Manufacturing method of semiconductor structure

By forming a seed conductive layer on the groove side of the semiconductor structure and electrically contacting the first conductive layer, the uniform growth of the second conductive layer is ensured, and the gap and high resistance problems caused by different growth rates of the conductive material are solved, and the semiconductor structure is improved Reliability and yield.

CN119028903AActive Publication Date: 2024-11-26CHANGXIN MEMORY TECH INC
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
CN202310562708.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-16
Publication Date
2024-11-26
Estimated Expiration
2043-05-16

AI Technical Summary

Technical Problem

During the semiconductor structure manufacturing process, the quality and performance of the target structure formed by deposition in specific areas or locations fluctuates greatly, affecting the reliability and yield of the semiconductor structure, especially the gaps caused by different growth rates of the conductive material on the sides of the grooves and High resistance problem.

Method used

By forming a seed conductive layer on the side of the groove and in electrical contact with the first conductive layer, the second conductive layer is deposited as a substrate to ensure that the growth rate is consistent, the resistance is reduced, and the resistivity is reduced by doping ion doping.

Benefits of technology

The formation of voids inside the second conductive layer is effectively avoided, the resistance is reduced, and the overall performance and yield of the semiconductor structure are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028903A_ABST
    Figure CN119028903A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to the field of semiconductors, and provides a manufacturing method of a semiconductor structure, and the manufacturing method comprises the steps: providing a substrate, the surface of the substrate is provided with a stacking structure, the stacking structure comprises a first dielectric layer, a first conductive layer and a second dielectric layer which are sequentially stacked, and the stacking structure is internally provided with a plurality of grooves penetrating through the thickness of the stacking structure, the groove extends into the substrate and is used for defining a bit line contact region; a seed conductive layer is formed, and the seed conductive layer at least covers the side face of the groove and is in electric contact with the first conductive layer; and forming a second conductive layer, wherein the second conductive layer covers the seed conductive layer and fills the groove. The probability and resistance of gaps in the second conductive layer can be reduced, and the overall performance of the semiconductor structure is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The disclosed embodiments relate to the field of semiconductor technology, and in particular to a method for manufacturing a semiconductor structure. Background Art

[0002] The manufacturing process of semiconductor structures including integrated circuits involves processes such as photolithography, etching, and thin film deposition. Through the etching process, at least one opening (including trenches, through holes, and contact windows, etc.) can be etched in a specific area or specific location of the semiconductor structure. Combined with the deposition process, a target structure such as gate lines, bit lines, storage cells, and metal interconnect structures can be formed in a specific area or specific location.

[0003] During the manufacturing process of semiconductor structures, when a target structure is deposited in a specific area or position, the quality and performance of the deposited target structure fluctuate greatly, which has a certain impact on the reliability and yield of the semiconductor structure. Summary of the invention

[0004] The embodiments of the present disclosure provide a method for manufacturing a semiconductor structure, which can at least improve the reliability and yield of the semiconductor structure and reduce the resistance of the second conductive layer in the semiconductor structure.

[0005] According to some embodiments of the present disclosure, on the one hand, an embodiment of the present disclosure provides a method for manufacturing a semiconductor structure, including: providing a substrate, the surface of the substrate having a stacking structure, the stacking structure including a first dielectric layer, a first conductive layer, and a second dielectric layer stacked in sequence, the stacking structure having a plurality of grooves running through the thickness of the stacking structure, the grooves extending into the substrate, the grooves being used to define a bit line contact area; forming a seed conductive layer, the seed conductive layer at least covering the sides of the grooves and being in electrical contact with the first conductive layer; forming a second conductive layer, the second conductive layer covering the seed conductive layer and filling the grooves.

[0006] In some embodiments, the seed conductive layer is formed by an atomic layer deposition process.

[0007] In some embodiments, the process parameters of the atomic layer deposition process include a temperature of 400° C. to 480° C.

[0008] In some embodiments, the process parameters of the atomic layer deposition process include a pressure of 0.1 torr to 1.5 torr.

[0009] In some embodiments, the thickness of the seed conductive layer is 1 nm to 3 nm.

[0010] In some embodiments, the material of the seed conductive layer is an intrinsic semiconductor material; after forming the seed conductive layer, the method further includes: introducing a first doping source gas into the groove, wherein the first doping source gas contains a first doping ion for reducing the resistivity of the seed conductive layer.

[0011] In some embodiments, the first doping source gas is introduced for a period of 30 minutes to 90 minutes.

[0012] In some embodiments, the process steps for forming the second conductive layer include: forming an initial second conductive layer using a full-surface deposition process, wherein the initial second conductive layer fills the groove and covers the top surface of the stacked structure; removing the initial second conductive layer on the top surface of the stacked structure to expose the stacked structure, and the remaining initial second conductive layer serves as the second conductive layer.

