Fireproof glass fiber reinforced plastic pipeline and preparation method thereof

By combining the fiberglass felt layer, polyester felt layer and fire-resistant outer layer on the fiberglass pipe, and using the combination of hollow glass microbeads and other materials, the problem of poor fire resistance in fire is solved, achieving efficient Fire resistance performance is improved and structural strength is maintained.

CN118977473AInactive Publication Date: 2024-11-19NANJING XINHE COMPOSITES CO LTD +1
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202411408592.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-11-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Traditional fiberglass pipes have poor fire resistance during fire, which is prone to loss of structural strength, resulting in safety hazards. The existing solutions affect appearance and increase weight, and the fire resistance is gradually degraded.

Method used

Adhesives are used to combine glass fiber felt layer, polyester felt layer and refractory outer layer in sequence on the substrate pipe. The adhesive contains hollow glass microbeads, combined with triphenyl phosphate, aluminum hydroxide, zinc borate and other materials, and through specific Ratio and process flow improve fire resistance.

Benefits of technology

It significantly improves the fire resistance of the pipeline, maintains structural strength for a long time during fire, reduces safety hazards, and improves the overall performance of the pipeline by evenly dispersing and enhancing the adhesive performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005077370400000061
    Figure BDA0005077370400000061
  • Figure BDA0005077370400000071
    Figure BDA0005077370400000071
  • Figure HDA0005077370420000011
    Figure HDA0005077370420000011
Patent Text Reader

Abstract

The invention relates to the technical field of fireproof materials, and particularly discloses a fireproof glass fiber reinforced plastic pipeline and a preparation method thereof. A fireproof glass fiber reinforced plastic pipeline comprises a base material pipeline, a glass fiber felt layer is arranged on the base material pipeline, a polyester felt layer is arranged on the glass fiber felt layer, a fireproof outer layer is arranged on the polyester felt layer, and the base material pipeline, the glass fiber felt layer, the polyester felt layer and the fireproof outer layer are connected through an adhesive. The adhesive comprises the following raw materials: resin, water, a curing agent and hollow glass beads. The glass fiber felt layer, the polyester felt layer and the fireproof outer layer are sequentially compounded on the base material pipeline through the adhesive, the hollow glass beads in the adhesive have good flame retardant performance, the fireproof performance of the pipeline is remarkably improved, and when a fire disaster occurs, the pipeline can keep the structural strength for a long time, and potential safety hazards are reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of fireproof materials, and in particular to a fireproof glass fiber reinforced plastic pipe and a preparation method thereof. Background Art

[0002] FRP pipes are widely used in the fields of construction, chemical industry, etc. due to their excellent corrosion resistance and light weight and high strength. However, traditional FRP pipes have poor fire resistance when exposed to fire and are prone to lose structural strength, thus causing safety hazards. Specific solutions of existing technologies: At present, in order to improve the fire resistance of FRP pipes, the conventional practice is to apply fire retardant coatings or wrap fire retardant materials on the outside of the pipes. These methods often affect the appearance of the pipes, increase weight, and the fire resistance may gradually decrease during long-term use. Summary of the invention

[0003] In order to improve the fireproof performance of a pipeline, the present application provides a fireproof fiberglass reinforced plastic pipeline and a preparation method thereof.

[0004] In the first aspect, the present application provides a fireproof glass fiber reinforced plastic pipe, which adopts the following technical solution: A fireproof glass fiber reinforced plastic pipe comprises a base pipe, a glass fiber felt layer is arranged on the base pipe, a polyester felt layer is arranged on the glass fiber felt layer, a fire-resistant outer layer is arranged on the polyester felt layer, and the base pipe, the glass fiber felt layer, the polyester felt layer and the fire-resistant outer layer are connected by an adhesive; the raw materials of the adhesive include resin, water, a curing agent and hollow glass microspheres.

[0005] By adopting the above technical scheme, a glass fiber felt layer, a polyester felt layer and a fire-resistant outer layer are compounded in sequence on the base pipe using adhesive, and the hollow glass microbeads in the adhesive have good flame retardant properties, which significantly improves the fire resistance of the pipe. When encountering a fire, the pipe can maintain its structural strength for a longer period of time, reducing safety hazards.

