Laser processing system for annealing perovskite solar cell
By using a 450nm wavelength dark blue semiconductor diode laser and a one-dimensional relative motion mode laser processing system in perovskite solar cell manufacturing, the problem of high cost and large footprint of laser annealing system in large-scale production is solved, and high efficiency is achieved , low-cost annealing effect.
Patent Information
- Application Number
- CN202411332256.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-24
- Publication Date
- 2024-11-26
AI Technical Summary
In the manufacturing process of perovskite solar cells, the lack of suitable large-scale production laser annealing systems leads to high cost, large footprint and incompatible with other manufacturing processes.
A laser processing system for perovskite solar cells was designed, using a dark blue semiconductor diode laser with a wavelength of about 450nm, and annealing was achieved through one-dimensional relative motion mode. The system can be expanded to match different workpiece widths and increase the number of lasers. Achieve annealing range expansion and reduce costs.
Higher annealing efficiency and cost control are achieved, and with the lowest cost and higher reliability compared to other lasers, suitable for large-scale production.
Smart Images

Figure CN119031803A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of solar cells, and in particular relates to a laser processing system for annealing perovskite solar cells. Background Art
[0002] Annealing is a process that applies heat to a material and then cools it to cause a phase change in the material, for example, from an amorphous state to a crystalline state. Laser annealing is a type of annealing process in which the heat source of the annealing is one or more lasers, i.e., one or more lasers irradiate the material to heat the material by absorbing the light energy provided by the laser.
[0003] Annealing is an essential step in the manufacture of perovskite solar cells (PSCs). The initial perovskite film, which is prepared from a solution mixture of the constituent materials and deposited on a substrate, is not photovoltaically active, that is, it has no photovoltaic effect and therefore cannot be used as a solar cell. Only after annealing, when the amorphous state of the film becomes crystalline, will the photovoltaic effect be activated.
[0004] There are various techniques / methods for PSC annealing, such as hot plate, oven / heating chamber, and laser. The quality of annealed perovskite films depends on many factors, such as peak temperature, heating and cooling rates. Among the different annealing techniques, laser annealing can provide greater flexibility and facilitate the control of key factors affecting the annealing process.
[0005] Other major factors to consider when selecting an annealing process for PSCs, especially for large-scale production, include cost, floor space, and compatibility with other PSC manufacturing processes, such as roll-to-roll manufacturing. Taking all these factors into consideration, laser annealing has certain advantages. Therefore, it is of great positive significance to develop laser annealing technology, processes, and equipment for PSC manufacturing. Summary of the invention
[0006] The technical problem to be solved by the present invention is: how to develop a laser annealing system suitable for PSC board manufacturing.
[0007] In order to achieve the above technical objectives, the present invention adopts the following technical solutions:
[0008] A laser processing system for annealing a perovskite solar cell comprises a solar cell panel moving platform, a laser array lifting rail, a laser array lifting motor, a laser line shaping optical element bracket, a semiconductor laser array water cooling bracket, a semiconductor laser, and a laser line shaping optical element, wherein the laser array lifting rail extends vertically, a laser line shaping optical element bracket is slidably connected to the laser array lifting rail, the laser array lifting motor drives the laser line shaping optical element bracket, a semiconductor laser array water cooling bracket is fixedly connected to the laser line shaping optical element bracket, a plurality of semiconductor lasers are installed in the semiconductor laser array water cooling bracket, a laser line shaping optical element is installed in the laser line shaping optical element bracket, a plurality of semiconductor lasers are arranged in a straight line, the laser line shaping optical element is located below the plurality of semiconductor lasers, and the movement stroke of the solar cell panel moving platform passes below the laser line shaping optical element.
[0009] Preferably, it also includes a support plate and a gantry, wherein the gantry is fixedly connected to the support plate, the gantry is perpendicular to the support plate, two laser array lifting rails are provided, and the two laser array lifting rails are respectively fixed on the inner side of the left frame line and the inner side of the right frame line of the gantry.
