Automatic welding method for narrow-gap argon tungsten-arc welding of VVER reactor type composite steel main pipeline
Through the automatic welding method of narrow gap tungsten arc welding of VVER stack composite steel main pipeline, the problem of difficult control of the welding quality of the main pipeline of VVER stack nuclear power plant is solved, and an efficient and uniform welding process is achieved, which significantly reduces the labor intensity of the welder and The construction period is also improved, and the internal quality and corrosion resistance of the welds are improved.
Patent Information
- Application Number
- CN202310567162.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-19
- Publication Date
- 2024-11-22
AI Technical Summary
The welding quality of the main pipeline of VVER recharge nuclear power plant is difficult to control stably, and the rework rate is high. Due to the use of special materials, traditional manual welding technology is still used at home and abroad, which has a high labor intensity, which affects the construction efficiency and environment.
The automatic welding method of narrow gap tungsten argon arc welding of VVER stack composite steel main pipes is adopted, including low alloy high-strength steel pipe processing, cleanliness inspection, group test pieces, thermocouple arrangement, induction heating preheating, TOCE welding, and return Thermal treatment and hand arc welding ensure welding quality and efficiency.
It significantly improves the welding qualification rate, reduces the labor intensity of welders, improves welding efficiency, shortens construction period, makes the weld quality more uniform and dense, the internal quality is significantly improved, and the corrosion resistance is excellent.
Smart Images

Figure CN118989529A_ABST
Abstract
Description
Technical Field The invention belongs to the technical field of welding, and in particular relates to a narrow gap tungsten inert gas arc welding automatic welding method for a VVER stack type composite steel main pipeline. Background Art In recent years, the main circuit pipelines of domestic M310, CPR1000, AP1000 and other reactor-type nuclear power plants have been automatically welded one after another, which has achieved remarkable results in improving construction efficiency and quality. However, because the Russian main pipelines used in VVER reactor units are made of special materials, the traditional manual welding process is still used at home and abroad. The labor intensity is high, and the welding quality is affected by many uncertain factors such as the working environment, welding materials and welders, making it difficult to stably control the quality of the weld, resulting in a higher rework rate than automatic welding. In order to improve the working environment of VVER reactor composite steel main pipeline welding, improve welding efficiency and the intrinsic quality of welds, and make full use of the resource advantages of manpower, equipment, technology, experience and other resources currently owned by the nuclear island installation company in automatic welding, on this basis, expand the research and development of main pipeline composite steel automatic welding technology, so that domestic nuclear power main pipelines of various reactor types can be fully automated. It has become a possibility, which can form new breakthroughs in improving welding quality and progress, reducing labor intensity, and improving construction environment; it can make full use of Russian resources, promote Sino-Russian nuclear power plant cooperation in new projects, promote new processes, and promote international cooperation to open a new chapter. Summary of the invention The purpose of the present invention is to provide a narrow gap tungsten inert gas arc welding automatic welding method for VVER stack type composite steel main pipeline, which solves the problem of automatic welding of domestic VVER stack type main pipeline, fills the blank page of domestic automatic welding, reduces the work intensity of construction personnel, improves the construction environment, improves the welding quality, and improves the welding production efficiency. The technical solution to achieve the purpose of the present invention is: A narrow gap tungsten inert gas welding automatic welding method for a VVER stack type composite steel main pipeline, the method comprising the following steps: S1: Provide low alloy high strength steel pipelines, and process the grooves at the ends of single pipelines; S2: Carry out cleanliness inspection and non-destructive testing on the area of the pipeline to be welded; S3: pair of test pieces; S4: Setting up welding equipment tracks; S5: Thermocouple arrangement and induction heating equipment preheating; S6: TOCE welding of the root, TOCE welding of 50-60% of the base layer, and non-destructive testing after welding; S7: Base TOCE filling and covering; S8: Intermediate tempering heat treatment, post-heat treatment, and non-destructive testing of base welds; S9: Final tempering heat treatment and non-destructive testing after final tempering; S10: Multi-layer manual arc welding and non-destructive testing. The length of the single pipe in S1 is not less than 350 mm, and the groove is processed into a double "V" shape. The test pieces are paired in S3, and the maximum allowable misalignment shall not be greater than 0.003S+0.3mm, where S represents the rated thickness of the pipe section. The thermocouple arrangement in S5 is specifically as follows: monitoring areas are set on the upper surface, lower surface and both sides of the pipeline respectively, and two thermocouples, one main and one auxiliary, are set