Semiconductor structure and manufacturing method thereof

By forming doped regions in the substrate trench in the transient voltage suppression tube and growing the field area oxide layer at high temperature and high pressure, the problems of beak and leucorrhea effect caused by unreasonable thickness of the field area are solved, and the device is improved Voltage resistance and yield.

CN119008661APending Publication Date: 2024-11-22GTA SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411143395.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-20
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the transient voltage suppression tube, unreasonable thickness of the oxide layer in the field will lead to the beak effect and the leucorrhea effect, affecting the voltage resistance and yield of the device.

Method used

By forming doped regions in the trench of the substrate and growing the field oxide layer under high temperature and high pressure conditions, the thickness is controlled at the micron level, improving the oxidation rate and growth control, and avoiding the beak effect and leucorrhea effect.

Benefits of technology

It effectively improves the voltage withstandability of the semiconductor structure, prevents device breakdown, and improves device yield and performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008661A_ABST
    Figure CN119008661A_ABST
Patent Text Reader

Abstract

The invention relates to a semiconductor structure and a manufacturing method thereof. The manufacturing method of the semiconductor structure comprises the following steps: providing a substrate; one side of the substrate is provided with a pre-oxidation layer and a barrier layer which are sequentially stacked from bottom to top; etching the pre-oxidation layer and the barrier layer to form a groove; the groove at least penetrates through the pre-oxidation layer and the barrier layer and exposes at least part of the active region of the substrate; doping the substrate in the groove so as to at least form a substrate doped region in the substrate at the bottom of the groove; forming a field region oxide layer in the substrate doped region; the growth temperature of the field region oxide layer is greater than a target temperature, and the growth pressure of the field region oxide layer is greater than a target pressure; wherein under the same growth condition, the growth rate of the field region oxide layer is greater than that of the front oxide layer. Thickness control of the field region oxide layer is facilitated, the thickness of the field region oxide layer is made to be in a micron order, and the beak effect and the leucorrhea effect are effectively improved on the premise that the voltage resistance of the semiconductor structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for manufacturing the same. Background Art

[0002] In current transient voltage suppressors (TVS), a trench structure is usually used to improve the high-voltage resistance of the device. In actual applications, transient high voltage (up to 850V) will appear at the input end of the TVS, which can easily lead to device breakdown. Therefore, it is necessary to use a field oxide layer in the trench structure to improve the voltage resistance of the TVS device.

[0003] However, in the process of forming the field oxide layer, the bird's beak effect and white ribbon effect (WRE) problems are prone to occur due to unreasonable thickness. Since the angle of the bird's beak in the bird's beak effect is proportional to the thickness of the field oxide layer, if the thickness of the field oxide layer is too thick, the bird's beak effect will be easily aggravated. Moreover, if the thickness of the field oxide layer is too thin, it will not be able to offset the stress of the nitride layer on the substrate, which will easily cause substrate dislocation problems and form defects, thereby resulting in reduced device yield and reduced device performance. Summary of the invention

[0004] Based on this, an embodiment of the present application provides a semiconductor structure and a manufacturing method thereof, which is conducive to controlling the thickness of the field oxide layer, and making the thickness of the field oxide layer reach the micron level, thereby effectively improving the bird's beak effect and white band effect while improving the voltage resistance performance of the semiconductor structure.

[0005] In order to achieve the above-mentioned purpose, on the one hand, some embodiments of the present application provide a semiconductor structure and a method for manufacturing the same. The method for manufacturing the semiconductor structure includes: providing a substrate; one side of the substrate has a pre-oxide layer and a barrier layer stacked in sequence from bottom to top; etching the pre-oxide layer and the barrier layer to form a groove; the groove at least penetrates the pre-oxide layer and the barrier layer and exposes at least part of the active area of ​​the substrate; doping the substrate in the groove to form a substrate doping region at least in the substrate at the bottom of the groove; forming a field oxide layer in the substrate doping region; the growth temperature of the field oxide layer is greater than the target temperature, and the growth pressure of the field oxide layer is greater than the target pressure; wherein, under the same growth conditions, the growth rate of the field oxide layer is greater than the growth rate of the pre-oxide layer.

[0006] In some embodiments, the thickness of the field oxide layer is positively correlated with the doping concentration of the substrate doping region, the target temperature, and the target pressure.

