Polishing pad and design method thereof

By dividing the wafer into multiple hardness regions and designing the hardness regions of the polishing pad, the problem of difficulty in adjusting the material removal rate in each area of ​​the wafer in the prior art is solved, and thickness uniformity adjustment is achieved without changing the polishing process parameters. .

CN119017253APending Publication Date: 2024-11-26SHANGHAI INST OF IC MATERIALS
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202310595360.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-25
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

In ultra-large-scale integrated circuit manufacturing, existing polishing pads are difficult to accurately adjust the material removal rate of each area of ​​the wafer, resulting in the problem of uneven thickness.

Method used

By dividing the wafer into multiple regions along its radial direction, different hardness regions are divided according to the change curve of material removal rate, and the hardness regions of the polishing pad are designed to ensure that the material removal is adjusted everywhere without changing the polishing process parameters. to obtain a wafer of uniform thickness.

Benefits of technology

It realizes accurate adjustment of material removal rate across the wafer surface without changing the polishing process parameters, expands the process adjustment range, and ensures uniformity of wafer thickness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119017253A_ABST
    Figure CN119017253A_ABST
Patent Text Reader

Abstract

The invention provides a polishing pad and a design method thereof.The design method includes the steps that a wafer is divided into a plurality of areas in the radial direction, under certain chemical mechanical polishing process parameters, movement areas of all the areas of the wafer on the polishing pad are found, and the polishing pad is divided into different hardness areas according to the movement areas; and finally, the hardness of the polishing pad is designed according to the relation between the hardness and the material removal rate. According to the method and the device, partition hardness design is carried out on the polishing pad, the material removal rate of each part of the surface of the wafer can be adjusted under the condition that polishing process parameters are not changed, so that the wafer with the uniform thickness is obtained, the problem that the material removal rate of each area of the wafer cannot be accurately adjusted in the prior art is solved, and the process adjustment interval is expanded.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of chemical mechanical polishing, and specifically relates to a polishing pad and a design method thereof. Background Art

[0002] In the manufacture of very large-scale integrated circuits, chemical mechanical polishing (CMP) has become the most widely used planarization technology. At present, the polishing pads used in integrated circuit manufacturing are mainly polymer polishing pads, the main components of which are polyurethane cured from foam and non-woven fabrics. The surface has a certain density of micro-convex peaks and the overall hardness is uniform. Before the wafer is chemically mechanically polished, various techniques such as thinning and chemical etching are used to gradually remove the damaged layer on the surface of the wafer. In this process, the processing errors of each step will continue to accumulate, resulting in uneven thickness of the wafer. Therefore, when the wafer is chemically mechanically polished, the material removal rate (MRR) of each part of the wafer surface needs to be adjusted to obtain a wafer with uniform thickness. Summary of the invention

[0003] In view of the shortcomings of the prior art described above, the present invention provides a polishing pad and a design method thereof, wherein the wafer is first divided into multiple regions along its radial direction, and under certain chemical mechanical polishing process parameters, the movement regions of each region of the wafer on the polishing pad are found, and the polishing pad is divided into different hardness zones according to the movement zones, and finally the hardness of the polishing pad is designed according to the relationship between hardness and material removal rate. The present invention can adjust the material removal rate at various locations on the surface of the wafer without changing the polishing process parameters by designing the hardness of the polishing pad by partitioning, so as to obtain a wafer with uniform thickness, thereby solving the problem in the prior art that the material removal rate of each region of the wafer cannot be accurately adjusted, and expanding the process adjustment range.

[0004] To achieve the above object and other related objects, the present invention provides a method for designing a polishing pad, comprising the following steps:

[0005] S1: providing a wafer to be polished, and obtaining a variation curve of the material removal rate of each point on the surface of the wafer in the radial direction of the wafer according to the thickness distribution of the wafer in the radial direction;

[0006] S2: Divide the wafer into N regions along its radial direction, obtain the boundary of each adjacent region from the change curve, and the distance between the boundary and the center of the wafer is R i , i=1, 2, ... N-1;

[0007] S3: Select a point k on each of the boundaries i, i = 1, 2...N-1, select a point k on the edge of the wafer N , respectively draw the point k when the wafer is polished on the polishing pad i Movement area Z on the polishing pad i , and point k N Movement area Z on the polishing pad N ;

[0008] S4: Divide the polishing pad into N regions with different hardness, wherein the motion region Z1 is the first hardness region, the motion region Z2 is subtracted from Z1 to obtain the second hardness region, and so on. N With Z N-1 Subtract to get the Nth hardness zone;

[0009] S5: Perform hardness design on the first hardness zone, the second hardness zone, ... the Nth hardness zone respectively to obtain the polishing pad with hardness zone design.