[0013] In some embodiments, the initial second conductive layer is formed by a chemical vapor deposition process.

[0014] In some embodiments, the material of the seed conductive layer is the same as that of the second conductive layer and both are semiconductor materials; the second conductive layer is formed by a selective epitaxial growth process.

[0015] In some embodiments, the process step of forming the second conductive layer further includes: performing a doping treatment on the second conductive layer to dope second doping ions in the second conductive layer, wherein the second doping ions are used to reduce the resistivity of the second conductive layer.

[0016] In some embodiments, the doping method includes: in the process step of forming the second conductive layer, a second doping source gas is further provided to perform in-situ doping, and the second doping source gas contains the second doping ions.

[0017] In some embodiments, after forming the seed conductive layer and before forming the second conductive layer, it also includes: removing the seed conductive layer on the bottom surface of the groove to expose the bottom surface of the groove, and the second conductive layer contacts the bottom surface of the groove.

[0018] In some embodiments, the material of the seed conductive layer is metal; and the material of the second conductive layer is semiconductor material.

[0019] In some embodiments, after forming the second conductive layer, the method further includes: removing the second dielectric layer; and patterning the first conductive layer to form a plurality of spaced-apart bit lines.

[0020] The technical solution provided by the embodiments of the present disclosure has at least the following advantages: by first forming a seed conductive layer covering the side of the groove and electrically contacting the first conductive layer on the side of the groove defining the bit line contact area, the substrate is made uniform when the second conductive layer is deposited using the side of the groove as a substrate, so that the growth rate of the second conductive layer on the side of the groove remains consistent, avoiding the problem of gaps formed inside the second conductive layer due to inconsistent deposition speeds at different positions of the stacked structure, reducing the resistance of the formed second conductive layer, and improving the overall performance and yield of the second conductive layer and the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] One or more embodiments are exemplarily illustrated by pictures in the corresponding drawings, and these exemplified descriptions do not constitute a limitation on the embodiments. Unless otherwise specified, the pictures in the drawings do not constitute a scale limitation. In order to more clearly illustrate the embodiments of the present disclosure or the technical solutions in the traditional technology, the drawings required for use in the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0022] Figures 1 to 6 A schematic diagram of each step of a method for manufacturing a semiconductor structure provided in an embodiment of the present disclosure. DETAILED DESCRIPTION

[0023] As can be seen from the background art, when a target structure is deposited at a specific location or a specific area of ​​a current semiconductor structure, the quality and yield of the target structure are very unstable, which in turn leads to poor overall performance and yield of the semiconductor structure.

[0024] In the process of manufacturing the bitline contact structure of the semiconductor structure, it is usually necessary to fill the groove that defines the bitline contact structure with conductive material. The side of the groove includes multiple exposed functional layers, and the growth rate of the conductive material on each functional layer is different. Since the bitline contact structure needs to be in direct contact with the substrate, the groove filled with the conductive material extends through the stacked structure into the substrate, that is, the groove has a large depth. Therefore, when the conductive material is filled in the groove, due to the difference in the growth rate of the conductive material on the side of the groove and the large depth of the groove, it is easy for gaps to exist in the prepared bitline contact structure, which in turn causes the resistance of the bitline contact structure in the groove to be too large, affecting the overall performance and yield of the semiconductor structure.

[0025] An embodiment of the present disclosure provides a method for manufacturing a semiconductor structure, wherein a seed conductive layer is formed on the side of the groove, covering the side of the groove and electrically contacting the first conductive layer, so that when the second conductive layer is deposited using the side of the groove as a substrate, the substrate is homogenized, thereby avoiding the problem of gaps formed inside the second conductive layer due to inconsistent deposition speeds at different positions of the stacked structure, reducing the resistance of the formed second conductive layer, and improving the overall performance and yield of the second conductive layer and the semiconductor structure.

[0026] The following will describe the various embodiments of the present disclosure in detail with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the various embodiments of the present disclosure, many technical details are provided in order to enable the reader to better understand the present disclosure. However, even without these technical details and various changes and modifications based on the following embodiments, the technical solutions claimed in the present disclosure can be implemented.

[0027] Figures 1 to 6 A schematic diagram of each step of a method for manufacturing a semiconductor structure provided by the present invention.

[0028] Figure 1 A schematic diagram of the structure of a substrate without a seed conductive layer provided in an embodiment of the present disclosure, Figure 2 A schematic diagram of a substrate structure for completing the preparation of a seed conductive layer provided in an embodiment of the present disclosure, Figure 3 A schematic diagram of another substrate structure for completing the preparation of a seed conductive layer provided in an embodiment of the present disclosure, Figure 4 A schematic diagram of a substrate structure for completing the preparation of a second conductive layer provided in an embodiment of the present disclosure, Figure 5 A schematic diagram of a substrate structure for completing the preparation of an initial second conductive layer provided in an embodiment of the present disclosure, Figure 6 A schematic diagram of a substrate structure for forming an initial bit line contact structure provided in an embodiment of the present disclosure.

