Underwater encryption communication system based on self-powered bipolar ultraviolet detector and application and coding method thereof

Through the self-powered bipolar ultraviolet detector and signal encoding technology of Cu2O@α-Ga2O3 nanopillar array, the problems of low communication efficiency and insufficient safety in underwater communication are solved, and efficient and safe underwater ultraviolet communication are achieved. , suitable for applications in harsh environments.

CN118972155APending Publication Date: 2024-11-15ZHEJIANG SCI-TECH UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411321642.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2024-08-30
Filing Date
2024-09-23
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing ultraviolet detectors have problems with low communication efficiency and high bit error rate in underwater communication, and a single material cannot achieve secure communication and cannot meet cost saving and portability requirements.

Method used

Cu2O@α-Ga2O3 nanocolumn array is used as a self-powered bipolar ultraviolet detector, and the substrate surface is modified by electrochemical methods, combining Cu2O microspheres and α-Ga2O3 porous sponge nanocolumn array to achieve self-self of heterojunction structure Power supply operation, and signal encoding is performed using ASCII and HDB3 encoding methods.

Benefits of technology

It improves the efficiency and security of underwater communication, realizes low-energy communication in harsh environments, has self-error detection capabilities and anti-interference capabilities, and provides dual security guarantees for channel encryption and encoding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118972155A_ABST
    Figure CN118972155A_ABST
Patent Text Reader

Abstract

The invention relates to an underwater encryption communication system based on a self-powered bipolar ultraviolet detector and application and a coding method thereof. The underwater encryption communication system specifically comprises an electrochemical workstation, a working electrode, a reference electrode, a counter electrode, an electrolyte, an electrolytic bath and an ultraviolet lamp arranged outside the electrolytic bath. According to the underwater encryption communication system, communication can be completed in underwater and high-voltage severe environments, due to the fact that the self-power-supply design is adopted, energy consumption is low, bias voltage does not need to be additionally provided, a communication signal adopts an ultraviolet light signal of invisible light and is difficult to detect, encryption information can be coded, the convenience of the system is greatly improved, and the communication cost is reduced. The method has double security assurance of channel encryption and coded signal encryption.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an underwater encrypted communication system based on a self-powered bipolar ultraviolet detector and an application and encoding method thereof. Background Art

[0002] With the increasing demand for communication anytime and anywhere, even in harsh environments such as magnetic interference, underwater and high voltage, UV communication technology has gradually emerged. UV communication does not require the pre-installation of optical fiber cables as transmission channels, and has the advantages of large transmission capacity, low power consumption and high flexibility. Its inherent non-visible light communication and negligible background noise make it very attractive. UV communication can significantly solve information security risks, external environment or third-party interference and even information leakage problems, providing a powerful solution for safe and reliable communication. At present, most UV detection equipment adopts MOCVD or CVD growth methods, which are costly, complex and polluting. These limiting factors prevent UV communication technology from meeting the growing industrial demand for cost savings, energy efficiency and portability. In recent years, photoelectrochemical (PEC) devices have attracted widespread attention due to their high responsiveness, simple manufacturing process, low cost and environmental friendliness. It is worth noting that PEC photodetectors combine the synergistic effects of physical and chemical processes in the photoelectric conversion process, providing a multifunctional strategy for the optimization and system implementation of underwater communication equipment.

[0003] In recent years, photoelectrochemical (PEC) devices have attracted extensive attention due to their high responsiveness, simple manufacturing process, low cost and environmental friendliness. It is worth noting that PEC photodetectors combine the synergistic operation of physical and chemical processes in the photoelectric conversion process, which provides a versatile strategy for underwater communication equipment optimization and system implementation. The materials of PEC photodetectors currently used for underwater applications include p-AlGaN / n-GaN, AlGaN / AlN / GaN, n++-GaN / InGaN / p++-GaN and CuSe. These systems usually rely on visible light for communication, which poses security risks and cannot ensure communication security. Gallium oxide (Ga2O3) is a semiconductor material with high potential application value. Because the band gap can reach 4.9eV, this wide band gap characteristic is highly matched with the ultraviolet wavelength in the solar blind zone (UVC range, wavelength between 100-280nm), and can effectively convert the ultraviolet radiation in the solar blind zone into electrical signals, making it an ideal material for making solar blind zone ultraviolet detection devices.