[0010] Preferably, it also includes support rods, a base plate, slide rails, a connecting plate, and strip holes, wherein a plurality of support rods are fixedly connected to the bottom end of the support plate, the base plate is fixedly connected to the plurality of support rods, the base plate and the support plate are parallel to each other, a slide rail is fixed to the base plate, strip holes are opened on the support plate, and a connecting plate is provided on the solar panel mobile platform, the connecting plate passes through the strip holes and is slidably connected to the slide rails.
[0011] Preferably, the semiconductor laser is a semiconductor diode laser having an emission wavelength of 440 to 460 nm.
[0012] Preferably, the emission wavelength of the semiconductor laser is 450 nm.
[0013] The present invention provides a laser processing system for annealing perovskite solar cells. The system uses a deep blue semiconductor diode laser (LD) with a wavelength of about 450nm, which has a higher absorption rate for perovskite materials, thereby achieving higher annealing efficiency. The system designs a one-dimensional relative motion mode between the LD array and the workpiece, and the array width can be arbitrarily expanded as needed to match the entire workpiece width. Over the entire array width of the LD, the line beam uniformity is very good and has nothing to do with the array width; the present invention only needs to increase the number of LDs to achieve the expansion of the annealing range, and the cost is controllable. In addition, compared with fiber lasers and solid-state lasers, the present invention directly uses LD annealing to achieve the lowest cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is the external structure diagram of the whole invention.
[0015] Figure 2 It is a partial cross-sectional view (fast axis cross section) of the laser line shaping optical element support and the semiconductor laser array water cooling support in the present invention.
[0016] Figure 3 It is a partial longitudinal cross-sectional view (slow axis cross-sectional view) of the laser line shaping optical element support and the semiconductor laser array water cooling support in the present invention.
[0017] Figure 4 It is a working principle diagram of the present invention.
[0018] Figure 5 This is the laser emission pattern of 450nm LD.
[0019] Figure 6 2 is an exemplary optical design diagram of a PSC annealing system; wherein (a) is a slow axis profile and (b) is a fast axis profile.
[0020] Figure 7 It is a beam profile diagram of an exemplary optical design of a PSC annealing system on the PSC panel plane; wherein (a) is a two-dimensional image, (b) is the beam intensity in the fast axis direction (X-axis), and (c) is the beam intensity along the slow axis direction (Y-axis).
[0021] Figure 8 Figure 1 is an example of the scalability of the PSC laser annealing system; (a) is an example of the optical design when the number of LDs increases from 11 to 21 and the width of the LD array increases from 100 mm to 200 mm, and (b) is the beam intensity when the portion of the uniform beam increases from 50 mm to 150 mm.
[0022] Fig. 9 This is a simple semiconductor laser tube driver schematic; (a) is a standard DC power supply for driving the series LDs, and (b) is an adjustable resistor in parallel with each LD for LD output power balance.
[0023] In the figure:
[0024] 1. Solar panel mobile platform 2. Laser array lifting rail
[0025] 3. Laser array lifting motor 4. Laser line shaping optical element bracket
[0026] 5. Water cooling bracket for semiconductor laser array 6. Semiconductor laser
[0027] 7. Laser line shaping optical element 8. Support plate
[0028] 9. Gantry 10. Support rod
[0029] 11. Bottom plate 12. Slide rail
[0030] 13. Connecting plate 14. Strip hole. DETAILED DESCRIPTION
[0031] The specific embodiments of the present invention will be described in detail below. In order to avoid too much unnecessary details, the well-known structures or functions will not be described in detail in the following examples. The approximate language used in the following examples can be used for quantitative expression, indicating that the quantity can be allowed to have a certain change without changing the basic function. Unless otherwise defined, the technical and scientific terms used in the following examples have the same meaning as those generally understood by those skilled in the art to which the present invention belongs.
