Compound demulsifier based on magnetic nanoparticles and preparation method thereof

By using magnetic nanoparticles and hyperbranched polymers in the deemulsion agent to form a composite deemulsion agent, the problems of poor deemulsion effect and environmental pollution in the existing technology at high temperatures are solved, and rapid decomposition is achieved The effect of milk and multiple recycles.

CN119020064AInactive Publication Date: 2024-11-26YANGZHOU POLYTECHNIC INST
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411313196.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-20
Publication Date
2024-11-26
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing chemical demulsifiers have demulsive effect at high temperatures, which is difficult to degrade, and cause secondary pollution to the environment, have poor universality, and are harsh in applicable conditions, making it difficult to meet high performance requirements.

Method used

Magnetic nanoparticles were prepared by co-precipitation method, and hyperbranched polymers were prepared by SCVP-RAFT polymerization method. Combined with polymeric ferrous aluminum silicate, magnetic nanoparticles and silane coupling agent were introduced to form a complex deemulsifier, which was magnetic and capable. Degradability, can quickly demulsify and recover through an external magnetic field.

Benefits of technology

It realizes rapid demulsification at high temperatures, with small amount of demulsifier, easy to degrade, high universality, can quickly adsorb the surface of oil droplets, reduce environmental pollution, and recover through external magnetic fields. The number of cycles is greater than ten times, saving costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_2
    Figure SMS_2
  • Figure SMS_3
    Figure SMS_3
Patent Text Reader

Abstract

The invention relates to a compound demulsifier based on magnetic nanoparticles and a preparation method of the compound demulsifier. The preparation method comprises the following steps: firstly, carrying out SCVP-RAFT (Reversible Addition-Fragmentation Chain Transfer) polymerization on vinyl trithiocarbonate, AIBN (Azobisisobutyronitrile), p-chloromethyl styrene and MDO (Methane Diisocyanate); then carrying out chlorine substitution reaction with mPEG; the obtained product and KH570-Fe3O4 are subjected to a chain extension reaction under the initiation of AIBN; and after the reaction is finished, mixing with polysilicate aluminum ferric to obtain the product. The hyperbranched multi-branched-chain polydemulsifier with main chain polyester and branched chain polyether is firstly prepared, has the characteristics of large molecular weight, multiple aromatic rings and the like, is high in universality, can be used for quickly demulsifying different types of crude oil, is small in dosage and easy to degrade, and can also reduce pollution to the environment; and then magnetism is introduced through silane-modified magnetic nanoparticles, and poly-aluminum ferric silicate is compounded, so that the demulsification rate is increased, the emulsion can be recycled through an external magnetic field, the emulsion can be recycled, the cycle index is more than ten, and the use cost is saved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of demulsifiers, and in particular to a composite demulsifier based on magnetic nanoparticles and a preparation method thereof. Background Art

[0002] Petroleum is called "the blood of industry" and has extremely high application value in industrial development. With the continuous exploitation of crude oil in various countries, its storage volume is decreasing. At the same time, in the process of exploitation, with the promotion and application of alkali flooding, surfactant flooding, polymer flooding and other technologies, the water content of crude oil emulsion increases, the oilfield sewage is seriously emulsified, and the difficulty of demulsification increases. Chemical demulsifier is a commonly used demulsifier, including SP series, AP series, AE series and OP series. Chemical demulsifier can be molecularly designed according to the components of crude oil produced fluid from different oil fields, and a variety of special demulsifiers have been developed, but it also causes problems such as poor universality and harsh application conditions of traditional chemical demulsifiers. Among the many series of demulsifiers, polyether demulsifiers (OP series) are more widely used. They are mostly block-polymerized with ethylene oxide, propylene oxide and other components. They have the advantages of acid and alkali resistance and obvious crude oil dehydration effect, but the demulsification effect is significantly worse at high temperature, and it is difficult to degrade and easily causes secondary pollution to the environment. With the continuous development of crude oil, the performance requirements for demulsifiers are becoming higher and higher. Therefore, it is necessary to strengthen the research and development and innovation of new demulsifiers. Summary of the invention

[0003] In view of the deficiencies in the prior art, the present invention aims to prepare a composite hyperbranched demulsifier containing rich polyether, aromatic ring and polyester structures in combination with magnetic nanoparticles. The demulsifier has a special structure, rich functional groups, good demulsification properties, is easy to recover and can be recycled.

