Anti-fog lens and preparation method thereof
By designing hollow structure and plasma treatment on the surface of the lens, the existing anti-fog lenses have solved the problem of mist droplets and the poor friction resistance of the anti-fog film in the temperature difference environment, achieving a more stable and durable anti-fog effect.
Patent Information
- Application Number
- CN202411089221.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-12-03
AI Technical Summary
The existing anti-fog lenses are prone to fog droplets in temperature difference environments, and the anti-fog film is unstable, has poor friction resistance, and has a short service life.
A method of preparing anti-fog lenses, including lens injection molding, dust removal, surface treatment, hardening liquid coating, pre-baking, baking, auxiliary layer removal, anti-fog liquid injection and baking, etc., through plasma treatment and auxiliary layer design , a hollow structure is formed to improve the connection firmness and wear resistance of the anti-fog layer.
It effectively improves the connection firmness and wear resistance of the anti-fog layer, extends the anti-fog effect, avoids wear of the anti-fog layer during the wiping process, and significantly improves the anti-fog performance of the lens.
Smart Images

Figure CN119060394A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of anti-fog lens preparation, and in particular to an anti-fog lens and a preparation method thereof. Background Art
[0002] Existing lenses are particularly prone to fog droplets in temperature-difference environments. The principle of fog droplet formation is that the saturated vapor pressure of water on the surface of the resin lens is lower than the partial pressure of water vapor in the air due to the lower temperature, causing the water vapor to condense into small water droplets. These fog droplets will refract and scatter light, changing the optical properties of the lens and affecting light transmittance, thus causing many inconveniences in life.
[0003] In order to avoid fog droplets on the lens, an anti-fog film is often coated on the surface of the lens. However, the existing anti-fog technology process is unstable, and because the anti-fog film is coated on the outer surface, it will be wiped many times during normal life, and the anti-fog film is not resistant to friction, resulting in a short service life. Summary of the invention
[0004] The technical solution of the present invention aims at the technical problem that the existing technical solutions are too single, and provides a solution that is significantly different from the existing technologies. The embodiment of the present invention provides an anti-fog lens and a preparation method thereof to solve the technical problems that the existing anti-fog liquid has unstable connection due to the processing technology, and the anti-fog layer will be lost after being wiped on the surface for many times.
[0005] The embodiment of the present invention adopts the following technical scheme: an anti-fog lens and a preparation method thereof, 1. A preparation method of an anti-fog lens, characterized in that it comprises the following steps;
[0006] S1. Lens injection molding: First, the lens raw materials are dried, and then injected into the injection molding machine for injection molding;
[0007] S2. Dust removal of lens: Use an air gun to blow away the dust on the surface of the product and use the exhaust system to suck it away;
[0008] S3, lens surface treatment: apply an auxiliary layer on the anti-fogging surface of the lens after dust removal, the auxiliary layer is applied in the central area of the lens, and the application area is smaller than the area of the lens, so that it can be fully applied to the position of the lens that needs to be anti-fogging, and then use a negative pressure air pipe to suck away excess auxiliary liquid, and then cool it to solidify it, and then use etching or corrosion to form a larger uneven surface on the surface of the auxiliary layer, and then place it on a plasma treatment machine at an angle, and perform ion impact on the corroded surface, so that the surface of the auxiliary layer finally forms a connected irregular shape;
[0009] S4, applying hardening liquid: applying hardening liquid on the treated surface of the auxiliary layer. Before applying the hardening liquid, a barrier is placed at the application position so that a through hole is left between the hardening liquid and the auxiliary layer. When the hardening liquid is in full contact with the auxiliary layer and the part of the lens not coated with the auxiliary layer, the excess hardening liquid is sucked away by a negative pressure air pipe;
[0010] S5. Pre-baking: Place the product coated with the hardening liquid in the drying tunnel and bake it at 85°C for more than three minutes to make its surface preliminarily dry;
[0011] S6. Baking: Put the pre-baked product into the oven and fully bake it. The oven temperature is set to 108°C and the baking time is set to 120 minutes.