[0029] refer to Figure 1 , Figure 2 and Figure 4In some embodiments, a method for manufacturing a semiconductor structure includes: providing a substrate 100, wherein the surface of the substrate 100 has a stacked structure 110, wherein the stacked structure includes a first dielectric layer 111, a first conductive layer 112, and a second dielectric layer 113 stacked in sequence, wherein the stacked structure 110 has a plurality of grooves 120 that penetrate the thickness of the stacked structure, wherein the grooves 120 extend into the substrate 100, and wherein the grooves 120 are used to define a bit line contact region. Forming a seed conductive layer 130, wherein the seed conductive layer 130 at least covers the side of the groove 120 and is in electrical contact with the first conductive layer 112. Forming a second conductive layer 140, wherein the second conductive layer 140 covers the seed conductive layer 130 and fills the groove 120. By forming the seed conductive layer 130 that at least covers the side of the groove 120 and is in electrical contact with the first conductive layer 112 in the groove 120, the growth substrate on the side of the groove 120 is as uniform as possible during the subsequent deposition of the conductive material, and the growth rate of the second conductive layer 140 on the side of the groove 120 is very small or has no difference. This greatly reduces the probability of voids existing inside the grown second conductive layer 140 , thereby reducing the resistance of the second conductive layer 140 and the formed bit line contact structure, and improving the reliability and yield of the formed bit line contact structure and the subsequently prepared semiconductor structure.

[0030] In some embodiments, the material of the substrate 100 may include a semiconductor material, such as but not limited to silicon. In some embodiments, the substrate 100 may include: a basic semiconductor, a compound semiconductor, or an alloy semiconductor. For example, the basic semiconductor includes germanium; the compound semiconductor includes silicon carbide, gallium arsenide, gallium phosphide, indium phosphide, indium arsenide, indium antimonide, and / or III-V semiconductor materials, etc.; the alloy semiconductor includes silicon germanium, silicon germanium carbide, germanium tin, silicon germanium tin, gallium arsenic phosphide, gallium indium phosphide, gallium indium arsenide, indium gallium arsenide phosphide, aluminum indium arsenide, and / or aluminum gallium arsenide, etc. In some embodiments, the substrate 100 may also be a silicon-on-insulator structure, a silicon-germanium-on-insulator structure, a germanium-on-insulator structure, or a combination thereof.

[0031] In addition, the substrate 100 may be doped according to design requirements (e.g., a P-type substrate or an N-type substrate). In some embodiments, the substrate 100 may be doped with P-type doping ions (e.g., boron ions, aluminum ions) or N-type doping ions (e.g., phosphorus ions, arsenic ions). In some embodiments, the first dielectric layer 111 may be a nitride layer.

[0032] In some embodiments, the second dielectric layer 113 may be an oxide layer.

[0033] In some embodiments, the first conductive layer 112 may be a conductive layer of a semiconductor material such as a polycrystalline silicon layer, a single crystal silicon layer or a single crystal germanium layer, or may be a metal conductive layer of a metal material such as gold, silver or copper.

[0034] In some embodiments, the material of the seed conductive layer 130 can be an elemental semiconductor material with good conductivity, such as germanium, silicon, selenium, boron or antimony, or a compound semiconductor material, such as gallium arsenide, indium phosphide, indium antimonide, silicon carbide or cadmium sulfide.

[0035] The seed conductive layer 130 at least covers the side of the groove 120 and is in contact with the first conductive layer 112. That is, the seed conductive layer 130 covering the side of the groove 120 extends from the bottom of the groove 120 in a direction away from the substrate 100. The top surface of the seed conductive layer 130 can be located at any position between the first surface and the second surface, wherein the first surface is the surface of the first conductive layer 112 in contact with the first dielectric layer 111, and the second surface is the surface of the second dielectric layer 113 away from the first conductive layer 112. For example, the seed conductive layer 130 extends from the bottom of the groove 120 to the position of the surface of the second dielectric layer 113 in contact with the first conductive layer 112, the position of the surface of the second dielectric layer 113 away from the first conductive layer 112, or the position of the surface of the first conductive layer 112 in contact with the first dielectric layer 111. In some embodiments, the seed conductive layer 130 can also completely cover the side of the groove 120 and extend to the outside of the groove 120, covering the surface of the second dielectric layer 113 away from the first conductive layer 112.

[0036] In addition, reference Figure 3 The seed conductive layer 130 may not only cover the side surface of the groove 120 , but also cover the bottom surface of the groove 120 and the top surface of the stacked structure constituting the groove 120 .

