High voltage transistor using buried insulating layer as gate dielectric
By using embedded insulating layer as gate dielectric material and substrate material as gate electrode material in semiconductor devices, the compatibility problem of high-voltage transistors and small-signal transistors is solved, process complexity and manufacturing cost are reduced, and the process is complex and manufacturing cost is realized. Improved compatibility and integration density between high-voltage transistors and small-signal transistors.
Patent Information
- Application Number
- CN202411155902.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2017-07-12
- Filing Date
- 2018-07-11
- Publication Date
- 2024-11-29
AI Technical Summary
In semiconductor devices, the manufacturing process of high voltage transistors requires major modifications to meet high voltage requirements, resulting in increased manufacturing costs and difficulty in compatibility with small signal transistors on the same chip.
Using an embedded insulating layer as the gate dielectric material and the substrate material below it is used as the gate electrode material, reducing the dependence on the traditional gate electrode structure, thereby achieving compatibility between high-voltage transistors and small-signal transistors.
Through this method, process complexity and manufacturing cost are reduced, the possibility of integrating high-voltage and small-signal transistors on the same chip is realized, and the integration density and functionality are improved.
Smart Images

Figure CN119050141A_ABST
Abstract
Description
[0001] This application is a divisional application of the Chinese patent application with Chinese patent application number 201810756784.9, invention name “High voltage transistor using buried insulating layer as gate dielectric”, and application date July 11, 2018. Technical Field
[0002] The present disclosure generally relates to semiconductor devices and fabrication techniques to provide transistor elements formed based on semiconductor or silicon-on-insulator (SOI) architectures. Background Art
[0003] Due to the continuous reduction of the critical dimensions of field effect transistors, significant progress has been achieved in the field of semiconductor devices. In recent developments, the critical dimensions of transistor elements have reached 30 nanometers or even less in complex planar device architectures, thereby achieving extremely high integration densities and thus providing the possibility of integrating more and more functions in a single integrated circuit. The continuous reduction of the critical dimensions (such as gate length) of complex field effect transistors generally involves specific challenges that must be solved to achieve appropriate functions of the field effect transistors with reduced dimensions. Some of these negative effects of the continuous reduction of the gate length of complex field effect transistors involve capacitive coupling between the conductive channel formed under the gate electrode structure, the parasitic capacitance of the remaining transistor body relative to the gate electrode structure, thereby increasing static and dynamic leakage currents into and through the very thin gate dielectric material, etc. For example, the problem of reduced capacitive coupling of the gate electrode structure to the channel region has led to a continuous reduction in the physical thickness of the gate dielectric material to increase the capacitive coupling, which, on the other hand, may significantly contribute to an increase in leakage current into and through the thin gate dielectric material. Therefore, complex material systems and fabrication techniques have been developed to introduce high-k dielectric materials into the gate dielectric material to achieve physical thicknesses suitable to maintain leakage current at acceptable levels while further reducing the electrical thickness or oxide equivalent thickness formed thereby.
[0004] In order to further enhance the overall controllability of the channel region of highly miniaturized field effect transistors, in recent developments, the problem of inevitable dopant fluctuations in the channel region having a length of about 30 nanometers and significantly less can be solved by further reducing the dopant concentration in the channel region, thereby also reducing the probability of scattering events and thus increasing the overall velocity of carriers in the channel region. In this context, it has been recognized that a fully depleted transistor body region (that is, the channel region and any area in the vicinity thereof substantially does not contain migrating carriers at 0V applied to the gate electrode structure) can provide superior transistor performance, especially in terms of overall channel controllability. A fully depleted transistor configuration can be achieved by using an extremely thin semiconductor material to implement the channel region therein (e.g., an extremely thin silicon material, a silicon / germanium material, etc.), thereby obtaining the desired fully depleted state in combination with no or extremely low dopant concentration in this extremely thin semiconductor material.
[0005] Furthermore, in at least some aspects, transistor performance may also be increased by using an SOI architecture (i.e., an architecture in which a buried insulating material is formed below a corresponding active semiconductor material). Thus, complex circuit designs have been developed based on fully depleted planar transistor elements formed based on an SOI architecture, wherein even for highly complex transistor elements having critical dimensions of 30 nanometers and significantly smaller, higher switching speeds of transistors may be achieved in combination with lower power consumption. Thus, even highly complex control circuits may be implemented in a corresponding circuit design, wherein even complex stand-alone devices may have any such complex circuits due to lower power consumption.
[0006] Since fully depleted transistor configurations in planar transistor architectures are essentially used to implement highly complex circuits in a single semiconductor chip, transistor elements that operate at higher voltages are also required compared to complex fully depleted transistor elements for small signal applications. That is, these complex small signal transistors are typically operated at a supply voltage of about 2V or even less to reduce static and dynamic leakage currents and thus reduce power consumption, thereby also providing the possibility of reducing the physical thickness of the corresponding gate dielectric material, which may need to be reduced to maintain the desired degree of channel controllability even when complex high-k dielectric materials are used, as described above. Therefore, when implementing additional functions in an integrated circuit chip, such as radio frequency (RF) components with corresponding output stages, charge pumps, or any other power devices that may have to operate at about 5V and significantly higher voltages (e.g., 10 to 50V and higher), corresponding high voltage transistors must be implemented in specific device areas of the corresponding integrated circuit chip. Although the respective high voltage transistors can essentially be formed on separate substrates according to separate manufacturing strategies and can subsequently be transferred to another substrate (which carries the complex small signal transistor elements), the results show that such process strategies may still significantly affect the overall manufacturing costs and may therefore make such approaches less than ideal.
[0007] In other methods, the corresponding high-voltage transistor elements can be formed together with the complex small-signal transistors, however, major modifications are required to meet the requirements for forming reliable high-voltage transistors. For example, the patterning of the corresponding gate electrode structure may have to be performed based on different strategies, because in addition to the different gate lengths of the complex small-signal transistors and the high-voltage transistors, in particular, for the high-voltage transistors, the physical thickness of the gate dielectric material is required to be significantly increased. Therefore, the patterning of the gate dielectric material may have to be performed in two different sequences to provide a commonly used high-k dielectric material stack for complex small-signal transistors and a corresponding high-voltage gate dielectric material, such as a silicon dioxide material, with a sufficient physical thickness to meet the voltage requirements of the high-voltage transistors. Therefore, a lot of efforts have been made to implement a fully depleted transistor architecture for high-voltage transistors or to try to use a specific architecture of an SOI device to implement the corresponding high-voltage transistor, for example, by using a buried insulating material as a gate dielectric layer.
[0008] For example, U.S. Pat. No. 7,939,395 describes a semiconductor device in which a buried insulating layer can be used as a gate dielectric material, wherein a gate electrode is formed in an "active" semiconductor layer above the buried insulating layer, and a drain region and a source region are formed in a silicon substrate material. To this end, a first contact region is formed to extend through the buried silicon dioxide layer and connect to a highly doped drain region, while a second contact region is formed through the buried insulating layer and connects to a highly doped source region.