[0007] In some embodiments, the thickness of the field oxide layer ranges from 1.5 μm to 2.5 μm.

[0008] In some embodiments, a ratio between the thickness of the pre-oxidation layer and the thickness of the barrier layer ranges from 1:3 to 2:3.

[0009] In some embodiments, the target doping element of the substrate doping region includes boron.

[0010] In some embodiments, the target temperature ranges from 800° C. to 1100° C.; the target pressure ranges from 4 MPa to 15 MPa.

[0011] In some embodiments, the process of forming the field oxide layer includes a local oxidation process of silicon.

[0012] In some embodiments, the front oxide layer and the barrier layer are etched to form a groove, including: forming a mask layer on the side of the barrier layer facing away from the front oxide layer; the mask layer includes a mask pattern for defining the groove; according to the mask pattern, the front oxide layer and the barrier layer are etched to form a groove; the groove penetrates the front oxide layer and the barrier layer and exposes the top surface of the substrate.

[0013] On the other hand, the present disclosure also provides a semiconductor structure according to some embodiments; the semiconductor structure includes a substrate, a pre-oxide layer, a barrier layer, a trench, a substrate doping region and a field oxide layer; the pre-oxide layer is located on one side of the substrate; the barrier layer is located on the side of the pre-oxide layer facing away from the substrate; the trench at least penetrates the pre-oxide layer and the barrier layer and exposes at least part of the active area of ​​the substrate; the substrate doping region is located at least in the substrate at the bottom of the trench; the field oxide layer is located in the substrate doping region; wherein the growth temperature of the field oxide layer is greater than the target temperature, and the growth pressure of the field oxide layer is greater than the target pressure; under the same growth conditions, the growth rate of the field oxide layer is greater than the growth rate of the pre-oxide layer.

[0014] In some embodiments, at least a portion of the field oxide layer is located inside the substrate, and a surface of the field oxide layer facing away from the substrate is higher than a surface of the substrate.

[0015] The embodiments of the present application may or at least have the following advantages:

[0016] In the embodiment of the present application, a substrate doping region is formed in the substrate at the bottom of the groove, so as to relatively increase the oxidation rate of the substrate doping region; and, since the growth rate of the field region oxide layer depends on the rate at which the oxidant moves from the gas phase to the substrate interface, in the process of forming the field region oxide layer in the substrate doping region, the growth temperature of the field region oxide layer is greater than the target temperature, and the growth pressure is greater than the target pressure, so that the growth rate of the field region oxide layer can be effectively controlled. In this way, the oxidation rate of the substrate doping region is increased, which is conducive to making the thickness of the field region oxide layer micrometer-level, so as to effectively improve the withstand voltage performance of the semiconductor structure and prevent the device breakdown problem caused by transient high voltage at the input end of the device; at the same time, by controlling the growth temperature and growth pressure of the field region oxide layer, the thickness of the field region oxide layer is controlled, and the bird's beak effect (bird's beak) caused by the excessive thickness of the field region oxide layer and the white ribbon effect (WRE) caused by the excessive thickness of the field region oxide layer and the substrate dislocation problem are effectively improved, which is conducive to improving the device yield and device performance.

[0017] The details of one or more embodiments of the present application are set forth in the following drawings and description. Other features, objects, and advantages of the present application will become apparent from the description, drawings, and claims. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0019] Figure 1 A schematic flow chart of a method for manufacturing a semiconductor structure provided in some embodiments;

[0020] Figure 2 A schematic flow chart of another method for manufacturing a semiconductor structure provided in some embodiments;

[0021] Figure 3 A schematic flow chart of another method for manufacturing a semiconductor structure provided in some embodiments;

[0022] Figure 4 is a schematic structural diagram of a substrate provided in some embodiments;

[0023] Figure 5 A schematic diagram of a structure obtained after forming a groove provided in some embodiments;

[0024] Figure 6A schematic diagram of a structure obtained after forming a substrate doping region provided in some embodiments;

[0025] Figure 7 A schematic diagram of a structure obtained after forming a field oxide layer provided in some embodiments;

[0026] Figure 8 A schematic diagram of a semiconductor structure provided in some embodiments;

[0027] Fig. 9 A scanning electron microscope image of a semiconductor structure provided in some embodiments.

