Contact-optimized oxide semiconductor transistor and preparation method thereof
By inserting oxide semiconductor contact layers with different carrier concentrations into the contact area of the oxide semiconductor field effect transistor, a dipole pair is formed, which solves the problem of increased contact resistance and achieves the density improvement of high-performance small-size transistors and integrated circuits , while maintaining the stability of the threshold voltage.
Patent Information
- Application Number
- CN202411121504.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-22
AI Technical Summary
The reduction in contact length of oxide semiconductor transistors leads to an increase in contact resistance, limiting the open state performance of the transistor, and high carrier concentration will lead to a negative shift in the threshold voltage, affecting the normal operation of the integrated circuit.
An oxide semiconductor contact layer is inserted into the contact area of the oxide semiconductor field effect transistor. The carrier concentration is different from the channel layer, forming a dipole pair, increasing the carrier concentration below the contact area and reducing the contact resistance , and separate the carrier concentrations of the channel and the source and drain regions to keep the threshold voltage unchanged.
A high-performance small-size transistor is realized, which reduces contact resistance, increases the density of the integrated circuit, breaks the contradiction between the threshold voltage and the open-state current, and significantly improves the electrical characteristics of the oxide semiconductor field effect transistor.
Smart Images

Figure CN119008702A_ABST
Abstract
Description
Technical Field
[0001] The patent of this invention relates to a contact-optimized oxide semiconductor transistor and a preparation method, belonging to the field of information materials and device technology. Background Art
[0002] In the past decade, oxide semiconductor materials have been widely used in the display field due to their advantages of high transmittance, high mobility and large-area uniformity, and their device sizes are mostly at the micron level. In recent years, with the continuous development of the integrated circuit industry, oxide semiconductor materials with low thermal budget processes have shown great potential in the fields of logic, storage and radio frequency compatible with the back-end. At present, through the optimization of materials and preparation processes, oxide transistors with a channel length of less than 10 nanometers have been realized, but the reduction in the lateral size of the transistor is mainly reflected in the miniaturization of the contacted gate pitch (CGP), including the channel length and the contact length. At present, the contact length of oxide transistors remains at the submicron level, and as the contact length decreases, the contact resistance increases, which limits the on-state performance of the transistor. Therefore, in order to achieve high-density, low-power, and high-performance oxide semiconductor transistors, the present invention proposes a contact-optimized oxide semiconductor field effect transistor and a preparation method. This invention patent has great potential in improving the performance of oxide semiconductor transistors and their back-end compatible process integration density.
[0003] As the channel length and contact length of oxide semiconductor transistors shrink in size, the impact of contact resistance on on-state performance becomes more significant. According to the unique percolation conduction mechanism of oxide semiconductors, increasing carrier concentration can increase carrier mobility, thereby reducing contact resistance and increasing on-state current. However, high carrier concentration can cause a negative shift in the threshold voltage and even affect the normal shutdown of the transistor, which is not conducive to integrated circuit applications. Therefore, seeking a coordinated optimization process for threshold voltage and on-state current is crucial to promoting the application of oxide semiconductors. Summary of the invention
[0004] In order to solve the size shrinking bottleneck of existing oxide semiconductor devices and improve the density of integrated circuits, the present invention proposes a contact-optimized oxide semiconductor field effect transistor and a preparation method thereof.
[0005] To achieve the above purpose, the technical solution adopted by the present invention is as follows:
[0006] An oxide semiconductor field effect transistor comprises a substrate, a gate electrode layer, a gate dielectric layer, an oxide semiconductor channel layer and a source / drain metal electrode layer, characterized in that an oxide semiconductor contact layer is in-situ inserted into the contact region between the source / drain metal electrode layer and the oxide semiconductor channel layer, the carrier concentration of the oxide semiconductor contact layer is different from the carrier concentration of the oxide semiconductor channel layer, and a dipole pair is formed at the contact interface.
[0007] Furthermore, the transistor device structure includes but is not limited to a bottom gate structure (back-gate), a top gate structure (top-gate), a dual-gate structure (dual-gate), a fin gate structure (FinFET), a gate all around structure (GAA), a channel ring structure (CAA), a vertical channel structure (VFET), etc.
[0008] Furthermore, the substrate is a glass substrate, a silicon substrate, a silicon carbide substrate, a diamond substrate, a diamond-like carbon film substrate, or a PI or PET flexible substrate.
[0009] Furthermore, the gate electrode layer material is Ti, Ni, Au, Pt, Pd, Al, W, Y, Sc, Mo and their alloys, TiN, metallic oxide ITO, IZO, and its thickness is 5 to 300 nanometers.