[0010] Optionally, in step S1, the material removal rate at the center of the wafer is V0, and the material removal rate at other points on the surface of the wafer is V, V=c×V0, where c is a constant greater than 1.

[0011] Optionally, in step S2, the maximum value V of the material removal rate in the variation curve is found. m , the material removal rate i(V m = -V0) / N+V0 The radial distance of the wafer corresponding to is the distance R between the i-th boundary and the center of the wafer i , i=1, 2...N-1.

[0012] Optionally, in step S4, the first hardness zone, the second hardness zone, ... the Nth hardness zone are concentrically distributed circular ring areas.

[0013] Optionally, in step S4, the first hardness zone includes a circular ring-shaped area, the second hardness zone includes two circular ring-shaped areas separated by the first hardness zone...the Nth hardness zone includes two circular ring-shaped areas separated by the N-1th hardness zone.

[0014] Optionally, the surface hardness of the polishing pad gradually increases from the first hardness zone to the Nth hardness zone.

[0015] The present invention also provides a polishing pad, which includes a first hardness zone, a second hardness zone...an Nth hardness zone that are concentrically distributed, and the surface hardness of the polishing pad gradually increases from the first hardness zone to the Nth hardness zone. The polishing pad is made by the polishing pad design method described in any one of the above items.

[0016] Optionally, the first hardness zone includes a circular ring-shaped area, the second hardness zone includes two circular ring-shaped areas separated by the first hardness zone... The Nth hardness zone includes two circular ring-shaped areas separated by the N-1th hardness zone.

[0017] The polishing pad and the design method thereof provided by the present invention have at least the following beneficial effects:

[0018] The present invention designs the hardness of the polishing pad in different zones, and can adjust the material removal rate at various locations on the wafer surface without changing the polishing process parameters to obtain a wafer with uniform thickness. This solves the problem in the prior art that the material removal rate of each area of ​​the wafer cannot be accurately adjusted, and expands the process adjustment range. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a curve diagram showing wafer thickness distribution in step S1 of the first embodiment.

[0020] Figure 2 It is a curve diagram showing the variation of the material removal rate in the radial direction of the wafer in step S1 of the first embodiment.

[0021] Figure 3a to 3c It is a schematic diagram of the motion areas Z1 to Z3 in step S3 of the first embodiment.

[0022] Figure 4 It is a schematic diagram of the polishing pad in step S4 of the first embodiment.

[0023] Component number description

[0024] 100 Polishing Pad

[0025] 101 First hardness zone

[0026] 102 Second hardness zone

[0027] 103 Third hardness zone

[0028] Z1: Movement area of ​​point k1 on the polishing pad

[0029] Z2: Movement area of ​​point k2 on the polishing pad

[0030] Z3: Movement area of ​​point k3 on the polishing pad DETAILED DESCRIPTION

[0031] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0032] It should be noted that the illustrations provided in this embodiment only illustrate the basic concept of the present invention in a schematic manner. Although the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation, the form, quantity, positional relationship and proportion of each component in actual implementation can be changed at will under the premise of realizing the technical solution of this party, and the component layout form may also be more complicated.

[0033] Embodiment 1

[0034] This embodiment provides a polishing pad design method, comprising the following steps:

[0035] S1: providing a wafer to be polished, and obtaining a variation curve of the material removal rate of each point on the surface of the wafer in the radial direction of the wafer according to the thickness distribution of the wafer in the radial direction;

[0036] As an example, a wafer to be polished is provided. In this embodiment, the radius of the wafer is 150 mm. Before the wafer is polished, various technologies such as thinning and chemical etching are used to gradually remove the damaged layer on the surface of the wafer. During this process, the processing errors of each step will continue to accumulate, resulting in uneven thickness of the wafer. Figure 1 As shown, from the center of the wafer to its edge, that is, as the distance r between the point on the wafer surface and the center of the wafer O increases, the thickness d of the wafer gradually increases. Therefore, in order to make the thickness of the polished wafer uniform everywhere, the material removal rate needs to be gradually increased from the center of the wafer to its edge during the polishing process.

