Diode integrated manufacturing method and integrated diode

By integrating TMBS and TVS on a single epitaxial substrate in a photovoltaic solar cell pack, the problems of high costs and application failure risk are solved, and a lower cost and higher reliability bypass protection system is achieved.

CN118969733APending Publication Date: 2024-11-15捷捷微电(南通)科技有限公司
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411050572.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

In existing photovoltaic solar cell packs, trench Schottky barrier diodes (TMBS) and transient suppression diodes (TVS) need to be packaged and wired separately, resulting in high costs and high application failure risk.

Method used

The TMBS region and the TVS region are divided on an epitaxial substrate to form a PN junction, a trench gate and a metal layer. Through photolithography and passivation layer processing, the integrated manufacturing of TMBS and TVS is realized to form a parallel integrated diode.

Benefits of technology

It reduces the cost of substrate materials, process processes, packaging and wires, reduces the risk of application failure caused by individual packaging wiring, and improves the reliability of the bypass protection system of the solar cell module.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118969733A_ABST
    Figure CN118969733A_ABST
Patent Text Reader

Abstract

The invention provides a diode integrated manufacturing method and an integrated diode, and belongs to the technical field of semiconductors, and the manufacturing method comprises the steps: dividing a TMBS region and a TVS region on an epitaxial substrate of a TMBS, forming a PN junction on the TVS region, forming a TVS trench gate on the TVS region, and forming a TMBS trench gate on the TMBS region; forming an insulating layer and an interlayer dielectric layer in the TMBS region, generating a TMBS metal layer in the TMBS region, and generating a TVS metal layer in the TVS region to obtain a third intermediate wafer; growing a passivation layer on the third intermediate wafer, and photoetching a TMBS metal layer and a TVS metal layer on the passivation layer; and forming a back metal layer on the back of the epitaxial substrate to obtain the integrated diode with the TMBS and the TVS connected in parallel. Therefore, the TMBS and the TVS are integrated on one epitaxial substrate, so that the costs of substrate materials, technological processes, packaging, wires and the like are greatly reduced. Meanwhile, packaging is achieved together, so that the risk of application failure caused by independent packaging and wiring can be avoided, and the risk of application failure is greatly reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a diode integrated manufacturing method and an integrated diode. Background Art

[0002] Trench MOS Barrier Schottky Diode (TMBS) and Transient Voltage Suppressor (TVS) are the core freewheeling and protection devices of modern photovoltaic new energy. They are important components of the bypass protection system of photovoltaic solar cells and are formed by processing metal, oxide and semiconductor materials.

[0003] TMBS is used in photovoltaic bypass integrated module junction boxes and is the core component of photovoltaic connection protection systems, making photovoltaic modules safer and more reliable. TVS is used for overvoltage protection. When a surge pulse voltage appears in the protected circuit, the bidirectional breakdown diode can quickly break down and change from a high resistance state to a low resistance state, shunting and clamping the surge voltage, thereby protecting the components in the circuit from being damaged by the instantaneous surge pulse voltage. In photovoltaic solar panels, the two protection devices, TMBS and TVS, need to be packaged and wired separately to form a photovoltaic solar cell group bypass protection system, which plays a key role in protecting solar modules.

[0004] Conventional solar modules require TMBS and TVS for freewheeling and protection. The separate packaging and wiring of a single device greatly increases the cost of substrate materials, process, packaging and wires. The separate packaging and wiring of two devices also leads to a higher risk of application failure. Summary of the invention

[0005] In view of this, the object of the present invention is to provide a diode integrated manufacturing method and an integrated diode to improve the high cost problem of trench Schottky barrier diodes and transient suppression diodes used as bypass protection systems for photovoltaic solar cell groups, while reducing the risk of failure.

[0006] In a first aspect, the present invention provides a diode integrated manufacturing method, the method comprising:

[0007] Dividing a TMBS region and a TVS region on the epitaxial substrate of the TMBS, and forming a PN junction on the TVS region to obtain a first intermediate wafer;

[0008] forming a TVS trench gate on the TVS region of the first intermediate wafer, and forming a TMBS trench gate on the TMBS region of the first intermediate wafer, so as to obtain a second intermediate wafer;

[0009] forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer, generating a TMBS metal layer in the TMBS region, and generating a TVS metal layer in the TVS region, so as to obtain a third intermediate wafer; wherein the interlayer dielectric layer is located on the terminal trench of the TMBS trench gate;

[0010] Growing a passivation layer on the third intermediate wafer, and photolithographically forming the TMBS metal layer and the TVS metal layer on the passivation layer;

[0011] A back metal layer is formed on the back side of the epitaxial substrate to obtain an integrated diode in which the TMBS and the TVS are connected in parallel.

