Forming method of full-fluorine-lined self-operated micro-pressure regulating valve
By employing a multi-layer progressive fluoropolymer lining process and pulse cooling technology, the corrosion resistance and sealing issues of the micro-pressure regulating valve have been resolved, improving the overall performance and stability of the valve. This makes it suitable for micro-pressure regulation of highly corrosive media such as chemical and pharmaceutical products.
Patent Information
- Application Number
- CN202411527498.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-30
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-10-30
AI Technical Summary
Existing micro-pressure regulating valves are inadequate in terms of corrosion resistance, sealing, and regulating accuracy. In particular, when handling highly corrosive media, the service life and stability of the valves cannot meet the actual requirements.
A multi-layer progressive fluoropolymer lining process is adopted, which includes electrostatic spraying of fluoroplastic powder and melting it layer by layer, combined with pulse cooling technology, and ultrasonic cleaning and chemical polishing pretreatment of the metal valve body to ensure the adhesion of fluoroplastic to the metal surface, and corrosion resistance and airtightness tests are carried out.
It significantly improves the valve's sealing performance and corrosion resistance, extends its service life, and ensures stable operation under low pressure conditions. It is suitable for low pressure regulation of highly corrosive media such as chemical and pharmaceutical products.
Smart Images

Figure CN119036002A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of regulating valve production, and in particular to a molding method of a fully fluorine-lined self-operated micro-pressure regulating valve. Background Art
[0002] Fully lined fluorine self-operated micro-pressure regulating valve is a regulating valve used in industrial fields, especially in chemical and pharmaceutical industries with high requirements for medium corrosiveness. This type of regulating valve can automatically adjust the micro-pressure in the system without an external power source through a self-operated structural design to ensure the stability of fluid pressure. Due to its easy operation and no need for an external control system, it has been widely used in micro-pressure regulation and control of gases and liquids.
[0003] However, in actual use, the existing micro-pressure regulating valves have certain deficiencies in terms of corrosion resistance, sealing and adjustment accuracy, especially when dealing with highly corrosive media, the service life and stability of the valves often cannot meet actual needs. Therefore, a new molding method is needed to improve the overall performance and reliability of the valve. Summary of the invention
[0004] In view of the shortcomings of the prior art, the present invention provides a molding method for a fully fluorine-lined self-operated micro-pressure regulating valve, which solves the problems that the existing micro-pressure regulating valves have certain shortcomings in corrosion resistance, sealing and adjustment accuracy, especially when dealing with highly corrosive media, the service life and stability of the valve often cannot meet actual needs.
[0005] To achieve the above objectives, the present invention is implemented through the following technical solutions: a method for forming a fully lined fluorine self-operated micro-pressure regulating valve, comprising the following steps: S1: Provide a metal valve body, which is made of high-pressure resistant material and has a preset micro-pressure regulating structure; S2: Surface pretreatment of the metal valve body, including ultrasonic cleaning and chemical polishing of the inner cavity of the valve body, to enhance the adhesion between the fluoroplastic and the metal surface; S3: Preheat the metal valve body to a temperature range of 200 °C to 250 °C; S4: performing a fluorine lining operation on the inner surface of the preheated metal valve body through a multi-layer progressive fluorine lining process, wherein the multi-layer progressive fluorine lining process includes electrostatically spraying fluorine plastic powder and melting it multiple times until the thickness required by the design is reached; S5: Pulse cooling technology is used to control the cooling process to avoid the generation of internal stress in the fluoroplastic layer; S6: Assemble valve components, including key components such as regulating structure, sealing device and micro-pressure regulating device, to ensure coordination with the molding process of the fluorine lining layer to form a complete micro-pressure regulating valve structure; S7: Perform performance tests on the molded control valve, including corrosion resistance, air tightness and regulation accuracy tests, to ensure stable operation under micro-pressure conditions.
[0006] Preferably, the multi-layer progressive fluorine lining process adopts an electrostatic spraying method to uniformly adhere fluoroplastic powder to the metal surface through electric field force to form a fluorine lining layer.
[0007] Preferably, the material of the fluorine lining layer is polytetrafluoroethylene, and its spraying thickness is controlled between 0.1 mm and 0.2 mm.
[0008] Preferably, the pulse cooling technology maintains lower internal stress during the cooling process by controlling the flow rate and temperature of the cooling medium in sections.
[0009] Preferably, the cooling medium is a combination of gas cooling or liquid cooling, and the flow rate and temperature of the cooling medium are adjusted according to the material of the metal valve body.
