Fast recovery diode and manufacturing method thereof
By forming a passivation layer in the fast recovery diode and introducing a local current barrier layer, the hole outflow path is defined, and the compromise relationship between conduction loss and reverse recovery loss is solved, the device performance is optimized, and forward conduction is reduced Voltage drop and reverse recovery loss.
Patent Information
- Application Number
- CN202411114946.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-22
AI Technical Summary
The existing fast recovery diodes will increase switching losses when reducing conduction losses, and there is a problem that the compromise relationship between conduction losses and reverse recovery losses is difficult to optimize.
By forming a passivation layer on the second main surface of the substrate and penetrates the opening in the passivation layer along its thickness direction, filling and covering the cathode metal layer to form a local current barrier layer, defining the hole flow near the cathode side of the drift region toward the cathode side path, increasing carrier concentration, thereby reducing the forward conduction voltage drop without sacrificing reverse recovery time.
Without increasing the reverse recovery time, the compromise relationship between forward conduction voltage drop and reverse recovery loss is reduced, the performance of the device is optimized, and the balance between conduction loss and reverse recovery loss is improved.
Smart Images

Figure CN119008402A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductors, and in particular relates to a fast recovery diode and a manufacturing method thereof. Background Art
[0002] In high-power fast switching applications, the new generation of power switching devices is developing towards high frequency. Fast recovery diodes (FRDs) have the advantages of low on-state voltage and low reverse recovery loss, and are widely used in pulse width modulation (PWM), switching power supplies, inverters and other applications to perform high-frequency rectification and freewheeling functions.
[0003] When the FRD is forward-conducting, the holes in the P-type anode region and the electrons in the N-type cathode region are respectively injected into the drift region and recombine in the drift region, resulting in a conductivity modulation effect, which reduces the on-state voltage drop of the device. However, the holes flow out through the drift region, which weakens the conductivity modulation effect at the bottom of the drift region. When a reverse voltage is applied to the FRD in the forward-conducting state, the minority carriers remaining in the drift region need to be completely extracted or recombined before the reverse shutdown is achieved, resulting in high device turn-off losses. When the FRD is working, conduction losses and reverse recovery losses will be generated, and there is a compromise relationship between the two.
[0004] Therefore, an improved structure of a fast recovery diode and a manufacturing method thereof are provided.
[0005] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because they are described in the background technology section of the present application. Summary of the invention
[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a fast recovery diode and a manufacturing method thereof, so as to solve the problem that the switching loss of the device increases while the conduction loss is reduced in the existing fast recovery diode.
[0007] To achieve the above objectives and other related objectives, the present invention provides a fast recovery diode and a method for manufacturing the same, comprising:
[0008] A substrate is provided, the substrate comprising a first main surface and a second main surface opposite to each other, an anode region and a drift region are sequentially formed from the first main surface of the substrate toward the inside, and the drift region has a conductivity type opposite to that of the anode region;
[0009] Covering the anode region to form an anode metal layer;
[0010] forming a buffer layer extending inwardly from the second main surface of the substrate, the buffer layer having the same conductivity type as the drift region;
[0011] forming a passivation layer on the second main surface of the substrate, and forming an opening penetrating through the passivation layer along the thickness direction thereof;
[0012] A cathode metal layer is formed by filling and covering the opening, and the cathode metal layer contacts the buffer layer through the opening.
[0013] Optionally, the material of the passivation layer includes one of oxide, silicon nitride, silicon-phosphorus glass, polyimide, or a combination thereof.
[0014] Optionally, the step of forming the anode region includes: performing ion implantation of boron impurities into the first main surface of the substrate to form a P-type doped region.
[0015] Optionally, the step of forming the opening includes: etching the passivation layer based on a graphic mask to form a plurality of openings penetrating the passivation layer, wherein the bottom of the opening exposes the second main surface of the substrate; wherein the shape of the opening includes at least one of a circle, a rectangle, a regular polygon, and a ring.
[0016] Optionally, before the step of forming the anode metal layer, the step includes: forming a P-type heavily doped region on the surface layer of the P-type doped region.
