Preparation method and application of phycoerythrin-nano-selenium compound

The phycoerythrin-selenium nanocomplex solves the problem of nano-selenium aggregation by preparing stable PE-SeNPs, thereby improving the activity of plant antioxidant enzymes and stress resistance, promoting photosynthesis, alleviating salt stress, and enhancing plant growth.

CN118975577APending Publication Date: 2024-11-19LUDONG UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411052339.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

Nano-elemental selenium tends to aggregate without a dispersing template, which affects its biological activity. Furthermore, existing technologies are insufficient to effectively enhance the activity of antioxidant enzymes and stress resistance in plants to alleviate salt stress.

Method used

Phycoerythrin reacts with sodium selenite to generate phycoerythrin-selenium nanocomplexes (PE-SeNPs). Glutathione is used as a reducing agent to form stable PE-SeNPs, which are then applied to plants as foliar sprays to enhance their antioxidant capacity and photosynthetic properties.

Benefits of technology

Phycoerythrin-nano-selenium complex effectively improves plant stress resistance, alleviates salt stress, promotes photosynthesis, reduces proline content, increases net photosynthetic rate, and enhances plant growth and development.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118975577A_ABST
    Figure CN118975577A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method and application of a phycoerythrin-nano-selenium compound, the optimal preparation conditions of the compound are determined, and the structural characteristics of the compound are represented; the prepared nano-selenium compound is used as an additive, and a foliage spraying experiment is carried out on salt-stressed soybean seedlings. Two plant universal important photosynthesis and stress resistance indexes, namely the net photosynthetic rate and the proline content, are detected, and analysis experiment results prove that the compound prepared by the invention can effectively promote photosynthesis and relieve salt stress of soybean seedlings, so that the compound can be widely applied as a novel efficient green nano-selenium additive.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of organic complexes, and specifically relates to a preparation method of a phycoerythrin-nano selenium complex (PE-SeNPs) and its application as a novel and efficient green nano selenium additive in alleviating plant salt stress and improving photosynthesis. Background Art

[0002] Nano-selenium has the characteristics of high surface activity, high catalytic efficiency, low toxicity, and is easily absorbed and transported by plants. However, in the absence of a dispersed template, nano-element selenium will aggregate, thus affecting its biological activity. Phycoerythrin (PE) is a type of light-harvesting pigment protein that is highly soluble in water and has high quantum efficiency fluorescence properties, natural antioxidant properties and nutritional effects. It can also be used as a template regulator to control the aggregation or aggregation of nano-selenium, thereby obtaining an ideal phycoerythrin-nanoselenium complex. Through the reduction reaction with glutathione as a reducing agent, SeO3 2 -First reduced to Se by glutathione 0 , then the generated Se 0 It is firmly wrapped and passivated by PE to form selenium-oxygen coordination bonds (CO…Se) or selenium-nitrogen coordination bonds (CN…Se), thereby preventing the accumulation and precipitation of nano-selenium (SeNPs) and forming well-dispersed and stable PE-SeNPs.

[0003] Selenium is an active factor of important physiologically active enzymes in plants. It can increase the activity of antioxidant enzymes in plants, effectively regulate crop growth, stimulate plant growth and development, increase crop yields and improve quality, and enhance stress resistance. Phycoerythrin helps plants capture light to promote their photosynthesis, and then synergizes with its antioxidant and nutritional effects, thereby promoting their growth and development and improving stress resistance. Phycoerythrin and nano-selenium are combined into a new type of nanomaterial that synergistically alleviates salt stress and improves the overall photosynthetic efficiency of plants.

[0004] The present invention prepares a novel phycoerythrin nano-selenium foliar spray agent, and finds that it can effectively improve the stress resistance of soybean seedlings, alleviate salt stress, and promote its photosynthesis, and has great application value in production. Therefore, the phycoerythrin nano-selenium complex in the present invention meets the needs of sustainable agricultural development and has broad application prospects. Summary of the invention

[0005] The purpose of the present invention is to provide a preparation method of a phycoerythrin nano-selenium complex and its application, and to provide a new type of foliar spray for improving the stress resistance of plant seedlings, alleviating salt stress and promoting growth.

[0006] In order to achieve the above object, the technical solution of the present invention is summarized as follows:

[0007] A method for preparing a phycoerythrin-nanoselenium complex, the method comprising the following steps:

[0008] A certain proportion of phycoerythrin solution and sodium selenite solution are respectively mixed under the action of magnetic stirring to obtain a mixture; then an appropriate amount of glutathione solution is dropped into the mixture under vigorous stirring, stirred and fully reacted under light-proof conditions to obtain a phycoerythrin nano-selenium particle dispersion; the dispersion is dialyzed and centrifuged under light-proof conditions, the precipitate is collected, washed, and freeze-dried to obtain a phycoerythrin nano-selenium complex, namely, a PE-SeNPs complex.

