Non-ferrous metal composite plate strip rolling process
By using impurity removal, cleaning and pre-pressing components in the non-ferrous metal composite plate rolling process, the metal oxide layer and stress are solved, and the metal oxide layer affects the rolling effect and high energy consumption are achieved, and more efficient rolling is achieved Process and stronger metal bond strength.
Patent Information
- Application Number
- CN202411392519.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-08
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-10-08
AI Technical Summary
In the existing non-ferrous metal composite plate rolling process, the existence of metal oxide layer affects the rolling effect and high energy consumption, and the cracking problem caused by internal stress of metal is difficult to solve.
The oxide layer on the metal surface is removed by using the decompression assembly, the oxide layer and stress are removed by the shot peening assembly and inert gas. The cleaning assembly is cleaned through the jet assembly and brush rollers, and the pre-pressure assembly is initially fixed in the inert gas environment to reduce the The oxide layer is generated to improve the rolling quality.
It improves the rolling effect, reduces the annealing time and energy consumption, reduces the requirements for the rolling mill, enhances the metal bonding strength, and avoids interlayer cracking.
Smart Images

Figure CN119016496A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of non-ferrous metal composite strip preparation, and in particular to a non-ferrous metal composite strip rolling process. Background Art
[0002] Metal composite plates combine the advantages of each component metal and have physical and chemical properties that a single metal does not have. They are widely used in aerospace, national defense, transportation, equipment manufacturing and other fields. The promotion and application of metal composite plates is of great significance to solving the outstanding problems of the current energy structure and industrial structure.
[0003] At present, the main methods for preparing metal composite plates include rolling, extrusion, explosion and diffusion welding. The rolling method is one of the most widely used preparation methods. The metal plate to be composited is subjected to the strong rolling pressure of the rolling mill to break the coating on the contact surface of the dissimilar metals, and plastic flow is generated in the entire contact surface. The fresh base metal squeezed out from the surface cracks comes into close contact and produces microscopic atomic reactions, and finally the contact interface between the metal layers forms a metallurgical bond of a certain strength. Compared with other methods, the rolling method has the advantages of low pollution, stable operation and good continuity of mass production.
[0004] At present, before non-ferrous metals are rolled, the metal bonding surface needs to be polished to remove the metal oxides, because the metal oxide layer will affect the metal bonding strength after rolling and cause interlayer cracking. In the prior art, a sanding machine or a metal brush roller is usually used to polish the metal surface. Since most non-ferrous metals have strong reducibility and are easily oxidized by air, an oxide layer is easily generated on the surface again after polishing and before rolling. In addition, the raw materials of metal plates and strips are generally coiled materials for easy transportation. After uncoiling, the internal stress of the metal is easy to cause cracking during rolling, which places high requirements on the rolling mill, and annealing treatment is required as soon as possible after rolling to eliminate stress. Annealing consumes a lot of energy. Summary of the invention
[0005] In order to make up for the above deficiencies, the present invention provides a non-ferrous metal composite plate and strip rolling process.
[0006] The technical solution of the present invention is:
[0007] A non-ferrous metal composite strip rolling process, comprising:
[0008] S1: Select a first metal strip and a second metal strip, wherein the second metal strip has less deformation resistance than the first metal strip, and send the first metal strip and the second metal strip into an impurity removal assembly to remove oxide layers on the surfaces of the first metal strip and the second metal strip;
[0009] S2: sending the first metal strip and the second metal strip after impurities removal into a cleaning assembly to remove oxide layer debris attached to the surfaces of the first metal strip and the second metal strip in an inert gas environment;
[0010] S3: sending the cleaned first metal strip and the second metal strip into a pre-pressing assembly, stacking them in an inert gas environment according to the principle of soft in the middle and hard on both sides, and performing preliminary fixation to obtain a composite slab;
[0011] S4: The composite slab is subjected to a first rolling process to obtain a corrugated composite slab. The first rolling process uses a rolling mill with double corrugated rollers. The upper and lower surfaces of the corrugated composite slab are corrugated surfaces. The bonding surface of the three layers of metal plates of the corrugated composite slab is also a corrugated surface. The first rolling process has a reduction ratio of 10% to 65%.