[0037] In some embodiments, the seed conductive layer 130 is formed by an atomic layer deposition process. The main function of the seed conductive layer 130 is to serve as a substrate on the side of the groove 120 when the conductive layer is grown in the groove 120, so that the growth rate of the conductive layer in the groove 120 is as consistent as possible. Therefore, the thickness of the seed conductive layer 130 formed does not need to be too large, and it is sufficient to ensure that the seed conductive layer 130 can cover the side of the groove 120 as evenly as possible. In the process of forming the seed conductive layer 130, an atomic layer deposition process can be used to deposit the material constituting the seed conductive layer 130 in the groove 120 layer by layer in the form of a single atomic film on the side of the groove 120, thereby forming a seed conductive layer 130 in the groove 120 that uniformly covers the side of the groove 120 and has a small thickness, thereby improving the uniformity and morphology of the seed conductive layer 130, thereby avoiding the quality of the conductive layer formed subsequently being affected by the different thicknesses of the seed conductive layer 130 in different areas on the side of the groove 120, and further improving the overall performance of the prepared conductive layer.

[0038] In some embodiments, the process parameters of the atomic layer deposition process include a temperature of 400°C to 480°C. During the deposition of the seed conductive layer 130, if the temperature during the deposition process is too high, the precursor used during the deposition is prone to cause a parasitic chemical vapor deposition reaction due to the high temperature or even exceeding the decomposition temperature of the precursor, and may also cause the film layer of the deposited seed conductive layer 130 to fall off from the side of the groove 120. If the temperature during the deposition process is too low, it may not provide enough energy for the reaction during the deposition process. At the same time, the precursor selected during the deposition process is prone to accumulate on the surface of the side wall of the groove 120 due to condensation, and a uniform seed conductive layer 130 cannot be formed, and the morphology of the side of the groove 120 is destroyed.

[0039] Therefore, in the process of forming the seed conductive layer 130 by the atomic layer deposition process, the temperature in the process parameters can be set within the range of 400° C. to 480° C., for example, the temperature in the deposition process can be set to 405° C., 410° C., 420° C., 425° C., 440° C., 450° C., 465° C. or 475° C., etc. By setting the temperature in the atomic layer deposition process to a suitable value, the parasitic chemical vapor deposition reaction can be avoided, and the uniformity and morphology of the formed seed conductive layer 130 can be improved, the stability of the seed conductive layer 130 combined with the side of the groove 120 can be improved, and the probability of the seed conductive layer 130 falling off can be reduced.

[0040] It should be noted that when the material of the seed conductive layer 130 is metal, the precursor in the atomic layer deposition process can be titanium tetrachloride, tungsten boride or an organic metal compound; when the material of the seed conductive layer 130 is a semiconductor material, the precursor in the atomic layer deposition process can be silane, disilane or dichlorodisilane.

[0041] In some embodiments, the process parameters of the atomic layer deposition process include a pressure of 0.1 torr to 1.5 torr. In the process of forming the seed conductive layer 130 by the atomic layer deposition process, if the pressure during the deposition process is too high, the precursor used in the deposition process cannot be diffused in a timely and uniform manner, resulting in poor uniformity and morphology of the seed conductive layer 130 covering the side of the groove 120 during the deposition process; if the pressure during the deposition process is too low, the deposition speed of the seed conductive layer 130, which is mainly deposited by adsorption, is slow during the deposition process, and the seed conductive layer 130 cannot be efficiently formed.

[0042] Therefore, in the process of forming the seed conductive layer 130 by the atomic layer deposition process, the pressure of the deposition process can be set in the range of 0.1 torr to 1.5 torr, for example, the pressure of the deposition process can be set in 0.15 torr, 0.2 torr, 0.25 torr, 0.35 torr, 0.5 torr, 0.75 torr, 0.9 torr, 1 torr, 1.15 torr, 1.25 torr, 1.35 torr or 1.45 torr, etc. By setting the pressure in the atomic layer deposition process in a suitable range, a seed conductive layer 130 with good uniformity and morphology is formed on the side of the groove 120, and the formation efficiency of the seed conductive layer 130 is ensured, and the time required for the semiconductor structure manufacturing is shortened as much as possible.

[0043] In some embodiments, the seed conductive layer 130 may be formed by a chemical vapor deposition process.

[0044] In some embodiments, the thickness of the seed conductive layer 130 is 1 nm to 3 nm. The thickness of the seed conductive layer 130 refers to the interval d between the surface of the seed conductive layer 130 in contact with the groove 120 and the surface of the seed conductive layer 130 away from the groove 120 in the direction perpendicular to the side of the groove 120. The main function of the seed conductive layer 130 is to serve as a uniform matrix in the deposition process of the conductive material, and it is difficult to achieve high-concentration doping of doped ions due to its thin thickness. In the case where the thickness of the seed conductive layer 130 is too large, the volume of the seed conductive layer 130 is also correspondingly large. After the conductive material deposition and subsequent processes are completed, the volume of the seed conductive layer 130 is large and it is difficult to achieve high-concentration doping, which will lead to a low overall doping concentration and high resistance of the formed bit line contact structure. In the case where the thickness of the seed conductive layer 130 is too small, the bonding strength between the seed conductive layer 130 and the side of the groove 120 is low, and the seed conductive layer 130 is prone to fall off during the deposition of the conductive material, which will lead to an increase in resistance of the conductive layer and the formed semiconductor structure and a decrease in yield.

