Novel single ion conductor polymer electrolyte and preparation method thereof

By using lithium phosphorus sulfonimide single-ion conductor polymer electrolyte material in lithium-ion batteries, the safety hazards caused by low lithium ion migration number of solid electrolyte are solved, and higher lithium ion migration number and stronger Cycle stability significantly improves the safety performance of lithium-ion batteries.

CN118978626AInactive Publication Date: 2024-11-19UNIV OF ELECTRONICS SCI & TECH OF CHINA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411165699.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-19
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Due to the low migration number of lithium ions in solid electrolytes, lithium ion batteries lead to large concentration polarization, which is difficult to inhibit the growth of lithium dendrites, which poses safety risks.

Method used

Using lithium phosphorus sulfonylimide single-ion conductor polymer electrolyte material, the lithium phosphorus sulfonylimide group is grafted through PVDF-CTFE as the main chain, which significantly increases the number of lithium ion migrations and combines specific preparation methods, including Multi-step reaction and precipitation process form a high-performance single-ion conductor polymer electrolyte.

Benefits of technology

The lithium ion migration number of lithium ion batteries is significantly improved and the safety performance of the battery is enhanced. The discharge specific capacity of the first circle reaches 125mAh/g, and the cycle stability is stronger, and the performance is better than that of traditional PVDF materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118978626A_ABST
    Figure CN118978626A_ABST
Patent Text Reader

Abstract

The invention provides a single ion conductor polymer electrolyte and a preparation method thereof, polyvinylidene fluoride-trifluorochloroethylene (PVDF-CTFE) is dissolved in a solvent to form a solution, phosphate grafted PVDF copolymer (PVDF-phosphate) is generated through Michaelis-Arbuzov reaction, phosphoric acid grafted modified PVDF (PVDF-phosphoric acid) is obtained after the PVDF-phosphate is hydrolyzed with acid, the PVDF-phosphoric acid modified PVDF is subjected to acid hydrolysis, and the single ion conductor polymer electrolyte is obtained. The preparation method comprises the following steps: carrying out phosphorylation chlorination on PVDF-phosphoric acid by using phosphorus pentachloride to obtain phosphoryl chloride grafted and modified PVDF (PVDF-phosphoryl chloride), carrying out a reaction on the PVDF-phosphoryl chloride and sulfonamide to obtain sulfonyl phosphorimide modified PVDF, and lithiating the sulfonyl phosphorimide modified PVDF by using lithium hydroxide to obtain the sulfonyl phosphorimide lithium modified PVDF copolymer. The lithium sulfonyl phosphoramide modified PVDF copolymer can be used for a single-ion conduction gel electrolyte of a lithium ion battery.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of battery preparation, and in particular to a novel single ion conductor polymer electrolyte and a preparation method thereof. Background Art

[0002] Lithium-ion batteries are rechargeable batteries that are widely used in life due to their high energy density and long cycle life. However, lithium-ion batteries have safety hazards caused by electrolyte leakage or combustion. To solve the safety problem of lithium-ion batteries, one of the current solutions to improve the safety performance of lithium batteries is to develop solid electrolytes. However, solid electrolytes have a low lithium ion migration number (generally less than 0.5), resulting in large concentration polarization, and it is still difficult to inhibit the growth of lithium dendrites, posing a major safety hazard.

[0003] Lithium-ion batteries are rechargeable batteries that are widely used in life due to their high energy density and long cycle life. However, lithium-ion batteries have safety hazards caused by electrolyte leakage or combustion. To solve the safety problem of lithium-ion batteries, one of the current solutions to improve the safety performance of lithium batteries is to develop solid electrolytes. However, solid electrolytes have a low lithium ion migration number (generally less than 0.5), resulting in large concentration polarization, and it is still difficult to inhibit the growth of lithium dendrites, posing a major safety hazard. Summary of the invention

[0004] Lithium-ion batteries are rechargeable batteries that are widely used in life due to their high energy density and long cycle life. However, lithium-ion batteries have safety hazards caused by electrolyte leakage or combustion. To solve the safety problem of lithium-ion batteries, one of the current solutions to improve the safety performance of lithium batteries is to develop solid electrolytes. However, solid electrolytes have a low lithium ion migration number (generally less than 0.5), resulting in large concentration polarization, and it is still difficult to inhibit the growth of lithium dendrites, posing a major safety hazard.