[0032] A laser processing system for annealing perovskite solar cells, such as Figure 1 to Figure 3 As shown, it includes a solar panel moving platform 1, a laser array lifting guide rail 2, a laser array lifting motor 3, a laser line shaping optical element bracket 4, a semiconductor laser array water cooling bracket 5, a semiconductor laser 6, and a laser line shaping optical element 7, wherein the laser array lifting guide rail 2 extends vertically, the laser array lifting guide rail 2 is slidably connected with the laser line shaping optical element bracket 4, the laser array lifting motor 3 drives the laser line shaping optical element bracket 4, the semiconductor laser array water cooling bracket 5 is fixedly connected to the laser line shaping optical element bracket 4, a plurality of semiconductor lasers 6 are installed in the semiconductor laser array water cooling bracket 5, a laser line shaping optical element 7 is installed in the laser line shaping optical element bracket 4, the plurality of semiconductor lasers 6 are arranged in a straight line, the laser line shaping optical element 7 is located below the plurality of semiconductor lasers 6, and the movement stroke of the solar panel moving platform 1 passes below the laser line shaping optical element 7. It also includes a support plate 8 and a gantry 9, wherein the gantry 9 is fixedly connected to the support plate 8, the gantry 9 is perpendicular to the support plate 8, and two laser array lifting rails 2 are provided, and the two laser array lifting rails 2 are respectively fixed to the inner side of the left frame line and the inner side of the right frame line of the gantry 9. It also includes a support rod 10, a bottom plate 11, a slide rail 12, a connecting plate 13, and a strip hole 14, wherein a plurality of support rods 10 are fixedly connected to the bottom end of the support plate 8, the bottom plate 11 is fixedly connected to a plurality of support rods 10, the bottom plate 11 and the support plate 8 are parallel to each other, a slide rail 12 is fixed to the bottom plate 11, a strip hole 14 is opened on the support plate 8, and a connecting plate 13 is provided on the solar panel mobile platform 1, and the connecting plate 13 passes through the strip hole 14 and is slidably connected to the slide rail 12. The semiconductor laser 6 is a semiconductor diode laser with an emission wavelength of 440 to 460 nm.
[0033] In the present invention, multiple semiconductor diode lasers (LDs) with an emission wavelength of about 450 nm are arranged in a line array to form a laser source module. The light emitted from the lasers passes through a beam shaping optical device and is focused into a thin line on the PSC panel to be annealed.
[0034] The present invention selects a deep blue laser diode as the laser source for many reasons:
[0035] First, the deep blue wavelength of around 450nm is ideal for laser annealing because its absorption rate in perovskite films is higher than that of longer wavelength lasers, which are generally 800-1000nm from other existing LDs, so heating is more efficient. On the other hand, the wavelength is not too short compared to other available laser wavelengths, such as ultraviolet lasers (355nm, obtained by tripling the frequency of Nd:YAG solid-state lasers) or ultraviolet excimer lasers (308nm, 248nm, etc.), which may cause adverse effects such as photochemical decomposition of perovskite materials.
[0036] Second, 450nm LDs are inexpensive, and they are actually the lowest cost per watt laser source in this wavelength range. For example, a 5W 447nm LD from ams-OSRAM is packaged in a TO-9 package, part number PLPT9 450LB_E (https: / / ams-osram.com / products / lasers / color-lasers-eel / osr am-metal-can-plpt9-450lb-e), and retails for less than RMB 200, or less than RMB 40 per watt. This is the LD that the present invention chose to use in the prototype PSC laser annealing device. When mass-producing the device, the cost should be significantly reduced through volume discounts.
[0037] Third, these laser sources are more reliable than other types of lasers and can operate over a wide range of operating conditions. For example, a 5W ams-OSRAM laser can operate over a temperature range of -20–90°C.
[0038] Fourth, compared with using fiber laser or solid laser as pump source, directly using LD for laser processing has the highest electro-optical conversion efficiency. The above ams-OSRAM LD produces 5W laser output with 12.9W electrical input power (4.3V, 3A), and the electro-optical conversion efficiency is close to 40%. Higher efficiency means less power consumption and lower operating costs.
[0039] Fifth, the laser annealing process using a single LD array as the laser source has excellent scalability, which is an important consideration for industrial production. The present invention can simply add additional LDs to the array to increase the array width to accommodate different PSC panel widths.
[0040] The optical device between the LD and the PSC panel shapes, homogenizes and focuses the light emitted by the LD on the PSC panel to form a uniform line beam. The unique light-emitting characteristics of the LD make the beam shaping optical device relatively simple. For example, in the prototype PSC laser annealing device of the present invention, a simple cylindrical lens is used to produce a uniform line beam on the PSC surface. (More details are provided in the examples in Section 6.)