[0045] Therefore, when forming the seed conductive layer 130, the thickness of the formed seed conductive layer 130 can be controlled within the range of 1 nm to 3 nm, for example, a seed conductive layer 130 with a thickness of 1.2 nm, 1.25 nm, 1.5 nm, 1.75 nm, 2 nm, 2.25 nm, 2.5 nm or 2.8 nm can be formed. By forming a seed conductive layer 130 with an appropriate thickness, the volume proportion of the seed conductive layer 130 in the semiconductor structure is reduced, the overall doping concentration of doped ions in the subsequently formed bit line contact structure is increased, the probability of the seed conductive layer 130 falling off is reduced, and the yield of the semiconductor structure is improved.

[0046] In some embodiments, the material of the seed conductive layer 130 is an intrinsic semiconductor material; after forming the seed conductive layer 130, the method further includes: introducing a first doping source gas into the groove 120, wherein the first doping source gas contains first doping ions for reducing the resistivity of the seed conductive layer 130. The seed conductive layer 130 is located inside the word line contact structure finally formed and is in electrical contact with the first conductive layer 112. When the material of the seed conductive layer 130 is an intrinsic semiconductor material, the resistance of the seed conductive layer 130 itself is relatively large, which will cause the overall resistance of the word line contact structure of the semiconductor structure formed by subsequent processes to be relatively large, thereby affecting the performance of the semiconductor structure.

[0047] After the seed conductive layer 130 is formed, a first doping source gas is introduced into the groove 120 at least one side of which is covered by the seed conductive layer 130. The first doping ions contained in the first doping source gas diffuse into the seed conductive layer 130, thereby doping the first doping ions that are beneficial to reducing the resistivity of the seed conductive layer 130 into the seed conductive layer 130, thereby reducing the resistance of the seed conductive layer 130. By introducing the first doping source gas into the groove 120 where the seed conductive layer 130 has been formed, the first doping source ions are doped into the seed conductive layer 130, thereby effectively reducing the resistance of the seed conductive layer 130 composed of an intrinsic semiconductor material, thereby improving the performance of the word line contact structure and the semiconductor structure finally formed.

[0048] In some embodiments, the method of introducing the first doping source gas into the groove 120 can be to continuously introduce the first doping source gas into the groove 120 at a preset flow rate, and by continuously providing a large amount of first doping source ions, the speed of doping the first doping ions into the seed conductive layer 130 and the doping concentration in the seed conductive layer 130 after doping are increased as much as possible, thereby reducing the resistance of the seed conductive layer 130 as much as possible.

[0049] In some embodiments, the method of introducing the first doping source gas into the groove 120 can be to intermittently introduce the first doping source gas into the groove 120 according to a preset period. By periodically introducing the first doping source gas, the total amount of the first doping gas required to dope the first doping ions into the seed conductive layer 130 is reduced, thereby reducing the cost of doping the seed conductive layer 130 with the first doping ions, thereby effectively controlling the preparation cost of the bit line contact structure and the semiconductor structure.

[0050] In some embodiments, the first doping source gas may be introduced into the groove 120 intermittently at random time intervals or gradually varying time intervals.

[0051] In some embodiments, the time for introducing the first doping source gas into the groove 120 is 30 minutes to 90 minutes. When other external conditions, such as the concentration of the first doping source gas, the pressure and temperature in the groove 120, are consistent when introducing the first doping source gas into the groove 120, the time for introducing the first doping source gas into the groove 120 will affect the doping effect of the first doping ions in the seed conductive layer 130. When the time for introducing the first doping source gas is too short, the total amount of the first doping ions provided is small, and the diffusion time of the first doping ions is short, and the concentration and uniformity of the first doping ions in the seed conductive layer 130 are poor. When the time for introducing the first doping source gas is too long, the total amount of the first doping ions provided is too large. Since the upper limit of the doping concentration of the first doping ions in the seed conductive layer 130 is low, there are too many useless first doping ions, and the doping cost of the seed conductive layer 130 is too high.

[0052] Therefore, when the first doping source gas is introduced into the groove 120, the time for introducing the first doping source gas can be controlled within the range of 30 minutes to 90 minutes, for example, the time for introducing the first doping source gas is set to 35 minutes, 40 minutes, 45 minutes, 50 minutes, 60 minutes, 65 minutes, 75 minutes or 85 minutes, etc. The time for introducing the first doping source gas is controlled within a suitable range, and a certain concentration of the first doping source ions is uniformly doped in the seed conductive layer 130 to effectively reduce the resistance of the seed conductive layer 130, while reducing the doping cost of the seed conductive layer 130.