[0012] S5: The corrugated composite plate blank is rolled in the second pass to obtain a flat composite plate. The second pass is rolled using a rolling mill with double flat rollers. The upper and lower surfaces of the flat composite plate are flat surfaces. The bonding surface of the three metal plates of the flat composite plate is a corrugated surface. The reduction rate of the second pass is 30%-60%;
[0013] S6: The straight composite board is processed by trimming, heat treatment, straightening and segmentation to obtain the finished product.
[0014] Preferably, the impurity removal component includes an impurity removal box, which is provided with a plurality of feed ports and a plurality of first discharge ports, and a plurality of feed rollers are provided on the left and right sides of the impurity removal box, and the feed rollers are used to drive the first metal belt and the second metal belt to enter from the feed port and pass through the first discharge port.
[0015] Preferably, a first isolation brush is provided inside the feed port, and a second isolation brush is provided inside the first discharge port, and the first isolation brush and the second isolation brush are in contact with upper and lower sides of the first metal belt and the second metal belt.
[0016] Preferably, a plurality of shot peening assemblies are provided in the impurity removal box and between the first metal belt and the second metal belt, and the shot peening assemblies are used to remove oxide layers on opposite surfaces of the first metal belt and the second metal belt, and the shot peening assemblies use inert gas as working gas.
[0017] Preferably, the cleaning assembly includes a cleaning tube, which is fixedly installed on one side of the first discharge port of the impurity removal box, and a second discharge port is provided at the tail end of the cleaning tube, a third isolation brush is provided in the second discharge port, and the first metal belt and the second metal belt pass through the second discharge port.
[0018] Preferably, a first guide roller and a second guide roller are provided in the cleaning assembly, and the first metal belt is close to the second metal belt after passing around the first guide roller and the second guide roller.
[0019] Preferably, a jet assembly is provided between the first guide roller and the second guide roller and between the first metal belt and the second metal belt, and the jet assembly is used to blow air toward the opposite surfaces of the first metal belt and the second metal belt to remove attached impurities, and the jet assembly uses inert gas as the working gas.
[0020] Preferably, a first brush roller is provided on the right side of the second guide roller and between the first metal belt and the second metal belt, and the first brush roller is used to remove remaining impurities on the opposite surfaces of the first metal belt and the second metal belt.
[0021] Preferably, the pre-pressing assembly comprises a pre-pressing bin, which is fixedly mounted at the tail end of the cleaning tube, and a third discharge port is provided at the tail end of the pre-pressing bin, in which a fourth isolation brush is provided.
[0022] Preferably, a first pre-pressing roller and a second pre-pressing roller are provided on the left and right sides of the pre-pressing bin near the fourth isolation brush, and the first pre-pressing roller and the second pre-pressing roller are used to press and combine the first metal strip and the second metal strip into a composite slab.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] 1. The present invention, by providing an impurity removal component, uses a shot peening component to remove the oxide layer on the surface of the first metal strip and the second metal strip by means of surface shot peening, and can also use shot peening to eliminate the residual stress of the first metal strip and the second metal strip, thereby improving the rolling effect, reducing the subsequent annealing time, and reducing energy consumption. In addition, using an inert gas as a working gas can reduce the secondary oxidation of oxygen on the surface of the raw material;
[0025] 2. By setting a cleaning component, using the air blowing of the jet component and the first brush roller to work, the residual oxide powder on the surface of the metal strip can be cleaned before the metal strip is pre-pressed to improve the surface cleanliness. At the same time, using inert gas as the working gas can prevent the metal strip from being oxidized before entering the pre-pressing process, thereby improving the rolling quality;
[0026] 3. By setting up a pre-pressing component and connecting the pre-pressing pipe and the cleaning pipe, inert gas can enter the pre-pressing pipe from the cleaning pipe to ensure that the metal strip is in an inert gas environment before bonding, reducing the formation of an oxide layer, and fixing the metal strip with the first pre-pressing roller and the second pre-pressing roller. Before the metal strip is rolled, the oxidation of the bonding surface by air is reduced, the rolling effect is improved, and the requirements for the rolling mill are reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 It is a schematic diagram of the overall structure of the present invention;
[0028] Figure 2 It is a schematic diagram of the structure of the impurity removal component in the present invention;
[0029] Figure 3 It is a schematic diagram of the structure of the cleaning component in the present invention;
[0030] Figure 4 It is a schematic diagram of the structure of the pre-pressing component in the present invention;
[0031] Figure 5 It is a schematic diagram of the first rolling process in the present invention;
[0032] Figure 6 It is a schematic diagram of the second rolling process in the present invention;
[0033] Figure 7 This is a schematic diagram of the structure of the corrugated composite slab in the present invention;
[0034] Figure 8 It is a schematic diagram of the structure of the straight composite plate strip in the present invention.
