sleeve and a second sleeve; the first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve;
[0008] Wherein, the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the heat preservation medium respectively.
[0009] Further, the temperature of the heat preservation medium in the inner tube is 20-70°C; the temperature of the heat preservation medium in the second casing is 20-70°C;
[0010] Preferably, the temperature difference between the heat preservation medium in the inner tube and the second sleeve is less than 5°C.
[0011] Furthermore, the polyacrylonitrile solution is transferred to a metering pump through a delivery pipeline by a booster pump for metering to obtain a spinning solution, and then the spinning solution is transferred to a spinning device;
[0012] Wherein, the delivery pipeline includes a first pipeline and a second pipeline;
[0013] The first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump;
[0014] The head end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0015] The temperature Q1 of the heat preservation medium in the inner tube of the first pipeline and the second casing is 40-70°C; the temperature Q2 of the heat preservation medium in the inner tube of the second pipeline and the second casing is 20-60°C.
[0016] Further, spinning is performed by a wet spinning process or a dry-jet wet spinning process;
[0017] Wherein, the wet spinning and dry-jet wet spinning both include coagulation forming treatment, water washing treatment, hot water drawing treatment, oiling treatment, drying densification treatment and steam drawing treatment in sequence;
[0018] Preferably, during the coagulation forming process, the stretching multiple applied to the fiber is K1; during the hot water stretching process, the stretching multiple applied to the fiber is K2; during the steam stretching process, the stretching multiple applied to the fiber is K3; wherein, K1:K2:K3=1:0.6-1.0:1.0-2.0.
[0019] Furthermore, when wet spinning is adopted, Q2 is 40-60°C, and Q1≤Q2≤the coagulation bath temperature during coagulation forming;
[0020] When dry-jet wet spinning is adopted, Q2 is 20-40°C and Q2≤Q1.
[0021] Furthermore, when wet spinning is adopted, Q2-Q1≤35°C;
[0022] When dry-jet wet spinning is used, Q1-Q2≤35℃.
[0023] Furthermore, the first pipe is arranged at an angle, and the end of the first pipe is inclined upward by 1-10 degrees.
[0024] Furthermore, the solid content of the polyacrylonitrile solution is 18-25wt%; and / or
[0025] The falling ball viscosity H1 of the polyacrylonitrile solution at 40°C is 60-110 Pa.s; and / or
[0026] The falling ball viscosity H2 of the spinning solution is 70-120 Pa.s, and the CV value is ≤0.5%;
[0027] Preferably, H2-H1 or H1-H2≤10Pa.s.
[0028] Furthermore, the inner wall surface of the first sleeve is a polished surface with a roughness of ≤Ra0.1; and / or
[0029] The first sleeve is made of stainless steel; and / or
[0030] The heat-insulating medium is water, and preferably, the heat-insulating medium is desalted water.
[0031] On the other hand, the present invention provides a polyacrylonitrile fiber, wherein the monofilament diameter of the polyacrylonitrile fiber is 8-12 μm; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the linear density of the polyacrylonitrile fiber are both ≤0.5%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the oiling rate of the polyacrylonitrile fiber are both ≤1.0%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the tensile strength, elastic modulus and elongation of the polyacrylonitrile fiber are both ≤1.5%;
[0032] Preferably, the polyacrylonitrile fiber is obtained by any of the preparation methods described above.
[0033] The polyacrylonitrile fiber and the preparation method thereof provided by the present invention have the following beneficial effects:
[0034] 1. The present invention transmits a polyacrylonitrile solution to a spinning device through a conveying pipeline for spinning, and then performs spinning to obtain polyacrylonitrile fibers; wherein the conveying pipeline includes an inner tube, a first sleeve and a second sleeve; the first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; wherein the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are respectively used to store a heat preservation medium; through the above design, the temperature difference between the core and the outside of the polyacrylonitrile solution (i.e., the polyacrylonitrile solution close to the inner wall of the conveying pipeline and the polyacrylonitrile solution close to the core of the conveying pipeline) is reduced, thereby ensuring that the viscosity of the polyacrylonitrile solution is uniform.