[0004] To achieve the above object, the present invention provides the following technical solutions: A method for preparing a composite demulsifier based on magnetic nanoparticles comprises the following steps: S1, preparing Fe3O4 magnetic nanoparticles by coprecipitation method, and then modifying their surface with KH570 to obtain KH570-Fe3O4 magnetic nanoparticles for standby use; S2. Add vinyl trithiocarbonate, AIBN, p-chloromethylstyrene and 2-methylene-1,3-dioxepane into a reaction flask, then add an organic solvent and stir to mix evenly, introduce an inert gas to bubble for 30 minutes, then heat to 70-80°C under the protection of inert gas and react for 6-8 hours; S3. After the reaction is completed, remove the inert gas, cool to room temperature, add organic solvent for dilution, add CTAB and methoxy polyethylene glycol, add a certain amount of sodium hydroxide solution, heat to 70-80 °C and react overnight, cool to room temperature, add anhydrous ether solution, filter and vacuum dry; S4. Add a certain amount of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide to the reaction bottle, disperse them evenly by ultrasound, then add a certain amount of the product of step S3 and AIBN, bubble inert gas for 30 min, then heat to 70-80°C under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

[0005] Further, the structural formula of the vinyl trithiocarbonate is .

[0006] Furthermore, the molar ratio of the vinyl trithiocarbonate, AIBN, p-chloromethylstyrene and 2-methylene-1,3-dioxepane is 1:0.2:30-60:40-70.

[0007] Furthermore, the organic solvent is a mixed solution of equal volumes of toluene and N,N-dimethylformamide.

[0008] Furthermore, the molecular weight of the methoxy polyethylene glycol is 400-1000, and the molar ratio of the methoxy polyethylene glycol to p-chloromethylstyrene is 1-1.5:1.

[0009] Furthermore, the mass fraction of the sodium hydroxide solution is 30%.

[0010] Furthermore, in the step S4, the mass ratio of KH570-Fe3O4 magnetic nanoparticles to the product of step S3 and AIBN is 10:1:0.001; the mass ratio of the polyaluminium ferrosilicate to the product of step S3 is 0.2-0.8:1.

[0011] The present invention further provides a composite demulsifier based on magnetic nanoparticles prepared by the preparation method as described above.

[0012] Among the topological structures of many polymer chemical demulsifiers, the order of demulsification ability should be star-shaped > branch-shaped > comb-shaped > linear. Therefore, in this case, a hyperbranched polymer was prepared by SCVP-RAFT polymerization, and MDO was used as a comonomer to polymerize with p-chloromethylstyrene free radicals. p-chloromethylstyrene has a similar conjugated aromatic ring chemical structure with asphaltene, and forms a strong π-π interaction with asphaltene. It is a functional structure often introduced in the preparation of demulsifiers. In this case, p-chloromethylstyrene was selected. In addition to introducing a benzene ring structure to improve the adsorption of asphaltene, the chloromethyl group at the para position of the benzene ring can also be used as an active site to react with methoxy polyethylene glycol to form a long polyether chain on its side chain. The monomer MDO opens the ring to form a main chain polyester structure during the polymerization process, making the hyperbranched macromolecular polymer degradable and reducing the harm to the environment. The rich ester groups and polyethers have good lipophilic and hydrophilic properties, which can reduce the strength of the interfacial film, and the hyperbranched polymer chains and long side chains can be quickly adsorbed on the surface of oil droplets to achieve the purpose of rapid demulsification and oil removal.

[0013] Although the demulsifier prepared by the above scheme has a good demulsification effect, it is difficult to recycle. Therefore, in the present application, magnetic nanoparticles are used to give the demulsifier magnetism. The magnetic nanoparticles have unsaturated double bonds after surface modification by a silane coupling agent. The hyperbranched polymer prepared in the above scheme has polymerization activity and can be used as a macromolecular RAFT agent to graft copolymerize the magnetic nanoparticles into the polymer chain, so that the magnetism of the polymer is more stable and easy to recycle; at the same time, the demulsifier is also compounded with polyaluminum ferrosilicate, which effectively improves the demulsification rate of the demulsifier and accelerates the demulsification time to 30 minutes.

[0014] Compared with the prior art, the beneficial effects of the present invention are as follows: firstly, based on the SCVP-RAFT method and combined with the chlorine substitution method, a hyperbranched multi-branched polyether demulsifier of main chain polyester and branched polyether is prepared, which has the characteristics of large molecular weight, high branching degree, long molecular chain, multiple aromatic rings, etc., has high universality, can quickly demulsify different types of crude oil, uses a small amount of demulsifier and is easy to degrade, and can also reduce pollution to the environment; subsequently, magnetism is introduced through silane-modified magnetic nanoparticles, and polyaluminum ferrosilicate is compounded to accelerate the demulsification rate, can be recovered through an external magnetic field, can be recycled, and the number of cycles is greater than ten times, thereby saving the use cost. DETAILED DESCRIPTION

