Preparation method of electronic-grade sulfuric acid
By heating oxygen, SO2 is prepared and catalyzed, and adsorption technology of oxidizing agents and modified activated carbon, the problems of high energy consumption and low purity in electronic-grade sulfuric acid production are solved, and high purity and stable sulfuric acid preparation is achieved, which is suitable for industrial production.
Patent Information
- Application Number
- CN202411084849.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
AI Technical Summary
The existing electronic-grade sulfuric acid production methods have problems such as high energy consumption, high cost, difficult to remove trace sulfur dioxide, harmful waste gas to the human body, unfavorable environment, low yield and difficult to obtain high-purity products, which affect product quality and performance.
SO2 is prepared by heating oxygen, and SO3 is obtained through catalytic reaction, and evaporation is carried out twice to improve the purity. Oxidation agent is used to oxidize and modified activated carbon to remove trace impurities, ensuring the high purity and stability of electron-grade sulfuric acid.
It realizes the preparation of high-purity electronic-grade sulfuric acid, reduces energy consumption and costs, reduces pollutant emissions, is suitable for industrial production, and has stable product quality in line with the requirements of the high-end electronic industry.
Abstract
Description
Technical Field
[0001] The present application belongs to the technical field of preparation of electronic-grade sulfuric acid, and specifically relates to a method for preparing electronic-grade sulfuric acid. Background Art
[0002] With the development of the electronic information industry, electronic-grade sulfuric acid is widely used in the electronics industry. Electronic-grade sulfuric acid is an indispensable key basic chemical reagent in the development of microelectronics technology. It is widely used in the assembly and processing of semiconductors and ultra-large-scale integrated circuits. It is mainly used for cleaning and etching of silicon wafers. It can effectively remove impurity particles, inorganic residues and carbon deposits on the wafers. Therefore, electronic-grade sulfuric acid is one of the key basic chemical materials in the modern electronic manufacturing industry.
[0003] At present, the production of electronic-grade sulfuric acid generally adopts the distillation method, but the distillation purification consumes a lot of energy and is costly. Some trace sulfur dioxide is difficult to remove, and the waste gas and acid mist generated are harmful to the human body and are not conducive to environmental protection. The output is low and it is only suitable for small-scale production. It is also difficult to obtain high-purity products, which affects the quality and performance of the final electronic-grade sulfuric acid product, resulting in unstable product quality and failure to meet the strict requirements of the high-end electronics industry for purity and accuracy. Summary of the invention
[0004] In order to effectively improve the above problems, the present application provides a method for preparing electronic grade sulfuric acid, which adopts the following technical solution: A method for preparing electronic grade sulfuric acid comprises the following steps: S1: Preparation of fuming sulfuric acid: Liquid sulfur and heated oxygen are introduced and oxidized to obtain SO2; preheated O2 is then introduced to obtain SO3 through catalytic reaction; SO3 flue gas raw materials are demisted, filtered and absorbed to obtain fuming sulfuric acid; S2: low-temperature evaporation: evaporating the fuming sulfuric acid to evaporate part of the SO3 gas and obtain evaporated fuming sulfuric acid; condensing the SO3 gas into SO3 liquid after demisting, and evaporating it again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: The high-purity SO3 gas is subjected to defoaming, demisting, absorption and cooling treatment to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: oxidation by oxidant, adsorption by modified activated carbon, cooling, degassing, and finally obtaining electronic grade sulfuric acid.
[0005] By adopting the above technical scheme, SO2 is prepared by replacing air with heated oxygen, and SO3 is catalyzed to ensure the yield of the product, and the purity and stability of the product are improved by two evaporations. Then, some trace impurities in high-purity sulfuric acid are first oxidized and removed by an oxidant, and then adsorbed by modified activated carbon. The modified adsorbent has a greater removal capacity for low-concentration SO2, which promotes the adsorption of low-concentration SO2. Finally, the electronic-grade sulfuric acid obtained has a high product purity, effectively controls the content of trace sulfur dioxide impurities in ultra-pure sulfuric acid, is simple to operate, and has stable quality. It meets the requirements of electronic-grade sulfuric acid and is suitable for industrial production.
[0006] In a specific embodiment, the preparation method of the modified activated carbon includes: calcining and carbonizing phenolic resin, and activating it under steam conditions to obtain activated carbon; immersing the activated activated carbon in an oxidizing solution to obtain oxidized activated carbon, then soaking it in alkali solution to obtain alkali-modified activated carbon, and then adding nano-silicon dioxide, stirring and filtering to obtain modified activated carbon.