[0028] Description of reference numerals:

[0029] 1. Substrate, 2. Pre-oxide layer, 3. Barrier layer, G. Trench, A. Substrate doping region, 4. Field oxide layer, P. Mask layer. DETAILED DESCRIPTION

[0030] In order to facilitate understanding of the present application, the present application will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present application are given in the drawings. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application belongs. The terms used herein in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application.

[0032] It should be understood that when an element or layer is referred to as being "on," "adjacent to," or "connected to" other elements or layers, it may be directly on, adjacent to, connected to, or coupled to other elements or layers, or there may be intervening elements or layers. It should be understood that, although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types, and / or portions, these elements, components, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer, doping type, or portion from another element, component, region, layer, doping type, or portion. Therefore, without departing from the teachings of the present application, the first element, component, region, layer, doping type, or portion discussed below may be represented as a second element, component, region, layer, or portion.

[0033] When used herein, the singular forms "a", "an", and "said / the" may also include plural forms, unless the context clearly indicates otherwise. It should also be understood that when the terms "consisting of" and / or "comprising" are used in this specification, the presence of the features, integers, steps, operations, elements and / or parts can be determined, but the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups is not excluded. At the same time, when used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0034] Embodiments of the invention are described herein with reference to cross-sectional views that are schematic representations of idealized embodiments (and intermediate structures) of the present application, such that variations in the shapes shown due to, for example, manufacturing techniques and / or tolerances are anticipated. Embodiments of the present application should not be limited to the specific shapes of the regions shown herein, but include deviations in shapes due to, for example, manufacturing techniques. Therefore, the regions shown in the figures are schematic in nature, their shapes do not represent the actual shapes of the regions of the device, and do not limit the scope of the present application.

[0035] The embodiment of the present application provides a semiconductor structure and a manufacturing method thereof, which are conducive to achieving thickness control of the field oxide layer, and the thickness of the field oxide layer is reduced to micron level, while improving the voltage resistance performance of the semiconductor structure, effectively improving the bird's beak effect and white ribbon effect (White Ribben Effect, referred to as WRE).

[0036] In order to achieve the above objectives, on the one hand, some embodiments of the present application provide a semiconductor structure and a method for manufacturing the same.

[0037] In some embodiments, see Figure 1 , the manufacturing method of the semiconductor structure includes the following steps S100~S400.

[0038] S100, providing a substrate; one side of the substrate has a pre-oxidation layer and a barrier layer stacked in sequence from bottom to top.

[0039] S200, etching the pre-oxide layer and the barrier layer to form a trench; the trench at least penetrates the pre-oxide layer and the barrier layer and exposes at least a portion of the active area of ​​the substrate.

[0040] S300 , doping the substrate in the trench to form a substrate doping region at least in the substrate at the bottom of the trench.

[0041] S400, forming a field oxide layer in the doped region of the substrate to obtain a semiconductor structure; the growth temperature of the field oxide layer is greater than the target temperature, and the growth pressure of the field oxide layer is greater than the target pressure; wherein, under the same growth conditions, the growth rate of the field oxide layer is greater than the growth rate of the pre-oxide layer.

[0042] In the embodiment of the present application, a substrate doping region is formed in the substrate at the bottom of the groove, so as to relatively increase the oxidation rate of the substrate doping region; and, since the growth rate of the field region oxide layer depends on the rate at which the oxidant moves from the gas phase to the substrate interface, in the process of forming the field region oxide layer in the substrate doping region, the growth temperature of the field region oxide layer is greater than the target temperature, and the growth pressure is greater than the target pressure, so that the growth rate of the field region oxide layer can be effectively controlled. In this way, the oxidation rate of the substrate doping region is increased, which is conducive to making the thickness of the field region oxide layer micrometer-level, so as to effectively improve the withstand voltage performance of the semiconductor structure and prevent the device breakdown problem caused by transient high voltage at the input end of the device; at the same time, by controlling the growth temperature and growth pressure of the field region oxide layer, the thickness of the field region oxide layer is controlled, and the bird's beak effect (bird's beak) caused by the excessive thickness of the field region oxide layer and the white ribbon effect (WRE) caused by the excessive thickness of the field region oxide layer and the substrate dislocation problem are effectively improved, which is conducive to improving the device yield and device performance.

