The step height and flatness of the shallow trench isolation structure and gate oxide layer are controlled through the photolithography process, which solves the damage and electrical properties of the semiconductor silicon surface by RCA wet cleaning, and achieves better structural flatness and electrical properties Performance.
Patent Information
- Application Number
- CN202310728994.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-24
- Filing Date
- 2023-06-19
- Publication Date
- 2024-11-26
AI Technical Summary
In the existing semiconductor manufacturing process, RCA wet cleaning can easily damage the boundaries of shallow trench isolation structures, resulting in mismatch problems in conduction currents during electrical performance tests. At the same time, insufficient cleaning leads to poor flatness and abnormal gate oxide layer thickness.
The photolithography process is used to control the order height and flatness of the shallow trench isolation structure and gate oxide layer in the high-voltage component area. The unnecessary layers are removed through multiple photoresist etching processes to ensure the shallow trench isolation structure. Flush with the top surface of the gate oxide layer, reducing RCA cleaning time to avoid damage to the silicon surface.
It effectively avoids the problem of on-current mismatch, and maintains good structural flatness and high order, reduces damage to the silicon surface by RCA cleaning, and improves the electrical performance of semiconductor components.
Smart Images

Figure CN119028976A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a semiconductor manufacturing process, and more specifically, to a method for manufacturing a semiconductor structure with a flush shallow trench isolation structure and a gate oxide layer. Background Art
[0002] With the advancement of semiconductor manufacturing process technology, the size of semiconductor components is getting smaller and smaller, and there are more precise requirements for the manufacturing process technology of high voltage complementary metal oxide semiconductor (HVCMOS) components. Under the design of small line width and high integration, the interference between components is becoming more and more obvious, so the shallow trench isolation (STI) structure used for isolation between components and related manufacturing processes have become more and more important. In addition, the high-voltage component area usually has a thicker gate oxide layer, which will cause the step height of the high-voltage component area to be higher than the step height of the lower voltage component area, causing problems for the manufacturing process. Therefore, the step height control of the shallow trench isolation structure in the high-voltage component area and the adjacent active area is very important in the semiconductor manufacturing process.
[0003] There are some common methods in the prior art to achieve the purpose of step height and flatness control, such as using chemical mechanical polishing (CMP), etching or cleaning processes, and RCA wet cleaning process is one of them. However, although the RCA wet cleaning process can achieve the purpose of step height control, excessive RCA cleaning can easily damage the silicon surface at the boundary of the shallow trench isolation structure, causing on-current mismatch (I on On the other hand, insufficient RCA cleaning will lead to poor flatness, which may cause the gate formed on the shallow trench isolation structure and the gate oxide layer to be disconnected or the thickness of the gate oxide layer to be abnormal. Therefore, the relevant manufacturing process of this part must balance between step height control and electrical performance. Based on the above situation, technical personnel in this field need to improve the existing manufacturing process practices in order to achieve better results in terms of both flatness and electrical properties of the device structure. Summary of the invention
[0004] In view of the problems encountered in the above-mentioned existing practices, the present invention proposes a novel semiconductor manufacturing process, which is characterized in that the step height and topography of the shallow trench isolation structure and the gate oxide layer on the high-voltage component area are controlled by a photolithography manufacturing process that removes the gate oxide layer on the low-voltage component area after RCA wet cleaning, thereby avoiding excessive RCA wet cleaning to damage the silicon surface at the boundary of the shallow trench isolation structure, causing the on-current mismatch problem in subsequent electrical testing, while maintaining good structural flatness and step height.