[0005] 1. A method for preparing a single ion conductor solid electrolyte, characterized in that the method comprises the following steps: Step (1), dissolving polyvinylidene fluoride-chlorotrifluoroethylene in a solvent; adding phosphite to the solution obtained in step (1), stirring for a period of time under high temperature conditions under the protection of an inert atmosphere, then cooling the reaction solution, dropping the reaction solution into a poor solvent for precipitation, filtering and washing the precipitate to obtain phosphate-modified PVDF; Step (2), after dissolving the phosphate-modified PVDF, adding acid dropwise into the solution and heating it for a period of time, then pouring the reactant into water for precipitation, filtering, washing, and drying the precipitate to obtain the phosphate-grafted modified PVDF; Step (3), dissolving the PVDF modified by phosphoric acid grafting, adding phosphorus pentachloride to the resulting solution, stirring at a certain temperature for a certain time, then pouring the reactants into a poor solvent for precipitation, filtering, washing, and drying the precipitate to obtain phosphorus oxychloride modified PVDF; Step (4), dissolving the phosphorus oxychloride modified PVDF in a solvent, adding a base, a catalyst, and a sulfonamide, reacting at a certain temperature for a period of time and then dissolving; Step (5), adding the solution obtained in step (5) into a lithium hydroxide aqueous solution to obtain a single ion conductor polymer; Step (6), dissolving the single ion conductor polymer obtained in step (6) in a solvent to prepare a single ion conductor polymer solution; coating the single ion conductor polymer solution on a substrate, and drying to obtain a single ion conductor polymer electrolyte; Step (7), swelling the single ion conductor electrolyte with a plasticizer to obtain a single ion conductor polymer electrolyte.

[0006] Furthermore, the solvents of the prepared various polymer solutions include one or more of N-methylpyrrolidone, N,N-dimethylformamide, N,N-dimethylacetamide, tetrahydrofuran, acetone, cyclohexanone, methyl isobutyl ketone, ethyl acetate, butyl acetate, butyl butyrate, hexyl hexanoate, ethylene glycol methyl ether, and diisobutyl ketone.

[0007] Furthermore, the phosphite used in step (1) is preferably trimethyl phosphite, triethyl phosphite, or triphenyl phosphite, the reaction temperature is 60° C. to 180° C., and the reaction time is 1 h to 96 h.

[0008] Furthermore, the reaction temperature of step (2) is 20°C to 150°C, and the reaction time is 1h-96h.

[0009] Furthermore, the reaction temperature of step (3) is -20°C to 150°C, and the reaction time is 1h-96h.

[0010] Furthermore, the reaction temperature of step (4) is -20°C to 150°C, and the reaction time is 1h-96h. The base used in the reaction is triethylamine, trimethylamine, etc., the catalyst used is preferably dimethylaminopyridine, and the sulfonamide used is preferably trifluorosulfonamide, benzenesulfonamide, substituted benzenesulfonamide.

[0011] Compared with the prior art, the beneficial technical effects of the present invention are: (1) the single-ion conductor polymer electrolyte designed in the present invention selects PVDF-CTFE as the polymer main chain, which has better electron-absorbing ability than PVDF material; (2) the polymer material grafted with lithium phosphosulfonyl imide group has a higher dielectric constant, which can significantly improve the lithium ion migration number. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0013] Figure 1 The present invention is a flow chart of the preparation method of the single ion conductor polymer.

[0014] Figure 2 Comparison of battery cycle curves between Example 1 and Comparative Example 1.