[0012] Optionally, the step of forming a PN junction on the TVS region includes:

[0013] Growing a layer of silicon dioxide on the epitaxial substrate as a first mask;

[0014] Using a first photoresist to open a window in the TVS region of the first mask, removing silicon dioxide on the TVS region, and injecting boron ions into the TVS region;

[0015] After the boron ion implantation is completed, the silicon dioxide on the epitaxial substrate is removed, and a high-temperature push-junction is performed to form a PN junction on the TVS region.

[0016] Optionally, the step of performing high temperature push-knot includes:

[0017] Perform high-temperature pushing according to the preset pushing temperature and pushing time;

[0018] Wherein, the pushing temperature is 1000-1200 degrees Celsius, and the pushing time is 120-180 minutes.

[0019] Optionally, the step of forming a TVS trench gate on the TVS region of the first intermediate wafer and forming a TMBS trench gate on the TMBS region of the first intermediate wafer includes:

[0020] growing a layer of silicon dioxide on the first intermediate wafer as a second mask;

[0021] Using a first photomask to open a window in the TVS region of the second mask, injecting phosphorus ions, and depositing a dielectric layer;

[0022] Using a second photomask to open a window in the TVS region of the second mask, performing silicon etching and oxidation to obtain a TVS trench, and growing a gate oxide layer and depositing polysilicon for each of the TVS trenches to form a TVS trench gate;

[0023] A third photomask is used to open a window in the TMBS region of the second mask, silicon etching and oxidation are performed to obtain TMBS trenches, and a gate oxide layer is grown and polysilicon is deposited for each TMBS trench to form a TMBS trench gate.

[0024] Optionally, the implantation energy of the phosphorus ions is 90-120 kev, and the implantation dose of the phosphorus ions is 10 14 ~10 16 Pieces / cm 2 .

[0025] Optionally, the step of forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer includes:

[0026] depositing a dielectric layer on the second intermediate wafer;

[0027] Using a fourth photomask to open a window on the dielectric layer, removing the area in contact with the metal from the dielectric layer, so as to form an interlayer dielectric layer composed of the remaining dielectric layer in the TMBS region;

[0028] A fifth photomask is used to open windows only in the metal region of the TMBS region, and an insulating layer is formed in the metal region of the TMBS region.

[0029] Optionally, the step of forming an insulating layer in the metal region of the TMBS region includes:

[0030] A barrier metal is deposited in the metal region of the TMBS region and rapidly annealed to form an insulating layer.

[0031] Optionally, the step of generating a TMBS metal layer in the TMBS region and generating a TVS metal layer in the TVS region includes:

[0032] sputtering an aluminum-silicon-copper composite metal onto the entire second intermediate wafer after the insulating layer is formed, to form a metal layer;

[0033] A fifth photomask is used to open a window in the metal layer, and the metal layer in the window opening area is etched to form a TMBS metal layer in the TMBS area and a TVS metal layer in the TVS area; wherein the TMBS metal layer and the TVS metal layer are not in contact with each other.

[0034] Optionally, the step of forming a back metal layer on the back side of the epitaxial substrate comprises:

[0035] Thinning the back side of the epitaxial substrate;

[0036] After thinning, cleaning is performed, and the back side of the epitaxial substrate is etched according to a preset etching thickness;

[0037] After the etching is completed, metal evaporation is performed on the back side of the epitaxial substrate to form a back side metal layer.

[0038] In a second aspect, the present invention provides an integrated diode, wherein the integrated diode is manufactured by the diode integrated manufacturing method as described in the first aspect, and the integrated diode comprises an epitaxial substrate, a back metal layer on the back side of the epitaxial substrate, a TMBS structure and a TVS structure and a passivation layer on the epitaxial substrate;

[0039] The TMBS structure comprises a TMBS trench gate on an epitaxial substrate, an interlayer dielectric layer and an insulating layer located above the TMBS trench gate, and a TMBS metal layer covering the interlayer dielectric layer and the insulating layer;

[0040] The TVS structure includes a PN junction, a TVS trench gate formed in the PN junction, and a TVS metal layer located on the PN junction;

[0041] The passivation layer covers the front side of the integrated diode, and does not cover the TMBS metal layer and the TVS metal layer.