[0053] The duration of introducing the first doping source gas into the groove 120 refers to the time interval between the moment when the first doping source gas starts to be introduced into the groove 120 and the moment when the seed conductive layer 130 is doped with the first doping source ions. When the first doping source gas is introduced continuously, it is the duration between the beginning of the introduction of the first doping source gas and the stopping of the introduction of the first doping source gas. When the first doping source gas is introduced intermittently, it is the duration between the first beginning of the introduction of the first doping source gas and the last stopping of the introduction of the first doping source gas.

[0054] In some embodiments, the first doping ions may be P-type doping ions, such as boron, indium or gallium, or may be N-type doping ions, such as phosphorus or antimony. Depending on the type of the substrate 100, P-type doping ions or N-type doping ions are selectively used as the first doping ions to ensure that the semiconductor structure has normal working performance.

[0055] In some embodiments, the intrinsic semiconductor material of the seed conductive layer 130 may be one or a combination of polycrystalline silicon, single crystal silicon, single crystal germanium, or gallium arsenide.

[0056] refer to Figure 1 , Figure 4 and Figure 5 In some embodiments, the process steps for forming the second conductive layer 140 include: forming an initial second conductive layer 150 by a whole-surface deposition process, wherein the initial second conductive layer 150 fills the groove 120 and covers the top surface of the stacked structure; removing the initial second conductive layer 150 on the top surface of the stacked structure to expose the stacked structure, and the remaining initial second conductive layer 150 is used as the second conductive layer 140. When the second conductive layer 140 is formed by a whole-surface deposition process, the initial second conductive layer 150 that fills the groove 120 and covers the top surface of the stacked structure can be efficiently formed, thereby improving the formation efficiency of the second conductive layer 140. After the initial second conductive layer 150 is formed, the portion of the initial second conductive layer 150 that is above the top surface of the stacked structure is removed by an etch-back process until the stacked structure covered by the initial second conductive layer 150 is exposed. The second conductive layer 140 is accurately formed by the etch-back method, which is convenient for subsequent process steps and improves the manufacturing efficiency of the semiconductor structure.

[0057] In some embodiments, the process steps of forming the initial second conductive layer 150 include: using a chemical vapor deposition process to form the initial second conductive layer 150. The initial second conductive layer 150 is used to subsequently form the second conductive layer 140 for constructing the bit line contact structure. The chemical vapor deposition process can form the initial second conductive layer 150 as efficiently as possible, thereby reducing the time required to form the second conductive layer 140 and the bit line contact structure, and improving the production efficiency of the semiconductor structure.

[0058] In some embodiments, the material of the seed conductive layer 130 is metal; the material of the second conductive layer 140 is semiconductor material. The seed conductive layer 130, as the substrate for the growth of the second conductive layer 140, needs to be in electrical contact with the second conductive layer 140 and the first conductive layer 112 respectively. As part of the bit line contact structure, it needs to have good conductivity. Since the seed conductive layer 130 is thin and difficult to be doped, the seed conductive layer 130 can be directly formed by metal material, and then the second conductive layer 140 can be formed by semiconductor material. The seed conductive layer 130 is formed by metal material, and the second conductive layer 140 is formed by semiconductor material, while the probability of generating voids in the second conductive layer 140 is reduced, and the conductivity of the seed conductive layer 130 is increased as much as possible, thereby reducing the resistance of the bit line contact structure and improving the overall performance of the semiconductor structure.

[0059] In some embodiments, the material of the seed conductive layer 130 can be a material composed of a single metal element, such as copper, silver, aluminum or gold, or an alloy composed of multiple metal elements, such as copper-aluminum alloy, copper-silver alloy, copper-tin alloy, etc.

[0060] In some embodiments, the materials of the seed conductive layer 130 and the second conductive layer 140 can be elemental semiconductors such as polycrystalline silicon, single crystal silicon, germanium, selenium, boron or antimony, or can be compound semiconductor materials, for example, gallium arsenide, indium phosphide, indium antimonide, silicon carbide or cadmium sulfide.

[0061] In some embodiments, the material of the seed conductive layer 130 is the same as that of the second conductive layer 140 and both are semiconductor materials, and a selective epitaxial growth process is used to form the second conductive layer 140. Forming the second conductive layer 140 using a selective epitaxial growth process can improve the uniformity and morphology of the grown second conductive layer 140, improve the yield of the second conductive layer 140, and reduce the resistance of the second conductive layer 140.