[0007] By adopting the above technical scheme, phenolic resin is carbonized and then activated under water vapor conditions to generate porous activated carbon, which is then oxidized to increase the number of active sites on the activated carbon. The active surface of the activated carbon is then etched with alkaline solution. On the one hand, the pore size and surface area of the pores on the surface of the activated carbon are increased, so that the activated carbon is loaded with more active components, greatly increasing the reaction contact area of the catalytic active components. On the other hand, the alkali-modified activated carbon has a strong chemical adsorption effect on SO2, and silica has water absorption and moisture-proof protection, providing a large number of adsorption sites through its micropores and surface, making the adsorbent easy to regenerate, and having a larger adsorption capacity for SO2, further enhancing the yield of electronic-grade sulfuric acid.
[0008] In a specific embodiment, the oxidizing solution is an 8%-12% hydrogen peroxide solution, and the immersion time is 5-8 hours.
[0009] By oxidizing activated carbon with hydrogen peroxide, a large number of oxygen-containing functional groups are formed on the surface of the pores inside the activated carbon. These oxygen-containing functional groups are adsorbed on the inner surface of the pores, causing the pores to become narrower, which can better enable the active sites to adsorb SO2. The extent of the increase in adsorption activity is related to modification conditions such as immersion time.
[0010] In a specific implementation scheme, the alkali solution is 0.8-1.2 mol / L KOH, and the soaking time is 12-48 hours.
[0011] In order to improve the ability of activated carbon to adsorb and remove SO2 in the atmosphere, the activated carbon filled in it is usually modified to load potassium hydroxide to specifically remove alkaline substances of SO2, and has a strong adsorption capacity for acidic gases. After the activated carbon is soaked in alkali solution, it adsorbs and fills with the strength of the adsorption potential. The smaller the pore size, the stronger the adsorption potential. After the smaller pores are fully adsorbed, the slightly larger pores are filled. For alkali-modified activated carbon, the influence of its pore structure characteristics on the adsorption characteristics of activated carbon is more obvious. Within a certain range, the longer the soaking time, the greater the degree of modification, the better the activation performance, and the better the adsorption and removal effect of SO2.
[0012] In a specific embodiment, the calcination and carbonization conditions are 600-800° C. and calcination for 2-4 hours.
[0013] By calcining within a certain temperature range, the activated carbon has a larger specific surface area, which can increase the contact area for SO2 reaction and increase the number of reaction sites, which is beneficial for the active components to attack the chain segments of the polymer, promote the cracking of the polymer, and form porous activated carbon.
[0014] In a specific embodiment, the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of the ferric sulfate, vanadium pentoxide, and copper oxide is 1:(3-4):(5-8).
[0015] By taking advantage of the strong electron-accepting ability of iron ions, S(Ⅳ) in SO2 is oxidized to S(Ⅵ) in H2SO4 in the solution, thereby converting gaseous SO2 into liquid sulfuric acid. In theory, metal ions are not consumed, so the purpose of removing SO2 can be achieved. Adding CuO to the oxidant can enhance the adsorption capacity of activated carbon. This is because by adding acidic substances, alkaline substances, transition metal salts and oxides including CuO to activated carbon, other chemical reactions such as coordination adsorption can be used to enhance the adsorption effect of volatile organic compounds and become active sites for adsorbing SO2. While CuO introduces the target gas into the surface of modified activated carbon through copper metal groups, it also acts as a catalytic transition metal. Finally, mixing vanadium pentoxide can enhance the catalytic activity and is used to quickly convert SO2 in S03 into SO3. Not only does it improve the yield and purity of electronic grade sulfuric acid, it can also turn part of the impurity SO2 into a usable resource and reduce the emission of pollutants.
[0016] In a specific embodiment, the mass ratio of the oxidant to the modified activated carbon is 1:(1.2-1.8).
[0017] By first oxidizing it, part of the sulfuric acid is converted into SO3, and the adsorption sites and catalytic adsorption activity of the activated carbon are enhanced. The remaining SO2 that has not been removed is then adsorbed by modified activated carbon, so that the removal of SO2 has a fine removal effect. By adding a certain proportion of oxidant and modified activated carbon, the yield and purity of the electronic grade sulfuric acid are greatly improved.
[0018] In a specific embodiment, the catalytic reaction conditions are: under the catalysis of vanadium pentoxide, the reaction temperature is 450-530°C.
[0019] Using specific vanadium pentoxide as a catalyst, SO2 is converted into SO3 as much as possible, which greatly enhances the conversion efficiency of SO2 and further improves the yield and purity of electronic grade sulfuric acid.