[0005] One aspect of the present invention is to provide a method for manufacturing a semiconductor structure with a flush shallow trench isolation structure and a gate oxide layer, the steps of which include providing a substrate, on which a shallow trench isolation structure protrudes from the substrate and a pad oxide layer covers the substrate; forming a first photoresist on a drain region on one side of the shallow trench isolation structure, the first photoresist covering a portion of the top surface of the shallow trench isolation structure from the side; performing a first etching process using the first photoresist as a mask to remove the pad oxide layer on the other side of the shallow trench isolation structure and to make the substrate concave, the first etching process also forming a concave portion not covered by the first photoresist and a convex portion covered by the first photoresist (108) on the shallow trench isolation structure; removing the first photoresist; forming a gate oxide layer on the concave substrate, the gate oxide layer adjacent to the shallow trench isolation structure; The invention relates to a method for manufacturing a first electrode layer of the shallow trench isolation structure and a second etching process. The method comprises the following steps: forming a second photoresist on the gate oxide layer, wherein the second photoresist covers almost all of the shallow trench isolation structure, and only the edge of the convex portion on the side is not covered; performing a second etching process using the second photoresist as a mask to remove the convex portion and the pad oxide layer on the drain region; removing the second photoresist; forming a first oxide layer on the drain region; forming a third photoresist on the gate oxide layer, wherein the third photoresist only covers the edge of the shallow trench isolation structure on the other side, and the shallow trench isolation structure area covered by the third photoresist does not overlap with the shallow trench isolation structure area covered by the first photoresist; and performing a third etching process using the third photoresist as a mask to remove part of the shallow trench isolation structure and the entire first oxide layer, so that the top surface of the shallow trench isolation structure is flush with the gate oxide layer.
[0006] Another aspect of the present invention is to provide a semiconductor structure with a flush shallow trench isolation structure and a gate oxide layer, the structure comprising a substrate having a well region, a source region located on one side of the well region and a drift region located on the other side of the well region; a shallow trench isolation structure is located in the drift region, the outer side of the shallow trench isolation structure has a convex portion and a first bird's beak structure, the first bird's beak structure is connected to the convex portion; a gate oxide layer is located on the well region and the source region and is connected to the shallow trench isolation structure, and the shallow trench isolation structure is flush with the top surface of the gate oxide layer, the outer side of the gate oxide layer has a second bird's beak structure located on the source region; and a gate is located on the gate oxide layer and part of the shallow trench isolation structure.
[0007] These and other objects of the present invention will become more apparent to the reader after reading the following detailed description of the preferred embodiment which is described in various figures and drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] Figures 1 to 11 A cross-sectional schematic diagram of a manufacturing process of a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer in a preferred embodiment of the present invention;
[0009] Fig.12 It is a schematic plan view of a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer in a preferred embodiment of the present invention.
[0010] Please note that all illustrations in this manual are of a legend nature. For the sake of clarity and convenience of illustration, the components in the illustrations may be exaggerated or reduced in size and proportion. Generally speaking, the same reference symbols in the figures will be used to indicate corresponding or similar component features after modification or in different embodiments.
[0011] Explanation of symbols
[0012] 100 Base
[0013] 100a Well region
[0014] 100b Drift Zone
[0015] 100c Source region
[0016] 100d Base region
[0017] 102 Shallow Trench Isolation Structure
[0018] 102a recess
[0019] 102b convex part
[0020] 102c Bird beak structure
[0021] 103 Shallow Trench Isolation Structure
[0022] 104 Pad oxide layer
[0023] 106 hard mask layer
[0024] 108 first photoresist
[0025] 110 Drain region
[0026] 112 Gate Oxide
[0027] 112c Bird beak structure
[0028] 114 First Oxide Layer
[0029] 116 second photoresist
[0030] 118 Second Oxide Layer
[0031] 120 third photoresist
[0032] 122 Gate
[0033] 124 Drain
[0034] 126 Source
[0035] E1 First Etching Process
[0036] E2 Second Etching Process
[0037] E3 Third Etching Process
[0038] R Depression
[0039] R1 Range
[0040] R2 Range
[0041] R3 Range DETAILED DESCRIPTION
[0042] Now, the exemplary embodiments of the present invention will be described in detail below, and the features described will be shown with reference to the accompanying drawings so that the reader can understand and achieve the technical effects. The reader will understand that the description in the text is only by way of example and is not intended to limit the present invention. The various embodiments of the present invention and the various features that do not conflict with each other in the embodiments can be combined or reset in various ways. Without departing from the spirit and scope of the present invention, modifications, equivalents or improvements to the present invention are understandable to those skilled in the art and are intended to be included in the scope of the present invention.