[0037] As an example, according to Figure 1 The thickness distribution in the radial direction of the wafer is shown, and the curve of the material removal rate at each point on the wafer surface in the radial direction of the wafer is obtained. Figure 2 As shown, the material removal rate at the center of the wafer is V0, and the material removal rate at other points on the wafer surface is V, V=c×V0, where c is a constant greater than 1.

[0038] S2: Divide the wafer into N regions along its radial direction, obtain the boundary of each adjacent region from the change curve, and the distance between the boundary and the center of the wafer is R i , i=1, 2, ... N-1;

[0039] First, the wafer is divided into N regions along its radial direction. The specific value of N can be determined manually according to actual needs. In this embodiment, the wafer is divided into three regions along its radial direction.

[0040] Then, by Figure 2 The variation curve shown obtains the boundaries of each adjacent area. As an example, find the maximum value V of the material removal rate in the variation curve m , the material removal rate in the change curve i(V m -V0) / N+V0 corresponds to the radial distance of the wafer, which is the distance R between the i-th boundary and the center O of the wafer. i , i = 1, 2...N-1. Figure 2 As shown, in this embodiment, the maximum value of the material removal rate V m The radial distance of the wafer corresponding to the material removal rate of 1.43V0 is the distance R1 between the first boundary and the wafer center O, which is about 104mm; the radial distance of the wafer corresponding to the material removal rate of 1.87V0 is the distance R2 between the second boundary and the wafer center O, which is about 133.6mm. It should be noted that the above-mentioned material removal rate V and the distance R between the boundary and the wafer center O are i The specific values ​​are only examples and are not very accurate. The exact values ​​can be read during the detailed calculation process.

[0041] S3: Select a point k on each of the boundaries i , i = 1, 2...N-1, select a point k on the edge of the wafer N , respectively draw the point k when the wafer is polished on the polishing pad i Movement area Z on the polishing pad i , and point k N Movement area Z on the polishing pad N ;

[0042] As an example, when a wafer is polished on a polishing pad, the wafer rotates around its own center while also rotating around the center of the polishing pad. Figure 3a As shown, a point k1 is selected on the first boundary, and the distance R1 between k1 and the center O of the wafer is about 104 mm. When the wafer is polished on the polishing pad 100, the movement area of ​​the point k1 on the polishing pad 100 is shown as Z1; Figure 3b As shown, a point k2 is selected on the second boundary, and the distance R2 between k2 and the center O of the wafer is about 133.6 mm. When the wafer is polished on the polishing pad 100, the movement area of ​​the point k2 on the polishing pad 100 is shown as Z2.

[0043] like Figure 3cAs shown, a point k3 is selected on the edge of the wafer, and the distance between k3 and the center O of the wafer is 150 mm. When the wafer is polished on the polishing pad 100, the movement area of ​​the point k3 on the polishing pad 100 is shown as Z3.

[0044] S4: Divide the polishing pad into N regions with different hardness, wherein the motion region Z1 is the first hardness region, the motion region Z2 is subtracted from Z1 to obtain the second hardness region, and so on. N With Z N-1 Subtract to get the Nth hardness zone;

[0045] As an example, the polishing pad 100 is divided into N regions with different hardnesses, such as Figure 4 As shown, in this embodiment, the polishing pad 100 is divided into three areas with different hardness, wherein the motion area Z1 is the first hardness area 101, the motion area Z2 is subtracted from Z1 to obtain the second hardness area 102, and the motion area Z3 is subtracted from Z2 to obtain the third hardness area 103. The first hardness area 101, the second hardness area 102 and the third hardness area 103 are concentrically distributed annular areas, wherein the first hardness area 101 includes one annular area, the second hardness area 102 includes two annular areas separated by the first hardness area 101, and the third hardness area 103 includes two annular areas separated by the second hardness area 102.

[0046] S5: Perform hardness design on the first hardness zone, the second hardness zone, ... the Nth hardness zone respectively to obtain the polishing pad with hardness zone design.