[0017] Optionally, after the step of forming the opening, the step includes: filling the opening with a metal electrode material and covering the passivation layer to form a cathode metal layer, wherein the metal electrode material is deposited by one of a chemical vapor deposition process, a physical vapor deposition process, and an atomic layer deposition process; and performing an alloying treatment on the cathode metal layer so that the cathode metal layer forms an ohmic contact with the substrate surface exposed from the opening.
[0018] The present invention also provides a fast recovery diode, comprising an anode metal layer, an anode region, a drift region, a buffer layer and a cathode metal layer stacked from top to bottom, wherein the anode metal layer covers the anode region and is electrically connected to the cathode region; the anode region has a conductivity type opposite to that of the drift region and the buffer layer, a passivation layer is arranged between the buffer layer and the cathode metal layer, and an opening is arranged in the passivation layer that penetrates along the thickness direction thereof; the cathode metal layer fills and covers the opening, and the cathode metal layer forms contact with the buffer layer through the opening.
[0019] Optionally, a plurality of openings are formed through the passivation layer, and the shapes of the openings include at least one of a circle, a rectangle, a regular polygon, and a ring.
[0020] Optionally, the buffer layer is disposed adjacent to the drift region, and a doping concentration of the buffer layer is greater than a doping concentration of the drift region.
[0021] Optionally, the anode region includes a P-type doped region, and a P-type heavily doped region is provided on a surface of the P-type doped region away from the drift region for forming an ohmic contact with the anode metal layer.
[0022] As described above, the fast recovery diode and its manufacturing method of the present invention form a passivation layer before forming a cathode metal layer, and introduce a local current blocking layer by forming an opening in the passivation layer. The opening is used to limit the hole outflow path of the drift region close to the cathode side, thereby increasing the carrier concentration of the drift region close to the cathode side, thereby reducing the forward conduction voltage drop without sacrificing the reverse recovery time, improving the compromise relationship between the conduction loss and reverse recovery loss of the device, and optimizing the device performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 Shown is a flow chart of a method for manufacturing a fast recovery diode in an embodiment of the present invention.
[0024] Figure 2a to Figure 2f It is a schematic diagram showing the structure obtained in multiple stages of manufacturing a fast recovery diode in an embodiment of the present invention.
[0025] Figure 3 It is a curve diagram of the hole density in the fast recovery diode in the on state in the examples of the present invention and the comparative examples.
[0026] Figure 4 It is a curve diagram of the output characteristics of the fast recovery diode in the example of the present invention and the comparative example when the fast recovery diode is in the on state.
[0027] Component number description
[0028] 1 Substrate
[0029] 20 Anode metal layer
[0030] 30 Cathode metal layer
[0031] 11 Drift Zone
[0032] 121 P-type doping region
[0033] 122 P-type heavily doped region
[0034] 13 Buffer layer
[0035] 310 Passivation layer
[0036] 31 Local current blocking layer
[0037] 32 Opening
[0038] Steps S1-S5 DETAILED DESCRIPTION
[0039] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0040] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.
[0041] For ease of description, spatially relative terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or one or more intervening layers may also be present.
[0042] In the context of the present application, unless otherwise specified and limited, the structural terminology of a first feature described as "above" a second feature should be understood broadly, for example, it may include embodiments in which the first and second features are formed in direct contact, and it may also include embodiments in which additional features are formed between the first and second features, so that the first and second features may not be in direct contact.
[0043] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0044] The semiconductor field vocabulary used in this article is technical vocabulary commonly used by technical personnel in this field. For example, for P-type and N-type impurities, in order to distinguish the doping concentration, P+ type represents P-type with heavy doping concentration, P-type represents P-type with medium doping concentration, P-type represents P-type with light doping concentration, N+ type represents N-type with heavy doping concentration, N-type represents N-type with medium doping concentration, and N-type represents N-type with light doping concentration.
[0045] The following combination Figures 1 to 2a ~ Figure 2f As shown, the method for manufacturing the fast recovery diode of the present invention is specifically described, wherein one of the first conductivity type and the second conductivity type is N type and the other is P type. In this embodiment, the first conductivity type is N type and the second conductivity type is P type.