[0006] In a specific embodiment, the resin includes phenolic resin or MR-7100 resin.

[0007] By adopting the above technical solution, the phenolic resin and MR-7100 resin have a network structure after curing, and the MR-7100 resin has a high content of nitrogen and phosphorus elements, so that the pipeline has excellent heat and fire resistance and outdoor durability.

[0008] In a specific embodiment, the curing agent includes one of 1,4-butyrolactone, benzenesulfonic acid, and RH-7007 curing agent.

[0009] In a specific embodiment, the weight ratio of the resin, water, curing agent and hollow glass microspheres in the adhesive is 100:5:100:10.

[0010] By adopting the above technical solution, the ratio of resin, water, curing agent and hollow glass microspheres is further limited, and the bonding performance of the formed adhesive can be improved.

[0011] In a specific embodiment, the raw materials of the adhesive further include triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talc.

[0012] By adopting the above technical scheme, the fire retardant performance of the adhesive can be further improved by utilizing the combination of triphenyl phosphate, aluminum hydroxide and zinc borate. Talc can make the components in the adhesive evenly dispersed. Wollastonite fiber can increase the strength of the final pipe. Water glass adhesive can further enhance the bonding performance of the adhesive.

[0013] In a specific embodiment, the weight ratio of the resin, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass binder and talc in the adhesive is 100:(3-5):(3-5):(3-5):(1-3):(1-2):(3-4).

[0014] By adopting the above technical scheme, the proportions of resin, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive and talcum powder in the adhesive are further limited, thereby improving the bonding performance and fire resistance of the adhesive.

[0015] In a specific embodiment, the fire-resistant outer layer is a fire-resistant resin layer or a fire-resistant fiber layer.

[0016] In a second aspect, the present application provides a method for preparing a fireproof glass fiber reinforced plastic pipe, which adopts the following technical solution: A method for preparing a fireproof glass fiber reinforced plastic pipe comprises the following steps: Preparation of base material pipe: winding the pipe using the existing winding process, and curing to obtain the base material pipe; Glue preparation: preheat the resin first, add water and stir to mix evenly, then add curing agent, hollow glass microspheres and other additives, stir and mix evenly to obtain adhesive; Felt winding: Add adhesive into the glue dipping tank, pass the glass fiber felt through the glue dipping tank so that the glass fiber felt is soaked with glue, then start winding from one end of the base pipe, overlap half of the width, and wind to the other end to ensure that there are 2 layers of glass fiber felt thickness to form a glass fiber felt layer; pass the polyester felt through the glue dipping tank so that the polyester felt is soaked with glue, then start winding on the glass fiber felt layer from one end of the base pipe, overlap half of the width, and wind to the other end, return and wind back to the starting point with zero overlap to ensure that there are 3 layers of polyester felt thickness to form a polyester felt layer; Preparation of fire-resistant outer layer: a fire-resistant outer layer is provided on the polyester felt layer to obtain a semi-finished product; Curing: Place the semi-finished product in an oven at 60-80°C for curing; Post-curing: Aging the cured semi-finished product in an oven at 120°C for 2 hours to obtain a fire-resistant FRP pipe.

[0017] By adopting the above technical scheme, a base pipe is first prepared, and then a glass fiber felt layer, a polyester felt layer and a fire-resistant outer layer are compounded on the base pipe in sequence using an adhesive, and then cured, and finally post-cured to obtain a fire-resistant fiberglass pipe with good fire resistance.

[0018] In a specific embodiment, in the glue preparation step, the preheating temperature is 45-50°C, and the water is heated to 50°C.

[0019] By adopting the above technical solution, the preheating temperature and the water temperature are further limited, so that the resin and water can be better mixed.

[0020] In a specific implementation scheme, the semi-finished product is first hot-pressed, then placed in an oven for curing at 60° C. for 1 hour, and then heated to 80° C. for curing for 1 hour.