[0043] In some embodiments, see Figure 2 , step S200 includes the following steps S210~S220.

[0044] S210, forming a mask layer on a side of the barrier layer away from the front oxide layer; the mask layer includes a mask pattern for defining a trench.

[0045] S220, etching the front oxide layer and the barrier layer according to the mask pattern to form a trench; the trench penetrates the front oxide layer and the barrier layer and exposes the top surface of the substrate.

[0046] In some embodiments, see Figure 3 Before step S400, the method for manufacturing the semiconductor structure further includes the following step S401.

[0047] S401, removing the mask layer.

[0048] It should be understood that although Figure 1~Figure 3 The steps in the flowchart are shown in sequence as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified in this document, there is no strict order restriction for the execution of these steps, and these steps can be executed in other orders. Moreover, Figure 1~Figure 3At least part of the steps may include multiple steps or multiple stages. These steps or stages are not necessarily performed at the same time, but can be performed at different times. The execution order of these steps or stages is not necessarily sequential, but can be performed in turn or alternately with other steps or at least part of the steps or stages in other steps.

[0049] In order to more clearly illustrate the manufacturing method of the semiconductor structure in some of the above embodiments, the following embodiments are combined with Figure 4~Figure 8 Understand.

[0050] In some embodiments, the method for manufacturing a semiconductor structure includes steps S100 to S400.

[0051] In step S100, refer to Figure 4 , a substrate 1 is provided; one side of the substrate 1 has a pre-oxidation layer 2 and a barrier layer 3 stacked in sequence from bottom to top.

[0052] For example, the substrate 1 can be made of semiconductor material, insulating material, conductor material or any combination thereof. The substrate 1 can be a single-layer structure or a multi-layer structure. For example, the substrate 1 can be a silicon (Si) substrate, a silicon germanium (SiGe) substrate, a silicon germanium carbon (SiGeC) substrate, a silicon carbide (SiC) substrate, a gallium arsenide (GaAs) substrate, an indium arsenide (InAs) substrate, an indium phosphide (InP) substrate or other III / V semiconductor substrates or II / VI semiconductor substrates. Alternatively, for example, the substrate 1 can be a layered substrate including Si / SiGe, Si / SiC, silicon on insulator (SOI) or silicon germanium on insulator. Therefore, the type of substrate 1 should not limit the scope of protection of the present application.

[0053] For example, the material of the front oxide layer 2 (PAD Oxide) includes but is not limited to oxide (Oxide); the material of the front oxide layer 2 may be silicon oxide (SiO x ), such as silicon monoxide (SiO) or silicon dioxide (SiO2).

[0054] For example, the material of the barrier layer 3 includes, but is not limited to, nitride; the material of the barrier layer 3 may be, for example, silicon nitride (SiN) or the like.

[0055] In some embodiments, the front oxide layer 2 is reused as a stress buffer layer (Buffer Layer) to buffer the stress generated by the barrier layer 3 on the substrate 1, so as to improve the interface characteristics between the barrier layer 3 and the substrate 1, so as to improve the stability of the overall semiconductor structure, thereby reducing defect problems.

[0056] In some embodiments, the ratio between the thickness of the pre-oxidation layer 2 and the thickness of the barrier layer 3 ranges from 1:3 to 2:3.

[0057] For example, the ratio between the thickness of the pre-oxidation layer 2 and the thickness of the barrier layer 3 may be 1:3, 2:5, 1:2, or 2:3, etc.

[0058] It should be noted that the thickness of the pre-oxide layer 2 refers to the size of the pre-oxide layer 2 in a direction perpendicular to the substrate 1 ; the thickness of the barrier layer 3 refers to the size of the barrier layer 3 in a direction perpendicular to the substrate 1 .

[0059] In the embodiment of the present application, by reasonably matching the thickness of the pre-oxide layer 2 and the thickness of the barrier layer 3, the pre-oxide layer 2 plays a buffering role on the stress between the barrier layer 3 and the substrate 1, effectively preventing the interface (i.e., Si / SiO x Silicon nitride (SiN) is produced at the interface, thereby effectively improving the White Ribben Effect (WRE).