in a single area; the thermocouple is a nickel-chromium-nickel-silicon K-type armored thermocouple, and the measuring temperature range is 0 to 1000°C. The preheating of the induction heating equipment in S5 is specifically as follows: welding must be stopped when the induction heating equipment is running for heating, and the equipment heating is stopped when the interlayer temperature reaches the set temperature value for welding. The temperature during the welding process cannot be lower than the minimum preheating temperature. The root TOCE welding and base layer 50-60% TOCE welding of S6 are specifically as follows: before spot welding, argon is flushed 20 minutes in advance to replace the mixed gas retained in the exhaust pipe; spot welding adopts spot consolidation in the groove, and before welding, the forming of the spot welding area is verified. The welding materials used for spot welding TOCE are consistent with the base TOCE welding materials. The welding parameters adopt the TOCE base parameters. The number of tack welds should be evenly distributed 8-10 points along the circumference, the weld height is 3-6mm, and the length is 80-100mm. During the welding process, the root of the groove should be welded through, and the tack welding parameters (current, argon gas flow, etc.) should be recorded after the welding is completed. The S7 is specifically as follows: after each layer of weld is welded, impurities that affect the welding quality are cleaned up to avoid damaging the surface of the groove parent material and carefully check whether there are surface defects such as cracks and pores on the weld surface. The intermediate tempering heat treatment and post-heat treatment in S8 are specifically as follows: intermediate tempering heat treatment is carried out after the welding of the outer weld is completed, and only the induction heating 5G1T position is subjected to intermediate tempering; during the period from the completion of the welding of the outer weld to the intermediate tempering heat treatment, the temperature of the welded joint shall not be lower than the minimum value of the preheating temperature range; post-heat treatment is carried out after the welding of the outer weld is completed, the defects of the outer weld are removed, the repair welding is completed, and the outer weld is inspected and qualified, and during the period from the completion of welding and the completion of the repair welding to the post-heating, the temperature of the welded joint shall not be lower than the minimum value of the preheating temperature range specified for each. The final tempering heat treatment in S9 is specifically carried out after the outer weld is inspected and qualified or after the defects are corrected and qualified, and the time interval before the final tempering heat treatment is not limited. The S10 is specifically as follows: after the welding of the external base weld is completed and the non-destructive inspection is passed, the inside of the pipeline is welded by manual arc welding; each layer and each weld joint should be staggered by 10-15mm, it is strictly forbidden to strike the arc on the parent material other than the groove, and the thickness of each layer of the weld should not exceed 7mm during welding. The beneficial technical effects of the present invention are: 1. The invention provides a VVER stack composite steel main pipeline narrow gap tungsten inert gas arc welding automatic welding method, which can significantly improve the first-time welding pass rate of the main pipeline, significantly reduce the labor intensity of welders, improve welding efficiency, and shorten the construction period. 2. The invention provides a VVER stack composite steel main pipeline narrow gap tungsten inert gas arc welding automatic welding method, which can achieve more uniform welding heat input, more optimized weld intergranular structure, improved weld density, more significant internal quality, effectively improve strength, and better corrosion resistance. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 This is a schematic diagram of the dimensions of the automatic welding groove of the composite steel main pipeline provided by the present invention. Figure 1 The theoretical values of each point are: A: 2±0.1mm; B: 3±0.2mm; C: 7±0.5mm; D: 5° ±0.5° ; E: 20° ±0.5° ; Figure 2 Thermocouple arrangement diagram provided by the present invention; Figure 3 This is a schematic diagram of laying the heating belt / induction cable provided by the present invention. DETAILED DESCRIPTION The present invention is further described in detail below with reference to the accompanying drawings and embodiments. The invention provides a narrow gap tungsten inert gas arc welding automatic welding method for a VVER type composite steel main pipeline. The welding parameters of the secondary circuit of the M310 unit are used as the welding parameter basis of the external weld of the VVER type main pipeline, and the internal welding parameters of the VVER full-scale simulation test pipeline are used as the welding parameter basis of the VVER type main pipeline composite layer. Research work on new processes, new materials, new heat sources, weld forming and quality is carried out. In particular, the processability test of new processes and new materials is carried out. The welding is not preheated during the welding process, and the processability research of post-heating and heat treatment is finally performed to determine whether the welding quality can meet the various comprehensive performances required by the design, which is a key breakthrough in technical breakthroughs. The key research contents include welding process (including internal and external welding groove dimensions), heat treatment process and equipment application, weld structure, performance characterization, cladding layer corrosion behavior, weld formation mechanism, defect formation mechanism, etc. The invention provides a narrow gap tungsten inert gas arc welding automatic welding method for a VVER stack type composite steel main pipeline, which specifically comprises the following steps: The following steps are involved: S1: Provide 2 low-alloy high-strength steel pipes, and process the grooves at the ends of the single pipes; Select a pipe section with a single test piece length of not less than 350mm, pipe size: φ990×70mm, groove processed into double "V" shape, relevant dimensions such as Figure 1 shown. S2: Carry out cleanliness inspection and non-destructive testing on the area of the pipeline to be welded; In order to eliminate the risk of weld defects caused by defects in the base material, cleanliness inspection and non-destructive testing are carried out on the processed specimens. The inspection requirements are shown in Table 1 below. Table 1: Nondestructive testing requirements S3: pair of test pieces; When pairing the test pieces, the maximum allowable misalignment shall not be greater than 0.003S+0.3mm (S: rated thickness of the pipe section). If there is a deviation in pairing, the inner wall of the pipe can be polished to ensure the misalignment. S4: Setting up welding equipment tracks; The track is set up without affecting the heating requirements. The track setting principle is: the machine head can move freely along the circumference without collision; Since automatic welding equipment has relatively high requirements for the assembly dimensional accuracy of the workpiece and relatively strict requirements for the welding environment conditions, a control area must be set up in the welding equipment operation area to prevent unauthorized personnel from touching it. S5: Thermocouple arrangement and induction heating equipment preheating; A total of 10 thermocouple monitoring points are set up around the pipeline, of which T1, T2, and T3 are monitoring areas on the upper surface of the pipeline, and a single area is set with one main and one secondary thermocouple (one main and one secondary: to prevent the failure of a single thermocouple from causing temperature monitoring failure); T4, T04, T5, and T05 are monitoring areas on both sides of the pipeline, and a single area is also set with one main and one secondary thermocouple; T01, T02, and T03 are monitoring areas on the lower surface of the pipeline, and a single area is also set with one main and one secondary thermocouple, such as Figure 2 shown. The heating tape / induction cable is laid outside the insulation layer on the pipeline surface, such as Figure 3 shown. Use a thermocouple with an automatic recording device for working condition parameters. The thermocouple is a nickel-chromium-nickel-silicon K-type armored thermocouple with a measuring temperature range of 0 to 1000°C. The thermocouple should be calibrated according to regulations, the number and layout of the thermocouple should be correct, and the cold end of the thermocouple must be at room temperature. The thermocouple and the temperature control part should be connected with a compensation wire that matches the thermocouple and clearly marked. In the preheating stage, in order to avoid the impact of induction heating equipment on welding and welding machine, welding must be stopped when the induction heating equipment is running and heating. When the interlayer temperature reaches the set temperature value, the equipment heating can be stopped and welding can be carried out. The temperature during the welding process must not be lower than the preheating minimum temperature of 150°C, and this is repeated; the same is true for the preheating stage of the repair welding. The resistance heating equipment has no effect on welding and can continue to operate for heating and heat preservation; the heating timing in the preheating stage is shown in Table 2 below. Table 2: Heating timing for each heating stage S6: TOCE welding of the root, TOCE welding of 50-60% of the base layer, and non-destructive testing after welding; Complete welding activities at each stage according to the requirements of the welding process data sheet, paying attention to inter-layer inspection and defect treatment; Before spot welding, argon flushing should be performed 20 minutes in advance to replace the mixed gas retained in the gas pipe. Spot welding uses spot fixation inside the groove. Before welding, verify the shape of the spot welding area. If necessary, grind the spot welding arc start or arc end into a gentle slope. The welding materials used for spot welding TOCE are consistent with the TOCE welding materials for base welding. The welding parameters use the TOCE base parameters. The number of positioning welds should be evenly distributed along the circumference at 8 to 10 points, the weld height is 3 to 6 mm, and the length is 80 to 100 mm. During the welding process, the root of the groove should be welded through. After welding, record the positioning welding parameters (current, argon gas flow, etc.); When defects such as pores, tungsten inclusions, and cracks appear during welding, they are removed mechanically, and the area where surface defects have been removed is visually inspected, and the area where cracks have been removed is subjected to liquid penetration inspection. Nondestructive testing is performed on the root TOCE weld after completion and the weld after 50% to 60% welding of the base layer. The inspection requirements are shown in Table 3 below, and