[0015] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0016] In addition, the technical features involved in the different embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0017] Embodiment: A composite demulsifier based on magnetic nanoparticles is prepared by the following preparation method: S1, preparing Fe3O4 magnetic nanoparticles by coprecipitation method, and then modifying their surface with KH570 to obtain KH570-Fe3O4 magnetic nanoparticles for standby use; S2. Add vinyl trithiocarbonate, AIBN, p-chloromethylstyrene and 2-methylene-1,3-dioxepane into a reaction flask, then add an organic solvent and stir to mix evenly, introduce an inert gas to bubble for 30 minutes, then heat to 70-80°C under the protection of inert gas and react for 6-8 hours; S3. After the reaction is completed, remove the inert gas, cool to room temperature, add organic solvent for dilution, add CTAB and methoxy polyethylene glycol, add a certain amount of sodium hydroxide solution, heat to 70-80 °C and react overnight, cool to room temperature, add anhydrous ether solution, filter and vacuum dry; S4. Add a certain amount of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide to the reaction bottle, disperse them evenly by ultrasound, then add a certain amount of the product of step S3 and AIBN, bubble inert gas for 30 min, then heat to 70-80°C under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

[0018] The raw materials used in the above reaction process can be purchased from the market unless otherwise specified. Among them, the KH570-Fe3O4 magnetic nanoparticles can be prepared by conventional technical means in the art, for example, by the following steps: Add 5g FeCl3·6H2O and 2g FeSO4·7H2O, 1ml hydrazine hydrate and 30ml water into the reaction bottle, stir to dissolve, add 10ml ammonia water during stirring, and then slowly add ammonia water until the pH reaches 9. After the reaction is completed, separate the Fe3O4 magnetic particles, wash with water and then vacuum dry; dissolve the prepared magnetic particles in 150ml 50% ethanol, pass nitrogen, add an equal amount of KH570, adjust the pH to weak acidity, heat to 60℃ for reaction for 3h, separate magnetically and vacuum dry to obtain.

[0019] The organic solvent is a mixed solution of equal volumes of toluene and N,N-dimethylformamide (DMF).

[0020] The vinyl trithiocarbonate is prepared by referring to paragraph [0026-0029] in the applicant's patent 2020110194314.

[0021] Embodiment 1: S1. Add 1 mmol of vinyl trithiocarbonate, 0.2 mmol of AIBN, 30 mmol of p-chloromethylstyrene and 70 mmol of MDO into a reaction flask, then add 10 ml of an organic solvent and stir to mix evenly, introduce argon gas for 30 min, then heat to 80 °C under argon protection and react for 8 h; S2. After the reaction is completed, remove the argon gas, cool to room temperature, add 40 ml of organic solvent for dilution, add a catalytic amount of CTAB and 30 mmol mPEG400, add 40 g of 30 wt% sodium hydroxide solution, heat to 70 °C and react overnight, cool to room temperature, add to anhydrous ether solution, filter and vacuum dry; S3, add 10g of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide into the reaction bottle, disperse them evenly by ultrasound, then add 1g of the product of S3 and 1 mg of AIBN, bubble inert gas for 30 min, then heat to 70-80℃ under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add 0.5g of polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

[0022] Embodiment 2: S1. Add 1 mmol of vinyl trithiocarbonate, 0.2 mmol of AIBN, 50 mmol of p-chloromethylstyrene and 50 mmol of MDO into a reaction flask, then add 10 ml of an organic solvent and stir to mix evenly, introduce argon gas for 30 min, then heat to 80 °C under argon protection and react for 8 h; S2. After the reaction is completed, remove the argon gas, cool to room temperature, add 40 ml of organic solvent for dilution, add a catalytic amount of CTAB and 50 mmol mPEG400, add 40 g of 30 wt% sodium hydroxide solution, heat to 70 °C and react overnight, cool to room temperature, add to anhydrous ether solution, filter and vacuum dry; S3, add 10g of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide into the reaction bottle, disperse them evenly by ultrasound, then add 1g of the product of S3 and 1 mg of AIBN, bubble inert gas for 30 min, then heat to 70-80℃ under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add 0.5g of polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

[0023] Embodiment 3: S1. Add 1 mmol of vinyl trithiocarbonate, 0.2 mmol of AIBN, 50 mmol of p-chloromethylstyrene and 50 mmol of MDO into a reaction flask, then add 10 ml of an organic solvent and stir to mix evenly, introduce argon gas for 30 min, then heat to 80 °C under argon protection and react for 8 h; S2. After the reaction is completed, remove the argon gas, cool to room temperature, add 40 ml of organic solvent for dilution, add a catalytic amount of CTAB and 50 mmol mPEG600, add 40 g of 30 wt% sodium hydroxide solution, heat to 70 °C and react overnight, cool to room temperature, add to anhydrous ether solution, filter and vacuum dry; S3, add 10g of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide into the reaction bottle, disperse them evenly by ultrasound, then add 1g of the product of S3 and 1 mg of AIBN, bubble inert gas for 30 min, then heat to 70-80℃ under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add 0.5g of polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