[0009] U.S. Patent No. 7,745,879 relates to a fully depleted silicon-on-insulator field effect transistor based on an SOI architecture and a corresponding manufacturing technology, wherein a thin silicon layer can be used to set a drain region including a lightly doped region, which can be regarded as a drift region, providing a large length to allow a corresponding voltage drop. Moreover, a channel region is located between the drift region and the source region, and a gate electrode structure with a suitable configuration (that is, a gate dielectric material with an appropriate size design) is located above the channel region and also connects a carrier recombination element.
[0010] U.S. Patent No. 7,151,303 relates to an access transistor for a memory device having superior robustness against radiation or particle induced carrier generation, wherein a fully depleted state can be obtained by providing a specially doped gate electrode. That is, in this concept, a gate electrode material having an inverse doping compared to the drain-source doping can be used to obtain a fully depleted state in the channel region.
[0011] Due to the considerable effort invested in providing high voltage transistors in SOI configurations, it has been shown that significant modifications may still have to be implemented compared to mature processes for forming complex fully depleted small signal transistors, thereby adding significant additional cost to such devices formed according to known strategies.
[0012] In view of the above, the present disclosure relates to semiconductor devices and manufacturing techniques, wherein it is possible to provide field effect transistors based on SOI architecture according to a fully depleted transistor configuration while avoiding or at least mitigating the effects of the above problems. Summary of the invention
[0013] A brief summary of the disclosure is provided below to provide a basic understanding of some aspects of the present invention. The present disclosure is not intended to be an exhaustive overview of the present invention. It is not intended to identify key or important elements of the present invention or to delimit the scope of the present invention. Its sole purpose is to provide some concepts in simplified form as a prelude to a more detailed description discussed later.
[0014] In general, the present disclosure is based on the concept that a buried insulating layer of a semiconductor device can be advantageously used as a gate dielectric material, wherein any substrate or bulk material formed below the buried insulating material can be effectively used as a gate electrode material. Thus, in such device configurations, a "standard" gate electrode structure formed above the corresponding semiconductor material may no longer be required.
[0015] In some aspects disclosed herein, the semiconductor layer formed above the buried insulating layer (which may serve as a gate dielectric material) may be configured to have a thickness suitable for obtaining a fully depleted state in the channel region, thereby providing advantages associated with a fully depleted transistor configuration, such as reduced parasitic capacitance, superior controllability of the channel region, high carrier mobility due to a reduced number of scattering centers, an overall reduction in dopant fluctuations when considering transistor length reductions, etc. Moreover, by using an extremely thin initial semiconductor layer (e.g., which may also be used for complex fully depleted small-signal transistor elements), a high degree of compatibility with respect to process technology may be achieved, resulting in a reduction in overall manufacturing costs.
[0016] Furthermore, when such fully depleted transistor elements are formed in combination with fully depleted small signal transistor elements within a single semiconductor chip, a significant increase in overall functionality can be achieved, particularly because the thicker buried insulating material can allow the physical thickness of the gate dielectric material to be increased, which can therefore allow operation of any such transistor element at an elevated supply voltage. Thus, corresponding circuit portions requiring transistors with high operating voltages can be formed based on the fully depleted transistor architecture with high compatibility with configurations and processes relative to fully depleted small signal transistors. Thus, superior design flexibility combined with enhanced functionality at increased integration density can be achieved, since any such high voltage transistor element can be implemented in any desired device area, thereby making it possible to form small signal transistors and high voltage transistors in adjacent device areas.
[0017] According to an example embodiment disclosed herein, a semiconductor device includes a channel region located in a semiconductor layer. Furthermore, a drain region and a source region are located on the semiconductor layer to laterally connect the channel region. The semiconductor device also includes a buried insulating layer, which includes a portion located below the channel region. In addition, the semiconductor device includes a doped region located below the buried insulating layer connected to a gate contact region, wherein the portion of the buried insulating layer and the doped region form a gate electrode structure of a transistor element.
[0018] According to another example embodiment disclosed herein, a transistor element includes a channel region between a drain region and a source region. Furthermore, the transistor element includes a portion of a buried insulating layer located below at least the channel region. Furthermore, the transistor element includes a doped semiconductor region located below the portion of the buried insulating layer and connected to a control terminal, wherein the portion of the buried insulating layer and the doped semiconductor region form a gate electrode structure.
[0019] According to another example embodiment disclosed herein, a method is provided. The method includes forming a gate electrode structure of a transistor element by doping a portion of a substrate material of a semiconductor substrate below a portion of a buried insulating layer. The method also includes forming a drain region and a source region on a semiconductor layer formed on the buried insulating layer. In addition, the method includes forming an interlayer dielectric material between the drain region and the source region. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The present disclosure may be understood by reference to the following description taken in conjunction with the accompanying drawings, in which like reference numerals represent like elements, and in which:
[0021] Figure 1A and Figure 1B Schematically showing a cross-sectional view and a top view of a transistor element having a gate electrode structure formed based on a buried insulating material and an electrode material located below the buried insulating layer according to an exemplary embodiment;
[0022] Figure 1C and Figure 1D A cross-sectional view and a top view of another transistor element are schematically shown, respectively, including a gate electrode structure formed based on a buried insulating material and a doped substrate material formed below the buried insulating layer, wherein Figure 1A and Figure 1B A reduced parasitic capacitance is obtained compared to a transistor element of FIG. 1 ; and
[0023] Figures 2A to 2L The schematic diagram shows a cross-sectional view of a semiconductor device during different manufacturing stages, wherein a transistor element can be formed based on a gate electrode structure formed by a buried insulating material and a substrate material located thereunder, and a complex small signal transistor can be formed based on a manufacturing flow with high process compatibility.
[0024] Although the inventive subject matter disclosed herein is susceptible to various modifications and alternative forms, specific embodiments of the inventive subject matter are shown by way of example in the drawings and described in detail herein. However, it should be understood that the description of specific embodiments herein is not intended to limit the invention to the specific forms disclosed, but rather is intended to cover all modifications, equivalents and alternatives falling within the spirit and scope of the invention as defined by the appended claims. DETAILED DESCRIPTION
[0025] Various example embodiments of the present invention are described below. For purposes of clarity, not all features of an actual implementation are described in this specification. Of course, it should be understood that in the development of any such actual embodiment, a large number of specific implementation decisions must be made to achieve the developer's specific goals, such as meeting system-related and business-related constraints, and these decisions will vary from implementation to implementation. Moreover, it should be understood that such development efforts may be complex and time-consuming, but they are still routine procedures performed by ordinary technicians in the field with the help of this disclosure.
