Process for treating p-nitroanisole high-salinity wastewater
Through the synergistic effect of modified gasification slag and guanidine oligomer composite, the problems of high energy consumption and unstable pollutant recovery in the treatment of high-salt p-nitroanisole are solved, and efficient pollutant removal is achieved and improved Water quality and resource recycling are achieved.
Patent Information
- Application Number
- CN202411410214.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-10
- Publication Date
- 2024-11-22
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing high-salt wastewater treatment process for p-nitroanisole has problems such as high energy consumption, unstable impurity recycling, and volatilization of methanol, which affects the recycling and use of sodium chloride and lacks efficient pollutant removal methods.
The modified gasification slag and guanidine oligomer composite are used for wastewater treatment. By stirring and filtration after standing, the adsorption capacity of the modified gasification slag and the flocculation effect of the guanidine oligomer are combined to remove pollutants in the wastewater. Reduce salt content and water quality pollution.
Effectively reduce the content of pollutants in sewage, improve water quality, achieve the recycling of wastewater standards, avoid high energy consumption evaporation treatment, reduce treatment costs, and realize the resources for sodium chloride, sodium paranitrophenol and other substances Recycle.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of wastewater treatment, and in particular relates to a process for treating p-nitroanisole high-salt wastewater. Background Art
[0002] 4-Nitroanisole, also known as p-nitroanisole, is an organic compound with the chemical formula C7H7NO3. It is a colorless to light yellow crystalline powder. It is insoluble in water but soluble in most organic solvents such as ethanol and ether. It is mainly used as a dye and pharmaceutical intermediate, mainly used in the production of p-aminoanisole, dye blue salt VB, etc.
[0003] The most commonly used synthesis method of p-nitroanisole in industry is as follows: methoxylation reaction is carried out with p-nitrochlorobenzene, methanol and sodium hydroxide as raw materials, wherein methanol is used as both reactant and solvent; after the reaction is completed, the methanol in the system is evaporated for reuse; finally, a certain amount of water is added to dissolve the by-products p-nitrophenol and sodium chloride, and p-nitroanisole is obtained by standing and stratification. The applicant's p-nitroanisole device and o-aminophenol device will produce high-concentration sodium chloride wastewater during the production process. Among them, the impurities contained in the p-nitroanisole high-salt wastewater include methanol, sodium p-nitrophenol, p-nitroanisole, p-aminoanisole and other organic substances; o-aminophenol wastewater contains sodium o-nitrophenol.
[0004] Since this type of wastewater is an environmental pollutant, it is extremely harmful to the human body, water sources, fish and crops. If it is discharged directly without treatment, it will not only waste precious chemical raw materials, but also cause water pollution. At present, the treatment processes of this wastewater mainly include MVR evaporation, cooling crystallization, resin adsorption, etc. However, the brine evaporation process consumes a lot of energy, and the concentration of organic impurities in the evaporated salt is unstable, which affects the recovery and use of sodium chloride; methanol in the wastewater is easy to volatilize with water vapor into the evaporation condensate, resulting in the MVR system condensate water cannot be recovered or discharged in compliance with the standards.
[0005] Therefore, further optimization of the treatment process for this type of high-salt wastewater plays a vital role in energy conservation and consumption reduction, as well as wastewater emission reduction. Summary of the invention
[0006] The purpose of the present invention is to overcome the problems existing in the prior art and provide a process for treating p-nitroanisole high-salt wastewater. The wastewater treated by the process of the present invention meets the water quality standards and can be recycled.
[0007] The purpose of the present invention and the solution to the technical problem are achieved by adopting the following technical solutions.
[0008] One aspect of the present invention provides a process for treating p-nitroanisole high-salt wastewater, comprising the following steps:
[0009] The pH of the p-nitroanisole high-salt wastewater is adjusted to 7-7.5, and the modified gasification slag is added in an amount of 50-150 mg per 1L of wastewater, and stirred at a speed of 600-800 rpm for 5-10 minutes to obtain primary treated wastewater;
[0010] Then, the guanidine oligomer solution is added into the primary wastewater in the amount of 50-150 mL:1 L of the primary treated wastewater and stirred for 5-10 minutes, allowed to stand for 20-40 minutes, filtered, and the treated effluent is obtained.