[0035] The meanings of the punctuation marks in the figure are:
[0036] 1. First metal belt; 2. Second metal belt;
[0037] 3. De-dusting assembly; 31. De-dusting box; 32. Feed port; 33. First discharge port; 34. First isolation brush; 35. Second isolation brush; 36. Feed roller; 37. Spray pipe; 38. Nozzle; 39. Pad;
[0038] 4. Cleaning assembly; 41. Cleaning pipe; 42. Second discharge port; 43. Third isolation brush; 44. First guide roller; 45. Second guide roller; 46. Air duct; 47. Air nozzle; 48. Third feeding roller; 49. First brush roller;
[0039] 5. Pre-pressing assembly; 51. Pre-pressing bin; 52. Third discharge port; 53. Fourth isolation brush; 54. Third guide roller; 55. First pre-pressing roller; 56. Correction roller; 57. Second pre-pressing roller;
[0040] 6. Composite slab; 7. Corrugated composite slab; 8. Straight composite plate; 9. Corrugated roller; 10. Straight roller. DETAILED DESCRIPTION
[0041] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0042] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0043] The present invention describes the above technical solution in detail through the following embodiments:
[0044] Embodiment 1:
[0045] See attached Figure 1-8 , a non-ferrous metal composite strip rolling process, comprising:
[0046] S1: Oxide layer treatment: select a first metal strip 1 and a second metal strip 2, wherein the deformation resistance of the second metal strip 2 is smaller than that of the first metal strip 1, and send the first metal strip 1 and the second metal strip 2 to an impurity removal component 3 to remove the oxide layers on the surfaces of the first metal strip 1 and the second metal strip 2;
[0047] The first metal strip 1 and the second metal strip 2 are rolled non-ferrous metal strips.
[0048] The impurity removal component 3 includes an impurity removal box 31, which is provided with a plurality of feed ports 32 and a plurality of first discharge ports 33. A plurality of feed rollers 36 are provided on the left and right sides of the impurity removal box 31. The feed rollers 36 are used to drive the first metal strip 1 and the second metal strip 2 to enter from the feed port 32 and pass through the first discharge port 33.
[0049] The impurity removal box 31 is a metal box, and the feed roller 36 is rotatably connected to the impurity removal box 31 through a bearing. The feed roller 36 is a rubber roller, which clamps the first metal strip 1 and the second metal strip 2 from the upper and lower sides, and is driven by a motor to drive the first metal strip 1 and the second metal strip 2 to move. It should be noted that the feed roller 36 should have the ability to adjust up and down to meet the needs of the first metal strip 1 and the second metal strip 2 of different thicknesses.
[0050] A first isolation brush 34 is provided inside the feed port 32 , and a second isolation brush 35 is fixedly installed inside the first discharge port 33 . The first isolation brush 34 and the second isolation brush 35 are in contact with upper and lower sides of the first metal strip 1 and the second metal strip 2 .
[0051] The first isolation brush 34 and the second isolation brush 35 can be common plastic brushes, which are fixed in the feed port 32 and the first discharge port 33 by screws, and can reduce the material exchange inside and outside the impurity removal box 31. At the same time, the surfaces of the first metal belt 1 and the second metal belt 2 are preliminarily cleaned.
[0052] A plurality of shot peening assemblies are provided in the impurity removal box 31 and between the first metal belt 1 and the second metal belt 2. The shot peening assemblies are used to spray and remove the oxide layer on the opposite surfaces of the first metal belt 1 and the second metal belt 2. The shot peening assemblies use inert gas as the working gas.