[0026] The present disclosure will now be described with reference to the accompanying drawings. Various structures, systems and devices are illustrated in the drawings only for the purpose of explanation and to avoid confusing the present disclosure with details known to those skilled in the art, but the drawings are still included to illustrate and explain examples of the present disclosure. The meaning of the words and phrases used herein should be understood and interpreted as consistent with the understanding of these words and phrases by those skilled in the relevant art. The coherent use of the terms or phrases herein is not intended to imply a special definition, that is, a definition that is different from the usual customary meaning understood by those skilled in the art. If a term or phrase is intended to have a specific meaning, that is, a meaning different from that understood by those skilled in the art, such a special definition will be clearly expressed in the specification in a definition manner that directly and clearly provides a specific definition of the term or phrase.
[0027] The present disclosure is based on the concept that field effect transistors (which may require gate dielectric materials having increased physical thickness) can be formed based on the buried insulating layer portion of the SOI device to avoid any of the numerous additional processes and material systems typically associated with the formation of gate dielectric materials having different material compositions and / or different thicknesses. Furthermore, it has been recognized that, in order to maintain a high degree of compatibility with many existing CMOS process strategies, the substrate material or bulk material located below the buried insulating layer can be used as the gate electrode material, so that in some example embodiments, the overall control mode for operating the corresponding transistor element can be provided as a "buried" gate electrode structure, which can also be referred to as a gate-last electrode structure, wherein the implementation of the buried gate electrode structure can be achieved with reduced overall process complexity. In some example embodiments, for example, by using thinner semiconductor materials in conjunction with the corresponding buried insulating layer (in and above which the corresponding "standard" complex field effect transistor can be formed), a high degree of compatibility with complex process technologies used to form fully depleted SOI transistors for small signal or low power applications can be achieved. In some exemplary embodiments, transistor elements utilizing a buried insulating layer as a gate dielectric material (also referred to herein as high voltage transistor elements due to the thicker gate dielectric material) may be formed together with low power or small signal transistor elements within the same semiconductor chip, thereby providing the possibility of extending functionality to complex SOI device integration formed based on fully depleted transistor elements. In other cases, the corresponding high voltage transistor elements may be formed with or without any additional small signal transistors, depending on the overall circuit and device requirements.
[0028] Figure 1A Schematically shows a cross-sectional view of a semiconductor device 100 including a transistor element (also referred to as a high voltage transistor 150) according to an exemplary embodiment. The semiconductor device 100 may include a substrate 101, which may be provided in the form of any suitable crystalline semiconductor material (e.g. silicon, silicon / germanium, germanium and the like). It should be understood that, due to cost considerations and due to the very mature process technology available in the context of silicon substrates, most complex integrated circuits are currently manufactured based on silicon substrates. In the sense used herein, the substrate material or substrate 101 will be understood to represent a crystalline semiconductor material of a substrate or carrier in and on which a corresponding semiconductor device is formed, while in other cases, the substrate 101 may represent only the upper part of any other suitable carrier material. In this case, the substrate material 101 may, for example, be provided in the form of a semiconductor layer having a specific thickness of 1 μm (micrometer) or more. It should also be understood that, depending on the overall configuration of the semiconductor device 100, the substrate 101 may be divided laterally (that is, in a horizontal direction and in a direction perpendicular to the illustrated plane of FIG. 1 ) into specific device areas.
[0029] For example, the transistor element 150 as shown may be located in a device region where a plurality of corresponding high-voltage transistor elements may be required, without including any other transistor elements therein, such as low-power transistors, etc. In other cases, the transistor 150 may be formed in conjunction with a low-power transistor in a corresponding transistor region to establish a desired functional behavior of at least a portion of the semiconductor device 100. In other cases, the functional behavior of a specific device region of the semiconductor device 100 may be obtained based on a plurality of transistors 150, while in other independent regions of the semiconductor device 100, different types of functional behaviors may be implemented without providing one or more of the transistors 150.
[0030] The semiconductor device 100 may also include isolation structures 102, 102A, which are formed to laterally delimit respective regions, such as transistor regions, etc. For example, the isolation structures 102 may be provided in the form of shallow trench isolations (which may or may not extend into the substrate region 101), that is, shallow trenches filled with any suitable dielectric material, such as silicon dioxide, silicon nitride, etc. In some example embodiments, in conjunction with the shallow trench isolation structures 102, "deep" isolation structures 102A may be provided to achieve superior lateral isolation of respective doped regions formed in the upper portion of the substrate material 101 in accordance with overall device requirements. In this regard, it should be noted that the "deep" isolation structures 102A may extend into the substrate material 101 to a depth of about 50 nanometers or more (e.g., 200 nanometers), but may not exceed a depth of several hundred nanometers, etc.
[0031] Furthermore, the semiconductor device 100 may include a buried insulating layer 122, which may represent a portion of a buried insulating material that may be initially disposed throughout the substrate 101 and may have been patterned in accordance with design requirements. In other cases, the buried insulating material 122 may be substantially disposed in specific device regions where an SOI architecture is desired, while in other device regions, a "bulk" configuration may have to be implemented. It should be understood that a configuration such as that shown in the context of the transistor 150 may be considered a hybrid configuration, since the buried insulating layer 122 may be located below the active semiconductor layer 103, while in the region 106, the buried insulating layer 122 may be removed, thereby providing direct access to the upper portion of the substrate material 101. Typically, a "deep" isolation structure 102A may define this "hybrid" region.
[0032] The semiconductor layer 103, for example, provided in the form of silicon, silicon / germanium, etc., may have a suitable thickness and dopant concentration required for the appropriate operating behavior of the transistor 150. In some example embodiments, the semiconductor layer 103 may have a thickness, material composition, and / or dopant concentration that supports a fully depleted transistor configuration. In this case, in some example embodiments, the thickness 131T of the semiconductor layer 103 (at least at the channel region 130 formed therein) may be about 15 nanometers or less. It is well known that in many complex semiconductor devices, corresponding thicknesses of active semiconductor materials (e.g., 15 nanometers and less, or even 10 nanometers and less) can be used to form complex fully depleted SOI transistor elements with gate lengths of 30 nanometers and less. Moreover, a source region 152 and a drain region 153 in the form of a highly doped semiconductor material are formed on the ends of the semiconductor layer 103, thereby laterally defining the channel region 130. Therefore, the source region 152 and the drain region 153 define a channel length 131L, wherein a conductive channel can be formed according to the specific conditions for operating the transistor 150. Channel length 131L may be selected depending on overall device requirements (eg, with respect to a desired voltage drop along channel region 130 when operating transistor 150 based on a desired supply voltage) and may substantially correspond to the gate length of a “standard” transistor element.