[0012] S7, cooling the lens; taking out the baked product and cooling it at room temperature for more than 30 minutes;
[0013] S8, auxiliary layer removal: secondary heating to make its temperature reach the melting temperature of the auxiliary layer, and use the barrier left when applying the hardening layer to suck out the auxiliary layer between the lens and the hardening layer, so that a hollow is formed between the lens and the hardening layer;
[0014] S9, anti-fog liquid injection: remove the barrier, and a flow hole will be left after the barrier is removed. The anti-fog liquid is injected into the original auxiliary layer through the flow hole. At the same time, the anti-fog layer overflows to the surface of the hardening layer, thereby replacing the original auxiliary layer, so that the anti-fog layer is located between the lens and the hardening layer, and at this time, the surface of the hardening layer also has an anti-fog layer;
[0015] S10, baking: putting the product coated with the nano anti-fog liquid into an oven for baking, the oven temperature is set to 65°C, and the baking time is set to 90 minutes;
[0016] S11. Inspect the product and put it on a plate: inspect the baked product and put it on a plate for use in the next process.
[0017] Furthermore, in step S1, the lens raw material is polycarbonate, the drying box temperature is 110°C-130°C, the drying time is 2h-4h, the drying box temperature of the top hopper is 100°C-120°C, the moisture content of the raw material after drying is less than 0.03%, the injection molding temperature is 280-320°C, the injection pressure is 70-140MPa, the molding time is 40s-65s, and the mold temperature is between 80°C and 120°C.
[0018] Furthermore, in step S3, the auxiliary liquid is made of thermoplastic resin material, so that it can be repeatedly heated to melt and cooled to solidify, and the hot melting temperature is greater than the baking temperature of the hardened layer.
[0019] Furthermore, the hardening liquid in step S5 comprises 30% organic silicone resin, 30% ethanol, 20% isopropanol, 10% acetic acid and 10% water.
[0020] Furthermore, the specific steps of plasma treatment in step S9 are to place the cooled product at an angle on the electrode plate of the plasma processor, evacuate the plasma chamber to make the gas pressure reach below 20Pa, and then bombard the chamber with ions, while injecting oxygen and argon in a ratio of 3:1 to enhance the plasma effect.
[0021] Furthermore, the anti-fog liquid in step S10 comprises 0.16%-0.2% chlorphenesin, 0.21%-0.41% polyhexamethylene guanidine, 4%-4.5% polydimethylsiloxane, 1%-1.5% polyvinyl alcohol, 3%-8% ethanol, and the rest is water.
[0022] Furthermore, the lens includes a lens base layer, an anti-fog layer and a hardening layer.
[0023] Compared with the prior art, the beneficial effects of the present invention are:
[0024] First, during the plasma impact process, a high-frequency and high-energy electric field is applied to the gas, so that the gas molecules are excited to the ion state. The ions have energy. On the one hand, they will physically bombard the microscopic dirt on the surface of the material to clean the surface of the material, and at the same time, the roughness of the material surface will change at the nanometer level, so that the surface contact area will increase, and the potion will be easier to adhere. On the other hand, due to chemical action, the ions will bombard and break the chemical bonds such as C=C and C=H in the polymer, and some oxygen ions will be generated during the gas ionization process. The oxygen ions and the chemical bonds broken on the surface of the material will be re-bonded to form C=O and OH and other hydrophilic functional groups. Using oxygen can introduce more oxygen ions, and the argon ions generated by introducing a small amount of argon are heavier. On the one hand, they help to break the chemical bonds on the surface of the material, and on the other hand, they can stimulate more oxygen ions by colliding with oxygen molecules, thereby increasing the active functional groups on the surface of the material. These functional groups are attached or bonded to the surface of the material, so that the surface of the material is activated, greatly improving the surface energy and adhesion of the material.