[0053] The shot blasting assembly comprises a nozzle 37, at the end of which a nozzle 38 is threadedly mounted. The nozzle 38 is directed toward the first metal strip 1 and the second metal strip 2.
[0054] The bottom of the impurity removal box 31 can be filled with pellets for shot blasting, and the type of pellets is selected according to the type of the first metal strip 1 and the second metal strip 2. Driven by the inert gas, the pellets impact the surface of the first metal strip 1 and the second metal strip 2, remove the curing layer and eliminate the stress of the first metal strip 1 and the second metal strip 2.
[0055] A backing plate 39 is welded inside the impurity removal box 31 . The backing plate 39 is located on the side of the first metal strip 1 away from the shot peening assembly to prevent the first metal strip 1 from bending due to shot peening.
[0056] S2: Surface cleaning: The first metal strip 1 and the second metal strip 2 after impurities removal are sent to the cleaning assembly 4 to remove oxide layer debris attached to the surface of the first metal strip 1 and the second metal strip 2 in an inert gas environment;
[0057] The cleaning assembly 4 includes a cleaning pipe 41, which is fixedly installed on one side of the first discharge port 33 of the impurity removal box 31 by bolts. A second discharge port 42 is provided at the rear end of the cleaning pipe 41, and a third isolation brush 43 is fixedly installed in the second discharge port 42. The first metal strip 1 and the second metal strip 2 pass through the second discharge port 42.
[0058] After being cleaned of impurities, the first metal strip 1 and the second metal strip 2 directly enter the cleaning pipe 41 .
[0059] A first guide roller 44 and a second guide roller 45 are rotatably mounted in the cleaning assembly 4 via bearings. After the first metal belt 1 passes around the first guide roller 44 and the second guide roller 45 , it approaches the second metal belt 2 .
[0060] The second metal belt 2 is rotatably mounted with third feeding rollers 48 on both sides. The third feeding rollers 48 are steel rollers driven by a motor to drive the second metal belt 2 to move toward the second discharge port 42 and prevent the second metal belt 2 from falling due to its own weight.
[0061] The distance between the two third feeding rollers 48 is adjustable.
[0062] A jet assembly is provided between the first guide roller 44 and the second guide roller 45 and between the first metal belt 1 and the second metal belt 2. The jet assembly is used to blow air toward the opposite surfaces of the first metal belt 1 and the second metal belt 2 to remove attached impurities. The jet assembly uses inert gas as the working gas.
[0063] The jet assembly includes an air duct 46, which is bent toward the surface opposite to the first metal strip 1 and the second metal strip 2. A nozzle 47 is threadedly installed at the end of the air duct 46. The nozzle 47 adopts a duckbill nozzle. After the inert gas is introduced into the air duct 46, the oxide impurities attached to the surface of the first metal strip 1 and the second metal strip 2 can be blown away through the nozzle 47. It is ensured that the cleaning tube 41 is filled with inert gas.
[0064] A first brush roller 49 is rotatably mounted on the right side of the second guide roller 45 and between the first metal belt 1 and the second metal belt 2 . The first brush roller 49 is used to remove remaining impurities on the opposite surfaces of the first metal belt 1 and the second metal belt 2 .
[0065] The first brush roller 49 adopts a nylon brush and is driven by a motor. The first brush roller 49 rotates to clean the impurities that have not been blown off the surfaces of the first metal belt 1 and the second metal belt 2 to ensure that the contact surface is clean.
[0066] S3: Pre-pressing and fixing: The cleaned first metal strip 1 and the second metal strip 2 are sent to the pre-pressing assembly 5, and are stacked in an inert gas environment according to the principle of soft in the middle and hard on both sides, and are preliminarily fixed to obtain a composite slab 6;
[0067] The pre-pressing assembly 5 includes a pre-pressing bin 51 , which is fixedly mounted at the tail end of the cleaning tube 41 by bolts. A third discharge port 52 is provided at the tail end of the pre-pressing bin 51 , and a fourth isolation brush 53 is fixedly mounted in the third discharge port 52 .
[0068] The inert gas in the cleaning tube 41 can enter the pre-pressing bin 51 through the second discharge port 42 , and the third isolation brush 43 can reduce the amount of impurities in the cleaning tube 41 that enter the pre-pressing bin 51 .