[0060] In step S200, refer to Figure 5 , the pre-oxide layer 2 and the barrier layer 3 are etched to form a trench G; the trench G at least penetrates the pre-oxide layer 2 and the barrier layer 3 and exposes at least a portion of the active area of ​​the substrate 1.

[0061] In some embodiments, step S200 includes steps S210 to S220.

[0062] In step S210 , a mask layer P is formed on a side of the barrier layer 3 facing away from the pre-oxide layer 2 ; the mask layer P includes a mask pattern for defining the trench G.

[0063] By way of example, the material of the mask layer P includes, but is not limited to, photoresist.

[0064] For example, the process for forming the mask layer P includes but is not limited to a glue coating process; the process for forming the mask layer P may be, for example, a spin coating process, a spray coating process, an electrodeposition process, and the like.

[0065] It should be noted that the mask pattern is used to define a local oxidation of silicon (LOCOS) region in the substrate 1 , so as to form a field oxide layer 4 in the defined local oxidation of silicon region in a subsequent process.

[0066] In step S220, please continue to refer to Figure 5According to the mask pattern, the pre-oxide layer 2 and the barrier layer 3 are etched to form a trench G; the trench G penetrates the pre-oxide layer 2 and the barrier layer 3 and exposes the top surface of the substrate 1.

[0067] For example, the etching process of the front oxide layer 2 and the barrier layer 3 includes but is not limited to a dry etching process; the etching process of the front oxide layer 2 and the barrier layer 3 may be, for example, a photolithography process.

[0068] It should be noted that the trench G exposes at least a portion of the active area (Active Area, AA for short) of the substrate 1 .

[0069] In step S300, refer to Figure 6 , doping the substrate 1 in the trench G to form a substrate doping region A at least in the substrate 1 at the bottom of the trench G;

[0070] By way of example, the doping process of the substrate 1 includes but is not limited to an ion implantation (IMP for short) process.

[0071] In some embodiments, the doping concentration of the substrate doping region A is greater than the target concentration.

[0072] In some embodiments, the target doping element of the substrate doping region A includes boron (B).

[0073] In some embodiments, the thickness of the field oxide layer 4 is positively correlated with the doping concentration of the substrate doping region A, the target temperature, and the target pressure.

[0074] It should be noted that during the formation of the field oxide layer 4, the growth of the oxide can be divided into two stages: a linear stage and a parabolic stage. When the thickness of the field oxide layer 4 is less than 150A, the growth of the oxide is in a linear stage, and the control of the growth rate of the oxide is mainly achieved by controlling the reaction rate; when the thickness of the field oxide layer 4 is greater than or equal to 150A, the growth of the oxide is in a parabolic stage, and the control of the growth rate of the oxide is mainly achieved by controlling the diffusion rate. Among them, the growth rate of the oxide in the parabolic stage is much slower than its growth rate in the linear stage, so the greater the thickness of the field oxide layer 4, the slower the growth rate.

[0075] In the embodiment of the present application, a substrate doping region A is formed in the substrate 1, so that during the formation of the field oxide layer 4, the oxide tends to mix with the doping ions (for example, boron ions) in the substrate doping region A, so as to weaken the chemical bond structure (for example, ionic bonds, covalent bonds, etc.) inside the oxide, thereby increasing the diffusion rate, accelerating the oxidation reaction, and effectively increasing the growth rate of the field oxide layer 4 in the parabolic stage, which is conducive to the formation of a thick field oxide layer 4 (for example, a field oxide layer 4 with a thickness of microns), thereby ensuring the voltage resistance performance of the semiconductor structure.

[0076] In step S400, refer to Figure 7 , a field oxide layer 4 is formed in the substrate doping region A to obtain a semiconductor structure; the growth temperature of the field oxide layer 4 is greater than the target temperature, and the growth pressure of the field oxide layer 4 is greater than the target pressure; wherein, under the same growth conditions, the growth rate of the field oxide layer 4 is greater than the growth rate of the pre-oxide layer 2.

[0077] By way of example, the semiconductor structure includes but is not limited to a transient voltage suppressor (TVS for short).

[0078] In some embodiments, the process for forming the field oxide layer 4 includes but is not limited to a high temperature pressurized furnace tube process.

[0079] By way of example, the equipment for forming the field oxide layer 4 includes, but is not limited to, a high-temperature tube furnace.

