Tundish and processing method thereof

By using anti-erosion-proof refractory material plates on both sides of the splash-proof barrel of the tundra and filling them with high-temperature resistant materials, the problem of frequent maintenance of anti-erosion coatings in continuous casting operations is solved, and the resistance of the tundra structure is improved Erosion performance and production efficiency.

CN118989305APending Publication Date: 2024-11-22SHANGHAI BAOSTEEL METALLURGICAL CONSTRUCTION CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310549793.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-16
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing tundra structure cannot adapt to long-term continuous casting operations, resulting in frequent maintenance of anti-erosion coatings, especially when silicon steel smelting, the melting erosion speed is increased due to the use of desulfurization agents, which affects the steelmaking production efficiency.

Method used

Anti-erosion-reinforced refractory material plates are used to replace the traditional anti-erosion coating, and combine high-temperature resistant materials to fill the gap between the splash-proof barrel and the material plate to form a tundra structure with stronger corrosion resistance.

Benefits of technology

The tundra's corrosion resistance to molten steel is improved, so that it can adapt to long-term continuous casting operations, reduce maintenance needs, and ensure the quality and production efficiency of the tundra.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118989305A_ABST
    Figure CN118989305A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of ferrous metallurgy, in particular to a tundish. The tundish comprises a tundish main body and a splash-proof barrel, the tundish main body is of a groove body structure with an opening in the top, the splash-proof barrel is arranged at the groove bottom of the tundish main body, the tundish further comprises anti-erosion reinforced refractory material plates, and the two anti-erosion reinforced refractory material plates are laid on the two inner side walls, at the splash-proof barrel, of the tundish main body respectively. And anti-erosion coatings are laid on other inner walls of the tundish main body. According to the tundish, anti-erosion materials close to the two side walls of the splash-proof barrel are replaced with the anti-erosion reinforced refractory material plates from traditional anti-erosion coatings, and the anti-erosion infiltration capacity of the dense anti-erosion reinforced refractory material plates is higher than that of the anti-erosion coatings, so that the anti-erosion reinforced refractory material plates make contact with molten steel firstly, and the anti-erosion reinforced refractory material plates make contact with the molten steel; the anti-erosion performance of the part can be improved, and the tundish can adapt to long-time continuous casting operation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of iron and steel metallurgy, and in particular to a tundish and a processing method of the tundish. Background Art

[0002] The tundish is a transition container located between the ladle and the crystallizer. In the continuous casting process, the tundish is used to divert the molten steel from the ladle to each crystallizer. In tundish metallurgy, the tundish is the intermediate link in the steelmaking production process and the connection point from intermittent operation to continuous operation. In addition, the tundish also has important functions such as pressure reduction, flow stabilization, impurity removal, steel storage, diversion, and protection of casting.

[0003] In order to prevent erosion and penetration by molten steel, the existing tundish is coated with a high-temperature resistant anti-corrosion coating on the inner surface. The two side walls of the tundish close to the splash-proof barrel will contact the molten steel before other areas of the inner surface when the molten steel is injected into the tundish, and are therefore most severely eroded and penetrated by the molten steel. Molten steel seepage often occurs on the two side walls of the tundish close to the splash-proof barrel.

[0004] With the promotion and application of converter slag splashing protection technology, various high-grade, fine and advanced steels can be smelted and produced. However, since the existing tundish structure cannot adapt to long-term continuous casting operations, the anti-corrosion coating of the tundish needs to be repaired after each continuous casting operation, which greatly restricts the efficiency of steelmaking production. Especially when smelting silicon steel with high-grade, fine and advanced materials, the use of a large amount of desulfurizer increases the salinity of the slag, further aggravates the melting and erosion rate of the anti-corrosion coating of the tundish, and significantly increases the maintenance workload of the tundish. Summary of the invention

[0005] In order to solve the above technical problems, the present invention provides a tundish that can adapt to long-term continuous casting operations.

[0006] The present invention adopts the following technical solution:

[0007] The present invention provides a tundish, comprising a tundish main body and a splash-proof barrel. The tundish main body is a trough structure with an opening at the top, the splash-proof barrel is arranged at the bottom of the trough of the tundish main body, and also comprises anti-erosion reinforced refractory material plates. Two anti-erosion reinforced refractory material plates are respectively laid on the two inner side walls of the tundish main body at the position of the splash-proof barrel, and anti-erosion coatings are laid on the other inner walls of the tundish main body.

[0008] Preferably, it also includes an edge flange, which is used to fix the tundish body. The tundish body is sleeved in the edge flange, and the upper edge of the anti-corrosion reinforced refractory material plate is spaced apart from the edge flange.