[0043] The reader should be able to easily understand that the meanings of "on", "above", and "over" in this case should be interpreted in a broad sense, such that "on" not only means "directly on" something, but also includes the meaning of being on something with intervening features or layers therebetween, and "above" or "over" not only means "above" or "over" something, but can also include the meaning of being "above" or "over" something with no intervening features or layers therebetween (i.e., directly on something). In addition, spatial-related terms such as "under", "below", "lower", "over", "upper", etc. may be used herein for convenience of description to describe the relationship of one element or feature to another or more elements or features, as shown in the accompanying drawings.
[0044] As used herein, the term "substrate" refers to a material onto which subsequent materials are added. The substrate itself may be patterned. The material added on top of the substrate may be patterned or may remain unpatterned. In addition, the substrate may include a wide range of semiconductor materials such as silicon, germanium, gallium arsenide, indium phosphide, etc. Alternatively, the substrate may be made of a non-conductive material such as glass, plastic, or a sapphire wafer.
[0045] As used herein, the term "layer" refers to a portion of a material that includes a region having a thickness. The layer may extend over the entirety of a structure below or above, or may have a scope less than the scope of the structure below or above. In addition, the layer may be a region of a homogeneous or heterogeneous continuous structure having a thickness less than the thickness of the continuous structure. For example, the layer may be located between the top and bottom surfaces of the continuous structure or between any horizontal planes at the top and bottom surfaces. The layer may extend horizontally, vertically, and / or along an inclined surface. The substrate may be a layer, which may include one or more layers, and / or may have one or more layers on, above, and / or below it. The layer may include multiple layers. For example, an interconnect layer may include one or more conductors and contact layers (wherein contacts, interconnect lines, and / or vias are formed) and one or more dielectric layers.
[0046] The reader can generally understand the terms at least partially from their usage in context. For example, at least partially depending on the context, the term "one or more" as used herein may be used to describe any feature, structure, or property in a singular sense, or may be used to describe a combination of features, structures, or properties in a plural sense. Similarly, at least partially depending on the context, terms such as "a", "an", "the", or "said" may likewise be understood to convey a singular usage or a plural usage. Additionally, the term "based on" may be understood to not necessarily aim to convey an exclusive set of factors, but may allow for the existence of additional factors that are not necessarily explicitly described, which also at least partially depends on the context.
[0047] The reader can further understand that when the words "include" and / or "contain" are used in this specification, they specify the existence of the stated features, regions, wholes, steps, operations, elements and / or parts, but do not exclude the possibility of the existence or addition of one or more other features, regions, wholes, steps, operations, elements, parts and / or their combinations.
[0048] Now the following will refer to Figures 1 to 11 The following is a flow chart of the manufacturing process of a semiconductor structure having a flush shallow trench isolation (STI) and a gate oxide layer according to an embodiment of the present invention. The figure uses a cross-sectional view to illustrate the relative positions and connection relationships of various components in the vertical direction during the manufacturing process. Fig.12 The plan view of the invention is used to understand the coverage and overlap of these features. The method of the invention is generally applied to the manufacture of high voltage complementary metal oxide semiconductor (HV CMOS) devices, and the cross section shown in the figure is also a high voltage device area. However, other semiconductor structures with shallow trench isolation structures and gate oxide layer step height and flatness requirements can also be applied to the invention, and are not limited thereto.
[0049] Please refer to Figure 1. At the beginning of the manufacturing process, a semiconductor substrate 100 is provided as the setting foundation of the semiconductor element of the present invention. The material of the substrate 100 is preferably a silicon substrate, such as a P-type doped silicon substrate, but other silicon-containing substrates may also be used, including III-V silicon-coated substrates (such as GaN-on-silicon) or silicon-coated insulator (silicon-on-insulator, SOI) substrates, etc., or other doping types of substrates, but are not limited to this. The substrate 100 includes a well region 100a covering the entire semiconductor structure, such as a P-type doped well region (p-well). Through the ion implantation process, the substrate surface is formed with a base region (body) 100d, a source region 100c, a P-type well region 100a and a drift region (drift) 100b, which are adjacent to each other in sequence. The source region 100c and the drift region 100b are separated by the P-type well region 100a. The base region 100d is adjacent to the source region 100c. The drift region 100b can be an N-type doped well region (n-well), the source region 100c can be an N-type heavily doped (N+) region, and the base region 100d can be a P-type heavily doped (P+) region. In the embodiment of the present invention, two shallow trench isolation structures 102 and 103 are respectively formed in the drift region 100b and the base region 100d of the substrate 100 and protrude from the surface of the substrate 100, and the material thereof can be silicon oxide. In addition to the shallow trench isolation structures 102 and 103, a pad oxide layer 104 is formed on the surface of the substrate 100 around the shallow trench isolation structures 102 and 103, and a conformal hard mask layer 106 is also formed on the pad oxide layer 104 and the surface of the shallow trench isolation structure 102. The materials of the pad oxide layer 104 and the hard mask layer 106 can be silicon oxide and silicon nitride respectively.
