Electron beam etching method for reducing pixel size of organic light emitting diode
Through the improved electron beam etching method, using electron beam photoresist as a fixed mask plate, simplifies process steps and reduces errors, and reduces the pixel size of the organic light emitting diode to several hundred nanometers, solving the difficulty in reducing the size in the prior art and the problems of large errors, give full play to the advantages of the electron beam etching process.
Patent Information
- Application Number
- CN202411075087.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-07
- Publication Date
- 2024-11-19
AI Technical Summary
The prior art is difficult to reduce the pixel size of the organic light emitting diode to 100 nanometers, and the complex structure introduced by the electron beam etching process limits further reduction, and the shadow effect of the evaporative coating and the positioning error of the fine metal mask make it difficult to finely control the size.
Using improved electron beam etching methods, including cleaning substrates, sputtering conductive anodes, spin coating electron beam photoresist, etching blind hole structures, improving the surface work function of the conductive anode and evaporating organic light-emitting diode levels, using electron beams Photoresist acts as a fixed mask, replacing fine metal masks, simplifying process steps and reducing errors.
The pixel size of the organic light emitting diode is reduced to several hundred nanometers, which gets rid of the shadow effect of the evaporative coating and the positioning error of the fine metal mask plate, fully utilizes the advantages of the minimum line width of the electron beam etching process, and simplifies the process flow.
Smart Images

Figure CN118984637A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of improved preparation technology of organic light emitting diodes, and in particular to an electron beam etching method for reducing the pixel size of organic light emitting diodes. Background Art
[0002] Organic light-emitting diodes are a type of electroluminescent device made of stacked organic thin film structures. As the third generation display technology after cathode ray tube displays and liquid crystal displays, it has become a research hotspot in the display field due to its advantages such as full solid-state, self-luminescence, low power consumption, high contrast, high brightness, high resolution, large area, wide viewing angle, short response time, ultra-thinness, and flexibility. The development of the ultra-high-definition video industry must rely on display technology, and the display of ultra-high-definition video cannot be separated from ultra-high resolution.
[0003] At present, the industry manufactures organic light-emitting diode display screens mostly by evaporation through fine metal masks, that is, using active fine metal masks to separate the evaporated materials to form red, green and blue primary color pixels of organic light-emitting diodes. However, due to the shadow effect of the evaporated coating, the opening size and position accuracy of the fine metal mask, the thermal expansion and contraction of the material, and the positioning error when moving / changing the fine metal mask (all at the micron level), the size of the organic light-emitting diode is difficult to further reduce after it is reduced to a few microns. Although there are documents that reduce the size of organic light-emitting diodes to about one micron through electron beam etching, a more complex structure is introduced, which cannot give full play to the advantage of the small minimum line width of the electron beam etching process, so that the size of the organic light-emitting diode pixel is further reduced to hundreds of nanometers.
[0004] To solve this problem, the journal Science, Vol. 370, No. 6515, pp. 459-463, 2020, used electron beam etching and reactive ion etching processes to reduce the pixel size of organic light-emitting diodes to 1.2 microns × 1.2 microns, achieving ultra-high pixel density (>10,000 pixels per inch), getting rid of the dependence on fine metal masks, and greatly reducing the shadow effect of evaporated coatings. However, because the process introduces nano-patterned metasurface reflectors (Fabry-Perot resonant cavities), it limits the electron beam etching to further reduce the size of organic light-emitting diodes to a certain extent. Summary of the invention
[0005] Purpose of the invention: The present invention provides an electron beam etching method for reducing the pixel size of an organic light emitting diode. Based on the electron beam etching method, the etching process steps are improved, the structure of the organic light emitting diode is simplified, and its pixel size is reduced to hundreds of nanometers.
[0006] Technical solution: The present invention provides an electron beam etching method for reducing the pixel size of an organic light emitting diode, comprising the following steps:
[0007] (1) Cleaning the substrate;
[0008] (2) sputtering a conductive anode onto a substrate;
[0009] (3) spin coating electron beam photoresist onto the conductive anode;
[0010] (4) etching a blind hole structure on the electron beam photoresist;
[0011] (5) Improving the surface work function of the conductive anode on the substrate;
[0012] (6) A hole transport layer, a light-emitting layer and electron transport layer, and a cathode of an organic light-emitting diode are evaporated on the electron beam photoresist to produce an organic light-emitting diode.