[0035] 2. Furthermore, the present invention sets two-stage conveying temperature to match the spinning process, which is beneficial to continuous and stable spinning; specifically, the temperature Q1 of the insulation medium after the booster pump and before the metering pump (i.e., the first-stage conveying temperature) is set to 40-70°C to improve the fluidity of the polyacrylonitrile solution and ensure that there is no lumps and gels during the conveying process; the temperature Q2 of the insulation medium after the metering pump and before spinning (i.e., the second-stage conveying temperature) is set to 20-60°C to improve the spinnability of the spinning solution and ensure that the spinning process is stable and continuous.
[0036] 3. Furthermore, the present invention controls the feed temperature (i.e., the delivery temperature Q1 and Q2) to perform secondary concentration adjustment on the polyacrylonitrile solution (i.e., adjust the viscosity of the polyacrylonitrile solution), thereby improving the spinnability of the spinning solution and its compatibility with the spinning process, and preparing high-quality polyacrylonitrile fibers and polyacrylonitrile-based carbon fibers; specifically, the polyacrylonitrile solution after polymerization has a certain viscosity, and then the spinnable viscosity or the required viscosity H1 for producing a certain specification of raw silk (polyacrylonitrile fiber) is reached through stripping and concentration, and then the viscosity is fine-tuned for a secondary time by controlling the feed temperature, so that the obtained spinning solution viscosity H2 satisfies H2-H1 or H1-H2≤10Pa.s, thereby improving the spinnability and compatibility with the spinning process, and preparing high-quality polyacrylonitrile fibers and polyacrylonitrile-based carbon fibers. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. The drawings described below are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.
[0038] Figure 1 is a schematic diagram of the delivery pipeline in this application;
[0039] Figure 2 is an end view of the polyacrylonitrile fiber prepared in Example 1 of the present invention;
[0040] Figure 3 This is the pipe blocking condition of the polyacrylonitrile solution in Comparative Example 1 of the present invention;
[0041] Figure 4 is an end view of the polyacrylonitrile fiber prepared in Comparative Example 2 of the present invention;
[0042] The accompanying drawings are marked as: 1-inner tube, 2-first sleeve, 3-second sleeve. DETAILED DESCRIPTION
[0043] In order to more clearly illustrate the implementation methods of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for the implementation methods or the description of the prior art. The drawings described below are only exemplary, and for ordinary technicians in this field, other implementation drawings can be derived from the provided drawings without creative work.
[0044] The present invention improves the uniformity of the spinning solution in the entire feeding process through a double-tube delivery pipeline, and adjusts the viscosity of the polyacrylonitrile solution for a second time by adjusting the feeding temperature, thereby improving the spinnability, continuity and stability of the polyacrylonitrile solution, and finally preparing polyacrylonitrile fibers with excellent performance and high production and quality control stability. The specific scheme is as follows:
[0045] In one aspect, the present invention provides a method for preparing polyacrylonitrile fiber, comprising the following steps:
[0046] The polyacrylonitrile solution is transferred to a spinning device through a conveying pipeline for spinning, and then spinning is performed to obtain polyacrylonitrile fibers;
[0047] Wherein, the conveying pipeline comprises an inner pipe, a first sleeve and a second sleeve; the first sleeve is sleeved on the outside of the inner pipe; the second sleeve is sleeved on the outside of the first sleeve;
[0048] Among them, the first sleeve is used to transmit polyacrylonitrile solution; the inner tube and the second sleeve are used to store insulation medium respectively; the temperature of the insulation medium in the inner tube is 20-70℃; the temperature of the insulation medium in the second sleeve is 20-70℃; preferably, the temperature difference of the insulation medium in the inner tube and the second sleeve is less than 5℃, preferably the same; the insulation medium can be tap water or desalted water.
[0049] Based on the above-mentioned conveying pipeline, the temperature difference between the polyacrylonitrile solution near the inner wall of the conveying pipeline and the polyacrylonitrile solution near the core of the conveying pipeline can be reduced, thereby ensuring that the viscosity of the polyacrylonitrile solution is uniform.
