Small-size internal insulation metal sleeve and preparation method thereof

Through the combination of polyethylene naphthalate film and UV curing glue, the problem of internal insulation difficulty of small-sized metal thin-wall sleeves is solved, and high-standard insulation effect and simplicity of operation is achieved. It is suitable for micro electronic equipment High frequency application.

CN119028680APending Publication Date: 2024-11-26BEIJING RES INST OF TELEMETRY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411021928.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-29
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The internal insulation of small-sized metal thin-wall sleeves is difficult, and traditional methods are difficult to ensure the uniformity and reliability of the insulating layer, especially in micro-equipment, where the insulating layer is easily displaced or contaminated with the welding area.

Method used

The internal insulation method of combining polyethylene naphthalate film with UV curing glue is adopted. The insulating film is attached to the inner surface of the metal sleeve by ultraviolet curing glue layer to form a high-reliability inner insulation layer, simplifying the process and reducing the difficulty of operation .

Benefits of technology

It realizes high standard internal insulation of small-size metal thin-walled sleeves, ensures uniformity of the insulation layer and cleanliness of the welding area, is suitable for micro electronic equipment, and improves processing quality and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028680A_ABST
    Figure CN119028680A_ABST
Patent Text Reader

Abstract

The invention provides a small-size internal insulation metal sleeve and a preparation method thereof, and the small-size internal insulation metal sleeve comprises a metal thin-wall sleeve, a curing glue layer and an insulation film which are sequentially connected from outside to inside; the metal thin-wall sleeve is a hollow cylinder with the wall thickness smaller than 0.5 mm, the outer diameter smaller than 10 mm and the height smaller than 10 mm. The curing adhesive layer is UV curing adhesive, the curing adhesive layer is cured under the action of ultraviolet rays, the insulating film is attached to the metal thin-wall sleeve to form an inner insulating layer, and the curing adhesive layer and the insulating film both cover the inner surface of the metal thin-wall sleeve. According to the method, the polyethylene naphthalate film is used as an insulating material, and a specific fixing technology is combined, so that efficient internal insulation of the small-size metal thin-wall sleeve is realized, and the insulation stability and reliability are remarkably improved. The tool provided by the invention is simplified and convenient to operate, so that the insulation method is more suitable for batch production and has remarkable economic benefits and application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrical components, and in particular to a small-sized internally insulated metal sleeve and a preparation method thereof. Background Art

[0002] With the continuous miniaturization and increasing functionality of electronic devices, the insulation requirements for internal components are becoming more and more stringent. Among the many electronic components, small-sized thin-walled metal sleeves are widely used in various types of microelectronic devices as an important connection component. However, due to the relatively small size of these sleeves, their internal insulation is difficult, especially in micro sleeves with a wall thickness of less than 0.5mm, an outer diameter of less than 10mm, and a height of less than 10mm. This challenge is particularly prominent.

[0003] Traditional internal insulation methods, such as spraying or dipping, make it difficult to ensure the uniformity of the insulation layer during the process, which affects reliability. In addition, due to the limited internal space of the small-sized sleeve, the operation is difficult, and the insulation layer is prone to shifting or contaminating the welding area, further increasing the difficulty of insulation.

[0004] Therefore, there is an urgent need for a new internal insulation method that can meet the high insulation requirements of small-sized metal thin-walled sleeves, while being easy to operate and providing a uniform and reliable insulation layer to meet the development needs of miniaturized electronic equipment. Summary of the invention

[0005] The present invention aims to solve the insulation problem of small-sized metal thin-walled sleeves and provides a small-sized internally insulated metal sleeve and a preparation method thereof, which can significantly improve the processing quality, effectively achieve high-standard internal insulation requirements, and ensure the convenience of assembly and the cleanliness of the welding area. At the same time, it focuses on the simplification of the process, is easy to operate, is suitable for large-scale production, and has significant practical value.

[0006] The present invention provides a small-sized inner insulating metal sleeve, comprising a metal thin-wall sleeve, a curing adhesive layer, and an insulating film connected in sequence from outside to inside;

[0007] The metal thin-walled sleeve is a hollow cylinder with a wall thickness of less than 0.5 mm, an outer diameter of less than 10 mm, and a height of less than 10 mm;

[0008] The curing adhesive layer is a UV curing adhesive. The curing adhesive layer is cured under the action of ultraviolet rays and adheres the insulating film to the metal thin-walled sleeve to form an inner insulating layer. Both the curing adhesive layer and the insulating film cover the inner surface of the metal thin-walled sleeve.