[0047] As an example, in order to make the thickness of the wafer uniform after polishing, it is necessary to design the hardness of the partitions of the polishing pad 100. Since the material removal rate needs to gradually increase from the center of the wafer to its edge during the polishing process, the surface hardness of the polishing pad 100 needs to gradually increase from the first hardness zone 101 to the third hardness zone 103 when designing the hardness, so that the thickness of the wafer after polishing is uniform. For example, in this embodiment, the hardness of the first hardness zone 101 is H, the hardness of the second hardness zone 102 is 1.3H, and the hardness of the third hardness zone 103 is 1.5H. It should be noted that the hardness relationship between the N hardness zones and the specific hardness value of each zone are determined according to actual needs.

[0048] Embodiment 2

[0049] The present embodiment provides a polishing pad, which is made by the design method of the polishing pad provided in the first embodiment. The polishing pad includes a first hardness zone, a second hardness zone...an Nth hardness zone distributed concentrically, and the surface hardness of the polishing pad gradually increases from the first hardness zone to the Nth hardness zone.

[0050] In this embodiment, if Figure 4 As shown, the polishing pad 100 includes a first hardness zone 101, a second hardness zone 102, and a third hardness zone 103 that are concentrically distributed, wherein the first hardness zone 101 includes a circular ring region, the second hardness zone 102 includes two circular ring regions separated by the first hardness zone 101, and the third hardness zone 103 includes two circular ring regions separated by the second hardness zone 102. As an example, the surface hardness of the polishing pad 100 gradually increases from the first hardness zone 101 to the third hardness zone 103.

[0051] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A method for designing a polishing pad, It is characterized in that The steps include: S1: providing a wafer to be polished, and obtaining a variation curve of the material removal rate of each point on the surface of the wafer in the radial direction of the wafer according to the thickness distribution of the wafer in the radial direction; S2: Divide the wafer into N regions along its radial direction, obtain the boundary of each adjacent region from the change curve, and the distance between the boundary and the center of the wafer is R i , i=1, 2, ... N-1; S3: Select a point k on each of the boundaries i , i = 1, 2...N-1, select a point k on the edge of the wafer N , respectively draw the point k when the wafer is polished on the polishing pad i Movement area Z on the polishing pad i , and point k N Movement area Z on the polishing pad N ; S4: Divide the polishing pad into N regions with different hardness, wherein the motion region Z 1 The first hardness zone, the movement zone Z 2 With Z 1 Subtract to get the second hardness zone... and so on, the motion zone Z N With Z N-1 Subtract to get the Nth hardness zone; S5: Perform hardness design on the first hardness zone, the second hardness zone, ... the Nth hardness zone respectively to obtain the polishing pad with hardness zone design.

2. The method for designing a polishing pad according to claim 1, It is characterized in that In step S1, the material removal rate at the center of the wafer is V 0 , the material removal rate at other points on the wafer surface is V, V = c × V 0 , where c is a constant greater than 1.

3. The method for designing a polishing pad according to claim 2, It is characterized in that In step S2, the maximum value V of the material removal rate in the variation curve is found. m , the material removal rate i(V m -V 0 ) / N+V 0 The corresponding wafer radial distance is the distance R between the i-th boundary and the wafer center. i , i=1, 2...N-1.

4. The method for designing a polishing pad according to claim 1, It is characterized in that In step S4, the first hardness zone, the second hardness zone, ... the Nth hardness zone are concentrically distributed annular areas.

5. The method for designing a polishing pad according to claim 4, It is characterized in that In step S4, the first hardness zone includes a circular ring area, the second hardness zone includes two circular ring areas separated by the first hardness zone...the Nth hardness zone includes two circular ring areas separated by the N-1th hardness zone.

6. The method for designing a polishing pad according to claim 1, It is characterized in that The surface hardness of the polishing pad gradually increases from the first hardness zone to the Nth hardness zone.

7. A polishing pad, It is characterized in that The polishing pad comprises a first hardness zone, a second hardness zone, ... an Nth hardness zone which are concentrically distributed, and the surface hardness of the polishing pad gradually increases from the first hardness zone to the Nth hardness zone. The polishing pad is made by the polishing pad design method according to any one of claims 1 to 6.

8. The polishing pad according to claim 7, It is characterized in that The first hardness zone includes a circular ring-shaped area, the second hardness zone includes two circular ring-shaped areas separated by the first hardness zone... The Nth hardness zone includes two circular ring-shaped areas separated by the N-1th hardness zone.

Citation Information

Cited By

  • Polishing pad and chemical mechanical polishing equipment

    CN120244825A