[0025] Secondly, the surface state of the contact surface between the hardened layer and the auxiliary layer is controlled by treating the surface of the auxiliary layer. If the ion impact method is used directly, the inner surface of the hardened layer needs to be changed, and the inner surface cannot be treated during the ion impact process. Therefore, the auxiliary layer is firstly added and the surface of the auxiliary layer is treated. At this time, when the hardened layer is applied to the surface of the auxiliary layer, the contact surface between the hardened layer and the auxiliary layer will naturally follow the auxiliary layer to form an uneven and irregular state. At this time, when the anti-fog liquid is noticed to contact the hardened layer at the hollow part, the uneven and irregular state can be better connected with the anti-fog liquid, which effectively improves the connection firmness. Compared with the existing method of using ion impact to achieve an uneven state (although it is uneven, the overall trend is relatively regular, so the actual connection firmness is still poor), the effect is better;
[0026] Thirdly, since the anti-fog liquid is located between the hardening layer and the lens and on the surface of the hardening layer, it has a longer service life and is more wear-resistant than the anti-fog liquid directly applied to the surface. If the anti-fog liquid is only applied to the surface, according to human living habits, wiping the lens will be indispensable. At this time, during the wiping process, the wiping cloth is in direct contact with the anti-fog layer. Although the wiping cloth feels relatively smooth, it is still woven, resulting in gaps. In the process of wiping, dust particles constantly rub and roll on the surface of the anti-fog layer, thereby scraping the anti-fog layer, causing the anti-fog layer itself to be constantly worn. After a long time, the effect of the anti-fog layer will be greatly reduced. After placing the anti-fog layer in the middle position, while retaining the anti-fog function of the lens, the wear of the anti-fog layer during wiping can be effectively avoided. Because the hardening layer is in direct contact with the wiping cloth during wiping, the anti-fog effect of the lens is greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0028] Figure 1 It is a schematic diagram of the production process change of the present invention;
[0029] Figure 2 It is a schematic diagram of the position of the anti-fog layer of the present invention. DETAILED DESCRIPTION
[0030] The technical solution of the present invention will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.
[0031] The components of the embodiments of the present invention generally described and shown in the drawings herein may be arranged and designed in various different configurations. Therefore, the following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention.
[0032] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without making any creative work shall fall within the scope of protection of the present invention.
[0033] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0034] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0035] Combine the following Figure 1 to Figure 2 As shown, an embodiment of the present invention provides an anti-fog lens and a preparation method thereof, comprising the following steps:
[0036] 1. A method for preparing an anti-fog lens, characterized in that it comprises the following steps:
[0037] S1. Lens injection molding: First, the lens raw materials are dried, and then injected into the injection molding machine for injection molding;
[0038] S2. Dust removal of lens: Use an air gun to blow away the dust on the surface of the product and use the exhaust system to suck it away;
[0039] S3, lens surface treatment: apply an auxiliary layer on the anti-fogging surface of the lens after dust removal, the auxiliary layer is applied in the central area of the lens, and the application area is smaller than the area of the lens, so that it can be fully applied to the position of the lens that needs to be anti-fogging, and then use a negative pressure air pipe to suck away excess auxiliary liquid, and then cool it to solidify it, and then use etching or corrosion to form a larger uneven surface on the surface of the auxiliary layer, and then place it on a plasma treatment machine at an angle, and perform ion impact on the corroded surface, so that the surface of the auxiliary layer finally forms a connected irregular shape;
[0040] S4, applying hardening liquid: applying hardening liquid on the treated surface of the auxiliary layer. Before applying the hardening liquid, a barrier is placed at the application position so that a through hole is left between the hardening liquid and the auxiliary layer. When the hardening liquid is in full contact with the auxiliary layer and the part of the lens not coated with the auxiliary layer, the excess hardening liquid is sucked away by a negative pressure air pipe;
[0041] S5. Pre-baking: Place the product coated with the hardening liquid in the drying tunnel and bake it at 85°C for more than three minutes to make its surface preliminarily dry;
[0042] S6. Baking: Put the pre-baked product into the oven and fully bake it. The oven temperature is set to 108°C and the baking time is set to 120 minutes.