[0020] In summary, the present application includes at least one of the following beneficial technical effects: 1. By adopting the above technical scheme, SO2 is prepared by replacing air with heated oxygen, and SO3 is catalyzed to ensure the yield of the product, and the purity and stability of the product are improved by two evaporations. Then, some trace impurities in high-purity sulfuric acid are first oxidized and removed by an oxidant, and then adsorbed by modified activated carbon. The modified adsorbent has a greater removal capacity for low-concentration SO2, which promotes the adsorption of low-concentration SO2. Finally, the electronic-grade sulfuric acid is obtained with high product purity, and the content of trace sulfur dioxide impurities in ultra-pure sulfuric acid is effectively controlled. The operation is simple, the quality is stable, it meets the requirements of electronic-grade sulfuric acid, and it is suitable for industrial production.
[0021] 2. Iron ions have a strong ability to receive electrons. Ferric sulfate allows S(Ⅳ) to be oxidized to S(Ⅵ) in the solution, thereby converting gaseous SO2 into liquid sulfuric acid. In theory, metal ions are not consumed, so the purpose of removing SO2 can be achieved. Adding CuO to the oxidant can enhance the adsorption capacity of activated carbon. This is because, by adding acidic substances, alkaline substances, transition metal salts and oxides including CuO to activated carbon, other chemical reactions such as coordination adsorption can be used to enhance the adsorption effect of volatile organic compounds and become active sites for adsorbing SO2. While CuO introduces the target gas to the surface of modified activated carbon through the copper metal group, it also acts as a catalytic transition metal. Finally, mixing vanadium pentoxide can enhance the catalytic activity and is used to quickly convert SO2 in S03 into SO3. Not only does it improve the yield and purity of electronic grade sulfuric acid, it can also turn part of the impurity SO2 into a usable resource, reducing the emission of pollutants. DETAILED DESCRIPTION
[0022] In the present application, sulfur: purchased from Luoyang Yuchen Petrochemical Products Co., Ltd.; phenolic resin model: 2130, purchased from Wuxi Jiunai Anticorrosion Materials Co., Ltd.; nano-silicon dioxide purchased from Shijiazhuang Jingsheng Mineral Products Co., Ltd.; 8%-12% hydrogen peroxide is obtained by diluting hydrogen peroxide with water; KOH: purchased from Jinan Zi'an Chemical Co., Ltd.; vanadium pentoxide: purchased from Jinan Jiayang Chemical Co., Ltd.; copper oxide and ferric sulfate: both purchased from Langfang Qianyao Technology Co., Ltd.; other raw materials can be obtained commercially.
[0023] Preparation Example Preparation Example 1 100g of phenolic resin was calcined until carbonized at a temperature of 600°C for 2h to obtain carbonized particles; the carbonized particles were placed in a carbonization furnace and activated for 1h under water vapor at 600°C to obtain activated activated carbon; the activated activated carbon was immersed in a hydrogen peroxide solution with a concentration of 0.8% for 5h to obtain oxidized activated carbon; 20g of oxidized activated carbon was immersed in 100mL of 0.8mol / L sodium hydroxide solution for 12h, filtered, and washed with water to obtain alkali-modified activated carbon; the alkali-modified activated carbon was placed in a beaker containing 100mL of water, 6g of nano-silicon dioxide was added, stirred at 300r / min for 2h, filtered, and dried in a vacuum oven at 80°C for 3h to obtain modified activated carbon.
[0024] Preparation Example 2 100g of phenolic resin was calcined until carbonized at 700°C for 3h to obtain carbonized particles; the carbonized particles were placed in a carbonization furnace and activated for 1h under water vapor at 600°C to obtain activated activated carbon; the activated activated carbon was immersed in a 1% hydrogen peroxide solution for 5h to obtain oxidized activated carbon; 20g of oxidized activated carbon was immersed in 100mL 1mol / L sodium hydroxide solution for 24h, filtered, and washed with water to obtain alkali-modified activated carbon; the alkali-modified activated carbon was placed in a beaker containing 100mL of water, 6g of nano-silicon dioxide was added, stirred at 300r / min for 2h, filtered, and dried in a vacuum oven at 80°C for 3h to obtain modified activated carbon.