[0009] The small-sized inner insulating metal sleeve described in the present invention is preferably made of any one of the following materials: stainless steel, copper, silver, gold or a metal composite material;

[0010] The material of the insulating film is polyethylene naphthalate, and the thickness of the insulating film is 0.05 to 2 mm.

[0011] In the small-sized inner insulating metal sleeve described in the present invention, as a preferred embodiment, the material of the cured adhesive layer is a silicone prepolymer with acrylic acid-based functions, and the thickness of the cured adhesive layer is 1 to 20 μm.

[0012] The small-sized inner-insulated metal sleeve described in the present invention is preferably configured such that the wavelength of the ultraviolet rays is 315-400 nm.

[0013] The present invention provides a method for preparing a small-sized inner insulating metal sleeve, which, as a preferred embodiment, comprises the following steps:

[0014] S1. Select the materials of the curing adhesive layer and the insulating film and prepare the UV curing adhesive and the insulating film used for the curing adhesive layer;

[0015] S2. Cut the size of the insulating film according to the inner diameter of the metal thin-walled sleeve. The length of the insulating film is 3 to 5 mm larger than the inner diameter of the metal thin-walled sleeve, and the width is 0.1 to 1 mm larger than the height of the metal thin-walled sleeve.

[0016] S3, preparing an insulating film installation tool, the insulating film installation tool comprising a connected end and a rod, the end is a truncated cone structure, and the rod is a cylindrical structure;

[0017] S4. Put the insulating film on the front end of the end to form a junction with a width of 3 to 5 mm, use a cotton swab to dip the UV curing glue and evenly apply it to the junction area of ​​the insulating film, and use an ultraviolet lamp to irradiate the area coated with the UV curing glue for rapid curing;

[0018] S5. Use a cotton swab to dip UV curing glue and evenly apply it to the surface of the insulating film. Slowly insert the insulating film installation tool with the insulating film on the end into the metal thin-walled sleeve. Make use of the ductility of the insulating film and the diameter change of the end to make the insulating film flat and close to the inner wall of the metal thin-walled sleeve.

[0019] S6. Adjust the position of the insulating film under a stereo microscope, position the insulating film in a predetermined area inside the metal thin-walled sleeve, and make the insulating film fully cover the inner wall of the metal thin-walled sleeve; use an ultraviolet lamp to irradiate the area coated with UV curing glue to quickly cure it to obtain a cured glue layer and bond the insulating film to the inner wall of the metal thin-walled sleeve;

[0020] S7. Check the coverage of the insulating film on the inner wall of the metal thin-walled sleeve under a stereo microscope, and use a surgical blade to remove excess film at both ends of the metal thin-walled sleeve to obtain a small-sized inner insulating metal sleeve;

[0021] S8. Perform an insulation performance test. When the resistance value of the small-sized inner insulating metal sleeve does not reach a threshold value, use alcohol to remove the insulating film, return to step S2, and re-prepare. When the resistance value of the small-sized inner insulating metal sleeve is greater than the threshold value, a preparation method for a small-sized inner insulating metal sleeve is completed.

[0022] The method for preparing a small-sized internally insulated metal sleeve described in the present invention is, as a preferred embodiment, in step S2, the diameter of the rod is the same as the inner diameter of the metal thin-walled sleeve, the minimum diameter of the end is 0.1 to 0.5 mm smaller than the inner diameter of the metal thin-walled sleeve, and the length is greater than the height of the metal thin-walled sleeve.

[0023] The method for preparing a small-sized inner insulating metal sleeve described in the present invention is, as a preferred embodiment, in steps S4 and S6, an ultraviolet lamp with a wavelength of 365 nm is used to irradiate the treatment area for 60 seconds to quickly cure the UV curing adhesive.

[0024] The method for preparing a small-sized inner insulating metal sleeve of the present invention is preferably such that in step S8, the threshold value is 10 12 Ω.

[0025] The invention provides a processing method for the internal insulation of a small-sized metal thin-walled sleeve to improve the electrical insulation performance thereof, and is suitable for the insulation requirements in the fields of electronics, electricity and precision machinery.

[0026] The present invention aims at the problem of internal insulation of a small-sized metal thin-walled sleeve, especially in the application field of piezoelectric high-frequency response dynamic force sensitive sensors, and proposes an implementation method that meets high-standard internal insulation requirements.