[0013] Preferably, the specific steps of step (1) are as follows: first, the substrate is carefully cleaned; then, the substrate is immersed in ultrapure water, acetone, isopropanol, and ultrapure water in turn for 15 minutes to 20 minutes respectively, and an ultrasonic bath is used to clean the substrate during immersion; finally, the substrate is blown dry with compressed gas.
[0014] Preferably, the substrate in step (1) is a transparent insulating substrate.
[0015] Preferably, the conductive anode in step (2) is indium tin oxide ITO.
[0016] Preferably, the specific steps of step (2) are as follows: first, a pre-cleaned substrate is placed in the chamber of a magnetron sputtering coating apparatus, the substrate is placed with the surface to be sputtered facing downward and fixed on a sample tray, and the ITO target material to be sputtered is placed in the sputtering source position of the magnetron sputtering coating apparatus; then, a mechanical pump is started to pre-evacuate the sample chamber to control the vacuum degree in the sample chamber to below 10Pa, and then a molecular pump is started to evacuate the chamber to 1×10 -5 Pa and above; finally, start the AC sputtering source, and the sample tray where the substrate is placed rotates at a speed of 20 rmin -1 , ITO with a thickness of 50nm to 200nm is sputtered on the substrate at a speed of 0.1nm / s as a conductive anode of the organic light-emitting diode. After the conductive anode material ITO is evaporated, high-purity nitrogen is filled into the sample chamber of the magnetron sputtering coater, and the substrate is taken out after reaching atmospheric pressure.
[0017] Preferably, the electron beam photoresist in step (3) is PMMA 950.
[0018] Preferably, the specific steps of step (3) are as follows: firstly, the substrate with the conductive anode is placed on the coating machine, with the side to be spin-coated facing upward, and the mechanical pump is started to firmly adsorb and fix the sample; then, an appropriate amount of PMMA 950 solution is dropped on the substrate with the conductive anode, and the spin-coated film is placed on the coating machine at 500 r / min.-1 Spin coating speed 5s, 5000rmin -1 The rotation speed is spin coated for 45s to 60s to make the PMMA 950 solution form a uniform film on the substrate; finally, the substrate is heated on a heating plate at 180°C for 60s to allow the solvent anisole in the PMMA 950 to fully escape; after PMMA 950 is dried and cured, an electron beam photoresist with a smooth surface and firm adhesion to the substrate is obtained.
[0019] Preferably, the specific steps of step (4) are as follows: first, the sample prepared in step (3) is placed in a chamber of an electron microscope, with the surface to be observed and etched facing upward, fixed on a sample stage, and a mechanical pump and a molecular pump are used to evacuate the sample and focus the electron beam photoresist; then, an electron beam exposure device matched with the electron microscope is used to expose a circular array pattern of different diameters on PMMA 950 with a precisely focused 15kV to 30kV high-energy electron beam; then, high-purity nitrogen is filled into the chamber of the electron microscope, and the sample is taken out after reaching atmospheric pressure; then, the sample after electron beam exposure is immersed in a special developer for 45s to 60s and isopropyl alcohol for 15s to 20s, blown dry with compressed air and heated on a heating table at 100°C for 30s to 60s; finally, a plasma degumming machine is used to reduce the thickness of the electron beam photoresist to 40nm to 80nm, so as to obtain an electron beam photoresist with a specific thickness and a blind hole structure.
[0020] Preferably, the specific steps of step (5) are: first, place the sample with blind hole structure into the chamber of plasma cleaning machine, turn on the mechanical pump to evacuate to a pressure of 350Pa; then inject oxygen to make the pressure 550Pa, turn on the plasma cleaning function and continue cleaning for 300s, fill the chamber of ion cleaning machine with high-purity nitrogen, and take out the sample after reaching atmospheric pressure.
[0021] Preferably, the specific steps of step (6) are as follows: first, the sample obtained in step (5) is placed in the sample chamber of the evaporation coating machine, with the side of the film to be evaporated facing downward, and the sample is fixed on the sample tray, and the hole transport layer material, the light-emitting layer and electron transport layer material, and the cathode material are placed on each evaporation source of the evaporation coating machine; then, the mechanical pump is started to pre-evacuate the sample chamber, and the vacuum degree in the sample chamber is controlled below 10Pa, and then the molecular pump is started to evacuate the chamber to 5×10 -4 Pa and above; finally, the materials on the evaporation source are heated in sequence, and 10nm to 60nm hole transport layer materials, 30nm to 60nm light-emitting layer materials, 10nm to 60nm electron transport layer materials, and 50nm to 200nm cathode materials are deposited in sequence; wherein, the sample tray for placing the substrate rotates at a speed of 20rmin -1 The deposition rates of hole transport layer materials, light emitting layer materials, and electron transport layer materials are all 0.1ns. -1, the deposition rate of cathode material is 1nms -1 After the cathode material is evaporated, high-purity nitrogen is filled into the sample chamber of the evaporation coating machine, and the sample is taken out after reaching atmospheric pressure.