[0024] Comparative Example: S1. Add 1 mmol of vinyl trithiocarbonate, 0.2 mmol of AIBN, 50 mmol of p-chloromethylstyrene and 50 mmol of MDO into a reaction flask, then add 10 ml of an organic solvent and stir to mix evenly, introduce argon gas for 30 min, then heat to 80 °C under argon protection and react for 8 h; S2. After the reaction is completed, remove the argon gas, cool to room temperature, add 40 ml of organic solvent for dilution, add catalytic amount of CTAB and 50 mmol mPEG600, add 40 g of 30 wt% sodium hydroxide solution, raise the temperature to 70 °C and react overnight, cool to room temperature and add to anhydrous ether solution, add Fe3O4 magnetic particles and polyaluminum ferrosilicate, stir well, filter and dry in vacuum; the product is obtained.

[0025] Demulsifier performance test: The demulsifier prepared as above was used to evaluate the demulsification performance of Jiangsu Oilfield Wei 5 crude oil. According to the industry standard SY-T5281-2000 crude oil demulsifier performance test method, the water content of the oil sample was 46%, the demulsifier addition amount was 100 mg / L, and the test temperature was 50°C. The test results are recorded in Table 1.

[0026] Table 1 In the same period of work, the applicant verified that a hyperbranched multi-branched polymer material of a main chain polyester and a branched polyether prepared by the SCVP-RAFT method combined with the chlorine substitution method can quickly demulsify crude oil, and when the demulsifier dosage is 100 mg / ml, the dehydration rate can reach more than 90% within 60 minutes. In this application, magnetic nanoparticles are combined with polysilicate aluminum iron, which further accelerates the demulsification rate, and the dehydration rate can reach more than 90% within half an hour; in addition, due to the presence of magnetic nanoparticles, the composite demulsifier of this application can also be recovered by an external magnetic field and can be recycled for more than ten times, while the comparative solution can be recycled up to three times.

[0027] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation modes, and they can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to the specific details and the illustrations shown and described herein.

Claims

1. A method for preparing a composite demulsifier based on magnetic nanoparticles, characterized in that: The steps include: S1, preparing Fe3O4 magnetic nanoparticles by coprecipitation method, and then modifying their surface with KH570 to obtain KH570-Fe3O4 magnetic nanoparticles for standby use; S2. Add vinyl trithiocarbonate, AIBN, p-chloromethylstyrene and 2-methylene-1,3-dioxepane into a reaction flask, then add an organic solvent and stir to mix evenly, introduce an inert gas to bubble for 30 minutes, then heat to 70-80°C under the protection of inert gas and react for 6-8 hours; S3. After the reaction is completed, remove the inert gas, cool to room temperature, add organic solvent for dilution, add CTAB and methoxy polyethylene glycol, add a certain amount of sodium hydroxide solution, heat to 70-80 °C and react overnight, cool to room temperature, add anhydrous ether solution, filter and vacuum dry; S4. Add a certain amount of KH570-Fe3O4 magnetic nanoparticles and N,N-dimethylformamide to the reaction bottle, disperse them evenly by ultrasound, then add a certain amount of the product of step S3 and AIBN, bubble inert gas for 30 min, then heat to 70-80°C under the protection of inert gas and react for 6-8 h; after cooling to room temperature, add polyaluminum ferrosilicate and stir well, then pour into anhydrous ether solution, filter and dry in vacuum to obtain.

2. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: The structural formula of the vinyl trithiocarbonate is .

3. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: The molar ratio of the vinyl trithiocarbonate, AIBN, p-chloromethylstyrene and 2-methylene-1,3-dioxepane is 1:0.2:30-60:40-70.

4. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: The organic solvent is a mixed solution of equal volumes of toluene and N,N-dimethylformamide.

5. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: The molecular weight of the methoxy polyethylene glycol is 400-1000, and the molar ratio of the methoxy polyethylene glycol to p-chloromethylstyrene is 1-1.5:

1.

6. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: The mass fraction of the sodium hydroxide solution is 30%.

7. The method for preparing a composite demulsifier based on magnetic nanoparticles according to claim 1, characterized in that: In the step S4, the mass ratio of KH570-Fe3O4 magnetic nanoparticles to the product of step S3 and AIBN is 10:1:0.001; the mass ratio of the polyaluminium ferrosilicate to the product of step S3 is 0.2-0.8:

1.

8. A composite demulsifier based on magnetic nanoparticles obtained by the preparation method according to any one of claims 1 to 7.

Citation Information

Cited By

  • Hyperbranched chain polyether demulsifier and preparation method thereof

    CN119144002A

  • A hyperbranched multi-branched polyether demulsifier and its preparation method

    CN119144002B