[0050] Re-reference Figure 1 After the above structure is prepared, a first photoresist 108 is then formed on the hard mask layer 106. In the embodiment of the present invention, the first photoresist 108 exposes the area where the gate oxide layer is to be formed in the subsequent manufacturing process, such as Figure 1 As shown, it includes part of the source region 100c, the P-type well region 100a, part of the drift region 100b and part of the shallow trench isolation structure 102. The first photoresist 108 will cover the part of the drift region 100b where the drain region 110 is to be formed and the part of the shallow trench isolation structure 102 adjacent to the drain region 110, and will also cover the shallow trench isolation structure 103, the base region 100d and part of the source region 100c adjacent to the base region 100d. The exposed range of the first photoresist 108 is shown in FIG. Fig.11In the embodiment of the present invention, the first photoresist 108 defines the area where the gate oxide layer is to be formed and the area where the step height of the shallow trench isolation structure 102 is to be reduced, so as to expose the substrate 100 in the area and make the step height of the gate oxide layer formed subsequently and the adjacent shallow trench isolation structure 102 not differ too much. After the first photoresist 108 is formed, a first etching process E1 is then performed using the first photoresist 108 as a mask, such as an anisotropic dry etching process, to etch the substrate 100 and the shallow trench isolation structure 102.
[0051] Please refer to Figure 2 . After the first etching process E1, as shown in the figure, the substrate 100 not covered by the first photoresist 108 will be partially etched to form a recess R, which is roughly located on the P-type well region 100a of the substrate 100 and the source region 100c and drift region 100b on both sides, serving as a space for the subsequent formation of a thick gate oxide layer required for high-voltage components. The original pad oxide layer 104 and the hard mask layer 106 above the recess R will be removed to expose the surface of the silicon substrate for the subsequent silicon oxidation process. Furthermore, the first etching process E1 will also partially etch the portion of the shallow trench isolation structure 102 not covered by the first photoresist 108 to form a recess 102a thereon, and the portion covered by the first photoresist will form a convex portion 102b relative to the recess 102a because it is not affected by the etching. It can be seen that at this stage, the convex portion 102b is located on the side of the shallow trench isolation structure 102 close to the predetermined drain region 110, and only occupies a small part of the horizontal area of the shallow trench isolation structure 102, and the concave portion 102a is located on the side of the shallow trench isolation structure 102 close to the P-type well region 100a and occupies most of the horizontal area of the shallow trench isolation structure 102. In the embodiment of the present invention, the formation of the concave portion 102a helps to reduce the step height of the shallow trench isolation structure 102 so that it will not differ too much from the step height of the gate oxide layer formed subsequently. The steps of the above-mentioned etching process can specifically include first removing the uncovered hard mask layer 106 with the first photoresist 108, and then continuing to etch with the patterned hard mask layer 106 as a mask to remove the pad oxide layer 104 below and the substrate 100 and the shallow trench isolation structure 102 to be removed, and removing the first photoresist 108 after the etching process.