[0033] Conductive control in the channel region 130 may be achieved based on a "buried" gate electrode structure 120, which may include a buried insulating layer 122 formed below the semiconductor layer 103, an electrode material in the form of a doped semiconductor region 121 (which may represent a specific portion of the substrate material 101), and a gate contact region 123 (which may be provided in the form of a highly doped semiconductor material and may have a configuration similar to the drain region 153 and the source region 152 in terms of material composition and dopant concentration). For example, for an N-type transistor, the drain region 153 and the source region 152 may include a higher dopant concentration of an N-type dopant species, and the contact region 123 may also have a higher dopant concentration of an N-type species to connect to the doped region 121 (the doped region 121 may have a higher, but in some example embodiments, reduced, N-type dopant concentration compared to the contact region 123). However, it should be understood that the doping pattern in the gate electrode structure 120 may be selected according to other criteria, such as with respect to adjusting the threshold voltage of the transistor 150, so that for an N-type transistor even a P-doping species may be incorporated in the semiconductor region 121 and thus in the contact region 123, as deemed appropriate with respect to the desired operating behavior of the transistor 150. Moreover, for P-type transistor elements, as described above, the corresponding doping may be reversed, so that both N-type and P-type transistors having the basic geometrical configuration of the transistor 150 may be provided in the semiconductor device 100, if desired.
[0034] exist Figure 1AIn the manufacturing stage shown in , the semiconductor device 100 may also include a highly conductive metal semiconductor compound 154, such as a nickel silicide region, to further reduce the contact resistance of any semiconductor region in which the metal semiconductor compound 154 may be implemented. As shown, the metal semiconductor compound 154 may be formed on the outer upper portion of the drain region 153 and the source region 152 and the upper portion of the contact region 123. In this way, the contact resistance to the corresponding contact elements 105A, 105B and 105C may be reduced. The contact elements 105A, 105B, 105C in combination with one or more dielectric materials 104 may represent the contact level 105 of the semiconductor device 100, thereby providing contact to any circuit elements formed in the semiconductor level, and additional metallization levels (not shown) may provide electrical contact to each contact element in the contact level 105 depending on the overall circuit design.
[0035] Figure 1B The schematic diagram shows a top view of the semiconductor device 100, wherein the line IA represents Figure 1A The cross-section shown in . As shown in the figure, the transistor 150 is laterally embedded in the shallow trench isolation structure 102, and the shallow trench isolation structure is correspondingly surrounded by the "deep" isolation structure 102A. Moreover, the channel region 130 and the drain region 153 and the source region 152 and the contact region 123 are schematically shown, wherein, for convenience, it can be assumed that the contact level 105 does not exist or is transparent, however, the contact elements 105A, 105B, 105C are still marked in this figure. Moreover, for convenience, the doped semiconductor region, that is, the gate electrode material 121, is shown in dotted lines because this region is covered by the isolation structure 102, the channel region 130, the drain region 153 and the source region 152 and the contact region 123, also as shown Figure 1A As shown in the figure, the channel length 131L extends along the length direction L of the transistor 150, while the drain region 153 and the source region 152 extend along the width direction of the transistor, that is, along Figure 1B As described above, specific transistor characteristics can be adjusted based on the geometry of other given parameters, such as the thickness of the semiconductor layer 103 and the resulting channel region 130 (see Figure 1A ), the dopant concentration therein, the thickness of the “gate dielectric” (i.e., the buried insulating layer 122), the channel length 131L, and the corresponding width of the transistor 150. Thus, after applying a specific supply voltage to the source region 152 and the drain region 153 (which can be selected to be significantly higher than low-power transistors, which can be formed based on complex gate electrode structures with physical thicknesses of the corresponding gate dielectric of about 10 nanometers and significantly less), when a suitable control voltage is applied to the contact region 123, a conductive channel is formed in the channel region 130 between the source region 152 and the drain region 153.
[0036] like Figure 1A and Figure 1B The semiconductor device 100 shown in FIG. Figures 2A to 2L The manufacturing techniques are described in more detail.
[0037] Figure 1C Schematic display including comparison Figure 1A and Figure 1B 1 is a cross-sectional view of a semiconductor device 100 having a transistor 150A with a modified configuration. In this example embodiment, the transistor 150A may have substantially the same configuration except that Figure 1A and Figure 1B In addition to the reduced gate / drain and gate / source capacitances compared to the transistor 150, a doped semiconductor region 121A (serving as a gate electrode material) may be formed to extend along the length direction of the transistor (i.e., Figure 1C In other words, the doped semiconductor region 121A is embedded in the substrate material 101 to deviate from the isolation structure 102 by a certain distance, and the distance substantially corresponds to the lateral extension of the drain region 153 and the source region 152 along the length direction of the transistor. On the other hand, as Figure 1A As shown in FIG. 1 , at least in the vicinity of the buried insulating layer 122 , the doped semiconductor region 121 of the transistor 150 is laterally bounded by the isolation structure 102 . Figure 1A and Figure 1B Compared with the configuration of transistor 150, Figure 1C The transistor 150A may have reduced parasitic capacitance, thereby achieving increased switching speed.
[0038] Figure 1D Schematic display Figure 1C A top view of a semiconductor device 100, wherein line IC is shown as Figure 1C Furthermore, as shown in the figure, the channel length 131L extends along the length direction of the transistor, which is now Figure 1D On the other hand, the doping of region 121A is established so that the gate electrode material 121A is located below the channel region 130 at least along the transistor length direction L, and does not substantially extend into the drain region 153 and the source region 152, as described above with reference to Figure 1C Therefore, after applying the corresponding supply voltage and the appropriate control voltage to transistor 150A, for the same geometry (that is, Figure 1A and Figure 1B Compared with devices with the same transistor length and transistor width), a certain degree of increased switching speed can be achieved.
[0039] like Figure 1C and Figure 1DThe transistor 150A of the device 100 shown in FIG. 1 may be configured as described below with reference to FIG. Figures 2A to 2L The manufacturing technology described is formed.
[0040] Moreover, if Figure 1A and Figure 1C The transistors 150, 150A shown in the drawings may not have a specific device structure between the corresponding drain region 153 and the source region 152. That is, in these example embodiments, the one or more interlayer dielectric materials 104 of the contact level 105 may be formed to extend continuously between the drain region 153 and the source region 152 without any additional transistor-related structures. In other example embodiments, as described later, one or more additional components may be formed on or over the channel region 130 or a portion thereof, such as one or more material layers for adjusting transistor characteristics, dummy gate electrodes, possibly in combination with parameter adjustment materials, etc., as deemed appropriate for the overall device configuration.
[0041] Please refer to Figures 2A to 2L , further example embodiments will now be described, wherein the process technology is used to form a gate electrode structure (including a buried insulating layer and a doped semiconductor region formed below the buried insulating layer, such as described above with reference to Figures 1A to 1D The transistor element is formed.
[0042] Figure 2A The schematic diagram shows a cross-sectional view of a semiconductor device 200 including a first device region 200A and a second device region 200B. In the first device region 200A, a transistor may be formed, such as the one previously described with reference to FIG. Figures 1A to 1D The transistor 150 described above or any other transistor of a similar configuration in which a buried gate electrode structure is to be implemented. The second device region 200B may represent a portion of the semiconductor device 200 in which or over which a small signal or low power transistor may be formed. Thus, in some example embodiments, a low power transistor and a high voltage transistor element including a buried gate electrode structure may be formed in a common process within the same semiconductor device 200.
