Mosquito sticking glue and preparation process thereof
By using the formulation and preparation process of thermoplastic elastomers, hydrogenated petroleum resins and other materials, the problems of insufficient viscosity and poor durability of mosquito adhesives are solved, and efficient, stable and environmentally friendly mosquito-killing effects are achieved, and production costs are reduced. In various places.
Patent Information
- Application Number
- CN202411362018.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-27
- Publication Date
- 2024-11-15
AI Technical Summary
The existing mosquito-sticky adhesives have insufficient viscosity, poor durability, may cause pollution to the environment, and have high production costs, which limits their wide application.
The formula consists of thermoplastic elastomers, hydrogenated petroleum resins, hydrogenated rosin, cycloane oil, paraffin base oil, antioxidants and UV absorbers, and mix and mold through specific preparation processes to form a strong viscosity and stability of glue.
It has achieved significant mosquito-killing effects, stable performance, reduced production costs, and is convenient and environmentally friendly to use, free of harmful chemicals, and is suitable for a variety of places and reduces environmental pollution.
Smart Images

Figure CN118956340A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of adhesives, in particular to an adhesive for sticking mosquitoes and insects and a preparation process thereof. Background Art
[0002] As living standards continue to improve, people's requirements for the quality of their living environment are also getting higher and higher. Mosquitoes, as common pests, not only bite the human body, causing itching and discomfort, but also may spread various diseases, posing a threat to people's health.
[0003] At present, the common mosquito killing methods on the market include mosquito coils, electric mosquito swatters, insecticides, etc. However, these methods have some shortcomings. Mosquito coils and insecticides may have a certain impact on human health, and electric mosquito swatters are not convenient to use. Therefore, a safer, more convenient and effective mosquito killing method is needed.
[0004] As a new type of mosquito-killing product, mosquito-sticking glue has the following advantages: safe and environmentally friendly, no harm to human health; easy to use, just place the glue in places where mosquitoes are present; effective, can effectively stick to mosquitoes and prevent them from escaping. It can be placed in bedrooms, living rooms, kitchens and other places to effectively catch mosquitoes, flies and other pests, especially in summer, to provide a mosquito-free and comfortable space for the family. Or placed in office places, it can reduce the interference of mosquitoes on employees' work and improve work efficiency.
[0005] There are some disadvantages of the current mosquito repellent glues on the market, such as insufficient viscosity, which makes it easy for mosquitoes to escape; poor durability, which reduces the viscosity after a period of use; and possible pollution to the environment. In addition, the production cost of some mosquito repellent glues is high, which limits their wide application.
[0006] Therefore, it is necessary to propose an improved technical solution to solve the above problems. Summary of the invention
[0007] In order to overcome the above-mentioned shortcomings, the present invention aims to provide a technical solution that can solve the above-mentioned problems.
[0008] A mosquito-repellent glue, comprising the following components in percentage by weight: Thermoplastic elastomer 1-10%; Hydrogenated petroleum resin 25-35%; Hydrogenated rosin 5-15%; Naphthenic oil 30-40%; Paraffin base oil 10-20%; Antioxidant 0.4%; UV absorber 0.2%.
[0009] As a further solution of the present invention: the thermoplastic elastomer includes thermoplastic elastomer A and thermoplastic elastomer B; The thermoplastic elastomer A is rubber SIS, and its weight percentage is 1-5%; The thermoplastic elastomer B is rubber SEBS, and its weight percentage is 1-5%.
[0010] As a further embodiment of the present invention: the antioxidant includes antioxidant 168 and antioxidant 1010, wherein: The weight percentage of the antioxidant 168 is 0.2%; The weight percentage of the antioxidant 1010 is 0.2%.
