Wiring manufacturing method, wiring structure and chip packaging structure

By using cutting and electroplating technology to form a high-precision trace structure on the insulating layer during semiconductor packaging, the problem of poor linearity and fine line production in the prior art is solved, and more regular and stable signal transmission is achieved.

CN119028850APending Publication Date: 2024-11-26CHENGDU ESWIN SYST IC CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411138094.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

During the semiconductor packaging process, the prior art has poor line linearity and poor resistance due to insufficient resolution capabilities of the exposure machine and insufficient filming capabilities of the film material, and the inability to achieve fine line production and small line spacing.

Method used

A groove is formed on the insulating layer by cutting, a seed metal layer is made, and conductive metal is deposited in the insulating layer groove by electroplating to form a high-precision trace structure.

Benefits of technology

A more refined pattern design is achieved, and lines with line widths less than 2 microns are significantly improved, the regularity of the pattern is ensured, the uniformity and stability of signal transmission are avoided, and the pattern width fluctuations caused by inconsistent spacing are avoided.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028850A_ABST
    Figure CN119028850A_ABST
Patent Text Reader

Abstract

The invention provides a wiring manufacturing method, a wiring structure and a chip packaging structure. The wiring manufacturing method comprises the following steps: providing an insulating layer, forming a wiring pattern formed by an insulating layer groove on the insulating layer in a cutting mode, then manufacturing a seed metal layer on the insulating layer, then electroplating conductive metal on the seed metal layer, and taking the conductive metal in the insulating layer groove as wiring. Thus, according to the scheme, finer pattern design can be achieved, a line with the line width smaller than 2 micrometers can be formed, meanwhile, pattern regularity can be remarkably improved, the problem of pattern width fluctuation caused by inconsistent intervals is solved, and uniformity and stability of signal transmission are ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor manufacturing, and in particular to a wiring manufacturing method, a wiring structure and a chip packaging structure. Background Art

[0002] Re-distribution Layer (RDL) is a key technology in semiconductor packaging technology. It achieves more efficient electrical connection and interconnection by rearranging the I / O ports on the chip and extending them from their original positions to a wider area on the chip surface.

[0003] In the RDL packaging design and manufacturing process, a film material (such as photoresist) is usually coated on the film layer on the silicon wafer, and then the pattern is transferred to the film material by exposure and development using a mask, and finally a precisely patterned film layer is obtained by etching. However, the pattern (such as the circuit) obtained by the above method may cause poor circuit linearity, poor tolerance or high defect rate due to factors such as insufficient resolution capability of the exposure machine and insufficient film-standing capability of the film material. At the same time, the circuit spacing is also limited, and the production of fine circuits cannot be achieved. Summary of the invention

[0004] In order to overcome the technical problems mentioned in the above technical background, an embodiment of the present application provides a method for manufacturing an antenna line, the method comprising:

[0005] providing an insulating layer;

[0006] Forming a wiring pattern formed by insulating layer grooves on the insulating layer by cutting;

[0007] forming a sub-metal layer on the insulating layer;

[0008] Conductive metal is electroplated on the seed metal layer, and the conductive metal located in the groove of the insulating layer is used as a routing line.

[0009] In a possible implementation manner, after the step of manufacturing a sub-metal layer on the insulating layer, the method further includes:

[0010] An isolation layer is formed on a side of the seed metal layer outside the insulating layer groove away from the insulating layer.

[0011] In a possible implementation, the step of electroplating a conductive metal on the seed metal layer and using the conductive metal in the groove of the insulating layer as a routing line includes:

[0012] Electroplating a conductive metal on the seed metal layer;

[0013] removing the isolation layer;

[0014] The seed metal layer located between adjacent insulating layer grooves is removed to obtain the routing line formed by the conductive metal located in the insulating layer grooves.