[0041] The PSC panel to be annealed is placed on a translation stage that moves in an orthogonal direction relative to the stationary laser beam. The temperature rise of the laser-irradiated PSC depends on the time each point of the PSC film is irradiated, which is easily controlled by the speed of the translation stage.
[0042] PSC thin film annealing is a key step in the manufacturing process of PSC solar panels. Without it, perovskite is not a solar cell. Among various annealing methods, laser annealing process and equipment can be more energy-efficient, compact, and have controllable heating and cooling speeds, which can be more advantageous.
[0043] For laser annealing, there are different ways to perform the process, such as different laser sources, beam shapes, scanning methods, etc. The laser annealing technology and equipment disclosed in the present invention are particularly suitable for PSC board manufacturing. The following table compares the use of standard lasers and the LD array disclosed in the present invention for PSC laser annealing:
[0044] Table 1 Comparison of the characteristics of standard laser annealing and laser annealing of the present invention
[0045]
[0046]
[0047] Figure 4 This is a schematic diagram of the present invention. Figure 4 In addition to the key components in Figure 1 Also shown are some of the mechanical components of the system, including a water-cooled mechanical mount for the LD array, mounts for the beam-shaping optics, a vertical translation stage for the LD array and optics module for adjusting the focus of the beam, and the PSC panel mounted on a translation stage for moving the panel perpendicular to the direction of the laser beam. Other components, such as the power supply, LD driver, electronic and computer control components, laser power and temperature monitors, and safety enclosures are not shown for simplicity. For further illustration and clarity, Figure 2The fast axis cross section (XZ plane) is shown. Figure 3 The slow axis cross section is shown.
[0048] The laser source consists of a single 450nm LD in a linear array. A typical LD is manufactured by ams-OSRAM, part number PLPT9 450LB_E, 5W, 447nm LD, in TO-9 package. As a commercially available product, its specifications and operating parameters can be found from public channels (such as website information). Figure 5 is the laser angular emission pattern. Like a typical edge-emitting LD, the angular emission pattern is highly asymmetric in two orthogonal directions, with a typical fast axis angle (49°) being approximately five times that of the slow axis (9°). Usually, this emission pattern is not conducive to obtaining a good circular focused spot, however, the present invention utilizes this asymmetry to shape the output of multiple LDs into a uniform beam using simple optical elements, so this disadvantage actually becomes an advantage in the present invention.
[0049] Figure 6 Here is the design and layout of a simple optical system (made using the optical design software Zemax) for generating uniform line beams from these LD arrays. Due to the size constraints of the TO-9 package of the LD (TO-9 has an outer diameter of 9mm), the center-to-center distance between the LDs in the array is 10mm. The LDs are arranged in such a way that the fast axis of the LD is along the linear array direction and the slow axis is orthogonal to it. A standard cylindrical lens (focal length f=10mm in the exemplary embodiment) images the light output in the slow axis direction (YZ plane) so that the PSC is at a distance (60mm from the cylindrical lens in the exemplary embodiment) where the PSC panel is placed. However, the fast axis (XZ plane) is free to diverge in this direction without a lens. The diffusion of the fast axis beam causes the light from different LDs to overlap along this direction on the plane of the PSC panel. The diffusion and overlap homogenize the distribution of light along the fast axis. The result is a uniform line beam on the plane of the PSC panel, as shown in Figure 1. Figure 7 In this example, 11 LDs are used to form an LD array with a span of 100 mm, and the resulting line beam has a uniform section of approximately 50 mm. The uniform section is where the light contributions from the LDs on both sides are equal, so the light is uniform, whereas this is not true near the edge of the line beam.
[0050] As mentioned above, a key point of the present invention is scalability. As a laser annealing device for PSC panels, the present invention hopes that a uniform portion of the laser beam covers the entire width of the panel. Different solar panels have different widths, and a typical standard width is 1.2m or 2.4m. In order to adapt the laser annealing technology and equipment to different PSC panel widths, the present invention can simply change the number of LDs in the array while maintaining the same optical design. Figure 8 An example of the scalability of the present invention is shown, where the number of LDs increases from 11 to 21 as the array width increases from 100 mm to 200 mm, as shown in FIG. Figure 8 As a result of the design, the uniform portion of the line beam also increases from ~50 mm to ~150 mm, in the same manner as the array width increases. This relationship holds true when the array width increases to any value.