[0080] By way of example, the field oxide layer 4 is grown by thermal oxidation.

[0081] In the embodiment of the present application, a high temperature and high pressure process is used to form the field oxide layer 4, and the growth temperature of the field oxide layer 4 is controlled to be greater than the target temperature and the growth pressure is controlled to be greater than the target pressure; since the growth rate of the oxide depends on the rate at which the oxidant moves from the gas phase to the surface of the substrate 1 (for example, a silicon substrate), the growth rate of the field oxide layer 4 is positively correlated with the growth pressure and the growth temperature. The use of high pressure and high temperature conditions can effectively accelerate the movement rate of oxygen atoms so that they can pass through the growing field oxide layer 4 more quickly, thereby effectively increasing the growth rate of the field oxide layer 4 in the linear stage and the parabolic stage, which is conducive to the formation of a thick field oxide layer 4 (for example, a field oxide layer with a thickness of micrometers), thereby ensuring the voltage resistance performance of the semiconductor structure.

[0082] In some embodiments, the thickness of the field oxide layer 4 ranges from 1.5 μm to 2.5 μm.

[0083] For example, the thickness of the field oxide layer 4 may be 1.5 μm, 1.8 μm, 2 μm, 2.3 μm or 2.5 μm.

[0084] It should be explained that the thickness of the field oxide layer 4 refers to the size of the field oxide layer 4 in a direction perpendicular to the substrate 1 .

[0085] In some embodiments, the target temperature ranges from 800° C. to 1100° C.; the target pressure ranges from 4 MPa to 15 MPa.

[0086] For example, the target temperature may be 800° C., 900° C., 1000° C., or 1100° C., etc.

[0087] For example, the value of the target pressure may be 4 MPa, 5 MPa, 8 MPa, 10 MPa, 12 MPa or 15 MPa, etc.

[0088] In some embodiments, the process of forming the field oxide layer 4 includes a local oxidation of silicon (LOCOS) process.

[0089] In some embodiments, before step S400 , the method for manufacturing a semiconductor structure further includes step S401 .

[0090] In step S401, refer to Figure 8 , remove the mask layer P.

[0091] For example, the removal process of the mask layer P includes but is not limited to a photoresist removal process; the removal process of the mask layer P may be, for example, a debonding process or the like.

[0092] In summary, in order to verify the effect of the manufacturing method of the semiconductor structure provided in the embodiments of the present application on the thickness control of the field oxide layer 4 in the semiconductor structure and the improvement of the bird's beak effect in the semiconductor structure; in some embodiments, taking the target doping element of the substrate doping region A as boron (B) as an example, the field oxide layer 4 in the semiconductor structure prepared by the manufacturing method of the semiconductor structure provided in some of the above embodiments of the present application is subjected to an electrical microscope scan to obtain a scanning electron microscope image of the field oxide layer 4 as shown in FIG. Fig. 9 As shown. Among them, according to Fig. 9 As can be seen from Figure (a), the thickness of the field oxide layer 4 is about 2 μm, which effectively realizes the thickness control of the field oxide layer 4; Fig. 9 As can be seen from Figure (b), the bird's beak angle is about 70° and the bird's beak length is about 1.3μm, which effectively improves the bird's beak effect.

[0093] As described above, the manufacturing method of the semiconductor structure provided in the embodiment of the present application can achieve thickness control of the field oxide layer 4, effectively improving the bird's beak effect caused by excessive thickness of the field oxide layer 4, thereby facilitating improving device yield and device performance.

[0094] The present application also provides a semiconductor structure according to some embodiments, which can be prepared by the manufacturing method of the semiconductor structure in some of the above embodiments. The semiconductor structure also has the technical advantages of the manufacturing method of the above semiconductor structure. It should be noted that the parts that are the same or corresponding to the above embodiments can refer to the corresponding description of the above embodiments, and will not be described in detail below.