[0062] In some embodiments, the process step of forming the second conductive layer 140 further includes: performing a doping treatment on the second conductive layer 140 to dope the second doping ions in the second conductive layer 140, and the second doping ions are used to reduce the resistance of the second conductive layer. The second conductive layer 140 is used to construct a bit line contact structure, and therefore needs to have good conductivity. In the case where the material of the second conductive layer 140 is a semiconductor material, the resistance of the second conductive layer 140 is relatively large. When the second conductive layer 140 is formed by a whole-surface deposition process combined with a selective removal process or by a selective epitaxial growth process, by doping the second conductive layer 140 with second doping ions that are beneficial to reducing the resistivity of the second conductive layer 140, the conductivity of the formed second conductive layer 140 can be effectively improved, the overall resistance of the second conductive layer 140 and the formed bit line contact structure can be reduced, and the bit line contact structure and performance can be improved.

[0063] In some embodiments, the method of doping treatment includes: in the process step of forming the second conductive layer 140, a second doping source gas is also provided for in-situ doping, and the second doping source gas contains second doping ions. When the second conductive layer 140 is doped, the second doping source gas is directly provided synchronously during the process of growing the second conductive layer 140, and the growing second conductive layer 140 is in-situ doped, so that the second doping ions in the second doping source gas can be uniformly doped into the second conductive layer 140, thereby improving the doping uniformity of the second doping ions in the second conductive layer 140 and reducing the resistivity of the second conductive layer 140 as much as possible. At the same time, the in-situ doping method can also reduce the process steps and manufacturing time of forming the second conductive layer 140, and reduce the manufacturing time of the bit line contact structure.

[0064] In some embodiments, the doping treatment method can also be to inject second doping ions into the second conductive layer 140 by ion implantation to reduce the resistivity of the second conductive layer 140 after forming the second conductive layer 140 by a deposition process. The use of ion implantation is beneficial to reducing the process requirements and difficulty in the formation of the second conductive layer 140.

[0065] In some embodiments, the second doping ion may be a P-type doping ion, such as boron, indium or gallium, or an N-type doping ion, such as phosphorus or antimony. In addition, the first doping ion and the second doping ion may be the same doping ion or different doping ions.

[0066] In some embodiments, after forming the seed conductive layer 130 and before forming the second conductive layer 140, the process further includes: removing the seed conductive layer 130 located on the bottom surface of the groove 120 to expose the bottom surface of the groove 120, and the second conductive layer 140 is in contact with the bottom surface of the groove 120. When the seed conductive layer 130 is formed by a deposition process, a layer of seed conductive layer 130 covering the bottom surface is generally formed on the bottom surface of the groove 120. In the case where the material of the seed conductive layer 130 is a semiconductor material, the resistance of the seed conductive layer 130 on the bottom surface of the groove 120 is relatively large, which will cause the contact resistance between the formed bit line contact structure and the substrate 100 to be too large. Therefore, after forming the seed conductive layer 130 and before forming the second conductive layer 140, the seed conductive layer 130 located on the bottom surface of the groove 120 is removed to expose the bottom surface of the groove 120, and then the second conductive layer 140 is formed in the groove 120 so that the second conductive layer 140 is directly in contact with the substrate 100 at the bottom surface of the groove 120. By removing the seed conductive layer 130 on the bottom surface of the groove 120 and forming a second conductive layer 140 directly contacting the substrate 100 at the bottom surface of the groove 120, the bit line contact structure is in contact with the substrate 100 through the second conductive layer 140, thereby reducing the contact resistance between the bit line contact structure and the substrate 100 and improving the overall performance of the semiconductor structure.

[0067] In addition, since the thickness of the seed conductive layer 130 is relatively small, it is also difficult to achieve high-concentration doping of the seed conductive layer 130 on the bottom surface of the groove 120. After the seed conductive layer 130 on the bottom surface of the groove 120 is removed, the bit line contact structure will contact the substrate 100 through the second conductive layer 140. After the second conductive layer 140 is doped with the second doping ion by in-situ doping or ion implantation, the doping concentration of the second doping ion in the second conductive layer 140 is much greater than the doping concentration of the first doping ion in the seed conductive layer 130, and the resistivity of the second conductive layer 140 is also lower than the resistivity of the seed conductive layer 130, thereby further reducing the contact resistance between the bit line contact structure and the substrate 100.

[0068] In addition, during the doping process of the second conductive layer 140, the interface where the second conductive layer 140 contacts the substrate 100 will repel the second doping ions, thereby ensuring that the second doping ions remain in the second conductive layer 140 as much as possible, and while increasing the doping concentration of the second conductive layer 140, the damage to the substrate 100 caused by the diffusion of the second doping ions into the substrate 100 is reduced. For example, when the material of the second conductive layer 140 is polycrystalline silicon, the material of the substrate 100 is single crystal silicon, and the second doping ions are phosphorus ions, when phosphorus ions are provided in the second conductive layer 140, the polycrystalline silicon-single crystal silicon interface where the second conductive layer 140 contacts the substrate 100 will repel the phosphorus ions, and the provided phosphorus ions will remain in the second conductive layer 140 as much as possible.