[0046] It should be noted that the sequence described below does not strictly represent the preparation sequence of the method for manufacturing the fast recovery diode protected by the present invention, and those skilled in the art may change it according to the actual process steps.
[0047] First, step S1 is performed to provide a substrate, wherein the substrate comprises a first main surface and a second main surface opposite to each other, wherein an anode region and a drift region are sequentially formed from the first main surface of the substrate to the inside, and the anode region has a conductivity type opposite to that of the drift region.
[0048] Specifically, the material of the substrate 1 can be a semiconductor material commonly used in the relevant technical field, such as silicon, germanium, diamond, or a compound semiconductor material, such as silicon carbide, gallium arsenide, indium arsenide or indium phosphide. The substrate 1 generally has a first conductivity type, and the drift region can be epitaxially grown on the substrate; or, the drift region can be a section of the substrate. In this embodiment, the substrate 1 is an N-type silicon substrate, for example, a phosphorus or arsenic-doped <111> N-type silicon substrate with crystal orientation.
[0049] like Figure 2a As shown, the step of forming the anode region includes: introducing P-type impurities into the first main surface of the substrate by ion implantation and thermal diffusion to form a P-type doped region 121. In this embodiment, ion implantation is performed into the first main surface of the substrate to form the P-type doped region 121.
[0050] For example, boron impurities may be introduced by doping the first main surface of the substrate with boron impurities by ion implantation or thermal diffusion, or by coating a liquid boron source.
[0051] Furthermore, after the step of forming the P-type doping region 121, it also includes: performing deep junction diffusion by pre-depositing metal impurities and / or boron impurities to form a P-type heavily doped region 122 on the surface of the P-type doping region, which is used as an ohmic contact region of the P surface. The distribution, size and morphology of the P-type heavily doped region are not excessively limited here.
[0052] As an example,
[0053] Then, execute step S2, see Figure 2b , forming an anode metal layer on the first main surface of the substrate.
[0054] Specifically, an anode metal layer 20 is formed on the first main surface of the substrate; then, an alloying treatment is performed on the anode metal layer 20 so that the anode metal layer 20 forms an ohmic contact at the P-type heavily doped region 122 .
[0055] As an example, the first metal electrode material is deposited on the first main surface of the substrate by a deposition process such as chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), etc. to form an anode metal layer 20. For example, the anode metal layer 20 is formed on the first main surface of the substrate by evaporation or sputtering, and the anode metal layer 20 can be a single layer of Al, or a stack of Ti-Al or Ti-Ni-Al.
[0056] Then, step S3 is performed to form a buffer layer extending inward from the second main surface of the substrate, wherein the buffer layer has the same conductivity type as that of the drift region.
[0057] See also Figure 2c The step of forming the buffer layer 13 includes: introducing N-type impurities into the first main surface of the substrate by ion implantation and thermal diffusion. Phosphorus impurities are doped into the first main surface of the substrate by ion implantation and thermal diffusion to form a buffer layer 13 extending inward from the second main surface of the substrate, which can improve the reverse withstand voltage characteristics of the device.
[0058] Furthermore, before the step of forming the passivation layer 310 , the second main surface of the substrate away from the drift region is thinned, and the removed film layer may be a part of the substrate away from the drift region.
[0059] Then, step S4 is performed to form a passivation layer on the second main surface of the substrate, and to form an opening penetrating through the passivation layer along the thickness direction of the passivation layer.
[0060] See also Figure 2d to Figure 2e The step of forming the opening 32 includes: performing anisotropic dry etching on the passivation layer 310 based on a pattern mask until the second main surface of the substrate is exposed, and forming an opening 32 penetrating along the thickness direction of the passivation layer 310, thereby obtaining a local current blocking layer 31 sandwiched between the anode metal layer and the passivation layer. The opening corresponding to the pattern mask can be defined on the passivation layer by conventional processes in the art, such as photolithography, and will not be described in detail here.