[0050] In some embodiments, the polyacrylonitrile solution is transferred to a metering pump through a delivery pipeline by a booster pump for metering to obtain a spinning solution, and then the spinning solution is transferred to a spinning device; wherein the delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0051] Among them, the inner wall surface of the first sleeve is a polished surface with a roughness of ≤Ra0.1; the material of the first sleeve is stainless steel.
[0052] The polyacrylonitrile solution after polymerization, de-monomerization and degassing becomes viscous after being left naturally. By setting the temperature of the heat preservation medium in the inner tube of the first pipeline and the second sleeve (i.e., the temperature of the heat preservation medium after the booster pump and before the metering pump) Q1 to 40-70°C, the fluidity of the polyacrylonitrile solution can be improved to ensure that there is no agglomeration and gel during the transportation process; the temperature of the heat preservation medium in the inner tube of the second pipeline and the second sleeve (i.e., the temperature of the heat preservation medium after the metering pump and before the spinning) Q2 is set to 20-60°C to improve the spinnability of the spinning solution and ensure that the spinning process is stable and continuous; that is, if the temperature during the transmission process is too low, the polyacrylonitrile solution is prone to agglomeration and gel; if the temperature is too high, the polyacrylonitrile solution is prone to accelerate cross-linking and become viscous, and the spinnability will also deteriorate;
[0053] If Q1 is too low, the viscosity of the polyacrylonitrile solution is high and the fluidity is poor; if it is too high, it is easy to cause the residual initiator to decompose, and the polyacrylonitrile solution is prone to generate bubbles and cause wire breakage;
[0054] In addition, the present invention adjusts the viscosity of the polyacrylonitrile solution by controlling the feed temperature (i.e., the delivery temperature Q1 and Q2), thereby improving the spinnability of the spinning solution and its compatibility with the spinning process, and preparing high-quality polyacrylonitrile fibers and polyacrylonitrile-based carbon fibers; specifically, the polyacrylonitrile solution after polymerization has a certain viscosity, and then the spinnable viscosity or the required viscosity H1 for producing a certain specification of raw silk (polyacrylonitrile fiber) is reached through stripping and concentration, and then the viscosity is fine-tuned for a second time by controlling the feed temperature, so that the viscosity H2 of the obtained spinning solution satisfies H2-H1 or H1-H2≤10Pa.s, thereby improving the spinnability and compatibility with the spinning process, and preparing high-quality polyacrylonitrile fibers and polyacrylonitrile-based carbon fibers.
[0055] In some embodiments, the solid content of the polyacrylonitrile solution after polymerization, de-monomerization and degassing is 18-25 wt %, and the falling ball viscosity H1 of the polyacrylonitrile solution is 60-110 Pa.s at 40° C.
[0056] An online viscometer is set between the metering pump and the spinneret to regulate the feed temperatures Q1 and Q2 to adjust the viscosity of the spinning solution; specifically, when the detected viscosity H2 of the spinning solution is high, the feed temperatures Q1 and Q2 are increased; when the detected viscosity H2 of the spinning solution is low, the feed temperatures Q1 and Q2 are reduced.
[0057] In some embodiments, spinning is performed using a wet spinning process or a dry-jet wet spinning process;
[0058] Among them, wet spinning and dry-jet wet spinning both include coagulation and forming treatment, water washing treatment, hot water drawing treatment, oiling treatment, drying and densification treatment and steam drawing treatment in sequence;
[0059] Preferably, during the coagulation forming process, the drafting multiple applied to the fiber is K1; during the hot water drafting process, the drafting multiple applied to the fiber is K2; during the steam drafting process, the drafting multiple applied to the fiber is K3; wherein K1:K2:K3=1:0.6-1.0:1.0-2.0;
[0060] The spinning device in the above method includes a spinneret, the spinneret hole diameter is 0.05-0.12mm, and the viscosity of the polyacrylonitrile solution, the spinneret hole diameter, and the stretching multiples applied to the fiber during coagulation, hot water stretching treatment, and steam stretching treatment affect the single filament diameter of the polyacrylonitrile fiber.