[0015] Figure 3 The figure is a comparison of the battery rate curves of Example 1 and Comparative Example 1. DETAILED DESCRIPTION

[0016] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0017] The phosphorylsulfonyl imide lithium single ion conductor polymer electrolyte material provided by the invention can not only be used for preparing a diaphragm, but also can be used as a binder for preparing a lithium ion battery.

[0018] The phosphorylsulfonyl imide lithium single ion conductor polymer electrolyte material provided by the invention comprises the following weight components: 80-95 parts of PVDF and its copolymer, and 5-20 parts of phosphorylsulfonyl imide lithium salt.

[0019] The following is explained by specific examples, and the examples and comparative examples are as follows:

[0020] Example 1 The preparation of phosphorylsulfonyl imide lithium single ion conductor polymer electrolyte, the specific steps are as follows: (1) Dissolve 10 g PVDF-CTFE in 50 ml NMP and stir until dissolved; (2) 4.79 g of triethyl phosphite was slowly added to the solution obtained in step (1), nitrogen was introduced for protection, and the mixture was stirred at 60° C. for 24 h. After cooling, methanol was added dropwise to precipitate and filtered. After washing and drying, a phosphate-modified PVDF copolymer was obtained; (3) dissolving the phosphate-modified PVDF copolymer obtained in step (2) in 50 ml of NMP, slowly adding 20 ml of hydrochloric acid to the solution and stirring at 60° C. for 2 h, cooling and pouring into water to precipitate and filter, washing and drying to obtain a phosphate-grafted modified PVDF copolymer; (4) dissolving the PVDF copolymer grafted with phosphoric acid obtained in step (3) in 50 ml of NMP, slowly adding 6.01 g of phosphorus pentachloride to the solution obtained in step (3), stirring at below 80° C. for 24 h, cooling, pouring into water for precipitation and filtering, washing and drying to obtain the PVDF copolymer grafted with phosphoric acid; (5) dissolving the chlorophosphate grafted modified PVDF copolymer obtained in step (4) in 50 ml of NMP, dropping 3.84 ml of triethylamine and 3.52 g of dimethylaminopyridine into the solution, stirring at below 80° C. for 1 h, then slowly adding 4.3 g of trifluoromethanesulfonamide into the solution, stirring at below 80° C. for 24 h; (6) preparing a 0.1 mol / L lithium hydroxide aqueous solution, slowly pouring the solution obtained in step (5) into the lithium hydroxide aqueous solution for precipitation, and washing and drying to obtain a phosphorylsulfonyl imide lithium single ion conductor polymer material; (7) Weigh 1 g of lithium phosphosulfonyl imide single ion conductor polymer material and add it to 4 ml of NMP, stirring to dissolve; (8) coating the solution obtained in step (7) on a substrate, and drying to obtain a phosphorylsulfonyl imide single ion conductor polymer electrolyte membrane; (9) Soaking the obtained polymer electrolyte membrane in an organic solvent with a ratio of EC:DMC=1:1 for 24 h; (10) The diaphragm obtained in step (9) is equipped with a button-type lithium battery and corresponding tests are performed.

[0021] Comparative Example 1 (1) Weigh 0.4 g PVDF and add it to 4 ml NMP, stirring to dissolve; (2) coating the solution obtained in step (1) on a substrate, and obtaining a PVDF polymer electrolyte membrane after drying; (3) Soaking the obtained polymer electrolyte membrane in an organic solvent with a ratio of EC:DMC=1:1 for 24 h; (4) Equip the diaphragm obtained in step (3) with a button-type lithium battery and perform corresponding tests.

[0022] Figure 1 It is a flow chart of the preparation method of phosphorylsulfonyl imide lithium single ion conductor polymer material.

[0023] Figure 2Comparing the battery cycle curves of Example 1 and Comparative Example 1, it can be seen that the first-cycle discharge capacity of the phosphorus sulfonyl imide lithium single-ion conductor solid electrolyte invented in this patent reaches 125 mAh / g, and the cycle stability is stronger.