[0010] Preferably, a combined process of ultrasonic cleaning and chemical polishing is used in the surface pretreatment step of the metal valve body to remove tiny particles and oil stains on the metal surface.
[0011] Preferably, the solvent used in the chemical polishing is an acidic or alkaline solution.
[0012] Preferably, the preheating step is performed by far infrared heating or resistance heating to make the surface of the metal valve body reach a desired temperature, so that the fluoroplastic powder can be uniformly melted and attached to the metal surface.
[0013] Preferably, the melting operation in the fluorine lining process is carried out through a layer-by-layer heating and cooling cycle, and each layer of fluoroplastic is partially cooled after melting to reduce stress accumulation between layers.
[0014] Preferably, after the fluorine lining operation is completed, the entire valve surface is subjected to a corrosion resistance test and a high temperature test.
[0015] Beneficial Effects The present invention provides a method for forming a fully fluorine-lined self-operated micro-pressure regulating valve. Compared with the prior art, it has the following beneficial effects: The present invention proposes a molding method for a fully fluorine-lined self-operated micro-pressure regulating valve. Fluoroplastic powder is uniformly attached to the surface of a metal valve body by an electrostatic spraying method and melted layer by layer, which effectively avoids the generation of weak areas and significantly improves the sealing and corrosion resistance of the valve under micro-pressure regulation conditions, thereby enhancing the overall performance of the valve. During the molding process, the surface pretreatment process is combined with ultrasonic cleaning and chemical polishing, which not only effectively removes tiny particles and oil stains on the metal surface, but also improves the adhesion between the fluorine plastic and the metal surface. Good adhesion ensures the stability of the fluorine lining layer during use and extends the service life of the valve. In addition, after this pretreatment step, the corrosion resistance of the valve in the face of various corrosive media is further improved. During the cooling process, the present invention adopts pulse cooling technology to effectively control the flow rate and temperature of the cooling medium, thereby avoiding the problem of cracking or falling off of the fluorine lining layer caused by excessive temperature difference. This technical innovation not only improves the integrity and consistency of the fluorine lining layer, but also reduces the risk of failure caused by internal stress accumulation, laying a solid foundation for the long-term stable operation of the valve. In the performance test after molding, the present invention covers the corrosion resistance, gas A comprehensive evaluation of the tightness and adjustment accuracy, through a strict testing process, ensures the stable operation of the valve under micro-pressure conditions, meeting the requirements of different application fields, especially in the micro-pressure regulation of highly corrosive media such as chemical and pharmaceutical industries. Finally, the optimization of the overall process has significantly improved the working stability and reliability of the valve. The preheating step using far-infrared or resistance heating ensures the uniform melting of fluoroplastic powder, thereby effectively improving the overall performance of the valve. This series of process improvements has not only made a major technical breakthrough in the molding method of the fully lined fluorine self-operated micro-pressure regulating valve, but also provided more efficient and safe micro-pressure regulation solutions for related industries. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] FIG1 is a schematic flow chart of the steps of a molding method of a fully fluorine-lined self-operated micro-pressure regulating valve proposed by the present invention; FIG. 2 is a schematic diagram of the fluorine lining process of a fully fluorine-lined self-operated micro-pressure regulating valve molding method proposed by the present invention. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0018] Please refer to Figures 1-2, the present invention provides a technical solution, which specifically includes the following embodiments:
[0019] Example: A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve comprises the following steps: S1: Provide a metal valve body, which is made of high-pressure resistant materials and has a preset micro-pressure adjustment structure. The metal valve body is the basic component of the regulating valve, and its main function is to withstand the pressure during operation and maintain the stability of the fluid passing through. The metal valve body must be made of high-pressure resistant materials, such as stainless steel, carbon steel and other metal materials, with high mechanical strength and corrosion resistance. When designing the metal valve body, it is necessary to ensure that the preset micro-pressure adjustment structure meets the use requirements, such as the shape of the valve chamber, the layout of the channel and the accuracy of the sealing surface, so that the subsequent adjustment function can operate normally; S2: Surface pretreatment of the metal valve body, including ultrasonic cleaning and chemical polishing of the inner cavity of the valve body, to enhance the adhesion between the fluoroplastic and the metal surface. In order to enhance the adhesion between the fluoroplastic and the metal valve body, the inner cavity of the valve