[0027] The core of the present invention is to use polyethylene naphthalate film in combination with UV curing adhesive fixing method to achieve high reliability internal insulation of thin-walled metal sleeves. The present invention is further described in detail:

[0028] Step 1: Material selection: Select polyethylene naphthalate film as the insulating material, which has excellent electrical insulation performance, heat resistance and chemical stability. Select a suitable UV curing adhesive to connect the polyethylene naphthalate film and the metal sleeve.

[0029] Step 2: Cutting to size: According to the inner diameter of the metal thin-walled sleeve, cut out the polyethylene naphthalate film of the corresponding size. The length of the film is 3 to 5 mm larger than the sleeve diameter, and the width is slightly larger than the sleeve height.

[0030] Step 3: Preliminary treatment of the insulating film: Put the insulating film on the end of the special installation tool to form a junction with a width of 3 to 5 mm. Use a cotton swab to apply an appropriate amount of UV curing glue evenly to the junction area of ​​the film. Use an ultraviolet lamp to irradiate the area coated with UV curing glue to achieve rapid curing.

[0031] Step 4: Film loading: Use a cotton swab to apply an appropriate amount of UV curing glue evenly to the film surface. Slowly insert the special installation tool with an insulating film on the end into the metal thin-walled sleeve, and use the ductility of the film and the variable diameter of the tool to ensure that the film can be flat and close to the inner wall of the sleeve.

[0032] Step 5: Film positioning: Adjust the position of the insulating film under a stereo microscope and position the film in the appropriate area inside the sleeve to ensure that the insulating film fully covers the inner wall of the metal sleeve. Use an ultraviolet lamp to irradiate the area coated with UV curing glue to achieve rapid curing.

[0033] Step 6: Internal insulation inspection: Check the film coverage inside the metal sleeve under a stereo microscope and use a surgical blade to remove excess film at both ends of the sleeve.

[0034] Step 7: Performance test: Perform insulation performance test on the treated metal thin-walled sleeve to ensure that the resistance value of its internal insulation layer is greater than 10 12 Ω, meeting the requirements of high insulation performance.

[0035] The present invention has the following advantages:

[0036] (1) The present invention proposes for the first time to use polyethylene naphthalate film material as the inner insulation layer of a small-sized metal thin-walled sleeve, which has excellent electrical insulation performance and high-temperature stability and is particularly suitable for high-frequency application environments. This application not only meets the requirements of more than 10 12 The insulation requirements of Ω are met, while also ensuring the performance stability of the material in extreme environments.

[0037] (2) The present invention provides an innovative inner insulation layer fixing technology: by introducing UV curing glue as a fixing method between the insulation film and the metal sleeve, the problem of positioning and fixing the insulation layer in a small space is innovatively solved. Compared with traditional physical fixing or thermal curing methods, UV curing glue provides a fast, efficient and non-polluting solution for the welding area.

[0038] (3) The present invention has innovated and simplified the process: The internal insulation method proposed in the present invention simplifies the traditional complex process flow, reduces the difficulty of operation, and is easy to implement quickly on production lines of different scales. This is of great significance for improving production efficiency and reducing production costs, especially in the development of new products that require rapid response and small-batch customized production. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] Figure 1 It is a schematic diagram of the structure of a small-sized inner insulating metal sleeve;

[0040] Figure 2 The present invention is a flow chart of a method for preparing a small-sized inner insulating metal sleeve;

[0041] Figure 3 A schematic diagram of an insulating film installation tool in step S3 of a method for preparing a small-sized inner insulating metal sleeve;

[0042] Figure 4 It is a front end schematic diagram of a method for preparing a small-sized inner insulating metal sleeve, in which step S4 an insulating film is sleeved on the end of an insulating film installation tool;

[0043] Figure 5 A flow chart of a method for preparing a small-sized inner insulating metal sleeve, step S4, forming a junction with a width of 3 to 5 mm;

[0044] Figure 6 The present invention is a cross-sectional schematic diagram of a method for preparing a small-sized inner insulating metal sleeve and curing it by ultraviolet irradiation.

[0045] Reference numerals:

[0046] 1. Metal thin-walled sleeve; 2. Cured adhesive layer; 3. Insulation film; 4. Insulation film installation tool; 41. End; 42. Rod. DETAILED DESCRIPTION

[0047] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments.