[0042] The diode integrated manufacturing method and the integrated diode provided by the embodiment of the present invention include: dividing the TMBS region and the TVS region on the epitaxial substrate of the TMBS, forming a PN junction on the TVS region to obtain a first intermediate wafer; forming a TVS trench gate on the TVS region of the first intermediate wafer, forming a TMBS trench gate on the TMBS region of the first intermediate wafer to obtain a second intermediate wafer; forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer, and generating a TMBS metal layer in the TMBS region, generating a TVS metal layer in the TVS region, to obtain a third intermediate wafer; growing a passivation layer on the third intermediate wafer, and photolithography a TMBS metal layer and a TVS metal layer on the passivation layer; forming a back metal layer on the back of the epitaxial substrate to obtain an integrated diode in which the TMBS and TVS are connected in parallel. In this way, the TMBS and TVS are integrated on an epitaxial substrate, which greatly reduces the costs of substrate materials, process, packaging, and wires. At the same time, by integrating TMBS and TVS into one and packaging them together, the risk of application failure caused by separate packaging and wiring can be avoided, greatly reducing the risk of application failure.

[0043] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, preferred embodiments are given below and described in detail with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0044] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0045] Figure 1 The planar structure diagram of the existing TMBS and TVS is shown.

[0046] Figure 2 The application circuit diagram of TMBS and TVS in solar cell modules is shown.

[0047] Figure 3 A schematic flow chart of a diode integrated manufacturing method provided in an embodiment of the present invention is shown.

[0048] Figure 4 Shows Figure 3 Schematic diagram of the process flow of some sub-steps of step 11.

[0049] Figure 5 A schematic cross-sectional view of the first intermediate wafer after step 11 is performed is shown.

[0050] Figure 6 Shows Figure 3 Schematic diagram of the process flow of some sub-steps of step 13.

[0051] Figure 7 FIG. 4 is a schematic cross-sectional view of the second intermediate wafer after step 13 is performed.

[0052] Figure 8 Shows Figure 3 Schematic diagram of the process of some sub-steps of step 15.

[0053] Fig. 9 A schematic cross-sectional view of the third intermediate wafer after step 15 is performed is shown.

[0054] Fig.10 A schematic cross-sectional view of the third intermediate wafer after step 17 is performed is shown.

[0055] Fig.11 Shows Figure 3 Schematic diagram of the process of some sub-steps of step 19.

[0056] Fig.12 The cross-sectional schematic diagram of the integrated diode obtained after executing step 19 is shown.

[0057] Fig.13 The planar structure diagram of the integrated diode provided by the embodiment of the present invention is shown.

[0058] Explanation of the reference numerals: 1-epitaxial substrate; 101-substrate; 102-epitaxial layer; 103-PN junction; 2-TMBS region; 3-TVS region; 4-TVS trench gate; 5-TMBS trench gate; 6-insulating layer; 7-interlayer dielectric layer; 8-TMBS metal layer; 9-TVS metal layer; 10-back metal layer; 12-passivation layer. DETAILED DESCRIPTION

[0059] The following will be combined with the accompanying drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Generally, the components of the embodiments of the present invention described and shown in the drawings here can be arranged and designed in various different configurations.

[0060] Therefore, the following detailed description of the embodiments of the present invention provided in the accompanying drawings is not intended to limit the scope of the invention claimed for protection, but merely represents selected embodiments of the present invention. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative work are within the scope of protection of the present invention.

[0061] It should be noted that relational terms such as "first" and "second" are used only to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0062] See also Figure 1 , is a planar structure diagram of a trench MOS barrier Schottky diode (TMBS) and a transient voltage suppressor diode (TVS). It should be noted that, Figure 1 (a) and Figure 1(b) is different, which is only for the convenience of comparing the planar structures of TMBS and TVS. In practical applications, the side length ratio of the outer frame square of TMBS and the outer frame square of TVS can be 15:1, for example, Figure 1 The side length of the outer square of (a) is 3 mm. Figure 1 The side length of the outer frame square of (b) is 0.2 mm.

[0063] At present, the common planar structures of TMBS are as follows Figure 1 As shown in (a), TMBS is applied to the photovoltaic bypass integrated module junction box and is the core device of the photovoltaic connection protection system, making the operation of photovoltaic modules safer and more reliable. Figure 1 As shown in (b), TVS is used for overvoltage protection. When a surge pulse voltage appears in the protected circuit, the bidirectional breakdown diode can quickly break down and change from a high resistance state to a low resistance state, shunting and clamping the surge voltage, thereby protecting the components in the circuit from being damaged by the instantaneous surge pulse voltage. Figure 2 As shown, each solar cell module is connected in parallel with a TMBS and a TVS, and the TMBS and the TVS are packaged and wired separately to form a photovoltaic solar cell group bypass protection system, which plays a key role in protecting the solar cell module.