[0061] As an example, the passivation layer 310 is deposited on the second main surface of the substrate by a chemical vapor deposition process, wherein the passivation layer 310 can be selected from a surface passivation material commonly used in the art, and its material includes but is not limited to one of oxides, silicon nitride, silicon phosphorus glass, polyimide, or a combination of the above, such as silicon oxide, or a combination of silicon oxide and silicon nitride. The chemical vapor deposition process referred to herein may include a low pressure chemical vapor deposition (LPCVD) process, a plasma chemical vapor deposition (PECVD) process, or a similar process. Since the holes in the drift region can only flow out through the opening 32 in the forward conduction state of the device, this effectively reduces the outflow path of the minority carriers at the bottom of the drift region, and at the same time can ensure that the minority carriers stored in the drift region are completely extracted or recombined during the reverse recovery process, thereby improving the trade-off relationship between the forward conduction voltage drop and the reverse recovery loss.
[0062] Under the premise of ensuring the current uniformity of the fast recovery diode, the geometric shape and size of the opening can be appropriately set according to the required device performance, and no excessive restrictions are made here. In some examples, a plurality of openings 32 are formed in the passivation layer 310 throughout the thickness direction thereof, and the shape of the opening includes at least one of a circle, a rectangle, a regular polygon, and a ring.
[0063] Then, execute step S5, see Figure 2f , filling and covering the opening to form a cathode metal layer, wherein the cathode metal layer contacts the buffer layer through the opening.
[0064] Specifically, the opening 32 is filled and covered with a second metal electrode material to form a cathode metal layer 30 , and the cathode metal layer 30 forms contact through the substrate surface exposed from the opening 32 .
[0065] As an example, the second metal electrode material is deposited by a deposition process such as chemical vapor deposition (CVD), physical vapor deposition (PVD), atomic layer deposition (ALD), etc. to form the cathode metal layer 30. For example, the cathode metal layer 30 is formed by vacuum evaporation or sputtering, and the cathode metal layer 30 can be a stack of Ti / Ni / Ag or Ti / Ni / Au.
[0066] Furthermore, after the step of forming the cathode metal layer 30 , an alloying treatment is performed on the cathode metal layer 30 so that the cathode metal layer forms an ohmic contact with the substrate surface exposed from the opening 32 , so as to ensure good electrical performance of the device.
[0067] This embodiment also provides a fast recovery diode, which is preferably manufactured using the manufacturing method of the fast recovery diode described in the previous embodiment, and of course, it can also be manufactured using other methods. The features of each structure / layer in the fast recovery diode in this embodiment can refer to the description of the manufacturing method of the fast recovery diode in the previous embodiment, and will not be repeated here.
[0068] like Figure 2f As shown, the fast recovery diode includes an anode metal layer 20, an anode region, a drift region 11, a buffer layer 13 and a cathode metal layer 30 stacked from top to bottom, the anode metal layer 20 covers the anode region and is electrically connected to the cathode region, the anode region has a conductivity type opposite to that of the drift region and the buffer layer, and is used to reduce the injection of holes; a local current blocking layer 31 is arranged between the buffer layer 13 and the cathode metal layer 30, and the local current blocking layer 31 includes an opening 32 penetrating along the thickness direction thereof; the cathode metal layer fills and covers the opening, and the cathode metal layer 30 forms an ohmic contact through the opening 32.
[0069] The local current blocking layer 31 is configured as a passivation layer with an opening, the opening runs through the thickness direction of the passivation layer, and the opening is used to limit the carrier transmission path, thereby reducing the path for holes to flow out, and the area outside the passivation layer opening is sandwiched between the cathode metal layer and the cathode region to play a current blocking role. In some examples, the shape of the opening 32 includes at least one of a circle, a rectangle, a regular polygon, and a ring. Figure 2f As shown, a plurality of openings 32 are provided through the passivation layer, and the plurality of openings 32 may be arranged laterally at equal intervals along the surface of the local current blocking layer 31 .
[0070] As an example, the buffer layer 13 is disposed adjacent to the drift region 11 , and the doping concentration of the buffer layer is greater than the doping concentration of the drift region.
[0071] As an example, the anode region includes a P-type doped region 121 , and a P-type heavily doped region 122 is disposed on a surface of the P-type doped region away from the drift region for forming an ohmic contact with the anode metal layer.