[0011] As a further solution of the present invention: According to the above-mentioned mosquito glue, its preparation process includes the following steps: Step 1: Raw material preparation: The raw materials are configured according to the formula ratio and production volume, including rubber SIS, rubber SEBS, hydrogenated petroleum resin, hydrogenated rosin, naphthenic oil, paraffin-based oil, antioxidant 168, antioxidant 1010 and ultraviolet light absorber; Step 2: Add oxidant and part of naphthenic oil and heat: Add antioxidant 168, antioxidant 1010, and 40% naphthenic oil into the reactor and heat the material temperature to 120 degrees; Step 3: Add rubber and melt: Add rubber SIS and rubber SEBS and wait for the rubber to be completely melted; Step 4: Add hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, remaining naphthenic oil and ultraviolet light absorber: After the rubber is melted, hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, the remaining 60% of naphthenic oil, and ultraviolet light absorber are added successively; Step 5: Vacuum and stir: Perform vacuum operation and continue stirring for 40-50 minutes; Step 6: Discharging and forming: After stirring, discharge the material at a temperature between 135-145 degrees; Step 7: Cooling and packaging: Cool naturally to form a rubber block, and pack it when the temperature of the rubber block drops below 40 degrees.
[0012] Compared with the prior art, the present invention has the following beneficial effects: 1) Significant mosquito killing effect: The strong stickiness can quickly stick to mosquitoes and prevent them from escaping, and has a good capture effect on various pests; it can be placed in a variety of places and is widely used in different environments such as homes and offices, providing people with a comfortable mosquito-free space and reducing the interference of mosquitoes on work; 2) Stable and reliable performance: Antioxidants and UV absorbers can prevent the adhesive from being oxidized and damaged by UV rays, thus extending its service life; good temperature adaptability enables the adhesive to maintain appropriate hardness and viscosity at different temperatures; a uniform bonding system ensures uniform viscosity during use, thus stably exerting its mosquito-killing effect; 3) Obvious cost advantage: some materials in the formula are relatively low in cost, such as cyclohexane oil and paraffin-based oil, which reduces production costs; the production process is simple, which improves production efficiency and further reduces costs; 4) Convenient and environmentally friendly: It is easy to use and only needs to be placed in places where mosquitoes are present; it is easy to replace and the replaced adhesive can be recycled without polluting the environment; it is safe and environmentally friendly, does not contain harmful chemicals, and has no harm to human health.
[0013] Additional aspects and advantages of the present invention will be given in part in the following description and in part will be obvious from the following description, or will be learned through practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0015] Figure 1 It is a schematic diagram of the process flow of the present invention. DETAILED DESCRIPTION
[0016] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0017] In an embodiment of the present invention, a mosquito-repellent glue is composed of the following components in percentage by weight: Thermoplastic elastomer 1-10%; Hydrogenated petroleum resin 25-35%; Hydrogenated rosin 5-15%; Naphthenic oil 30-40%; Paraffin base oil 10-20%; Antioxidant 0.4%; UV absorber 0.2%.
[0018] In the embodiment of the present invention, the thermoplastic elastomer includes thermoplastic elastomer A and thermoplastic elastomer B; The thermoplastic elastomer A is rubber SIS, and its weight percentage is 1-5%; The thermoplastic elastomer B is rubber SEBS, and its weight percentage is 1-5%.
[0019] In the embodiment of the present invention, the antioxidant includes antioxidant 168 and antioxidant 1010, wherein: The weight percentage of the antioxidant 168 is 0.2%; The weight percentage of the antioxidant 1010 is 0.2%.
[0020] In the embodiment of the present invention, please refer to Figure 1 According to the above mosquito glue, its preparation process includes the following steps: (step S10-step S70) Step 1: Raw material preparation: The raw materials are configured according to the formula ratio and production volume, including rubber SIS, rubber SEBS, hydrogenated petroleum resin, hydrogenated rosin, naphthenic oil, paraffin-based oil, antioxidant 168, antioxidant 1010 and ultraviolet light absorber; Step 2: Add oxidant and part of naphthenic oil and heat: Add antioxidant 168, antioxidant 1010, and 40% naphthenic oil into the reactor and heat the material temperature to 120 degrees; Step 3: Add rubber and melt: Add rubber SIS and rubber SEBS and wait for the rubber to be completely melted; Step 4: Add hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, remaining naphthenic oil and ultraviolet light absorber: After the rubber is melted, hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, the remaining 60% of naphthenic oil, and ultraviolet light absorber are added successively; Step 5: Vacuum and stir: Perform vacuum operation and continue stirring for 40-50 minutes; Step 6: Discharging and forming: After stirring, discharge the material at a temperature between 135-145 degrees; Step 7: Cooling and packaging: Cool naturally to form a rubber block, and pack it when the temperature of the rubber block drops below 40 degrees.
