Doped and modified tobacco sheet as well as preparation method and application thereof
By adding two-dimensional/mesoporous carbon frame stacked superlattice modified materials to tobacco sheets, the problem of poor aroma stability of existing tobacco sheets is solved, the combustion performance and aroma release are improved, and the suction quality and taste are improved. .
Patent Information
- Application Number
- CN202411275537.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-12
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-09-12
AI Technical Summary
The aroma content of existing tobacco flakes is significantly reduced in the later stage of suction, resulting in poor suction sense and poor stability of fragrance. The additives used are prone to denaturation during suction, affecting the product absorption experience.
Add a two-dimensional/mesoporous carbon frame stacked superlattice modified material to the tobacco sheet, and form a two-dimensional/mesoporous carbon frame stack by modifying and assembling layered titanium carbide and oleic acid-coated Fe3O4 nanocrystals to form a two-dimensional/mesoporous carbon frame stack The layer superlattice enhances heat and mass transfer performance, improves the release of fragrance and the fullness of smoke.
It significantly improves the combustion performance and aroma fullness of cigarettes, improves the quality and taste of the smoking, and improves the structural stability and breathability of tobacco flakes.
Smart Images

Figure CN119054943A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of tobacco products and relates to an doped and modified tobacco sheet and a preparation method and application thereof. Background Art
[0002] As an important component of cigarette formula, tobacco flakes have good tar reduction and harm reduction regulatory effects, and the stability of its quality indicators is increasingly valued by cigarette supporting manufacturers. Since the raw materials of tobacco flakes are tobacco stems and broken tobacco flakes, these raw materials are different from woody plant fibers, with less fiber content and more thin-walled cells and miscellaneous cells.
[0003] CN118266611A discloses a tobacco sheet with multiple aromas, comprising a tobacco sheet substrate, a conventional adhesive layer on at least one surface of the tobacco sheet substrate, a multi-aroma flavor layer arranged between the tobacco sheet substrate and the conventional adhesive layer, and the conventional adhesive layer is doped with multi-aroma flavors.
[0004] CN105901761A discloses a tobacco shred containing mangosteen shell, which is prepared from the following raw materials in parts by weight: 40-60 parts of tobacco dust, 20-30 parts of tobacco stem, 5-10 parts of mangosteen shell, 3-5 parts of mangosteen juice, 3-5 parts of ginger juice, 0.5-1 parts of octenylsuccinic anhydride, 0.05-0.1 parts of xanthan gum, 5-10 parts of calcium carbonate, 2-4 parts of butyl titanate, 1-2 parts of glycerol and 0.5-1 parts of sodium gluconate.
[0005] In order to ensure that tobacco flakes have sufficient combustibility and aroma in cigarette production, the above-mentioned schemes all increase the combustibility and aroma of tobacco by adding flavors or additives. However, such flavor addition methods result in sufficient aroma content in the smoke at the initial stage of smoking, while in the later stage of smoking, the flavor has volatilized at the initial smoke temperature and the aroma content is significantly reduced, resulting in a poor smoking sensation. The additives used are also less stable and undergo denaturation during the smoking process, resulting in a significantly reduced smoking experience in the later stage of smoking. Summary of the invention
[0006] The purpose of the present invention is to provide a doped and modified tobacco sheet and its preparation method and application. The present invention adds a two-dimensional / mesoporous carbon skeleton laminated superlattice modified material to the tobacco sheet, which can enhance the heat and mass transfer performance of the tobacco sheet, improve the combustion performance of the cigarette, and increase the release of flavors and fragrances added to the coating liquid, increase the fullness and flavor components of the smoke, improve the smoking quality, and improve the taste. To achieve this purpose of the invention, the present invention adopts the following technical solutions:
[0007] In a first aspect, the present invention provides a method for preparing a doped and modified tobacco sheet, the method comprising the following steps:
[0008] (1) subjecting Ti3AlC2 to a one-step etching treatment and then mixing it with ammonium oleate and a solvent to obtain an ammonium oleate-modified layered titanium carbide dispersion;
[0009] (2) mixing the ammonium acid-modified layered titanium carbide dispersion with the oleic acid-coated Fe3O4 nanocrystal dispersion, removing the solvent, annealing, and then performing a two-step etching process to obtain a modified material;
[0010] (3) The modified material, tobacco raw material, adhesive and solvent are mixed, and the doped and modified tobacco sheet is obtained through post-processing.