[0009] Preferably, the concentration of the phycoerythrin solution is 0-8 mg / mL, the concentration of the sodium selenite solution is 0.5-3 mM, the concentration of the glutathione solution is 80 mM, the volume ratio of the phycoerythrin solution to the sodium selenite solution is 1:0.5:1-5, and the volume ratio of the mixture to the added glutathione solution is 1:1-6:1.

[0010] Preferably, the conditions for light-shielding dialysis are: dialysis with deionized water in a 3500Da dialysis bag for 48-50 hours, a centrifugal speed of 12000-15000 r / min, and a time of 5-12 minutes.

[0011] Preferably, the particle size of the PE-SeNPs complex is 20-200 nm.

[0012] Preferably, the concentration of PE-SeNPs for foliar spraying is 40-60 μmol / mL.

[0013] The PE-SeNPs complex prepared according to the above preparation method is also within the protection scope of the present invention.

[0014] The above PE-SeNPs complex is used as a foliar spray. The prepared foliar spray can affect some physiological indicators and photosynthetic indicators of soybean seedlings under salt stress. Experiments have shown that it can greatly alleviate the salt stress of soybean seedlings. Therefore, the foliar spray prepared by the present invention can improve the stress resistance of soybean seedlings, alleviate salt stress, and promote photosynthesis.

[0015] Advantages of the present invention:

[0016] The present invention provides a phycoerythrin-nano-selenium complex and optimal preparation conditions of the complex. Experiments also show that spraying PE-SeNPs can reduce the proline content of soybean seedlings under salt stress and increase the net photosynthetic rate (Pn) of soybean seedlings. Therefore, phycoerythrin-nano-selenium effectively improves the stress resistance of soybean seedlings and promotes photosynthesis, providing an experimental reference for further developing a new type of highly efficient green nano-selenium additive, which is of great significance for alleviating salt stress of crops. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 is a schematic diagram of preparing PE-SeNPs;

[0018] Figure 2 is a transmission electron microscopy characterization result diagram of PE-SeNPs prepared in Example 1;

[0019] Figure 3 is the potential diagram of PE-SeNPs prepared in Example 1;

[0020] Figure 4 is a particle size diagram of PE-SeNPs prepared in Example 1;

[0021] Figure 5 is the infrared spectrum of PE-SeNPs prepared in Example 1;

[0022] Figure 6 is the UV spectrum of PE-SeNPs prepared in Example 1;

[0023] Figure 7 This is a comparison of three groups of soybean seedling plants;

[0024] Figure 8 This is a comparison chart of taproot lengths of soybean seedlings;

[0025] Fig. 9 This is a comparison chart of the net photosynthetic rate of soybean seedlings; in the figure, CK: blank control group; Y: salt treatment; YG: salt treatment + phycoerythrin nanoselenium; YA: salt treatment + sodium selenite; YI: salt treatment + PE-SeNPs;

[0026] Fig.10 This is a comparison chart of proline content in soybean seedlings; in the figure, CK: blank control group; Y: salt treatment; YG: salt treatment + phycoerythrin nanoselenium; YA: salt treatment + sodium selenite; YI: salt treatment + PE-SeNPs;

[0027] Fig.11 is a comparison of the net photosynthetic rates of salt-treated soybean seedlings at different PE-SeNPs concentrations;

[0028] Fig.12 It is a comparison chart of proline content in salt-treated soybean seedlings under different concentrations of PE-SeNPs. DETAILED DESCRIPTION

[0029] The present invention will be further described below in conjunction with specific examples, and the advantages and features of the present invention will become clearer as the description proceeds. However, the specific experimental methods involved in the following examples are all conventional methods or implemented under the conditions recommended by the manufacturer's instructions unless otherwise specified.

[0030] Unless otherwise specified, the technical means used in the examples are conventional means known to those skilled in the art. The test methods in the following examples are conventional methods unless otherwise specified. Unless otherwise specified, the reagents and materials used can all be purchased from the market.

[0031] Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein may be applied to the present invention. The preferred implementation methods and materials described herein are for demonstration purposes only.

[0032] Example 1 A method for preparing a phycoerythrin-nanoselenium complex ( Figure 1 )

[0033] 0.5 mL of 5 mg / mL phycoerythrin solution and 2 mL of 0.5 mM sodium selenite solution were mixed under magnetic stirring to obtain a mixture. Then 1.5 mL of freshly prepared 80 mM glutathione solution was dropped into the mixture under vigorous stirring, and 6 mL of water was added, and stirred for 4 h in a light-proof environment at 40 ° C to obtain a phycoerythrin nano-selenium particle dispersion. Finally, the phycoerythrin nano-selenium particle dispersion was dialyzed with deionized water through a 3500 Da dialysis bag for 48 h, centrifuged, and the precipitate was collected, washed, and freeze-dried to obtain a PE-SeNPs complex.