[0021] By adopting the above technical solution, the pipeline is hot-pressed before the curing process, so that the resin mixture is more evenly distributed in the outer material of the pipeline, thereby improving the overall performance of the pipeline.

[0022] In summary, the present application includes at least one of the following beneficial technical effects: 1. In this application, the glass fiber felt layer, the polyester felt layer, and the fire-resistant outer layer are sequentially compounded on the base pipe by using adhesive, and the hollow glass microspheres in the adhesive have good flame retardant properties, which significantly improves the fire resistance of the pipe. When encountering a fire, the pipe can maintain its structural strength for a long time, reducing safety hazards; 2. In the present application, the combination of triphenyl phosphate, aluminum hydroxide and zinc borate can further improve the fireproof performance of the adhesive, talcum powder can make the components in the adhesive disperse evenly, wollastonite fiber can improve the strength of the final pipe, and water glass adhesive can further improve the bonding performance of the adhesive; 3. The method in the present application first prepares a base pipe, then uses an adhesive to compound a glass fiber felt layer, a polyester felt layer and a fire-resistant outer layer on the base pipe in sequence, and then cures it, and finally performs post-curing to obtain a fire-resistant fiberglass pipe with good fire resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a cross-sectional schematic diagram used to illustrate the fireproof fiberglass reinforced plastic pipe in Example 1 of the present application.

[0024] Explanation of the reference numerals: 1. Base material pipe; 2. Glass fiber felt layer; 3. Polyester felt layer; 4. Fire-resistant outer layer. DETAILED DESCRIPTION

[0025] The present application is further described in detail below with reference to the embodiments.

[0026] All raw materials in the examples can be obtained from the market. The glass fiber felt is made of high-silica glass fiber; the phenolic resin is NR9420 phenolic resin provided by Changshu Southeast Plastic Co., Ltd.; and the MR-7100 resin and RH-7007 curing agent are provided by Jiangsu Hao Neng Chemical Co., Ltd. Example

[0027] Example 1 Example 1 provides a fireproof fiberglass pipe.

[0028] Reference Figure 1 A fireproof glass fiber reinforced plastic pipe comprises a base pipe 1, a glass fiber felt layer 2 is arranged on the outer peripheral wall of the base pipe, a polyester felt layer 3 is arranged on the outer peripheral wall of the glass fiber felt layer 2, and a fire-resistant outer layer 4 is arranged on the outer peripheral wall of the polyester felt layer 3.

[0029] Embodiment 1 also provides a method for preparing a fireproof glass fiber reinforced plastic pipe, comprising the following steps: Preparation of the base material pipe 1: winding the pipe using the existing winding process, and curing to obtain the base material pipe 1; Preparation of adhesive: preheat the resin at 47.5°C, add 50°C water and stir to mix evenly, then add curing agent and hollow glass microspheres, stir to mix evenly to obtain adhesive; wherein the weight ratio of resin, water, curing agent and hollow glass microspheres is 100:5:100:10; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; Felt winding: Add adhesive into the glue dipping tank, pass the glass fiber felt through the glue dipping tank so that the glass fiber felt is soaked with glue, then start winding from one end of the base pipe 1, overlap half of the width, and wind to the other end to ensure that there are 2 layers of glass fiber felt, forming a glass fiber felt layer 2; pass the polyester felt through the glue dipping tank so that the polyester felt is soaked with glue, then start winding on the glass fiber felt layer 2 from one end of the base pipe 1, overlap half of the width, and wind to the other end, return and wind back to the starting point with zero overlap to ensure that there are 3 layers of polyester felt, forming a polyester felt layer 3; Preparation of the fire-resistant outer layer 4: a layer of the fire-resistant outer layer 4 is arranged on the polyester felt layer 3 to obtain a semi-finished product; wherein the fire-resistant outer layer 4 is a fire-resistant fiber layer, and basalt winding yarn is selected, and the basalt winding yarn is passed through a glue dipping tank so that the basalt winding yarn is soaked with glue, and a layer of the basalt winding yarn is spirally wound on the polyester felt layer 3 to form the fire-resistant outer layer 4; Curing: Place the semi-finished product in an oven and cure it at 60°C for 1 hour, then heat it up to 80°C and cure it for 1 hour; Post-curing: Aging the cured semi-finished product in an oven at 120°C for 2 hours to obtain a fire-resistant FRP pipe.