[0021] In the technical solution of the present invention: 1. Material characteristics: Thermoplastic elastomers: Thermoplastic elastomer A (rubber SIS) and thermoplastic elastomer B (rubber SEBS) have unique characteristics in molecular structure. They are composed of hard segments and soft segments. The hard segments provide physical crosslinking points, giving the material a certain strength and stability; the soft segments give the material high elasticity and flexibility. Within a certain temperature range, the movement of the soft segments allows the material to remain soft and sticky, providing basic adhesion properties for the adhesive; at the same time, the thermoplasticity of thermoplastic elastomers allows them to melt when heated, making them easy to mix with other ingredients and process into shapes; Hydrogenated petroleum resin and hydrogenated rosin: Hydrogenated petroleum resin is a resin obtained by hydrogenation of petroleum fractions. It has a high molecular weight and viscosity. It can interact with thermoplastic elastomers to form a stable bonding system and increase the bonding strength and cohesion of the adhesive. Hydrogenated rosin is a hydrogenated rosin with better stability and oxidation resistance. It can further improve the viscosity and flexibility of the adhesive, so that it can have a good adhesion effect on different surfaces. Naphthenic oil and paraffin-based oil: Naphthenic oil is a mineral oil composed of cycloalkanes, which has good solubility and stability. It can make other components disperse better in the system, and can also adjust the hardness and flexibility of the adhesive. Paraffin-based oil is a mineral oil composed of paraffin hydrocarbons, which has a high melting point and good low-temperature resistance. It can improve the low-temperature resistance of the adhesive and enable it to maintain good viscosity at lower temperatures. Antioxidants and UV absorbers: Antioxidant 168 and Antioxidant 1010 are two commonly used antioxidants. They can capture free radicals and prevent the adhesive from being oxidized during storage and use; UV absorbers can absorb ultraviolet rays, reduce the damage of ultraviolet rays to the adhesive, and maintain the stable performance of the adhesive.
[0022] (II) Preparation process: First, add part of the naphthenic oil and antioxidant and heat to 120 degrees. This is because at this temperature, the antioxidant can fully play its role and prevent other components from being oxidized during the heating process. At the same time, part of the naphthenic oil can provide a good dissolving environment for the antioxidant, so that it can be evenly dispersed in the system; then add rubber SIS and rubber SEBS to fully melt in the naphthenic oil. The melting of rubber requires a certain temperature and time. The temperature of 120 degrees can make the rubber melt quickly without causing adverse effects on other components; then add hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, remaining naphthenic oil and ultraviolet light absorber in turn. This order of addition is determined based on the properties and functions of each component. Hydrogenated rosin and hydrogenated petroleum resin need to be added after the rubber is melted so as to be fully mixed with the rubber to form a stable bonding system. Paraffin-based oil and remaining naphthenic oil can be added later to adjust the hardness and flexibility of the adhesive. The ultraviolet light absorber is added last to avoid being damaged in the previous processing process; During the stirring process, vacuuming can remove bubbles in the adhesive. The presence of bubbles will reduce the quality and stability of the adhesive, affect its viscosity and mosquito-killing effect. Vacuuming can put the adhesive in a negative pressure state during the stirring process, and the bubbles escape under the action of pressure, thereby improving the quality and stability of the adhesive. At the same time, stirring can make the various components more evenly mixed to form a uniform bonding system. The stirring speed and time need to be adjusted according to the specific situation to ensure that the various components can be fully mixed and achieve the best performance state. During the discharging and molding stage, the material temperature is controlled between 135 and 145 degrees. This is because within this temperature range, the fluidity and molding performance of the adhesive are optimal. If the temperature is too high, the adhesive may decompose or deteriorate; if the temperature is too low, the fluidity of the adhesive will deteriorate and it will be difficult to mold; the stirring time is 40 to 50 minutes, which allows the components to fully react and mix to achieve the best performance state. If the stirring time is too short, the components may not be fully mixed; if the stirring time is too long, it may waste energy and time, and may also have an adverse effect on the performance of the adhesive; natural cooling can allow the adhesive to gradually solidify during the cooling process to form a stable structure. The speed of natural cooling needs to be properly controlled to avoid problems such as shrinkage or deformation of the adhesive during the cooling process; In the packaging process, it can be produced into 5kg, 1kg, 0.5kg and other pieces according to product specifications.