[0061] In some embodiments, when wet spinning is used, Q2 is 40-60° C., and Q1≤Q2≤the temperature of the coagulation bath during coagulation forming;
[0062] When dry-jet wet spinning is adopted, Q2 is 20-40°C and Q2≤Q1.
[0063] Furthermore, when wet spinning is adopted, Q2-Q1≤35°C;
[0064] When dry-jet wet spinning is used, Q1-Q2≤35℃. During spinning, if the temperature difference between Q1 and Q2 is too large, gel or uneven material temperature may occur easily. Among them, during wet spinning, Q1≤Q2≤. The setting of the gradient temperature rise of the coagulation bath during coagulation is to ensure heating uniformity and reduce the difference between the coagulation of the fiber surface and the core during the coagulation process. In dry-jet wet spinning, the viscosity of the polyacrylonitrile solution is generally high and the feed pipeline is long. If Q1<Q2, gel blocks are easily generated during the conveying process. Q1 is set higher to improve the fluidity of the polyacrylonitrile solution and avoid the generation of gel blocks. Q2 is set at a low temperature to improve spinnability. In dry-jet wet spinning, the spinning speed is generally faster and passes through a 2-5mm air section. The Q2 temperature is low, which is conducive to the continuous stability of spinning. However, too low a temperature may also easily lead to interruption of the spinning process or the generation of blocks.
[0065] In some embodiments, the first pipe is inclined, and the end of the first pipe is inclined upward by 1-10 degrees. The inclined setting of the first pipe can avoid the generation of bubbles in the polyacrylonitrile solution in the conveying pipe, further ensure the spinning stability, and prepare polyacrylonitrile fibers with excellent performance.
[0066] On the other hand, the present invention provides a polyacrylonitrile fiber, wherein the monofilament diameter of the polyacrylonitrile fiber is 8-12 μm; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the linear density of the polyacrylonitrile fiber are both ≤0.5%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the oiling rate of the polyacrylonitrile fiber are both ≤1.0%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the tensile strength, elastic modulus and elongation of the polyacrylonitrile fiber are both ≤1.5%; wherein the dispersion coefficient is the CV value, the ratio of the standard deviation to the mean; between batches refers to between different production batches, and within batch refers to between different spinning positions in the production process of the same batch and the same spinning position over a long distance;
[0067] Preferably, the polyacrylonitrile fiber is obtained by any of the above preparation methods.
[0068] The present invention is further described below with reference to specific embodiments and comparative examples.
[0069] It should be noted that the following embodiments and comparative examples are described by taking dry-jet wet spinning as an example.
[0070] Example 1
[0071] This embodiment provides a method for preparing T800S-12K polyacrylonitrile fiber, which specifically includes the following steps:
[0072] Under the action of the booster pump, the polyacrylonitrile solution after polymerization, de-singling and degassing is filtered and metered by a metering pump through a conveying pipeline to obtain a spinning solution; the spinning solution is then conveyed to the spinneret and sprayed out through a spinneret to form a thin stream of the solution, which is then subjected to coagulation forming, water washing, hot water drawing, oiling, drying and densification, and steam drawing in sequence, and finally rolled up to obtain polyacrylonitrile fibers.
[0073] The conveying pipeline includes an inner pipe 1, a first casing pipe 2 and a second casing pipe 3. Figure 1 ; The first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the insulation water respectively;
[0074] The delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0075] The solid content of the polyacrylonitrile solution after polymerization, stripping and degassing is 20wt%, and the falling ball viscosity H1 of the polyacrylonitrile solution is 110Pa.s at 40°C; the falling ball viscosity H2 of the spinning solution is 118Pa.s, and the CV value is 0.2%; the roughness of the inner wall of the first sleeve in the conveying pipeline is Ra0.1, and the first pipeline is inclined upward by 5° from the head end to the end;
[0076] The temperature Q1 of the insulation water after the booster pump and before the metering pump is 55°C, and the temperature Q2 of the insulation water after the metering pump and before spinnereting is 20°C; during coagulation forming, the temperature of the coagulation bath area is 20°C, and the humidity of the coagulation bath area is 60%; the aperture of the spinneret is 0.12mm, and the stretching multiples applied to the fiber during coagulation forming, hot water stretching treatment, and steam stretching treatment are 3.0, 2.5, and 4.5, respectively.