[0052] Please refer to Figure 3. After the above-mentioned recess R and recess 102a are formed, an RCA wet cleaning process (or standard cleaning process) is then performed to clean the process surface. Generally, two standard cleaning steps SC-1 and SC-2 are performed, and the cleaning solution used may include an alkaline mixture such as ammonia water and an acidic mixture such as diluted hydrofluoric acid (DHF). In an embodiment of the present invention, the RCA cleaning process may include pre-cleaning the area (i.e., the recess R) where a sacrificial layer (not shown) and a gate oxide layer are to be generated. In addition to removing impurity particles on the surface of these areas, the RCA cleaning process can further reduce the step height of the shallow trench isolation structure 102. In some prior arts, this RCA cleaning process is an important step in controlling the step height of the shallow trench isolation structure. Excessive RCA cleaning can easily damage the silicon substrate surface at the boundary of the shallow trench isolation structure 102, resulting in a mismatch in the on-current (I on The problem of mismatch is that insufficient RCA cleaning will lead to insufficient step height reduction and poor flatness, which may cause the gate formed later on the shallow trench isolation structure and the gate oxide layer to be disconnected or the thickness of the gate oxide layer to be abnormal. In this regard, the present invention uses less RCA cleaning treatment at this stage, for example, the treatment time is 30 seconds less than that of general RCA cleaning to avoid damaging the substrate surface. The step height control of the trench isolation structure 102 will be achieved through subsequent manufacturing processes.
[0053] Re-reference Figure 3. After the RCA cleaning process, a thermal oxidation process is then performed, such as the rapid temperature rise method (RTP), to oxidize the exposed silicon substrate, so that a thick gate oxide layer 112 is formed in the recess R, and other areas such as the predetermined drain area 110 and the adjacent parts of the source area 100c and the base area 100d are not affected because they are blocked by the pad oxide layer 104 and the hard mask layer 106. For high-voltage components, the formed gate oxide layer 112 will be adjacent to the shallow trench isolation structure 102 on the drift region 100b, and the two can be used together as the gate barrier layer of the high-voltage component. The surrounding and bottom of the shallow trench isolation structure 102 can be regarded as the drift region 100b of the collector. Therefore, the step height control between the adjacent gate oxide layer 112 and the shallow trench isolation structure 102 is very important in the high-voltage component manufacturing process. At this stage, the step height of the concave portion 102a of the shallow trench isolation structure 102 is controlled to be slightly higher than the step height of the gate oxide layer 112. In the embodiment of the present invention, this step height difference will be eliminated in the subsequent manufacturing process. Furthermore, in the embodiment of the present invention, since the gate oxide layer 112 is formed by a thermal oxidation manufacturing process, the adjacent portions of the shallow trench isolation structure 102 and the pad oxide layer 104 and the adjacent portions of the gate oxide layer 112 and the pad oxide layer 104 will form bird beak structures (birdbeak) 102c, 112c of silicon oxide components due to the lateral diffusion of oxygen elements. Among them, the convex portion 102b that originally protrudes vertically upward on the shallow trench isolation structure 102 will be inclined toward the pre-bird beak structure 102c due to the formation of the adjacent bird beak structure 102c, and its vertical height is higher than the vertical height of the bird beak structure 112c.
[0054] Please refer to Figure 4 After the gate oxide layer 112 is formed, a selective wet etching process is then performed to remove the remaining hard mask layer 106 on the substrate to expose the protrusion 102 b and the pad oxide layer 104 below.
[0055] Please refer to Figure 5 After the hard mask layer 106 is removed, a first oxide layer 114 is then formed on the pad oxide layer 104. The first oxide layer 114 may be a gate oxide layer on a general device region (not shown, whose driving voltage is between 2 and 4 V, as opposed to 10 to 15 V for high voltage devices). ) is thicker than the gate oxide layer 112 used for the previously formed high voltage device (e.g. ) is much thinner. The first oxide layer 114 can also be formed by thermal oxidation. In the high-voltage component area shown in the figure, it can be combined with the pad oxide layer below to form a thicker oxide layer and adjacent to the bird's beak structure 102c, 112c. The gate oxide layer for the formed high-voltage component is extremely thick and will not be affected by the thermal oxidation method to change its thickness. Since the manufacturing process in the general component area is not the focus of the present invention, the relevant illustrations and descriptions will be omitted in the specification.