[0011] The present invention prepares layered titanium carbide (the layered titanium carbide is a two-dimensional ultra-thin material with a chemical formula of Ti3C2T x , has many excellent physical and chemical properties. It is a kind of titanium carbide, in which "T x " represents its surface functional groups, which can be hydroxyl, carboxyl or other functional groups) and then surface modified, the two-dimensional nanosheets of layered titanium carbide can be stably mixed with the colloidal nanocrystals terminated by long-chain ligands (oleic acid-coated Fe3O4 nanocrystals) in a non-polar solvent. Slowly evaporating the solvent at the gas-liquid interface can induce the co-assembly of the two to form a two-dimensional / zero-dimensional stacked heterojunction. A two-dimensional / zero-dimensional stacked superlattice can be obtained. After carbonization and etching away the nanocrystals, a two-dimensional / mesoporous carbon skeleton stacked superlattice, i.e., a modified material, can be obtained. Adding two-dimensional / mesoporous carbon skeleton laminated superlattice to tobacco sheets can improve the structure of tobacco sheets, improve the air permeability and oxygen storage capacity of tobacco sheets while improving their structural stability, and improve the combustibility of tobacco sheets. The modified material is a layered structure, and mesoporous carbon is contained between layers. Such a unique structure can greatly enhance the heat and mass transfer performance of tobacco sheets, improve the combustion performance of cigarettes on the one hand, and increase the release of flavors and fragrances added to the coating liquid on the other hand, increase the fullness of smoke and flavor components, improve the smoking quality, and improve the taste. .
[0012] Preferably, the etchant used in the one-step etching process in step (1) comprises hydrofluoric acid and / or hydrochloric acid.
[0013] Preferably, the etching process in step (1) is followed by centrifugation and washing.
[0014] Preferably, the solvent in step (1) comprises deionized water.
[0015] Preferably, the mixing in step (1) is followed by extraction treatment.
[0016] Preferably, the extractant of the extraction treatment comprises chloroform.
[0017] Preferably, the mass concentration of the ammonium oleate-modified layered titanium carbide dispersion in step (2) is 1 to 10 g / L, for example, 1 g / L, 2 g / L, 5 g / L, 8 g / L or 10 g / L, etc., not limited to the listed values, and other values not listed within the numerical range are also applicable.
[0018] Preferably, the mass concentration of the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is 5 to 15 g / L, for example: 5 g / L, 8 g / L, 10 g / L, 12 g / L or 15 g / L, etc., not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0019] Preferably, the mass ratio of the solute in the ammonium oleate-modified layered titanium carbide dispersion to the solute in the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is 1:(0.6-1), for example: 1:0.6, 1:0.7, 1:0.8, 1:0.9 or 1:1, etc., is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0020] Preferably, the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is prepared by the following method:
[0021] Oleic acid iron, oleic acid and a first solvent are mixed, and oleic acid-coated Fe3O4 nanoparticles are obtained by pyrolysis treatment. The oleic acid-coated Fe3O4 nanoparticles are mixed with a second solvent to obtain an oleic acid-coated Fe3O4 nanocrystal dispersion.
[0022] Preferably, the first solvent comprises octadecene.
[0023] Preferably, the molar ratio of the iron oleate to oleic acid is 1:(0.6-0.9), for example: 1:0.6, 1:0.68, 1:0.7, 1:0.8 or 1:0.9, etc., not limited to the listed values, other unlisted values within the numerical range are also applicable.
[0024] Preferably, the temperature of the pyrolysis treatment is 300-350°C, for example, 300°C, 310°C, 320°C, 340°C or 350°C.