[0043] In the manufacturing stage shown, the semiconductor device 200 may include a substrate material 201, such as any suitable crystalline semiconductor material, such as silicon material, etc., as also described above with reference to Figures 1A to 1DThe buried insulating layer 222 may be formed in the first device region 200A and the second device region 200B and may include any suitable dielectric material such as silicon dioxide, silicon nitride, high-k dielectric material (if deemed appropriate), or any other material deemed suitable to provide sufficient physical thickness to ensure proper electrical isolation of the substrate material 201 relative to the semiconductor layer 203 formed on the buried insulating layer 222. For example, in some example embodiments, the buried insulating layer 222 may have a thickness of about 10 nanometers or more. For example, in some mature CMOS process technologies for forming fully depleted SOI low-power transistors, the buried insulating layer provided therein may have a thickness of about 20 nanometers. The semiconductor layer 203 in its initial state may represent any suitable semiconductor material, such as silicon, silicon / germanium, silicon / carbon, etc., depending on the specific requirements of the transistor device to be formed based on the semiconductor layer 203. In some example embodiments, the initial thickness 203T of the semiconductor layer 203 may be 15 nanometers and less. Furthermore, it should be appreciated that any aspects previously discussed in the context of semiconductor layer 103 of semiconductor device 100 may also be applicable to semiconductor layer 203 , as appropriate.
[0044] Furthermore, the isolation structures 202, 202A may be provided to laterally define respective regions in the first device region 200A and the second device region 200B. For example, the shallower isolation structures 202 may laterally define respective transistor regions, i.e., current flow regions, while the deeper trench isolation structures 202A may surround regions representing "mixed" regions, such as region 206, where the buried insulating layer 222 may be removed in a subsequent manufacturing stage to provide a direct connection to a portion of the substrate material 201.
[0045] like Figure 2AThe semiconductor device 200 shown in FIG. 1 can be formed based on the following process. After providing a substrate 201 (which may already include a buried insulating layer 222 and an initial semiconductor layer 203, and if necessary, the characteristics of these layers can also be adjusted, such as taking into account material composition, initial thickness, dopant concentration, etc., wherein any such modification can be performed locally or globally in the semiconductor device 200 as required), a process sequence can be applied to form the isolation structure 202, 202A. To this end, well-established oxidation, deposition and photolithography techniques can be applied, followed by a corresponding etching sequence, to form trenches in the semiconductor layer 203 and the buried insulating layer 222, which can extend into the substrate material 201 at a specific depth. Then, one or more suitable dielectric materials can be deposited and can be subsequently planarized by well-established process techniques. It should be understood that even after the corresponding process sequence, one or more protective layers (not shown) can still cover the semiconductor layer 203, if necessary. Furthermore, as already discussed, before or after forming the trench isolation structures 202, 202A, corresponding processes may be performed to adjust the initial thickness of the semiconductor layer 203 to any desired value, wherein, for example, the thickness 203T of the layer 203 in the first semiconductor region 200A may be adjusted to a greater thickness than the thickness of the semiconductor layer 203 in the second device region 200B (where low-power transistors may be formed). Similarly, other material properties such as initial dopant concentration (if non-intrinsic semiconductor materials are to be used), overall material composition, etc. may be appropriately adjusted based on corresponding masking techniques and processes such as implantation, epitaxial growth, etching processes, etc.
[0046] Figure 2B Schematically shows a cross-sectional view of a semiconductor device 200 in a next manufacturing stage. As shown, in the corresponding region 206, the initial semiconductor layer 203 and the buried insulating layer 222 can be removed to expose the surface 201S of the substrate material 201 of the corresponding mixed region in the first device area 200A and the second device area 200B. To this end, a suitable masking process can be performed by using photolithography and deposition techniques, followed by an etching process to etch through the materials 203, 222. Then, any etching mask can be removed. In addition, in this case, one or more optional protective layers can still be present on the semiconductor layer 203, as deemed appropriate. In other cases, after the opening is formed in the region 206 to expose the surface 201S, an additional protective layer or shielding layer can be formed, as deemed appropriate. For this purpose, any well-established deposition and / or oxidation recipe can be used.
[0047] Figure 2C Schematically shows a cross-sectional view of a semiconductor device 200 in a manufacturing stage in which a doped semiconductor region 221 is formed at least below a buried insulating layer 222 in a first device region 200A. Similarly, a doped region 201B may be formed in a second device region 200B. Figure 2CIn the embodiment shown in FIG. 2 , it is assumed that in the first device region 200A, the overall geometry of the transistor elements to be formed is equivalent to that of FIG. Figure 1B , so that the doped semiconductor region 221 can extend laterally along the entire length of the buried insulating layer 222 and be laterally bounded by the isolation structure 202. In other exemplary embodiments (not shown), the doped semiconductor region 221 can correspond to Figure 1D , so that along the length direction of the transistor, the doped semiconductor region 221 can extend along a portion of the buried insulating layer 222 and be laterally offset relative to the isolation structure 202, for example, as Figure 1C As shown in FIG. 1 , the doped semiconductor region 121A.
[0048] The doped semiconductor region 221 may represent the electrode material of a gate electrode structure consisting of a buried insulating layer 222 or a portion of this layer between a corresponding isolation structure 202 in the first device region 200A and a contact region to be formed in a region 206 of the first semiconductor region 200A, as previously described with reference to the semiconductor device 100. To this end, the dopant species introduced into the region 221 may have any suitable distribution to meet the requirements of threshold adjustment, overall conductivity, etc. For example, a relatively high concentration of N-type dopant species may be included, while in other cases, a doping pattern may be implemented in the doped region 221 along the depth direction (i.e., in the region 206). Figure 2C A generally gradient dopant profile in the vertical direction (in the middle, vertical direction) may be provided, as deemed appropriate. In other cases, a P-type dopant species may be included, depending on the desired overall transistor characteristics.
[0049] In some exemplary embodiments, when the same type of dopant species and the same type of dopant distribution can meet the requirements of the transistor to be formed in the second device area 200B, the doped semiconductor region 201B formed in the second device area 200B can have a configuration similar to the doped region 221. In other cases, the doped region 201B can be specially designed to meet the requirements of the transistor element in terms of providing a back bias control mechanism and a "standard" gate structure to be formed above the second device area 200B. It should be understood that additional doped regions can be provided in the first device area 200A and the second device area 200B as needed, for example, to electrically isolate the regions 221 and / or 201B from the substrate material 201, etc.