[0056] Please refer to Figure 6 After the first oxide layer 114 is formed, a second photoresist 116 is then formed on the high voltage device region. In the embodiment of the present invention, the second photoresist 116 covers the gate oxide layer 112, the bird's beak structure 112c and almost all of the shallow trench isolation structure 102. Only a small portion of the shallow trench isolation structure 102 protrusion 102b near the drain region 110, the bird's beak structure 102c and the first oxide layer 114 are not covered by the second photoresist 116. The range covered by the second photoresist 116 is as follows: Fig.12 As shown in the range R2 in the figure. In the embodiment of the present invention, the second photoresist 116 defines the unnecessary first oxide layer 114 area and the area where the step height of the convex portion 102b of the shallow trench isolation structure 102 is to be reduced. After the second photoresist 116 is formed, a second etching process E2 is then performed using the second photoresist 116 as a mask, such as a wet etching process, to etch the exposed convex portion 102b and the first oxide layer 114. This wet etching process can use BOE (NH4F:HF=6:1) or DHF etching solution, which has a better etching selectivity to silicon oxide.
[0057] Please refer to Figure 7 . After the second etching process E2, as shown in the figure, the first oxide layer 114 and the pad oxide layer 104 on the high-voltage component area will be removed to expose the predetermined drain area 110 below. Furthermore, part of the convex portion 102b of the shallow trench isolation structure 102 will also be removed in this step to reduce its step height to be lower than the bird's beak structure 112c. The second photoresist 116 is removed after the second etching process E2. In an embodiment of the present invention, the first etching process E1 reduces the step height of the shallow trench isolation structure 102 on the side of the P-type well region 100a, and the second etching process E2 reduces the step height on the side of the convex portion 102b of the shallow trench isolation structure 102, both of which have the effect of controlling the step height.
[0058] Please refer to Figure 8After the second etching process E2, a second oxide layer 118 is formed on the exposed drain region 110 and part of the adjacent source region 100c and base region 100d. The second oxide layer 118 may be a gate oxide layer on a low voltage device region (not shown, whose driving voltage is about 1.2V, compared to 2-4V for general devices and 10-15V for high voltage devices). The thickness (e.g. ) is thicker than the gate oxide layer 112 used for the previously formed high voltage device (e.g. ) and the gate oxide layer used in general components (such as the first oxide layer 114 ) is much thinner. The second oxide layer 118 is adjacent to the bird's beak structures 102c, 112c. Similarly, since the manufacturing process in the low-voltage component area is not the focus of the present invention, the relevant illustrations and descriptions will be omitted in the specification.
[0059] Please refer to Fig. 9 After the second oxide layer 118 is formed, a third photoresist 120 is then formed on the high voltage element region. In the embodiment of the present invention, the third photoresist 120 covers the gate oxide layer 112 and a small portion of the shallow trench isolation structure 102 near the gate oxide layer 112 and a portion of the bird's beak structure 112c. Almost most of the shallow trench isolation structure 102 is not covered by the third photoresist 120. The area of the shallow trench isolation structure 102 covered by the third photoresist 120 does not overlap with the area of the shallow trench isolation structure 102 previously covered by the first photoresist 108. The range covered by the third photoresist 120 is as follows: Fig.12 As shown in the range R3 in the figure. In the embodiment of the present invention, the second photoresist 116 defines the unnecessary second oxide layer 118 area. More importantly, it defines the area where the step height of the shallow trench isolation structure 102 is to be reduced, so that the subsequent shallow trench isolation structure 102 can be flush with the adjacent gate oxide layer 112. Similar to the second etching process E2, after the third photoresist 120 is formed, a third etching process E3 is then performed using the third photoresist 120 as a mask, such as a wet etching process, to etch the exposed shallow trench isolation structure 102 and the second oxide layer 118. This wet etching process can use BOE or DHF etching solution, which has a better etching selectivity to silicon oxide.
[0060] Please refer to Fig.10. After the third etching process E3, as shown in the figure, the second oxide layer 118 on the high voltage element area will be removed, exposing the drain region 110 below and the adjacent source region 100c and base region 100d. Furthermore, part of the shallow trench isolation structure 102 will also be removed, so that its step height is reduced to be flush with the adjacent gate oxide layer 112. The third photoresist 120 is removed after the third etching process E3. It should be noted that although part of the shallow trench isolation structure 102 is covered by the photoresist in the third etching process E3, due to the isotropic etching property of the wet etching process, the covered part of the shallow trench isolation structure 102 will also be removed, so that the part is also flush with the surrounding parts. Furthermore, the third etching process E3 will also reduce the step height of the bird's beak structure 112c and the protrusion 102b, but the reduced step height of the bird's beak structure 112c is still higher than the step height of the protrusion 102b.