[0077] The end view of the polyacrylonitrile fiber prepared in this embodiment is as follows Figure 1 As shown, it can be seen that the end surface is smooth; the monofilament diameter of the prepared polyacrylonitrile fiber is 10 μm, the linear density CV value is 0.5%, the tensile strength CV value is 1%, the elastic modulus CV value is 1.2%, and the elongation CV value is 1%.
[0078] Example 2
[0079] This embodiment provides a method for preparing T800S-12K polyacrylonitrile fiber, which specifically includes the following steps:
[0080] Under the action of the booster pump, the polyacrylonitrile solution after polymerization, de-singling and degassing is filtered and metered by a metering pump through a conveying pipeline to obtain a spinning solution; the spinning solution is then conveyed to the spinneret and sprayed out through a spinneret to form a thin stream of the solution, which is then subjected to coagulation forming, water washing, hot water drawing, oiling, drying and densification, and steam drawing in sequence, and finally rolled up to obtain polyacrylonitrile fibers.
[0081] The conveying pipeline includes an inner pipe, a first casing and a second casing, see Figure 1 ; The first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the insulation water respectively;
[0082] The delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0083] The solid content of the polyacrylonitrile solution after polymerization, de-monomerization and degassing is 23wt%, and the falling ball viscosity H1 of the polyacrylonitrile solution is 110Pa.s at 40°C; the falling ball viscosity H2 of the spinning solution is 110Pa.s, and the CV value is 0.2%; the roughness of the inner wall of the first sleeve in the conveying pipeline is Ra0.1, and the first pipeline is inclined upward by 10° from the head end to the end end;
[0084] The temperature Q1 of the insulation water after the booster pump and before the metering pump is 40°C, and the temperature Q2 of the insulation water after the metering pump and before spinneret is 40°C; during coagulation forming, the temperature of the coagulation bath area is 25°C, and the humidity of the coagulation bath area is 60%; the aperture of the spinneret is 0.12mm, and the stretching multiples applied to the fiber during coagulation forming, hot water stretching treatment, and steam stretching treatment are 3.0, 2.5, and 4.5, respectively.
[0085] The monofilament diameter of the polyacrylonitrile fiber prepared in this embodiment is 9 μm, the linear density CV value is 0.3%, and the tensile strength CV value is 0.8%.
[0086] Comparative Example 1
[0087] This comparative example provides a method for preparing T800S-12K polyacrylonitrile fiber, which specifically comprises the following steps:
[0088] Under the action of the booster pump, the polyacrylonitrile solution after polymerization, de-singling and degassing is filtered and metered by a metering pump through a conveying pipeline to obtain a spinning solution; the spinning solution is then conveyed to the spinneret and sprayed out through a spinneret to form a thin stream of the solution, which is then subjected to coagulation forming, water washing, hot water drawing, oiling, drying and densification, and steam drawing in sequence, and finally rolled up to obtain polyacrylonitrile fibers.
[0089] The conveying pipeline includes an inner pipe, a first casing and a second casing, see Figure 1 ; The first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the insulation water respectively;
[0090] The delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0091] The solid content of the polyacrylonitrile solution after polymerization, de-monomerization and degassing is 20wt%, and the falling ball viscosity H1 of the polyacrylonitrile solution is 110Pa.s at 40°C; the falling ball viscosity H2 of the spinning solution is 118Pa.s, and the CV value is 0.8%; the roughness of the inner wall of the first sleeve in the conveying pipeline is Ra0.8, and the first pipeline is arranged horizontally;
[0092] The temperature Q1 of the insulation water after the booster pump and before the metering pump is 55°C, and the temperature Q2 of the insulation water after the metering pump and before spinnereting is 20°C; during coagulation forming, the temperature of the coagulation bath area is 20°C, and the humidity of the coagulation bath area is 60%; the aperture of the spinneret is 0.12mm, and the stretching multiples applied to the fiber during coagulation forming, hot water stretching treatment, and steam stretching treatment are 3.0, 2.5, and 4.5, respectively.