[0025] Preferably, the pyrolysis treatment time is 20 to 40 minutes, for example, 20 minutes, 25 minutes, 30 minutes, 35 minutes or 40 minutes, etc., but is not limited to the listed values, and other values not listed within the numerical range are also applicable.
[0026] Preferably, the second solvent comprises n-hexane.
[0027] Preferably, the method of removing the solvent in step (2) comprises evaporation.
[0028] Preferably, the temperature of the annealing treatment in step (2) is 350-450°C, for example, 350°C, 380°C, 400°C, 420°C or 450°C, etc., and is not limited to the listed values. Other values not listed within the numerical range are also applicable.
[0029] Preferably, the annealing time in step (2) is 1 to 3 hours, for example, 1 hour, 1.5 hours, 2 hours, 2.5 hours or 3 hours, etc., and is not limited to the listed values. Other values not listed within the numerical range are also applicable.
[0030] Preferably, the etchant used in the two-step etching process in step (2) includes hydrochloric acid.
[0031] Preferably, the two-step etching treatment in step (2) is followed by centrifugation, washing and drying.
[0032] Preferably, the mass ratio of the modified material, tobacco raw material and adhesive in step (3) is (2-8):100:(3-5), for example: 2:100:3, 5:100:3, 6:100:5, 4:100:4 or 8:100:5, etc., and is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0033] Preferably, an atomizer is also added during the mixing in step (3).
[0034] Preferably, the atomizer comprises 1,3-butanediol and / or propylene glycol.
[0035] Preferably, the mass ratio of the atomizer to the tobacco raw material is (5-10):100, for example: 5:100, 6:100, 8:100, 9:100 or 10:100, etc., and is not limited to the listed values, and other unlisted values within the numerical range are also applicable.
[0036] In a second aspect, the present invention provides a doped and modified tobacco sheet, wherein the doped and modified tobacco sheet is prepared by the method described in the first aspect.
[0037] In a third aspect, the present invention provides a tobacco product, comprising the doped and modified tobacco sheet as described in the second aspect.
[0038] Compared with the prior art, the present invention has the following beneficial effects:
[0039] The present invention adds two-dimensional / mesoporous carbon skeleton laminated superlattice modified materials to tobacco sheets, which can enhance the heat and mass transfer performance of tobacco sheets, improve the combustion performance of cigarettes on the one hand, and increase the release amount of flavors and fragrances added to the coating liquid on the other hand, increase the fullness and flavor components of smoke, improve the smoking quality, and improve the taste. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Figure 1 It is a schematic diagram of the preparation process of the modified material described in Example 1 of the present invention.
[0041] Among them, 1 is Fe3O4 nanocrystal coated with oleic acid, 2 is layered titanium carbide modified with ammonium oleate, 3 is a two-dimensional / zero-dimensional stacked heterojunction, 4 is a two-dimensional / zero-dimensional stacked superlattice, 5 is a two-dimensional / mesoporous carbon skeleton stacked superlattice (modified material), a is a volatile solvent, b is annealing, and c is etching. DETAILED DESCRIPTION
[0042] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0043] Example 1
[0044] This embodiment provides a doped and modified tobacco sheet, and the preparation method of the doped and modified tobacco sheet is as follows:
[0045] (1) Take 1g of Ti3AlC2 and slowly add it to 20mL of etching solution, which is composed of 2mL 50% HF, 12mL concentrated hydrochloric acid, and 6mL deionized water, and stir at 25°C for 24h. Then wash the reaction solution with deionized water by repeated centrifugation (6500rpm, 5min) until the pH is about 6-7, add 10mL 25% tetramethylammonium hydroxide (TMAOH) aqueous solution, and stir at room temperature for 12h to perform TMA + Ion intercalation. Excess TMAOH is then removed by centrifugation (6500 rpm, 5 min), followed by centrifugation (3500 rpm, 1 h) to obtain layered titanium carbide nanosheets, the layered titanium carbide nanosheets are mixed with deionized water, excess ammonium oleate is added, stirred for 2 h, and then extracted with chloroform to obtain an ammonium oleate-modified layered titanium carbide dispersion;
[0046] (2) Dissolve oleic acid iron and oleic acid in 400g of octadecene at a molar ratio of 1:0.75, pyrolyze at 320°C for 30min, and then cool rapidly. After cooling to room temperature, wash the resulting mixture with ethanol, isopropanol and n-hexane, centrifuge, mix the obtained solid with n-hexane to obtain an oleic acid-coated Fe3O4 nanocrystal dispersion, mix 10mL of ammonium oleate-modified layered titanium carbide dispersion (5g / L) with 5mL of oleic acid-coated Fe3O4 nanocrystal dispersion (8g / L) and ultrasonicate for 3min to form a two-dimensional / zero-dimensional stacked heterojunction. The mixture is then slowly evaporated in a covered porcelain boat, followed by annealing at 400°C Ar for 2h to obtain a two-dimensional / zero-dimensional stacked superlattice, which is then etched with 3mol / L hydrochloric acid, and washed and dried to obtain a two-dimensional / mesoporous carbon skeleton stacked superlattice modified material. The schematic diagram of the preparation process of the modified material is shown in the figure. Figure 1 As shown;
[0047] (3) 5 g of the modified material, 100 g of tobacco raw material, 4 g of adhesive, 2 g of 1,3-butanediol, 3 g of propylene glycol and 300 g of water are mixed, stirred, pressed and dried to obtain the doped modified tobacco sheet.
[0048] Example 2
[0049] This embodiment provides a doped and modified tobacco sheet, and the preparation method of the doped and modified tobacco sheet is as follows:
[0050] (1) Take 1g of Ti3AlC2 and slowly add it to 20mL of etching solution, which is composed of 2mL 50% HF, 12mL concentrated hydrochloric acid, and 6mL deionized water, and stir at 25°C for 24h. Then wash the reaction solution with deionized water by repeated centrifugation (6500rpm, 5min) until the pH is about 6-7, add 10mL 25% tetramethylammonium hydroxide (TMAOH) aqueous solution, and stir at room temperature for 12h to perform TMA + Ion intercalation. Excess TMAOH is then removed by centrifugation (6500 rpm, 5 min), followed by centrifugation (3500 rpm, 1 h) to obtain layered titanium carbide nanosheets, the layered titanium carbide nanosheets are mixed with deionized water, excess ammonium oleate is added, stirred for 2 h, and then extracted with chloroform to obtain an ammonium oleate-modified layered titanium carbide dispersion;
[0051] (2) Dissolve oleic acid iron and oleic acid in 400g of octadecene at a molar ratio of 1:0.75, pyrolyze at 300°C for 40min, and then cool rapidly. After cooling to room temperature, wash the resulting mixture with ethanol, isopropanol and n-hexane, centrifuge, mix the obtained solid with n-hexane to obtain an oleic acid-coated Fe3O4 nanocrystal dispersion, mix 10mL of ammonium oleate-modified layered titanium carbide dispersion (1g / L) with 1mL of oleic acid-coated Fe3O4 nanocrystal dispersion (6g / L) and ultrasonicate for 5min to form a two-dimensional / zero-dimensional stacked heterojunction. Subsequently, the mixture was slowly evaporated in a covered porcelain boat, and then annealed at 350°C Ar for 3h to obtain a two-dimensional / zero-dimensional stacked superlattice, which was then etched with 3mol / L hydrochloric acid, and washed and dried to obtain a two-dimensional / mesoporous carbon skeleton stacked superlattice modified material;
[0052] (3) 2 g of the modified material, 100 g of tobacco raw material, 3 g of adhesive, 3 g of 1,3-butanediol, 5 g of propylene glycol and 300 g of water are mixed, stirred, pressed and dried to obtain the doped modified tobacco sheet.