[0048] Example 1

[0049] like Figures 1 to 6 As shown, a small-sized internally insulated metal sleeve and its preparation method, the surface of the metal thin-walled sleeve 1 is covered with an insulating film 3, and a curing glue 2 is applied between the metal thin-walled sleeve 1 and the insulating film 3, wherein the insulating film 3 is a polyethylene naphthalate film. The thin-walled sleeve is cut into corresponding sizes according to the length and the width of the welding weld, and its thickness is selected to be 0.05 to 2 mm according to the required insulation tolerance;

[0050] The curing adhesive 2 is composed of UV curing adhesive, and a prepolymer with high thermal stability is selected, such as a silicone prepolymer with acrylic acid group function, and its thickness is 1 to 20 μm;

[0051] The metal thin-walled sleeve 1 is characterized by a wall thickness of less than 0.5 mm, an outer diameter of less than 10 mm, and a height of less than 10 mm;

[0052] The metal thin-walled sleeve 1 is made of stainless steel, copper, silver, gold or a metal composite material;

[0053] The light irradiating the curing adhesive 2 to cure it is ultraviolet light with a wavelength range of 315 to 400 nm.

[0054] Taking a metal thin-walled sleeve with an outer diameter of 8 mm, a height of 8 mm, and a wall thickness of 0.3 mm as an example, the specific steps of implementing the present invention are described in detail:

[0055] S1. Material selection: Use polyethylene naphthalate film with a width of 8.5 mm and a thickness of 0.05 mm, and UV curing adhesive suitable for bonding metal to polyethylene naphthalate film.

[0056] S2. Film cutting: Cut the polyethylene naphthalate film into strips with a length of 28 mm, ensuring the intersection area.

[0057] S3. Prepare the insulating film installation tool 4, such as Figure 3 As shown, the insulating film installation tool 4 includes a connected end 41 and a rod 42, the end 41 is a truncated cone structure, and the rod 42 is a cylindrical structure; the front end diameter of the end 41 is 0.2mm smaller than the inner diameter of the metal sleeve 1, and the bottom is the same as the inner diameter of the metal tube 1, and the bottom and the metal sleeve have the same diameter. The length of the end 41 is 20mm.

[0058] S4. Preliminary treatment of insulating film: reference Figure 4 , put the insulating film on the end of the special installation tool, refer to Figure 5 , forming a junction with a width of about 5mm, use a cotton swab to apply an appropriate amount of UV curing glue evenly to the junction area of ​​the film. Figure 6 , use ultraviolet lamp with a wavelength of 365nm to irradiate the treated area for 60 seconds to achieve rapid curing of UV curing adhesive.

[0059] S5. Film loading: Use a cotton swab to apply an appropriate amount of UV curing glue evenly to the surface of the film 3. Slowly insert the special installation tool 4 with the insulating film 3 on the end into the metal thin-walled sleeve 1, and use the ductility of the film 3 and the variable diameter of the tool 4 to ensure that it is close to the inner wall.

[0060] S6. Film positioning: Adjust the position of the insulating film 3 under a stereo microscope and position the film 3 in a suitable area inside the sleeve 1 to ensure that the insulating film 3 fully covers the inner wall of the metal sleeve 1. Figure 6 The treated area is irradiated with an ultraviolet lamp having a wavelength of 365 nm for 60 seconds to achieve rapid curing of the UV curing adhesive, thereby obtaining a cured adhesive layer 2 and an insulating film 3 bonded to the surface of the cured adhesive layer 2.

[0061] S7. Internal insulation inspection: Check the coverage of the film layer inside the metal sleeve 1 under a stereo microscope, and use a surgical blade to remove excess film 3 at both ends of the sleeve.

[0062] S8. Insulation performance test: After curing, test the insulation resistance of sleeve 1 to ensure that it is greater than 10 12 Ω.

[0063] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes according to the technical scheme and inventive concept of the present invention within the technical scope disclosed by the present invention, which should be covered by the protection scope of the present invention.

Claims

1. A small-sized inner insulating metal sleeve, characterized in that: It comprises a metal thin-wall sleeve (1), a curing adhesive layer (2), and an insulating film (3) which are connected in sequence from outside to inside; The metal thin-walled sleeve (1) is a hollow cylinder with a wall thickness of less than 0.5 mm, an outer diameter of less than 10 mm, and a height of less than 10 mm; The curing adhesive layer (2) is a UV curing adhesive. The curing adhesive layer (2) is cured under the action of ultraviolet rays and adheres the insulating film (3) to the metal thin-walled sleeve (1) to form an inner insulating layer. The curing adhesive layer (2) and the insulating film (3) both cover the inner surface of the metal thin-walled sleeve (1).