the nondestructive testing requirements are shown in Table 1. Table 3: Root TOCE post-welding inspection requirements S7: Base TOCE filling and covering; After each layer of weld is completed, the grinding personnel shall clean the oxide scale or impurities that affect the welding quality. During the grinding process, pay attention to avoid damaging the surface of the groove parent material and carefully check whether there are surface defects such as cracks and pores on the weld surface. If there are, they must be removed before continuing welding. In any case, once cracks appear, the welder should stop welding immediately and report to the welding engineer. Before the cause of the crack is analyzed clearly, suspend welding. S8: Intermediate tempering heat treatment, post-heat treatment, and non-destructive testing of base welds; As shown in Table 2, after the outer weld is welded, intermediate tempering heat treatment is performed, and only the 5G1T position is induction heated for intermediate tempering; during the period from the end of the outer weld welding to the intermediate tempering heat treatment, the temperature of the welded joint shall not be lower than the minimum value of the preheating temperature range (150°C); It is carried out after the outer weld is welded, the outer weld defects are removed, the repair welding is completed, and the inspection is qualified; the post-heating using induction heating is only carried out after the defects are removed and the repair welding is completed. During the period from the end of welding and the completion of the repair welding to the post-heating, the temperature of the welded joint shall not be lower than the minimum value (150℃) of the preheating temperature range specified for each. The completed welds of the base welds are subjected to non-destructive testing. The inspection requirements are shown in Table 3, and the non-destructive testing requirements are shown in Table 1. S9: Final tempering heat treatment and non-destructive testing after final tempering; The final heat treatment is carried out after the external weld inspection is qualified or the defects are corrected. The time interval before the final tempering heat treatment is not restricted. After the final tempering, the weld is subjected to non-destructive testing. The inspection requirements are shown in Table 3 and the non-destructive testing requirements are shown in Table 1. S10: Multi-layer manual arc welding and non-destructive testing. After the external base weld is completed and the non-destructive test is passed, the inside of the pipeline is clad. The welding method uses hand arc, and the welding materials are shown in Table 4 below; Table 4: Specifications for internal welding consumables Each layer and each weld joint should be staggered by 10-15mm. It is strictly forbidden to strike the arc on the parent material other than the groove, and the thickness of each layer (weld pass) of the weld should not exceed 7mm. The interlayer temperature during welding should be controlled within the range specified in the process card. After each layer of weld is completed, the grinding personnel shall clean up the slag and spatter. During the grinding process, pay attention to avoid damaging the surface of the groove parent material and carefully check whether there are surface defects such as cracks, pores, slag inclusions, etc. on the weld surface. If there are, they must be removed before continuing welding. In any case, once cracks appear, the welder shall stop welding immediately and report to the welding engineer. Before the cause of the crack is analyzed clearly, the welding shall be suspended. The welds completed by internal welding are subject to non-destructive testing. The inspection requirements are shown in Table 3 and the non-destructive testing requirements are shown in Table 1. Example 1 Welding process test results stage In the welding of composite steel for nuclear power supply in Russia, the use of automatic welding as a welding method is the first in China. In order to ensure the smooth development of the automatic welding process research and development, test contents were formulated and the automatic welding process research and development was completed in stages. See Table 5 below for details. Table 5: Automatic welding R&D phase test Example 2 Product welding process assessment parameter solidification stage The welding process data sheet (curing parameters) are fixed parameters of the equipment and are generally not changed. The welding process data sheet (variable parameters) are range parameters, which are adaptively adjusted according to the welding quality and weld formation. The adjustment range cannot be infinitely changed and must meet the table parameter range. See Table 6 and Table 7 below for details. Table 6: Welding process data sheet (curing parameters) Table 7: Welding process data sheet (variable parameters) Example 3 Product Welding Process Assessment Heat Treatment Parameters Curing Stage Heat treatment parameters are one of the important parameters in process evaluation and development. The parameters are solidified during process development. Temperature control is carried out according to the table below. The parameter range is shown in Table 8 below. Table 8: Thermal treatment parameters for curing Example 4 Welding Efficiency Analysis Taking the current M310 improved unit as an example, each nuclear power unit has a total of 24 welds, and automatic welding is used to replace the original manual welding. The construction period is reduced from about 170 days to 105 days, and the construction period of the entire nuclear power plant can be shortened by about 35 days.