[0010] Furthermore, the gate dielectric layer material is SiO2, SiN x , Al2O3, HfO2, HfSiOx, HfLaO x 、HfAlOx、HfZrO x And its multi-doped combination medium, the thickness of which is 2 to 100 nanometers.
[0011] Furthermore, the channel layer material is a composite material of In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO, ITWO oxide semiconductor film and a multi-layer oxide film stack, and its thickness is 0.5 to 50 nanometers.
[0012] Furthermore, the oxide semiconductor contact layer material is In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO, ITWO oxide semiconductor thin film and a composite material of multi-layer oxide thin film stacking, and its thickness is 0.5 to 50 nanometers.
[0013] Furthermore, the source and drain metal electrode layer materials are Ti, Ni, Au, Pt, Pd, W, Al, Y, Sc, Mo and their alloys, TiN, metallic oxide ITO, IZO, and their thickness is 3 to 300 nanometers.
[0014] The present invention further provides a method for preparing a dual-gate structure oxide semiconductor field effect transistor, comprising the following process steps:
[0015] Step 1.1, cleaning the substrate;
[0016] Step 1.2, defining the gate pattern by optical lithography, electron beam lithography or laser direct writing, and preparing the bottom gate metal electrode layer by electron beam evaporation, magnetron sputtering, thermal evaporation or atomic layer deposition;
[0017] Step 1.3, preparing a bottom gate dielectric layer by thermal oxidation, plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition;
[0018] Step 1.4, preparing an oxide semiconductor channel layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition;
[0019] Step 1.5, preparing an oxide semiconductor contact layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition;
[0020] Step 1.6, preparing source and drain contact metal electrodes by electron beam evaporation, magnetron sputtering, ion beam sputtering, thermal evaporation or atomic layer deposition process;
[0021] Step 1.7, preparing a top gate dielectric by the same method as in step 1.3;
[0022] Step 1.8, prepare the top gate electrode using the same method as in step 1.2.
[0023] Furthermore, a method for preparing a vertical structure oxide semiconductor field effect transistor includes the following process steps:
[0024] Step 2.1, cleaning the substrate;
[0025] Step 2.2, preparing a source electrode and an oxide semiconductor contact layer by electron beam evaporation, magnetron sputtering, ion beam sputtering, thermal evaporation or atomic layer deposition;
[0026] Step 2.3, preparing a passivation layer by plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition;
[0027] Step 2.4, defining the gate pattern by optical lithography, electron beam lithography or laser direct writing, and preparing the gate electrode by electron beam evaporation, magnetron sputtering, thermal evaporation or atomic layer deposition;
[0028] Step 2.5, preparing a low dielectric constant passivation layer using the same method as in step 2.3;
[0029] Step 2.6, using optical lithography, electron beam lithography or laser direct writing to define the channel region, and using dry or wet etching to open the channel region to form a groove;
[0030] Step 2.7, preparing a gate dielectric layer by thermal oxidation, plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition, wherein the gate dielectric layer is located between the gate electrode layer and the oxide semiconductor channel layer;
[0031] Step 2.8, preparing an oxide semiconductor channel layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition;
[0032] Step 2.9, growing a filling layer in the trench using a plasma enhanced chemical vapor deposition or atomic layer deposition process;
[0033] Step 2.10, the oxide semiconductor contact layer and the metal drain electrode layer are prepared by using coating, baking, photolithography, development, electron beam evaporation, magnetron sputtering, and stripping processes.
[0034] The beneficial effects of the present invention are as follows:
[0035] The present invention inserts an oxide semiconductor contact layer in the contact area between the source and drain metal electrode layers and the oxide semiconductor channel layer. The carrier concentration of the oxide semiconductor contact layer is different from that of the oxide semiconductor channel layer, and a dipole pair is formed at the contact interface, thereby increasing the carrier concentration below the contact area, thereby reducing the contact resistance and transmission length, realizing high-performance small-size transistors, and facilitating the improvement of integrated circuit density. At the same time, the present invention separates the carrier concentrations of the channel and the source and drain regions, and simultaneously realizes low contact resistance and positive threshold voltage. The present invention relates to all other structures formed by equivalent transformation or equivalent transformation, such as bottom gate structure, top gate structure, double gate structure, fin-type gate structure, surrounding gate structure, ring channel structure, vertical channel structure, etc. That is, this contact method does not change the carrier concentration in the channel region, can keep the threshold voltage unchanged, and breaks the contradiction between the threshold voltage and the on-state current of the oxide semiconductor. It has great potential in improving the electrical characteristics of oxide semiconductor field effect transistors and reducing the overall size of transistors. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is a schematic diagram of a dual-gate structure oxide semiconductor field effect transistor according to a specific embodiment of the present invention;
[0037] Figure 2This is a flow chart of a method for preparing a dual-gate structure oxide semiconductor field effect transistor according to a specific embodiment of the present invention;
[0038] Figure 3 It is a schematic structural diagram of a vertical structure oxide semiconductor field effect transistor according to a specific embodiment of the present invention;
[0039] Figure 4 This is a flow chart of a method for preparing a vertical structure oxide semiconductor field effect transistor according to a specific embodiment of the present invention;
[0040] Figure 5 for Figure 1 — Figure 4 Legend for the figure;
[0041] Figure 6 The diagram is a comparison diagram of an oxide semiconductor transistor using an oxide semiconductor contact prepared by the present invention and a planar oxide semiconductor transistor using a metal contact, wherein (a) is a transfer characteristic curve; and (b) is a transfer transconductance curve. DETAILED DESCRIPTION
[0042] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present invention, and cannot be interpreted as limiting the present invention.