[0011] In some preferred embodiments, the modified gasified slag is obtained by acid washing, calcining and ionic liquid infiltration of gasified slag;
[0012] The pickling step is: immersing the gasified slag in acid and stirring at 40-60° C. and 200-400 rpm for 1-3 hours;
[0013] The calcination is as follows: the acid-washed gasified slag is calcined at 800-1200° C. for 4-10 hours;
[0014] The ionic liquid infiltration is as follows: the gasified slag cooled to 100-150° C. after calcination is quickly immersed in the ionic liquid solution until it reaches room temperature, then epichlorohydrin is added and stirred for 4-8 hours, and then the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
[0015] In some preferred embodiments, the acid is an inorganic acid or an organic acid, the inorganic acid includes at least one of hydrochloric acid, nitric acid, carbonic acid, phosphoric acid, and boric acid, and the organic acid includes at least one of acetic acid, oxalic acid, malic acid, citric acid, and tartaric acid.
[0016] In some preferred embodiments, the mass fraction of the acid is 30-50 wt%, preferably 35-45 wt%, and more preferably 40 wt%.
[0017] In some preferred embodiments, the calcination is carried out in an inert atmosphere, which includes at least one of nitrogen, hydrogen, argon, helium, and neon, preferably argon, nitrogen, or hydrogen, and more preferably argon.
[0018] In some preferred embodiments, the calcination is programmed calcination, and the specific process is: first, the temperature is increased to 400-600°C at a heating rate of 1-5°C / min and kept warm for 20-40 minutes, then the temperature is increased to 800-1200°C at a heating rate of 5-10°C / min and kept warm for 4-10 hours.
[0019] In some preferred embodiments, the ionic liquid solution is obtained by mixing ionic liquid, methanol and water in a volume ratio of 1:3-10:10-30, preferably 1:4-8:15-25, and more preferably 1:6:20.
[0020] In some preferred embodiments, the ionic liquid is selected from any one of 1,2-dimethyl-3-ethoxyethylimidazolium bis trifluoromethanesulfonyl imide salt, 1-methyl-3-ethoxyethylimidazolium bis trifluoromethanesulfonyl imide salt, N-butyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt, 1-methyl-3-ethoxymethylimidazolium bis trifluoromethanesulfonyl imide salt, N-ethoxymethyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt, 1-methyl-3-butylimidazolium bis trifluoromethanesulfonyl imide salt, N-ethoxyethyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt, and N,N-diethyl-2-methoxyethyl-N-methylamine bis trifluoromethanesulfonyl imide salt.
[0021] In some preferred embodiments, the volume ratio of epichlorohydrin to ionic liquid is 1:1-5, preferably 1:2-4, and more preferably 1:3.
[0022] In some preferred embodiments, the gasification slag includes coarse coal gasification slag and fine coal gasification slag; the mass ratio of the coarse coal gasification slag to the fine coal gasification slag is 1:1-5, preferably 1:2-4, and more preferably 1:3.
[0023] In some preferred embodiments, the concentration of the guanidine oligomer solution is 80-95 wt %, preferably 85-95 wt %, and more preferably 90 wt %.
[0024] In some preferred embodiments, the guanidine oligomer is obtained by mixing a polyamine small molecule and a guanidine salt in a mass ratio of 1:1.5 to 3 and stirring at 150 to 200° C. until the mixture is completely fused.
[0025] In some preferred embodiments, the polyamine small molecule includes at least one of 2,2'-(diethoxy)diethylamine, trimethylhexanediamine, diethylenetriamine, triethylenetetramine, and tetraethylenepentamine.
[0026] In some preferred embodiments, the guanidine salt includes at least one of guanidine hydrochloride, guanidine nitrate, aminoguanidine hydrochloride, triaminoguanidine hydrochloride, and biguanide hydrochloride.