[0015] In a possible implementation, the step of forming a wiring pattern formed by insulating layer grooves on the insulating layer by cutting includes:

[0016] Using laser cutting to form a wiring pattern formed by insulating layer grooves on the insulating layer; or,

[0017] Using electron beam cutting to form a wiring pattern formed by insulating layer grooves on the insulating layer; or,

[0018] Ion beam cutting is used to form a wiring pattern formed by insulating layer grooves on the insulating layer.

[0019] Another object of the present application is to provide a wiring structure, wherein the wiring structure is manufactured by using a plurality of wiring manufacturing methods provided by the present application, and the wiring structure comprises:

[0020] An insulating layer, one side of the insulating layer is provided with a routing pattern formed by insulating layer grooves;

[0021] A seed metal layer, located on the sidewall and bottom of the insulating layer groove;

[0022] A wiring is located in the insulating layer groove and in contact with the seed metal layer.

[0023] In a possible implementation, a side of the wiring away from the bottom of the insulating layer groove is parallel to the surface of the insulating layer, and the side away from the bottom of the insulating layer groove is protruding relative to the surface of the insulating layer;

[0024] In a possible implementation, in a cross section perpendicular to the insulating layer and the extension direction of the wiring, the cross-sectional shape of the wiring is a rectangle;

[0025] At different positions in the extending direction of the routing, the cross-sectional dimensions of the routing are the same.

[0026] In a possible implementation, in a cross section perpendicular to the insulating layer and the extending direction of the wiring, the size of the wiring is 0.5 micrometers to 2.0 micrometers, and the spacing between adjacent insulating layer grooves is 0.5 micrometers to 2.0 micrometers.

[0027] In a possible implementation, the seed metal layer is a metal copper layer, or a stacked structure of a metal titanium layer and a metal copper layer;

[0028] The wiring is a metal copper wiring.

[0029] Another object of the present application is to provide a chip packaging structure, which includes a plurality of routing structures provided by the present application.

[0030] Based on any of the above aspects, the embodiments of the present application provide a routing method, routing structure and chip packaging structure. Thus, through the above scheme, not only can a more sophisticated pattern design be achieved, forming a line with a line width of less than 2 microns, but also the regularity of the pattern can be significantly improved, avoiding the pattern width fluctuation problem caused by inconsistent spacing, and ensuring the uniformity and stability of signal transmission. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0032] Figure 1 This embodiment provides a possible state of the circuit when the film material has insufficient film-standing capacity;

[0033] Figure 2 A possible state of the circuit provided in this embodiment when the exposure machine has insufficient resolution capability;

[0034] Figure 3 A schematic diagram of a flow chart of a wiring production method provided in this embodiment;

[0035] Figure 4 for Figure 3 The corresponding process diagram;

[0036] Figure 5 Part of the process flow chart provided for this embodiment;

[0037] Figure 6 A schematic diagram of a wiring structure provided in this embodiment;

[0038] Figure 7 A partial structural diagram of a wiring structure provided in this embodiment.

[0039] Icon: 10-line, 20-routing structure, 200-insulating layer, 2001-insulating layer groove, 210-seed metal layer, 220-routing, 230-isolation layer. DETAILED DESCRIPTION

[0040] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations.

[0041] Therefore, the following detailed description of the embodiments of the present application provided in the accompanying drawings is not intended to limit the scope of the present application for which protection is sought, but merely represents selected embodiments of the present application. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the present application.

[0042] It should be noted that similar reference numerals and letters denote similar items in the following drawings, and therefore, once an item is defined in one drawing, further definition and explanation thereof is not required in subsequent drawings.

[0043] In the description of this application, it should be noted that the terms "upper", "lower", etc. indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings, or the orientation or positional relationship in which the product of the application is usually placed when in use, which is only for the convenience of describing this application and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on this application. In addition, the terms "first", "second", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.

[0044] It should be noted that, in the absence of conflict, different features in the embodiments of the present application may be combined with each other.