body must be strictly pretreated. First, ultrasonic cleaning technology is used to remove impurities, oil stains and tiny particles attached to the metal surface to ensure the surface is clean. Ultrasonic cleaning uses the action of high-frequency sound waves in the liquid to produce a strong cavitation effect in the liquid, which peels off the pollutants attached to the surface. Subsequently, chemical polishing is performed, using acidic or alkaline solutions to further clean and smooth the metal surface. This step improves the adhesion between the contact surface of the fluoroplastic and the metal, ensuring that the subsequent fluorine lining layer is more stable and durable; S3: Preheat the metal valve body to a temperature range of 200 °C to 250 °C. Before the fluorine lining operation, the metal valve body must be preheated to a temperature range of 200 °C to 250 °C. The purpose of this step is to make the metal valve body reach a temperature that matches the melting temperature of the fluoroplastic powder, thereby ensuring that the fluoroplastic powder can be evenly melted and attached to the metal surface. Preheating can be performed by far-infrared heating or resistance heating. The temperature must be strictly controlled to avoid excessively high or low temperatures that affect the subsequent fluorine lining effect. S4: The inner surface of the preheated metal valve body is lined with fluorine by a multi-layer progressive fluorine lining process. The multi-layer progressive fluorine lining process includes electrostatic spraying of fluoroplastic powder and melting it multiple times until the thickness required by the design is reached. The inner surface of the preheated metal valve body is lined with fluorine by a multi-layer progressive fluorine lining process. This process uses electrostatic spraying to evenly attach fluoroplastic powder to the metal surface, and uses the electric field force to adsorb the fluoroplastic powder to the preheated metal surface. After each layer of fluoroplastic powder is melted, it needs to be repeated many times until the fluorine lining layer reaches the thickness required by the design. Compared with one-time spraying, the multi-layer spraying process can effectively avoid bubbles, gaps or weak areas on the surface, ensure that the fluorine lining layer on the entire valve body surface is uniform and dense, and improve the corrosion resistance of the valve; S5: Pulse cooling technology is used to control the cooling process to avoid the generation of internal stress in the fluoroplastic layer. After the fluoroplastic lining operation is completed, the metal valve body and the fluoroplastic lining need to be cooled. In order to avoid the generation of internal stress in the fluoroplastic layer during the cooling process, pulse cooling technology is used. This technology controls the flow rate and temperature of the cooling medium in sections to gradually cool the metal valve body to avoid the accumulation of internal stress and cracking of the fluoroplastic lining layer caused by rapid temperature changes. The cooling medium can be gas or liquid, and the cooling method is adjusted according to the different metal valve body materials and working environments to ensure uniform and stable cooling; S6: Assemble valve components, including key components such as regulating structure, sealing device and micro-pressure regulating device, ensure that they are coordinated with the molding process of the fluorine lining layer to form a complete micro-pressure regulating valve structure. After cooling, assemble all valve components. Including seals, micro-pressure regulating devices, etc. After assembly, perform performance tests on the regulating valve, including corrosion resistance test, air tightness test, high temperature performance test, etc., to ensure that the valve can work normally in the designed working environment and maintain stable regulating function under corrosive media, micro-pressure environment and high temperature conditions; S7: Perform performance tests on the molded control valve, including corrosion resistance, air tightness and regulation accuracy tests, to ensure stable operation under micro-pressure conditions; The multi-layer progressive fluorine lining process uses electrostatic spraying to evenly attach fluoroplastic powder to the metal surface through electric field force to form a fluorine lining layer; electrostatic spraying is an advanced spraying technology that evenly adsorbs charged fluoroplastic powder on the surface of the metal valve body through electric field force. The electrostatic spraying process can make fluoroplastic powder form a uniform coating on the metal surface and can cover the inner cavity and surface of complex shapes. Under the action of electric field force, the powder material can adhere more closely to the metal surface, avoiding the accumulation or unevenness of powder in traditional spraying methods.
[0020] The material of the fluorine lining layer is polytetrafluoroethylene, and its spraying thickness is controlled between 0.1mm and 0.2mm; polytetrafluoroethylene has excellent corrosion resistance and high temperature resistance, and is often used in chemical, pharmaceutical and other occasions that require corrosion protection. The thickness of the fluorine lining layer is very important. Controlling it within the range of 0.1mm to 0.2mm can ensure that the fluoroplastic has sufficient protection and will not affect the micro-pressure regulation function of the metal valve body. Too thick or too thin a coating may cause performance problems, so strict thickness control is the key to ensuring product quality.