[0027] In another aspect, the present invention also provides a process for directly treating p-nitroanisole high-salt wastewater with a p-nitroanisole high-salt wastewater treatment agent composited with modified gasification slag and guanidine oligomers, comprising:
[0028] The pH of the p-nitroanisole high-salt wastewater is adjusted to 7-7.5, and 50-150 mg of the modified gasification slag / guanidine oligomer complex is added to every 1L of wastewater, and the mixture is stirred at 600-800 rpm for 10-20 minutes, allowed to stand for 20-40 minutes, and filtered to obtain treated effluent.
[0029] In some preferred embodiments, the modified fumed slag / guanidine oligomer composite is obtained by acid washing, calcining and infiltration of guanidine oligomer solution into the fumed slag;
[0030] The pickling step is: immersing the gasified slag in acid and stirring at 40-60° C. and 200-400 rpm for 1-3 hours;
[0031] The calcination is as follows: the acid-washed gasified slag is calcined at 800-1200° C. for 4-10 hours;
[0032] The guanidine oligomer solution infiltration is as follows: immersing the fumed slag cooled to room temperature after calcination in the guanidine oligomer solution, then adding epichlorohydrin and stirring for 4 to 8 hours, then taking out the fumed slag, washing and drying it to obtain the modified fumed slag / guanidine oligomer composite.
[0033] In some preferred embodiments, the acid is an inorganic acid or an organic acid, the inorganic acid includes at least one of hydrochloric acid, nitric acid, carbonic acid, phosphoric acid, and boric acid, and the organic acid includes at least one of acetic acid, oxalic acid, malic acid, citric acid, and tartaric acid.
[0034] In some preferred embodiments, the mass fraction of the acid is 30-50 wt%, preferably 35-45 wt%, and more preferably 40 wt%.
[0035] In some preferred embodiments, the calcination is carried out in an inert atmosphere, which includes at least one of nitrogen, hydrogen, argon, helium, and neon, preferably argon, nitrogen, or hydrogen, and more preferably argon.
[0036] In some preferred embodiments, the calcination is programmed calcination, and the specific process is: first, the temperature is increased to 400-600°C at a heating rate of 1-5°C / min and kept warm for 20-40 minutes, then the temperature is increased to 800-1200°C at a heating rate of 5-10°C / min and kept warm for 4-10 hours.
[0037] In some preferred embodiments, the mass ratio of epichlorohydrin to guanidine oligomer is 1:1-3, preferably 1:2-3, and more preferably 1:2.
[0038] In some preferred embodiments, the gasification slag includes coarse coal gasification slag and fine coal gasification slag; the mass ratio of the coarse coal gasification slag to the fine coal gasification slag is 1:1-5, preferably 1:2-4, and more preferably 1:3.
[0039] In some preferred embodiments, the concentration of the guanidine oligomer solution is 80-95 wt %, preferably 85-95 wt %, and more preferably 90 wt %.
[0040] In some preferred embodiments, the guanidine oligomer is obtained by mixing a polyamine small molecule and a guanidine salt in a mass ratio of 1:1.5 to 3 and stirring at 150 to 200° C. until the mixture is completely fused.
[0041] In some preferred embodiments, the polyamine small molecule includes at least one of 2,2'-(diethoxy)diethylamine, trimethylhexanediamine, diethylenetriamine, triethylenetetramine, and tetraethylenepentamine.
[0042] In some preferred embodiments, the guanidine salt includes at least one of guanidine hydrochloride, guanidine nitrate, aminoguanidine hydrochloride, triaminoguanidine hydrochloride, and biguanide hydrochloride.
[0043] By means of the above technical solution, the present invention has at least the following advantages:
[0044] The present invention compounds modified gasified slag with ionic liquid, wherein epichlorohydrin serves as a coupling agent to play a bridging role, connecting the ionic liquid to the modified gasified slag, so that the modified gasified slag has a very strong ability to adsorb pollutant molecules and surface chemical activity that combines with pollutant molecules, and can effectively reduce the salt content in sewage.