[0053] Example 3
[0054] This embodiment provides a doped and modified tobacco sheet, and the preparation method of the doped and modified tobacco sheet is as follows:
[0055] (1) Take 1g of Ti3AlC2 and slowly add it to 20mL of etching solution, which is composed of 2mL 50% HF, 12mL concentrated hydrochloric acid, and 6mL deionized water, and stir at 25°C for 24h. Then wash the reaction solution with deionized water by repeated centrifugation (6500rpm, 5min) until the pH is about 6-7, add 10mL 25% tetramethylammonium hydroxide (TMAOH) aqueous solution, and stir at room temperature for 12h to perform TMA + Ion intercalation. Excess TMAOH is then removed by centrifugation (6500 rpm, 5 min), followed by centrifugation (3500 rpm, 1 h) to obtain layered titanium carbide nanosheets, the layered titanium carbide nanosheets are mixed with deionized water, excess ammonium oleate is added, stirred for 2 h, and then extracted with chloroform to obtain an ammonium oleate-modified layered titanium carbide dispersion;
[0056] (2) Dissolve oleic acid iron and oleic acid in 400g of octadecene at a molar ratio of 1:0.9, pyrolyze at 350°C for 30min, and then cool rapidly. After cooling to room temperature, wash the resulting mixture with ethanol, isopropanol and n-hexane, centrifuge, mix the obtained solid with n-hexane to obtain an oleic acid-coated Fe3O4 nanocrystal dispersion, mix 1mL of ammonium oleate-modified layered titanium carbide dispersion (10g / L) with 1mL of oleic acid-coated Fe3O4 nanocrystal dispersion (10g / L) and ultrasonicate for 5min to form a two-dimensional / zero-dimensional stacked heterojunction. Subsequently, the mixture was slowly evaporated in a covered porcelain boat, and then annealed at 450°C Ar for 1h to obtain a two-dimensional / zero-dimensional stacked superlattice, which was then etched with 3mol / L hydrochloric acid, and washed and dried to obtain a two-dimensional / mesoporous carbon skeleton stacked superlattice modified material;
[0057] (3) 8 g of the modified material, 100 g of tobacco raw material, 5 g of adhesive, 4 g of 1,3-butanediol, 6 g of propylene glycol and 300 g of water were mixed, stirred, pressed and dried to obtain the doped modified tobacco sheet.
[0058] Example 4
[0059] The only difference between this embodiment and embodiment 1 is that the volume of the oleic acid-coated Fe3O4 nanocrystal dispersion is 2.5 mL, and the other conditions and parameters are exactly the same as those in embodiment 1.
[0060] Example 5
[0061] The only difference between this embodiment and embodiment 1 is that the volume of the oleic acid-coated Fe3O4 nanocrystal dispersion is 7.5 mL, and the other conditions and parameters are exactly the same as those in embodiment 1.
[0062] Example 6
[0063] The only difference between this embodiment and embodiment 1 is that the mass of the modified material is 1 g, and the other conditions and parameters are exactly the same as those in embodiment 1.
[0064] Example 7
[0065] The only difference between this embodiment and embodiment 1 is that the mass of the modified material is 10 g, and the other conditions and parameters are exactly the same as those in embodiment 1.
[0066] Comparative Example 1
[0067] The only difference between this comparative example and Example 1 is that ammonium oleate is not used to modify the layered titanium carbide nanosheets, and other conditions and parameters are exactly the same as those in Example 1.
[0068] Comparative Example 2
[0069] The only difference between this comparative example and Example 1 is that no oleic acid-coated Fe3O4 nanocrystal dispersion is added, and other conditions and parameters are exactly the same as those in Example 1.
[0070] Comparative Example 3
[0071] The only difference between this comparative example and Example 1 is that the oleic acid-coated Fe3O4 nanocrystal dispersion is directly used as the modified material by carbonization and then etching to prepare mesoporous carbon, and the other conditions and parameters are exactly the same as those in Example 1.
[0072] Performance Test:
[0073] The examples, comparative examples and blank samples were tested for suction experience, and the test results are as follows:
[0074] Blank sample: small amount of smoke, faint aroma, there is aroma in the first and second puffs, but almost no aroma in the following puffs.