[0025] Preparation Example 3 100g of phenolic resin was calcined until carbonized at 800°C for 4h to obtain carbonized particles; the carbonized particles were placed in a carbonization furnace and activated at 600°C for 1h to obtain activated activated carbon; the activated activated carbon was immersed in a 1.2% hydrogen peroxide solution for 8h to obtain oxidized activated carbon; 20g of oxidized activated carbon was immersed in 100mL 1.2mol / L sodium hydroxide solution for 48h, filtered, and washed with water to obtain alkali-modified activated carbon; the alkali-modified activated carbon was placed in a beaker containing 100mL of water, 6g of nano-silicon dioxide was added, stirred at 300r / min for 2h, filtered, and dried in a vacuum oven at 80°C for 3h to obtain modified activated carbon.
[0026] Preparation Example 4 100 g of phenolic resin was calcined until carbonized at 700° C. for 3 h to obtain carbonized particles; the carbonized particles were placed in a carbonization furnace and activated under water vapor at 600° C. for 1 h to obtain modified activated carbon.
[0027] Preparation Example 5 100g of phenolic resin was calcined until carbonized at 700°C for 3h to obtain carbonized particles; the carbonized particles were placed in a carbonization furnace and activated under water vapor at 600°C for 1h to obtain activated activated carbon; the activated activated carbon was immersed in a 1% hydrogen peroxide solution for 5h to obtain oxidized activated carbon; 20g of oxidized activated carbon was immersed in 100mL1mol / L sodium hydroxide solution for 24h, filtered, and washed with water to obtain modified activated carbon.
[0028] Example 1 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0029] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0030] Example 2 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 530°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0031] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0032] Example 3 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.8; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0033] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0034] Example 4 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:4:6.
[0035] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0036] Example 5 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:8.
[0037] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0038] Example 6 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is defoamed, demisted, and cooled to obtain high-purity sulfuric acid, and electronic-grade ultrapure water is added to absorb the high-purity SO3 gas, followed by cooling to obtain high-purity sulfuric acid; S4: Preparation of electronic-grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 2, cooled, and stripped to obtain electronic-grade sulfuric acid. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0039] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0040] Example 7 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 3, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0041] After testing, the sulfuric acid produced by this method has reached the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are stable.
[0042] Example 8 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 4, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0043] After testing, the sulfuric acid produced by this method reaches the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are unstable.
[0044] Example 9 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 5, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0045] After testing, the sulfuric acid produced by this method reaches the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are unstable.
[0046] Example 10 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:0.8; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0047] After testing, the sulfuric acid produced by this method reaches the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are unstable.
[0048] Embodiment 11 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining a sulphuric acid having a concentration of 1.5-1.0 after evaporation. 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation Example 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:0.2:5.
[0049] After testing, the sulfuric acid produced by this method reaches the international SEMI-C12, that is, electronic grade sulfuric acid standard, and the quality and properties of the product are unstable.
[0050] Comparative Example 1 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: introducing sulfur and preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 250°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtain oleum with a concentration of 45% after evaporation. Sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: high-purity sulfuric acid is oxidized with an oxidant, adsorbed by the modified activated carbon obtained in Preparation 1, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of ferric sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0051] After testing, the sulfuric acid produced by this method did not meet the standard of electronic grade sulfuric acid.
[0052] Comparative Example 2 A method for preparing electronic-grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 and transporting it to a reactor, reacting at a temperature of 450°C under the catalysis of vanadium pentoxide to obtain SO3; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low-temperature evaporation: evaporating the oleum; S3: preparing high-purity sulfuric acid: adding electronic-grade ultrapure water to the high-purity sulfuric acid obtained after defoaming, demisting and cooling the high-purity SO3 gas to absorb the high-purity SO3 gas, and then cooling the high-purity sulfuric acid to obtain the high-purity sulfuric acid; S4: preparing electronic-grade sulfuric acid: oxidizing the high-purity sulfuric acid with an oxidant, adsorbing the modified activated carbon obtained in step 1, cooling and stripping the high-purity sulfuric acid to finally obtain the electronic-grade sulfuric acid. The mass ratio of the oxidant to the modified activated carbon is 1:1.2; the oxidant includes ferric sulfate, vanadium pentoxide and copper oxide, and the mass ratio of the ferric sulfate, vanadium pentoxide and copper oxide is 1:3:5.
[0053] After testing, the sulfuric acid produced by this method did not meet the standard of electronic grade sulfuric acid.
[0054] Comparative Example 3 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on SO3 flue gas raw materials to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtaining evaporated The concentration of 45% fuming sulfuric acid; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is defoamed, demisted and cooled to obtain high-purity sulfuric acid, and electronic grade ultrapure water is added to absorb the high-purity SO3 gas, followed by cooling to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: the high-purity sulfuric acid is adsorbed by the modified activated carbon obtained in Preparation 1, cooled and then blown off to finally obtain electronic grade sulfuric acid.