[0095] In some embodiments, see Figure 8 The semiconductor structure includes a substrate 1, a pre-oxide layer 2, a barrier layer 3, a trench G, a substrate doping region A and a field oxide layer 4; the pre-oxide layer 2 is located on one side of the substrate 1; the barrier layer 3 is located on the side of the pre-oxide layer 2 away from the substrate 1; the trench G at least penetrates the pre-oxide layer 2 and the barrier layer 3 and exposes at least part of the active area of ​​the substrate 1; the substrate doping region A is at least located in the substrate 1 at the bottom of the trench G; the field oxide layer 4 is located in the substrate doping region A; wherein the growth temperature of the field oxide layer 4 is greater than the target temperature, and the growth pressure of the field oxide layer 4 is greater than the target pressure; under the same growth conditions, the growth rate of the field oxide layer 4 is greater than the growth rate of the pre-oxide layer 2.

[0096] By way of example, the semiconductor structure includes but is not limited to a transient voltage suppressor (TVS for short).

[0097] For example, the substrate 1 can be made of semiconductor material, insulating material, conductor material or any combination thereof. The substrate 1 can be a single-layer structure or a multi-layer structure. For example, the substrate 1 can be a silicon (Si) substrate, a silicon germanium (SiGe) substrate, a silicon germanium carbon (SiGeC) substrate, a silicon carbide (SiC) substrate, a gallium arsenide (GaAs) substrate, an indium arsenide (InAs) substrate, an indium phosphide (InP) substrate or other III / V semiconductor substrates or II / VI semiconductor substrates. Alternatively, for example, the substrate 1 can be a layered substrate including Si / SiGe, Si / SiC, silicon on insulator (SOI) or silicon germanium on insulator. Therefore, the type of substrate 1 should not limit the scope of protection of the present application.

[0098] For example, the material of the front oxide layer 2 (PAD Oxide) includes but is not limited to oxide (Oxide); the material of the front oxide layer 2 may be silicon oxide (SiO x), such as silicon monoxide (SiO) or silicon dioxide (SiO2).

[0099] For example, the material of the barrier layer 3 includes, but is not limited to, nitride; the material of the barrier layer 3 may be, for example, silicon nitride (SiN) or the like.

[0100] In some embodiments, the front oxide layer 2 is reused as a stress buffer layer (Buffer Layer).

[0101] It should be noted that the stress buffer layer can relieve the stress generated between the substrate 1 and the barrier layer 3 due to factors such as lattice constant mismatch or different thermal expansion coefficients, thereby avoiding defects such as substrate dislocations; the stress buffer layer can also be used to achieve chemical isolation between the substrate 1 and the barrier layer 3 to prevent chemical reactions between the two, thereby ensuring the clarity and stability of the interface between the two; the stress buffer layer can also be used to prevent defects from the substrate 1 (such as dislocations, microcracks, etc.) from propagating to the upper structure, which is beneficial to improving the crystal quality of the upper structure.

[0102] In some embodiments, the thickness of the field oxide layer 4 ranges from 1.5 μm to 2.5 μm.

[0103] For example, the thickness of the field oxide layer 4 may be 1.5 μm, 1.8 μm, 2 μm, 2.3 μm or 2.5 μm.

[0104] It should be noted that the thickness of the field oxide layer 4 refers to the size of the field oxide layer 4 in a direction perpendicular to the substrate 1 .

[0105] In some embodiments, the ratio between the thickness of the pre-oxidation layer 2 and the thickness of the barrier layer 3 ranges from 1:3 to 2:3.

[0106] For example, the ratio between the thickness of the pre-oxidation layer 2 and the thickness of the barrier layer 3 may be 1:3, 2:5, 1:2 or 2:3, etc.

[0107] In the embodiment of the present application, the interface between the substrate 1 (eg, silicon substrate) and the front oxide layer 2 (ie, Si / SiO x No silicon nitride (SiN) is produced at the interface, which effectively improves the White Ribben Effect (WRE).

[0108] It should be noted that the thickness of the pre-oxide layer 2 refers to the size of the pre-oxide layer 2 in a direction perpendicular to the substrate 1 ; the thickness of the barrier layer 3 refers to the size of the barrier layer 3 in a direction perpendicular to the substrate 1 .