[0064] However, when TMBS and TVS are applied to solar cell modules, a single device is packaged and wired separately, which increases the cost of substrate materials, process, packaging and wire materials. In addition, the separate packaging and wiring of two devices can easily lead to a higher risk of application failure.

[0065] In view of this, an embodiment of the present invention provides a diode integrated manufacturing method, which manufactures TMBS and TVS on an epitaxial substrate at the same time, integrates TMBS and TVS on the same tube die, and greatly reduces the cost of substrate materials, process, packaging and wire materials. At the same time, TMBS and TVS integrated on the same tube die can be packaged and wired together, thereby avoiding problems caused by separate packaging and wiring, and reducing the risk of application failure.

[0066] The diode integrated manufacturing method provided by the present invention is exemplarily described below.

[0067] The embodiment of the present invention provides a diode integrated manufacturing method, please refer to Figure 3 , may include steps 11 to 19.

[0068] Step 11, dividing the TMBS2 and TVS regions on the TMBS epitaxial substrate, and forming a PN junction on the TVS region to obtain a first intermediate wafer.

[0069] Step 13, forming a TVS trench gate on the TVS region of the first intermediate wafer, and forming a TMBS trench gate on the TMBS region of the first intermediate wafer, to obtain a second intermediate wafer.

[0070] Step 15, forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer, generating a TMBS metal layer in the TMBS region, and generating a TVS metal layer in the TVS region, so as to obtain a third intermediate wafer.

[0071] The interlayer dielectric layer is located on the terminal trench of the TMBS trench.

[0072] Step 17, growing a passivation layer on the third intermediate wafer, and photolithographically forming a TMBS metal layer and a TVS metal layer on the passivation layer.

[0073] Step 19, forming a back metal layer on the back side of the epitaxial substrate to obtain an integrated diode in which the TMBS and the TVS are connected in parallel.

[0074] In step 11, the epitaxial substrate is an epitaxial substrate obtained by growing an N-type epitaxial layer on a substrate, and the size of the epitaxial substrate is consistent with the size of the epitaxial substrate of the required TMBS, that is, the epitaxial substrate can be manufactured according to the requirements of the substrate and epitaxial layer of the TMBS. In addition, the method of forming the PN junction on the TVS region 3 can be flexibly set, for example, an alloy method, a diffusion method, an ion implantation method, or an epitaxial growth method can be used, and the above method is only an example and is not limited in this embodiment.

[0075] In order to quickly form a PN junction, ion implantation and junction pushing are combined in the process of forming a PN junction in step 11. Figure 4 , a PN junction may be formed on the TVS region by following steps 111 to 113 .

[0076] Step 111, growing a layer of silicon dioxide on the epitaxial substrate as a first mask.

[0077] In the implementation process, the thickness of the grown carbon dioxide can be adjusted according to actual needs, and is not limited in this embodiment. In order to provide isolation protection for the area outside the TVS area in the epitaxial substrate to protect it from the subsequent ion implantation and high-temperature push-in, the thickness of the grown carbon dioxide in step 111 can be A sufficiently thick first mask is provided for protecting the epitaxial substrate outside the TVS region.

[0078] Step 112, using a first photoresist to open a window in the TVS region of the first mask, removing silicon dioxide on the TVS region, and injecting boron ions into the TVS region.

[0079] The first photomask blocks all areas except the TVS area, and only opens the TVS window. The energy and dose of the implanted boron ions can be adjusted according to the performance requirements of the TVS, and are not limited in this embodiment.

[0080] In order to make the resistivity and thickness of the PN junction of the TVS region meet the requirements of the solar cell module for overvoltage protection. In this embodiment, the implantation dose of boron ions in the TVS region can be 10 16 ~10 19 Pieces / cm 2 , the injection energy can be 500~1000kev.

[0081] Step 113, after the boron ion implantation is completed, the silicon dioxide on the epitaxial substrate is removed, and a high temperature push-junction is performed to form a PN junction on the TVS region.

[0082] The method of removing carbon dioxide on the epitaxial substrate 1 in step 113 can be flexibly set. For example, wet removal (such as wet cleaning with dilute hydrofluoric acid) can be used, or dry removal can be used, that is, plasma etching technology is used to selectively remove the dielectric layer from the device surface. The above-mentioned method of removing carbon dioxide is only an example and its specific implementation method is not limited.