[0093] The linear density CV value of the polyacrylonitrile fiber prepared in this comparative example is 1.0%, and the tensile strength CV value is 1.5%. Due to the large roughness of the inner wall of the first sleeve in the conveying pipeline, the pipeline is prone to material hanging during feeding, and the flow is easily interrupted, strands are broken, and gel is easily generated during the spinning process. Figure 3 As shown, a large amount of gel is formed; the first pipeline is laid horizontally, and bubbles are likely to exist in the first pipeline, which leads to flow interruption and strand breakage during the spinning process, unstable spinning position production operation, and intermittent yarn breakage and roller winding problems, resulting in higher linear density CV value and tensile strength CV value of the polyacrylonitrile fiber prepared in this comparative example.
[0094] Comparative Example 2
[0095] This comparative example provides a method for preparing T800S-12K polyacrylonitrile fiber, which specifically comprises the following steps:
[0096] Under the action of the booster pump, the polyacrylonitrile solution after polymerization, de-singling and degassing is filtered and metered by a metering pump through a conveying pipeline to obtain a spinning solution; the spinning solution is then conveyed to the spinneret and sprayed out through a spinneret to form a thin stream of the solution, which is then subjected to coagulation forming, water washing, hot water drawing, oiling, drying and densification, and steam drawing in sequence, and finally rolled up to obtain polyacrylonitrile fibers.
[0097] The conveying pipeline includes an inner pipe, a first casing and a second casing, see Figure 1 ; The first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the insulation water respectively;
[0098] The delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0099] The solid content of the polyacrylonitrile solution after polymerization, de-monomerization and degassing is 20wt%, and the falling ball viscosity H1 of the polyacrylonitrile solution is 110Pa.s at 40°C; the falling ball viscosity H2 of the spinning solution is 125Pa.s, and the CV value is 0.2%; the roughness of the inner wall of the first sleeve in the conveying pipeline is Ra0.1, and the head end to the tail end is inclined upward by 5°;
[0100] The temperature Q1 of the insulation water after the booster pump and before the metering pump is 30°C, and the temperature Q2 of the insulation water after the metering pump and before spinneret is 30°C; during coagulation forming, the temperature of the coagulation bath area is 20°C, and the humidity of the coagulation bath area is 60%; the aperture of the spinneret is 0.12mm, and the stretching multiples applied to the fiber during coagulation forming, hot water stretching treatment, and steam stretching treatment are 3.0, 2.5, and 4.5, respectively.
[0101] The linear density CV value of the polyacrylonitrile fiber prepared in this comparative example is 3.5%, and the tensile strength CV value is 5%. Since the feed temperature Q1 is too low, the viscosity of the polyacrylonitrile solution increases, the fluidity is poor during transportation, and gel is easily generated in the transportation pipeline, resulting in more material blocks during the spinning process, resulting in unstable spinning production and easy wire breakage and roller winding, resulting in higher linear density CV value and tensile strength CV value of the polyacrylonitrile fiber prepared in this comparative example.
[0102] Comparative Example 3
[0103] This comparative example provides a method for preparing T800S-12K polyacrylonitrile fiber, which specifically comprises the following steps:
[0104] Under the action of the booster pump, the polyacrylonitrile solution after polymerization, de-singling and degassing is filtered and metered by a metering pump through a conveying pipeline to obtain a spinning solution; the spinning solution is then conveyed to the spinneret and sprayed out through a spinneret to form a thin stream of the solution, which is then subjected to coagulation forming, water washing, hot water drawing, oiling, drying and densification, and steam drawing in sequence, and finally rolled up to obtain polyacrylonitrile fibers.