[0004] However, using pure gallium oxide as a detector for a single UV signal still has vulnerabilities, low communication efficiency and high bit error rate. Since secure communication cannot be achieved with devices made of a single material, heterojunctions are needed to help achieve encrypted communication. The heterojunction structure combines the advantages of different materials, improves device performance, achieves self-powered operation, and expands the scope of application. Cu2O has a high hole mobility and is an excellent p-type semiconductor material. It is relatively stable in redox reactions, making it effective for photoelectrochemical applications. Modifying gallium oxide with Cu2O can provide more active sites and better carrier transport properties, adding an extra dimension to underwater PEC UV communication photodetectors for transmitting information. Summary of the invention

[0005] To solve the above technical problems, the present invention relates to an underwater encrypted communication system based on a self-powered bipolar ultraviolet detector, specifically including a method for manufacturing a Cu2O@α-Ga2O3 nanorod array ultraviolet photodetector and a corresponding ultraviolet light signal encoding method.

[0006] On the one hand, the present invention provides an underwater encrypted communication system based on a self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3, the system comprising an electrochemical workstation, a working electrode, a reference electrode, a counter electrode, an electrolyte, an electrolytic cell and an ultraviolet lamp arranged outside the electrolytic cell, characterized in that the working electrode comprises a substrate, a portion of the surface of the substrate is an α-phase gallium oxide porous sponge-like nanocolumn array modified with Cu2O microspheres.

[0007] Furthermore, the partial surface of the substrate accounts for 20-80% of the surface area of ​​the substrate.

[0008] Furthermore, the substrate is selected from one or more of aluminum-doped zinc oxide (ZnO) transparent conductive glass AZO, fluorine-doped SnO2 conductive glass FTO, or conductive glass ITO coated with a layer of indium tin oxide on the surface.

[0009] Furthermore, the counter electrode is one of a platinum counter electrode, a gold counter electrode, and a carbon counter electrode.

[0010] Furthermore, the reference electrode is a calomel electrode.

[0011] Furthermore, the electrolyte is NaCl or Na2SO4 solution.

[0012] Furthermore, the preparation method of the Cu2O microsphere-modified α-phase gallium oxide porous sponge-like nanocolumn array comprises: (1) ultrasonically cleaning the substrate in acetone, anhydrous ethanol and deionized water for 5-60 minutes respectively, placing the cleaned substrate face down in a reactor, and dripping 1-10 mL of Ga(NO3)3·9H2O solution into the reactor, wherein the concentration of the solution is 1-20 mg / mL; heating at 100-300° C. for 8-24 h, and generating GaOOH crystals on the surface of the substrate after hydrothermal treatment, and annealing the prepared GaOOH crystals at 200-600° C. for 4 h to obtain an α-Ga2O3 porous sponge-like nanocolumn array; (2) The grown substrate is placed obliquely in a beaker containing 0.05-5.0 g / 40 mL of Cu(NO3)2·3H2O copper nitrate hydrate solution, ensuring that α-Ga2O3NRAs are immersed in the solution with their faces facing down; 1-20 mL of triethanolamine complexing agent is added to the solution, and the beaker is placed in a constant temperature environment of 25° C. A magnetic stirrer is used to continuously stir for 10 minutes at a speed of 10-800 r / min to ensure that the solution is evenly mixed; during the stirring process, 10-1000 μL of hydrazine hydrate is slowly added dropwise, and stirring is continued for 2 hours to promote the reduction reaction, thereby obtaining a Cu2O microsphere-modified α-phase gallium oxide porous sponge-like nanocolumn array.

[0013] The present invention also provides an application of the underwater encrypted communication system of the self-powered bipolar ultraviolet detector, wherein the underwater encrypted communication system of the self-powered bipolar ultraviolet detector is applied to channel encrypted optical communication of non-visible light.