[0083] After removing all silicon dioxide on the epitaxial substrate, the epitaxial substrate is placed in a high-temperature furnace for high-temperature junction pushing (also known as thermal annealing) to diffuse the boron ions injected into the TVS region to obtain a PN junction with the required concentration distribution and junction depth.

[0084] In order to form a PN junction quickly and ensure that the concentration distribution and junction depth of boron ions meet the requirements of TVS, in step 113, a high-temperature junction can be performed according to a preset junction temperature and junction time. The junction temperature is 1000 to 1200 degrees Celsius and the junction time is 120 to 180 minutes.

[0085] After the above steps 111 to 113, the structure of the first intermediate wafer is as follows: Figure 5 As shown, the TMBS region 2 includes an N-type substrate 101 and an N-type epitaxial layer 102 , and the TVS region 3 includes a PN junction 103 formed by the N-type substrate 101 and a P-type silicon dioxide layer.

[0086] After obtaining the first intermediate wafer, a variety of processes may be used to form the TVS trench gate and the TMBS trench gate in step 13. For example, they may be manufactured separately or together, which is not limited in this embodiment.

[0087] In order to further reduce process and material costs, refer to Figure 6 , step 13 can be performed through the following steps 131 to 135.

[0088] Step 131 , growing a layer of silicon dioxide on the first intermediate wafer as a second mask.

[0089] Similar to the generation of the first mask in step 111, during the implementation process, the thickness of the carbon dioxide grown in step 131 can be adjusted according to actual needs, and is not limited in this embodiment. In order to provide isolation protection for the area that does not need to be opened in the subsequent photolithography, so as to protect it from the influence of subsequent photolithography window opening, ion implantation and etching processes, the thickness of the carbon dioxide grown in step 131 can be To provide a sufficiently thick second mask for isolation protection.

[0090] Step 132, using the first photoresist to open a window in the TVS region of the second mask, injecting phosphorus ions, and depositing a dielectric layer.

[0091] The values ​​of the phosphorus ion implantation dose and implantation energy can be adjusted according to the process design, design purpose and design situation, etc., and are not limited in this embodiment. In order to obtain a TVS trench gate that meets the design goal, the phosphorus ion implantation dose can be 10 14 ~10 16 Pieces / cm 2 The implantation energy can be 90-120 keV. By implanting N-type phosphorus ions on the N-type epitaxy, the epitaxial resistivity of the device is reduced.

[0092] Also, the deposited dielectric layer can be understood as plasma-enhanced tetraethoxysilane (PETEOS) interlayer dielectric (ILD) deposition, also known as ILD PETEOS deposition, and the thickness of the deposited dielectric layer can be

[0093] Step 133, using a second photoresist to open a window in the TVS region of the second mask, performing silicon etching and oxidation to obtain a TVS trench.

[0094] Among them, a plurality of photolithography holes are opened on the second photolithography plate, and the shape of the photolithography holes is consistent with the cross-sectional shape of the groove of the TVS to be manufactured. Therefore, the second photolithography plate is used to open a window in the TVS area of ​​the second mask, and the photolithography hole area exposed by the second photolithography plate is silicon etched and oxidized to form a TVS groove.

[0095] Silicon etching, namely TRH SI ETCH, is an etching process for silicon materials, and oxidation, namely selective accelerated chemical oxidation process. Moreover, silicon etching and selective accelerated chemical oxidation processes are mature processes and will not be described in detail here.

[0096] In order to make the TVS trench meet the performance requirements of the TVS device, the depth of the TVS trench may be 8 to 12 um.

[0097] Step 134, using a third photomask to open a window in the TMBS region of the second mask, performing silicon etching and oxidation to obtain a TMBS trench.

[0098] Similar to step 133, a plurality of photolithography holes are opened on the third photolithography plate, and the shape of the photolithography holes is consistent with the cross-sectional shape of the TMBS groove to be manufactured. Therefore, the third photolithography plate is used to open a window in the TMBS area of ​​the second mask, and the photolithography hole area exposed by the third photolithography plate is silicon etched and oxidized to form a TMBS groove.

[0099] In order to make the TMBS trench meet the performance requirements of the TMBS device, the depth of the TMBS trench may be 1.5 to 2.5 um.

[0100] Step 135 , growing a gate oxide layer for each TVS trench and each TMBS trench, and depositing polysilicon to form a TVS trench gate and a TMBS trench gate.