[0022] Beneficial effects: (1) The minimum pixel size of the organic light-emitting diode is reduced to several hundred nanometers;
[0023] (2) By introducing the electron beam lithography process, the current method of manufacturing organic light-emitting diode display screens by evaporation through fine metal masks is abandoned; insulating electron beam photoresist is used as a fixed mask to replace the movable fine metal mask in the traditional method; the errors caused by the shadow effect of evaporation coating, the opening size and position accuracy of the fine metal mask are greatly reduced, and the thermal expansion and contraction of materials and the positioning errors when moving / changing the fine metal mask are avoided, all of which are at the micron level;
[0024] (3) Simplify the complex structure introduced in the electron beam etching process and give full play to the advantage of the small minimum line width of the electron beam etching process. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 is a process flow chart of the present invention;
[0026] Figure 2 A comparison diagram of the improved electron beam lithography process of the present invention, the evaporation process through a fine metal mask, and the classic electron beam lithography process;
[0027] Figure 3 This is a structural diagram of an organic light emitting diode prepared by the present invention;
[0028] Figure 4 This is a diagram of a 16×15 blind hole array with a diameter of 800nm on the electron beam photoresist after being magnified 1000 times under an optical microscope;
[0029] Figure 5 This is a diagram of a 6×3 blind hole array with a diameter of 800 nm on the electron beam photoresist after being magnified 1900 times under a scanning electron microscope;
[0030] Figure 6 This is a diagram of a 3×3 blind hole array with a diameter of 800 nm on an electron beam photoresist after being magnified 3300 times under a scanning electron microscope;
[0031] Figure 7 This is a structural diagram of a single blind hole with a diameter of 800 nm on the electron beam photoresist after being magnified 40,000 times under a scanning electron microscope;
[0032] Figure 8The present invention is a 2×3 blind hole array diagram with a diameter of 800nm on the electron beam photoresist under an atomic force microscope and a thickness diagram of the electron beam photoresist;
[0033] Fig. 9 This is a luminescence image of an organic light emitting diode with a diameter of 800nm and 16×15 pixels under an optical microscope magnified 1000 times;
[0034] Fig.10 This is a spectrum diagram of the organic light emitting diode with a diameter of 800nm and 16×15 pixels in the spectrometer test of the present invention.
[0035] Among them, 2. cathode; 3. light-emitting layer and electron transport layer; 4. hole transport layer; 5. conductive anode; 6. substrate; 7. electron beam photoresist. DETAILED DESCRIPTION
[0036] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.
[0037] Combination Figure 1 and Figure 2 As shown, the present invention provides an electron beam etching method for reducing the pixel size of an organic light emitting diode to hundreds of nanometers, comprising the following steps:
[0038] (1) Cleaning - Cleaning substrate 6:
[0039] The substrate is a transparent insulating substrate with a thickness of about 150 microns, preferably a thin glass substrate ( Figure 3 6).
[0040] First, the substrate 6 is carefully cleaned of oil, dust and other impurities with detergent water. Then, the substrate 6 is immersed in ultrapure water, acetone, isopropanol, and ultrapure water for 15 to 20 minutes respectively, and an ultrasonic bath is used to clean the substrate during immersion. Finally, the substrate 6 is blown dry with compressed gas.
[0041] (2) Sputtering - Sputtering the conductive anode 5 to the substrate 6:
[0042] The conductive anode 5 is made of indium tin oxide (ITO) ( Figure 3 5) in the above.
[0043] First, place the pre-cleaned substrate 6 into the chamber of the magnetron sputtering coating instrument, with the substrate 6 to be sputtered facing downward, and fix it on the sample tray. Place the ITO target material to be sputtered into the sputtering source position of the magnetron sputtering coating instrument. Then, start the mechanical pump to pre-vacuum and control the vacuum degree in the sample chamber to below 10Pa. Then start the molecular pump to evacuate the chamber to 1×10 -5 Pa or higher. Finally, start the AC sputtering source and control the sample tray with the fixed substrate to rotate at 20 rmin.-1 , sputtering ITO with a thickness of 50nm to 200nm on the substrate at a speed of 0.1nm / s as the conductive anode 5 of the organic light-emitting diode. After the conductive anode material ITO is evaporated, high-purity nitrogen is filled into the sample chamber of the magnetron sputtering coating instrument, and the sample is taken out after the sample chamber reaches atmospheric pressure.