[0014] The present invention also provides an ultraviolet signal encoding method for the underwater encrypted communication system of the self-powered bipolar ultraviolet detector. The ultraviolet signal encoding method comprises: performing three-source code encoding based on the encoding rules of ASCII. At the receiving end, an α-phase gallium oxide porous sponge-like nanocolumn array modified with Cu2O microspheres is used as a detector to receive ultraviolet signals of two selected bands. The encoded AMI code sequence is 0+0000000-0+-0+00-0+00-+0-0+0-00+0 -0+0-; in the AMI code, "+" represents positive photoelectricity, "-" represents negative photocurrent, and "0" represents dark current; the α-phase gallium oxide porous sponge nanocolumn array modified with Cu2O microspheres is used as the detector to receive the ultraviolet light signals of the two selected bands. The HDB3 code is: "0++00000--0+-0+00-0+00-+0-0+0-00+0-0+0-000+0-0+0-", in the HDB3 code, "+" represents positive photoelectricity, "-" represents negative photocurrent, and "0" represents dark current.

[0015] In order to achieve the above technical purpose, the present invention adopts the following technical solutions:

[0016] Advantages and beneficial effects of the present invention:

[0017] (1) The underwater encrypted communication system of the high-performance self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 prepared by the method of the present invention has the characteristics of being able to complete communication in harsh environments such as underwater and high voltage, and because of the self-powered design, the energy consumption is low and no additional bias voltage is required, which greatly improves the convenience of the system, is simple to operate, and is recoverable after repeated testing, and has great application prospects.

[0018] (2) The underwater encrypted communication system of the high-performance self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 prepared by the method of the present invention can perform ternary code communication (such as AMI and HDB3 coding) underwater through ultraviolet light. AMI coding uses positive and negative currents alternately to represent "1", and has self-error detection capability, thereby improving the reliability of the system. In addition, the current change of AMI coding helps the receiving end to extract the clock signal from the signal without the need for an additional clock synchronization signal, which is particularly useful in PEC underwater communication systems without a return path. In contrast, HDB3 coding further solves the problem of long strings of "0" in data transmission, and improves error detection capability and anti-interference capability.

[0019] (3) The underwater encrypted communication system of the high-performance self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 prepared by the method of the present invention uses visible light ultraviolet light signals, which are difficult to detect, and the bipolar photocurrent generated by irradiation with light of different bands can realize the encoding of encrypted information, providing dual security protection of channel encryption and coding signal encryption. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is an underwater encrypted communication system of a self-powered bipolar ultraviolet detector designed by the method of the present invention, specifically including a schematic diagram of the structure of a Cu2O@α-Ga2O3 nanocolumn array ultraviolet photodetector;

[0021] Figure 2 This is the SEM surface spectrum of Cu2O@α-Ga2O3 designed by the method of the present invention;

[0022] Figure 3 The photoelectric performance of the Cu2O@α-Ga2O3 nanorod array after modification of microspheres prepared by the method of the present invention in an electrolyte solution;

[0023] Figure 4 The Cu2O@α-Ga2O3 underwater ultraviolet ternary code communication made by the method of the present invention includes ASCII code, AMI code and HDB3 code;

[0024] Figure 5 The Cu2O@α-Ga2O3 underwater ultraviolet light encrypted communication is manufactured by the method of the present invention.

[0025] Reference numerals:

[0026] 1-Electrochemical workstation 2-Working electrode 3-Reference electrode 4-Counter electrode 5-UV lamp 6-Cu2O@α-Ga2O3 DETAILED DESCRIPTION

[0027] The present invention is further described below with reference to examples.

[0028] Example 1

[0029] The invention discloses an underwater encrypted communication system based on a high-performance self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3, which comprises one or more of aluminum-doped zinc oxide (ZnO) transparent conductive glass AZO, fluorine-doped SnO2 conductive glass FTO or conductive glass ITO coated with a layer of indium tin oxide as a substrate, an α-phase gallium oxide porous sponge-like nanocolumn array, Cu2O microspheres, a calomel electrode and a platinum counter electrode. The α-phase gallium oxide porous sponge-like nanocolumn array is grown on the selected substrate, and the area is 20-80% of the surface area of ​​the substrate. The Cu2O microspheres are modified on the semiconductor nanocolumn array, and the counter electrode is one of a platinum counter electrode, a gold counter electrode and a carbon counter electrode. Ultraviolet light is irradiated onto the receiving device of the communication system through quartz glass, and the device absorbs ultraviolet light energy and generates electrons and holes. When electrons are transmitted from the device to the electrochemical workstation, a positive photocurrent is formed; when electrons are transmitted back to the device from the circuit, a negative photocurrent is formed.