[0105] The conveying pipeline includes an inner pipe, a first casing and a second casing, see Figure 1 ; The first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the insulation water respectively;
[0106] The delivery pipeline includes a first pipeline and a second pipeline; the first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; the first end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device;
[0107] The solid content of the polyacrylonitrile solution after polymerization, de-monomerization and degassing is 20wt%, and the falling ball viscosity H1 of the polyacrylonitrile solution is 110Pa.s at 40°C; the falling ball viscosity H2 of the spinning solution is 118Pa.s, and the CV value is 0.2%; the roughness of the inner wall of the first sleeve in the conveying pipeline is Ra0.1, and the head end to the tail end is inclined upward by 5°;
[0108] The temperature Q1 of the insulation water after the booster pump and before the metering pump is 55°C, and the temperature Q2 of the insulation water after the metering pump and before spinnereting is 20°C; during coagulation forming, the temperature of the coagulation bath area is 20°C, and the humidity of the coagulation bath area is 60%; the aperture of the spinneret is 0.12mm, and the stretching multiples applied to the fiber during coagulation forming, hot water stretching treatment, and steam stretching treatment are 3.0, 4.0, and 2.8, respectively.
[0109] The monofilament diameter of the polyacrylonitrile fiber prepared in this comparative example is 10 μm, the linear density CV value is 3.5%, and the tensile strength CV value is 4.2%. The viscosity, spinneret aperture, and product of the draw multiples (i.e., the total draw multiple, which is the product of the draw multiples applied to the fiber in the steps of coagulation, washing, hot water drawing, oiling, drying and densification, and steam drawing) of the polyacrylonitrile solution in this comparative example are the same as those in Example 1, so the monofilament diameter of the obtained polyacrylonitrile fiber is 10 μm. However, the ratio of the draw multiples applied to the fiber in the coagulation, hot water drawing, and steam drawing does not match the viscosity of the polyacrylonitrile solution, i.e., the ratio of the draw multiples applied to the fiber in the coagulation, hot water drawing, and steam drawing does not satisfy 1:0.6-1.0:1.0-2.0. The draw multiple applied to the fiber in the hot water drawing is too large, which makes it easy to damage and fluff the filament bundle during spinning. Figure 4 As shown, the polyacrylonitrile fiber has many hairy ends, resulting in unstable production operation and frequent roller entanglement at the hot water drawing point. The polyacrylonitrile fiber has many hairy ends and broken strands, resulting in higher linear density CV values and tensile strength CV values of the polyacrylonitrile fiber prepared in this comparative example.
[0110] The specific comparison of the performance of the polyacrylonitrile fibers prepared in the examples of the present invention and the comparative examples is shown in the following table:
[0111]
[0112] It is easy for those skilled in the art to understand that, without conflict, the advantageous technical features of the above-mentioned methods can be freely combined and superimposed.
[0113] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principle of the present invention shall be included in the protection scope of the present invention. The above description is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and variations can be made without departing from the technical principles of the present invention. These improvements and variations should also be regarded as the protection scope of the present invention.
Claims
1. A method for preparing polyacrylonitrile fiber, characterized in that: The following steps are involved: The polyacrylonitrile solution is transferred to a spinning device through a conveying pipeline for spinning, and then spinning is performed to obtain polyacrylonitrile fibers; Wherein, the conveying pipeline comprises an inner tube, a first sleeve and a second sleeve; the first sleeve is sleeved on the outside of the inner tube; the second sleeve is sleeved on the outside of the first sleeve; Wherein, the first sleeve is used to transmit the polyacrylonitrile solution; the inner tube and the second sleeve are used to store the heat preservation medium respectively.
2. The method for preparing polyacrylonitrile fiber according to claim 1, characterized in that: The temperature of the heat preservation medium in the inner tube is 20-70°C; the temperature of the heat preservation medium in the second casing is 20-70°C; Preferably, the temperature difference between the heat preservation medium in the inner tube and the second sleeve is less than 5°C.