[0075] Example 1-3: The smoke is sufficient, the aroma volume is significantly increased, the aroma is full, the strength is appropriate, the suction is coordinated, non-irritating, and the aftertaste is comfortable.
[0076] Example 4-5: The amount of smoke is slightly increased, the amount of aroma is increased, the suction is still coordinated, and the aftertaste is still comfortable, but the overall aroma enhancement effect is not very obvious.
[0077] Example 6-7: The aroma of the tobacco is improved, but the permeability is poor, the strength is slightly strong, slightly irritating, and the aftertaste is still comfortable.
[0078] Comparative Example 1: The amount of smoke is small, the fragrance is weak, the suction is not harmonious, and the irritation is strong.
[0079] Comparative Example 2: The amount of smoke is slightly increased, the fragrance is slightly increased, the suction is not coordinated, and the irritation is strong.
[0080] Comparative Example 3: The smoke volume is sufficient, the fragrance is light, the suction is harmonious, and the stimulation is strong.
[0081] By comparing Example 1 with Examples 4-5, it can be seen that in the preparation process of the doped and modified tobacco sheet of the present invention, the ratio of the layered titanium carbide modified by ammonium oleate to the Fe3O4 nanocrystals coated with oleic acid will affect its performance. The mass ratio of the layered titanium carbide modified by ammonium oleate to the Fe3O4 nanocrystals coated with oleic acid is controlled at 1:0.6-1, and the effect of obtaining the doped and modified tobacco sheet is better. If the addition amount of the Fe3O4 nanocrystals coated with oleic acid modified by ammonium oleate is too low, the filling amount of the porous carbon material between the layered titanium carbide layers of the modified material is low, and the improvement effect is poor. If the addition amount of the Fe3O4 nanocrystals coated with oleic acid modified by ammonium oleate is too high, excessive porous carbon material adheres to the surface of the layered titanium carbide, resulting in reduced stability of the layered structure and easy collapse.
[0082] By comparing Example 1 with Examples 6-7, it can be seen that in the preparation process of the doped modified tobacco sheet of the present invention, the mass ratio of the modified material to the tobacco raw material will affect its performance. When the mass ratio of the modified material to the tobacco raw material is controlled at 2 to 8:100, the effect of preparing the doped modified tobacco sheet is better. If the amount of the modified material added is too low, the modification effect is not obvious. If the amount of the modified material added is too high, too much smoke and nicotine will be generated during smoking, and the user experience will be reduced.
[0083] By comparing Example 1 and Comparative Example 1, it can be seen that without modifying the layered titanium carbide, the layered titanium carbide two-dimensional nanosheets cannot self-assemble with the colloidal nanocrystals terminated with long-chain ligands, resulting in the inability to generate a two-dimensional / zero-dimensional stacked heterojunction, and the modified material of the present application cannot be obtained, only a simple mixture, and the modification effect is greatly reduced.
[0084] From the comparison between Example 1 and Comparative Examples 2-3, it can be seen that using only simple layered titanium carbide or mesoporous carbon material as a modification material cannot achieve a synergistic modification effect, and the effect of preparing tobacco sheets is not obvious.
[0085] In summary, the tobacco sheets prepared in Examples 1-3 of the present invention can significantly increase the amount of smoke, make the smoke round, enhance the aroma, cover up the miscellaneous smell, have a full and delicate aroma, a suitable strength, a comfortable aftertaste, good overall suction coordination, and a strong sense of pleasure.
[0086] The pyrolysis products of Example 1 and the blank sample were specifically analyzed, and " / " indicates that no pyrolysis products were detected. The analysis results are shown in Table 1:
[0087] Table 1
[0088]
[0089]
[0090]
[0091] It can be seen from Table 1 that the use of the modified tobacco sheet of the present invention can significantly increase the aroma components of the smoke, enrich the smoke aroma, and improve the smoking quality.
[0092] The applicant declares that the above is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention shall fall within the protection scope and disclosure scope of the present invention.