[0021] The pulse cooling technology controls the flow rate and temperature of the cooling medium in stages to maintain low internal stress during the cooling process. The temperature change during the cooling process directly affects the internal stress accumulation of the fluorine lining layer. The pulse cooling technology controls the temperature and flow rate of the cooling medium in stages to make the temperature difference between the metal valve body and the fluorine lining layer change smoothly. This can prevent stress concentration and cracking of the fluoroplastic layer caused by rapid cooling. The segmented controlled cooling can also reduce the tension between materials with different thermal expansion coefficients, making the entire fluorine lining layer more stable.
[0022] The cooling medium is a combination of gas cooling or liquid cooling. The flow rate and temperature of the cooling medium are adjusted according to the material of the metal valve body. According to the material characteristics of the metal valve body, a suitable cooling medium is selected to cool it. Gas cooling can quickly take away heat and is suitable for mild cooling; liquid cooling is suitable for a more precise and uniform cooling process. Through the combination of the two, an ideal cooling effect can be achieved while maintaining the controllability of the cooling speed to prevent local stress or thermal deformation during the cooling process.
[0023] The surface pretreatment step of the metal valve body uses a combination of ultrasonic cleaning and chemical polishing to remove tiny particles and oil stains on the metal surface; ultrasonic cleaning can effectively remove tiny particles, oil stains and oxides attached to the metal surface through the cavitation effect produced by sound wave vibration in the liquid. Chemical polishing further makes the metal surface smoother, providing a good foundation for the adhesion of fluoroplastics. Through the combination of these two processes, the surface treatment effect of the metal valve body is better, the bonding force between fluoroplastics and metal is also stronger, and the risk of coating shedding is avoided.
[0024] The solvent used in chemical polishing is an acidic or alkaline solution. Depending on the characteristics of different metal materials, chemical polishing can be treated with acidic or alkaline solutions. Acidic solutions are suitable for treating corrosion-resistant materials such as stainless steel, while alkaline solutions are suitable for aluminum or other non-ferrous metal materials. Through chemical polishing, the roughness of the metal surface is greatly reduced, thereby achieving the effect of enhancing the adhesion of fluoroplastics and reducing microcracks.
[0025] The preheating step adopted is to make the surface of the metal valve body reach the required temperature through far-infrared heating or resistance heating, so that the fluoroplastic powder can be evenly melted and attached to the metal surface; the preheating is to make the surface of the metal valve body reach the temperature range suitable for the melting of fluoroplastic powder. Both far-infrared heating and resistance heating can transfer heat to the metal surface evenly, ensuring that the fluoroplastic powder can be evenly melted and attached to the metal surface. Far-infrared heating has the characteristics of strong penetration and fast heating, and is suitable for larger metal structures, while resistance heating has better temperature control accuracy and is suitable for small valve bodies with complex shapes.
[0026] The melting operation in the fluorine lining process is carried out through a layer-by-layer heating and cooling cycle. Each layer of fluoroplastic is partially cooled after melting to reduce the stress accumulation between layers. In the fluorine lining process, each layer of fluoroplastic powder is partially cooled after melting, and then the next layer is heated and melted. This layered melting and cooling cycle process can effectively reduce the stress accumulation between layers and prevent the fluorine lining layer from cracking or separation due to differences in thermal expansion coefficients or uneven cooling.
[0027] After the fluorine lining operation is completed, the entire valve surface is subjected to corrosion resistance test and high temperature test; the last step is to conduct strict performance test on the entire valve, especially the corrosion resistance test and high temperature test under harsh working conditions. These tests can simulate the actual use environment to ensure that the valve can maintain stable working performance for a long time in corrosive media or high temperature environment. The valve can be put into use only after passing the test.
[0028] During operation, the metal valve body is made of high-pressure resistant material and is pre-treated with ultrasonic cleaning and chemical polishing to remove tiny particles and oil stains on the inner surface, thereby improving the adhesion between the fluoroplastic and the metal surface. The pre-treated metal valve body is heated to a suitable temperature range of 200°C to 250°C to prepare for the subsequent fluorine lining process. In the fluorine lining process, a multi-layer progressive fluorine lining process is adopted. The fluoroplastic powder is evenly attached to the inner surface of the metal valve body by electrostatic spraying. The electrostatic spraying method uses the effect of electric field force to enable the fluoroplastic powder to be evenly covered on the metal surface, avoiding the uneven thickness of the fluorine lining layer and the generation of weak areas. Through layer-by-layer heating and melting, each layer of fluoroplastic is partially cooled after melting, reducing the accumulation of internal stress between the layers, thereby improving the stability and durability of the fluorine lining layer. In order to further optimize the cooling process, the present invention adopts pulse cooling technology to control the flow rate and temperature of the cooling medium in sections to ensure that the fluoroplastic does not produce excessive temperature gradients during cooling. To avoid internal stress accumulation or cracking of the fluorine lining layer caused by rapid cooling, the cooling medium can be selected as a combination of gas cooling or liquid cooling according to the material of the metal valve body, and precisely adjusted, thereby effectively reducing the stress that may be generated during the cooling process. After the fluorine lining process is completed, the entire valve undergoes corrosion resistance testing and high temperature testing to ensure its performance stability and reliability under extreme working conditions. This molding method not only improves the corrosion resistance of the valve, but also improves the accuracy and stability of micro-pressure regulation. It is suitable for micro-pressure regulation scenarios in corrosive media such as chemicals and pharmaceuticals.