[0045] The present invention uses guanidine oligomers as flocculants, which can play a flocculation and sedimentation role on pollutants, reduce the content of pollutants in sewage, and improve water quality. Guanidine oligomers are a highly efficient and broad-spectrum antibacterial agent, which is safe for human body and can be widely used in the fields of medicine, food, agriculture and industrial products. Due to its good water solubility, the application is mainly in the form of solution. At present, guanidine oligomers have not been used in sewage treatment. Since guanidine oligomers have strong polarity and good thermal stability, they are used in the treatment of p-nitroanisole high-salinity wastewater to effectively remove sodium p-nitrophenol in sewage.
[0046] The modified gasification slag of the present invention and guanidine oligomers synergistically remove pollutants in p-nitroanisole high-salt wastewater, which can significantly reduce the content of pollutants in the wastewater and improve water quality. The treatment process of the present invention is simple, the conditions are mild, and it is suitable for industrial promotion and use.
[0047] The above description is only an overview of the technical solution of the present invention. In order to more clearly understand the technical means of the present invention and implement it according to the contents of the specification, the preferred embodiments of the present invention are described in detail as follows. DETAILED DESCRIPTION
[0048] In order to make the technical means, creative features, objectives and effects of the present invention easy to understand, the technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0049] Unless otherwise specified, the p-nitroanisole high-salt wastewater used in the embodiments of the present invention is collected from the same chemical plant production wastewater. Before treatment, the wastewater has the following indicators: COD: 72538 mg / L, ammonia nitrogen: 3528 mg / L, Cl-: 25400 mg / L, sodium p-nitrophenolate: 45362 mg / L. Before treatment, the wastewater is subjected to a pretreatment process in which most of the sodium p-nitrophenolate and sodium chloride are recovered after conventional extraction and evaporation crystallization, and the wastewater to be treated has the following indicators: COD: 1063 mg / L, ammonia nitrogen: 79 mg / L, Cl-: 482 mg / L, sodium p-nitrophenolate: 379 mg / L. Unless otherwise specified, the wastewater in the embodiments of the present invention is the above-mentioned pretreated wastewater.
[0050] Unless otherwise specified, the preparation method of the guanidine oligomer used in the embodiments of the present invention is as follows: 10 g of 2,2'-(diethoxy)diethylamine and 22 g of guanidine hydrochloride are stirred at 180° C. until they are completely fused to obtain an oligomeric product, poly-(2-(2-ethoxy)-ethoxyethyl-guanidine hydrochloride).
[0051] Embodiment 1:
[0052] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0053] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, and 100 mg of modified gasification slag was added and stirred at 700 rpm for 7.5 min to obtain primary treated wastewater;
[0054] Then, 90 wt% guanidine oligomer solution was added to the primary wastewater in the amount of 100 mL:1 L primary treated wastewater and stirred for 7.5 min, allowed to stand for 30 min, and filtered to obtain treated effluent. The effluent index was tested, and the results are shown in Table 1.
[0055] The above modified gasified slag preparation process is as follows:
[0056] Pickling: soak the gasification slag (the mass ratio of the gasification coarse slag to the gasification fine slag is 1:3) in 40wt% hydrochloric acid at 50℃ and 300rpm for 2h;
[0057] Calcination: In an argon atmosphere, the acid-washed gasified slag was calcined at 1000°C for 7 hours; the specific process was: firstly, the temperature was increased to 500°C at a heating rate of 3°C / min and kept at that temperature for 30 minutes, then the temperature was increased to 1000°C at a heating rate of 7.5°C / min and kept at that temperature for 7 hours;
[0058] Ionic liquid infiltration: The calcined and cooled gasified slag is quickly immersed in N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt solution (N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt, methanol, and water are mixed in a volume ratio of 1:6.5:20) to room temperature, and then epichlorohydrin is added (the added amount is 1:3 with N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt The volume ratio is 1:3) and stirred for 6 hours. After that, the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
[0059] Embodiment 2:
[0060] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0061] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, and 150mg of p-nitroanisole was added to the modified gasification slag and stirred at 600rpm for 10min to obtain primary treated wastewater;
[0062] Then, 80 wt% guanidine oligomer solution was added to the primary wastewater in the amount of 50 mL:1 L primary treated wastewater and stirred for 10 min, allowed to stand for 20 min, and filtered to obtain treated effluent. The effluent index was tested, and the results are shown in Table 1.