[0050] In general, the doped regions 221, 201B can be formed based on a suitable implantation sequence, including corresponding photolithography processes and masking techniques. For example, when a transistor element requiring a dopant distribution suitable for the doped semiconductor region 221 is to be formed in the second device region 200B, a corresponding implantation mask can be formed to expose the corresponding areas in the second device region 200B and the first device region 200A, so as to implant the corresponding dopant species. In other cases, the corresponding implantation process can be performed specifically for any type of transistor element to be formed in the first device region 200A and the second device region 200B, so that the corresponding implantation mask is required. In particular, when the doped semiconductor region 221 can be formed based on the same process recipe as one of the transistor types to be formed in and above the second device region 200B, no additional process steps are required to set the doped semiconductor region 221 in the first device region 200A compared to the standard process for forming transistors in the second device region 200B.
[0051] In other example embodiments (not shown), the references may be performed in a different order. Figure 2B and Figure 2C That is, one or both of the doped semiconductor regions 201B and 221 can be formed based on the above-mentioned process technology and then an opening 206 (see FIG. 2 ) for exposing the surface 201S can be formed. Figure 2B ).
[0052] Figure 2DSchematically showing a cross-sectional view of the semiconductor device 200 in the next manufacturing stage. As shown, a gate electrode structure 220B may be formed on the semiconductor layer 203 of the second device area 200B to meet the requirements of the low-power transistor element to be formed in the second device area 200B. For example, the gate electrode structure 220B may include a gate dielectric material 222B having any suitable configuration, wherein, in complex applications, the gate dielectric material 222B may include a high-k dielectric material, which is understood to be a dielectric material having a dielectric constant of 20 or higher. In this case, the metal-containing material 224 may be provided as a barrier material and / or a material for increasing the overall conductivity and / or adjusting the threshold voltage of the transistor to be formed. Moreover, the electrode material 221B, such as polysilicon, amorphous silicon, silicon / germanium, etc., or any combination thereof, may be provided together with a dielectric cap material 225, such as a silicon nitride material, etc. It should be understood that in complex semiconductor devices, the length of the gate electrode structure 220B may be in the range of 30 nanometers and significantly smaller, such as 28 nanometers, 22 nanometers, and smaller. It should also be understood that other transistor elements may still exist in the second device region 200B, which may have a different configuration relative to the transistor element to be formed based on the gate electrode structure 220B. For example, the gate electrode structure 220B may represent a gate electrode structure for an N-type transistor, while a similar gate electrode structure (not shown) may be used for a P-type transistor.
[0053] Moreover, in this manufacturing stage, a spacer material layer 226B may be formed above the semiconductor device 200, the material composition of which is suitable for forming a spacer element in the next process sequence. For example, the spacer layer 226B may be provided in the form of a silicon nitride material having a suitable thickness. Moreover, an etching mask 207, such as a resist material, etc., may be provided to cover any portion of the semiconductor device 200, and the spacer layer 226B will be maintained on any portion of the semiconductor device 200 during some additional process steps. In the example shown, it can be assumed that the spacer layer 226B may be exposed in other areas in the second device area 200B, wherein the side spacers will be formed on the corresponding gate electrode structure 220B (not shown), for example, a gate electrode structure of a transistor type having an opposite conductivity type compared to the transistor to be formed based on the gate electrode structure 220B as shown. Layers 226B and 207 may be formed based on mature process technologies, including deposition technologies, photolithography processes, etc. Next, an etching process may be performed to form sidewall spacers on any corresponding gate electrode structures not covered by the mask layer 207 in the second device region 200B. On the other hand, the spacer layer 226B is reliably covered by the mask layer 207 located on the first device region 200A and in corresponding regions of the second device region 200B (e.g., the region surrounding the gate electrode structure 220B as shown).
[0054] Figure 2E The semiconductor device 200 is schematically shown in a next manufacturing stage, wherein additional spacer material 226A may be formed to combine with previously formed and unremoved portions of the spacer layer 226B (see FIG. Figure 2D and not in Figure 2E 200A) to provide a desired overall thickness of the spacer material for forming the side spacers on the corresponding gate electrode structure. To this end, any mature deposition recipe can be applied to form, for example, silicon nitride material. In addition, a mask layer such as a resist material can be formed and patterned by photolithography to obtain a mask 208 located above the spacer layer 226A in the first device area 200A, thereby exposing portions corresponding to the drain region and source region to be formed in the first device area 200A.
[0055] Figure 2F The semiconductor device 200 is schematically shown in a manufacturing stage, in which the semiconductor device 200 is manufactured based on the Figure 2E The configuration shown in FIG. 1 may have been subjected to an etching process to remove the spacer layer 226A (see FIG. 2A ). Figure 2E ). Therefore, any uncovered gate electrode structure 220B in the second device region 200B may be provided with a corresponding spacer 226, while in other regions, including those covered by the mask 208 (see Figure 2E ), the previously formed spacer elements and a portion of layer 226A may still be present. Similarly, a portion of layer 226A (also indicated by the same reference numeral) may be disposed on semiconductor layer 203 in first device region 200A, thereby substantially defining the size, shape and position of channel region 230 in semiconductor layer 203. Figure 2F The configuration shown in FIG. 1 can be obtained based on a mature anisotropic etching recipe, followed by removal of the mask 208 (see FIG. Figure 2E ). Therefore, in this manufacturing stage, the corresponding drain and source regions of the low-power transistor to be formed in the second device area 200B can be exposed, while in other areas of the second device area 200B, the corresponding semiconductor regions can still be partially covered by the layer 226A. It should be understood that in Figure 2F In the configuration shown in FIG. , the drain region and the source region may be configured in accordance with the embodiment of the present invention. Figure 2F The transistor formed by the gate electrode structure 220B shown in FIG. 2 and the transistor to be formed in the first device region 200A are formed in a common process sequence. Therefore, a corresponding process or process sequence can be applied to prepare any exposed semiconductor surface area for deposition of high-position doped semiconductor material. For this purpose, any well-established process recipe can be applied.
[0056] Figure 2GThe schematic diagram shows a cross-sectional view of the semiconductor device 200 in the next manufacturing state. As shown in the figure, the drain region 253 and the source region 252 of the transistor 250 can be formed laterally adjacent to the spacer material 226A, wherein when the transistor 250 will represent an N-type transistor, the drain region 253 and the source region 252 can represent a highly doped semiconductor material, such as a highly N-doped semiconductor material. Similarly, in the region 206 of the first device area 200A, a contact region 223 formed of a highly doped semiconductor material is provided to connect to the doped semiconductor region 221. The contact region 223 is aligned with the drain region 253 and the source region 252 in terms of material composition and dopant concentration along the height direction (that is, Figure 2G vertical direction) can have basically the same configuration.
[0057] In the second semiconductor region 200B, the transistor 250B may include a gate electrode structure 220 including a spacer 226 previously formed based on the spacer material 226A, as described above, wherein a corresponding drain region 253B and a source region 252B may be formed adjacent to the gate electrode structure 220. Similarly, a contact region 223B may be formed in the corresponding region 206 to connect the doped region 201B. It should be understood that the drain region 253 and the source region 252 of the transistor 250 and the drain region 253B and the source region 252B of the transistor 250B may have substantially the same configuration, except for their lateral dimensions, because in the illustrated embodiment, it may be assumed that these regions and the corresponding contact regions 223, 223B may be formed based on a common selective epitaxial growth process. Moreover, other transistors located in the second semiconductor region 200B can be set up and can have basically the same configuration as the transistor 250B, except for the oppositely doped drain and source regions and corresponding contact regions, wherein the doped region located below the buried insulating layer 222 can also have inverse doping, as also described above.