[0023] 3. Deep synergy of material properties and fine optimization of preparation processes: The high viscosity of the mosquito-repellent glue mainly comes from the synergistic effect of hydrogenated petroleum resin, hydrogenated rosin and thermoplastic elastomer. Hydrogenated petroleum resin and hydrogenated rosin have high molecular weight and viscosity, and can interact with thermoplastic elastomer to form a stable bonding system. This bonding system can quickly stick to mosquitoes and make them unable to escape. Compared with traditional mosquito killing methods, the glue has stronger viscosity and can effectively capture mosquitoes of various sizes, including mosquitoes, flies, moths, etc. The antioxidant and ultraviolet light absorber in the formula of the mosquito-repellent glue can effectively prevent the glue from being oxidized and damaged by ultraviolet light during storage and use, and keep its performance stable. This is because the antioxidant can capture free radicals and prevent the occurrence of oxidation reactions; the ultraviolet light absorber can absorb ultraviolet light and reduce the damage of ultraviolet light to the glue; the synergistic effect of these two ingredients can extend the service life of the glue, so that it can maintain good adhesion and mosquito-killing effect under different environmental conditions; The mosquito-repellent glue can be placed in various places because it has good stability and adaptability. Whether it is in indoor places such as homes, offices, hotels, restaurants, or outdoor places such as gardens, balconies, and courtyards, the glue can play a good mosquito-killing effect. It can be placed in different locations such as the ground, desktops, and windowsills, and can also be hung on walls, ceilings, and other high places to meet different usage requirements. In addition, the mosquito-repellent glue can also be adjusted according to different places and seasons. For example, the amount of glue can be increased in summer to improve the mosquito-killing effect; the amount of glue can be reduced in winter to avoid waste. The mosquito-repellent glue does not contain harmful chemicals, such as pesticides, mosquito coils, etc., and will not harm human health. At the same time, it will not produce smoke, odor and other factors that pollute the environment. It is a safe and environmentally friendly mosquito-killing product. Compared with traditional mosquito-killing methods, the glue is safer and more reliable, and is especially suitable for families with special groups such as the elderly, children, and pregnant women. The addition of cyclohexane oil and paraffin-based oil makes the adhesive have good low-temperature resistance and thermal stability. At different temperatures, the adhesive can maintain appropriate hardness and viscosity and will not lose its mosquito-killing function due to temperature changes; for example, at high temperatures in summer, the adhesive will not become soft and flow; at low temperatures in winter, the adhesive will not become hard and crack; this temperature adaptability allows the adhesive to be used in different seasons and regions and has a wide range of applicability, which allows the adhesive to be used throughout the year to meet people's mosquito-killing needs in different seasons; in addition, the types and numbers of mosquitoes in different seasons are also different, and the adhesive can be adjusted according to the characteristics of different seasons to improve the mosquito-killing effect; Through the optimized preparation process, all components can be fully mixed to form a uniform bonding system. This bonding system has good stability and consistency, and can maintain uniform viscosity and mosquito-killing effect during use, without the situation of insufficient or uneven local viscosity, thus ensuring the stability of the mosquito-killing effect of the adhesive. In addition, the uniform bonding system can also improve the quality and reliability of the adhesive, and reduce waste and losses caused by quality problems; The formula of this mosquito-repellent glue uses some relatively low-cost materials, such as cyclohexane oil, paraffin-based oil, etc. These materials are in sufficient supply in the market and are relatively low in price, which reduces the production cost of the glue; at the same time, the prices of thermoplastic elastomer A (rubber SIS) and thermoplastic elastomer B (rubber SEBS) are also relatively reasonable, and have certain cost advantages compared with other high-performance materials; in addition, the amount of antioxidant and ultraviolet light absorber used in the formula is relatively small, which will not have a significant impact on the cost; The optimized preparation process is simple and easy to implement, and does not require complicated equipment and technology, which