[0063] The above modified gasified slag preparation process is as follows:
[0064] Pickling: soak the gasification slag (the mass ratio of the coarse gasification slag to the fine gasification slag is 1:1) in 30wt% nitric acid and stir at 60°C and 200rpm for 1h;
[0065] Calcination: The acid-washed gasified slag was calcined at 800°C for 10 h in an argon atmosphere; the specific process was as follows: first, the temperature was raised to 400°C at a heating rate of 1°C / min and kept at that temperature for 40 min, then the temperature was raised to 1200°C at a heating rate of 10°C / min and kept at that temperature for 4 h;
[0066] Ionic liquid infiltration: The gasified slag cooled to 150° C. after calcination is quickly immersed in a 1-methyl-3-butylimidazole bistrifluoromethanesulfonyl imide salt solution (1-methyl-3-butylimidazole bistrifluoromethanesulfonyl imide salt, methanol, and water are mixed in a volume ratio of 1:3:10) to room temperature, and then epichlorohydrin is added (the added amount is 1-methyl-3-butylimidazole bistrifluoromethanesulfonyl imide salt The volume ratio is 1:1) and stirred for 4 hours. After that, the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
[0067] Embodiment 3:
[0068] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0069] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, and 50mg of modified gasification slag was added and stirred at 800rpm for 5min to obtain primary treated wastewater;
[0070] Then, 95 wt% guanidine oligomer solution was added to the primary wastewater in the amount of 150 mL:1 L primary treated wastewater and stirred for 5 minutes, allowed to stand for 40 minutes, and filtered to obtain treated effluent. The effluent index was tested, and the results are shown in Table 1.
[0071] The above modified gasified slag preparation process is as follows:
[0072] Pickling: soak the gasification slag (the mass ratio of the coarse gasification slag to the fine gasification slag is 1:5) in 50wt% acetic acid and stir at 40°C and 400rpm for 3h;
[0073] Calcination: The acid-washed gasified slag was calcined at 1200°C for 4 h in an argon atmosphere; the specific process was as follows: first, the temperature was raised to 600°C at a heating rate of 5°C / min and kept at that temperature for 20 min, then the temperature was raised to 1200°C at a heating rate of 5°C / min and kept at that temperature for 10 h;
[0074] Ionic liquid infiltration: The calcined and cooled gasified slag is quickly immersed in N-ethoxyethyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt solution (N-ethoxyethyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt, methanol, and water are mixed in a volume ratio of 1:10:30) to room temperature, and then epichlorohydrin is added (the added amount is 1:5 with N-ethoxyethyl-N-methylpyrrolidine bis trifluoromethanesulfonyl imide salt The volume ratio is 1:5) and stirred for 8 hours. After that, the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
[0075] Embodiment 4:
[0076] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0077] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, and 100 mg of the modified gasification slag / guanidine oligomer complex was added and stirred at 700 rpm for 15 min, allowed to stand for 30 min, and filtered to obtain the treated effluent. The effluent indicators were tested, and the results are shown in Table 1.
[0078] The preparation process of the modified gasified slag / guanidine oligomer composite is as follows:
[0079] Pickling: soak the gasification slag (the mass ratio of the gasification coarse slag to the gasification fine slag is 1:3) in 40wt% hydrochloric acid at 50℃ and 300rpm for 2h;
[0080] Calcination: In an argon atmosphere, the acid-washed gasified slag was calcined at 1000°C for 7 hours; the specific process was: firstly, the temperature was increased to 500°C at a heating rate of 3°C / min and kept at that temperature for 30 minutes, then the temperature was increased to 1000°C at a heating rate of 7.5°C / min and kept at that temperature for 7 hours;
[0081] Guanidine oligomer solution infiltration: The fumed slag cooled to room temperature after calcination is immersed in a 90wt% guanidine oligomer solution, and then epichlorohydrin is added (the added amount is 1:2 with the mass ratio of guanidine oligomer) and stirred for 6 hours, and then the fumed slag is taken out, washed and dried to obtain the modified fumed slag / guanidine oligomer composite.