[0009] Preferably, a filling block is further included, the lower edge of the anti-erosion reinforced refractory material plate is lower than the top of the splash-proof bucket, and the filling block is arranged in the interval space between the lower edge of the anti-erosion reinforced refractory material plate and the splash-proof bucket.

[0010] Preferably, the tundish body is an inverted trapezoidal trough body, the anti-erosion reinforced refractory material plate is a trapezoidal plate, and the upper edge of the anti-erosion reinforced refractory material plate is longer than the lower edge.

[0011] Preferably, the thickness of the erosion-resistant reinforced refractory material plate gradually increases from the lower edge to the upper edge.

[0012] Preferably, the upper edge of the anti-erosion reinforced refractory material plate is provided with a lifting lug.

[0013] Preferably, it further comprises a partition plate, which is vertically arranged on the inner bottom wall of the tundish body.

[0014] The present invention also provides a method for processing a tundish as described in any one of the above items, comprising the following steps:

[0015] S1: Install the splash-proof barrel at the bottom of the trough of the tundish body, and reserve installation space for installing the anti-erosion reinforced refractory material plate on the two inner side walls of the tundish body at the splash-proof barrel position;

[0016] S2: Applying a coating material on the inner wall of the tundish body except the installation space to form an anti-corrosion coating;

[0017] S3: installing two anti-erosion reinforced refractory plates in the installation spaces on the two inner side walls of the tundish body respectively;

[0018] S4: Fill the peripheral gap of the anti-erosion reinforced refractory material plate and the interval space between the anti-erosion reinforced refractory material plate and the splash-proof barrel with high-temperature resistant materials.

[0019] Preferably, the upper edge and the gaps on both sides of the anti-erosion reinforced refractory material plate are filled with coating material, and the interval space between the lower edge of the anti-erosion reinforced refractory material plate and the splash bucket is filled with seat brick ramming material or clay bricks.

[0020] Preferably, the thickness of the upper edge and both side edges of the anti-erosion reinforced refractory material plate is consistent with the thickness of the anti-erosion coatings they are in contact with.

[0021] Compared with the prior art, the present invention has the following beneficial effects:

[0022] The tundish of the present invention replaces the anti-corrosion materials on the two side walls close to the splash-proof barrel from traditional anti-corrosion coatings with anti-corrosion reinforced refractory plates. Since the dense anti-corrosion reinforced refractory plates have stronger anti-corrosion penetration ability than the anti-corrosion coating, the anti-corrosion reinforced refractory plates first come into contact with the molten steel, which is beneficial to improving the anti-corrosion performance of this part, so that the tundish can adapt to long-term continuous casting operations.

[0023] The tundish processed by the tundish processing method of the present invention has the outer peripheral gap of the anti-erosion reinforced refractory plate and the interval space between the anti-erosion reinforced refractory plate and the splash-proof barrel filled with high-temperature resistant materials. The molten steel in the tundish cannot penetrate into the working layer bricks of the tundish body through the gaps around the anti-erosion reinforced refractory plate, so the quality of the tundish is guaranteed. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1 It is a schematic diagram of the three-dimensional structure of the tundish in an embodiment of the present invention.

[0025] Figure 2 It is a schematic diagram of the cross-sectional structure of the tundish in an embodiment of the present invention.

[0026] Figure 3 It is a schematic diagram of the top view structure of the tundish in an embodiment of the present invention.

[0027] Figure 4 It is a front view of the anti-erosion reinforced refractory plate on the tundish in an embodiment of the present invention.

[0028] Figure 5 It is a left view of the anti-erosion reinforced refractory plate on the tundish in an embodiment of the present invention.

[0029] Figure 6 It is a top view of the anti-erosion reinforced refractory plate on the tundish after the lifting ears are removed in an embodiment of the present invention.

[0030] The reference numerals are described as follows:

[0031] 1. Tundish body

[0032] 2. Splash-proof bucket

[0033] 3. Anti-corrosion reinforced refractory board

[0034] 4. Anti-corrosion coating

[0035] 5. Flange

[0036] 6. Filling Blocks

[0037] 7. Lifting lugs

[0038] 8. Divider DETAILED DESCRIPTION

[0039] The specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings. These embodiments are only used to illustrate the present invention, but not to limit the present invention.

[0040] In the description of the present invention, it should be noted that the terms "center", "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.

[0041] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0042] Furthermore, in the description of the present invention, unless otherwise specified, “plurality” means two or more.

[0043] like Figures 1 to 6 FIG. 1 is an embodiment of the intermediate package of the present invention.