[0016] Combining the experience of automatic welding of the M310 reactor main pipeline, as well as the specifications, dimensions and construction characteristics of the VVER main pipeline, it is estimated that the single-pass weld can be reduced from the original 38 to 40 days (manual welding) to 27 to 30 days (automatic welding). A single-pass weld can save 8 to 11 days, and the welding period of the main circuit pipeline of a single unit can be saved by about 100 days. This contribution to the nuclear island installation and cold test period has great value during the construction period. Example 5 Welding Quality Analysis There are 507 welding joints of the main pipelines of nuclear power plants such as Ningde, Hongyanhe, Fuqing, Yangjiang, Fangjiashan, Taishan, Fangchenggang, Sanmen, and Haiyang, and the first-time qualified rate of negative film (RT) is 99.68%. The use of automatic welding technology, under the condition of reasonable organization and good equipment and tools, can significantly improve the first-time welding qualified rate of the main pipelines, significantly reduce the labor intensity of welders, improve welding efficiency, and shorten the construction period. The advantage of automatic welding lies not only in the improvement of weld qualification rate, but more importantly, its welding heat input is more uniform, the intergranular structure of the weld is more optimized, the weld density is improved, the internal quality is more significant, and the strength and corrosion resistance are better. The good application practices of many domestic nuclear power plants have once again proved that narrow gap tungsten electrode TOCE welding (N-TIG) has great advantages in welding quality, efficiency and other aspects. As a trend in the future development of nuclear power main pipeline manufacturing and installation, timely conduct welding process tests without preheating at the start of the project can fully reduce the difficulty of welding pairing and assembly during the welding process, provide automation efficiency, and provide test verification. After the expected goals are achieved through domestic and foreign expert meetings and confirmation by the design institute, all test data are submitted to the design institute as the basis for design verification. Combined with the construction regulations of Russian nuclear power plants, the modification of design parameters (mainly the confirmation of grooves, matching of welding materials, heat input parameters (no preheating, layer temperature control parameters), etc.) and improvement are included, and welding process assessment can be carried out. It will also be implemented in VVER reactor nuclear power projects. The future construction of this reactor unit can be combined with the country's "going out" strategy and has strategic significance and market value in improving welding quality and corporate competitiveness. The present invention is described in detail above with reference to the accompanying drawings and embodiments, but the present invention is not limited to the above embodiments, and various changes can be made within the knowledge of ordinary technicians in the field without departing from the purpose of the present invention. The contents not described in detail in the present invention can adopt the existing technology.
Claims
1. A narrow gap tungsten inert gas welding automatic welding method for VVER stack type composite steel main pipeline, characterized in that: The method comprises the following steps: S1: Provide low alloy high strength steel pipelines, and process the grooves at the ends of single pipelines; S2: Carry out cleanliness inspection and non-destructive testing on the area of the pipeline to be welded; S3: pair of test pieces; S4: Setting up welding equipment tracks; S5: Thermocouple arrangement and induction heating equipment preheating; S6: TOCE welding of the root, TOCE welding of 50-60% of the base layer, and non-destructive testing after welding; S7: Base TOCE filling and covering; S8: Intermediate tempering heat treatment, post-heat treatment, and non-destructive testing of base welds; S9: Final tempering heat treatment and non-destructive testing after final tempering; S10: Multi-layer manual arc welding and non-destructive testing.
2. According to claim 1, a VVER stack composite steel main pipeline narrow gap tungsten inert gas welding automatic welding method is characterized in that: The length of the single pipe in S1 is not less than 350 mm, and the groove is processed into a double "V" shape.