[0043] The present invention provides a contact-optimized oxide semiconductor field effect transistor and a preparation method thereof. The device structure includes but is not limited to a back-gate structure, a top-gate structure, a dual-gate structure, a fin-type gate structure (FinFET), a gate-all-around structure (GAA), a channel-around structure (CAA), a vertical channel structure (VFET), etc.
[0044] Figure 1 A contact-optimized dual-gate structure oxide semiconductor field effect transistor; comprising a substrate, a bottom gate electrode layer, a bottom gate dielectric layer, an oxide semiconductor channel layer, an oxide semiconductor contact layer, a source / drain metal electrode layer, a top gate dielectric layer and a top gate electrode layer stacked from bottom to top, wherein the carrier concentration of the oxide semiconductor contact layer is different from the carrier concentration of the oxide semiconductor channel layer, and a dipole pair is formed at the contact interface.
[0045] The present invention provides a method for preparing the above-mentioned dual-gate structure oxide semiconductor field effect transistor, which specifically comprises the following steps:
[0046] S001: Get and use a clean substrate. Use RCA1 to clean particles and organic matter on the substrate, and blow dry with high-purity nitrogen after cleaning.
[0047] The substrate may be a glass substrate, a silicon substrate, a silicon carbide substrate, a diamond substrate, a diamond-like carbon film substrate, or a flexible substrate such as PI, PET, etc. In this embodiment, the substrate is a high-resistance silicon substrate with a resistivity of >10000Ω·cm.
[0048] S002, the bottom gate electrode is prepared on the cleaned substrate by using the process steps of coating, baking, photolithography, development, electron beam evaporation, stripping, etc. In this embodiment, the bottom gate metal layer is 20nm Pt.
[0049] S003, using atomic layer deposition process to prepare a gate dielectric layer. In this embodiment, the bottom gate dielectric layer is 5nm HfLaO x .
[0050] S004, the preparation of the channel active region is completed by using process steps such as coating, baking, photolithography, development, magnetron sputtering, and stripping. In this embodiment, the oxide semiconductor channel layer is 8nm IGZO.
[0051] S005, using photolithography, magnetron sputtering and electron beam evaporation to prepare oxide semiconductor contact layer and metal source and drain electrode layer, using lift-off technology to complete source and drain region definition. In this embodiment, the oxide semiconductor contact layer is 8nm ITO, and the source and drain contact electrodes are 20nm Ni.
[0052] Furthermore, in order to achieve a contact electrode length of <20nm, we selected photoresists with higher exposure accuracy, such as PMMA A3, PMMA A2, ZEP520A, ARP6200.09, etc., and combined them with process technologies such as low-temperature development.
[0053] S006, using an atomic layer deposition process to prepare a top gate dielectric layer. In this embodiment, the top gate dielectric layer is 5nm HfLaO x .
[0054] S007, preparing a top gate electrode by using process steps such as photoresist, baking, photolithography, development, electron beam evaporation, and stripping. In this embodiment, the top gate electrode layer is 20 nm Pt.
[0055] S008, using photolithography and etching process, after etching and removing the resist, the test electrode is exposed.
[0056] The above S001-S008 correspond to Figure 2 (1)-(8) shown.