[0072] In order to illustrate the advantages of the device of the present invention, a fast recovery diode with a local current blocking layer is used as an example, and a fast recovery diode without a local current blocking layer is used as a comparative example for simulation analysis.
[0073] After simulation verification, the curve diagram of the hole density of the fast recovery diode of the example of the present invention and the comparative example in the forward conduction state is shown in Figure 3 The output characteristics of the two in the forward conduction state are shown in the curve diagram. Figure 4 .
[0074] Depend on Figure 3 It can be seen that due to the introduction of the local current blocking layer, the hole density in the drift region of the device is significantly increased, which indicates that the conductivity modulation effect in the device of the example is significantly enhanced; combined with Figure 4 It can be seen that when the device structure of the example and the device of the comparative example have the same forward conduction current density, the device of the example has a significantly lower forward conduction voltage drop V compared with the device of the comparative example. F .
[0075] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for manufacturing a fast recovery diode, characterized in that: include: A substrate is provided, the substrate comprising a first main surface and a second main surface opposite to each other, an anode region and a drift region are sequentially formed from the first main surface of the substrate toward the inside, and the drift region has a conductivity type opposite to that of the anode region; Covering the anode region to form an anode metal layer; forming a buffer layer extending inwardly from the second main surface of the substrate, the buffer layer having the same conductivity type as the drift region; forming a passivation layer on the second main surface of the substrate, and forming an opening penetrating through the passivation layer along the thickness direction thereof; A cathode metal layer is formed by filling and covering the opening, and the cathode metal layer contacts the buffer layer through the opening.
2. The method according to claim 1, characterized in that: The material of the passivation layer includes one of oxide, silicon nitride, silicon-phosphorus glass, polyimide, or a combination thereof.
3. The method according to claim 1, characterized in that: The step of forming the anode region includes: ion implanting boron impurities into the first main surface of the substrate to form a P-type doped region.
4. The method according to claim 3, characterized in that: The step of forming the openings comprises: etching the passivation layer based on a graphic mask to form a plurality of openings penetrating the passivation layer, wherein the bottoms of the openings expose the second main surface of the substrate; wherein the shapes of the openings include at least one of a circle, a rectangle, a regular polygon, and a ring.
5. The manufacturing method according to claim 3, characterized in that: Before the step of forming the anode metal layer, the method comprises: A P-type heavily doped region is formed on the surface layer of the P-type doped region.
6. The method according to claim 1 or 4, characterized in that: After the step of forming the opening, it includes: filling the opening with a metal electrode material and covering the passivation layer to form a cathode metal layer, wherein the metal electrode material is deposited by one of a chemical vapor deposition process, a physical vapor deposition process, and an atomic layer deposition process; performing an alloying treatment on the cathode metal layer so that the cathode metal layer forms an ohmic contact with the substrate surface exposed from the opening.
7. A fast recovery diode, characterized in that: It includes an anode metal layer, an anode region, a drift region, a buffer layer and a cathode metal layer stacked from top to bottom, the anode metal layer covers the anode region, and the anode metal layer is electrically connected to the cathode region; the anode region has a conductivity type opposite to that of the drift region and the buffer layer, a local current blocking layer is arranged between the buffer layer and the cathode metal layer, and the local current blocking layer includes an opening penetrating along the thickness direction thereof; the cathode metal layer fills and covers the opening, and the cathode metal layer forms contact with the buffer layer through the opening.
8. The fast recovery diode according to claim 7, characterized in that: A plurality of openings are formed through the passivation layer, and the shapes of the openings include at least one of a circle, a rectangle, a regular polygon, and a ring.
9. The fast recovery diode according to claim 7, characterized in that: The buffer layer is disposed adjacent to the drift region, and a doping concentration of the buffer layer is greater than a doping concentration of the drift region.
10. The fast recovery diode according to claim 7, characterized in that: The anode region includes a P-type doped region, and a surface layer of the P-type doped region away from the drift region is provided with a P-type heavily doped region for forming an ohmic contact with the anode metal layer.