[0055] After testing, the sulfuric acid produced by this method did not meet the standard of electronic grade sulfuric acid.
[0056] Comparative Example 4 A method for preparing electronic grade sulfuric acid comprises the following steps: S1: preparing oleum: heating sulfur to 130°C to become liquid and introducing preheated oxygen into a sulfur dioxide generator for oxidation to obtain SO2, continuing to introduce preheated O2 into a reactor, and reacting to obtain SO3 at a temperature of 450°C under the catalysis of vanadium pentoxide; performing demisting, filtration and absorption on the SO3 flue gas raw material to obtain oleum; S2: low temperature evaporation: evaporating the oleum to evaporate part of the SO3 gas and obtain After evaporation, the concentration of fuming sulfuric acid is 45%; the SO3 gas is condensed into SO3 liquid after demisting, and evaporated again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: the high-purity SO3 gas is subjected to defoaming, demisting and cooling treatment, and the high-purity sulfuric acid obtained is added with electronic grade ultrapure water to absorb the high-purity SO3 gas, and then cooled to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: the high-purity sulfuric acid is oxidized with an oxidant, cooled and stripped, and finally electronic grade sulfuric acid is obtained. Among them, the oxidant includes iron sulfate, vanadium pentoxide, and copper oxide, and the mass ratio of iron sulfate, vanadium pentoxide, and copper oxide is 1:3:5.
[0057] After testing, the sulfuric acid produced by this method did not meet the standard of electronic grade sulfuric acid.
[0058] The above are all preferred embodiments of the present application, and the protection scope of the present application is not limited thereto. Therefore, any equivalent changes made according to the structure, shape, and principle of the present application should be included in the protection scope of the present application.
Claims
1. A method for preparing electronic grade sulfuric acid, characterized in that: The following steps are involved: S1: Preparation of fuming sulfuric acid: Liquid sulfur and heated oxygen are introduced and oxidized to obtain SO2; preheated O2 is then introduced to obtain SO3 through catalytic reaction; SO3 flue gas raw materials are demisted, filtered and absorbed to obtain fuming sulfuric acid; S2: low-temperature evaporation: evaporating the fuming sulfuric acid to evaporate part of the SO3 gas and obtain evaporated fuming sulfuric acid; condensing the SO3 gas into SO3 liquid after demisting, and evaporating it again to obtain high-purity SO3 gas; S3: Preparation of high-purity sulfuric acid: The high-purity SO3 gas is subjected to defoaming, demisting, absorption and cooling treatment to obtain high-purity sulfuric acid; S4: Preparation of electronic grade sulfuric acid: oxidation by oxidant, adsorption by modified activated carbon, cooling, degassing, and finally obtaining electronic grade sulfuric acid.
2. A method for preparing electronic grade sulfuric acid according to claim 1, characterized in that: The preparation method of the modified activated carbon comprises: calcining and carbonizing phenolic resin, activating under steam conditions to obtain activated carbon; immersing the activated activated carbon in an oxidizing solution to obtain oxidized activated carbon, then soaking it in alkali solution to obtain alkali-modified activated carbon, adding nano-silicon dioxide, stirring and filtering to obtain the modified activated carbon.
3. A method for preparing electronic grade sulfuric acid according to claim 2, characterized in that: The oxidation solution is 8%-12% hydrogen peroxide solution, and the soaking time is 5-8 hours.
4. A method for preparing electronic grade sulfuric acid according to claim 2, characterized in that: The alkali solution is 0.8-1.2 mol / L KOH, and the soaking time is 12-48 hours.
5. The method for preparing electronic grade sulfuric acid according to claim 2, wherein: The calcination and carbonization conditions are 600-800° C. and calcination for 2-4 hours.
6. The method for preparing electronic grade sulfuric acid according to claim 1, wherein: The oxidant comprises ferric sulfate, vanadium pentoxide and copper oxide, and the mass ratio of the ferric sulfate, vanadium pentoxide and copper oxide is 1:(3-4):(5-8).
7. The method for preparing electronic grade sulfuric acid according to claim 1, characterized in that: The mass ratio of the oxidant to the modified activated carbon is 1:(1.2-1.8).
8. The method for preparing electronic grade sulfuric acid according to claim 1, characterized in that: The conditions of the catalytic reaction are: under the catalysis of vanadium pentoxide, the reaction temperature is 450-530°C.
Citation Information
Patent Citations
Process for preparing electronic-grade sulfuric acid by gas absorption method