[0061] Different from the prior art method of controlling the step height of the shallow trench isolation structure 102 and the gate oxide layer 112 through a relatively long RCA cleaning process and a first etching process, in an embodiment of the present invention, the step height of the adjacent shallow trench isolation structure 102 and the gate oxide layer 112 is finally achieved through a third etching process E3, thereby reducing the cleaning time of the previous RCA process, avoiding damage to the silicon surface and affecting the electrical properties, while maintaining the required flatness of the component structure, which is the advantage of the present invention.
[0062] Please refer to Fig.11 . After the third etching process E3, a gate 122 is then formed on the high-voltage component area, and its material can be polysilicon. In an embodiment of the present invention, the gate 122 is located on the same plane as a portion of the gate oxide layer 112 and the shallow trench isolation structure 102. The bird's beak structure 112c and the protrusion 102b are respectively located on both sides of the gate 122. The gate oxide layer 112 and the shallow trench isolation structure 102 jointly serve as a gate barrier layer of the gate 122. Below the gate 122 are the P-type well region 100a and the drift region 100b of the high-voltage component. The gate 122 is isolated from the drain region 110 by the shallow trench isolation structure 102. Preferably, one end of the gate 122 is aligned with the P-type well region 100a and the source region 100c, and the other end is aligned with the center line of the shallow trench isolation structure 102. Since the aforementioned manufacturing process provides a flat manufacturing process surface on the gate oxide layer 112 and the shallow trench isolation structure 102 , the gate 122 formed thereon will not have the disconnection problem as in the prior art.
[0063] According to the above manufacturing process, the present invention also proposes a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer. Fig.11 , and can also refer to Fig.12Floor plan, Fig.11 That is Fig.12 The cross-sectional view is made by the A-A' section line. The semiconductor structure of the present invention having a flush shallow trench isolation structure and a gate oxide layer includes a substrate 100. In a preferred embodiment, the substrate 100 has a well region 100a, a source region 100c located on one side of the well region 100a, and a drift region 100b located on the other side of the well region 100a. The source region 100c also has a base region 100d on the other side relative to the well region 100a. A shallow trench isolation structure 102 is located in the drift region 100b, and the outer side of the shallow trench isolation structure 102 has a convex portion 102b and a first bird's beak structure 102c, and the first bird's beak structure 102c is connected to the convex portion 102b. A gate oxide layer 112 is located on the well region 100a and the source region 100c and is connected to the shallow trench isolation structure 102, and the shallow trench isolation structure 102 is flush with the top surface of the gate oxide layer 112, and the flush top surface of the shallow trench isolation structure 102 and the gate oxide layer 112 is also at the same height as the top surface of the source region 100c and the drift region 100b. The drift region 100b on the other side of the shallow trench isolation structure 102 relative to the gate oxide layer 112 is a drain region 110. The outer side of the gate oxide layer 112 has a second bird's beak structure 112c located on the source region 100c, wherein the height of the second bird's beak structure 112c is higher than the height of the convex portion 102b, and the heights of the first bird's beak structure 102c, the second bird's beak structure 112c and the convex portion 102b are higher than the flush top surface of the shallow trench isolation structure 102 and the gate oxide layer 112. A gate 122 is located on the gate oxide layer 112 and a portion of the shallow trench isolation structure 102, wherein one side of the gate 122 is aligned with the boundary of the well region 100a and the source region 100c. In addition, a drain 124 is formed on the drain region 110 outside the first bird's beak structure 102c, and a source 126 is formed on the source region 100c and the base region 100d outside the second bird's beak structure 112c.
[0064] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.