[0043] S7, cooling the lens; taking out the baked product and cooling it at room temperature for more than 30 minutes;
[0044] S8, auxiliary layer removal: secondary heating to make its temperature reach the melting temperature of the auxiliary layer, and use the barrier left when applying the hardening layer to suck out the auxiliary layer between the lens and the hardening layer, so that a hollow is formed between the lens and the hardening layer;
[0045] S9, anti-fog liquid injection: remove the barrier, and a flow hole will be left after the barrier is removed. The anti-fog liquid is injected into the original auxiliary layer through the flow hole. At the same time, the anti-fog layer overflows to the surface of the hardening layer, thereby replacing the original auxiliary layer, so that the anti-fog layer is located between the lens and the hardening layer, and at this time, the surface of the hardening layer also has an anti-fog layer;
[0046] S10, baking: putting the product coated with the nano anti-fog liquid into an oven for baking, the oven temperature is set to 65°C, and the baking time is set to 90 minutes;
[0047] S11. Inspect the product and put it on a plate: inspect the baked product and put it on a plate for use in the next process.
[0048] Specifically, in step S1, polycarbonate is used as the lens raw material, the drying box temperature is selected to be 110°C-130°C, the drying time is 2h-4h, the drying box temperature of the top hopper is 100°C-120°C, the moisture content of the raw material after drying is less than 0.03%, the injection molding temperature is 280-320°C, the injection pressure is 70-140MPa, the molding time is 40s-65s, and the mold temperature is between 80°C and 120°C.
[0049] Specifically, the auxiliary liquid in step S3 is made of thermoplastic resin material, so that it can be repeatedly heated to melt and cooled to solidify, and the hot melting temperature is greater than the baking temperature of the hardened layer.
[0050] During operation, since thermoplastic resin material is used, it is first cured to form it. The formed material has a certain hardness, so it can be surface treated. The hot melt temperature of the thermoplastic material is higher than the hardening temperature and baking temperature of the hardened layer. The auxiliary layer will not be affected when the hardened layer is cured. When the hardened layer is processed, it can be heated for a second time to melt the auxiliary layer and then sucked out.
[0051] Specifically, the hardening liquid in step S5 comprises 30% organic silicone resin, 30% ethanol, 20% isopropyl alcohol, 10% acetic acid and 10% water.
[0052] Specifically, the specific steps of plasma treatment in step S9 are to place the cooled product at an angle on the electrode plate of the plasma processor, evacuate the plasma chamber to make the gas pressure reach below 20Pa, and then bombard the chamber with ions, while injecting oxygen and argon in a ratio of 3:1 to enhance the plasma effect.
[0053] Specifically, the anti-fog liquid in step S10 comprises 0.16%-0.2% chlorphenesin, 0.21%-0.41% polyhexamethylene guanidine, 4%-4.5% polydimethylsiloxane, 1%-1.5% polyvinyl alcohol, 3%-8% ethanol, and the rest is water.
[0054] Specifically, the lens includes a lens base layer, an anti-fog layer and a hardening layer.