3. The narrow gap tungsten inert gas welding automatic welding method for a VVER type composite steel main pipeline according to claim 1 is characterized in that: The test pieces are paired in S3, and the maximum allowable misalignment shall not be greater than 0.003S+0.3mm, where S represents the rated thickness of the pipe section.
4. The narrow gap tungsten inert gas welding automatic welding method for a VVER composite steel main pipeline according to claim 1 is characterized in that: The thermocouple arrangement in S5 is specifically as follows: monitoring areas are set on the upper surface, lower surface and both sides of the pipeline respectively, and two thermocouples, one main and one auxiliary, are set in a single area; the thermocouple is a nickel-chromium-nickel-silicon K-type armored thermocouple, and the measuring temperature range is 0 to 1000°C.
5. The narrow gap tungsten inert gas welding automatic welding method for a VVER type composite steel main pipeline according to claim 1 is characterized in that: The preheating of the induction heating equipment in S5 is specifically as follows: welding must be stopped when the induction heating equipment is running for heating, and the equipment heating is stopped when the interlayer temperature reaches the set temperature value for welding. The temperature during the welding process cannot be lower than the minimum preheating temperature.
6. The narrow gap tungsten inert gas welding automatic welding method for a VVER type composite steel main pipeline according to claim 1 is characterized in that: The root TOCE welding and base layer 50-60% TOCE welding of S6 are specifically as follows: before spot welding, argon is flushed 20 minutes in advance to replace the mixed gas retained in the exhaust pipe; spot welding adopts spot consolidation in the groove, and before welding, the forming of the spot welding area is verified. The welding materials used for spot welding TOCE are consistent with the base TOCE welding materials. The welding parameters adopt the TOCE base parameters. The number of tack welds should be evenly distributed 8-10 points along the circumference, the weld height is 3-6mm, and the length is 80-100mm. During the welding process, the root of the groove should be welded through, and the tack welding parameters (current, argon gas flow, etc.) should be recorded after the welding is completed.
7. The narrow gap tungsten inert gas welding automatic welding method for VVER composite steel main pipeline according to claim 1 is characterized in that: The S7 is specifically as follows: after each layer of weld is welded, impurities that affect the welding quality are cleaned up to avoid damaging the surface of the groove parent material and carefully check whether there are surface defects such as cracks and pores on the weld surface.
8. The narrow gap tungsten inert gas welding automatic welding method for VVER stack composite steel main pipeline according to claim 1 is characterized in that: The intermediate tempering heat treatment and post-heat treatment in S8 are specifically as follows: intermediate tempering heat treatment is carried out after the welding of the outer weld is completed, and only the induction heating 5G1T position is subjected to intermediate tempering; during the period from the completion of the welding of the outer weld to the intermediate tempering heat treatment, the temperature of the welded joint shall not be lower than the minimum value of the preheating temperature range; post-heat treatment is carried out after the welding of the outer weld is completed, the defects of the outer weld are removed, the repair welding is completed, and the outer weld is inspected and qualified, and during the period from the completion of welding and the completion of the repair welding to the post-heating, the temperature of the welded joint shall not be lower than the minimum value of the preheating temperature range specified for each.
9. The narrow gap tungsten inert gas welding automatic welding method for VVER stack composite steel main pipeline according to claim 1 is characterized in that: The final tempering heat treatment in S9 is specifically carried out after the outer weld is inspected and qualified or after the defects are corrected and qualified, and the time interval before the final tempering heat treatment is not limited.
10. The narrow gap tungsten inert gas welding automatic welding method for VVER composite steel main pipeline according to claim 1 is characterized in that: The S10 is specifically as follows: after the welding of the external base weld is completed and the non-destructive inspection is passed, the inside of the pipeline is welded by manual arc welding; each layer and each weld joint should be staggered by 10-15mm, it is strictly forbidden to strike the arc on the parent material other than the groove, and the thickness of each layer of the weld should not exceed 7mm during welding.
Citation Information
Cited By
Field welding manufacturing method for transition section and bent pipe of intermediate pressure cylinder of steam turbine
CN119609578A
On-site welding manufacturing method for the transition section and elbow of a steam turbine intermediate pressure cylinder
CN119609578B