[0082] Comparative Example 1:
[0083] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0084] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, 100mg of modified gasification slag was added, stirred at 700rpm for 15min, allowed to stand for 30min, and filtered to obtain treated effluent. The effluent index was tested, and the results are shown in Table 1.
[0085] The above modified gasified slag preparation process is as follows:
[0086] Pickling: soak the gasification slag (the mass ratio of the gasification coarse slag to the gasification fine slag is 1:3) in 40wt% hydrochloric acid at 50℃ and 300rpm for 2h;
[0087] Calcination: In an argon atmosphere, the acid-washed gasified slag was calcined at 1000°C for 7 hours; the specific process was: firstly, the temperature was increased to 500°C at a heating rate of 3°C / min and kept at that temperature for 30 minutes, then the temperature was increased to 1000°C at a heating rate of 7.5°C / min and kept at that temperature for 7 hours;
[0088] Ionic liquid infiltration: The calcined and cooled gasified slag is quickly immersed in N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt solution (N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt, methanol, and water are mixed in a volume ratio of 1:6.5:20) to room temperature, and then epichlorohydrin is added (the added amount is 1:3 with N,N-diethyl-2-methoxyethyl-N-methylamine bistrifluoromethanesulfonyl imide salt The volume ratio is 1:3) and stirred for 6 hours. After that, the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
[0089] Comparative Example 2:
[0090] A p-nitroanisole high-salt wastewater treatment process comprises the following treatment steps:
[0091] The pH of 1L of p-nitroanisole high-salt wastewater was adjusted to 7-7.5, 100mL of 90wt% guanidine oligomer solution was added and stirred at 700rpm for 15min, allowed to stand for 30min, and filtered to obtain treated effluent. The effluent index was tested, and the results are shown in Table 1.
[0092] Table 1 Water quality of effluent under different process treatments
[0093] COD(mg / L) Ammonia nitrogen (mg / L) Cl-(mg / L) Sodium p-nitrophenolate (mg / L) Example 1 41.6 5.5 27.4 22.7 Example 2 42.3 5.4 27.9 23.2 Example 3 42.7 5.8 27.6 23.5 Example 4 25.3 3.9 12.4 11.9 Comparative Example 1 154.8 19.3 92.5 178.1 Comparative Example 2 276.3 37.4 185.7 97.9
[0094] It can be seen from the results in Table 1 that the process treatment effects of Examples 1 to 4 of the present invention are significantly better than those of Comparative Examples 1 to 2, which indicates that the modified gasification slag of the present invention and the guanidine oligomers work synergistically to remove pollutants, and the modified gasification slag / guanidine oligomer composite (Example 4) has the best removal effect on pollutants.
[0095] Since the remaining trace organic matter is difficult to separate and remove using conventional physical means, chemical catalytic oxidation is used to deeply degrade the organic matter in the water. The oxidation process uses hydrogen peroxide as an oxidant, and titanium-based composite metals as catalysts at 140°C and pH 3 to mineralize the organic matter in the water into water and carbon dioxide, so that the TOC in the final wastewater can be reduced to less than 30 mg / L.
[0096] Through this treatment process, sodium chloride, methanol, sodium o-nitrophenolate, sodium p-nitrophenolate, p-aminoanisole, and p-nitroanisole in water can be recycled and utilized. No solid waste is generated, and the use of high-energy consumption evaporation treatment processes is avoided. Compared with the original evaporation treatment process, this treatment process can recover 220kg of sodium chloride, 13kg of sodium p-nitrophenolate, 5kg of o-nitrophenol, 1kg of p-nitroanisole, 2kg of p-aminoanisole, and 759kg of water per ton of wastewater. The treatment cost per ton of water is reduced from 140 yuan / t to 45 yuan / t.