makes the production process more efficient and reduces production costs. At the same time, the simple production process is also conducive to improving the quality stability and production efficiency of the product, and reducing the cost increase caused by mistakes and waste in the production process. In addition, the simple production process can also reduce the requirements for the production environment, reduce energy consumption and environmental pollution, and has good economic and social benefits. The mosquito-sticking glue is easy to use. It only needs to be placed in places where mosquitoes are present. When the viscosity of the glue decreases or it is covered with mosquitoes, it can be easily replaced without causing pollution to the environment. Compared with traditional mosquito-killing methods, the glue is more convenient and efficient, and does not require frequent replacement of batteries, addition of agents, and the like. At the same time, the replaced glue can be recycled and processed, without causing pollution to the environment, and meets environmental protection requirements. Specifically, the mosquito-sticking glue can be used as a mosquito-sticking sticker. The mosquito-sticking sticker uses high-quality paper as a substrate, and the mosquito-sticking glue of the present invention is evenly coated on its surface. The mosquito-sticking sticker can be designed into various cute shapes and patterns, such as flowers, animals, etc., which are both practical and decorative. At the same time, in order to facilitate user use, the mosquito-sticking sticker can be designed into different sizes to adapt to different usage scenarios. It is very simple to use the mosquito-sticking sticker. It only needs to be gently uncovered and then pasted in places where mosquitoes are present. For example, the mosquito-sticking sticker can be pasted on windows, door frames, walls, furniture, etc. The mosquito-sticking sticker has strong viscosity and can be firmly pasted on various surfaces without falling off easily. To sum up, the design principle of this mosquito repellent glue is scientific and reasonable. Through the deep synergy of material properties and the fine optimization of the preparation process, it achieves many beneficial effects such as efficient mosquito killing, stable performance, cost advantage and wide applicability. It provides people with a safer, more convenient and effective mosquito killing method, and has broad market prospects and application value.
[0024] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.
Claims
1. A mosquito-repellent glue, characterized in that: It is composed of the following components in weight percentage: Thermoplastic elastomer 1-10%; Hydrogenated petroleum resin 25-35%; Hydrogenated rosin 5-15%; Naphthenic oil 30-40%; Paraffin base oil 10-20%; Antioxidant 0.4%; UV absorber 0.2%.
2. The mosquito and insect glue according to claim 1, characterized in that: The thermoplastic elastomer includes thermoplastic elastomer A and thermoplastic elastomer B; The thermoplastic elastomer A is rubber SIS, and its weight percentage is 1-5%; The thermoplastic elastomer B is rubber SEBS, and its weight percentage is 1-5%.
3. The mosquito and insect glue according to claim 2, characterized in that: The antioxidants include antioxidant 168 and antioxidant 1010, wherein: The weight percentage of the antioxidant 168 is 0.2%; The weight percentage of the antioxidant 1010 is 0.2%.
4. A preparation process for the mosquito and insect glue according to claim 3, characterized in that: The following steps are involved: Step 1: Raw material preparation: The raw materials are configured according to the formula ratio and production volume, including rubber SIS, rubber SEBS, hydrogenated petroleum resin, hydrogenated rosin, naphthenic oil, paraffin-based oil, antioxidant 168, antioxidant 1010 and ultraviolet light absorber; Step 2: Add oxidant and part of naphthenic oil and heat: Add antioxidant 168, antioxidant 1010, and 40% naphthenic oil into the reactor and heat the material temperature to 120 degrees; Step 3: Add rubber and melt: Add rubber SIS and rubber SEBS and wait for the rubber to be completely melted; Step 4: Add hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, remaining naphthenic oil and ultraviolet light absorber: After the rubber is melted, hydrogenated rosin, hydrogenated petroleum resin, paraffin-based oil, the remaining 60% of naphthenic oil, and ultraviolet light absorber are added successively; Step 5: Vacuum and stir: Perform vacuum operation and continue stirring for 40-50 minutes; Step 6: Discharging and forming: After stirring, discharge the material at a temperature between 135-145 degrees; Step 7: Cooling and packaging: Cool naturally to form a rubber block, and pack it when the temperature of the rubber block drops below 40 degrees.