[0024] Figure 3 The battery rate curves of Example 1 and Comparative Example 1 are compared. Compared with the PVDF material, the material of the present invention shows more excellent performance. The battery of Comparative Example 1 has a capacity of about 91 mAh / g at 5C, while the battery of Example 1 has a capacity of about 34 mAh / g at 1C, and has more excellent performance.

[0025] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.

Claims

1. A method for preparing a single ion conductor solid electrolyte, It is characterized in that The method comprises the following steps: Step (1), dissolving polyvinylidene fluoride-chlorotrifluoroethylene in a solvent; adding phosphite to the solution obtained in step (1), stirring for a period of time under high temperature conditions under the protection of an inert atmosphere, then cooling the reaction solution, dropping the reaction solution into a poor solvent for precipitation, filtering and washing the precipitate to obtain phosphate-modified PVDF; Step (2), after dissolving the phosphate-modified PVDF, adding acid dropwise into the solution and heating it for a period of time, then pouring the reactant into water for precipitation, filtering, washing, and drying the precipitate to obtain the phosphate-grafted modified PVDF; Step (3), dissolving the PVDF modified by phosphoric acid grafting, adding phosphorus pentachloride to the resulting solution, stirring at a certain temperature for a certain time, then pouring the reactants into a poor solvent for precipitation, filtering, washing, and drying the precipitate to obtain phosphorus oxychloride modified PVDF; Step (4), dissolving the phosphorus oxychloride modified PVDF in a solvent, adding a base, a catalyst, and a sulfonamide, reacting at a certain temperature for a period of time and then dissolving; Step (5), adding the solution obtained in step (5) into a lithium hydroxide aqueous solution to obtain a single ion conductor polymer; Step (6), dissolving the single ion conductor polymer obtained in step (6) in a solvent to prepare a single ion conductor polymer solution; coating the single ion conductor polymer solution on a substrate, and obtaining a single ion conductor polymer electrolyte after drying.

2. Step (7), swelling the single ion conductor electrolyte with a plasticizer to obtain a single ion conductor polymer electrolyte.

3. The steps of the method according to claim 1 It is characterized in that The solvents for preparing various polymer solutions include one or more of N-methylpyrrolidone, N,N-dimethylformamide, N,N-dimethylacetamide, tetrahydrofuran, acetone, cyclohexanone, methyl isobutyl ketone, ethyl acetate, butyl acetate, butyl butyrate, hexyl hexanoate, ethylene glycol methyl ether, and diisobutyl ketone.

4. The steps of the method according to claim 1 It is characterized in that The solvents for preparing various polymer solutions include one or more of N-methylpyrrolidone, N,N-dimethylformamide, N,N-dimethylacetamide, tetrahydrofuran, acetone, cyclohexanone, methyl isobutyl ketone, ethyl acetate, butyl acetate, butyl butyrate, hexyl hexanoate, ethylene glycol methyl ether, and diisobutyl ketone.

5. According to step (2) of the method of claim 1, It is characterized in that The reaction temperature is 20°C to 150°C, and the reaction time is 1h-96h.

6. According to step (3) of the method of claim 1, It is characterized in that The reaction temperature is -20°C to 150°C, and the reaction time is 1h-96h.

7. According to step (4) of the method of claim 1, It is characterized in that The reaction temperature is -20°C to 150°C, and the reaction time is 1h-96h. The base used in the reaction is triethylamine, trimethylamine, etc., the catalyst used is preferably dimethylaminopyridine, and the sulfonamide used is preferably trifluorosulfonamide, benzenesulfonamide, and substituted benzenesulfonamide.

Citation Information

Patent Citations

  • Phosphorus-based organic flame retardant modified polyvinylidene fluoride composite gel electrolyte as well as preparation method and application thereof

    CN117239225A

  • Method for manufacturing dried yellow corvina using dendropanax morbifera and dendropanax morbifera dried yellow corvina prepared thereby

    KR102552711B1