3. The method for preparing polyacrylonitrile fiber according to claim 1 or 2, characterized in that: The polyacrylonitrile solution is transferred to a metering pump through a conveying pipeline by a booster pump for metering to obtain a spinning solution, and then the spinning solution is transferred to a spinning device; Wherein, the delivery pipeline includes a first pipeline and a second pipeline; The first end of the first pipeline is connected to the booster pump, and the end of the first pipeline is connected to the metering pump; The head end of the second pipeline is connected to the metering pump, and the end of the second pipeline is connected to the spinning device; The temperature Q1 of the heat preservation medium in the inner tube of the first pipeline and the second casing is 40-70°C; the temperature Q2 of the heat preservation medium in the inner tube of the second pipeline and the second casing is 20-60°C.
4. The method for preparing polyacrylonitrile fiber according to claim 3, characterized in that: Spinning is performed by a wet spinning process or a dry-jet wet spinning process; Wherein, the wet spinning and dry-jet wet spinning both include coagulation forming treatment, water washing treatment, hot water drawing treatment, oiling treatment, drying densification treatment and steam drawing treatment in sequence; Preferably, during the coagulation forming process, the stretching multiple applied to the fiber is K1; during the hot water stretching process, the stretching multiple applied to the fiber is K2; during the steam stretching process, the stretching multiple applied to the fiber is K3; wherein, K1:K2:K3=1:0.6-1.0:1.0-2.
0.
5. The method for preparing polyacrylonitrile fiber according to claim 4, characterized in that: When wet spinning is adopted, Q2 is 40-60°C, and Q1≤Q2≤the coagulation bath temperature during coagulation forming; When dry-jet wet spinning is adopted, Q2 is 20-40°C and Q2≤Q1.
6. The method for preparing polyacrylonitrile fiber according to claim 5, characterized in that: When wet spinning is used, Q2-Q1≤35℃; When dry-jet wet spinning is used, Q1-Q2≤35℃.
7. The method for preparing polyacrylonitrile fiber according to any one of claims 3 to 6, characterized in that: The first pipeline is arranged obliquely, and the end of the first pipeline is inclined upward by 1-10 degrees.
8. The method for preparing polyacrylonitrile fiber according to claim 3, characterized in that: The solid content of the polyacrylonitrile solution is 18-25wt%; and / or The falling ball viscosity H1 of the polyacrylonitrile solution at 40°C is 60-110 Pa.s; and / or The falling ball viscosity H2 of the spinning solution is 70-120 Pa.s, and the CV value is ≤0.5%; Preferably, H2-H1 or H1-H2≤10Pa.s.
9. The method for preparing polyacrylonitrile fiber according to claim 1, characterized in that: The inner wall surface of the first sleeve is a polished surface with a roughness of ≤Ra0.1; and / or The first sleeve is made of stainless steel; and / or The heat-insulating medium is water; preferably, the heat-insulating medium is desalted water.
10. A polyacrylonitrile fiber, characterized in that: The monofilament diameter of the polyacrylonitrile fiber is 8-12 μm; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the linear density of the polyacrylonitrile fiber are both ≤0.5%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the oiling rate of the polyacrylonitrile fiber are both ≤1.0%; the batch-to-batch dispersion coefficient and the batch-to-batch dispersion coefficient of the tensile strength, elastic modulus and elongation of the polyacrylonitrile fiber are both ≤1.5%; Preferably, the polyacrylonitrile fiber is obtained by the preparation method according to any one of claims 1 to 9.
Citation Information
Patent Citations
Method for precursor fiber curing molding during ultrahigh-molecular-weight polyethylene dry spinning
CN104911722A
Production line and production method of high-cleanliness fine-denier chinlon 6 filaments
CN107435170A
Novel heat insulation spinneret plate and spinning component thereof
CN203065652U
Heat preservation pipeline
CN205919065U
Pipeline insulation construction
CN205938347U