[0109] In the embodiment of the present application, the oxidation rate of the substrate doping region A is increased by the substrate doping region A located in the substrate 1 at the bottom of the groove G, which is conducive to making the thickness of the field oxide layer 4 to the micron level, so as to effectively improve the voltage resistance performance of the semiconductor structure and prevent the device breakdown problem caused by the transient high voltage at the input end of the device; at the same time, by controlling the growth temperature of the field oxide layer 4 to be greater than the target temperature and the growth pressure to be greater than the target pressure, the growth temperature and growth pressure of the field oxide layer 4 are controlled, thereby realizing the thickness control of the field oxide layer 4, effectively improving the bird's beak effect (bird's beak) caused by the excessive thickness of the field oxide layer 4 and the white ribbon effect (White Ribbon Effect, WRE for short) caused by the excessive thickness of the field oxide layer 4 and the dislocation problem of the substrate 1, which is conducive to improving the yield and performance of the semiconductor structure.

[0110] In some embodiments, please refer to Figure 8 At least part of the field oxide layer 4 is located inside the substrate 1 , and the surface of the field oxide layer 4 facing away from the substrate 1 is higher than the surface of the substrate 1 .

[0111] The present application also provides a semiconductor device according to some embodiments; the semiconductor device includes a semiconductor structure prepared by a method for manufacturing a semiconductor structure as described in some embodiments of the present application. The semiconductor device also has the technical advantages of the method for manufacturing the aforementioned semiconductor structure. It should be noted that for the parts that are the same or corresponding to the aforementioned embodiments, reference can be made to the corresponding description of the aforementioned embodiments, and will not be described in detail below.

[0112] By way of example, the semiconductor device includes a transient voltage suppressor (TVS for short).

[0113] By way of example, the semiconductor device includes, but is not limited to, a transient voltage suppressor blocking type surge protector.

[0114] The technical features of the above embodiments may be arbitrarily combined. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0115] The above-mentioned embodiments only express several implementation methods of the present application, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present application, and these all belong to the protection scope of the present application.

Claims

1. A method for manufacturing a semiconductor structure, characterized in that: include: providing a substrate; One side of the substrate has a pre-oxidation layer and a barrier layer stacked in sequence from bottom to top; Etching the front oxide layer and the barrier layer to form a trench; The trench at least penetrates the pre-oxidation layer and the barrier layer and exposes at least a portion of the active area of ​​the substrate; doping the substrate in the trench to form a substrate doping region at least in the substrate at the bottom of the trench; A field region oxide layer is formed in the substrate doping region to obtain a semiconductor structure; the growth temperature of the field region oxide layer is greater than a target temperature, and the growth pressure of the field region oxide layer is greater than a target pressure; Wherein, under the same growth conditions, the growth rate of the field oxide layer is greater than the growth rate of the front oxide layer.

2. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The thickness of the field region oxide layer is positively correlated with the doping concentration of the substrate doping region, the target temperature, and the target pressure.

3. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The thickness of the field oxide layer ranges from 1.5 μm to 2.5 μm.

4. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The ratio between the thickness of the pre-oxidation layer and the thickness of the barrier layer ranges from 1:3 to 2:

3.

5. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The target doping element of the substrate doping region includes boron.

6. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The target temperature has a value range of 800° C. to 1100° C.; the target pressure has a value range of 4 MPa to 15 MPa.

7. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The process for forming the field oxide layer includes a local oxidation process of silicon.

8. The method for manufacturing a semiconductor structure according to claim 1, wherein: The etching of the front oxide layer and the barrier layer to form a trench comprises: forming a mask layer on a side of the barrier layer away from the front oxide layer; the mask layer comprises a mask pattern for defining the trench; The pre-oxide layer and the barrier layer are etched according to the mask pattern to form a trench; the trench penetrates the pre-oxide layer and the barrier layer and exposes the top surface of the substrate.

9. A semiconductor structure, characterized in that: include: substrate; A front oxide layer, located on one side of the substrate; A barrier layer, located on a side of the front oxide layer facing away from the substrate; A groove at least penetrating the front oxide layer and the barrier layer and exposing at least a portion of the active area of ​​the substrate; a substrate doping region, located at least in the substrate at the bottom of the trench; A field region oxide layer, located in the substrate doping region; The growth temperature of the field oxide layer is greater than the target temperature, and the growth pressure of the field oxide layer is greater than the target pressure; under the same growth conditions, the growth rate of the field oxide layer is greater than the growth rate of the pre-oxide layer.

10. The semiconductor structure according to claim 7, characterized in that: At least a portion of the field oxide layer is located inside the substrate, and a surface of the field oxide layer facing away from the substrate is higher than a surface of the substrate.