[0029] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the application should be included in the protection scope of the present application.
Claims
1. A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve, characterized in that: The following steps are involved: S1: Provide a metal valve body, which is made of high-pressure resistant material and has a preset micro-pressure regulating structure; S2: Surface pretreatment of the metal valve body, including ultrasonic cleaning and chemical polishing of the inner cavity of the valve body, to enhance the adhesion between the fluoroplastic and the metal surface; S3: Preheat the metal valve body to a temperature range of 200 °C to 250 °C; S4: performing a fluorine lining operation on the inner surface of the preheated metal valve body through a multi-layer progressive fluorine lining process, wherein the multi-layer progressive fluorine lining process includes electrostatically spraying fluorine plastic powder and melting it multiple times until the thickness required by the design is reached; S5: Pulse cooling technology is used to control the cooling process to avoid the generation of internal stress in the fluoroplastic layer; S6: Assemble valve components, including key components such as regulating structure, sealing device and micro-pressure regulating device, to ensure coordination with the molding process of the fluorine lining layer to form a complete micro-pressure regulating valve structure; S7: Perform performance tests on the molded control valve, including corrosion resistance, air tightness and regulation accuracy tests, to ensure stable operation under micro-pressure conditions.
2. According to claim 1, a method for forming a fully fluorine-lined self-operated micro-pressure regulating valve is characterized in that: the multi-layer progressive fluorine-lined process adopts an electrostatic spraying method to uniformly adhere fluorine plastic powder to the metal surface through electric field force to form a fluorine-lined layer.
3. A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 2, characterized in that the material of the fluorine-lined layer is polytetrafluoroethylene, and its spraying thickness is controlled between 0.1 mm and 0.2 mm.
4. A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 1, characterized in that: the pulse cooling technology maintains low internal stress during the cooling process by controlling the flow rate and temperature of the cooling medium in sections.
5. A method for forming a fully lined fluorine self-operated micro-pressure regulating valve according to claim 4, characterized in that: the cooling medium is a combination of gas cooling or liquid cooling, and the flow rate and temperature of the cooling medium are The degree is adjusted according to the material of the metal valve body.
6. A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 1, characterized in that: in the surface pretreatment step of the metal valve body, a combined process of ultrasonic cleaning and chemical polishing is used to remove tiny particles and oil stains on the metal surface.
7. The method for forming a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 1, characterized in that: The solvent used in the chemical polishing is an acidic or alkaline solution.
8. A method for forming a fully lined fluorine self-operated micro-pressure regulating valve according to claim 1, characterized in that the preheating step adopts far-infrared heating or resistance heating to make the surface of the metal valve body reach the required temperature, so that the fluoroplastic powder can be uniformly melted and adhered to the metal surface.
9. A method for forming a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 1, characterized in that the melting operation in the fluorine-lined process is carried out through a layer-by-layer heating and cooling cycle, and each layer of fluoroplastic is partially cooled after melting to reduce stress accumulation between layers.
10. A molding method for a fully fluorine-lined self-operated micro-pressure regulating valve according to claim 1, characterized in that: after the fluorine-lined operation is completed, the entire valve surface is subjected to a corrosion resistance test and a high temperature test.
Citation Information
Patent Citations
High-precision valve resistant to abrasion and corrosion and manufacturing method thereof
CN104006198A
Wear-resisting processing process for valve for instrument
CN107722775A
Metal expansion joint inner surface FEP electrostatic powder spraying process
CN110280469A
Metal expansion joint inner surface ECTFE static powder spraying technology
CN110496766A
Electrostatic spraying process for fusible polytetrafluoroethylene anticorrosive coating of chemical equipment
CN112742680A
Cited By
High-temperature-resistant fluorine-lined valve and treatment process thereof
CN121339021A