[0034] Example 2 Preparation method of phycoerythrin-nanoselenium complex

[0035] 0.5 mL of 5 mg / mL phycoerythrin solution and 2.5 mL of 0.5 mM sodium selenite solution were mixed under magnetic stirring to obtain a mixture. Then 2.5 mL of freshly prepared 80 mM glutathione solution was dropped into the mixture under vigorous stirring, and 4.5 mL of water was added, and stirred for 4 h in a light-proof environment at 40 ° C to obtain a phycoerythrin nano-selenium particle dispersion. Finally, the phycoerythrin nano-selenium particle dispersion was dialyzed with deionized water through a 3500 Da dialysis bag for 48 h, centrifuged, and the precipitate was collected, washed, and freeze-dried to obtain a PE-SeNPs complex.

[0036] Example 3 Preparation method of phycoerythrin-nanoselenium complex

[0037] 0.5 mL of 5 mg / mL phycoerythrin solution and 1.5 mL of 0.5 mM sodium selenite solution were mixed under magnetic stirring to obtain a mixture. Then 0.5 mL of freshly prepared 80 mM glutathione solution was dropped into the mixture under vigorous stirring, and 7.5 mL of water was added, and stirred for 4 h in a light-proof environment at 40 ° C to obtain a phycoerythrin nano-selenium particle dispersion. Finally, the phycoerythrin nano-selenium particle dispersion was dialyzed with deionized water through a 3500 Da dialysis bag for 48 h, centrifuged, and the precipitate was collected, washed, and freeze-dried to obtain a PE-SeNPs complex.

[0038] Example 4 Preparation method of phycoerythrin-nanoselenium complex

[0039] 0.5 mL of 6 mg / mL phycoerythrin solution and 2 mL of 0.5 mM sodium selenite solution were mixed under magnetic stirring to obtain a mixture. Then 1 mL of freshly prepared 80 mM glutathione solution was dropped into the mixture under vigorous stirring, and 6.5 mL of water was added, and stirred for 4 h in a light-proof environment at 40 ° C to obtain a phycoerythrin nano-selenium particle dispersion. Finally, the phycoerythrin nano-selenium particle dispersion was dialyzed with deionized water through a 3500 Da dialysis bag for 48 h, centrifuged, and the precipitate was collected, washed, and freeze-dried to obtain a PE-SeNPs complex.

[0040] Example 5

[0041] A plant culture solution was prepared, and the soybean seedlings cultured to the 3 true leaf stage were transferred into the culture solution for hydroponics. Except for the control group (CK), 50 mM NaCl was added to the culture solution for the other experimental groups to implement salt stress, and the relief group was sprayed with phycoerythrin-nanoselenium complex, sodium selenite and phycoerythrin to form a control group, a salt stress group, a relief group sprayed with phycoerythrin, a relief group sprayed with sodium selenite, and a relief group sprayed with the nano foliar spray. After 10 days of hydroponic treatment, multiple photosynthesis and physiological indicators of the soybean seedlings in each group were tested and comprehensively analyzed.

[0042] The performance of the phycoerythrin-nanoselenium complex prepared by the present invention was tested as follows, and the results are as follows:

[0043] Figure 2 This is the transmission electron microscopy characterization result of PE-SeNPs prepared in Example 1. Figure 2 It can be seen that the prepared PE-SeNPs have uniform particle size, good sphericity, an average particle size of about 190 nm, and good dispersibility.

[0044] Figure 3 It is the potential diagram of PE-SeNPs prepared in Example 1. The absolute value of PE-SeNPs Zeta potential is 62.87 mV.

[0045] Figure 4 1 is a diagram of the hydrated particle size of PE-SeNPs prepared in Example 1. Through particle size analysis of PE-SeNPs, it was found that the average hydrated particle size of PE-SeNPs was 274.6 nm.

[0046] Figure 5 ] is an infrared spectrum of PE-SeNPs and PE-SeNPs prepared in Example 1. Figure 5 As shown, phycoerythrin is at 3243.68 cm- 1 and 3067.23cm- 1 The two absorption peaks are related to the pyrrole aromatic ring and carbon-carbon unsaturated bonds of phycoerythrin. In the PE-SeNPs composite, the two absorption peaks still exist, and the peak intensity remains almost unchanged, indicating that the presence of selenium particles does not affect the aromatic structure and unsaturated bonds of phycoerythrin. -1 、1049.57cm -1 and 607.95cm -1 The three absorption peaks disappeared after the formation of PE-SeNPs complex, which may be related to the formation of selenium-oxygen coordination bonds (CO…Se) between selenium and CO in the carboxyl group of phycoerythrin.