[0057] Figure 3The invention is a vertical structure oxide semiconductor field effect transistor, comprising a substrate, a source / drain metal electrode layer, a gate electrode layer, an oxide semiconductor channel layer, and a drain and source metal electrode layer. The oxide semiconductor channel layer is in a groove shape, an oxide semiconductor contact layer is arranged between the bottom of the groove of the oxide semiconductor channel layer and the source and drain metal electrode layers, a gate dielectric layer is arranged outside the groove, the gate dielectric layer is located between the gate electrode layer and the oxide semiconductor channel layer, a filling layer is grown in the groove of the oxide semiconductor channel layer, an oxide semiconductor contact layer is arranged between the top of the groove of the oxide semiconductor channel layer and the drain and source metal electrode layers, a passivation layer is arranged between the source and drain metal electrode layers, the gate electrode layer and the oxide semiconductor channel layer, the carrier concentration of the oxide semiconductor contact layer is different from the carrier concentration of the oxide semiconductor channel layer, and a dipole pair is formed at the contact interface.
[0058] The present invention provides a method for preparing the vertical structure oxide semiconductor field effect transistor, comprising the following steps:
[0059] S001: Get and use a clean substrate. Use RCA1 to clean particles and organic matter on the substrate, and blow dry with high-purity nitrogen after cleaning.
[0060] The substrate may be a glass substrate, a silicon substrate, a silicon carbide substrate, a diamond substrate, a diamond-like carbon film substrate, or a flexible substrate such as PI, PET, etc. In this embodiment, the substrate is a high-resistance silicon substrate with a resistivity of >10000Ω·cm.
[0061] S002, the cleaned substrate is subjected to the steps of coating, baking, photolithography, development, electron beam evaporation, magnetron sputtering, stripping, etc. to complete the preparation of the metal source electrode layer and the oxide semiconductor contact layer. In this embodiment, the oxide semiconductor contact layer is 8nm ITO, and the source and drain contact electrodes are 20nm Ni.
[0062] S003, growing a SiO2 passivation layer by plasma enhanced chemical vapor deposition or atomic layer deposition process.
[0063] S004, preparing a gate electrode by using the process steps of coating, baking, photolithography, development, electron beam evaporation, stripping, etc. In this embodiment, the gate electrode is 20nm Pt.
[0064] S005, growing a SiO2 passivation layer by plasma enhanced chemical vapor deposition or atomic layer deposition process.
[0065] S006, using process steps such as photoresist coating, baking, photolithography, development, etching, and photoresist stripping to complete the opening of the channel area and form a groove.
[0066] S007, using an atomic layer deposition process to prepare a gate dielectric layer outside the trench, the gate dielectric layer is located between the gate electrode layer and the oxide semiconductor channel layer. In this embodiment, the gate dielectric layer is 5nm HfLaO x .
[0067] S008, preparing the oxide semiconductor channel layer by atomic layer deposition, coating, baking, photolithography, development, etching and other process steps. In this embodiment, the oxide semiconductor channel layer is 8nm IGZO.
[0068] S009, growing a filling layer in the trench by using a plasma enhanced chemical vapor deposition or atomic layer deposition process. In this embodiment, the filling layer is SiO2.
[0069] S010, the oxide semiconductor contact layer and the metal drain electrode layer are prepared by coating, baking, photolithography, development, electron beam evaporation, magnetron sputtering, stripping and other process steps. In this embodiment, the oxide semiconductor contact layer is 8nm ITO, and the source and drain contact electrodes are 20nm Ni.
[0070] The above S001-S010 correspond to Figure 4 (1)-(10) shown.
[0071] Compared with the prior art, the present invention significantly reduces the contact resistance and shortens the effective transmission length without affecting the channel threshold voltage. Compared with pure metal contact, it achieves better electrical performance with smaller contact size. Figure 6 As shown in the figure, the transfer characteristic curve and transfer transconductance curve of the planar oxide semiconductor transistor prepared by the metal contact and the oxide semiconductor contact of the present invention are compared. The on-state current and transfer transconductance of the oxide semiconductor transistor with a channel length of 30nm and a contact length of 50nm are increased by more than 2 times after the oxide semiconductor contact insertion layer is used.
[0072] It should be noted that the above-mentioned embodiments illustrate rather than limit the invention and that those skilled in the art will be able to design alternative embodiments without departing from the scope of the appended claims.
Claims
1. An oxide semiconductor field effect transistor, comprising a substrate, a gate electrode layer, a gate dielectric layer, an oxide semiconductor channel layer, and source and drain metal electrode layers, characterized in that: An oxide semiconductor contact layer is in-situ inserted into the contact region between the source and drain metal electrode layers and the oxide semiconductor channel layer. The carrier concentration of the oxide semiconductor contact layer is different from that of the oxide semiconductor channel layer, and a dipole pair is formed at the contact interface.