Claims
1. A method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer, comprising: Providing a substrate having a shallow trench isolation structure protruding from the substrate and a pad oxide layer covering the substrate; Forming a first photoresist on the drain region on one side of the shallow trench isolation structure, wherein the first photoresist covers a portion of the top surface of the shallow trench isolation structure from the side; Performing a first etching process using the first photoresist as a mask to remove the pad oxide layer on the other side of the shallow trench isolation structure and to recess the substrate, wherein the first etching process also forms a concave portion not covered by the first photoresist and a convex portion covered by the first photoresist on the shallow trench isolation structure; removing the first photoresist; Forming a gate oxide layer on the recessed substrate, wherein the gate oxide layer is adjacent to the shallow trench isolation structure; forming a second photoresist on the gate oxide layer, wherein the second photoresist covers almost all of the shallow trench isolation structure, with only the edge of the convex portion on the side not being covered; Performing a second etching process using the second photoresist as a mask to remove the pad oxide layer on the protrusion and the drain region; removing the second photoresist; forming a first oxide layer on the drain region; Forming a third photoresist on the gate oxide layer, wherein the third photoresist only covers the edge portion of the shallow trench isolation structure on the other side, and the shallow trench isolation structure region covered by the third photoresist does not overlap with the shallow trench isolation structure region covered by the first photoresist; as well as A third etching process is performed using the third photoresist as a mask to remove a portion of the shallow trench isolation structure and the entire first oxide layer, so that the top surface of the shallow trench isolation structure is flush with the gate oxide layer.
2. The method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as claimed in claim 1, further comprising forming a gate on a portion of the gate oxide layer and the shallow trench isolation structure after the third etching process.
3. The method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as described in claim 1, wherein a hard mask layer is also provided on the shallow trench isolation structure and the pad oxide layer, and the first etching process also removes the hard mask layer not covered by the first photoresist. 4 . The method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as claimed in claim 3 , further comprising removing the hard mask layer after the gate oxide layer is formed.
5. The method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as described in claim 1 further comprises performing an RCA cleaning process after removing the first photoresist and before forming the gate oxide layer, wherein the RCA cleaning process reduces the height of the recess but is still higher than the gate oxide layer formed subsequently.
6. A method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as described in claim 1, wherein the shallow trench isolation structure, the gate oxide layer and the pad oxide layer are located in a high-voltage device area, and further comprises forming a second oxide layer on a general device area after the gate oxide layer is formed, wherein the second oxide layer is formed on the pad oxide layer in the high-voltage device area, and the second etching process completely removes the pad oxide layer and the second oxide layer.
7. A method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as described in claim 1, wherein the shallow trench isolation structure, the gate oxide layer and the pad oxide layer are located in a high-voltage device area, and the first oxide layer serves as a gate oxide layer on a low-voltage device area, and the third etching process removes the first oxide layer on the high-voltage device area.
8. A method for manufacturing a semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer as described in claim 1, wherein the gate oxide layer is formed by a thermal oxidation process, and the thermal oxidation process also forms a bird's beak structure on the side of the shallow trench isolation structure, and the bird's beak structure is located between the shallow trench isolation structure and the pad oxide layer and is adjacent to both.
9. A semiconductor structure having a flush shallow trench isolation structure and a gate oxide layer, comprising: A substrate including a well region, a source region located on one side of the well region, and a drift region located on the other side of the well region; A shallow trench isolation structure is located in the drift region, wherein the outer side of the shallow trench isolation structure has a convex portion and a first bird's beak structure, and the first bird's beak structure is connected to the convex portion; A gate oxide layer is located on the well region and the source region and connected to the shallow trench isolation structure, and the shallow trench isolation structure is flush with the top surface of the gate oxide layer, and the outer side of the gate oxide layer has a second bird's beak structure located on the source region; as well as The gate is located on the gate oxide layer and a portion of the shallow trench isolation structure. 10 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9 , wherein the drift region located on the other side of the shallow trench isolation structure relative to the gate oxide layer is a drain region. 11 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 10 , further comprising a drain formed on the drain region outside the first bird's beak structure. 12 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9 , further comprising a base region located on the other side of the source region relative to the well region. 13 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 12 , further comprising a source electrode formed on the source region and the base region outside the second bird's beak structure. 14 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9 , wherein a height of the second bird's beak structure is higher than a height of the protrusion.
15. The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9, wherein heights of the first bird's beak structure, the second bird's beak structure and the protrusion are higher than flush top surfaces of the shallow trench isolation structure and the gate oxide layer. 16 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9 , wherein the flush top surfaces of the shallow trench isolation structure and the gate oxide layer are at the same height as the top surfaces of the source region and the drift region. 17 . The semiconductor structure with flush shallow trench isolation structure and gate oxide layer as claimed in claim 9 , wherein one side of the gate is aligned with the boundary of the well region and the source region.