[0055] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for preparing an anti-fog lens, characterized in that: The steps include: S1. Lens injection molding: First, the lens raw materials are dried, and then injected into the injection molding machine for injection molding; S2. Dust removal of lens: Use an air gun to blow away the dust on the surface of the product and use the exhaust system to suck it away; S3, lens surface treatment: apply an auxiliary layer on the anti-fogging surface of the lens after dust removal, the auxiliary layer is applied in the central area of the lens, and the application area is smaller than the area of the lens, so that it can be fully applied to the position of the lens that needs to be anti-fogging, and then use a negative pressure air pipe to suck away excess auxiliary liquid, and then cool it to solidify it, and then use etching or corrosion to form a larger uneven surface on the surface of the auxiliary layer, and then place it on a plasma treatment machine at an angle, and perform ion impact on the corroded surface, so that the surface of the auxiliary layer finally forms a connected irregular shape; S4, applying hardening liquid: applying hardening liquid on the treated surface of the auxiliary layer. Before applying the hardening liquid, a barrier is placed at the application position so that a through hole is left between the hardening liquid and the auxiliary layer. When the hardening liquid is in full contact with the auxiliary layer and the part of the lens not coated with the auxiliary layer, the excess hardening liquid is sucked away by a negative pressure air pipe; S5. Pre-baking: Place the product coated with the hardening liquid in the drying tunnel and bake it at 85°C for more than three minutes to make its surface preliminarily dry; S6. Baking: Put the pre-baked product into the oven and fully bake it. The oven temperature is set to 108°C and the baking time is set to 120 minutes. S7, cooling the lens; taking out the baked product and cooling it at room temperature for more than 30 minutes; S8, auxiliary layer removal: secondary heating to make its temperature reach the melting temperature of the auxiliary layer, and use the barrier left when applying the hardening layer to suck out the auxiliary layer between the lens and the hardening layer, so that a hollow is formed between the lens and the hardening layer; S9, anti-fog liquid injection: remove the barrier, and a flow hole will be left after the barrier is removed. The anti-fog liquid is injected into the original auxiliary layer through the flow hole. At the same time, the anti-fog layer overflows to the surface of the hardening layer, thereby replacing the original auxiliary layer, so that the anti-fog layer is located between the lens and the hardening layer, and at this time, the surface of the hardening layer also has an anti-fog layer; S10, baking: putting the product coated with the nano anti-fog liquid into an oven for baking, the oven temperature is set to 65°C, and the baking time is set to 90 minutes; S11. Inspect the product and put it on a plate: inspect the baked product and put it on a plate for use in the next process.
2. The method for preparing an anti-fog lens according to claim 1, characterized in that: In the step S1, the lens raw material is polycarbonate, the drying box temperature is 110°C-130°C, the drying time is 2h-4h, the drying box temperature of the top hopper is 100°C-120°C, the moisture content of the raw material after drying is less than 0.03%, the injection molding temperature is 280-320°C, the injection pressure is 70-140MPa, the molding time is 40s-65s, and the mold temperature is between 80°C and 120°C.
3. The method for preparing an anti-fog lens according to claim 1, characterized in that: In step S3, the auxiliary liquid is made of thermoplastic resin material, so that it can be repeatedly heated to melt and cooled to solidify, and the hot melting temperature is greater than the baking temperature of the hardened layer.
4. The method for preparing an anti-fog lens according to claim 1, characterized in that: The hardening liquid in step S5 comprises 30% organic silicone resin, 30% ethanol, 20% isopropanol, 10% acetic acid and 10% water.
5. The method for preparing an anti-fog lens according to claim 1, characterized in that: The specific steps of plasma treatment in step S9 are to place the cooled product at an angle on the electrode plate of the plasma processor, evacuate the plasma chamber to make the gas pressure reach below 20Pa, and then bombard the chamber with ions, while injecting oxygen and argon in a ratio of 3:1 to enhance the plasma effect.
6. The method for preparing an anti-fog lens according to claim 1, characterized in that: The anti-fog liquid in step S10 comprises 0.16%-0.2% chlorphenesin, 0.21%-0.41% polyhexamethylene guanidine, 4%-4.5% polydimethylsiloxane, 1%-1.5% polyvinyl alcohol, 3%-8% ethanol, and the rest is water.
7. An anti-fog lens, prepared by the anti-fog lens preparation method according to any one of claims 1 to 6, comprising a lens base layer, an anti-fog layer and a hardening layer.
Citation Information
Cited By
Lens strengthening and antifogging production method
CN119588594A