[0047] Figure 6 is the UV spectrum of PE-SeNPs prepared in Example 1. Figure 6 It can be seen that the strong absorption of PE-SeNPs at 263nm is the characteristic absorption of nano-selenium.

[0048] In addition, plant experiments were conducted to explore the effects of PE-SeNPs on some physiological and photosynthetic indicators of soybean seedlings under salt stress. The specific results are as follows:

[0049] Figure 7 This is a comparison of three groups of soybean seedlings. It can be seen from the figure that compared with the blank control group and the salt stress group, the soybean seedlings sprayed with PE-SeNPs grew better.

[0050] Figure 8 This is a comparison chart of the root length of soybean seedlings. As can be seen from the figure, compared with spraying PE and sodium selenite, the root length of soybean seedlings sprayed with PE-SeNPs is significantly longer than that of other groups.

[0051] Fig. 9 The figure shows the comparison of the net photosynthetic rate of soybean seedlings. It can be seen from the figure that compared with the spraying of sodium selenite and phycoerythrin alone, spraying PE-SeNPs can increase the net photosynthetic rate (Pn) of soybean seedlings under salt stress, and compared with the blank control group, its net photosynthetic rate increased by 31.47%.

[0052] Fig.10 This is a comparison chart of proline content in soybean seedlings. Fig.10 It can be seen that compared with spraying selenium and phycoerythrin alone, spraying PE-SeNPs can reduce the proline content of soybean seedlings under salt stress. Compared with the blank control group, its proline content decreased by 64.17%.

[0053] In order to better improve the tolerance of soybean seedlings to salt stress, different concentrations of PE-SeNPs were sprayed on the soybean seedlings, and the photosynthetic and physiological indicators of the soybean seedlings were compared.

[0054] from Fig.11 It can be seen that when the concentration of PE-SeNPs is 50 μmol / mL, the net photosynthetic rate of soybean seedlings is the highest, so the optimal spraying concentration of PE-SeNPs is 50 μmol / mL.

[0055] from Fig.12 It can be seen that when the concentration of PE-SeNPs is 50 μmol / mL, the proline content of soybean seedlings is the lowest, so the optimal spraying concentration of PE-SeNPs is 50 μmol / mL.

[0056] The embodiments described above are only preferred embodiments of the present invention and are only used to explain the present invention, not to limit the scope of implementation of the present invention. For those skilled in the art, other implementation methods can certainly be easily made by replacement or modification based on the technical contents disclosed in this specification. Therefore, all changes and improvements made on the principles of the present invention should be included in the scope of the patent application of the present invention.

Claims

1. A method for preparing a phycoerythrin-nanoselenium complex, It is characterized in that The method comprises the following steps: A certain proportion of phycoerythrin solution and sodium selenite solution are respectively mixed under the action of magnetic stirring to obtain a mixture; then an appropriate amount of glutathione solution is dropped into the mixture under vigorous stirring, stirred and fully reacted under light-proof conditions to obtain a phycoerythrin nano-selenium particle dispersion; the dispersion is dialyzed in a light-proof environment, centrifuged, the precipitate is collected, washed, and freeze-dried to obtain a phycoerythrin-nano-selenium complex, namely, a PE-SeNPs complex.

2. The preparation method according to claim 1, It is characterized in that The concentration of the phycoerythrin solution is 1-8 mg / mL, the concentration of the sodium selenite solution is 0.5-3 mM, the concentration of the glutathione solution is 80 mM, the volume ratio of the phycoerythrin solution to the sodium selenite solution is 1:0.5-1:5, and the volume ratio of the mixture to the added glutathione solution is 1:1-6:

1.

3. The preparation method according to claim 1, It is characterized in that The conditions for light-proof dialysis are: dialysis with deionized water in a 3500Da dialysis bag for 48h-50h, a centrifugal speed of 12000-15000r / min, and a time of 5-12min.

4. The preparation method according to claim 1, It is characterized in that The particle size of the PE-SeNPs complex is 20-300 nm.

5. The PE-SeNPs complex prepared according to the preparation method according to any one of claims 1 to 4.

6. Use of the PE-SeNPs complex according to claim 5 as a foliar spray, It is characterized in that When sprayed on the leaves, the concentration of the PE-SeNPs is 40-60 μmol / mL.

7. The use according to claim 6, It is characterized in that The foliar spray can alleviate the salt stress of soybean seedlings and promote photosynthesis.