[0069] refer to Figure 1 and Figure 6 In some embodiments, after forming the second conductive layer 140, the process further includes: removing the second dielectric layer 113; and patterning the first conductive layer 112 to form a plurality of spaced-apart bit lines. After the second conductive layer 140 is prepared, the second dielectric layer 113 is removed to obtain an initial bit line contact structure formed by the first conductive layer 112, the seed conductive layer 130, and the second conductive layer 140 that are in electrical contact with each other. The first conductive layer 112 is then patterned to form a bit line contact structure corresponding to a plurality of spaced-apart bit lines, and then a plurality of spaced-apart bit lines are formed in combination with subsequent processes. After removing the second dielectric layer 113, the first conductive layer 112 is patterned to form a plurality of bit lines.

[0070] In the embodiment of the present disclosure, a seed conductive layer 130 is first formed on the side of the groove 120 defining the bit line contact area, covering the side of the groove 120 and electrically contacting the first conductive layer 112. This allows the side of the groove 120 to be used as a substrate for depositing the second conductive layer 140, thereby achieving uniform substrate. This allows the growth rate of the second conductive layer 140 on the side of the groove 120 to remain consistent, thereby avoiding the problem of voids being formed inside the second conductive layer 140 due to inconsistent deposition rates at different positions of the stacked structure, reducing the resistance of the formed second conductive layer 140, and improving the overall performance and yield of the second conductive layer 140 and the semiconductor structure.

[0071] Those skilled in the art can understand that the above-mentioned embodiments are specific examples for implementing the present disclosure, and in practical applications, various changes can be made to them in form and detail without departing from the spirit and scope of the embodiments of the present disclosure. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the embodiments of the present disclosure, so the protection scope of the embodiments of the present disclosure shall be based on the scope defined in the claims.

Claims

1. A method for manufacturing a semiconductor structure, characterized in that: include: A substrate is provided, wherein the surface of the substrate has a stacked structure, wherein the stacked structure comprises a first dielectric layer, a first conductive layer, and a second dielectric layer stacked in sequence, and wherein the stacked structure has a plurality of grooves penetrating the thickness of the stacked structure. The groove extends into the substrate, and the groove is used to define a bit line contact area; forming a seed conductive layer, wherein the seed conductive layer at least covers a side surface of the groove and is in electrical contact with the first conductive layer; A second conductive layer is formed, where the second conductive layer covers the seed conductive layer and fills the groove.

2. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The seed conductive layer is formed by an atomic layer deposition process, wherein process parameters of the atomic layer deposition process include a temperature of 400° C. to 480° C. and a pressure of 0.1 torr to 1.5 torr.

3. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The thickness of the seed conductive layer is 1 nm to 3 nm.

4. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The material of the seed conductive layer is an intrinsic semiconductor material; After forming the seed conductive layer, the method further comprises: A first doping source gas is introduced into the groove, wherein the first doping source gas contains first doping ions for reducing the resistivity of the seed conductive layer.

5. The method for manufacturing a semiconductor structure according to claim 4, characterized in that: The time length for introducing the first doping source gas is 30 minutes to 90 minutes.

6. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The process steps of forming the second conductive layer include: Forming an initial second conductive layer by a chemical vapor deposition process, wherein the initial second conductive layer fills the groove and covers the top surface of the stacked structure; The initial second conductive layer on the top surface of the stacked structure is removed to expose the stacked structure, and the remaining initial second conductive layer serves as the second conductive layer.

7. The method for manufacturing a semiconductor structure according to claim 6, characterized in that: The process step of forming the second conductive layer also includes: The second conductive layer is doped to dope second doping ions in the second conductive layer, where the second doping ions are used to reduce the resistivity of the second conductive layer.

8. The method for manufacturing a semiconductor structure according to claim 7, characterized in that: The doping treatment method comprises: in the process step of forming the second conductive layer, a second doping source gas is further provided to perform in-situ doping, and the second doping source gas contains the second doping ions.

9. The method for manufacturing a semiconductor structure according to claim 7, characterized in that: After forming the seed conductive layer and before forming the second conductive layer, the method further includes: The seed conductive layer on the bottom surface of the groove is removed to expose the bottom surface of the groove, and the second conductive layer is in contact with the bottom surface of the groove.

10. The method for manufacturing a semiconductor structure according to claim 1, characterized in that: The material of the seed conductive layer is metal; the material of the second conductive layer is semiconductor material.

Citation Information

Patent Citations

  • Semiconductor memory and preparation method thereof

    CN112563208A

  • Manufacturing method of semiconductor structure and semiconductor structure

    CN113690188A

  • Semiconductor structure and manufacturing method thereof

    CN115050647A

  • Semiconductor structure and preparation method of semiconductor structure

    CN115568207A

  • Semiconductor structure and preparation method thereof

    CN115884589A