2. The oxide semiconductor field effect transistor according to claim 1, wherein: The structure of the oxide semiconductor field effect transistor is a bottom gate structure, a top gate structure, a double gate structure, a fin gate structure, a surround gate structure, a ring channel structure or a vertical channel structure.
3. The oxide semiconductor field effect transistor according to claim 1, wherein: The substrate is a glass substrate, a silicon substrate, a silicon carbide substrate, a diamond substrate, a diamond-like carbon film substrate or a PI or PET flexible substrate.
4. The oxide semiconductor field effect transistor according to claim 1, wherein: The gate electrode layer material is Ti, Ni, Au, Pt, Pd, Al, W, Y, Sc, Mo and their alloys, TiN, metallic oxide ITO, IZO, and its thickness is 5 to 300 nanometers.
5. The oxide semiconductor field effect transistor according to claim 1, wherein: The gate dielectric layer material is SiO2, SiN x , Al2O3, HfO2, HfSiOx, HfLaO x 、HfAlOx、HfZrO x And its multi-doped combination medium, the thickness of which is 2 to 100 nanometers.
6. The oxide semiconductor field effect transistor according to claim 1, wherein: The channel layer material is In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO, ITWO oxide semiconductor film and a composite material of multi-layer oxide film stacking, and its thickness is 0.5 to 50 nanometers.
7. The oxide semiconductor field effect transistor according to claim 1, wherein: The oxide semiconductor contact insertion layer material is In2O3, SnO2, Ga2O3, ZnO, ITO, IGO, IZO, IGZO, IAZO, ITZO, IWO, ITWO oxide semiconductor film and a composite material of multi-layer oxide film stacking, and its thickness is 0.5 to 50 nanometers.
8. The oxide semiconductor field effect transistor according to claim 1, wherein: The source / drain metal electrode layer material is Ti, Ni, Au, Pt, Pd, W, Al, Y, Sc, Mo and their alloys, TiN, metallic oxide ITO, IZO, and its thickness is 3 to 300 nanometers.
9. A method for preparing a dual-gate structure oxide semiconductor field effect transistor, comprising the following process steps: Step 1.1, cleaning the substrate; Step 1.2, defining the gate pattern by optical lithography, electron beam lithography or laser direct writing, and preparing the bottom gate metal electrode layer by electron beam evaporation, magnetron sputtering, thermal evaporation or atomic layer deposition; Step 1.3, preparing a bottom gate dielectric layer by thermal oxidation, plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition; Step 1.4, preparing an oxide semiconductor channel layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition; Step 1.5, preparing an oxide semiconductor contact layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition; Step 1.6, preparing source and drain contact metal electrodes by electron beam evaporation, magnetron sputtering, ion beam sputtering, thermal evaporation or atomic layer deposition process; Step 1.7, preparing a top gate dielectric by the same method as in step 1.3; Step 1.8, prepare the top gate electrode using the same method as in step 1.
2.
10. A method for preparing a vertical structure oxide semiconductor field effect transistor, comprising the following process steps: Step 2.1, cleaning the substrate; Step 2.2, preparing a source electrode and an oxide semiconductor contact layer by electron beam evaporation, magnetron sputtering, ion beam sputtering, thermal evaporation or atomic layer deposition; Step 2.3, preparing a passivation layer by plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition; Step 2.4, defining the gate pattern by optical lithography, electron beam lithography or laser direct writing, and preparing the gate electrode by electron beam evaporation, magnetron sputtering, thermal evaporation or atomic layer deposition; Step 2.5, preparing a low dielectric constant passivation layer using the same method as in step 2.3; Step 2.6, using optical lithography, electron beam lithography or laser direct writing to define the channel region, and using dry or wet etching to open the channel region to form a groove; Step 2.7, preparing a gate dielectric layer by thermal oxidation, plasma enhanced chemical vapor deposition, inductively coupled plasma chemical vapor deposition, magnetron sputtering, electron beam evaporation, pulsed vapor deposition or atomic layer deposition, wherein the gate dielectric layer is located between the gate electrode layer and the oxide semiconductor channel layer; Step 2.8, preparing an oxide semiconductor channel layer by magnetron sputtering, chemical vapor deposition, molecular beam epitaxy or atomic layer deposition; Step 2.9, growing a filling layer in the trench using a plasma enhanced chemical vapor deposition or atomic layer deposition process; Step 2.10, the oxide semiconductor contact layer and the metal drain electrode layer are prepared by using coating, baking, photolithography, development, electron beam evaporation, magnetron sputtering, and stripping processes.
Citation Information
Cited By
Indium oxide interface layer field effect transistor with improved contact resistance and preparation method thereof