[0051] Fig. 9 A simple LD driver schematic is shown to ensure uniform illumination in a line beam. As is typical of LDs, the output power of an exemplary 450nm LD depends on the current flowing through it. To drive multiple LDs, as in the present invention, it is advantageous to drive them in series, i.e. the cathode of each LD is connected to the anode of the next LD, rather than driving them in parallel, i.e. the electrodes of the same polarity of all LDs are connected together. This is because it is generally easier and more cost-effective to manufacture a DC power supply with a higher voltage but lower current than a DC power supply with a lower voltage but higher current at the same output power. Fig. 9 (a) is a schematic diagram of a series LD drive circuit, where the current flowing through any LD is the same as the current flowing through any other LD. Ideally, if all LDs in the series are identical, this circuit is sufficient. In practice, the laser output power as a function of the drive current varies between different LDs in the series, i.e., some LDs produce higher laser output power than others at the same current. Fig. 9 (b) is a simple solution to this problem. Each LD has an adjustable resistor in parallel. A small portion of the total current flows through the resistor instead of the corresponding LD. The amount of current flowing through the resistor depends on the resistance value. By adjusting the resistance value of the shunt resistor, the current flowing through each LD can be adjusted, so that the laser output power of these LDs is equal.
[0052] The embodiments of the present invention are described in detail above, but the contents are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the scope of the present invention shall be included in the protection scope of the present invention.
Claims
1. A laser processing system for annealing perovskite solar cells, It is characterized in that The invention comprises a solar panel mobile platform (1), a laser array lifting rail (2), a laser array lifting motor (3), a laser line shaping optical element bracket (4), a semiconductor laser array water cooling bracket (5), a semiconductor laser (6), and a laser line shaping optical element (7), wherein the laser array lifting rail (2) extends vertically, the laser line shaping optical element bracket (4) is slidably connected to the laser array lifting rail (2), the laser array lifting motor (3) drives the laser line shaping optical element bracket (4), and the laser array lifting motor (4) drives the laser line shaping optical element bracket (4). A semiconductor laser array water cooling bracket (5) is fixedly connected to the laser line shaping optical element bracket (4), a plurality of semiconductor lasers (6) are installed in the semiconductor laser array water cooling bracket (5), a laser line shaping optical element (7) is installed in the laser line shaping optical element bracket (4), the plurality of semiconductor lasers (6) are arranged in a straight line, the laser line shaping optical element (7) is located below the plurality of semiconductor lasers (6), and the movement stroke of the solar cell panel mobile platform (1) passes below the laser line shaping optical element (7).
2. A laser processing system for annealing a perovskite solar cell according to claim 1, It is characterized in that It also includes a support plate (8) and a gantry (9), wherein the gantry (9) is fixedly connected to the support plate (8), the gantry (9) is perpendicular to the support plate (8), and two laser array lifting guide rails (2) are provided, and the two laser array lifting guide rails (2) are respectively fixed to the inner side of the left frame line and the inner side of the right frame line of the gantry (9).
3. A laser processing system for annealing perovskite solar cells according to claim 2, It is characterized in that The solar panel mobile platform (1) further comprises a support rod (10), a bottom plate (11), a slide rail (12), a connecting plate (13), and a strip hole (14), wherein a plurality of support rods (10) are fixedly connected to the bottom end of the support plate (8), the bottom plate (11) is fixedly connected to the plurality of support rods (10), the bottom plate (11) and the support plate (8) are parallel to each other, a slide rail (12) is fixed to the bottom plate (11), a strip hole (14) is provided on the support plate (8), and a connecting plate (13) is provided on the solar panel mobile platform (1), the connecting plate (13) passes through the strip hole (14) and is slidably connected to the slide rail (12).
4. A laser processing system for annealing a perovskite solar cell according to claim 1, It is characterized in that The semiconductor laser (6) is a semiconductor diode laser with an emission wavelength of 440 to 460 nm.
5. A laser processing system for annealing perovskite solar cells according to claim 4, It is characterized in that The emission wavelength of the semiconductor laser (6) is 450 nm.