2. A small-sized inner insulating metal sleeve according to claim 1, characterized in that: The material of the metal thin-walled sleeve (1) is any one of the following: stainless steel, copper, silver, gold or a metal composite material; The material of the insulating film (3) is polyethylene naphthalate, and the thickness of the insulating film (3) is 0.05 to 2 mm.

3. A small-sized inner insulating metal sleeve according to claim 1, characterized in that: The material of the cured adhesive layer (2) is a silicone prepolymer having acrylic acid-based functions, and the thickness of the cured adhesive layer (2) is 1 to 20 μm.

4. A small-sized inner insulating metal sleeve according to claim 1, characterized in that: The wavelength of the ultraviolet rays is 315-400nm.

5. A method for preparing a small-sized internally insulated metal sleeve according to any one of claims 1 to 4, characterized in that: The following steps are involved: S1, selecting the materials of the curing adhesive layer (2) and the insulating film (3) and preparing UV curing adhesive used for the curing adhesive layer (2) and the insulating film (3); S2, cutting the size of the insulating film (3) according to the inner diameter of the metal thin-walled sleeve (1), wherein the length of the insulating film (3) is 3 to 5 mm greater than the inner diameter of the metal thin-walled sleeve (1), and the width is 0.1 to 1 mm greater than the height of the metal thin-walled sleeve (1); S3, preparing an insulating film installation tool (4), wherein the insulating film installation tool (4) comprises a connected end portion (41) and a rod portion (42), wherein the end portion (41) is a truncated cone structure, and the rod portion (42) is a cylindrical structure; S4, putting the insulating film (3) on the front end of the end (41) to form a junction with a width of 3 to 5 mm, using a cotton swab to dip the UV curing glue and evenly apply it to the junction area of ​​the insulating film (3), and using an ultraviolet lamp to irradiate the area coated with the UV curing glue for rapid curing; S5. Use a cotton swab to dip the UV curing glue and evenly apply it to the surface of the insulating film (3). Slowly insert the insulating film installation tool (4) with the insulating film (3) on the end into the interior of the metal thin-walled sleeve (1). Make use of the ductility of the insulating film (3) and the diameter change of the end (41) to make the insulating film (3) flat and tightly attached to the inner wall of the metal thin-walled sleeve (1). S6. Adjust the position of the insulating film (3) under a stereo microscope, position the insulating film (3) at a predetermined area inside the metal thin-walled sleeve (1) and make the insulating film (3) completely cover the inner wall of the metal thin-walled sleeve (1); use an ultraviolet lamp to irradiate the area coated with the UV curing glue to quickly cure it to obtain the curing glue layer (2) and adhere the insulating film (3) to the inner wall of the metal thin-walled sleeve (1); S7, inspecting the coverage of the insulating film (3) on the inner wall of the metal thin-walled sleeve (1) under a stereo microscope, and removing the excess film at both ends of the metal thin-walled sleeve (1) with a surgical blade to obtain the small-sized inner insulating metal sleeve; S8, perform an insulation performance test. When the resistance value of the small-sized inner insulating metal sleeve does not reach a threshold value, use alcohol to remove the insulating film (3), return to step S2, and re-prepare. When the resistance value of the small-sized inner insulating metal sleeve is greater than the threshold value, a method for preparing a small-sized inner insulating metal sleeve is completed.

6. The method for preparing a small-sized internally insulated metal sleeve according to claim 5, characterized in that: In step S2, the diameter of the rod portion (42) is the same as the inner diameter of the metal thin-walled sleeve (1), the minimum diameter of the end portion (41) is 0.1 to 0.5 mm smaller than the inner diameter of the metal thin-walled sleeve (1), and the length is greater than the height of the metal thin-walled sleeve (1).

7. The method for preparing a small-sized internally insulated metal sleeve according to claim 5, characterized in that: In steps S4 and S6, an ultraviolet lamp with a wavelength of 365 nm is used to irradiate the treated area for 60 seconds to perform rapid curing of the UV curing adhesive.

8. The method for preparing a small-sized internally insulated metal sleeve according to claim 5, characterized in that: In step S8, the threshold is 10 12 Ω.