[0045] Currently, in the design and manufacturing process of redistribution layer (RDL) packaging, a film material (such as photoresist) is usually coated on a film layer on a silicon wafer, and then a mask is used to transfer the pattern to the film material through exposure and development, and finally an etching process is performed to obtain a precisely patterned film layer.

[0046] However, the pattern (such as circuit) obtained by this method may have problems such as uneven circuit spacing and irregular shape due to factors such as insufficient resolution capability of the exposure machine and insufficient film-forming capability of the film material. At the same time, this method also limits the production of fine circuits.

[0047] For example, see Figure 1 , Figure 1The present embodiment provides an irregular state that the circuit 10 may present when the film material has insufficient film-forming ability. The film-forming ability of the film material is the ability to form a uniform, stable and high-quality thin film. Insufficient film-forming ability may lead to uneven film thickness, affecting the precise transfer of patterns in subsequent exposure and etching steps. At the same time, uneven film thickness may lead to inaccurate line width control of the circuit 10, affecting product performance and quality.

[0048] For example, see Figure 2 , Figure 2 The present embodiment provides a state where the circuit 10 may present a state of uneven spacing when the exposure machine has insufficient resolution capability. The exposure machine's resolution capability refers to its ability to clearly distinguish and print out the minimum feature size. If the exposure machine has insufficient resolution capability, it may not be able to accurately print out the designed minimum line width or spacing, resulting in the size of the circuit 10 actually manufactured exceeding the requirement. At the same time, it will also cause the width of the circuit 10 to be inconsistent in different areas, causing the non-uniformity of the performance of the circuit 10, which also affects the performance and quality of subsequent products.

[0049] In order to solve the above-mentioned technical problems, the inventor innovatively designed the following technical solutions, and the specific implementation solutions of the present application will be described in detail below in conjunction with the accompanying drawings. It should be noted that the defects existing in the solutions in the above-mentioned prior art are the results obtained by the inventor after practice and careful research. Therefore, the discovery process of the above-mentioned technical problems and the solutions proposed in this embodiment below for the above-mentioned problems should all be the contributions made by the inventor to the present application in the process of invention and creation, and should not be understood as the technical content known to those skilled in the art.

[0050] See also Figure 3 and Figure 4 , Figure 3 A schematic diagram of the steps of a wiring production method provided in this embodiment, Figure 4 for Figure 3 The corresponding process diagram. The wiring production method includes the following steps:

[0051] Step S110 , providing an insulating layer 200 .

[0052] In this embodiment, the insulating layer 200 may be made of inorganic materials such as silicon dioxide (SiO2) or silicon nitride (Si3N4). It is worth noting that the insulating layer 200 is not specifically limited in material and may be selected according to actual conditions. For example, in some embodiments, photoresist may be used instead.

[0053] Step S120, forming a wiring pattern formed by the insulating layer grooves 2001 on the insulating layer 200 by cutting;

[0054] In this embodiment, the insulating layer groove 2001 is formed by removing part of the insulating layer 200 by high-energy cutting. The insulating layer groove 2001 forms a wiring pattern. The insulating layer groove 2001 with a regular and uniform shape can be formed on the insulating layer 200 by cutting.

[0055] It is worth noting that the specific shape of the routing pattern is not specifically limited here and needs to be designed and produced according to the requirements of the actual design scheme.

[0056] Step S130 , forming a seed metal layer 210 on the insulating layer 200 .

[0057] In this step, the seed metal layer 210 mainly serves as a plating cathode for the subsequent electroplating process to ensure that the metal conductive ions (e.g., Cu + ) can obtain electrons on the seed metal layer 210 to form metal conductive particles (for example, Cu atoms) which can be deposited in the insulating layer groove 2001.