[0030] Furthermore, a method for manufacturing an underwater encrypted communication system based on a high-performance self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 in the present invention comprises the following steps:

[0031] (1) Preparation of α-Ga2O3 porous sponge-like nanocolumn arrays:

[0032] One or more of the conductive glass FTO, ITO, and AZO are selected as the substrate layer, which can be used as the seed layer for the growth of the nanocolumn array. The selected substrate is ultrasonically cleaned in acetone, anhydrous ethanol, and deionized water for 5-60 minutes respectively, and the cleaned substrate is placed face down in a reactor made of one or more materials including polytetrafluoroethylene (PTFE), carbon manganese steel, stainless steel, zirconium, and nickel-based (Hastelloy, monel, Inconel). 1-10mL of Ga(NO3)3·9H2O solution is dripped into the reactor, and the solution concentration is 1-20mg / mL. Heat at 100-300℃ for 8-24h, and GaOOH crystals are generated on the surface of the substrate after hydrothermal treatment. The prepared GaOOH crystals are annealed at 200-600℃ for 4h to obtain an α-Ga2O3 porous sponge-like nanocolumn array.

[0033] (2) Cu2O@α-Ga2O3 heterostructure composition:

[0034] Prepare 0.05-5.0g / 40mL of Cu(NO3)2·3H2O copper nitrate hydrate solution, and place the FTO substrate with α-Ga2O3NRAs grown on it in a beaker at an angle, making sure that the α-Ga2O3 NRAs are facing down and immersed in the solution. Add 0-20mL of triethanolamine complexing agent to the solution to prevent early precipitation of metal ions, make the solution more stable, and create an environment conducive to copper ion complexation. Place the reaction beaker in a constant temperature environment of 25℃, and use a magnetic stirrer to stir continuously for 10 minutes at a speed of 0-800r / min to ensure that the solution is evenly mixed. During the stirring process, slowly add 0-1000μL of hydrazine hydrate and continue stirring for 2 hours to promote the reduction reaction.

[0035] (3) Composition of underwater encrypted communication system

[0036] In order to build an underwater encrypted communication system, an electrochemical workstation or other instrument that can control and monitor the current and potential of the electrochemical cell, as well as other electrochemical parameter changes, is used as the basic test environment. The prepared Cu2O@α-Ga2O3 NRAs is connected to the quartz electrolytic cell as the working electrode, and a saturated calomel electrode is used as the reference electrode. A platinum counter electrode, a gold counter electrode, and a carbon counter electrode are used as the counter electrode (the model is one of 5*5*0.1mm, 5*5*0.2mm, 5*10*0.1mm, 5*10*0.2mm, 10*10*0.1mm, 10*10*0.2mm, 10*10*0.3mm, etc.). Add 10-100mL of electrolyte (NaCl or Na2SO4 0.1-5.0mol / L) to the quartz electrolytic cell. When the electrochemical workstation is running, ensure that the working electrode is parallel to the selected counter electrode, and use LED ultraviolet light with a wavelength of 220-380nm as the control light source for external input conditions, and irradiate the working electrode and the counter electrode vertically.

[0037] An underwater ultraviolet communication system was built in the solar blind area to complete the channel encryption optical communication of visible light. In addition, the system uses bipolarity to realize ternary code communication and dual-frequency optical encryption communication. This experimental project is based on channel encryption and bipolar coding encryption communication technology to improve the security and reliability of underwater communication.

[0038] The fabrication process of the Cu2O@α-Ga2O3 porous sponge-like nanopillar array in steps (1) and (2) and the self-powered deep ultraviolet photoelectric driven logic gate structure in step (3) are as follows: Figure 1 As shown, the morphology of Cu2O@α-Ga2O3 is shown in Figure 2 shown.