[0044] See also Figures 1 to 3 The present embodiment provides a tundish, comprising a tundish body 1 and a splash-proof bucket 2. The tundish body 1 is a trough structure with an open top. The splash-proof bucket 2 is arranged at the bottom of the trough of the tundish body 1. It also includes anti-erosion reinforced refractory material plates 3. Two anti-erosion reinforced refractory material plates 3 are respectively laid on the two inner side walls of the tundish body 1 at the position of the splash-proof bucket 2, and an anti-erosion coating 4 is laid on the other inner walls of the tundish body 1.

[0045] Molten steel seepage often occurs on the two side walls of the tundish close to the splash-proof barrel 2. The tundish of this embodiment replaces the anti-corrosion material on the two side walls close to the splash-proof barrel 2 from the traditional anti-corrosion coating 4 with the anti-corrosion reinforced refractory plate 3. Since the dense anti-corrosion reinforced refractory plate 3 has stronger anti-corrosion penetration ability than the anti-corrosion coating 4, the anti-corrosion reinforced refractory plate 3 first contacts with the molten steel, which is beneficial to improving the anti-corrosion performance of this part, so that the tundish can adapt to long-term continuous casting operations.

[0046] Preferably, in this embodiment, the anti-erosion reinforced refractory material plate 3 is a magnesia refractory material, the oxidized magnesium content of which is greater than 80% and the bulk density is greater than 2.75 g / cm 3 Magnesium refractory materials have high refractoriness and good corrosion resistance to iron oxides and alkaline slag. With their good heat resistance, they are conducive to ensuring long-term continuous casting operations in the tundish.

[0047] Preferably, see Figures 1 to 3 The tundish of this embodiment further includes a flange 5 for fixing the tundish body 1. The tundish body 1 is sleeved in the flange 5, and the upper edge of the anti-erosion and reinforced refractory plate 3 is spaced from the flange 5. Since the anti-erosion and reinforced refractory plate 3 is in direct contact with the molten steel in the tundish and has a high temperature, the upper edge of the anti-erosion and reinforced refractory plate 3 is spaced from the flange 5, which can prevent the flange 5 from being damaged by heat conduction; at the same time, it can also avoid unnecessary waste caused by the excessive area of ​​the anti-erosion and reinforced refractory plate 3.

[0048] Specifically, in this embodiment, the spacing distance between the anti-corrosion reinforced refractory material plate 3 and the edge flange 5 is 190 mm.

[0049] Preferably, see Figure 2 The tundish of this embodiment further includes a filling block 6. The lower edge of the anti-erosion reinforced refractory plate 3 is lower than the top of the splash bucket 2. The filling block 6 is arranged in the interval between the lower edge of the anti-erosion reinforced refractory plate 3 and the splash bucket 2. The arrangement of the filling block 6 is conducive to preventing the molten steel from being concentrated in the interval between the lower edge of the anti-erosion reinforced refractory plate 3 and the splash bucket 2, which facilitates the cleaning of the molten steel in the tundish.

[0050] Preferably, see Figure 1 and Figure 4The tundish body 1 is an inverted trapezoidal trough, the anti-erosion reinforced refractory plate 3 is a trapezoidal plate, and the upper edge of the anti-erosion reinforced refractory plate 3 is longer than the lower edge. The inverted trapezoidal trough structure of the tundish is conducive to the rapid transfer of molten steel from the ladle to the tundish, and since the erosion degree of the inner side wall of the tundish closer to the top opening is higher, the trapezoidal structure of the anti-erosion reinforced refractory plate 3 can, on the one hand, ensure the protection of the most easily eroded position on the two side walls of the tundish close to the splash bucket 2, and on the other hand, it can also reduce the cost by reasonably reducing its own size.

[0051] Preferably, see Figure 5 The thickness of the anti-erosion reinforced refractory material plate 3 gradually increases from the lower edge to the upper edge. Similarly, the thickness of the anti-erosion reinforced refractory material plate 3 is set in this way to reduce costs without affecting the protection effect of the inner wall of the tundish.

[0052] Preferably, see Figure 4 and Figure 5 The upper edge of the anti-erosion reinforced refractory material plate 3 is provided with a lifting lug 7. The provision of the lifting lug 7 can facilitate the lifting and assembly and disassembly of the anti-erosion reinforced refractory material plate 3.

[0053] Preferably, see Figure 1 The tundish of this embodiment further includes a partition plate 8, which is vertically arranged on the inner bottom wall of the tundish body 1. The partition plate 8 can block the molten steel in the tundish, thereby adjusting the flow direction and movement trend of the molten steel, and can also achieve the purpose of blocking slag and purifying the molten steel.