Claims
1. A method for preparing a doped and modified tobacco sheet, characterized in that: The preparation method comprises the following steps: (1) subjecting Ti3AlC2 to a one-step etching treatment and then mixing it with ammonium oleate and a solvent to obtain an ammonium oleate-modified layered titanium carbide dispersion; (2) mixing the ammonium acid-modified layered titanium carbide dispersion with the oleic acid-coated Fe3O4 nanocrystal dispersion, removing the solvent, annealing, and then performing a two-step etching process to obtain a modified material; (3) The modified material, tobacco raw material, adhesive and solvent are mixed, and the doped and modified tobacco sheet is obtained through post-processing.
2. The preparation method according to claim 1, characterized in that The etchant for the one-step etching process in step (1) includes hydrofluoric acid and / or hydrochloric acid; Preferably, the etching process in step (1) is followed by centrifugation and washing.
3. The preparation method according to claim 1 or 2, characterized in that: The solvent in step (1) comprises deionized water; Preferably, the mixing in step (1) is followed by extraction treatment; Preferably, the extractant of the extraction treatment comprises chloroform.
4. The preparation method according to any one of claims 1 to 3, characterized in that: The mass concentration of the ammonium oleate-modified layered titanium carbide dispersion in step (2) is 1 to 10 g / L; Preferably, the mass concentration of the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is 5 to 15 g / L; Preferably, the mass ratio of the solute in the ammonium oleate-modified layered titanium carbide dispersion to the solute in the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is 1:(0.6-1); Preferably, the oleic acid-coated Fe3O4 nanocrystal dispersion in step (2) is prepared by the following method: The oleic acid iron and oleic acid are mixed with a first solvent, and oleic acid-coated Fe3O4 nanoparticles are obtained by pyrolysis treatment, and the oleic acid-coated Fe3O4 nanoparticles are mixed with a second solvent to obtain an oleic acid-coated Fe3O4 nanocrystal dispersion; Preferably, the first solvent comprises octadecene; Preferably, the molar ratio of the iron oleate to oleic acid is 1:(0.6-0.9); Preferably, the temperature of the pyrolysis treatment is 300-350°C; Preferably, the pyrolysis treatment time is 20 to 40 minutes; Preferably, the second solvent comprises n-hexane.
5. The preparation method according to any one of claims 1 to 4, characterized in that: The method for removing the solvent in step (2) comprises evaporation; Preferably, the temperature of the annealing treatment in step (2) is 350-450°C; Preferably, the annealing treatment time in step (2) is 1 to 3 hours.
6. The preparation method according to any one of claims 1 to 5, characterized in that: The etchant for the two-step etching process in step (2) includes hydrochloric acid; Preferably, the two-step etching treatment in step (2) is followed by centrifugation, washing and drying.
7. The preparation method according to any one of claims 1 to 6, characterized in that: The mass ratio of the modified material, tobacco raw material and adhesive in step (3) is (2-8):100:(3-5).
8. The preparation method according to any one of claims 1 to 7, characterized in that: The mixing in step (3) further includes adding an atomizer; Preferably, the atomizer includes 1,3-butanediol and / or propylene glycol; Preferably, the mass ratio of the atomizer to the tobacco raw material is (5-10):
100.
9. A doped and modified tobacco sheet, characterized in that: The doped and modified tobacco sheet is prepared by the method according to any one of claims 1-8.
10. A tobacco product, characterized in that: The tobacco product comprises the doped and modified tobacco sheet according to claim 9.
Citation Information
Patent Citations
Heat-not-burn tobacco sheets and preparing method thereof
CN107668775A
Efficient and general two-dimensional nanometer sheet-zero-dimensional nanocrystalline co-assembly method
CN109879328A
Preparation method of ordered mesoporous carbon-titanium carbide nanosheet laminated superstructure material
CN116332155A
Preparation method of universal two-dimensional mesoporous nitrogen-doped carbon composite material
CN117049502A
Composite mesoporous / microporous materials and their use in smoking articles for removing certain gas phase constituents from tobacco smoke
US20050133054A1