[0058] It is worth noting that in semiconductor manufacturing, the seed metal layer 210 is a very critical film, which is used as the basis for the growth of the metal layer (that is, the conductive metal in this embodiment) in the subsequent electroplating or chemical vapor deposition (CVD) process. The seed metal layer 210 is usually composed of a metal or alloy with a catalytic effect, such as copper, nickel, gold, etc. For example, in this embodiment, the seed metal layer 210 can be a metal copper layer, or a stacked structure of a metal titanium layer and a metal copper layer.

[0059] Step S140, electroplating a conductive metal on the seed metal layer 210, and using the conductive metal in the groove of the insulating layer as the wiring 220;

[0060] In this step, the conductive metal in the insulating layer groove 2001 forms a conductive trace.

[0061] For further information, see Figure 5 , Figure 5 for Figure 3 After step S130, the wiring manufacturing method provided in this embodiment further includes:

[0062] An isolation layer 230 is formed on a side of the seed metal layer 210 away from the insulation layer 200 and outside the insulation layer groove 2001 .

[0063] In this embodiment, the isolation layer 230 can be made of an insulating material. The main purpose of the isolation layer 230 is to prevent the electroplated conductive metal from growing in the area outside the insulating layer groove 2001 when the conductive metal is electroplated on the seed metal layer 210 in the insulating layer groove 2001, that is, to prevent the electroplated conductive metal from growing in the area between adjacent insulating layer grooves 2001, and to prevent the conductive metals in the insulating layer groove 2001 from being connected together.

[0064] Further, please see again Figure 5 After forming an isolation layer 230 on a side of the seed metal layer 210 away from the insulating layer 200 outside the insulating layer groove 2001, step S140 includes:

[0065] First, a conductive metal is electroplated on the seed metal layer 210;

[0066] Next, the isolation layer 230 is removed;

[0067] Finally, the seed metal layer 210 located between adjacent insulating layer grooves 2001 is removed to obtain a trace 220 composed of a conductive metal located in the insulating layer grooves 2001 .

[0068] In this embodiment, the seed metal layer 210 is set to control the deposition position of the conductive metal during the electroplating process. By way of example, in this embodiment, the seed metal layer 210 can control the deposition of the conductive metal in a specific area (i.e., the insulating layer groove 2001). After the electroplating is completed, removing the seed metal layer 210 outside the insulating layer groove 2001 can not only ensure the accuracy of the routing, but also disconnect the routing 220 in the adjacent insulating layer groove 2001, thereby avoiding short-circuiting of the routing 220 in the adjacent insulating layer groove 2001, which would affect the performance and reliability of subsequent packaging products.

[0069] Further, step S120 includes cutting using at least three different methods.

[0070] Illustratively, in an implementation manner of this embodiment, a routing pattern formed by the insulating layer grooves 2001 is formed on the insulating layer 200 by laser cutting.

[0071] In this embodiment, laser cutting can be used to control the cutting path and size very accurately, reducing mechanical stress and thermal damage to the material. At the same time, laser cutting is applicable to many different types of insulating layer materials, such as quartz, silicon dioxide, etc., which improves cutting flexibility and product consistency.

[0072] Illustratively, in another implementation of this embodiment, electron beam cutting is used to form a routing pattern formed by the insulating layer grooves 2001 on the insulating layer.

[0073] In this embodiment, electron beam cutting can provide extremely high spatial resolution and can produce very small feature sizes. At the same time, electron beam cutting can achieve sub-micron level precision, which is suitable for high-density integrated circuit design.

[0074] Illustratively, in another implementation of this embodiment, ion beam cutting is used to form a routing pattern formed by the insulating layer grooves 2001 on the insulating layer.

[0075] In this embodiment, the ion beam is composed of charged particles, has high energy, and can effectively cut various materials. Ion beam cutting can accurately control the cutting depth and shape by adjusting the intensity, speed and scanning path of the ion beam. At the same time, ion beam cutting can produce clear edges and sharp corners, which is suitable for the production of fine patterns.