[0054] This embodiment also provides a method for processing a tundish as described in any one of the above items, comprising the following steps:

[0055] S1: Install the splash-proof bucket 2 at the bottom of the tundish body 1, and reserve installation space for installing the anti-erosion reinforced refractory material plate 3 on the two inner side walls of the tundish body 1 at the position of the splash-proof bucket 2;

[0056] S2: applying a coating material on the inner wall of the tundish body 1 except the installation space to form an anti-corrosion coating 4;

[0057] S3: installing two anti-erosion reinforced refractory plates 3 in the installation spaces on the two inner side walls of the tundish body 1 respectively;

[0058] S4: Fill the peripheral gap of the anti-erosion reinforced refractory material plate 3 and the interval space between the anti-erosion reinforced refractory material plate 3 and the splash-proof barrel 2 with high-temperature resistant materials.

[0059] The tundish processed by the tundish processing method of the present embodiment has the outer peripheral gap of the anti-erosion reinforced refractory plate 3 and the interval space between the anti-erosion reinforced refractory plate 3 and the splash-proof barrel 2 filled with high-temperature resistant materials. The molten steel in the tundish cannot penetrate into the working layer bricks of the tundish body 1 through the gaps around the anti-erosion reinforced refractory plate 3, so that the quality of the tundish is guaranteed.

[0060] Preferably, the upper edge and the gaps on both sides of the anti-erosion reinforced refractory material plate 3 are filled with coating material, and the interval space between the lower edge of the anti-erosion reinforced refractory material plate 3 and the splash bucket 2 is filled with seat brick ramming material or clay bricks.

[0061] Preferably, the thickness of the upper edge and both side edges of the anti-erosion reinforced refractory plate 3 is consistent with the thickness of the anti-erosion coating 4 they are in contact with, so as to ensure the anti-erosion effect of the tundish.

[0062] The above is only a preferred embodiment of the present invention. It should be pointed out that for ordinary technicians in this technical field, several improvements and substitutions can be made without departing from the technical principles of the present invention. These improvements and substitutions should also be regarded as the scope of protection of the present invention.

Claims

1. A tundish, comprising a tundish body (1) and a splash-proof bucket (2), wherein the tundish body (1) is a trough structure with an open top, and the splash-proof bucket (2) is arranged at the bottom of the trough of the tundish body (1), characterized in that: It also includes an anti-erosion reinforced refractory material plate (3), two of which are respectively laid on the two inner side walls of the tundish body (1) at the position of the splash bucket (2), and an anti-erosion coating (4) is laid on the other inner walls of the tundish body (1).

2. The tundish according to claim 1, characterized in that: It also includes an edge flange (5), which is used to fix the intermediate ladle body (1). The intermediate ladle body (1) is sleeved in the edge flange (5), and the upper edge of the anti-corrosion reinforced refractory material plate (3) is spaced from the edge flange (5).

3. The tundish according to claim 1, characterized in that: It also includes a filling block (6), the lower edge of the anti-erosion reinforced refractory material plate (3) is lower than the top of the splash-proof bucket (2), and the filling block (6) is arranged in the interval space between the lower edge of the anti-erosion reinforced refractory material plate (3) and the splash-proof bucket (2).

4. The tundish according to claim 3, characterized in that: The tundish body (1) is an inverted trapezoidal trough body, the anti-erosion reinforced refractory material plate (3) is a trapezoidal plate, and the upper edge of the anti-erosion reinforced refractory material plate (3) is longer than the lower edge.

5. The tundish according to claim 4, characterized in that: The thickness of the anti-erosion reinforced refractory material plate (3) gradually increases from the lower edge to the upper edge.

6. The tundish according to claim 4, characterized in that: The upper edge of the anti-erosion reinforced refractory material plate (3) is provided with a lifting lug (7).

7. The tundish according to claim 1, characterized in that: It also comprises a partition plate (8), wherein the partition plate (8) is vertically arranged on the inner bottom wall of the tundish body (1).

8. The method for processing a tundish according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1: Install the splash-proof bucket (2) at the bottom of the trough of the tundish body (1), and reserve installation space for installing the anti-erosion reinforced refractory material plate (3) on the two inner side walls of the tundish body (1) at the position of the splash-proof bucket (2); S2: applying a coating material on the inner wall of the tundish body (1) other than the installation space to form the anti-corrosion coating (4); S3: installing the two anti-erosion reinforced refractory plates (3) in the installation spaces on the two inner side walls of the tundish body (1) respectively; S4: Filling the peripheral gap of the anti-erosion reinforced refractory material plate (3) and the spacing space between the anti-erosion reinforced refractory material plate (3) and the anti-splash bucket (2) with high-temperature resistant materials.

9. The method for processing a tundish according to claim 8, characterized in that: The upper edge and the gaps on both sides of the anti-erosion reinforced refractory material plate (3) are filled with smear material, and the interval space between the lower edge of the anti-erosion reinforced refractory material plate (3) and the splash-proof bucket (2) is filled with a seat brick ramming material or a clay brick.