[0030] Example 2 The difference between Example 2 and Example 1 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent and hollow glass microspheres are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent and hollow glass microspheres is 100:5:100:10; the resin is phenolic resin; the curing agent is 1,4-butyrolactone; and the remaining steps are consistent with Example 1.

[0031] Example 3 The difference between Example 3 and Example 1 is that the substrate pipe 1 is prepared by winding the pipe using the existing winding process and curing to obtain the substrate pipe 1; Preparation of adhesive: preheat the resin at 47.5°C, add 50°C water and stir to mix evenly, then add curing agent and hollow glass microspheres, stir to mix evenly, and obtain adhesive A; wherein the weight ratio of resin, water, curing agent and hollow glass microspheres is 100:5:100:10; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; take one sixth of adhesive A, add red pigment, the weight ratio of red pigment to resin is 0.2:100, stir to mix evenly, and obtain adhesive B; Felt winding: Add adhesive A to the glue dipping tank, pass the glass fiber felt through the glue dipping tank so that the glass fiber felt is soaked with glue, then start winding from one end of the base pipe 1, overlap half the width, and wind to the other end to ensure that there are 2 layers of glass fiber felt, forming a glass fiber felt layer 2; pass the polyester felt through the glue dipping tank so that the polyester felt is soaked with glue, then start winding on the glass fiber felt layer 2 from one end of the base pipe 1, overlap half the width, and wind to the other end, return and wind back to the starting point with zero overlap to ensure that there are 3 layers of polyester felt, forming a polyester felt layer 3; Preparation of the refractory outer layer 4: a refractory outer layer 4 is arranged on the polyester felt layer 3 to obtain a semi-finished product; wherein the refractory outer layer 4 is a refractory fiber layer, basalt winding yarn is selected, adhesive B is added to the dipping tank, the basalt winding yarn is passed through the dipping tank so that the basalt winding yarn is soaked with the adhesive, and one layer is spirally wound on the polyester felt layer 3 to form a refractory outer layer 4; the remaining steps are consistent with Example 1.

[0032] Example 4 The difference between Example 4 and Example 1 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent, hollow glass microspheres, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent, and hollow glass microspheres is 100:5:100:10:2:2:2:0.5:0.5:2.5; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; and the remaining steps are consistent with Example 1.

[0033] Example 5 The difference between Example 5 and Example 4 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent, hollow glass microspheres, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent, and hollow glass microspheres is 100:5:100:10:3:3:3:1:1:3; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; and the remaining steps are consistent with Example 4.

[0034] Example 6 The difference between Example 6 and Example 4 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent, hollow glass microspheres, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent, and hollow glass microspheres is 100:5:100:10:4:4:4:2:1.5:3.5; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; and the remaining steps are consistent with Example 4.

[0035] Example 7 The difference between Example 7 and Example 4 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent, hollow glass microspheres, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent, and hollow glass microspheres is 100:5:100:10:5:5:5:3:2:4; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; and the remaining steps are consistent with Example 4.

[0036] Example 8 The difference between Example 8 and Example 4 is that, in the preparation of the adhesive, the resin is first preheated at 47.5°C, 50°C water is added and stirred to mix evenly, then a curing agent, hollow glass microspheres, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added, and the mixture is stirred to mix evenly to obtain an adhesive; wherein the weight ratio of the resin, water, curing agent, and hollow glass microspheres is 100:5:100:10:6:6:6:3.5:2.5:5; the resin is MR-7100 resin; the curing agent is RH-7007 curing agent; and the remaining steps are consistent with Example 4.