[0097] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with this profession can make some changes or modifications to equivalent embodiments of equivalent changes by using the methods and technical contents disclosed above without departing from the scope of the technical solution of the present invention. However, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still fall within the scope of the technical solution of the present invention.
Claims
1. A p-nitroanisole high-salt wastewater treatment process, characterized in that, The processing steps include: The pH of the p-nitroanisole high-salt wastewater is adjusted to 7-7.5, and the modified gasification slag is added in an amount of 50-150 mg per 1L of wastewater, and stirred at a speed of 600-800 rpm for 5-10 minutes to obtain primary treated wastewater; Then, the guanidine oligomer solution is added into the primary wastewater in the amount of 50-150 mL:1 L of the primary treated wastewater and stirred for 5-10 minutes, allowed to stand for 20-40 minutes, filtered, and the treated effluent is obtained.
2. The treatment process according to claim 1, characterized in that: The modified gasified slag is obtained by acid washing, calcining and ion liquid infiltration of gasified slag; The pickling step is: immersing the gasified slag in acid and stirring at 40-60° C. and 200-400 rpm for 1-3 hours; The calcination is as follows: the acid-washed gasified slag is calcined at 800-1200° C. for 4-10 hours; The ionic liquid infiltration is as follows: the gasified slag cooled to 100-150° C. after calcination is quickly immersed in the ionic liquid solution until it reaches room temperature, then epichlorohydrin is added and stirred for 4-8 hours, and then the gasified slag is taken out, washed and dried to obtain the modified gasified slag.
3. The treatment process according to claim 2, characterized in that: The acid is an inorganic acid or an organic acid. The inorganic acid includes at least one of hydrochloric acid, nitric acid, carbonic acid, phosphoric acid, and boric acid. The organic acid includes at least one of acetic acid, oxalic acid, malic acid, citric acid, and tartaric acid.
4. The treatment process according to claim 2, characterized in that: The mass fraction of the acid is 30-50 wt %, preferably 35-45 wt %, and more preferably 40 wt %.
5. The treatment process according to claim 2, characterized in that: The calcination is carried out in an inert atmosphere, which includes at least one of nitrogen, hydrogen, argon, helium and neon, preferably argon, nitrogen or hydrogen, and more preferably argon.
6. The treatment process according to claim 2, characterized in that: The calcination is a programmed calcination, and the specific process is: firstly, the temperature is increased to 400-600°C at a heating rate of 1-5°C / min and kept at this temperature for 20-40 minutes, then the temperature is increased to 800-1200°C at a heating rate of 5-10°C / min and kept at this temperature for 4-10 hours.
7. The treatment process according to claim 2, characterized in that: The ionic liquid solution is prepared by mixing ionic liquid, methanol and water in a volume ratio of 1:3-10:10-30, preferably 1:4-8:15-25, and more preferably 1:6:
20.
8. The treatment process according to claim 2, characterized in that: The volume ratio of epichlorohydrin to ionic liquid is 1:1-5, preferably 1:2-4, and more preferably 1:
3.
9. The treatment process according to claim 2, characterized in that: The gasification slag includes coarse coal gasification slag and fine coal gasification slag; the mass ratio of the coarse coal gasification slag to the fine coal gasification slag is 1:1-5, preferably 1:2-4, and more preferably 1:
3.
10. The treatment process according to claim 1, characterized in that: The concentration of the guanidine oligomer solution is 80-95 wt %, preferably 85-95 wt %, and more preferably 90 wt %.
Citation Information
Patent Citations
Chemical industrial waste salt refining process
CN104649495A
Recycling treatment method for p-aminophenol production waste water
CN107117749A
Low linear expansion coefficient epoxy resin based cement concrete road fast repairing material and preparation method thereof
CN109534720A
Resource treatment process for inorganic salt hazardous wastes
CN110756172A
Phosphorus removal agent for treating phosphating wastewater
CN111977772A
Cited By
Preparation method of slow-release carbon source for enhancing nitrogen removal by denitrification
CN119080234A