[0101] It should be noted that the method used to grow the gate oxide layer can be flexibly selected. For example, the gate oxide layer can be grown by a dry oxidation process, or by a wet oxidation process, or by preparing two layers of gate oxide layers by in-situ water vapor generation and high-temperature oxidation deposition, and then introducing a small amount of oxygen to anneal the gate oxide layer. The method of growing the gate oxide layer is not limited in this embodiment.

[0102] Similarly, the method used for depositing polysilicon can be flexibly set. For example, low-pressure chemical vapor deposition can be used to deposit polysilicon on the TVS trench and the TMBS trench, or a modified Siemens method can be used to deposit polysilicon on the TVS trench and the TMBS trench. In this embodiment, the method used is not limited.

[0103] After step 131 to step 135, the structure of the obtained second intermediate wafer is as follows: Figure 7 As shown, at this time, a TVBS trench gate is formed on the N-type epitaxial layer 102 of the TMBS region 2, and a TVS trench gate 4 is formed on the PN junction 103 of the TVS region 3. Thus, through the above steps 131 to 135, the TVS trench gate 4 and the TMBS trench gate 5 can be formed simultaneously in one process flow, which reduces the process steps and also reduces the material cost.

[0104] In order to facilitate the subsequent generation of TMBS metal layer in the TMBS area and TVS metal layer in the TVS area through one process flow, the process flow of making TMBS and TVS can be further reduced. Figure 8The process of forming the insulating layer and the interlayer dielectric layer in step 15 may include steps 151 to 153 .

[0105] Step 151, depositing a dielectric layer on the second intermediate wafer.

[0106] Among them, the dielectric layer can be deposited on the entire second intermediate wafer by using methods such as ILD PETEOS deposition.

[0107] Step 152: Use a fourth photomask to open a window on the dielectric layer, remove the area in contact with the metal from the dielectric layer, and form an interlayer dielectric layer composed of the remaining dielectric layer in the TMBS region.

[0108] The fourth photomask opens a window in the area outside the terminal trench gate of the TMBS trench gate, and removes the dielectric layer in the area outside the terminal trench gate of the TMBS trench gate by photolithography, and the remaining dielectric layer forms the interlayer dielectric layer of the TMBS region.

[0109] Step 153 , using a fifth photomask to open windows only in the metal region of the TMBS region, and forming an insulating layer in the metal region of the TMBS region.

[0110] For step 153, the insulating layer may be formed by depositing a barrier metal in the metal region of the TMBS region and performing rapid annealing to form the insulating layer. That is, after only opening a window in the metal region of the TMBS region using the fifth photomask, a barrier metal such as Ti is deposited in the metal region with the window opened, and RTP annealing is performed to form an insulating layer composed of a TiSi compound.

[0111] Furthermore, in order to reduce process and material costs, please continue to refer to Figure 8 In step 15, a TMBS metal layer can be generated in the TMBS area and a TVS metal layer can be generated in the TVS area through the following steps 154 to 155.

[0112] Step 154 ​​, sputtering an aluminum-silicon-copper composite metal onto the entire second intermediate wafer after the insulating layer is formed, to form a metal layer.

[0113] Step 155 , using a fifth photomask to open windows in the metal layer, and etching out the metal layer in the window opening area, so as to form a TMBS metal layer in the TMBS area and a TVS metal layer in the TVS area.

[0114] The aluminum-silicon-copper composite metal in step 154 ​​is merely an example, and in actual manufacturing, it can be adjusted according to the performance requirements and process requirements of the device design.

[0115] After the above steps 151 to 155, the obtained third intermediate wafer can be Fig. 9As shown, the TMBS region 2 includes an epitaxial substrate 1, a TMBS trench gate 5, an interlayer dielectric layer 7, an insulating layer 6 and a TMBS metal layer 8, and the TVS region 3 includes a PN junction 103, a TVS trench gate 4 and a TVS metal layer 9.

[0116] Furthermore, in the above steps 154 to 155, the composite metal material only needs to be sputtered once in the process of generating the TMBS metal layer 8 and the TVS metal layer 9, and the TMBS metal layer 8 and the TVS metal layer 9 are generated together, which greatly reduces the material cost and process steps.

[0117] In addition, the TMBS metal layer 8 and the TVS metal layer 9 can also be formed in the following manner: forming a first metal layer on the insulating layer 6; forming a second metal layer on the first metal layer and the interlayer dielectric layer 7 to obtain the TMBS metal layer 8; and generating the TVS metal layer 9 on the TVS region 3.