[0058] Furthermore, in this manufacturing stage, additional sidewall spacers 227 may be formed on the gate electrode structure 220 and the raised drain region 253B and the source region 252B, wherein these sidewall spacers 227 may be formed of any suitable material, such as silicon dioxide, etc. In some exemplary embodiments, when it is desired to have superior integrity of the underlying semiconductor layer 203 after removing the spacer material 226A, the spacers 227 may also be selectively disposed on the sidewalls of the drain region 253 and the source region 252 and the contact region 223 of the transistor 250.
[0059] Figure 2G The semiconductor device 200 shown in FIG. 1 can be formed based on the following process. Figure 2FStarting with the configuration shown in , a selective epitaxial growth process can be performed to deposit crystalline semiconductor material on the exposed portions of the semiconductor layer 203 in the first device area 200A and the second device area 200B, while the semiconductor layer 203 in other device areas (not shown) of the second device area 200B can still be covered by the remaining portions of the material 226A. During the corresponding selective epitaxial growth process, suitable dopant species can also be introduced. Subsequently, any masked areas (not shown) still covered by the material 226A can be exposed by applying a corresponding selective etching process, wherein a further masking material, such as silicon nitride, can be deposited before performing the etching process and can be covered by a corresponding photolithography mask. After exposing the corresponding semiconductor regions and removing the photolithography mask, a further selective epitaxial growth process can be applied to deposit appropriate in-situ doped semiconductor materials to form corresponding drain and source regions (not shown). It should be understood that if the previously deposited drain regions 253, 253B and source regions 252, 252B are significantly different in material composition from the materials deposited in the subsequent epitaxial growth process, and thus effectively inhibit the deposition of a large amount of material on the previously formed drain regions and source regions, the coverage of these areas can be omitted.
[0060] Next, a spacer layer may be deposited and may be anisotropically etched to form spacer elements 227 in the second device region 200B and optionally in the first device region 200A.
[0061] Next, a sophisticated etching recipe may be applied to remove the silicon nitride capping layer 225 in the gate electrode structure 220 in the second device region 200B, thereby also removing the spacer material 226A in the first device region 200A, possibly in combination with any other silicon nitride-based masking material that may have been previously used to grow the corresponding semiconductor material of the drain region 253B and the source region 252B and the corresponding contact region 223B.
[0062] Figure 2H The semiconductor device 200 is schematically shown after the above-mentioned manufacturing sequence is completed. That is, the transistor 250 may include a drain region 253 and a source region 252 and a gate electrode structure 220, which is formed by a doped semiconductor region 221 as an electrode material, a buried insulating layer 222 as a gate dielectric, and a contact region 223 as a highly doped contact region to receive a control voltage to be applied to the doped semiconductor region 221. Moreover, in this manufacturing stage, since any mask material is previously removed, the semiconductor material of the channel region 230 may be exposed.
[0063] In the second device region 200B, the transistor 250B and any other transistors formed in the second device region 200B may include a gate electrode structure 220B, wherein the gate electrode structure 220B is formed by previously removing the capping material 225 (see FIG. Figure 2G), so that the electrode material 221B can be exposed. Therefore, in this manufacturing stage, the substantially completed transistor structure can be arranged in the first device area 200A and the second device area 200B, wherein, in some example embodiments, the small signal or low power transistor 250B located in the second device area 200B can have a fully depleted configuration, as described above. Similarly, in some example embodiments, the transistor 250 located in the first device area 200A can be configured as a fully depleted transistor element, wherein, for example, the channel region 230 can be appropriately adjusted in terms of dopant concentration, thickness, material composition, etc. to meet the specific requirements of the transistor 250. In particular, due to the increased physical thickness of the gate dielectric layer (i.e., the buried insulating layer 222), the transistor 250 is appropriately adjusted to operate based on a higher supply voltage, depending on the overall configuration of the transistor 250. It should be understood that a plurality of transistors 250 can be formed in the first device area 200A, wherein specific differences in configuration can be implemented when different types of high voltage transistors may be required. Moreover, it should be understood that the transistor 250 can have a configuration based on Figures 1A to 1D The configuration and characteristics are described in the context of the semiconductor device 100 shown and explained in .
[0064] Fig.2I The semiconductor device 200 is schematically shown in the next manufacturing stage. As shown, a mask layer 209, such as silicon nitride and the like, may be formed above the first device area 200A and the second device area 200B. For this purpose, any mature deposition technology may be applied. Moreover, an etching mask 210 may be formed in the first device area 200A to cover a portion of the transistor 250, thereby exposing the corresponding outer portions of the drain region 253 and the source region 252. The mask 210 may be formed based on any mature photolithography technology. Subsequently, any etching process may be performed based on a mature recipe to remove the exposed portion of the mask layer 209. For this purpose, a wet chemical etching recipe or a plasma assisted etching recipe may be used.
[0065] Figure 2J The schematic diagram shows the mask layer 209 after removal (see Fig.2I) and the semiconductor device 200 in the manufacturing stage where the photolithography mask 210 has also been removed. Therefore, the surface of the channel region 230 and the adjacent surface areas of the drain region 253 and the source region 252 can be reliably covered by a portion 209A of the previously patterned mask layer 209, while the outer surface areas 252S, 253S of the source region 252 and the drain region 253 are exposed. Subsequently, another process sequence can be applied to form a semiconductor metal compound in the exposed surface areas of the semiconductor material (such as the surface areas 252S, 253S) and any exposed semiconductor surface of the transistor (such as the transistor 250B in the second device area 200B). For example, nickel silicide can be formed when the corresponding exposed semiconductor surface area can include a large amount of silicon. To this end, mature deposition, annealing and etching processes can be applied to form the desired semiconductor metal compound, such as nickel silicide material.
[0066] Figure 2K The semiconductor device 200 is schematically shown after the above-described process sequence. That is, a metal-semiconductor compound region 254 with superior electrical conductivity is formed in and on the respective semiconductor surface region, wherein, in particular, in the transistor 250, the portion 209A of the mask material can reliably prevent the region 254 from being formed in the channel region 230. As a result, the respective contact regions of the transistors 250, 250B can have the respective metal-semiconductor compound 254 formed thereon, thereby providing superior contact resistance. Subsequently, further processing can be continued by forming a contact level according to a sophisticated process strategy.
[0067] It should be understood that at any appropriate time point during the entire process of the semiconductor device 200, corresponding thermal treatment, annealing process, etc. may be performed to meet the overall requirements such as activating dopant species, adjusting material properties, etc. For convenience, any such annealing process is not specifically described herein.