[0076] Based on the same inventive concept, another object of the present application is to provide a wiring structure 20, wherein the wiring structure 20 is manufactured by any of the aforementioned wiring manufacturing methods, see Figure 6 and Figure 7 , Figure 6 A cross-sectional view of a wiring structure 20 provided in this embodiment, Figure 7 This is a cross-sectional view of the insulating layer 200 provided in this embodiment.

[0077] The routing structure 20 includes: an insulating layer 200, a seed metal layer 210 and a routing line 220. A routing pattern formed by an insulating layer groove 2001 is provided on one side of the insulating layer 200. The seed metal layer 210 is located at the sidewall and bottom of the insulating layer groove 2001, and the routing line 220 is located in the insulating layer groove 2001 and in contact with the seed metal layer 210.

[0078] Further, please see again Figure 6 and Figure 7 The side of the trace 220 away from the bottom of the insulating layer groove 2001 is parallel to the surface of the insulating layer 200 , and the side away from the bottom of the insulating layer groove 2001 is protruding relative to the surface of the insulating layer 200 .

[0079] In this embodiment, the side of the trace 220 away from the bottom of the insulating layer groove 2001 is parallel to the surface of the insulating layer 200, indicating that the surface of the trace 220 is flat. For example, in RDL design, a higher interconnection density can be achieved in a limited space, which is very important for reducing the package size. It also helps to reduce the loss and delay in signal transmission and improve data transmission efficiency.

[0080] In addition, the side of the trace 220 away from the bottom of the insulating layer groove 2001 protrudes relative to the surface of the insulating layer 200 to provide a larger contact area. For example, in RDL design, the protruding conductive metal helps to achieve more efficient vertical interconnection.

[0081] The wirings in adjacent insulating layer grooves 2001 are insulated from each other.

[0082] In this embodiment, the wirings 220 in adjacent insulating layer grooves 2001 are insulated from each other to reduce or prevent electromagnetic interference between the wirings 220 , while ensuring that no accidental electrical connection occurs between the wirings 220 to prevent short circuits.

[0083] For further information, see Figure 6 , in a cross section perpendicular to the extending direction of the insulating layer 220 and the wiring 200 , the cross-sectional shape of the wiring 200 is a rectangle;

[0084] At different positions in the extending direction of the wiring 200 , the cross-sectional dimensions of the wiring 200 are the same.

[0085] In this embodiment, the wiring 220 in the wiring structure 20 has a consistent geometric shape and size, which solves the problem of irregular shapes and uneven spacing of the wiring 220 (i.e., lines) in the aforementioned background technology due to factors such as insufficient resolution capability of the exposure machine and insufficient film-forming capability of the film material. At the same time, the regular wiring 220 can better ensure uniform transmission of signals.

[0086] Further, please see again Figure 6 In a cross section perpendicular to the extension direction of the insulating layer 200 and the routing 220, a dimension d1 of the routing 220 is 0.5 microns to 2.0 microns. By way of example, the dimension d1 of the routing 220 includes 0.5 microns, 0.55 microns, 0.68 microns, 0.79 microns, 0.85 microns, 1 micron, 1.25 microns, 1.45 microns, 1.65 microns, 1.85 microns or 2 microns, etc.

[0087] See also Figure 7 In a cross section perpendicular to the extension direction of the insulating layer 200 and the trace 220, a spacing d2 between adjacent insulating layer grooves 2001 is 0.5 microns to 2.0 microns. Exemplarily, the spacing d2 between adjacent insulating layer grooves 2001 includes 0.5 microns, 0.55 microns, 0.68 microns, 0.79 microns, 0.85 microns, 1 micron, 1.25 microns, 1.45 microns, 1.65 microns, 1.85 microns or 2 microns, etc.

[0088] Furthermore, the seed metal layer 210 is a metal copper layer, or a stacked structure of a metal titanium layer and a metal copper layer, and the wiring 220 is a metal copper wiring.