[0044] (3) Spin coating - Spin coating the electron beam photoresist 7 onto the conductive anode 5:
[0045] Electron beam photoresist 7 uses PMMA950 ( Figure 3 7), which is an insulator and serves as a fixed mask to replace the movable fine metal mask in the fine metal mask evaporation process.
[0046] First, use tweezers to place the ITO-sputtered substrate 6 on the coating machine, with the side to be coated with photoresist facing up, and start the mechanical pump to firmly adsorb and fix it. Then, use a rubber-tipped dropper to drop an appropriate amount of PMMA950 on the ITO-sputtered substrate 6, and rotate it at 500 r / min. -1 Spin coating speed 5s, 5000rmin -1 The rotation speed is spin-coated for 45s to 60s to form a uniform film of PMMA 950 on the substrate 6. Finally, the substrate 6 is heated on a heating plate at 180°C for 60s to fully release the anisole solvent in the PMMA 950. After the PMMA 950 is dried and solidified, a fixed mask with a flat surface and firmly bonded to the substrate 6 is obtained.
[0047] (4) Etching - etching a blind hole structure on the electron beam photoresist 7: using an electron beam lithography process as a fixed mask on the electron beam photoresist 7, etching the blind hole structure required to isolate each pixel.
[0048] First, place the sample in the chamber of the scanning electron microscope JSM-7900F, place it with the surface to be observed and etched facing up, fix it on the sample stage, and use mechanical pumps and molecular pumps to evacuate the vacuum and focus the electron beam photoresist 7. Then, use the electron beam exposure equipment that matches the scanning electron microscope to expose a circular array pattern with a diameter of 800nm on PMMA950 with a precisely focused 15kV~30kV high-energy electron beam. Subsequently, fill the chamber of the electron microscope JSM-7900F with high-purity nitrogen gas, and take out the sample after reaching atmospheric pressure. Then, immerse the sample after electron beam exposure in a special developer in turn, with a ratio of methyl isobutyl ketone to isopropanol of 1:3, for 45s~60s, and isopropanol for 15s~20s, blow dry with compressed air and heat on a heating table at 100°C for 30s~60s to obtain a fixed mask sample with a blind hole structure. Observe the sample under an optical microscope at a magnification of 1000 times, as shown in Figure 4As shown in the figure, due to the magnification and diffraction limit of the optical microscope, the blind hole structure can be seen as black dots under the optical microscope. In order to see more clearly, the sample with the blind hole structure is put back into the scanning electron microscope for observation. The images magnified 1900 times, 3300 times, and 40000 times are as follows Figure 5 , Figure 6 , Figure 7 As shown in the figure, it can be clearly seen that with the increase of magnification, the circular hole array structure with a diameter of 800nm becomes clearer and clearer. In order to characterize the height of the circular blind hole structure (the thickness of PMMA950), the sample with the blind hole structure is placed under an atomic force microscope for observation, and the image is shown in the figure. Figure 8 As shown. It can be clearly seen that the height of the circular blind hole structure is about 140nm to 150nm. In order to make the sum of the thickness of each organic functional layer and the conductive cathode to be evaporated later greater than the thickness of the fixed mask. Finally, a plasma stripper is used to thin the thickness of the fixed mask to 40nm to 80nm, and a sample with a fixed mask of a specific thickness and a blind hole structure is obtained.
[0049] Note: From Figure 2 By comparing the three methods in the present invention, it can be seen that the improved electron beam lithography process ( Figure 2 (1)→(2)→(3.2)→(4.2)→(5.2)→(6.2)) is different from the process of evaporation through a fine metal mask ( Figure 2 (1)→(2)→(3.1)→(4.1)→(5.1)): In the process of evaporation using a fine metal mask, the gap between the fine metal mask and the substrate is large and movable. The errors caused by the shadow effect, the opening size and position accuracy of the fine metal mask, the thermal expansion and contraction of the material, and the positioning errors when moving / replacing the fine metal mask are all large (all at the micron level). In the improved electron beam lithography process, the fixed mask is tightly combined with the substrate without a gap, which greatly reduces the errors caused by the shadow effect of the evaporation coating, the opening size and position accuracy of the fine metal mask, and avoids the thermal expansion and contraction of the material and the positioning errors when moving / replacing the fine metal mask. Therefore, the pixel size of the organic light-emitting diode can be reduced to several hundred nanometers.