[0069] Two third guide rollers 54 are rotatably installed in the pre-pressing bin 51 near the cleaning pipe 41 , and the first metal strip 1 bypasses the third guide rollers 54 and approaches the second metal strip 2 .
[0070] The first pre-pressing roller 55 and the second pre-pressing roller 57 are rotatably installed on the left and right sides near the fourth isolation brush 53 in the pre-pressing bin 51. The first pre-pressing roller 55 and the second pre-pressing roller 57 are used to press and combine the first metal strip 1 and the second metal strip 2 into a composite slab 6.
[0071] There are two first pre-pressing rollers 55 and two second pre-pressing rollers 57 , and the first pre-pressing rollers 55 and the second pre-pressing rollers 57 press the first metal strip 1 and the second metal strip 2 into a composite slab 6 from the upper and lower sides.
[0072] It should be noted that the spacing between the two first pre-pressing rollers 55 and the spacing between the two second pre-pressing rollers 57 are adjustable to accommodate the first metal strip 1 and the second metal strip 2 of different thicknesses.
[0073] A deviation-correcting roller 56 is rotatably installed between the third guide roller 54 and the first pre-pressing roller 55 and located on the front and rear sides of the first metal belt 1 and the second metal belt 2. The deviation-correcting roller 56 clamps the first metal belt 1 and the second metal belt 2 from the front and rear sides to avoid position deviation of the first metal belt 1 and the second metal belt 2 and ensure that both sides of the composite slab 6 are aligned.
[0074] The distance between the two deviation correcting rollers 56 is adjustable.
[0075] S4: Rough rolling: The composite slab 6 is subjected to the first rolling process to obtain a corrugated composite slab 7. The first rolling process uses a rolling mill with double corrugated rollers 9. The upper and lower surfaces of the corrugated composite slab 7 are corrugated surfaces. The bonding surface of the three layers of metal plates of the corrugated composite slab 7 is also a corrugated surface. The first rolling process has a reduction ratio of 60%.
[0076] S5: Finish rolling: The corrugated composite plate blank 7 is rolled in the second pass to obtain a flat composite plate 8. The second pass rolling adopts a rolling mill with double flat rollers 10. The upper and lower surfaces of the flat composite plate 8 are flat surfaces. The bonding surface of the three layers of metal plates of the flat composite plate 8 is a corrugated surface. The reduction rate of the second pass rolling is 40%;
[0077] S6: The straight composite plate 8 is subjected to edge trimming, heat treatment, straightening and segmentation treatment to obtain a finished product.
[0078] The above shows and describes the basic principles, main features and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited by the above embodiments. The above embodiments and descriptions are only preferred examples of the present invention and are not intended to limit the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A non-ferrous metal composite strip rolling process, characterized in that: include: S1: selecting a first metal strip (1) and a second metal strip (2), wherein the second metal strip (2) has a lower deformation resistance than the first metal strip (1), and feeding the first metal strip (1) and the second metal strip (2) into an impurity removal component (3) to remove oxide layers on the surfaces of the first metal strip (1) and the second metal strip (2); S2: sending the first metal strip (1) and the second metal strip (2) after impurities are removed into a cleaning assembly (4), and removing oxide layer debris attached to the surfaces of the first metal strip (1) and the second metal strip (2) in an inert gas environment; S3: sending the cleaned first metal strip (1) and the second metal strip (2) into a pre-pressing assembly (5), stacking them in an inert gas environment according to the principle of soft in the middle and hard on both sides, and performing preliminary fixing to obtain a composite slab (6); S4: The composite slab (6) is subjected to a first rolling process to obtain a corrugated composite slab (7), wherein the first rolling process uses a rolling mill with double corrugated rollers (9), the upper and lower surfaces of the corrugated composite slab (7) are corrugated surfaces, and the bonding surface of the three layers of metal plates of the corrugated composite slab (7) is also a corrugated surface, and the first rolling process reduction rate is 10%-65%; S5: The corrugated composite plate blank (7) is subjected to a second rolling process to obtain a flat composite plate (8), wherein the second rolling process uses a rolling mill with double flat rollers (10), the upper and lower surfaces of the flat composite plate (8) are flat surfaces, the bonding surface of the three metal plates of the flat composite plate (8) is a corrugated surface, and the reduction rate of the second rolling process is 30%-60%; S6: The straight composite board (8) is subjected to edge trimming, heat treatment, straightening and segmentation treatment to obtain a finished product.