[0039] Example 2

[0040] According to claim 1, a high-performance self-powered bipolar ultraviolet detector based on Cu2O@α-Ga2O3 is used as an underwater encrypted communication system, which is composed of one or more of aluminum-doped zinc oxide (ZnO) transparent conductive glass AZO, fluorine-doped SnO2 conductive glass FTO or conductive glass ITO coated with a layer of indium tin oxide as a substrate, an α-phase gallium oxide porous sponge nanocolumn array, a Cu2O modified film, a calomel electrode, and a counter electrode. It corresponds to the deep ultraviolet spectrum of 220-380nm wavelength. The detector has a fast response speed, can be self-powered, has a low preparation cost, and has little environmental pollution. Its tested photoelectric performance is as follows: Figure 3 shown.

[0041] Example 3

[0042] Steps (1) and (2) are the same as those in Example 1. Figure 4 As shown, based on the design and research of the above Ga2O3-based detectors, in current optical communication systems, the American Standard Code for Information Interchange (ASCII) encoding scheme is often used to convert text information into digital signals for optical transmission. Specifically, each ASCII character is assigned a unique eight-bit binary number to represent it. For example, the uppercase letters "Z", "S", "T" and "U" have specific decimal code values ​​in ASCII. According to the ASCII encoding rules of the above characters, the system modulates the light source to send a specific sequence, selects the appropriate wavelength of light to correspond to the device's response to the day-blind ultraviolet light range, and then realizes the encoding and transmission of information. At the receiving end, the detector made of pure α-Ga2O3 is responsible for receiving the selected 254nm ultraviolet light signal. Further, three-source code encoding is performed on the basis of ASCII. At the receiving end, Cu2O@α-Ga2O3 is used as the detector to receive the selected two bands of ultraviolet light signals. The AMI code sequence after encoding is 0+0000000-0+-0+00-0+00-+0-0+0-00+0-0+0-. Figure 4 As shown in the figure, in the AMI code, "+" represents positive photoelectricity, "-" represents negative photocurrent, and "0" represents dark current. In addition, Cu2O@α-Ga2O3 is used as a detector to receive the ultraviolet light signals of the two selected bands. The HDB3 code is: "0++00000--0+-0+00-0+00-+0-0+0-000+0-0+0-" In the HDB3 code, "+" represents positive photoelectricity, "-" represents negative photocurrent, and "0" represents dark current. Figure 4 As shown, the HDB3 code optical signal carrying the information "ZSTU" and the photocurrent monitored by the underwater communication device.

[0043] Example 4

[0044] Steps (1) and (2) are the same as in Example 1.

[0045] Based on the above non-visible light communication channel encryption technology, the bipolarity of the photocurrent is used to encrypt and encode the information, and the channel and coding double encryption technology is used to ensure communication security. It can be seen from the figure that using two different wavelengths of ultraviolet light (254nm and 365nm) to represent the initial signal and the key file respectively can realize complex encryption and decryption processes.

[0046] like Figure 5As shown, the original signal is "ZSTU" and the ASCII code is the positive "0" and "1" signals, which are represented by ultraviolet light with a wavelength of 254nm, respectively. "LOVE" is the key information, which is represented by ultraviolet light with a wavelength of 365nm to represent "0" and "1". The initial signal is superimposed with the key information, and two different ultraviolet lights are manipulated at the same time, which is the encrypted communication code of "ZSTU". The initial signal is superimposed with the key information, and ultraviolet light with a wavelength of 254nm and ultraviolet light with a wavelength of 365nm are manipulated at the same time to generate an encrypted optical signal. The figure shows the encrypted photocurrent signal. This signal is generated by the combined action of ultraviolet light with a wavelength of 254nm and ultraviolet light with a wavelength of 365nm. The positive photocurrent represents "1", the negative photocurrent represents "-1", the absence of light represents "0", and the weak photocurrent generated by the simultaneous action of the two light sources also represents "0".

[0047] Obviously, the above embodiments are merely examples for clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, any modification, substitution, or improvement made on the basis of the above description and within the method and principle of the present invention should be included in the protection scope of the present invention. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the protection scope of the present invention.