[0050] At the same time, the improved electron beam lithography process of the present invention simplifies the classical electron beam etching process ( Figure 2 The complex structure introduced in (1)→(2)→(3.2)→(4.2)→(5.3)→(6.3)) fully utilizes the advantage of the small minimum line width of electron beam etching process.
[0051] (5) Improving the surface work function of the conductive anode 5 on the substrate:
[0052] First, place the sample with a blind hole structure into the plasma cleaning chamber, and turn on the mechanical pump to pump air to a pressure of 350 Pa. Then, inject oxygen to a pressure of 550 Pa, turn on the plasma cleaning function and continue cleaning for 300 seconds. Fill the chamber of the ion cleaning machine with high-purity nitrogen, and take out the sample after reaching atmospheric pressure.
[0053] (6) Evaporation: The hole transport layer 4, the light-emitting layer and electron transport layer 3 and the cathode 2 of the organic light-emitting diode are evaporated on the substrate 6 to prepare an organic light-emitting diode with a pixel diameter of 800 nm. It should be noted that the sum of the thickness of each organic functional layer and the cathode must be greater than the thickness of the fixed mask.
[0054] First, place the sample in the sample chamber of the evaporation coating machine, with the side to be evaporated facing down, and fix it on the sample tray. Place the hole transport layer 4 material, the light-emitting layer and electron transport layer 3 material, and the cathode 2 material on each evaporation source of the evaporation coating machine. Then, start the mechanical pump to pre-evacuate and control the vacuum degree in the sample chamber to below 10Pa. Then start the molecular pump to evacuate the chamber to 5×10 -4 Pa or higher. Finally, the materials on the evaporation source are heated in sequence, and 10nm to 60nm hole transport layer materials are deposited in sequence ( Figure 3 4) 30nm~60nm light-emitting layer and electron transport layer material ( Figure 3 3) 50nm~200nm cathode material ( Figure 3 2) in the above.
[0055] The sample tray on which the substrate is placed rotates at a speed of 20 rmin. -1 The deposition rates of hole transport layer materials, light emitting layer materials, and electron transport layer materials are all 0.1ns. -1 , the deposition rate of cathode material is 1nms -1 After the conductive cathode material is evaporated, high-purity nitrogen is filled into the sample chamber of the evaporation coating machine, and the substrate is taken out after reaching atmospheric pressure.
[0056] The cathode and anode electrodes of an organic light-emitting diode with a pixel diameter of 800nm are led out with conductive silver paste and copper wire, and the 800nm organic light-emitting diode is immediately tested without packaging:
[0057] 1. Luminescence test: Connect 10V voltage to the two electrodes, and the luminescence image of an organic light-emitting diode with a pixel diameter of 800nm under an optical microscope magnified 1000 times is as follows: Fig. 9 As shown;
[0058] 2. Spectral test: The OLED with a pixel diameter of 800nm was tested under the Ocean Optics QE65pro spectrometer to obtain the following spectrum: Fig.10 shown.
Claims
1. An electron beam etching method for reducing the pixel size of an organic light emitting diode, characterized in that: The following steps are involved: (1) cleaning the substrate (6); (2) sputtering a conductive anode (5) onto a substrate (6); (3) spin coating an electron beam photoresist (7) onto the conductive anode (5); (4) etching a blind hole structure on the electron beam photoresist (7); (5) improving the surface work function of the conductive anode (5) on the substrate; (6) The hole transport layer (4), the light-emitting layer and electron transport layer (3) and the cathode (2) of the organic light-emitting diode are sequentially deposited on the electron beam photoresist (7) to produce the organic light-emitting diode.
2. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The specific steps of step (1) are as follows: first, the substrate (6) is carefully cleaned; then, the substrate (6) is immersed in ultrapure water, acetone, isopropanol, and ultrapure water in turn for 15 minutes to 20 minutes respectively, and an ultrasonic bath is used to clean the substrate (6) during the immersion; finally, the substrate (6) is blown dry with compressed gas.
3. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The substrate (6) in step (1) is a transparent insulating substrate.
4. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: In the step (2), the conductive anode (5) is indium tin oxide (ITO).
5. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 4, characterized in that: The specific steps of step (2) are as follows: first, a pre-cleaned substrate (6) is placed in the chamber of the magnetron sputtering coating apparatus, the substrate (6) is placed with the surface to be sputtered facing downward and fixed on the sample tray, and the ITO target material to be sputtered is placed in the sputtering source position of the magnetron sputtering coating apparatus; then, a mechanical pump is started to pre-evacuate the sample chamber to control the vacuum degree in the sample chamber to below 10Pa, and then a molecular pump is started to evacuate the chamber to 1×10 -5 Pa and above; finally, start the AC sputtering source, and the sample tray where the substrate is placed rotates at a speed of 20 rmin -1 , ITO with a thickness of 50nm to 200nm is sputtered on a substrate (6) at a speed of 0.1nm / s as a conductive anode (5) of an organic light-emitting diode. After the conductive anode material ITO is evaporated, high-purity nitrogen is filled into the sample chamber of the magnetron sputtering coating instrument, and the substrate (6) is taken out after reaching atmospheric pressure.
6. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The electron beam photoresist (7) in step (3) is PMMA 950.
7. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 6, characterized in that: The specific steps of step (3) are as follows: firstly, the substrate with the conductive anode (5) is placed on a coating machine, with the side to be spin-coated facing upwards, and a mechanical pump is started to firmly adsorb and fix the substrate; then, an appropriate amount of PMMA 950 solution is dropped on the substrate with the conductive anode (5), and the coating is continued at 500 r / min. -1 Spin coating speed 5s, 5000rmin -1 The spin coating is performed at a rotation speed of 45s to 60s to make the PMMA950 solution uniformly form a film on the conductive anode (5); finally, the sample is heated on a heating plate at 180°C for 60s to allow the anisole solvent in the PMMA 950 to fully escape; and after the PMMA 950 is dried and solidified, an electron beam photoresist (7) with a smooth surface and firm adhesion to the substrate is obtained.
8. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The specific steps of step (4) are as follows: firstly, the sample prepared in step (3) is placed in a chamber of an electron microscope, the surface to be observed and etched is placed upward, and the sample is fixed on a sample stage, and a mechanical pump and a molecular pump are used to evacuate the sample and focus the electron beam photoresist (7) in sequence; then, an electron beam exposure device matched with the electron microscope is used to expose a circular array pattern of different diameters on PMMA 950 with a precisely focused 15kV to 30kV high-energy electron beam; then, high-purity nitrogen is filled into the chamber of the electron microscope, and the substrate is taken out after reaching atmospheric pressure; then, the substrate after the electron beam exposure is immersed in a special developer for 45s to 60s and isopropyl alcohol for 15s to 20s in sequence, and then dried with compressed air and heated on a heating table at 100° C. for 30s to 60s; finally, a plasma degumming machine is used to reduce the thickness of the electron beam photoresist (7) to 40nm to 80nm, so as to obtain an electron beam photoresist (7) with a specific thickness and a blind hole structure.
9. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The specific steps of step (5) are: first, place the sample with the blind hole structure into the chamber of the plasma cleaning machine, turn on the mechanical pump to evacuate the air to a pressure of 350Pa; then inject oxygen to make the pressure 550Pa, turn on the plasma cleaning function and continue cleaning for 300s, fill the chamber of the ion cleaning machine with high-purity nitrogen, and take out the sample after reaching atmospheric pressure.
10. The electron beam etching method for reducing the pixel size of an organic light emitting diode according to claim 1, characterized in that: The specific steps of step (6) are as follows: first, the sample obtained in step (5) is placed in the sample chamber of the evaporation coating machine, with the side to be evaporated facing downward, and the sample is fixed on the sample tray, and the hole transport layer (4) material, the light-emitting layer and electron transport layer (3) material, and the cathode (2) material are placed on each evaporation source of the evaporation coating machine; then, a mechanical pump is started to pre-evacuate the sample chamber to control the vacuum degree in the sample chamber to below 10Pa, and then a molecular pump is started to evacuate the chamber to 5×10 -4 Pa and above; finally, heating the materials on the evaporation source in sequence, and depositing 10nm to 60nm hole transport layer (4) material, 30nm to 60nm light-emitting layer material, 10nm to 60nm electron transport layer material, and 50nm to 200nm cathode (2) material in sequence; after the cathode (2) material is evaporated, high-purity nitrogen is filled into the sample chamber of the evaporation coating machine, and the sample is taken out after reaching atmospheric pressure.