2. A non-ferrous metal composite strip rolling process according to claim 1, characterized in that: The impurity removal component (3) comprises an impurity removal box (31), the impurity removal box (31) is provided with a plurality of feed ports (32) and a plurality of first discharge ports (33), a plurality of feed rollers (36) are provided on the left and right sides of the impurity removal box (31), and the feed rollers (36) are used to drive the first metal strip (1) and the second metal strip (2) to enter from the feed port (32) and pass through the first discharge port (33).
3. A non-ferrous metal composite strip rolling process as claimed in claim 2, characterized in that: A first isolation brush (34) is provided inside the feed port (32), and a second isolation brush (35) is provided inside the first discharge port (33). The first isolation brush (34) and the second isolation brush (35) are in contact with upper and lower sides of the first metal strip (1) and the second metal strip (2).
4. A non-ferrous metal composite strip rolling process as claimed in claim 2, characterized in that: A plurality of shot blasting assemblies are arranged in the impurity removal box (31) and between the first metal strip (1) and the second metal strip (2). The shot blasting assemblies are used to spray and remove oxide layers on the opposite surfaces of the first metal strip (1) and the second metal strip (2). The shot blasting assemblies use inert gas as working gas.
5. A non-ferrous metal composite strip rolling process as claimed in claim 2, characterized in that: The cleaning assembly (4) comprises a cleaning pipe (41), the cleaning pipe (41) being fixedly mounted on one side of a first discharge port (33) of a de-duster box (31), a second discharge port (42) being arranged at a rear end of the cleaning pipe (41), a third isolation brush (43) being arranged in the second discharge port (42), and the first metal belt (1) and the second metal belt (2) passing through the second discharge port (42).
6. A non-ferrous metal composite strip rolling process as claimed in claim 5, characterized in that: The cleaning assembly (4) is provided with a first guide roller (44) and a second guide roller (45), and the first metal belt (1) is brought close to the second metal belt (2) after passing the first guide roller (44) and the second guide roller (45).
7. A non-ferrous metal composite strip rolling process as claimed in claim 6, characterized in that: An air jet assembly is provided between the first guide roller (44) and the second guide roller (45) and between the first metal belt (1) and the second metal belt (2). The air jet assembly is used to blow air toward the opposite surfaces of the first metal belt (1) and the second metal belt (2) to remove attached impurities. The air jet assembly uses an inert gas as a working gas.
8. A non-ferrous metal composite strip rolling process as claimed in claim 7, characterized in that: A first brush roller (49) is provided on the right side of the second guide roller (45) and between the first metal belt (1) and the second metal belt (2), wherein the first brush roller (49) is used to remove remaining impurities on the opposite surfaces of the first metal belt (1) and the second metal belt (2).
9. A non-ferrous metal composite strip rolling process as claimed in claim 5, characterized in that: The pre-pressing assembly (5) comprises a pre-pressing bin (51), the pre-pressing bin (51) being fixedly mounted at the rear end of the cleaning tube (41), a third discharge port (52) being provided at the rear end of the pre-pressing bin (51), and a fourth isolation brush (53) being provided in the third discharge port (52).
10. A non-ferrous metal composite strip rolling process according to claim 9, characterized in that: A first pre-pressing roller (55) and a second pre-pressing roller (57) are provided on the left and right sides of the pre-pressing bin (51) near the fourth isolation brush (53). The first pre-pressing roller (55) and the second pre-pressing roller (57) are used to press and combine the first metal strip (1) and the second metal strip (2) into a composite slab (6).
Citation Information
Patent Citations
Multifunctional rolling processing device
CN103846279A
Method and device for preparing metal composite board
CN104826865A
Method and device for rolling metal composite plate strips
CN105032928A
Device and method for producing metal composite sheet strips through corrugated-flat continuous rolling
CN105057386A
Method for preparing composite metal plate through rolling
CN106799397A
Cited By
Carbon steel and stainless steel composite coiled plate production device
CN119870178A
A carbon steel and stainless steel composite coil production device