[0068] Figure 2L The schematic diagram shows a cross-sectional view of the semiconductor device 200 in a next manufacturing stage, in which a contact level 205 may be formed above the first device area 200A and the second device area 200B. As shown, the contact level 205 may include one or more dielectric materials 204, such as silicon nitride, silicon dioxide, etc., wherein for convenience, Figure 2L 205A-205F may be provided to connect the drain and source regions of transistor 250 and to contact region 223 (which represents the contact region of gate electrode structure 220, as previously described), and also to connect the drain and source regions of transistor 250B and to contact region 223B (which may be used to apply a suitable back bias voltage, if desired). It should also be appreciated that in some example embodiments, as Figure 2LAs shown in FIG. 1 , mask material 209A may also represent a portion of dielectric material 204, which may be disposed in first device region 200A. In this aspect, it should be noted that Figure 2L In the embodiment shown in , the dielectric material 204 including the mask material 209A can be formed between the drain region 253 and the source region 252 to extend continuously therebetween without any additional device structures therebetween. Figure 2L In the embodiment shown in , the dielectric materials 209A, 204 of the contact level 205 may extend between the drain region 253 and the source region 252 in an uninterrupted manner.
[0069] The contact level 205 may be formed according to a well-established process strategy, for example, including depositing one or more interlayer dielectric materials, such as silicon nitride, followed by silicon dioxide, etc., followed by appropriate planarization techniques as required. Subsequently, openings for the contact elements 205A to 205F may be formed based on photolithography and etching recipes, followed by depositing any appropriate conductive material and removing any excess material therefrom.
[0070] Therefore, the present disclosure provides semiconductor devices and manufacturing techniques, wherein transistors with increased breakdown voltage can be obtained based on SOI configurations, wherein a buried insulating layer can be used as a gate dielectric material, and a substrate material formed below the buried insulating layer can serve as a gate electrode material. In example embodiments, a fully depleted configuration can be achieved by appropriately selecting the characteristics of the channel region (e.g., considering thickness and / or dopant concentration), thereby improving controllability and carrier speed in the corresponding channel region. In some example embodiments, especially for fully depleted SOI transistors, a high degree of compatibility with process modes applied to low-power transistors can be achieved, thereby providing the possibility of integrating high-voltage transistors in complex low-power applications without requiring substantial modifications to the overall process.
[0071] Since the present invention can be modified and implemented in different but equivalent ways that are understood by those skilled in the art with the help of the teachings herein, the specific embodiments disclosed above are merely exemplary. For example, the above process steps can be performed in different orders. Moreover, the present invention is not intended to be limited to the details of the architecture or design shown herein, but as described in the accompanying claims. Therefore, it is obvious that the specific embodiments disclosed above can be modified or changed, and all such changes fall within the scope and spirit of the present invention. It should be noted that the use of terms such as "first", "second", "third" or "fourth" used to describe various processes or structures in this specification and the attached claims is only used as a quick reference to such steps / structures, and does not necessarily mean that such steps / structures are performed / formed in the order of arrangement. Of course, depending on the precise claim language, the order of arrangement of such processes may or may not be required. Therefore, the scope of protection requested by the present invention is as described in the attached claims.
Claims
1. A semiconductor device comprising: a channel region, located in the semiconductor layer; A drain region and a source region are located on the semiconductor layer to laterally connect the channel region; a buried insulating layer including a portion located below the channel region; a doped region, located below the buried insulating layer, embedded in the substrate and connected to the gate contact region between the first trench isolation structure and the second trench isolation structure, the portion of the buried insulating layer and the doped region forming a gate electrode structure of a transistor element; and The interlayer dielectric material continuously extends between the drain region and the source region and spans the entire height of the drain region and the entire height of the source region.
2. The semiconductor device according to claim 1, wherein: The buried insulating layer has a thickness of 30 nanometers or less.
3. The semiconductor device according to claim 1, wherein: The semiconductor layer has a thickness of 15 nanometers or less.
4. The semiconductor device according to claim 1, wherein: The doped region is laterally offset from the first trench isolation structure along the length direction of the transistor.
5. The semiconductor device according to claim 1, further comprising: a fully depleted low-power transistor element, wherein the fully depleted low-power transistor element comprises a gate electrode structure formed above the buried insulating layer; A highly conductive metal semiconductor compound is formed on the drain region, the source region and the upper portion of the gate contact region; and A contact element is located on the highly conductive metal semiconductor compound.
6. The semiconductor device according to claim 5, wherein: The gate electrode structure of the low power transistor device includes a high-k dielectric material.
7. The semiconductor device according to claim 1, wherein: The drain region and the source region are formed on the semiconductor layer as elevated drain regions and source regions.
8. A transistor element, comprising: A channel region, located between the drain region and the source region; a portion of the buried insulating layer located below at least the channel region; a doped semiconductor region, located below the portion of the buried insulating layer, embedded in the substrate and connected to the control terminal between the first trench isolation structure and the second trench isolation structure, the portion of the buried insulating layer and the doped semiconductor region forming a gate electrode structure, the transistor element does not include a gate electrode structure located above the channel region; and The interlayer dielectric material continuously extends between the drain region and the source region and spans the entire height of the drain region and the entire height of the source region.
9. The transistor element according to claim 8, wherein: The physical thickness of the channel region is 15 nanometers or less.
10. The transistor element according to claim 8, wherein: The drain region and the source region are elevated semiconductor regions.
11. The transistor element according to claim 8, wherein: The doped semiconductor region is laterally offset from the drain region and the source region along the length direction of the transistor.
12. The transistor element according to claim 8, wherein: The portion of the buried insulating layer has a thickness of 10 nanometers and greater.
13. A method of forming a semiconductor device, the method comprising: forming a gate electrode structure of a transistor element by doping a portion of a substrate material of a semiconductor substrate beneath a portion of a buried insulating layer, wherein doping the portion of the substrate material includes forming the portion to be embedded in the semiconductor substrate and connected to a gate contact region between the first trench isolation structure and the second trench isolation structure; forming a drain region and a source region on a semiconductor layer formed on the buried insulating layer; and An interlayer dielectric material is formed between the drain region and the source region and extends continuously across the entire height of the drain region and the entire height of the source region.
14. The method of claim 13, wherein: Doping the portion of the substrate material includes forming the portion laterally offset from the first trench isolation structure along a length direction of the transistor.
15. The method of claim 13, further comprising forming at least one additional transistor element having a drain region and a source region in the semiconductor layer and having a gate electrode structure formed on the semiconductor layer and laterally located between the drain region and the source region.
Citation Information
Patent Citations
Fully-depleted (FD) (SOI) MOSFET access transistor
US7151303B2
Method of fabricating high voltage fully depleted SOI transistor and structure thereof
US7745879B2
High-voltage SOI MOS device structure and method of fabrication
US7939395B2