[0037] Example 9 The difference between Example 9 and Example 6 is that, during curing, the semi-finished product is first hot-pressed, then placed in an oven and cured at 60° C. for 1 hour, and then heated to 80° C. and cured for 1 hour; the remaining steps are consistent with Example 6.

[0038] Comparative Example Comparative Example 1 Comparative Example 1 provides a method for preparing a glass fiber reinforced fireproof foam core, comprising the following steps: The phenolic resin, the flame retardant filler, the emulsifier, the toughening agent and the foaming agent are stirred and mixed uniformly to obtain a slurry; wherein the weight ratio of the phenolic resin, the flame retardant filler, the emulsifier, the toughening agent and the foaming agent is 100:60:5:6:5; the flame retardant filler is aluminum hydroxide; the emulsifier is polysiloxane; the toughening agent is ethylene glycol; and the foaming agent is dichloromethane; The glass fiber felt is impregnated in the slurry with an impregnation rate of 1000%, and then stacked in sequence and placed in a mold for curing and forming to obtain a fireproof foam core material.

[0039] Performance Test Fire resistance test: The refractory materials of each embodiment and comparative example were tested in accordance with IMO A.753 (18) to obtain fire resistance grades, which are divided into L0, L1, L2, L3, L4, and L5. The higher the grade, the better the fire resistance of the material.

[0040] Table 1 Performance test results of products In combination with Example 1 and Comparative Example 1, the fireproof performance of the fireproof glass fiber reinforced plastic pipe in Example 1 is relatively strong. It can be seen that the glass fiber reinforced plastic pipe in the present application uses an adhesive to sequentially compound a glass fiber felt layer 2, a polyester felt layer 3, and a fire-resistant outer layer 4 on a base pipe 1, and the hollow glass microbeads in the adhesive have good flame retardant properties. The combination of the glass fiber felt layer 2, the polyester felt layer 3, and the fire-resistant outer layer 4 improves the fireproof performance of the final pipe.

[0041] In combination with Example 1 and Example 2, the fireproof performance of the fireproof glass fiber reinforced plastic pipes in Example 1 and Example 2 is good. It can be seen that when preparing the adhesive, the resin is phenolic resin and the curing agent is 1,4-butyrolactone. The final pipe also has strong fireproof performance.

[0042] Combining Example 1 and Example 3, the fireproof performance of the fireproof glass fiber reinforced plastic pipes in Example 1 and Example 3 is good. It can be seen that when preparing the fire-resistant outer layer 4, adding red pigment to the adhesive can improve the appearance of the final pipe, but has little effect on the fireproof performance of the pipe.

[0043] Combining Example 1 and Example 4, the fireproof performance of the fireproof glass fiber reinforced plastic pipe in Example 4 is relatively strong. It can be seen that when preparing the adhesive, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder are added to the raw materials. The talcum powder can make the components in the adhesive evenly dispersed, the wollastonite fiber can improve the strength of the final pipe, and the water glass adhesive enhances the bonding performance of the adhesive. The combination of triphenyl phosphate, aluminum hydroxide, and zinc borate can further improve the fireproof performance of the obtained pipe.

[0044] Combined with Examples 4-8, the fireproof glass fiber reinforced plastic pipes in Examples 5-7 have stronger fireproof properties. It can be seen that when preparing the adhesive, the ratio of triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive, and talcum powder is preferably (3-5): (3-5): (3-5): (1-3): (1-2): (3-4), and the fireproof properties of the pipes finally obtained are stronger.

[0045] Combining Example 6 and Example 9, the fireproof performance of the fireproof glass fiber reinforced plastic pipes in Example 6 and Example 9 is good. It can be seen that before the semi-finished product is cured, it is first hot-pressed to make the adhesive more evenly distributed in the outer material of the pipe, which can improve the overall performance of the pipe.

[0046] This specific embodiment is merely an explanation of the present application and is not a limitation of the present application. After reading this specification, those skilled in the art may make modifications to the present embodiment without any creative contribution as needed, but such modifications are protected by the patent law as long as they are within the scope of the claims of the present application.