[0089] Based on the same inventive concept, another object of the present application is to provide a chip packaging structure, which includes any of the aforementioned routing structures 20. The routing structure provides consistency of electrical performance in the chip packaging structure, reduces signal interference, enhances mechanical stability and interconnection reliability, and improves the integration of the package.

[0090] In summary, the present application provides a routing method, routing structure and chip packaging structure. The routing method includes: providing an insulating layer, forming a routing pattern formed by insulating layer grooves on the insulating layer by cutting, and then making a seed metal layer on the insulating layer, and then electroplating a conductive metal on the seed metal layer, and using the conductive metal located in the insulating layer groove as the routing. In this way, through the above scheme, not only can a more sophisticated pattern design be achieved to form a line with a line width of less than 2 microns, but also the regularity of the pattern can be significantly improved, avoiding the problem of pattern width fluctuation caused by inconsistent spacing, and ensuring the uniformity and stability of signal transmission.

[0091] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. A wiring production method, characterized in that: The method comprises: providing an insulating layer; Forming a wiring pattern formed by insulating layer grooves on the insulating layer by cutting; forming a sub-metal layer on the insulating layer; Conductive metal is electroplated on the seed metal layer, and the conductive metal located in the groove of the insulating layer is used as a routing line.

2. The wiring production method according to claim 1, characterized in that: After the step of forming a sub-metal layer on the insulating layer, the method further comprises: An isolation layer is formed on a side of the seed metal layer outside the insulating layer groove away from the insulating layer.

3. The wiring production method according to claim 2, characterized in that: The step of electroplating a conductive metal on the seed metal layer and using the conductive metal in the groove of the insulating layer as a routing line comprises: Electroplating a conductive metal on the seed metal layer; removing the isolation layer; The seed metal layer located between adjacent insulating layer grooves is removed to obtain the routing line formed by the conductive metal located in the insulating layer grooves.

4. The wiring production method according to any one of claims 1 to 3, characterized in that: The step of forming a wiring pattern formed by the insulating layer grooves on the insulating layer by cutting comprises: Using laser cutting to form a wiring pattern formed by insulating layer grooves on the insulating layer; or, Using electron beam cutting to form a wiring pattern formed by insulating layer grooves on the insulating layer; or, Ion beam cutting is used to form a wiring pattern formed by insulating layer grooves on the insulating layer.

5. A wiring structure, characterized in that: The wiring structure is manufactured by the wiring manufacturing method according to any one of claims 1 to 4, and the wiring structure comprises: An insulating layer, one side of the insulating layer is provided with a routing pattern formed by insulating layer grooves; A seed metal layer, located on the sidewall and bottom of the insulating layer groove; A wiring is located in the insulating layer groove and in contact with the seed metal layer.

6. The wiring structure according to claim 5, characterized in that: The side of the wiring away from the bottom of the insulating layer groove is parallel to the surface of the insulating layer, and the side away from the bottom of the insulating layer groove is protruding relative to the surface of the insulating layer; The wirings in adjacent insulating layer grooves are insulated from each other.

7. The wiring structure according to claim 5, characterized in that: In a cross section perpendicular to the insulating layer and the extension direction of the wiring, the cross-sectional shape of the wiring is a rectangle; At different positions in the extending direction of the routing, the cross-sectional dimensions of the routing are the same.

8. The wiring structure according to claim 5, characterized in that: On a cross section perpendicular to the insulating layer and the extending direction of the wiring, the size of the wiring is 0.5 micrometers to 2.0 micrometers, and the spacing between adjacent insulating layer grooves is 0.5 micrometers to 2.0 micrometers.

9. The wiring structure according to claim 5, characterized in that: The seed metal layer is a metal copper layer, or a stacked structure of a metal titanium layer and a metal copper layer; The wiring is a metal copper wiring.

10. A chip packaging structure, characterized in that: The chip packaging structure includes the routing structure described in any one of claims 4-9.