Claims

1. An underwater encrypted communication system based on a self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3, the system comprising an electrochemical workstation, a working electrode, a reference electrode, a counter electrode, an electrolyte, an electrolytic cell and an ultraviolet lamp arranged outside the electrolytic cell, characterized in that: The working electrode comprises a substrate, a part of the surface of which is an α-phase gallium oxide porous sponge-like nano-column array modified by Cu2O microspheres.

2. According to claim 1, an underwater encrypted communication system based on a self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 is characterized in that: The partial surface of the substrate accounts for 20 to 80% of the surface area of ​​the substrate.

3. According to claim 1, the underwater encrypted communication system based on the self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 is characterized in that: The substrate is selected from one or more of aluminum-doped zinc oxide (ZnO) transparent conductive glass AZO, fluorine-doped SnO2 conductive glass FTO, or conductive glass ITO coated with a layer of indium tin oxide on the surface.

4. According to claim 1, the underwater encrypted communication system based on the self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 is characterized in that: The counter electrode is one of a platinum counter electrode, a gold counter electrode and a carbon counter electrode.

5. According to claim 1, the underwater encrypted communication system based on the self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 is characterized in that: The reference electrode is a calomel electrode.

6. According to claim 1, the underwater encrypted communication system based on the self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 is characterized in that: The electrolyte is NaCl or Na2SO4 solution.

7. The underwater encrypted communication system based on the self-powered bipolar ultraviolet detector of Cu2O@α-Ga2O3 according to claim 1 is characterized in that: The preparation method of the Cu2O microsphere-modified α-phase gallium oxide porous sponge-like nanocolumn array comprises: (1) ultrasonically cleaning a substrate in acetone, anhydrous ethanol and deionized water for 5-60 minutes respectively, placing the cleaned substrate face down in a reaction kettle, and dripping 1-10mL of Ga(NO3)3·9H2O solution into the reaction kettle, wherein the concentration of the solution is 1-20mg / mL; heating at 100-300°C for 8-24h, and generating GaOOH crystals on the surface of the substrate after hydrothermal treatment, and annealing the prepared GaOOH crystals at 200-600°C for 4h to obtain an α-Ga2O3 porous sponge-like nanocolumn array; (2) obliquely placing the grown substrate in a beaker containing 0.05-5.0g / 40mL of Cu(NO3)2·3H2O copper nitrate hydrate solution to ensure that the α-Ga2O3 The NRAs are immersed face down in the solution; 1-20 mL of triethanolamine complexing agent is added to the solution, and then the beaker is placed in a constant temperature environment of 25°C, and a magnetic stirrer is used to continuously stir for 10 minutes at a speed of 10-800 r / min to ensure that the solution is evenly mixed. During the stirring process, 10-1000 μL of hydrazine hydrate is slowly added dropwise, and stirring is continued for 2 hours to promote the reduction reaction, thereby obtaining a Cu2O microsphere-modified α-phase gallium oxide porous sponge-like nanocolumn array.

8. An application of an underwater encrypted communication system of the self-powered bipolar ultraviolet detector according to any one of claims 1 to 7, characterized in that: The underwater encrypted communication system of the self-powered bipolar ultraviolet detector is applied to the channel encrypted optical communication of non-visible light.

9. A method for encoding ultraviolet light signals in an underwater encrypted communication system based on the self-powered bipolar ultraviolet detector according to any one of claims 1 to 7, characterized in that: The ultraviolet light signal encoding method comprises: performing three-source code encoding based on the encoding rules of ASCII, at the receiving end, using an α-phase gallium oxide porous sponge-like nanocolumn array modified with Cu2O microspheres as a detector to receive ultraviolet light signals of two selected bands, and the encoded AMI code sequence is 0+0000000-0+-0+00-0+00-+0-0+0-00+0-0+0-; in the AMI code, "+" represents positive light. "-" represents negative photocurrent, and "0" represents dark current; the α-phase gallium oxide porous sponge nanocolumn array modified with Cu2O microspheres is used as the detector to receive the ultraviolet light signals of the two selected bands. The HDB3 code is: "0++00000--0+-0+00-0+00-+0-0+0-000+0-0+0-", in which "+" represents positive photocurrent, "-" represents negative photocurrent, and "0" represents dark current.