[0118] After obtaining the third intermediate wafer with the TMBS metal layer 8 and the TVS metal layer 9 formed thereon, in step 17, a SiN passivation layer is grown on the entire third intermediate wafer, and a window is opened in the area where the TMBS metal layer 8 and the TVS metal layer 9 are located in the SiN passivation layer through the sixth photomask, and the SiN passivation layer in the area where the TMBS metal layer 8 and the TVS metal layer 9 are located is removed through photolithography to expose the TMBS metal layer 8 and the TVS metal layer 9 for subsequent probe testing and packaging wire bonding. In this way, a passivation layer 12 is formed outside the TMBS metal layer 8 and the TVS metal layer 9 for protection. At this time, the structure of the third intermediate wafer can be as follows: Fig.10 shown.

[0119] After step 17, refer to Fig.11 In step 19, a back metal layer 10 can be formed on the back side of the epitaxial substrate by following steps 191 to 193.

[0120] Step 191, thinning the back side of the epitaxial substrate.

[0121] The reduced thickness may be adjusted according to the performance requirements or process conditions of the device, which is not limited in this embodiment.

[0122] In order to ensure that the final diode device can have both TMBS and TVS performance, the back side of the epitaxial substrate can be thinned by grinding, and the thickness of the thinned chip (ie wafer) can be 140-160 um.

[0123] Step 192, cleaning after thinning, and etching the back side of the epitaxial substrate according to a preset etching thickness.

[0124] After thinning, the residual particles in the grinding process are removed by cleaning, and the back side of the epitaxial substrate (usually silicon) is etched, wherein the etching thickness can also be flexibly set, for example, it can be 1-3um. The etching thickness can be adjusted according to the performance requirements or process conditions of the device, which is not limited in this embodiment.

[0125] Step 193, after the etching is completed, metal evaporation is performed on the back side of the epitaxial substrate to form a back side metal layer.

[0126] When the back metal is evaporated, the material used can be a titanium-nickel-silver composite metal, that is, the metal layer material is Ti / Ni / Ag.

[0127] After the above steps 191 to 193, the final integrated diode with TMBS and TVS connected in parallel is obtained. The structure of the integrated diode can be as follows: Fig.12 shown.

[0128] Based on the same inventive concept as the above-mentioned diode integrated manufacturing method, Fig.12 and Fig.13 The embodiment of the present invention further provides an integrated diode, which is an integrated diode in which a TMBS and a TVS are connected in parallel and is manufactured using the above-mentioned diode integrated manufacturing method.

[0129] The integrated diode comprises an epitaxial substrate 1 , a back metal layer 10 on the back side of the epitaxial substrate 1 , a TMBS structure and a TVS structure on the epitaxial substrate 1 , and a passivation layer 12 .

[0130] The TMBS structure includes a TMBS trench gate 5 on an epitaxial substrate 1 , an interlayer dielectric layer 7 and an insulating layer 6 located above the TMBS trench gate 5 , and a TMBS metal layer 8 covering the interlayer dielectric layer 7 and the insulating layer 6 .

[0131] The TVS structure includes a PN junction 103 , a TVS trench gate 4 formed in the PN junction 103 , and a TVS metal layer 9 located on the PN junction 103 .

[0132] The passivation layer 12 covers the front side of the integrated diode, and does not cover the TMBS metal layer 8 and the TVS metal layer 9 .

[0133] In summary, the diode integrated manufacturing method and the integrated diode provided by the embodiments of the present invention have at least the following advantages:

[0134] (1) Realize the integrated design and manufacturing of TMBS and TVS, reducing the cost of substrate materials, process, packaging and wire materials;

[0135] (2) The integrated diodes of TMBS and TVS used in solar cell modules can be packaged and wired together, which greatly reduces the risk of application failure and improves the reliability of the bypass protection system of the solar cell module.

[0136] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A diode integrated manufacturing method, characterized in that: The method comprises: Dividing a TMBS region and a TVS region on the epitaxial substrate of the TMBS, and forming a PN junction on the TVS region to obtain a first intermediate wafer; forming a TVS trench gate on the TVS region of the first intermediate wafer, and forming a TMBS trench gate on the TMBS region of the first intermediate wafer, so as to obtain a second intermediate wafer; forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer, generating a TMBS metal layer in the TMBS region, and generating a TVS metal layer in the TVS region, so as to obtain a third intermediate wafer; wherein the interlayer dielectric layer is located on the terminal trench of the TMBS trench gate; Growing a passivation layer on the third intermediate wafer, and photolithographically forming the TMBS metal layer and the TVS metal layer on the passivation layer; A back metal layer is formed on the back side of the epitaxial substrate to obtain an integrated diode in which the TMBS and the TVS are connected in parallel.