Claims

1. A fireproof glass fiber reinforced plastic pipe, characterized by: The invention comprises a base material pipe (1), a glass fiber felt layer (2) being arranged on the base material pipe (1), a polyester felt layer (3) being arranged on the glass fiber felt layer (2), a fire-resistant outer layer (4) being arranged on the polyester felt layer (3), and the base material pipe (1), the glass fiber felt layer (2), the polyester felt layer (3), and the fire-resistant outer layer (4) being connected by an adhesive; the raw materials of the adhesive include resin, water, a curing agent, and hollow glass microspheres.

2. The fireproof glass fiber reinforced plastic pipe according to claim 1, characterized in that: The resin includes phenolic resin or MR-7100 resin.

3. The fireproof glass fiber reinforced plastic pipe according to claim 2, characterized in that: The curing agent includes one of 1,4-butyrolactone, benzenesulfonic acid and RH-7007 curing agent.

4. The fireproof glass fiber reinforced plastic pipe according to claim 3, characterized in that: The weight ratio of the resin, water, curing agent and hollow glass microspheres in the adhesive is 100:5:100:

10.

5. The fireproof glass fiber reinforced plastic pipe according to claim 1, characterized in that: The raw materials of the adhesive further include triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive and talcum powder.

6. The fireproof glass fiber reinforced plastic pipe according to claim 5, characterized in that: The weight ratio of the resin, triphenyl phosphate, aluminum hydroxide, zinc borate, wollastonite fiber, water glass adhesive and talcum powder in the adhesive is 100: (3-5): (3-5): (3-5): (1-3): (1-2): (3-4).

7. The fireproof glass fiber reinforced plastic pipe according to claim 1, characterized in that: The fire-resistant outer layer (4) is a fire-resistant resin layer or a fire-resistant fiber layer.

8. A method for preparing a fireproof glass fiber reinforced plastic pipe according to any one of claims 1 to 7, characterized in that: The following steps are involved: Preparation of the base material pipe (1): winding the pipe using an existing winding process, and curing to obtain the base material pipe (1); Glue preparation: preheat the resin first, add water and stir to mix evenly, then add curing agent, hollow glass microspheres and other additives, stir and mix evenly to obtain adhesive; Felt winding: adding adhesive to a dipping tank, passing a glass fiber felt through the dipping tank so that the glass fiber felt is soaked in the adhesive, then winding it from one end of the base material pipe (1), overlapping half the width, winding it to the other end, ensuring that there are two layers of glass fiber felt, and forming a glass fiber felt layer (2); passing a polyester felt through a dipping tank so that the polyester felt is soaked in the adhesive, then winding it from one end of the base material pipe (1) on the glass fiber felt layer (2), overlapping half the width, winding it to the other end, returning and winding it back to the starting point with zero overlap, ensuring that there are three layers of polyester felt, and forming a polyester felt layer (3); Preparation of the fire-resistant outer layer (4): a fire-resistant outer layer (4) is provided on the polyester felt layer (3) to obtain a semi-finished product; Curing: Place the semi-finished product in an oven at 60-80°C for curing; Post-curing: Aging the cured semi-finished product in an oven at 120°C for 2 hours to obtain a fire-resistant FRP pipe.

9. The method for preparing a fireproof glass fiber reinforced plastic pipe according to claim 8, characterized in that: In the glue preparation step, the preheating temperature is 45-50°C, and the water is heated to 50°C.

10. The method for preparing a fireproof glass fiber reinforced plastic pipe according to claim 8, characterized in that: The curing step is: hot pressing the semi-finished product first, then curing it in an oven at 60° C. for 1 hour, and then heating it to 80° C. for curing for 1 hour.

Citation Information

Patent Citations

  • Fireproof flame-retardant resin composition and application thereof

    CN104262905A

  • High-strength glass fiber-reinforced plastic pipeline and production method thereof

    CN104405962A

  • Fireproof corrosion resistant physicochemical panel special for laboratory table top

    CN106009515A

  • Fireproof glass steel pipe

    CN106885059A

  • Rectangular winding glass fiber reinforced plastic

    CN110605873A