2. The diode integrated manufacturing method according to claim 1, characterized in that: The step of forming a PN junction on the TVS region comprises: Growing a layer of silicon dioxide on the epitaxial substrate as a first mask; Using a first photoresist to open a window in the TVS region of the first mask, removing silicon dioxide on the TVS region, and injecting boron ions into the TVS region; After the boron ion implantation is completed, the silicon dioxide on the epitaxial substrate is removed, and a high-temperature push-junction is performed to form a PN junction on the TVS region.

3. The diode integrated manufacturing method according to claim 2, characterized in that: The step of performing high temperature pushing includes: Perform high-temperature pushing according to the preset pushing temperature and pushing time; Wherein, the pushing temperature is 1000-1200 degrees Celsius, and the pushing time is 120-180 minutes.

4. The diode integrated manufacturing method according to claim 1, characterized in that: The step of forming a TVS trench gate on the TVS region of the first intermediate wafer and forming a TMBS trench gate on the TMBS region of the first intermediate wafer comprises: growing a layer of silicon dioxide on the first intermediate wafer as a second mask; Using a first photomask to open a window in the TVS region of the second mask, injecting phosphorus ions, and depositing a dielectric layer; Using a second photomask to open a window in the TVS region of the second mask, and performing silicon etching and oxidation to obtain a TVS trench; Using a third photomask to open a window in the TMBS region of the second mask, and performing silicon etching and oxidation to obtain a TMBS trench; A gate oxide layer is grown for each of the TVS trenches and each of the TMBS trenches, and polysilicon is deposited to form a TVS trench gate and a TMBS trench gate.

5. The diode integrated manufacturing method according to claim 4, characterized in that: The implantation energy of the phosphorus ions is 90-120 keV, and the implantation dose of the phosphorus ions is 10 14 ~10 16 Pieces / cm 2 .

6. The diode integrated manufacturing method according to claim 1, characterized in that: The step of forming an insulating layer and an interlayer dielectric layer in the TMBS region of the second intermediate wafer comprises: depositing a dielectric layer on the second intermediate wafer; Using a fourth photomask to open a window on the dielectric layer, removing the area in contact with the metal from the dielectric layer, so as to form an interlayer dielectric layer composed of the remaining dielectric layer in the TMBS region; A fifth photomask is used to open windows only in the metal region of the TMBS region, and an insulating layer is formed in the metal region of the TMBS region.

7. The diode integrated manufacturing method according to claim 6, characterized in that: The step of forming an insulating layer in the metal region of the TMBS region comprises: A barrier metal is deposited in the metal region of the TMBS region and rapidly annealed to form an insulating layer.

8. The diode integrated manufacturing method according to any one of claims 1 to 7, characterized in that: The step of generating a TMBS metal layer in the TMBS region and a TVS metal layer in the TVS region comprises: sputtering an aluminum-silicon-copper composite metal onto the entire second intermediate wafer after the insulating layer is formed, to form a metal layer; A fifth photomask is used to open a window in the metal layer, and the metal layer in the window opening area is etched to form a TMBS metal layer in the TMBS area and a TVS metal layer in the TVS area; wherein the TMBS metal layer and the TVS metal layer are not in contact with each other.

9. The diode integrated manufacturing method according to any one of claims 1 to 7, characterized in that: The step of forming a back metal layer on the back side of the epitaxial substrate comprises: Thinning the back side of the epitaxial substrate; After thinning, cleaning is performed, and the back side of the epitaxial substrate is etched according to a preset etching thickness; After the etching is completed, metal evaporation is performed on the back side of the epitaxial substrate to form a back side metal layer.

10. An integrated diode, characterized in that: The integrated diode is manufactured by the diode integrated manufacturing method according to any one of claims 1 to 9, and the integrated diode comprises an epitaxial substrate, a back metal layer on the back of the epitaxial substrate, a TMBS structure and a TVS structure and a passivation layer on the epitaxial substrate; The TMBS structure comprises a TMBS trench gate on an epitaxial substrate, an interlayer dielectric layer and an insulating layer located above the TMBS trench gate, and a TMBS metal layer covering the interlayer dielectric layer and the insulating layer; The TVS structure includes a PN junction, a TVS trench gate formed in the PN junction, and a TVS metal layer located on the PN junction; The passivation layer covers the front side of the integrated diode, and does not cover the TMBS metal layer and the TVS metal layer.

Citation Information

Cited By

  • A power device packaging structure based on TMBS

    CN224988029U